Improved catalytic reactor for the conversion of carbon dioxide and hydrogen to synthesis gas.

The catalytic reactor design addresses RWGS reactor inefficiencies by using refractory and high-temperature alloys with integrated heating, ensuring stable and efficient carbon dioxide conversion to carbon monoxide with reduced emissions.

JP2024541708AActive Publication Date: 2024-11-11INFINIUM TECHNOLOGY LLC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024525083
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-19
Filing Date
2022-11-04
Publication Date
2024-11-11
Estimated Expiration
2042-11-04

AI Technical Summary

Technical Problem

Current RWGS reactors face challenges in achieving stable and efficient conversion of carbon dioxide to carbon monoxide at high temperatures and pressures, with issues related to material selection, thermal management, and energy efficiency, leading to inefficiencies and potential reactor failure due to metal dusting and thermal stress.

Method used

A catalytic reactor design incorporating a refractory layer and high-temperature alloy inner sleeve, with integrated electrical heating elements, maintains consistent temperatures and minimizes adverse reactions, using materials that resist chemical interaction with reactants and products, and employs renewable energy for heating.

Benefits of technology

The design achieves carbon dioxide conversion rates exceeding 75% with minimal temperature drop and high carbon monoxide selectivity, extending reactor lifespan and reducing emissions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024541708000001_ABST
    Figure 2024541708000001_ABST
Patent Text Reader

Abstract

The present invention generally relates to a reactor for producing low carbon synthesis gas from captured carbon dioxide and renewable hydrogen. Hydrogen is produced from water using a renewable electricity powered electrolyzer or from other methods in low carbon hydrogen production. The improved catalytic reactor is energy efficient and robust when operating at temperatures up to 1800°F. Carbon dioxide conversion efficiency is greater than 75% and carbon monoxide selectivity is greater than 98%. The catalytic reactor is constructed of materials that are physically and chemically robust up to 1800°F. As a result, these materials are constructed of materials that do not react with the mixture of hydrogen and carbon dioxide or the products of carbon monoxide and water vapor. The reactor materials are not catalytically active or do not change the physical and chemical composition of the conversion catalyst. Electrical resistance heating elements are incorporated within the catalyst bed of the reactor, so that the internal temperature at any point in the reactor does not drop more than 100°F from the inlet. The catalytic process exhibits less than 0.5% degradation in performance per 1000 operating hours.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an improved catalytic reactor for carrying out endothermic reactions, and in particular to an improved catalytic reactor for efficiently converting carbon dioxide and hydrogen to synthesis gas. The stable and safe operation of the improved catalytic reactor can be maintained over long periods of time under a wide range of operating conditions, with conversions exceeding 75% in some cases. The catalytic reactor is constructed of materials that are physically and chemically robust at temperatures up to 1800°F and that do not react with the reactants hydrogen and carbon dioxide or the products carbon monoxide and water vapor. Separate hydrogen and carbon dioxide streams are compressed, heated to the desired temperature, mixed in the appropriate volumetric ratio, and delivered into the improved catalytic reactor. In another embodiment, hydrogen and carbon dioxide are heated together before being introduced into the catalytic reactor. An integrated reactor heater may utilize both natural gas and electricity to minimize emissions. The reactor design incorporates heating into the catalyst bed to provide thermal energy to the endothermic reaction. Alternatively, the gas may be heated before entering the bed to achieve the desired results without the use of built in heating. [Background technology]

[0002] The adverse effects of greenhouse gas emissions on the climate and ecological environment are becoming increasingly problematic, and what climate scientists have long predicted is becoming clear. Global average temperatures have risen by more than 1°C since pre-industrial times, with some regions warming by more than 5°C (Schuetzle, 2020; Rohde, 2021). Slowing and ultimately halting the rise in global temperatures requires drastic reductions in emissions of carbon dioxide and other greenhouse gases, ultimately to net zero. Carbon capture and utilization technologies, along with drastic reductions in carbon dioxide emissions, are essential components to achieve the Paris Agreement goal of limiting global warming to well below 2°C (Gutierrez et al, 2021).

[0003] Carbon capture and storage (CCS) will play a fundamental role in achieving these goals. Most of the CCS projects currently underway involve the injection of carbon dioxide into sedimentary basins, which require impermeable rocks to inhibit the return of carbon dioxide to the surface. Direct air capture (DAC) is a technology that captures carbon dioxide directly from the air using engineered mechanical systems. Atmospheric carbon dioxide capture has been under consideration for some time, with several small-scale pilot plants in operation (Spector and Dodge, 1946). The plant design usually includes fans and filtration systems that selectively remove the carbon dioxide. The captured carbon dioxide is later released, regenerating the filtration system. Permanent storage of captured carbon dioxide can be achieved by mineral carbonation. In-situ mineralization is a promising avenue for permanent carbon storage, but its large-scale implementation has yet to be explored much beyond pilot- and field-based experiments.

[0004] Carbon dioxide should be considered as a high-value carbon feedstock for the sustainable production of liquid fuels and chemicals. The importance of carbon dioxide utilization in carbon management has long been recognized, and carbon dioxide is predicted to play a key role as a future feedstock in the post-fossil fuel era (Hepburn et al, 2019). Alden and coworkers recently theoretically estimated the potential for carbon dioxide utilization (CDU) to convert carbon dioxide to chemicals to be around 0.3-0.6 GT CO2 / yr in 2050, and the potential for carbon dioxide to fuel CDU to be in the range of up to 1-4.2 GT CO2 / yr. Reverse water gas shift (RWGS) has been proposed and promoted as a potential solution to achieve decarbonization at the scale of several GT CO2 / yr (Artz et al, 2018).

[0005] Carbon dioxide hydrogenation (CO2H) involves the reverse water gas shift (RWGS) reaction and is a technology that converts carbon dioxide into other carbonaceous species such as carbon monoxide, an important precursor for producing liquid fuels and chemicals such as diesel and gasoline.

[0006] Although the CO2H and RWGS reaction approach has the advantages of fast reaction rate, good selectivity, and immediate technical readiness, renewable hydrogen production is required to minimize the carbon footprint. Currently, most hydrogen is produced from fossil fuels by steam reforming of natural gas or gasification of coal, depending on the desired ratio of hydrogen to carbon monoxide. Although this is an important method for hydrogen production for the time being, efforts must be made to reduce carbon dioxide emissions. Combining natural gas reforming with carbon capture, utilization, and storage is a step toward lower emissions. Biomass can also be converted to hydrogen in various ways. Since biomass removes carbon dioxide from the atmosphere, it can have a lower net carbon footprint in a CCS combination. Electricity is also used to produce hydrogen. Electricity is a promising option for carbon-free hydrogen production, as it can be supplied from a variety of renewable energy sources, such as solar, wind, and geothermal.

[0007] The RWGS reaction is a suitable method for sustainable synthesis gas production, especially in producing hydrogen from renewable energy sources such as wind or solar energy. A significant amount of research has been conducted towards the development of an industrial RWGS process, including efficient catalyst systems, reactor units, and even pilot-scale processes. However, there has been little progress in implementing RWGS on an industrial scale. One of the key challenges is the material selection of the reactor, piping, analytical equipment, and instrumentation. Handling carbonaceous gas mixtures remains a challenge at high temperatures and pressures. Another concern is the thermal management of the RWGS reactor to achieve safe and stable operation at high conversion rates for extended periods of time.

[0008] The RWGS reaction (equation 1) is the reversible hydrogenation of carbon dioxide to produce carbon monoxide and water vapor. Carbon dioxide is a relatively unreactive molecule, so the conversion of carbon dioxide to carbon monoxide is endothermic. It is energy intensive and is favored at high temperatures. At low temperatures, the RWGS reaction is favored by methanation, also known as the Sabatier reaction (equation 2). [ka]

[0009] The RWGS reaction is endothermic, requires high temperatures and is heat transfer limited, therefore optimization of heat transfer characteristics and residence time is particularly important in catalytic reactors.

[0010] Although much research has been conducted towards the development of CO2H or RWGS catalytic reactors, there is still a lack of understanding of optimal reactor geometry, thermal management and material selection. For an industrial RWGS reactor to be commercially viable, it must meet the following design and operational requirements: 1. Use catalytic reactor materials that are physically and chemically robust up to 1800°F. 2. The materials used in the walls and equipment of the catalytic reactor do not react adversely with hydrogen, carbon dioxide, carbon monoxide and water vapor. 3. Energy-efficient catalytic reactor heating systems that use renewable or low-carbon electricity. 4. Catalytic reactors and associated piping to minimize carbon production. 5. The linear drop in carbon dioxide conversion is less than 1.0% / 50°F from 1250 to 1750°F. 6. Carbon dioxide conversion is greater than 75% per pass at temperatures above 1250°F. 7. Carbon monoxide selectivity is greater than 98%.

[0011] Commercial reactors used for high temperature reactions are typically constructed of either precast refractory or stainless steel. Their shape is usually a cylindrical metal shell with a thick refractory layer and an inner metal liner. The refractory lining constitutes, by standard, a safety or backup layer behind the working lining that is in contact with the furnace contents. The temperature gradients in the system and the properties of all materials must be carefully considered, as they have different thermal expansion coefficients. The expansion of the refractory must not create excessive stresses that would lead to failure of the lining by cracking the reactor shell. While this is obviously a safety consideration, it also has a significant impact on the life of the reactor.

[0012] A common type of industrial catalytic reactor is for endothermic steam reforming of methane or other hydrocarbons. These endothermic steam reforming reactors consist of hot steel tubes packed with catalyst. The catalytic reactor is typically heated externally using gas burners or electric heaters. A difficulty with this design is that the reactor and tubes are not heated uniformly. This often leads to a reduced lifespan of the reactor shell and tubes. In areas where the reactor temperature is lower than the operating specifications, the conversion efficiency is reduced and carbon deposition can occur. In areas where the temperature is higher than the specifications, the metal can lose its shape and catalyst sintering, melting and surface loss can occur (Eigenberger et al, 2012). Metal dusting, where the metal carburizes and decomposes, is a specific type of corrosion that can occur in reforming reactors when the operating temperature exceeds the design temperature.

[0013] Combining endothermic catalytic reactors in series is known in the current art. Typically, one long endothermic reactor is split into three smaller reactors. The process stream is reheated between the reactors to bring the temperature of the process stream back to the temperature required to convert reactants efficiently and suppress undesirable secondary reactions. For example, in a three-catalyst reactor system, the reactors are typically longer and longer. The first catalyst bed is usually shorter than the next reactor because heat is quickly lost by the process stream, which can lead to undesirable reactions, and therefore the stream needs to be reheated to maintain efficiency (Process Technology and Operator Academy, 2015). Multi-reactor systems have drawbacks such as additional piping and high capital costs.

[0014] To reduce energy usage, the integration of endothermic and exothermic catalytic reactors has been proposed. However, in most cases, such integration is impractical and often involves significant costs (Rahimpour et al, 2012). The integration of endothermic and exothermic reactions is often a more economical means of producing syngas. Maass et al. (2021) disclose a two-section reactor in which coke oven gas is used, where in the first section hydrogen and carbon dioxide are converted to carbon monoxide and steam, and subsequently in the second section this generated steam reforms the hydrocarbons present in the coke oven gas, thereby producing syngas. Such a method requires the initial introduction of heat from an upstream heat source such as a coke oven, and requires the coupling of syngas production with an existing industrial process.

[0015] The use of the reformed gas product stream as a heat source in heat exchange reforming is known in the art. Fuderer (1984) describes an endothermic catalytic reactor in which the hydrocarbon feed is introduced in parallel into a tubular reformer and a heat exchange reformer. Partially reformed gas from the tubular reformer is used as the heat source for the reforming reaction in the heat exchange reformer.

[0016] Some previous studies found that at high temperatures the reactor metallurgy can affect catalyst performance and advised screening catalysts in quartz reactors only. Bustamante et al. (2004) found that an Inconel reactor achieved two orders of magnitude higher carbon dioxide conversion than a quartz reactor due to the catalytic effect of nickel in Inconel 600.

[0017] However, no research has been done to develop optimal metallurgy or refractories specifically addressed to the challenges of endothermic reactors operating at high temperatures, pressures and highly reducing environments, and no research exists that has investigated the long-term use of specific materials and reactor concepts.

[0018] Metal dusting is the carburization that occurs when carbonaceous gases pass over catalytic metal surfaces. The initial formation of powdery coke can impede gas flow, requiring higher pressures and temperature gradients. This is particularly important in industrial heat exchangers. This phenomenon can lead to the formation of metal particles on the material surface, material decomposition, and ultimately catastrophic failure, which is why proper material selection is a unique challenge in RWGS.

[0019] Carbon can form on metal surfaces by reactions such as: [ka] Grabke et al. (1975) and Shatynski et al. (1978) demonstrated that of the above reactions, Equation 3 exhibits the fastest kinetics and results in significant metal dusting in a high-temperature CO-H2 environment. Equation 4 is known as the Boudouard reaction, but is believed to play a minor role due to its relatively slow kinetics.

[0020] Carbon formation also occurs by solid-state reactions involving the dissolution of metal carbides. For iron and steel alloys, Hochman (1977) and Grabke (1999) proposed that carbon formed from metal dusting leads to the formation of cementite M3C (M = Fe, Ni) by diffusion of CO into the metal. Part of the cementite then resists subsequent penetration. Nevertheless, the high carbon activity at the metal surface results in localized nucleation of coke. The reduced carbon activity reduces the stability of Fe3C and Ni3C, which leads to their decomposition. Carbon and metal diffuse to the metal surface, which leads to the formation of more coke and metal particles on the surface. Metal nanoparticles on the surface then act as catalysts to further accelerate this process and material decomposition. Another issue related to the selection of RWGS process materials, the material corrosion mechanism, is a form of internal oxidation of chromium-nickel-iron alloys that causes embrittlement. The term was coined because the fracture surfaces have a green appearance due to the formation of Cr2O3 in various alloys. The newly formed fracture surfaces were green in color due to internal oxide precipitates that caused embrittlement, hence the term "green rot." Summary of the Invention

[0021] The present invention describes an improved commercial-scale catalytic reactor design for the efficient conversion of carbon dioxide and hydrogen mixtures to synthesis gas. The present invention also proposes novel material selection and assembly that can be employed in commercial-scale reactors, heat exchangers and analytical equipment to maximize performance and equipment life. [Brief description of the drawings]

[0022] [Figure 1]FIG. 1 shows an improved catalytic reactor 100. The reactor is comprised of an outer shell 101 capable of withstanding the desired maximum operating pressure, a refractory layer 102 directly inside the metal shell that is chemically unreactive with carbon monoxide, carbon dioxide, hydrogen and water vapor under high temperature and pressure, an inner sleeve 103 made of high temperature alloy and / or alumina, a catalyst bed 104, and an electric resistance heating element 105 embedded in the catalyst bed. Induction heating methods or other types of electric heating methods may also be used. A reactant gas blend 106 of hydrogen and carbon dioxide is fed into the catalytic reactor 100 and maintained at a temperature between 1200°F and 1700°F and a pressure between 0 and 500 psig throughout the reactor. The reactant gas mixture is converted to synthesis gas (hydrogen and carbon monoxide) and water along with unreacted carbon dioxide. [Diagram 2] FIG. 2 shows an embodiment of the catalytic reactor shown in FIG. 1, in which the catalyst bed is divided into multiple short sections 201 with sheathed electrical resistance heating elements 202 between each section. [Diagram 3] Figure 3 shows an embodiment of the catalytic reactor shown in Figure 1, where a heating element 301 is installed vertically within the catalyst bed 302. Induction heating or other forms of electrical heating may also be used. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] The structure of the catalytic reactor 100 is depicted in FIG. 1. The length and width of the reactor may range from 1 to 10 or more feet wide and 1 to 40 or more feet long depending on the desired syngas output. The outer shell 101 is constructed of metals capable of operating at differential pressures of 500 psi or more, including but not limited to carbon steel, stainless steel, and titanium. The outer shell defines the shape of the reactor and may be any shape known in the art of catalytic reactors. The thickness of the outer shell is determined by the desired maximum operating pressure of the reactor and may range from ¼ inch to 10 inches. The outer shell is protected from the corrosive and high temperature reactor internal environment by a refractory layer 102. This layer insulates the reactor so that the surface temperature of the outer shell does not exceed 600°F, more preferably does not exceed 400°F, and even more preferably does not exceed 200°F. The refractory may be made of any insulating material and is composed of materials including, but not limited to, alumina, calcium aluminate, magnesium aluminate, silicon carbide, and silicon nitride.

[0024] The refractory is non-reactive with carbon monoxide, carbon dioxide, hydrogen, and water vapor under operating conditions. In some embodiments, the refractory comprises a catalytically active material. In some embodiments, the refractory layer is comprised of a single layer or multiple sublayers of the same or different types of material. This layer may be cast directly into the reactor using castable refractories or may be comprised of refractory bricks bonded with cement. The total thickness of the refractory layer may vary from 6 to 18 inches.

[0025] In applications where there is a risk of the refractory cracking, an inner sleeve 103 may be installed. The inner sleeve is constructed of a high temperature alloy, including, but not limited to, those shown in Table 1. The material of the inner sleeve may be constructed of alumina. High temperature alloys include materials with a weight percentage of nickel between 29 and 75% and a weight percentage of chromium between 13 and 32%. The inner sleeve can withstand temperatures up to 1800°F and does not react with carbon monoxide, carbon dioxide, hydrogen, and water vapor under reactive conditions. Some of the materials listed may require a passivation treatment to minimize the risk of green lot formation or metal dusting. In some embodiments, this passivation consists of forming an oxide layer to reduce the chemical potential of green lot formation and metal dusting. In some embodiments, the passivation layer or coating may consist of the formation of a stable oxide under reactive conditions. The passivation layer comprises a metal oxide selected from the group including iron oxide, or nickel oxide, or chromium oxide, or cobalt oxide, or molybdenum oxide, or tungsten oxide, or copper oxide, or niobium oxide, or calcium oxide, or magnesium oxide, or alumina, or titania. The passivation layer may contain physical mixtures as well as mixed oxides of the above components. Depending on the type of equipment, the passivation may be established during material construction or during commercial plant start-up before exposure to CO2 and H2. The chemical stability of the alloys used in this application may also be enhanced by forming a nitride passivation layer. The thickness of the passivation layer may vary from a thin passivation of a few microns to deeper in the bulk phase. The thickness and selection of the passivation may be selected according to optimized heat conduction or thermal insulation properties, material strength, and chemical resistance.

[0026] [Table 1]

[0027] In FIG. 1, a reactant gas blend 106 including hydrogen and carbon dioxide is introduced into the reactor through an inlet nozzle 107 at a temperature of 1250-1750°F and a pressure of 0-500 psig. The inlet section 108 of the reactor is left empty to allow the reactant gas stream to fully develop before contacting the catalyst bed 104. Upon contacting the catalyst bed, the hydrogen and carbon oxide gas blend begins to react to produce carbon monoxide and steam. As the endothermic reaction proceeds, the temperature of the gas decreases, but the lost heat is returned to the gas mixture by a heater 105 built into the catalyst bed. The heater is protected by a layer of high temperature alloy, such as the inner sleeve 103, to prevent the process gas mixture from directly contacting the elements. Alternatively, the heater may be housed in a refractory material. The reactant gas blend undergoes conversion to synthesis gas along the reactor until it reaches the outlet nozzle 109. The overall conversion of carbon dioxide at the reactor outlet is at least 75%, and the outlet gas mixture 110 is not more than 100° F. cooler than the inlet gas mixture 106 .

[0028] In some embodiments, the heater 105 is comprised of a resistive electric heating element, a fuel-fired burner, or a combination of the two. The fuel to the firing burner may include natural gas, hydrogen, a combination thereof, or any other suitable fuel. The electric heater is powered from a carbon-free or low-carbon power source, such as wind, solar, geothermal, or nuclear. If a natural gas heater is used, it is incorporated to minimize the combustion of natural gas or other fuel and the emission of carbon dioxide. Combining electric and gas heaters within a single reactor catalyst bed can better optimize the emission of carbon dioxide. Electric heat can be used to bring the catalyst bed to a temperature of 1000-1200°F, thereby reducing the amount of natural gas required to heat the bed to a final temperature of 1600-1800°F.

[0029] In one embodiment of the improved catalytic reactor (FIG. 2), the catalyst bed is divided into multiple short sections 201 with electrical resistance heating elements 202 between each section. A reactant gas blend of hydrogen and carbon monoxide is introduced into the reactor at a temperature of 1250-1750°F and a pressure of 0-500 psig. The gas undergoes an endothermic RWGS reaction in contact with the first catalyst section, decreasing in temperature by less than 100°F along the section. A high temperature alloy sheath 203 passes horizontally through the outer shell and houses one of the resistive electrical heating elements 202. The sheath is positioned between the first and second catalysts and returns the gases to their original temperature. Power to the resistive heating element may be controlled based on the temperature of the gas exiting the first catalyst section. The process gas alternately flows around the heating elements through the remaining catalyst sections until the desired conversion of carbon dioxide is achieved. The number of catalyst sections may vary from 2 to 100. In another embodiment of the improved catalytic reactor, multiple sheaths containing resistive heating elements penetrate the reactor around the periphery in each heating zone and terminate in the center of the reactor. The number of heating elements per zone may vary from 1 to 10 or more.

[0030] In yet another embodiment of the improved catalytic reactor (FIG. 3), the reactor has a single catalyst bed 301 with sheaths 302 housing resistive or other types of electric heating elements 303 that penetrate vertically through the reactor and traverse the entire length of the catalyst bed. These sheaths and elements may enter the reactor through the top, bottom, or both, and the number of these sheaths and elements may vary from 1 to 10 or more. The heating elements 303 provide evenly distributed heat to the catalyst and process gases, thereby maintaining a relatively constant temperature along the reactor, allowing the reactor to operate quasi-isothermally. EXAMPLES

[0031] Example 1: A stream containing carbon dioxide and other waste gases is produced by an industrial process or captured from ambient air. This stream is fed to a carbon dioxide capture facility. The carbon dioxide capture facility uses an adsorbent, such as methyldiethanolamine (MDEA), to capture the carbon dioxide. Relatively pure carbon dioxide is regenerated from the adsorbent by heating.

[0032] Low-carbon electricity from wind, solar, nuclear or other low-carbon sources is available on-site at the carbon capture facility. High-purity water is produced from locally available water. Low-carbon hydrogen is produced from pure water by electrolysis.

[0033] Electrolysis uses low carbon electricity to split water into hydrogen and oxygen gases. The electrolyzer in this example is a proton exchange membrane (PEM) electrolyzer. The electrolyzer produces hydrogen and oxygen at 300 psig each.

[0034] Pressurized hydrogen is electrically heated to 1650° F. and mixed with carbon dioxide that is also compressed to 300 psig and electrically heated to 1650° F. The hydrogen and carbon dioxide are mixed in a volumetric ratio of 3.4 / 1.0 and the flow rate of the mixture is adjusted to provide a gas hourly space velocity of about 15,000 hr-1 in the catalytic reactor.

[0035] Since the catalytic reaction is endothermic, the temperature of the mixture decreases as the reactant gas is converted to synthesis gas on the catalyst bed. In this example, the heating elements are vertically positioned so that the temperature of the reactant gas does not drop more than 50° F. from the inlet at any point in the reactor. In this example, the overall carbon dioxide conversion is 85% and the CO selectivity is 99%. After water is removed from the product stream, the volumetric composition of the dry gas from the catalytic reactor is 72% H2, 4% CO2, and 4% CO2.

[0036] Example 2 A gas blend with a volume ratio of carbon dioxide / hydrogen of 3.0 / 1.0 is introduced into the catalytic reactor at a temperature of 1400° F. and a pressure of 100 psig. The gas flows over the catalyst bed and is reheated by an integrated electric heating element as in Example 1. The conversion of CO2 at the reactor outlet is 75% and the CO selectivity is 99%. After water is removed from the product stream, the volume composition of the dry syngas is 73% H2, 1% CO2 and 6% CO2.

[0037] References US Patent 4,337,170 A1 07 / 1982 Fuderer 7,718,832 B1 05 / 2010 Schuetzle et al. 11,078,077 08 / 2021 Maass et al.

[0038] US Patent Filing 2003 / 0113244 Al 06 / 2003 DuPont et al

[0039] Non-patent literature Artz, J., Muller, TE, Thenert, K., Kleinekorte, J., Meys, R., Sternberg, A., Bardow, A, Leitner, W: Sustainable conversion of carbon dioxide: An integrated review of catalysis and life cycle assessment. Chemical Reviews, 118, 434-504 (2018). Bustamante, F. et al: High-temperature kinetics of the homogeneous reverse water-gas shift reaction, American Institute of Chemical Engineers, AIChE J, 50, 1028-1041 (2004). Eigenberger, G., Ruppel, W.: Catalytic fixed-bed reactors, reaction engineering (part 10), Wiley Online Library, Hoboken, New Jersey (2012). Field, CB; Mach, KJ: Rightsizing carbon dioxide removal, Science 356, 706-707 (2017). Hepburn, C.; Adlen, E.; Beddington, J.; Carter, EA; Fuss, S.; Mac Dowell, N.; Minx, JC; Smith, P.; Williams, CK: The technological and economic prospects for CO2utilization and removal, Nature, 575 (7781), 87- 97 (2019). Gutierrez JM et al: Climate Change 2021: The Physical Science Basis. Intergovernmental Panel on Climate Change (IPCC): Sixth Assessment Report (AR6), August 9, 2021 (www.ipcc.ch / assessment-report / ar6). Mac Dowell, N.; Fennell, PS; Shah, N.: Maitland, GC The role of CO2capture and utilization in mitigating climate change. Nat. Climate Change, 7 (4), 243- 249 (2017). Process Technology and Operator Academy, Endothermic vs. Exothermic Reactors (2015) (www.processtechacademy.com). Ranjbar, A.; Aghamiri, SF Irankhah, A.: Effect of MgAl2O4 catalyst support synthesis method on the catalytic activity of nickel nano catalyst in reverse water gas sift reaction, Iranian Journal of Chemical Engineering, 16, 3 (2019). Rahimpour, MR, Dehnavi, MR, Allahgholipour, F., Iranshahi, D., Jokar, SM: Assessment and comparison of different catalytic coupling exothermic and endothermic reactions: a review, Applied Energy, 99, 496-512 (2012). Rohde, R., Global Temperature Report for 2020, Berkeley Earth (2021). Schuetzle, D.: Historical and predicted global climate changes and some potential accelerated climate moderation approaches, Global Climate Action Summit, San Francisco, CA, 1-42 (2020) (www.researchgate.net). Shukla, PR et al: Climate Change and Land: an IPCC special report on climate change, desertification, land degradation, sustainable land management, food security, and greenhouse gas fluxes in terrestrial ecosystems, 2019 Intergovernmental Panel on Climate Change (2019) (www.ipcc.ch). Spector, N .A., BF Dodge, Removal of carbon dioxide from atmospheric air, Trans. Am. Inst. Chem. Engrs., 42,827-48 (1946)

Claims

1. 1. A catalytic reactor for producing synthesis gas from a mixture of hydrogen and carbon dioxide, comprising: a. an inlet nozzle; b. a metal outer shell between ¼ inch and 10 inches thick; c. a refractory layer having a thickness of 6 to 18 inches, the refractory layer including an insulating material; d. an inner sleeve made from at least one high temperature alloy, said high temperature alloy comprising nickel and chromium, said nickel being 29-75% by weight of said alloy and said chromium being 13-32% by weight of said alloy; e. a catalyst bed capable of converting a mixture of carbon dioxide and hydrogen into carbon monoxide and steam; f. one or more resistive heating elements; g. An outlet nozzle; A catalytic reactor comprising:

2. 10. The catalytic reactor of claim 1, wherein a high temperature alloy sheath extends through the outer shell and houses one of a plurality of resistive electric heating elements.

3. 3. The catalytic reactor of claim 2, wherein the high temperature alloy comprises nickel and chromium, the nickel being 29-75% by weight of the alloy and the chromium being 13-32% by weight of the alloy.

4. 4. The catalytic reactor of claim 3, wherein there are multiple catalytic zones separated by at least one high temperature alloy sheath, and the number of catalytic zones is between 2 and 100.

5. 4. The catalytic reactor of claim 3, wherein the single catalyst bed is horizontally penetrated by a plurality of resistive electric heating elements.

6. 4. The catalytic reactor of claim 3, wherein a single catalyst bed is vertically penetrated by a plurality of resistive electric heating elements.

7. 10. The catalytic reactor of claim 1, wherein the refractory layer comprises one or more layers of alumina, calcium aluminate, magnesium aluminate, silicon carbide, or silicon nitride.

8. 10. The catalytic reactor of claim 1, wherein the surface of the inner sleeve is passivated to reduce the chemical potential of green rot and metal dusting.

9. 8. The catalytic reactor of claim 7, wherein the passivation layer comprises a metal oxide selected from the group consisting of iron oxide, or nickel oxide, or chromium oxide, or cobalt oxide, or molybdenum oxide, or tungsten oxide, or copper oxide, or niobium oxide, or calcium oxide, or magnesium oxide, or alumina, or titania.

10. 4. The catalytic reactor of claim 3, wherein a plurality of sheaths containing resistive electric heating elements penetrate the outer shell around its periphery in each heating zone and terminate in the center of the reactor, wherein the number of heating elements per zone varies from 2 to 10.

11. 1. A catalytic reactor for producing synthesis gas from a mixture of hydrogen and carbon dioxide, comprising: h. an inlet nozzle; i. a metal outer shell between ¼ inch and 10 inches thick; j. a refractory layer having a thickness of 6 to 18 inches, the refractory layer including an insulating material; k. an inner sleeve made from at least one high temperature alloy, said high temperature alloy comprising nickel and chromium, said nickel being 29-75% by weight of said alloy and said chromium being 13-32% by weight of said alloy; l. a catalyst bed capable of converting a mixture of carbon dioxide and hydrogen into carbon monoxide and steam; m. one or more fuel-fired burners; n. outlet nozzle; A catalytic reactor comprising:

12. 1. A method for producing synthesis gas, comprising: a. producing hydrogen by electrolysis using low carbon electricity; b. reacting a stream comprising hydrogen and carbon dioxide in a catalytic reactor, the catalytic reactor comprising: i. an inlet nozzle; ii. a metal outer shell having a thickness between ¼ inch and 10 inches; iii. a refractory layer having a thickness of 6 to 18 inches, the refractory layer including an insulating material; iv. an inner sleeve made from at least one high temperature alloy, said high temperature alloy comprising nickel and chromium, said nickel being 29-75% by weight of said alloy and said chromium being 13-32% by weight of said alloy; v. a catalyst bed capable of converting a mixture of carbon dioxide and hydrogen into carbon monoxide and steam; vi. one or more resistive heating elements; vii. An outlet nozzle; and Including, c. the catalytic reactor is operated at a temperature of 1250-1750° F. and a pressure of 0-500 psig; the carbon dioxide conversion is at least 75% per pass with a CO selectivity greater than 98% to produce a RWGS product stream comprising carbon monoxide; method.

13. 1. A method for producing synthesis gas, comprising: a. producing hydrogen by electrolysis using low carbon electricity; b. reacting a stream comprising hydrogen and carbon dioxide in a catalytic reactor, the catalytic reactor comprising: i. an inlet nozzle; ii. a metal outer shell having a thickness between ¼ inch and 10 inches; iii. a refractory layer having a thickness of 6 to 18 inches, the refractory layer including an insulating material; iv. an inner sleeve made from alumina; v. a catalyst bed capable of converting a mixture of carbon dioxide and hydrogen into carbon monoxide and steam; vi. An outlet nozzle; and Including, c. the catalytic reactor is operated at a temperature of 1250-1750° F. and a pressure of 0-500 psig; the carbon dioxide conversion is at least 75% per pass with a CO selectivity greater than 98% to produce a RWGS product stream comprising carbon monoxide; method.

Citation Information

Patent Citations

  • Catalyst heating device of reformer for fuel battery

    JP2002068704A

  • Reaction vessel for high temperature reaction

    JP2005007239A

  • Steam reforming heated by resistive heating

    JP2021525697A

  • Reverse water gas shift catalytic reactor systems

    US20210340015A1