Method for treating waste plastics
A two-step hydrotreatment process with catalysts like NiMo/Al2O3 and CoMo/Al2O3, combined with hydrocarbon blending, addresses impurity issues in LWP, ensuring catalyst stability and enabling efficient chemical recycling of waste plastics.
Patent Information
- Application Number
- JP2024525487
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-29
- Filing Date
- 2022-10-28
- Publication Date
- 2024-11-11
- Estimated Expiration
- 2042-10-28
AI Technical Summary
Existing methods for treating liquefied waste plastics (LWP) are inefficient in removing impurities, which deactivates catalysts used in subsequent catalytic processes, making chemical recycling of waste plastics economically unviable and technically challenging due to the presence of harmful impurities.
A two-step hydrotreatment process involving mild and severe conditions using catalysts like NiMo/Al2O3 and CoMo/Al2O3, combined with blending with hydrocarbons, to reduce impurities and prepare LWP for further processing, ensuring catalyst stability and continuous operation.
The process effectively reduces harmful impurities in LWP, preserving catalyst activity and enabling economical, continuous chemical recycling of waste plastics into higher-value products.
Smart Images

Figure 2024541709000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for treating waste plastics, in particular to treating liquefied waste plastics by hydrotreating. The method includes removing impurities and hydrotreating LWPs. In particular, the method includes two separate hydrotreating steps of LWPs, where the second hydrotreating step is carried out on a blend of hydrocarbons and already hydrotreated LWPs. [Background technology]
[0002] Environmental concerns and the desire to limit the use of fossil-based feedstocks have created a need to develop the potential of waste plastics. Waste plastics are of growing concern to the environment, as many of the polymers that make up plastics are very stable and do not decompose naturally. Incineration of waste plastics increases greenhouse gases and also causes other environmental problems in the form of air and land pollution. Incineration of waste plastics is primarily considered a waste of valuable raw materials, even when energy is recovered in the form of heat.
[0003] Plastics or polymers are primarily composed of carbon, hydrogen, and heteroatoms such as oxygen and / or nitrogen. However, waste plastics also contain many impurities such as metal and chlorine impurities. There is growing interest in utilizing waste plastics to produce various hydrocarbon components. Although fuels are mixtures of hydrocarbons, the production of liquid fuels from waste plastics is not generally considered useful. Direct incineration of waste plastics also produces energy, which can be recovered and utilized for heating and / or power generation, etc. Thus, there is a need to upgrade waste plastics to high-end hydrocarbon components that can be utilized for the production of new plastics, chemicals, or other materials.
[0004] Waste plastics have been processed by pyrolysis to produce liquefied waste plastics (LWP), but the LWP feed still contains large amounts of various impurities and contaminants and therefore needs to undergo various purification and pre-treatment steps before it can be used as a feedstock for various upgrading processes.
[0005] Patent Document 1 describes a process for treating a feed containing waste plastic pyrolysis oil, which includes a hydrogenation step at a temperature between 100° C. and 250° C., followed by a hydrotreating step at a temperature between 250° C. and 430° C. The resulting product is further separated into a gaseous effluent, an aqueous effluent and a hydrocarbon effluent.
[0006] The present invention provides an improved process for treating and purifying LWPs obtained, for example, by pyrolysis of waste plastics. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] International Publication No. 2021 / 110395 Summary of the Invention
[0008] The present invention aims to provide an optimized solution for the chemical recycling of waste plastics. The present invention seeks to make chemical recycling a viable and economical and thus a complementary solution for recycled waste plastic streams that are not suitable for mechanical recycling. The required chemical processes are conceived to be able to deal with the complexity of the chemical components in the waste product. Waste plastics are, at a general level, very heterogeneous materials. Depending on the type of polymer and in what application it was used, different plastic products will contain different types of additives, e.g. pigments, fillers, flame retardants, etc. When waste plastics are converted into LWP, e.g. via pyrolysis, the polymers and different additives etc. will react / decompose in a specific way and as a result a number of different compounds will be transferred to the product LWP. The conversion of LWP into higher quality value-added products involves the use of catalytic processes and the catalysts commonly used in such processes are sensitive to different impurities, i.e. the activity of the catalyst can be deactivated due to the volume of different catalyst poisons. It has been observed that LWP contains different impurities that are harmful to the catalyst and as a result its further catalytic processing is technically more challenging when compared to, e.g., conventional crude oil. This has led to the present invention, in which these problems are solved by the process steps described in the claims, which allow the processing of waste plastics to be continuous and economical, without worrying about damage and harmful effects caused to the assets carrying out those processes.
[0009] The object of the invention is achieved by a method which is characterized by what is stated in the independent claims. Preferred embodiments of the invention are disclosed in the dependent claims.
[0010] It is therefore an object of the present invention to provide a method for treating liquefied waste plastics (LWP), comprising the steps of: a) hydrotreating a stream of liquefied waste plastics (LWP) in a reactor system comprising at least one reactor each comprising at least one catalyst bed in the presence of hydrogen and a catalyst in a first hydrotreating step at mild hydrotreating conditions to form a stream of hydrotreated LWP; and b) blending said stream of hydrotreated LWP with a stream comprising hydrocarbons to form a mixed stream of hydrotreated LWP and hydrocarbons.
[0011] The present invention will now be described in more detail by way of preferred embodiments with reference to the accompanying drawings. [Brief description of the drawings]
[0012] [Figure 1] Figure 1 is a schematic diagram showing a particular embodiment of the invention. In Figure 1, dotted box = optional step; P1 = product 1; P2 = product 2; A1 / A2 = hydrotreating step a); B = blending step b); C = hydrotreating step c); CF = hydrocarbon stream. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] The present invention relates to a method for treating liquefied waste plastics, wherein the method comprises first hydrotreating LWP under mild conditions and then blending the hydrotreated LWP with a stream comprising hydrocarbons.
[0014] The term "liquefied waste plastic" as used herein means a liquid product produced from any waste plastic through a non-oxidative pyrolysis process. Typically, liquefied waste plastic is produced by the pyrolysis of waste plastic. Other processes for producing LWP include, but are not limited to, hydrothermal liquefaction processes. LWP are a mixture of hydrocarbon-based organic components with a wide range of carbon chain lengths. However, large variations in carbon chain length and chemical structure and properties of LWP depend on the type of plastic (polymer) used in the production of LWP, the type of liquefaction process, and the conditions of the liquefaction process. A typical waste plastic feedstock used in liquefaction processes contains primarily polyethylene with various amounts of polypropylene, polystyrene, and other minor components such as polyamide, polyethylene terephthalate, and polyvinyl chloride.
[0015] Liquefied waste plastics can be obtained by pyrolyzing waste plastics and then recovering the liquid fraction from the pyrolyzed waste plastics. In a typical pyrolysis process, solid waste plastics are heated to a temperature of 400-600°C under non-oxidizing conditions. The polymers pyrolyze and, as a result, release vapors and gases into the gas phase that escape the reactor. This vapor / gas stream is then cooled to condense the LWP products and separate the gases. LWPs typically have a boiling point range that is about 40°C-550°C, which roughly corresponds to the carbon chain length of C5-C55. Depending on the conversion technology, the final boiling point of LWPs can go up to 750°C.
[0016] LWPs are the products of pyrolysis of various polymers and are complex mixtures of mainly paraffins, olefins, naphthenes and aromatic hydrocarbons. The total amount of olefins is typically high, 40 wt.% to 60 wt.%, while the amount of aromatic hydrocarbons is typically less than 20 wt.%. LWPs also contain heteroatoms, e.g. oxygen, nitrogen, chlorine and sulfur, in the form of organic compounds with heteroatom substituents. The amount of heteroatoms varies depending on the polymer used to make the LWPs. Water is usually removed from the LWP product, but some dissolved water may still be present in the LWPs.
[0017] The liquefied waste plastics may also undergo a pretreatment process prior to hydrotreating according to the present invention. The LWP is subjected to a pretreatment step prior to the hydrotreating step a), and the pretreatment step comprises reactive extraction, solvent extraction, adsorption, filtration, centrifugation, oxidation, reduction, or any combination thereof.
[0018] According to the present invention, hydrotreating step a) is defined as the first hydrotreating step carried out on LWP under mild conditions. A stream of liquefied waste plastics (LWP) is subjected to hydrotreating step a) in the presence of hydrogen and a catalyst under mild conditions to form a stream of hydrotreated LWP. The mild conditions in hydrotreating step a) may be a temperature between 100° C. and 350° C., preferably between 170° C. and 340° C. Here, all temperatures in any hydrotreating step are defined as the weighted average temperature of the reactor in which hydrotreating is carried out, unless otherwise stated.
[0019] All hydrotreating described herein is carried out in the presence of at least one catalyst. The catalyst may, for example, comprise at least one component selected from IUPAC Group 6, 8 or 10 of the Periodic Table of Elements. When using a supported catalyst, the catalyst preferably comprises Mo and at least one additional transition metal on a support. Examples of such supported catalysts include, for example, supported NiMo catalysts or supported CoMo catalysts or a mixture of both. In the supported catalysts, the support preferably comprises alumina and / or silica. These catalysts are usually used as sulfided catalysts to ensure that the catalyst is in the active (sulfided) form. Converting the catalysts to their active (sulfided) form can be achieved by pre-sulfiding them (i.e., before starting the hydrotreating reaction) and / or by adding a sulfur-containing feed (containing sulfur, for example, as an organic or inorganic sulfide). The feed may contain sulfur from the beginning, or a sulfur additive may be mixed into the feed. In a preferred embodiment, the hydrotreating uses a catalyst and the catalyst is a supported NiMo catalyst and the support comprises alumina (NiMo / Al2O3) and / or the catalyst is a supported CoMo catalyst and the support comprises alumina (CoMo / Al2O3).
[0020] The catalyst for the hydrotreatment step a) is preferably supported NiMo, where the support preferably comprises alumina and / or silica.
[0021] The conditions for the hydrotreatment step a) are preferably selected from the following: H2 / oil ratio is 200~450Nm 3 / stdm 3 , preferably 220 to 400 Nm 3 / stdm 3 That is, 0.1~2.0h -1 , preferably 0.2 to 0.5 h -1 LHSV, A temperature of 100 to 350°C, preferably 170 to 340°C; The pressure is between 4000 and 6000 kPa(a), preferably between 4800 and 5500 kPa(a).
[0022] In one embodiment of the present invention, the hydrotreating step a) is repeated before the next blending step. The hydrotreating step a) can be repeated to ensure sufficient hydrotreating of the LWP in the stream. The possible need to repeat the hydrotreating step a) depends, among other things, on the hydrotreating conditions, the hydrotreating catalyst, and the reactor design, such as, for example, the number of reactors, the type of catalyst beds and the number of catalyst beds in the reactor.
[0023] In one embodiment of the present invention, the LWP stream consists only of LWP and hydrotreating in step a) is carried out only on the LWP. In this particular embodiment, hydrotreating at mild hydrotreating conditions a) is carried out only on the stream containing only LWP and no other stream is led to the first hydrotreating step (claimed step a)). Hydrotreating step a) in this embodiment is a step in which only the component of the LWP stream originating from waste plastics is hydrotreated at mild hydrotreating conditions.
[0024] In one embodiment of the invention, hydrotreating step a) comprises a step in which a part of the formed stream of hydrotreated LWP from hydrotreating step a) is recycled back to the reactor carrying out hydrotreating step a). If there is a recycle, the amount of recycle depends, inter alia, on the hydrotreating conditions, the hydrotreating catalyst and the reactor design, e.g. the number of reactors, the type of catalyst beds and the number of catalyst beds in the reactor.
[0025] As a result of the hydrotreating step a), a first hydrotreated LWP stream is formed. The formed hydrotreated LWP stream contains less impurities, contaminants and harmful components compared to the LWP feed before hydrotreating. By impurities, contaminants and harmful components is meant herein any material, compound or composition that has properties that are harmful to any component, equipment or catalyst downstream of hydrotreating. Particularly harmful components are compounds containing heteroatoms, metals and metal compounds. Particularly harmful heteroatoms include halogens such as chlorine. Particularly harmful metals include, but are not limited to, mercury, lead, sodium, arsenic, vanadium, iron, zinc and aluminum. Compounds containing silicon, phosphorus, oxygen, nitrogen and sulfur can also be problematic downstream of hydrotreating if not removed. Furthermore, conjugated diolefins and olefins are considered coking or plugging agents that must be minimized from the LWP in order for the treated LWP to be used downstream, for example as a feedstock for steam cracking.
[0026] The objective of hydrotreating a stream of liquefied waste plastics (LWP) according to the present invention is to reduce the risk of adverse and / or harmful properties of any impurities, contaminants and harmful components that may be present in the LWP. The hydrotreating step reduces the amount of these components and therefore reduces the risk and harm that they would otherwise pose to any components, equipment or catalyst downstream of the hydrotreating. After hydrotreating step a) at defined mild hydrotreating conditions, the conjugated diolefins content in the LWP is reduced to less than 0.2 wt.%.
[0027] The process of the present invention further comprises blending the hydrotreated LWP stream resulting from the mild hydrotreating step a) with a hydrocarbon-containing stream, the hydrocarbon being of any origin other than the LWP, and therefore "hydrocarbons" and "hydrocarbons of other origins" are meant as synonyms, so that the hydrocarbon-containing stream will have a different impurity profile than the LWP feed subjected to hydrotreating step a).
[0028] In one embodiment of the present invention, the hydrocarbons of other origin in the form of streams are selected from vacuum gas oil (VGO), gas oil (GO), heavy gas oil (HGO), kerosene, light gas oil, atmospheric residue (AR), vacuum residue (VR) and deasphalted oil (DAO). Other suitable hydrocarbon streams used for blending include, for example, feedstocks derived from crude oil, including at least one crude oil fraction, or bio-based fats or oils or fatty acids, or lignocellulosic-based hydrocarbons, or Fischer-Tropsch or other synthetic hydrocarbons.
[0029] In one embodiment, the hydrocarbon containing stream has one or more of the following characteristics: a boiling point range of 60°C to 700°C, most preferably 100°C to 600°C, where the boiling point can be measured according to ASTM D2887 or EN 15199-2, depending on the boiling point range; A molecular weight, measured according to ASTM D2887, of 250 to 400 g / mol, most preferably 280 to 350 g / mol; an aromatic content, measured according to ASTM D2549, greater than 10 wt.%, most preferably greater than 35 wt.%; Measured according to ENISO12185, 870~940kg / m 3 , and most preferably 890 to 920 kg / m3 density, which is; a sulfur content of less than 5 wt.%, preferably less than 1.8 wt.%; Bromine number according to ISO 3839M less than 10 gBr / 100 g, preferably less than 4 gBr / 100 g; an asphaltene content by TOTAL 642 of less than 300 mg / kg, preferably less than 250 mg / kg; and Silicon content according to ASTM D5185 of less than 2.5 mg / kg, preferably less than 1 mg / kg.
[0030] In one embodiment of the present invention, the mixed stream of hydrotreated LWP and hydrocarbons is kept at a temperature of at least 140° C., preferably the mixed stream containing hydrotreated LWP and hydrocarbons is kept at a temperature between 140° C. and 370° C., more preferably between 200° C. and 350° C., before subjecting the mixed stream to the subsequent hydrotreatment step c). Keeping the mixed stream at an elevated temperature ensures sufficient mixing of the two streams. Mixing at an elevated temperature also ensures that there is no or only minimal precipitation of impurities. The hydrocarbon stream to be blended with the hydrotreated LWP typically has a higher temperature compared to the hydrotreated LWP stream.
[0031] In one embodiment of the present invention, the hydrotreated mixed stream of LWPs and hydrocarbons contains up to 70 wt.% LWPs based on the total weight of the stream, preferably the LWP content in the stream is between 5 wt.% and 70 wt.%, more preferably between 10 wt.% and 50 wt.%, and even more preferably between 15 wt.% and 30 wt.%.
[0032] In one embodiment of the present invention, the method further comprises the steps of: c) hydrotreating said combined stream of hydrotreated LWP and hydrocarbons in the presence of hydrogen and a catalyst at severe hydrotreating conditions to provide a purified stream. Includes.
[0033] The hydrotreating step c) is defined by its demanding conditions, which may be carried out at temperatures between 355° C. and 400° C., preferably between 360° C. and 390° C. Furthermore, the hydrotreating step c) is referred to as the hydrotreating step subsequent to the hydrotreating step a), after the hydrotreated stream of step a) has been blended with other hydrocarbon streams of origin.
[0034] In one embodiment of the present invention, the catalyst of the hydrotreatment steps a) and c) is a supported catalyst, and the catalyst preferably comprises at least one component selected from IUPAC group 6, 8 or 10 of the periodic table of the elements. Furthermore, the supported catalyst may comprise Mo and at least one further transition metal on a support, such as for example a supported NiMo catalyst or a supported CoMo catalyst, where the support preferably comprises alumina and / or silica. In particular, the catalyst is a supported CoMo catalyst and the support comprises alumina (CoMo / Al2O3) and / or the catalyst is a supported NiMo catalyst and the support comprises alumina (NiMo / Al2O3).
[0035] The conditions for the hydrotreatment step c) are preferably selected from the following: The ratio of H2 to oil is 150-400Nm 3 / stdm 3 , preferably 180 to 250 Nm 3 / stdm 3 That is, 0.5~2.0h -1 , preferably 1.1 to 1.5 h -1 LHSV, A temperature of 355 to 400°C, preferably 360 to 390°C; The pressure is between 4000 and 6000 kPa(a), preferably between 4800 and 5500 kPa(a).
[0036] In one embodiment, the hydrotreating steps a) and c) can each be carried out in a single reactor unit comprising at least one catalyst bed. In another embodiment, the hydrotreating steps a) and c) can each be carried out in a reactor system comprising at least two reactor units, each of which comprises at least one catalyst bed.
[0037] In one embodiment of the invention, hydrogen is mixed with the LWP before carrying out the hydrotreatment step a) and / or step c).
[0038] In one embodiment of the present invention, the LWP undergoes a pretreatment step prior to the hydrotreating step a), and the pretreatment step comprises reactive extraction, solvent extraction, adsorption, filtration, centrifugation, oxidation, reduction, or any combination thereof.
[0039] In one embodiment, the method further comprises the steps of adding water to the process and / or removing an aqueous phase from the process after the hydrotreating step a) and / or after the hydrotreating step c). In one embodiment of the invention, water is added to the process after any hydrotreating step to remove impurities. The impurities are or become water soluble in the hydrotreating and can therefore be removed by washing the hydrotreated LWP stream with water. The water soluble impurities are dissolved in the water stream and the aqueous phase containing the impurities is decanted from the hydrotreated LWP stream.
[0040] In one embodiment of the present invention, the method further comprises subjecting the purified stream after hydrotreating step c) to one or more fractionation steps to form two or more product streams. Preferably, the fractionated product streams comprise a naphtha fraction having a 5-95 wt. % boiling range of 30-200°C, preferably about 30°C to about 180°C, more preferably about 30°C to about 110°C, a 5-95 wt. % middle fraction having a boiling range of about 150°C to about 400°C, preferably about 160°C to about 360°C, and more preferably about 160°C to about 330°C, and a liquefied petroleum gas (LPG) fraction comprising one or more of ethane, propane or butane. The naphtha fraction may be further subjected to steam cracking and / or the middle fraction may be further subjected to steam cracking and / or the LPG fraction may be further subjected to steam cracking.
[0041] In a further embodiment of the invention, hydrotreating step a) and hydrotreating step c) are carried out in a reactor system comprising one or more reactors, each reactor having one or more catalyst beds and at least one reactor being equipped with a direct hydrogen feed to the reactor. The reactors designated for hydrotreating steps a) and c) can also each be carried out in separate reactors, each having independent catalyst beds and independent reaction temperatures, or any combination thereof.
[0042] In one embodiment of the invention, it further relates to an LWP product P1 obtainable by hydrotreating an LWP according to hydrotreating step a) and blending according to step b), wherein said product is a reduced amount of silicon, as measured by ICP-MS / MS, to be less than 6 mg / kg, more preferably less than 1 mg / kg, and / or a reduced amount of phosphorus, as measured by ICP-MS / MS, to be less than 5 mg / kg, more preferably less than 1 mg / kg; a low ratio of diolefins to total olefin content, as measured by ASTM D8071, of less than 0.01, more preferably less than 0.001; a low ratio of conjugated diolefins to non-conjugated diolefins, measured by ASTM D8071, of less than 2, more preferably less than 1; Halogen content less than 5mg / kg, preferably less than 1mg / kg Includes.
[0043] Metal determination by ICP-MS / MS is performed on samples which are warmed to liquid state if necessary before weighing, digested with acid in a microwave oven to a clear water / acid matrix, diluted to a specified volume, and analyzed against an acid-based calibration using ICP-MS / MS. Low level elemental results are reported as ppb (μg / kg).
[0044] In one embodiment of the present invention, the method further comprises subjecting the purified stream, i.e. product P1, after hydrotreating step a) and blending step b) to one or more fractionation steps to form two or more product streams. Preferably, the fractionated product streams comprise a naphtha fraction having a 5-95 wt. % boiling range of 30-200°C, preferably about 30°C to about 180°C, more preferably about 30°C to about 110°C, a 5-95 wt. % middle fraction having a boiling range of about 150°C to about 400°C, preferably about 160°C to about 360°C, and more preferably about 160°C to about 330°C, and a liquefied petroleum gas (LPG) fraction comprising one or more of ethane, propane or butane. The naphtha fraction may be further subjected to steam cracking and / or the middle fraction may be further subjected to steam cracking and / or the LPG fraction may be further subjected to steam cracking.
[0045] It is obvious to a person skilled in the art that with the advancement of technology, the concept of the present invention can be implemented in various ways. The present invention and its embodiments are not limited to the examples described above, but can vary within the scope of the claims.
Claims
1. 1. A method for treating liquefied waste plastics (LWP), comprising: Step a) hydrotreating a stream of liquefied waste plastics (LWP) in the presence of hydrogen and a catalyst in a first hydrotreating step at mild hydrotreating conditions in a reactor system comprising at least one reactor each equipped with at least one catalyst bed to form a stream of hydrotreated LWP; step b) blending said hydrotreated LWP stream with a hydrocarbon-containing stream to form a mixed stream of hydrotreated LWP and hydrocarbons. The method includes:
2. The method further comprises step c) hydrotreating the hydrotreated LWP and hydrocarbon mixed stream in the presence of hydrogen and a catalyst at severe hydrotreating conditions to provide a purified stream. The method of claim 1 , comprising:
3. 3. The process of claim 1 or 2, wherein the mild hydrotreating conditions in the hydrotreating step a) comprise a temperature between 100°C and 350°C.
4. A process according to claim 2 or 3, wherein the severe hydrotreating conditions in the hydrotreating step c) comprise a temperature of from 355°C to 400°C.
5. 5. The method of any one of claims 1 to 4, wherein the LWP stream is subjected to a pretreatment step prior to the hydrotreating step a), and wherein the pretreatment step comprises reactive extraction, solvent extraction, adsorption, filtration, centrifugation, oxidation, reduction, or any combination thereof.
6. 6. The method of any one of claims 1 to 5, wherein the hydrocarbon-containing stream is a feedstock derived from crude oil comprising at least one crude oil fraction, or a bio-based fat or oil or fatty acid, or a lignocellulosic based hydrocarbon, or a Fischer-Tropsch hydrocarbon, and the crude oil fraction is selected from a vacuum gas oil (VGO) fraction, a gas oil (GO) fraction, a heavy gas oil (HGO) fraction, a kerosene fraction, a light gas oil fraction, an atmospheric residue (AR) fraction, a vacuum residue (VR) fraction and a deasphalted oil (DAO) fraction.
7. 7. The process according to any one of claims 2 to 6, wherein the mixed stream of hydrotreated LWP and hydrocarbons is kept at a temperature of from 140°C to 370°C before being subjected to hydrotreating step c), preferably the mixed stream of hydrotreated LWP and hydrocarbons is kept at a temperature of from 200°C to 350°C.
8. 8. The method of any one of claims 1 to 7, wherein the hydrotreated LWP and hydrocarbon mixed stream contains up to 70 wt.% LWP, based on the total weight of the stream, preferably the LWP content in the stream is between 5 wt.% and 70 wt.%, more preferably between 10 wt.% and 50 wt.%, and even more preferably between 15 wt.% and 30 wt.%.
9. 9. The process according to any one of claims 1 to 8, wherein the catalyst in the hydrotreatment step a) is a supported catalyst and said catalyst preferably comprises at least one component selected from IUPAC Groups 6, 8 or 10 of the Periodic Table of the Elements.
10. 10. The process of claim 9, wherein the supported catalyst comprises Mo and at least one further transition metal on a support, such as a supported NiMo catalyst or a supported CoMo catalyst, the support preferably comprising alumina and / or silica.
11. The catalyst is a supported CoMo catalyst, and the support comprises alumina (CoMo / Al 2 O 3 ), and / or the catalyst is a supported NiMo catalyst and the support comprises alumina (NiMo / Al 2 O 3 11. The method according to claim 10.
12. 12. The process according to any one of claims 1 to 11, wherein the process further comprises a step of adding water to the process and / or removing an aqueous phase from the process after the hydrotreating step a) and / or after the hydrotreating step c).
13. 13. The method of any one of claims 1 to 12, wherein the hydrotreating step a) is repeated prior to the step of blending the hydrotreated LWP stream with a hydrocarbon-containing stream to form a mixed stream of hydrotreated LWP and hydrocarbons.
14. A process according to any one of the preceding claims, wherein the stream of LWP consists exclusively of LWP and wherein the hydrotreating step a) is carried out exclusively on LWP.
15. The hydrotreating step a) is carried out under the following conditions: H 2 / Oil ratio is 200-450Nm 3 / stdm 3 , preferably 220 to 400 Nm 3 / stdm 3 That is, 0.1 to 2.0 hours -1 , preferably 0.2 to 0.5 h -1 LHSV, A temperature of 100 to 350° C., preferably 170 to 340° C. The method according to any one of claims 1 to 14, wherein the method is carried out at
16. The hydrotreating step c) is carried out under the following conditions: H against oil 2 The ratio is 150 to 400 Nm. 3 / stdm 3 , preferably 180 to 250 Nm 3 / stdm 3 That is, 0.5 to 2.0 hours -1 , preferably 1.0 to 1.5 h -1 LHSV, A temperature between 355 and 400° C., preferably between 360 and 390° C. The method according to any one of claims 2 to 15, wherein the method is carried out at
17. 17. The method of any one of claims 2 to 16, wherein the method further comprises subjecting the refinery stream to one or more fractionation steps to form two or more product streams, preferably the product streams comprise a naphtha cut having 5 to 95 wt. % boiling range of 30 to 200°C, preferably about 30°C to about 180°C, more preferably about 30°C to about 110°C, and a 5 to 95 wt. % middle cut having a boiling range of about 150°C to about 400°C, preferably about 160°C to about 360°C, and more preferably about 160°C to about 330°C.
18. 18. The process of claim 17, wherein the naphtha fraction is further subjected to steam cracking, and / or the middle fraction is further subjected to steam cracking, and / or the LPG fraction is further subjected to steam cracking.
19. 19. The process according to any one of claims 2 to 18, wherein the hydrotreating steps a) and c) are each carried out in a single reactor unit comprising at least one catalyst bed, or the hydrotreating steps a) and c) are each carried out in a reactor system comprising at least two reactor units, each of the reactor units comprising at least one catalyst bed, or a combination thereof.
20. 20. The method of any one of claims 1 to 19, wherein said at least one reactor is equipped with a direct hydrogen quench to the reactor.
21. A process according to any one of claims 2 to 20, wherein hydrogen is mixed with the LWP stream prior to carrying out the hydrotreatment step a) and / or step c).
22. A refined hydrocarbon product obtainable by hydrotreating LWP according to said hydrotreating step a) and blending according to said step b), a reduced amount of silicon, as measured by ICP-MS / MS, to be less than 6 mg / kg, more preferably less than 1 mg / kg, and / or a reduced amount of phosphorus, as measured by ICP-MS / MS, to be less than 5 mg / kg, more preferably less than 1 mg / kg; a low ratio of diolefins to total olefin content, as measured by ASTM D8071, of less than 0.01, more preferably less than 0.001; a low ratio of conjugated diolefins to non-conjugated diolefins, as measured by ASTM D8071, of less than 2, more preferably less than 1; A halogen content of less than 5 mg / kg, preferably less than 1 mg / kg 2. A refined hydrocarbon product comprising:
Citation Information
Patent Citations
Two-step process for converting liquefied waste plastics into steam cracker feed
WO2021105326A1
Optimized method for processing plastic pyrolysis oils for improving their use
WO2021165178A1
Purification of waste plastic based oil with a first trap and a first hydrotreatment and a second trap and a second hydrotreatment
WO2021204819A1
Method for processing plastic pyrolysis oils with a view to their use in a steam-cracking unit
WO2021110395A1
Cited By
Method for producing olefins
JP2026162838A
Olefin production process
JP7814584B1
Olefin production method and hydrogenated product production method