Display device having a watermark formed by a halftone image - Patents.com

The electro-optic display device with microcells of varying fill factors addresses the clumping issue in electrophoretic displays, enabling high-quality watermarks and variable images, enhancing both aesthetics and authentication.

JP2024541868AInactive Publication Date: 2024-11-13E INK CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2024523427
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-19
Filing Date
2022-10-31
Publication Date
2024-11-13
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing electrophoretic display devices struggle with long-term image quality issues due to particle clumping, limiting their widespread adoption for high-quality watermark images.

Method used

The invention introduces an electro-optic display device with a plurality of microcells separated by partition walls, each containing an electrophoretic medium with varying fill factors, forming a halftone image watermark for improved aesthetic and anti-counterfeiting capabilities.

Benefits of technology

The solution enhances the display device's ability to produce high-quality watermarks with improved aesthetic value and authentication, while maintaining variable image display capabilities without the need for external power sources.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024541868000001_ABST
    Figure 2024541868000001_ABST
Patent Text Reader

Abstract

The present invention is directed to a display device comprising a plurality of microcells. The electrophoretic display device comprises a plurality of microcells separated from one another by partitions, each microcell containing an electrophoretic medium. The plurality of microcells comprises different types of microcells having different fill factors. The device comprises a watermark formed from the different types of microcells by a halftone image. The watermark is intended to be used to protect against counterfeiting or for decorative purposes.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application claims priority to U.S. Provisional Patent Application No. 63 / 281,353, filed November 19, 2021. The entire contents of any patents, published applications or other published works referenced herein are incorporated by reference.

[0002] FIELD OF THEINVENTION The present invention is directed to an electrophoretic display device having a watermark. The electrophoretic display device comprises a plurality of microcells separated from one another by partitions, each microcell containing an electrophoretic medium. The watermark is formed by a halftone image from the partitions of the plurality of microcells. Display devices with watermark features are useful for counterfeit protection or decorative purposes. [Background technology]

[0003] BACKGROUND OF THEINVENTION The term "electro-optical," as applied to a material or display or display device, is used herein in its conventional sense in the imaging arts to refer to a material having first and second display states differing in at least one optical property, which can be changed from its first display state to its second display state by application of an electric field to the material. The optical property is usually color perceivable by the human eye, but can be other optical properties such as optical transmission, reflection, emission, or pseudocolor (in the sense of a change in reflection of electromagnetic wavelengths outside the visible range, for displays intended to be machine-readable).

[0004] The term "gray state" is used herein in its conventional sense in the imaging arts to indicate an intermediate state between two extreme optical states of a pixel, and does not necessarily mean a black-and-white transition between these two extreme optical states. For example, some of the E Ink patents and published applications referenced below describe electrophoretic display devices whose intermediate extreme states are white and deep blue, so that in fact an intermediate "gray state" would be light blue. In fact, as already mentioned, a change in optical state may not be a color change at all. The terms "black" and "white" may be used hereinafter to indicate two extreme optical states of a display device, and should be understood to normally include extreme optical states that are not strictly black and white (e.g., the white and deep blue states mentioned above). The term "monochrome" may be used hereinafter to refer to a driving scheme that only drives pixels to those two extreme optical states, with no intermediate gray states.

[0005] Some electro-optic materials are solid in the sense that they have a solid exterior surface, although they can, and often do, have internal liquid- or gas-filled spaces. Such display devices that use solid electro-optic materials may hereinafter be referred to as "solid electro-optic displays" for convenience. Thus, the term "solid electro-optic displays" includes rotating bichromal member displays, encapsulated electrophoretic displays, microcell electrophoretic displays, and encapsulated liquid crystal displays.

[0006] The terms "bistable" and "bistable" are used herein in their conventional sense in the imaging art to refer to a display device having display elements having first and second display states that differ in at least one optical property, such that after a given element is driven to either its first or second display state with an addressing pulse of finite duration, the state persists after the addressing pulse is terminated for at least several times (e.g., at least four times) the minimum duration of the addressing pulse required to change the state of the display element. In U.S. Pat. No. 7,170,670, it is shown that some particle-based electrophoretic display devices capable of gray scale are stable not only in their extreme black and white states, but also in their intermediate gray states, and that the same is true for some other types of electro-optic displays. Display devices of this type are correctly called "multistable" rather than bistable, although for convenience the term "bistable" may be used herein to encompass both bistable and multistable display devices.

[0007] One type of electro-optical display device that has been the subject of intense research and development for many years is the particle-based electrophoretic display device, in which a plurality of electrically charged particles move through a fluid under the influence of an electric field. Electrophoretic display devices can have good brightness and contrast characteristics, wide viewing angles, state bistability, and low power consumption compared to liquid crystal displays. Nevertheless, problems with the long-term image quality of these display devices have prevented their widespread adoption. For example, the particles that make up electrophoretic display devices tend to clump together, resulting in poor service life for these display devices.

[0008] Numerous patents and applications assigned to or in the name of the Massachusetts Institute of Technology (MIT), E Ink Corporation, E Ink California, LCC, and related companies describe various techniques used in encapsulated and microcellular electrophoretic media and other electro-optical media. Encapsulated electrophoretic media comprises a number of small capsules, each of which comprises an internal phase containing electrophoretically mobile particles in a fluid medium and a capsule wall surrounding the internal phase. Typically, the capsules are held in a polymeric binder to form a coherent layer that is positioned between two electrode layers. In microcell electrophoretic displays, the charged particles and fluid are not encapsulated in microcapsules, but instead are held in a number of cavities formed in a carrier medium, usually a polymeric film. Hereinafter, the term "microcavity electrophoretic display" may be used to encompass both encapsulated electrophoretic displays and microcell electrophoretic displays. Techniques described in these patents and applications include:

[0009] (a) Electrophoretic particles, electrophoretic fluids and electrophoretic fluid additives. See, e.g., U.S. Patent No. 7,002,728 and U.S. Patent No. 7,679,814.

[0010] (b) Capsules, binders and encapsulation processes, see, e.g., U.S. Patent No. 6,922,276 and U.S. Patent No. 7,411,719.

[0011] (c) Microcell structures, wall materials and methods of forming the microcells. See, e.g., U.S. Patent No. 7,072,095 and U.S. Patent No. 9,279,906.

[0012] (d) Methods for filling and sealing microcells, see, for example, U.S. Patent Nos. 7,144,942 and 7,715,088.

[0013] (e) Films and subassemblies containing electro-optical materials, see, for example, U.S. Patent Nos. 6,982,178 and 7,839,564.

[0014] (f) Backplanes, adhesive layers and auxiliary layers, and methods used in displays, see, e.g., U.S. Patent No. 7,116,318 and U.S. Patent No. 7,535,624.

[0015] (g) Color formation and color adjustment. See, for example, U.S. Patent No. 7,075,502 and U.S. Patent No. 7,839,564.

[0016] (h) Methods of driving a display, see, e.g., U.S. Patent Nos. 7,012,600 and 7,453,445.

[0017] (i) Display applications, see, for example, U.S. Patent No. 7,312,784 and U.S. Patent No. 8,009,348.

[0018] (j) Non-electrophoretic displays, such as those described in U.S. Patent Application Publication No. 2015 / 0277160, and non-display applications of encapsulation and microcell technology. See, for example, U.S. Patent Application Publication No. 2015 / 0005720 and U.S. Patent Application Publication No. 2016 / 0012710.

[0019] U.S. Patent No. 6,930,818 and U.S. Patent No. 6,795,138 disclose image display devices based on microcell technology. The patents describe the fabrication of microcells, such as display microcells, where the microcells are filled with an electrophoretic fluid. The top openings of the microcells may have the same size and shape, and such microcells may span the entire display surface.

[0020] U.S. Patent No. 9,470,917, U.S. Patent No. 10,401,668, U.S. Patent No. 10,831,052, U.S. Patent No. 9,436,057, U.S. Patent No. 10,073,318, and U.S. Patent No. 10,100,528 disclose an image display device based on microcell technology. The microcells of the image display device are separated by microcell walls. The image display device has a watermark area and a non-watermark area. In the watermark area, the thickness of the partition wall, the height of the partition wall, the top opening of the microcell, the size of the microcell, or the bottom thickness of the microcell are different from those of the microcells in the non-watermark area.

[0021] Prior art displays allow the presence of watermarks due to the existence of two different kinds of microcells in the watermark area. However, they cannot produce realistic and high quality watermark images, which resemble the results of halftoning in the printing field. The present invention achieves results that improve the aesthetic value and counterfeiting ability of watermarks. [Prior art documents] [Patent documents]

[0022] [Patent Document 1] U.S. Patent No. 7,002,728 [Patent Document 2] U.S. Pat. No. 7,679,814 Summary of the Invention [Means for solving the problem]

[0023] One aspect of the invention is directed to an electro-optic display device comprising an electro-optic material layer. The electro-optic material layer comprises a plurality of microcells separated from one another by partitions. Each microcell partition has a surface area. Each microcell of the plurality of microcells has a microcell opening, the microcell opening having a surface area and a fill factor. Each microcell of the plurality of microcells contains an electrophoretic medium, the electrophoretic medium comprising electrically charged pigment particles in a non-polar fluid. The electro-optic display device has a viewing surface, a surface opposite the viewing surface, and a watermark formed from the plurality of microcells with a halftone image. The plurality of microcells comprises more than five types of microcells. Each microcell of a type of microcells has a fill factor that is different from the fill factor of all microcells of other types of microcells. The fill factor of the microcells is determined by Equation 1: Fill factor = A1 / (A1+A2) (Equation 1) A1 is the surface area of ​​the microcell opening and A2 is the surface area of ​​the partition surrounding the microcell.

[0024] The plurality of microcells in the electro-optic material layer of the electro-optic display device may comprise more than six types of microcells, or more than seven types of microcells, or more than eight types of microcells, or more than nine types of microcells, or more than ten types of microcells, or more than twelve types of microcells, or more than fifteen types of microcells. Each microcell of a type of microcell has a fill factor that is different from the fill factor of all the microcells of the other types of microcells. The electro-optic display device may comprise microcells having the same fill factor but different partition heights. The electro-optic display device may comprise microcells having the same fill factor but different microcell shapes.

[0025] The partitions of the electro-optical material layer of the electro-optical display device can be opaque or transparent. The electro-optical display device can include at least two types of partitions, a first type of partitions and a second type of partitions, and the first type of partitions and the second type of partitions have different colors.

[0026] The electro-optic display device may further comprise a first light-transmissive electrode layer and a second electrode layer, with the electro-optic material layer disposed between the first and second electrode layers. The second electrode layer may also be light-transmissive. The first light-transmissive electrode layer may be tinted or untinted. The second light-transmissive electrode layer may be tinted or untinted. The electro-optic display device may further comprise a sealing layer spanning the microcell opening of each of the plurality of microcells. The sealing layer may be disposed between the electro-optic material layer and the second electrode layer. The sealing layer may be opaque or transparent. The sealing layer may be tinted or untinted.

[0027] The electro-optic display device may include an adhesive layer disposed between the sealing layer and the second electrode layer. The adhesive layer may be transparent. The adhesive layer may be colored or colorless. If the partition is transparent, the sealing layer may be transparent, the adhesive layer may be opaque, and the adhesive layer may also be colored. If the partition is transparent, the sealing layer may also be transparent, the adhesive layer may also be transparent, and the second electrode layer may be colored. If the layer is colored, the color of the colored layer may be transparent. may be selected from the group consisting of white, black, grey, green, blue, magenta, cyan, yellow, orange and violet.

[0028] The electro-optic display device may include a piezoelectric layer comprising piezoelectric material, which may be adjacent to a layer of electro-optic material. The electro-optic display device may include a photovoltaic layer for collecting light and powering the device without the need for an external power supply.

[0029] Electro-optic display devices may be used as part of a product, document or currency note for anti-counterfeiting purposes. [Brief description of the drawings]

[0030] [Figure 1] FIG. 1 shows a cross-sectional view of an electro-optic display device comprising a plurality of microcells. [Diagram 2] FIG. 2 illustrates a top view of an electro-optic display device comprising a plurality of microcells. [Diagram 3] 3 and 4 illustrate top views of multiple microcells having different types of microcells. [Figure 4] 3 and 4 illustrate top views of multiple microcells having different types of microcells. [Diagram 5] 5 and 6 illustrate top views of a plurality of microcells having different types of microcells. [Figure 6] 5 and 6 illustrate top views of a plurality of microcells having different types of microcells. [Figure 7] 7 and 8 show examples of devices having a watermark formed by a halftone image. [Figure 8] 7 and 8 show examples of devices having a watermark formed by a halftone image. [Figure 9] 9, 10 and 11 illustrate cross-sectional views of devices containing colored layers. [Figure 10] 9, 10 and 11 illustrate cross-sectional views of devices containing colored layers. [Figure 11] 9, 10 and 11 illustrate cross-sectional views of devices containing colored layers. [Figure 12] FIG. 12 illustrates a method for making the microcell of the present invention using a roll-to-roll process. [Figure 13-1]13A and 13B detail the creation of a microcell for an electro-optic display device using photolithographic exposure through a photomask of a conductive film coated with a thermoset precursor. [Figure 13-2] Figures 13C and 13D list an alternative embodiment in which microcells for an electro-optic display device are fabricated using photolithography, in which a combination of top and bottom exposure is used, with the partitions in one lateral orientation being cured by the top exposure of the photomask and the partitions in the other orientation being cured by the bottom exposure through the opaque base conductive film. [Figure 14] 14A-14D illustrate steps for filling and sealing an array of microcells used in an electro-optic display. [Figure 15] 15A and 15B illustrate an electro-optic display device comprising a piezoelectric layer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0031] (Detailed Description) The present invention has discovered that a watermark can be added to a display device, which can be useful to protect against counterfeiting when security measures are required on the display device. In addition, the watermark can also be used for ornamental design / decoration purposes.

[0032] A watermark is a fixed image that may be present on paper, a document, an electronic display, or other image substrate, usually used for authentication, identification, or aesthetic reasons. Watermarks are sometimes designed to be visible under certain circumstances, such as against a dark background, in reflected light, or in transmitted light, or at certain viewing angles.

[0033] Halftone imaging is a technique used in the publishing industry to create images by using dots of various sizes and spacing. It allows for the creation of extremely high quality images. The term "dot" is not specific to any particular shape. When halftone dots are extremely small, they appear to the human eye as a continuous smooth tone, but under a microscope, individual dots are distinguishable.

[0034] The terms "light-transmitting" and "transparent," referring to layer A, are synonymous and are used herein to mean that a layer so designated transmits sufficient light to enable an observer looking through the layer (such that layer A is between the observer and layer B) to observe the image or color present in layer B. In particular, a light-transmitting or transparent layer transmits 60% or more of the visible light incident on it. If the layer transmits less than 60% of the visible light incident on it, then the layer is opaque.

[0035] An "adhesive layer" of an electro-optic display device is a layer that establishes an adhesive connection between two other layers of the device. The adhesive layer may have a thickness of from 200 nm to 5 mm, or from 1 μm to 100 μm.

[0036] The term "microcell shape" refers to the two-dimensional shape of the microcell opening as seen by an observer looking above the opening.

[0037] The term "diaphragm height" refers to the distance between the bottom of the microcell cavity in the diaphragm and the top diaphragm. It defines the depth of the microcell and is shown in FIG. 1 (108).

[0038] The electro-optic display device of the present invention has a viewing side and an opposite side to the viewing side, as shown in FIG. 1. The electro-optic display comprises an electro-optic material layer 106 comprising a plurality of microcells. Three microcells 101 are shown in the electro-optic display device 100 of FIG. 1. The microcells have a bottom surface 102 and an opening 103, the opening 103 having a boundary. Each microcell may correspond to a number of partitions 104 that separate the microcell from adjacent microcells. The partition height 108 of the microcell defines the depth of the microcell and refers to the distance between the bottom surface of the microcell and the top partition of the partition. The partition height of the microcell may be 0.5 mm to 3 μm, or 300 μm to 5 μm, or 250 μm to 10 μm, or 200 μm to 12 μm, or 100 μm to 15 μm, or 50 μm to 20 μm. The electro-optic material layer 106 of the electro-optic display device 100 may include a sealing layer 120. The sealing layer 120 spans each microcell opening 103. The electro-optic display device may include a substrate 130.

[0039] The microcells of an electro-optic display device contain an electrophoretic medium with electrically charged pigment particles. In the example electro-optic device shown in Figure 1, there are three types of electrically charged pigment particles, depicted as black circles, white circles, and gray circles. The gray circles can represent colors other than white or black.

[0040] Figure 2 illustrates a portion of an electro-optic display device viewed from the side of the display device closer to the microcell openings. Nine microcells (101) are shown in Figure 2. Microcell K (center of Figure 2) is separated from adjacent microcells by partitions 104. The dotted line illustrates the boundary of the opening for microcell K. The surface area of ​​the microcell opening for that microcell K is simply the surface area inside the boundary of the opening.

[0041] The electro-optic display device may include a sealing layer spanning the microcell openings of the electro-optic material layer. The sealing layer seals the electrophoretic medium inside the microcells. The electro-optic material layer may be disposed between a first electrode layer and a second electrode layer. In an electro-optic display device including a sealing layer spanning the openings of each of a plurality of microcells, the electro-optic display device may include an adhesive layer disposed between the sealing layer and the second electrode layer or between the sealing layer and the first electrode layer. The sealing layer may be transparent. The adhesive layer may also be transparent.

[0042] The second electrode layer may comprise multiple electrode layers (pixel electrodes) which can be addressed independently of each other, thus allowing variable images throughout the display device.

[0043] An electro-optic display device may include an electro-optic material layer having six types of microcells, each type having microcells having the same fill factor, each type having a fill factor different from the fill factor of all other types of microcells, the electro-optic display device may include an electro-optic material layer having more than six types of microcells, or more than seven types of microcells, or more than eight types of microcells, or more than nine types of microcells, or more than ten types of microcells, or more than twelve types of microcells, or more than fifteen types of microcells, or more than twenty types of microcells, or more than thirty types of microcells.

[0044] The surface area of ​​the partition of a microcell refers to the area of ​​the surface of the partition, which is in the same plane as the microcell opening or in a plane parallel to the plane of the microcell opening. That is, assuming that an observer can view the microcell opening and the top surface of the partition of the microcell vertically from the side of the device that is closer to the microcell opening (as opposed to the side opposite the bottom surface of the microcell), the surface area of ​​the partition surrounding the microcell can be determined as shown in Figures 3 and 4 and the corresponding description.

[0045] Each microcell in an electro-optic display device has a fill factor. The fill factor of a microcell provides a measure of the surface of the electro-optic material layer that is electro-optically active, meaning that the image displayed on the surface can be changed. The fill factor of the microcell is determined by Equation 1: Fill factor = A1 / (A1+A2) (Equation 1) A1 is the surface area of ​​the microcell opening, and A2 is the surface area of ​​the partition wall surrounding the microcell when viewed from the side of the electro-optic display device closer to the microcell opening (as opposed to the side closer to the bottom of the microcell). The surface area A2 of the partition wall of microcell M (or any microcell) has been determined by the method described below.

[0046] One scenario, illustrated in Figures 3 and 4, involves an electro-optic display device having hexagonal microcell openings. Figures 3 and 4 illustrate views of a portion of the device from the side of the device closer to the microcell openings. In this scenario, microcell M has a microcell opening surface area A1, and microcell M is adjacent to other microcells, including microcell N, which has a microcell opening surface area A1 different from surface area A1. n1 In this case, the surface area A1 of the microcell opening of the microcell M is smaller than the surface area A n1As a first step in the determination of A2, the partition separating microcell M and microcell N is divided by a boundary line B. The boundary line B is defined by a set of points that are d1 away from each point of the boundary of the opening of microcell M and between the two microcells, where d1 is given by Equation 2: d1=[A1 / (A1+A n1 )]×d (Equation 2) d is the distance from the closest point to the boundary of the aperture of microcell N to a point on the boundary of the aperture of microcell M. In other words, microcell N is the microcell whose boundary of the aperture is closest to a particular point on the boundary of the aperture of microcell M.

[0047] The process of defining the boundary line for the partition separating microcell M from all other microcells adjacent to microcell M (other than microcell N) is repeated until the boundary line surrounding microcell N is defined and completed as a closed line. A microcell is considered adjacent to microcell N if any point of the boundary of the aperture of microcell N is closer in distance to any point of the boundary of the aperture of microcell M than any point on the boundary of the aperture of any other microcell in the device.

[0048] In another scenario of the same display device, also shown in FIG. 3, microcell M has a microcell opening surface area A1, and microcell M is adjacent to microcell O. Microcell O has the same microcell opening surface area A1. O1 In this scenario, the boundary line on the surface of the partition separating microcell M and microcell O is divided by boundary line L at the midpoint between the boundary of the opening of microcell M and the boundary of the opening of microcell O. The process of defining the boundary lines for the partition separating microcell M and all other microcells adjacent to microcell M (other than microcell O) is repeated until the boundary line surrounding microcell N is defined and completed as a closed line (see dotted lines in Figures 3 and 4).

[0049] When the boundary line surrounding the microcell is defined, the surface area A2 of the partition can be calculated geometrically or measured graphically for the corresponding microcell. After determining the surface area A2 (which is the surface area of ​​the microcell opening, which is easily calculated geometrically or determined graphically) and the given surface area A1, the fill factor for a particular microcell can be calculated from Equation 1. Each unit area of ​​the partition separating two microcells M, N from each other is calculated as the portion of the surface area (A2) of the partition surrounding the microcell M, or the portion of the surface area (A n2 ) and not part of any other microcell of the plurality of microcells.

[0050] Piezoelectric materials are materials that can generate an electric charge in response to the application of a mechanical load. When a mechanical load is applied to a piezoelectric material, the positive and negative charges concentrate in the material shift, resulting in the generation of an electric field that can be used to operate a device without the need for a battery or external power source. For example, a voltage can be generated by bending a device that includes a piezoelectric material or by introducing a mechanical load. This voltage can be utilized to operate the device. Non-limiting examples of piezoelectric materials include polyvinylidene fluoride (PVDF), quartz (SiO2), berlinite (AlPO4), gallium phosphate (GaPO4), tourmaline, barium titanate (BaTiO3), lead zirconate titanate (PZT), zinc oxide (ZnO), aluminum nitride (AlN), lithium tartanite, lanthanum gallium silicate, and potassium sodium tartrate. Examples of piezoelectric electrophoretic displays are disclosed in U.S. Patent Application No. 16 / 415022, published as U.S. Patent Application Publication No. 2019 / 0352973, which is incorporated by reference herein in its entirety. In the present invention, a layer comprising piezoelectric material can be used to operate an electro-optic display device to drive charged pigment particles in an electrophoretic material layer to change the color state of the electrophoretic display device.

[0051] The electro-optical display device of the present invention can also be a light-concentrating device. That is, it can collect energy for its operation by converting incident light energy into electrical energy. This can be accomplished by including a photovoltaic cell layer at the surface of the electro-optical display device or at or near the surface of the substrate to which the electro-optical display device is attached. Examples of light-concentrating electrophoretic display devices are disclosed in U.S. Patent Application No. 16 / 815,269 and published in U.S. Patent Application Publication No. 2020 / 0295222, which are incorporated by reference herein in their entirety. The electrical energy generated by the incident light energy can drive the charged pigment particles of the electrophoretic material layer to change the color state of the electrophoretic display device.

[0052] The watermark feature is designed with an electro-optic material layer having a number of microcells of different types, each with a different fill factor. The combination of microcells with different fill factors represents a "dot" in a halftone image, which is a technique used in the printing industry to produce high quality images.

[0053] 5, 6, 7, and 8 illustrate top views of an electro-optical display device according to the present invention. FIG. 5 illustrates a device comprising a plurality of microcells with hexagonal openings. The device comprises microcell walls that appear white. All microcells of the device are in a dark state. The plurality of microcells comprises various types of microcells having different fill factors. The lower part of the electro-optical device of FIG. 5 has microcells with a large fill factor, the surface area of ​​the microcell openings being much larger than the surface area of ​​the partition walls surrounding the microcells. Moving from the bottom to the top of the microcells of FIG. 5, the fill factor of the microcells becomes progressively smaller. Thus, the electro-optical display device comprises a number of types of microcells (having different fill factors). In fact, each column of microcells of the device comprises a different type of microcell from every other column, forming a halftone image. This results in the watermark shown in FIG. 5. The fill factor of the microcells of the electro-optic display device of the present invention can be from 0.01 to 0.99, or from 0.10 to 0.90, or from 0.15 to 0.85.

[0054] 6 illustrates a partial top view of an electro-optic display device, showing ten microcells (AJ). In this example, each of the ten microcells has a different fill factor than the other nine microcells. Thus, in this portion of the device, each microcell represents a different type of microcell.

[0055] 7 and 8 illustrate another example of a watermark made from microcells with different types of microcells having different fill factors with halftone images. The watermark made in this manner presents detailed and accurate images, improving the aesthetic value of the device as well as the authentication and anti-counterfeiting capabilities.

[0056] The improved aesthetics and authentication capabilities of the electro-optic display device of the present invention also rely on the fact that the device is capable of displaying a variable image. The electro-optic display device comprises an electro-optic material layer having a plurality of microcells, each of which comprises electrically charged pigment particles that can move in a non-polar fluid toward the viewing side or toward the side opposite the viewing side of the device in response to an electric field applied across the electro-optic material layer. The electric field can be applied via a first electrode layer and a second electrode layer, in which the electro-optic material layer is located between the first electrode layer and the second electrode layer. In this way, each microcell can have a variable color and the device can display a desired image in addition to a fixed watermark image formed by different types of microcells having different fill factors.

[0057] In particular, in one example, the microcells contain an electrophoretic medium with one type of charged pigment particles in a non-polar fluid that may be dyed with a soluble dye or that may be uncolored. When an electrical potential is applied between a first electrode layer and a second electrode layer on the microcell, the charged pigment particles migrate through the electrophoretic medium toward one side of the microcell, causing either the color of the pigment particles or the color of the solvent to be seen from the viewing side.

[0058] In another example, the plurality of microcells includes an electrophoretic medium with two types of charged pigment particles, such as white pigment particles and black pigment particles, in a non-polar fluid. The first type of pigment particles has a first charge polarity and the second type of pigment particles has a second charge polarity, which is opposite to the first charge polarity. In this case, when a voltage difference is imposed between the first and second electrode layers across the microcell, the two types of charged pigment particles move through the electrophoretic medium to opposite ends of the microcell. Thus, one of the colors of the two types of charged pigment particles will be visible at the viewing side of the microcell.

[0059] In another example, the plurality of microcells includes an electrophoretic medium having three types of charged pigment particles (a first type of charged pigment particles, a second type of charged pigment particles, and a third type of charged pigment particles) in a non-polar fluid, where the first type of charged pigment particles and the second type of charged pigment particles have a first charge polarity and the third type of charged pigment particles have a second charge polarity, the second charge polarity being opposite to the first charge polarity.

[0060] In another example, the plurality of microcells includes an electrophoretic medium having four types of charged pigment particles (a first type of charged pigment particles, a second type of charged pigment particles, a third type of charged pigment particles, and a fourth type of charged pigment particles) in a non-polar fluid. The first type of charged pigment particles and the second type of charged pigment particles have a first charge polarity, and the third type of charged pigment particles and the fourth type of charged pigment particles have a second charge polarity, which is opposite to the first charge polarity. The first type of charged pigment particles can have a higher charge than the second type of charged pigment particles, and the third type of charged pigment particles can have a higher charge than the fourth type of charged pigment particles.

[0061] In another example, the plurality of microcells includes an electrophoretic medium having four types of charged pigment particles (a first type of charged pigment particles, a second type of charged pigment particles, a third type of charged pigment particles, and a fourth type of charged pigment particles) in a non-polar fluid. The first type of charged pigment particles, the second type of charged pigment particles, and the third type of charged pigment particles have a first charge polarity and the fourth type of charged pigment particles have a second charge polarity, which is opposite to the first charge polarity. The first type of charged pigment particles can have a higher charge than the second type of charged pigment particles, and the third type of charged pigment particles can have a higher charge than the second type of charged pigment particles.

[0062] In another example, the plurality of microcells contains an electrophoretic medium comprising five or six types of charged pigment particles in a non-polar fluid.

[0063] The charged pigment particles in the electrophoretic medium may comprise charged pigment particles having a color selected from the group consisting of white, black, cyan, magenta, yellow, red, blue, and green.

[0064] The microcell openings may have different shapes, for example, triangles, squares, circles, ellipses, or polygons such as hexagonal (honeycomb) structures. The same electro-optic material layer may have a variety of microcell shapes.

[0065] Each microcell opening of the plurality of microcells may have a microcell width less than 300 μm. The width of the microcell opening is defined as the longest linear distance between two points of the boundary of the microcell opening. The microcell width may be different for each type of microcell. Microcells of the same type may have different widths. The width of the microcell opening may range from 300 μm to 1 μm, or 250 μm to 5 μm, or 200 μm to 10 μm, or 2 mm to 2 μm, or 1 mm to 4 μm, or 800 μm to 8 μm, or 500 μm to 10 μm, or 400 μm to 12 μm, or 300 μm to 15 μm. The partition width (or synonymously, the microcell wall thickness, represented by d in FIG. 4) separating the microcell openings also ranges between 2 mm and 3 μm, or 1 mm and 5 μm, or 800 μm and 8 μm, or 500 μm and 10 μm, or 400 μm and 12 μm, or 300 μm and 15 μm, or 300 μm and 1 μm.

[0066] The electro-optic display device of the present invention may comprise microcells of the microcell type, i.e., microcells having the same fill factor but different partition heights or different shapes. Different wall heights can be achieved by varying the thickness of the bottom of the microcell, i.e., the bottom surface of the microcell can be positioned at different heights inside the microcell.

[0067] The electro-optic display device of the present invention may comprise microcells of different microcell types, i.e., microcells having the same fill factor but different partition colors. In addition, the electro-optic display device of the present invention may comprise different types of microcells (having different fill factors), in which there are two types of microcells with partitions of different colors.

[0068] A watermark created by the present invention may be visible at certain viewing angles and / or under certain lighting conditions, and the watermark will not interfere with the desired regular image displayed (based on the movement of charged pigment particles in the fluid of the electrophoretic medium).

[0069] An example of an electrophoretic display device of the present invention is provided in Figure 9. Figure 9 is a cross-sectional view of a portion of a device 900 including a first electrode layer 910, a microcell 901A and a microcell 901B with partitions 904, a sealing layer 920, an optional adhesive layer 930, and a second electrode layer 940. The device has a viewing side and a side opposite the viewing side. In this example, the sealing layer may be located closer to the side of the device away from the viewing side in relation to the microcell cavities that contain the electrophoretic medium. However, in other device examples, the sealing layer may be located closer to the viewing side in relation to the microcell cavities that contain the electrophoretic medium.

[0070] In a first embodiment of the invention, the partitions are opaque. The opaque partitions of the device may all have a single color, or various partitions throughout the device may have different colors.

[0071] In a second embodiment of the invention, the partition may be transparent. In this second embodiment, the device may include a colored layer, which may enhance the appearance of the watermark. The sealing layer may also be opaque or transparent. In the example illustrated in FIG. 9, the sealing layer may be opaque and may be located closer to the side of the device away from the viewing side in relation to the microcell cavity containing the electrophoretic medium. In this example, the sealing layer may be colored. If the first electrode layer and the partition were transparent, the color of the opaque sealing layer would be visible to an observer looking from the viewing side of the device. That is, the watermark would appear to have the color of the sealing layer. The watermark would be visible to an observer when the optical state of the electrophoretic medium of the associated microcell is distinguishable from the optical state of the sealing layer.

[0072] In another example of the second embodiment of the electro-optic display device, the sealing layer is transparent. In this example, the device includes an adhesive layer located between the sealing layer and the second electrode layer. The adhesive layer can be opaque. This example is illustrated in FIG. 10, where the sealing layer is transparent and the adhesive layer is opaque. FIG. 10 illustrates a side view of an electro-optic display device 1000 including a first electrode 1010, a microcell 1001 having a partition 1004, a sealing layer 1020, an adhesive layer 1030, and a second electrode layer 1040. In this example of the electro-optic display device 1000, the adhesive layer 1030 can be colored. If the first electrode layer 1010, the partition 1004, and the sealing layer 1020 were all transparent, the color of the opaque adhesive layer 1030 would be visible to an observer looking from the viewing side of the device. That is, the watermark would appear to have the color of the adhesive layer 1030. A watermark will be visible to an observer when the state of the electrophoretic medium of the associated microcell is distinguishable from the state of the adhesive layer 1030. The color appearance of the watermark can be further controllably modified by including a dye in the transparent sealing layer 1020.

[0073] In yet another example of the second embodiment of the electro-optic display device, both the sealing layer and the adhesive layer are transparent. The second electrode layer can be opaque. This example is illustrated in FIG. 11, where the sealing layer and the adhesive layer are transparent and the second electrode layer is opaque. FIG. 11 illustrates a side view of an electro-optic display device 1100 comprising a first electrode layer 1101, a microcell 1011 having a partition 1104, a sealing layer 1120, an adhesive layer 1130, and a second electrode layer 1140. In this case, the second electrode layer 1140 can be colored. If the first electrode layer 1110, the partition 1104, the sealing layer 1120, and the adhesive layer 1130 were all transparent, the color of the opaque second electrode layer 1140 would be visible to an observer looking from the viewing side of the device. That is, the watermark would appear to have the color of the adhesive layer 1130. The watermark will be visible to an observer if the state of the electrophoretic medium of the associated microcell is distinguishable from the state of the second electrode layer. The color appearance of the watermark may be further controllably modified by including a dye in the transparent sealing layer 1120 and / or the transparent adhesive layer 1130.

[0074] If the sealing layer is located closer to the viewing side of the device, relative to the microcell cavity containing the electrophoretic medium, then the sealing layer is transparent. In this case, an analysis of the consents would show that the layer located on the other side of the electro-optical material layer, relative to the sealing layer, could be tinted.

[0075] In another example, the electro-optic display device of the present invention may comprise a first light-transmitting electrode layer, an electro-optic material comprising a plurality of microcells, an optional sealing layer, an optional adhesive layer, and a second light-transmitting electrode layer. The plurality of microcells are separated from one another by transparent partitions, each microcell of the plurality of microcells having an aperture and containing an electrophoretic medium, the electrophoretic medium comprising charged pigment particles in a non-polar fluid. The watermark is formed from the plurality of microcells by a halftone image, in which the plurality of microcells comprises more than five types of microcells, each type of microcell having a fill factor different from all other types. In this example, the partitions have the color of the substrate to which the device is attached. The substrate may be a printed image, making the appearance of the watermark highly complex, potentially enhancing the aesthetic and authentication value of the device. Furthermore, two or more such devices, similar or dissimilar, may be stacked onto the substrate, enhancing the complexity and value of the watermark even further.

[0076] If the electro-optic display device includes a colored layer, the color may be selected from the group consisting of white, black, gray, magenta, cyan, yellow, blue, green, red, orange, violet, and combinations thereof. The layer may also have a metallic shade.

[0077] Methods of Constructing Microcells Microcells can be formed in either a batch process or a roll-to-roll process as disclosed in U.S. Pat. No. 6,933,098. The latter offers a sustainable, low-cost, high-throughput manufacturing technique for the generation of compartments for use in a variety of applications, including electro-optic display devices. Microcell arrays suitable for use with the present invention can be made using microembossing, as illustrated in FIG. 12. A male mold 1220 can be placed either above the web 1240 as shown in FIG. 12 or below the web 1240 (not shown), although alternative arrangements are possible. See U.S. Pat. No. 7,715,088, which is incorporated by reference herein in its entirety. A conductive substrate can be constructed by forming a conductive film 1210 (first electrode) on a polymer substrate that will become the backside of the device. A composition comprising a thermoplastic, a thermoset, or a precursor thereof 1220 is then coated onto the conductive film. The thermoplastic or thermoset precursor layer is embossed by a male mold in the form of a roller, plate or belt at a temperature above the glass transition temperature of the thermoplastic or thermoset precursor layer.

[0078] The thermoplastic or thermosetting resin precursors for the preparation of the microcells can be multifunctional acrylates or methacrylates, vinyl ethers, epoxides and oligomers or polymers thereof, and the like. The combination of multifunctional epoxides and multifunctional acrylates is also very useful to achieve the desired physical-mechanical properties. Crosslinkable oligomers, such as urethane acrylates or polyester acrylates, that confer flexibility can be added to improve the bending resistance of the embossed microcells. The composition can contain only polymers, oligomers, monomers and additives, or oligomers, monomers and additives. The glass transition temperature (or T) of this class of materials is g) usually ranges from about -70°C to about 150°C, preferably from about -20°C to about 50°C. The microembossing process is usually g A heated male mold or a heated housing substrate against which the mold presses can be used to control the microembossing temperature and pressure.

[0079] The mold is released during or after the precursor layer has cured to reveal an array of microcells 1230, as shown in FIG. 12. The precursor layer can be cured by cooling, solvent evaporation, crosslinking by radiation, heat or moisture. If the thermosetting resin precursor is cured by UV radiation, the UV can radiate from the bottom or top of the web onto the transparent conductive film. Alternatively, a UV lamp can be placed inside the mold. In this case, the mold must be transparent to allow the UV light to radiate through the pre-patterned male mold onto the thermosetting resin precursor layer. The male mold can be prepared by any suitable method, such as a diamond cutting process or a photoresist process followed by either etching or electroplating. A master template of the male mold can be manufactured by any suitable method, such as electroplating. In electroplating, a glass base is sputtered with a thin layer (usually 3000 Å) of a seed metal such as chrome Inconel. The mold is then coated with a layer of photoresist and exposed to UV. A mask is placed between the UV and the layer of photoresist. The exposed areas of photoresist are hardened. The unexposed areas are then removed by washing them with a suitable solvent. The remaining hardened photoresist is dried and sputtered again with a thin layer of seed metal. The master is then ready for electroforming. The usual material used for electroforming is nickel-cobalt. Alternatively, the master can be made of nickel by electroforming or electroless nickel plating. The bottom surface of the mold is usually between about 50 microns and 400 microns. The master can also be made using other microengineering techniques including laser interference, electron beam writing, dry etching, chemical etching or laser writing, as described in “Replication techniques for micro-optics”, SPIE Proc. Vol. 3099, pp. 76-82 (1997). Alternatively, the mold can be made by photo-machining using plastics, ceramics or metals.

[0080] Prior to applying the UV curable resin composition, the mold may be treated with a release agent that aids in the demolding process. The UV curable resin may be degassed prior to dispensing and may optionally contain a solvent. The solvent, if present, evaporates easily. The UV curable resin is dispensed by any suitable means, such as coating, dipping, pouring, or the like, over the male mold. The dispenser may be moving or stationary. A conductive film is overlaid with the UV curable resin. Pressure may be applied, if necessary, to ensure proper bonding between the resin and the plastic and to control the thickness of the bottom surface of the microcell. The pressure may be applied using a laminating roller, vacuum forming, pressing device, or other similar means. If the male mold is metallic and opaque, the plastic substrate is transparent to the actinic radiation that is normally used to cure the resin. Conversely, the male mold can be transparent and the plastic substrate opaque to actinic radiation. To obtain good transfer of the molded features onto the transfer sheet, the conductive film needs to have good adhesion to the UV cured resin, which should have good release properties from the mold surface.

[0081] (Photolithography) Microcells can also be produced using photolithography. A photolithography process for fabricating a microcell array is illustrated in Figures 13A and 13B. As illustrated in Figures 13A and 13B, a microcell array 1340 can be prepared by exposure through a mask 1346 to UV light (or alternatively other forms of radiation, e-beam and the like) of a radiation curable material 1341a coated by known methods onto a conductive electrode film 1342 to form partitions 1341b corresponding to an image projected through the mask 1346. The base conductive film 1342 is mounted on a supporting substrate base web 1343, preferably (which may comprise a plastic material).

[0082] In the photomask 1346 in Fig. 13A, the dark squares 1344 represent the opaque areas and the spaces between the dark squares represent the transparent areas 1345 of the mask 1346. The UV radiates through the transparent areas 1345 onto the radiation curable material 1341a. The exposure is preferably direct onto the radiation curable material 1341a, i.e. the UV does not pass through the substrate 1343 or the base conductor 1342 (top exposure). For this reason, neither the substrate 1343 nor the conductor 1342 need to be transparent to the UV or other employed radiation wavelengths.

[0083] As shown in Figure 13B, the exposed areas 1341b are cured, at which time the unexposed areas (protected by the opaque areas 1344 of the mask 1346) are removed to form the microcells 1347 with a suitable solvent or developer. The solvent or developer is selected from those commonly used to dissolve or reduce the viscosity of radiation curable materials, such as methyl ethyl ketone (MEK), toluene, acetone, isopropanol, or the like. Preparation of the microcells can be similarly accomplished by placing a photomask under the conductive film / substrate supporting the web, in which case the UV light emanating from the bottom and the substrate through the photomask must be transparent to the radiation.

[0084] Image exposure Yet another alternative method of preparing the microcells of the present invention by image exposure is illustrated in Figures 13C and 13D. When opaque conductive lines are used, the conductive lines can be used as a photomask for exposure from the bottom. Durable microcell partitions are formed by additional exposure from the top through a second photomask having opaque lines perpendicular to the conductive lines. Figure 13C illustrates the use of both top and bottom exposure principles to produce a microcell array 1350 of the present invention. The base conductive film 1352 is opaque and patterned in lines. The radiation curable material 1351a coated on the base conductor 1352 and substrate 1353 is exposed from the bottom through the conductive line pattern 1352 (which functions as the first photomask). A second exposure is performed from the "top" side through a second photomask 1356 having a linear pattern perpendicular to the conductive lines 1352. The spaces 1355 between the lines 1354 are substantially transparent to UV light. In this process, the partition material 1351b cures from the bottom up in one lateral direction and cures from the top down in the orthogonal direction, combining to form complete microcells 1357. As shown in Figure 13D, the unexposed areas are then removed with a solvent or developer, as described above, to reveal the microcells 1357.

[0085] The microcell has good compatibility with the microcell and does not affect the electrophoretic medium. ) thermoplastic elastomers. Examples of useful thermoplastic elastomers include diblock, triblock and multiblock copolymers ABA and (AB) nIn the present invention, the following types of styrene, α-methylstyrene, ethylene, propylene or norbornene are included: A is styrene, α-methylstyrene, ethylene, propylene, butylene, dimethylsiloxane or propylene sulfide; and A and B cannot be the same chemical formula. The number n is ≧1, preferably 1 to 10. Particularly useful are diblock or triblock copolymers of styrene or ox-methylstyrene, such as SB (poly(styrene-b-butadiene)), SBS (poly(styrene-b-butadiene-styrene)), SIS (poly(styrene-b-isoprene-b-styrene)), SEBS (poly(styrene-b-ethylene / butylene-b-styrene)). Poly(styrene-b-dimethylsiloxane-b-styrene), poly(α-methylstyrene-b-isoprene), poly(α-methylstyrene-b-isoprene-b-α-methylstyrene), poly(α-methylstyrene-b-propylene sulfide-b-α-methylstyrene), poly(α-methylstyrene-b-dimethylsiloxane-b-α-methylstyrene). Particularly useful are commercially available styrene block copolymers, such as the Kraton D and G series (manufactured by Kraton Polymer, Houston, Tex.). Crystalline rubbers such as poly(ethylene-co-propylene-co-5-methylene-2-norbornene) or EPDM (ethylene propylene diene terpolymer) rubbers such as Vistalon 6505 (manufactured by Exxon Mobil, Houston, Tex.) and graft copolymers thereof have also been found to be very useful.

[0086] The thermoplastic elastomer may be dissolved in a solvent or solvent mixture that is immiscible with the display fluid in the microcell and elicits a specific attraction that is less than that of the display fluid. Low surface tension solvents are preferred in the overcoating composition due to their better wetting properties over the microcell partition and the electrophoretic fluid. Solvents or solvent mixtures having a surface tension of less than 35 dyne / cm are preferred. Surface tensions of less than 30 dyne / cm are more preferred. Suitable solvents include alkanes (preferably C 2 O 4 , such as heptane, octane, or Isopar solvents from Exxon Chemical Company). 6-12 Alkanes, nonanes, decanes and their isomers), cycloalkanes (preferably C such as cyclohexane and decalin and the like). 6-12 Cycloalkanes), alkylbenzenes (preferably mono C such as toluene, xylene and the like) 1-6 Alkylbenzene or DiC 1-6 alkylbenzenes), alkyl esters (preferably C such as ethyl acetate, isobutyl acetate and the like) 2-5 alkyl esters) and (such as isopropanol and the like and their isomers) C 3-5 Mixtures of alkyl benzenes and alkanes are particularly useful.

[0087] In addition to the polymer additive, the polymer mixture also contains a wetting agent (surfactant). Wetting agents (such as FC surfactants from 3M Company, Zonyl fluorosurfactants from DuPont, fluoroacrylic acids, fluoromethacrylic acids, fluorine-substituted long chain alcohols, prefluorinated long chain carboxylic acids and their derivatives, and Silwet Silicone surfactants from OSi (Greenwich, Conn.)) can also be included in the composition to improve adhesion of the sealant to the microcells and provide a more flexible coating process. Other materials including crosslinking agents (e.g., bisazides such as 4,4'-diazidodiphenylmetal and 2,6-di(4'-azidobenzal)-4-methylcyclohexanone), vulcanizing agents (e.g., 2-benzithiazolyl disulfide and tetramethylthiuram disulfide), multifunctional monomers or oligomers (e.g., hexanediol, diacrylates, trimethylolpropane, triacrylates, divinylbenzene, diallylphthalene), thermal initiators (e.g., dilauroyl peroxide, benzoyl peroxide) and photoinitiators (e.g., isopropylthioxanthene (ITX), Irgacure 651 and Irgacure 369 from Ciba-Geigy) are also very useful to enhance the physical and mechanical properties of the sealing layer by crosslinking or polymerization reactions during or after the overcoating process.

[0088] After the microcells are generated, they are filled with an appropriate electrophoretic medium. The microcell array 1460 may be prepared by any of the methods described above. As shown in cross section in Figures 14A-14D, the partitions 1461 of the microcells extend upward from the substrate 1463 to form open cells. The microcells may include a primer layer 1462 to passivate the mixture so that the microcell material does not interact with the mixture containing the electrophoretic medium 1465.

[0089] The microcells are then filled with an electrophoretic medium 1464 comprising electrically charged pigment particles 1465 in a non-polar fluid. The microcells can be filled using a variety of techniques. In some examples, blade coating can be used to fill the microcells to the depth of the microcell partitions 1461. In other examples, inkjet type microinjection can be used to fill the microcells. In yet other examples, a microneedle array can be used to fill an array of microcells.

[0090] After filling, the microcell is sealed by applying polymer 1466, which becomes a sealing layer, as shown in FIG. 14C. In some examples, the sealing process may involve exposure to heat, dry hot air, or UV radiation. Polymer 1466 is compatible with the electrophoretic medium, but is not dissolved by the fluid of electrophoretic medium 1464, making the final microcell structure nearly impervious to leakage and able to withstand bending without delamination.

[0091] A variety of individual microcells can be filled with the desired electrophoretic medium by repeatedly using photolithography, a process that typically involves coating an array of empty microcells with a layer of positive-working photoresist, selectively opening a certain number of the microcells by imagewise exposing the positive photoresist, subsequently developing the photoresist, filling the opened microcells with the desired mixture, and sealing the filled microcells by a sealing process.

[0092] After the microcells 1460 are filled, the sealed array may be laminated with a finishing layer 1468, preferably by pre-coating the finishing layer 1468 with an adhesive layer, which may be a pressure sensitive adhesive, a hot melt adhesive, or a heat, moisture or radiation curable adhesive. The laminating adhesive may be post-cured by radiation, such as UV, through a top conductive film, if the latter is transparent to the radiation.

[0093] The electro-optical display device of the device may comprise a piezoelectric layer, allowing the device to operate with the need for an external energy supply. FIG. 15A illustrates an example of such a device. The electro-optical display 1500 of FIG. 15 comprises a first electrode 1510, a second electrode 1540, a piezoelectric layer 1580 comprising a piezoelectric material, and an electro-optical material layer 1560 comprising a plurality of microcells. The device may also comprise one or more adhesive layers to bond two adjacent layers together. The one or more adhesive layers may be transparent. At least one of the electrode layers is optically transparent. Both electrode layers may be optically transparent. That is, all layers of the device 1500 may be transparent. If that is the case, the display image may be viewed from both sides. Application of a mechanical load to the piezoelectric layer (e.g., by bending the device) creates an electrical potential that can be utilized to cause the movement of the pigments of the electrophoretic material. That is, the optical state of the device may change. This type of device with a piezoelectric layer may operate without an external power source such as a battery.

[0094] Another example of an electro-optic display device with piezoelectric is provided in electro-optic display 1501 in FIG. 15B. The display device comprises a first electrode 1511, a second electrode 1541, an electro-optic material layer 1561 comprising a plurality of microcells, and a piezoelectric layer comprising piezoelectric material 1581. The device may also comprise one or more adhesive layers to bond two adjacent layers together. The one or more adhesive layers may be transparent. At least one of the electrode layers is light-transmitting. Both electrode layers may be light-transmitting. That is, all layers of device 1501 may be transparent. If that is the case, the display image may be viewed from both sides. Application of a mechanical load to the piezoelectric layer (e.g., by bending the device) creates an electric potential that can be utilized to cause the movement of the pigments of the electrophoretic material. That is, the optical state of the device may change. This type of device with a piezoelectric layer may operate without an external power source such as a battery.

[0095] Although the present invention has been described with reference to specific examples thereof, it should be understood by those skilled in the art that various changes may be made and equivalents may be substituted without departing from the scope of the invention. In addition, many modifications may be made to adapt a particular situation, material, composition of matter, process, process step(s) to the objective and scope of the present invention. All such modifications are intended to be within the scope of the claims appended hereto.

Claims

1. 1. An electro-optic display device comprising an electro-optic material layer, the electro-optic material layer comprising a plurality of microcells, the plurality of microcells being separated from one another by partitions, the partitions of each microcell having a surface area, each microcell of the plurality of microcells having a microcell opening, the microcell opening having a surface area and a fill factor, each microcell of the plurality of microcells including an electrophoretic medium, the electrophoretic medium comprising charged pigment particles in a non-polar fluid, the electro-optic display device having a view side, an opposite side to the view side, and a watermark formed from the plurality of microcells by a halftone image, the plurality of microcells comprising more than five types of microcells, each microcell of a type having a fill factor different from the fill factors of all microcells of other types, the fill factor of a microcell being determined by Equation 1, Fill factor = A 1 / (A 1 +A 2 ) (Formula 1) A 1 is the surface area of ​​the microcell opening, and A 2 is the surface area of ​​the partition surrounding the microcell.

2. 2. The electro-optic display device of claim 1, wherein the plurality of microcells comprises more than six types of microcells, each microcell of a type having a fill factor different from the fill factor of all microcells of other types of microcells.

3. 10. The electro-optic display device of claim 1, wherein the electro-optic display device comprises microcells having the same fill factor but different partition heights.

4. 10. The electro-optic display device of claim 1, wherein the electro-optic display device comprises microcells having the same fill factor but different microcell shapes.

5. 10. The electro-optic display device of claim 1, wherein said partition walls are transparent.

6. 10. The electro-optic display device of claim 1, wherein said partitions are opaque.

7. 2. The electro-optic display device of claim 1, wherein the electro-optic display device comprises at least two types of partitions, a first type of partitions and a second type of partitions, the first type of partitions and the second type of partitions having different colors.

8. 10. The electro-optic display device of claim 1 further comprising a first light-transmissive electrode layer and a second electrode layer, the electro-optic material layer being disposed between the first light-transmissive electrode layer and the second electrode layer.

9. 9. The electro-optic display device of claim 8 wherein the second electrode layer is light transmissive.

10. 9. The electro-optic display device of claim 8 wherein the second electrode layer is tinted.

11. 9. The electro-optic display device of claim 8 further comprising a sealing layer spanning the opening of each microcell of the plurality of microcells, the sealing layer being disposed between the electro-optic material layer and the second electrode layer.

12. 12. The electro-optic display device of claim 11 wherein the sealing layer is transparent.

13. 12. The electro-optic display device of claim 11 wherein the sealing layer is tinted.

14. 12. The electro-optic display device of claim 11, further comprising an adhesive layer disposed between the sealing layer and the second electrode layer.

15. 15. The electro-optic display device of claim 14 wherein the adhesive layer is transparent.

16. 15. The electro-optic display device of claim 14 wherein the adhesive layer is tinted.

17. 10. The electro-optic display device of claim 1 further comprising a piezoelectric layer comprising piezoelectric material.

18. 20. The electro-optic display device of claim 17, wherein the piezoelectric layer is located adjacent to the electro-optic material layer.

19. 8. The electro-optic display device of claim 7 further comprising a photovoltaic layer.

20. 10. The electro-optic display device of claim 1, wherein the electro-optic display device is used as part of a product, document or currency note for anti-counterfeiting purposes.

Citation Information

Patent Citations

  • Appearance alteration device, method for manufacturing such device, and equipment covered by such device.

    JP2011524548A

  • Display panel with pre-patterned image

    JP2016532163A

  • Piezoelectric electrophoretic display

    JP2021517671A

  • Display device with watermark

    US20130321744A1

  • Updating a display by applying pressure

    US20170285828A1