Apparatus and method for determining chiral optical properties from third-harmonic Mie scattering of semiconductor nanohelices

Third harmonic Mie scattering from chiral semiconductor nanoparticles allows for efficient characterization of chiral optical properties in ultrasmall volumes, addressing the limitations of traditional spectroscopy methods by enabling rapid, high-throughput analysis of chiral compounds in small volumes.

JP2024542786AActive Publication Date: 2024-11-15THE RGT UNIV OF MICHIGAN +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2024533022
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-12-01
Filing Date
2022-12-01
Publication Date
2024-11-15
Estimated Expiration
2042-12-01

AI Technical Summary

Technical Problem

Current optical spectroscopy methods for determining chiral optical properties require large sample volumes, making them incompatible with high-throughput synthesis and analysis of large chemical libraries, particularly in ultrasmall volumes such as 1-microliter droplets, and are technically complex for combinatorial nanochemistry applications.

Method used

The use of third harmonic Mie scattering (THMS) from chiral semiconductor nanoparticles, specifically CdTe nanohelices, to detect chiral properties in volumes as small as 1 microliter or less, utilizing circularly polarized light to generate forward-directed third harmonic radiation.

Benefits of technology

Enables rapid, high-throughput characterization of chiral nanostructures in ultrasmall volumes, providing a novel optical tool for analyzing chiral compounds in microscopic volumes with enhanced sensitivity and directionality, suitable for combinatorial chemical synthesis and analysis.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024542786000001_ABST
    Figure 2024542786000001_ABST
Patent Text Reader

Abstract

Methods and devices are provided for detecting chiral properties from a sample. Light can be directed toward the sample in contact with the chiral nanoparticles. Third harmonic Mie scattering (THMS) optical activity generated by the chiral nanoparticles in contact with the sample can then be detected. It is contemplated that the device for detecting chiral properties of a sample further includes at least one microwell having a volume of about 1 microliter or less configured to hold chiral nanoparticles capable of generating third harmonic Mie scattering (THMS) optical activity and the sample to be analyzed. The device includes a light source configured to generate light and direct the light toward at least one microwell containing the chiral nanoparticles and the sample, and at least one detector configured to detect third harmonic Mie scattering (THMS) generated by the chiral nanoparticles in the microwell.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application claims the benefit of U.S. Provisional Application No. 63 / 284,813, filed December 1, 2021, the entire disclosure of which is incorporated herein by reference.

[0002] Government Subsidy This invention was made with Government support under HQ00342010033 and N00014-18-1-2876 awarded by the Office of Naval Research. The Government has certain rights in the invention.

[0003] The present disclosure relates to an apparatus and method for determining chiral optical properties from third harmonic Mie scattering of chiral semiconductor nanoparticles. [Background technology]

[0004] This section provides background information related to the present disclosure that is not necessarily prior art.

[0005] Chiral optical spectroscopy provides new optical dimensions and informative data sets for the structural analysis of nanostructured particles. Determination of chiral optical properties in small volumes is an essential task in the synthesis of materials for drug discovery, biomedical sequencing, biotechnology, and photonics. Although they can be utilized in the robotic optimization of nanophotonic materials, these spectroscopy methods typically require sample volumes that are incompatible with generating large chemical libraries. Combinatorial nanochemistry allows the creation of tens to millions of mixtures in a single step, thereby generating large chemical libraries and enabling the implementation of artificial intelligence algorithms.

[0006] With the advent of rapid development of chiral nanostructures, such synthesis and analysis platforms can be applied for their high-throughput characterization as enzyme mimetics, modeling agents, antibiotics, drug delivery vehicles, and other uses of these bioinspired materials. These analyses are often performed in 1,536-, 3,456-, or 9,600-well microplates with sample volumes as small as 1 microliter (μL) or less, whereas traditional methods of kill optical spectroscopy typically require sample volumes 100 to 1,000 times larger. Thus, new optical tools must be developed for rapid characterization of ultrasmall volumes of chiral nanocompounds. Nonlinear kill optical spectroscopy can potentially be used to characterize chiral nanocompounds in volumes as small as tens of cubic micrometers (μm). 3 ) and are therefore well suited for microplates containing even the highest number of wells. Nonlinear kill optical effects applicable in isotropic liquids have been reported, but they are technically too complex for the needs of combinatorial nanochemistry and high-throughput synthesis.

[0007] Thus, the realization of such methods in a format suitable for rapid acquisition of large amounts of data is currently difficult with current implementations of kill optical spectroscopy, due to the need for relatively large sample volumes and low light flux. Although similar issues arise for robotic optimization of nanophotonic materials, these spectroscopy methods typically require sample volumes that are incompatible with generating large chemical libraries. New optical tools are needed to characterize chirality in ultra-small volumes, such as the 1-microliter droplets required for high-throughput synthesis and analysis stations for chiral compounds. [Prior art documents] [Non-patent literature]

[0008] [Non-Patent Document 1] J. Yan et al., “Self-Assembly of Chiral Nanoparticles into Semiconductor Helices with Tunable near-Infrared Optical Activity”, Chem.Mater.32(1), pp. 476-488 (2020) [Non-Patent Document 2] Publication (N. Gaponik et al., "Thiol-Capping of CdTe Nanocrystals: An Alternative to Organometallic Synthetic Routes", J.Phys.Chem.B, 106(29), 7177~7185(2002)) [Non-Patent Document 3] W. Feng et al., “Assembly of mesoscale helices with near-unity enantiomeric excess and light-matter interactions for chiral semiconductors”, Sci.Adv.3(3), e1601159(2017) [Non-Patent Document 4] Treharne et al., Phys.Conf.Ser., 286, 012038(2011) Summary of the Invention [Means for solving the problem]

[0009] This section provides a general overview of the disclosure, but is not an exhaustive disclosure of its entire scope or all of its features.

[0010] In certain aspects, the present disclosure relates to methods and apparatus for detecting chiral properties, and more particularly, third harmonic Mie scattering (THMS) optical activity from a sample in contact with one or more chiral nanoparticles.

[0011] In one variation, a method of detecting chiral properties from a sample is provided. The method may include directing light toward a sample in contact with chiral nanoparticles. The method may further include detecting third harmonic Mie scattering (THMS) optical activity generated by the chiral nanoparticles in contact with the sample.

[0012] In one embodiment, the third harmonic Mie scattering (THMS) optical activity is forward oriented third harmonic (TH) radiation that is circularly polarized.

[0013] In one embodiment, the sample has a volume of about 1 microliter or less.

[0014] In one embodiment, the sample is about 10 -5 It has a volume of at least a microliter and not more than about 1 microliter.

[0015] In one embodiment, the chiral nanoparticles comprise a semiconductor material.

[0016] In one embodiment, the chiral nanoparticles comprise cadmium telluride (CdTe).

[0017] In one embodiment, the chiral nanoparticles include a plurality of chiral nanoparticles self-assembled together to define at least one self-assembled nanostructured helix, such as a plurality of self-assembled nanostructured helices.

[0018] In one embodiment, the chiral nanoparticles include a plurality of chiral nanoparticles integrated together, each chiral nanoparticle being in the form of a nanohelix having a length of about 5 micrometers or more and about 8 micrometers or less and a thickness of about 10 nm or more and about 50 nm or less.

[0019] In one embodiment, the light is circularly polarized light.

[0020] In another variation, an apparatus for detecting chiral properties of a sample is provided. The apparatus may include at least one microwell having a volume of 1 microliter or less configured to hold chiral nanoparticles capable of generating third harmonic Mie scattering (THMS) optical activity. The at least one microwell is configured to contain a sample to be analyzed. The apparatus further includes a light source configured to generate light and direct the light toward the at least one microwell containing the chiral nanoparticles and the sample. Additionally, the apparatus includes at least one detector configured to detect third harmonic Mie scattering (THMS) generated by the chiral nanoparticles in the microwell.

[0021] In one embodiment, chiral nanoparticles are provided within a sample within a microwell.

[0022] In one embodiment, chiral nanoparticles are associated with the surface of a microwell.

[0023] In one embodiment, the microwell comprises about 10 -5 It has a volume of at least a microliter and not more than about 1 microliter.

[0024] In one embodiment, the chiral nanoparticles comprise a semiconductor material.

[0025] In one embodiment, the chiral nanoparticles comprise cadmium telluride (CdTe).

[0026] In one embodiment, the chiral nanoparticles include a plurality of chiral nanoparticles self-assembled together to define at least one self-assembled nanostructured helix, such as a plurality of self-assembled nanostructured helices.

[0027] In one embodiment, the chiral nanoparticles include a plurality of chiral nanoparticles assembled together, each chiral nanoparticle being in the form of a nanohelix having a length of about 5 micrometers to about 8 micrometers and a thickness of about 10 nm or more and about 50 nm or less.

[0028] In one aspect, the light source is configured to generate and guide circularly polarized light.

[0029] In one aspect, the apparatus further includes at least one processor.

[0030] In one embodiment, the at least one microwell comprises an array of microwells.

[0031] Further areas of applicability will become apparent from the description provided herein. The description and specific examples in this summary are intended for purposes of illustration only and are not intended to limit the scope of the present disclosure.

[0032] The drawings described herein are only for purposes of illustrating selected embodiments and not all possible implementations, and are not intended to limit the scope of the present disclosure. [Brief description of the drawings]

[0033] [Figure 1A] 1 shows a CdTe nanohelix for third harmonic Mie scattering optical activity prepared according to certain embodiments of the present disclosure, and a schematic diagram of THMS optical activity. Following illumination with left circularly polarized (LCP) light of wavelength λ, the intensity of the THMS light (at λ / 3) depends on the symmetry of the CdTe nanohelix. [Figure 1B] FIG. 1 shows scanning electron micrographs (SEM) of left-handed and right-handed CdTe nanohelices, designated as Λ-CdTe and Δ-CdTe, respectively, illustrating CdTe nanohelices for third harmonic Mie scattering optical activity prepared according to certain embodiments of the present disclosure. [Figure 1C]1 shows a CdTe nanohelix for third harmonic Mie scattering optical activity prepared according to certain embodiments of the present disclosure, and the experimental ellipticity spectrum and numerically computed differential extinction cross section spectrum from the nanohelix in the linear optical regime, where the wavelengths of illumination and detection of the THMS experiment are indicated by the vertical lines. [Figure 1D] FIG. 1 shows a CdTe nanohelix for third harmonic Mie scattering optical activity prepared according to certain embodiments of the present disclosure, illustrating the emission patterns from a Λ-CdTe nanohelix illuminated along its major axis for LCP and right circularly polarized light (RCP). [Figure 1E] 1 shows a CdTe nanohelix for third harmonic Mie scattering optical activity prepared according to certain embodiments of the present disclosure, and is a diagram of the TH scattering setup: WP: quarter wave plate, F1: optical filter that accepts λ, L1: focusing lens, L2: collimating lens, F2: bandpass filter that only allows λ / 3 to pass. [Figure 2A] FIG. 1 shows electromagnetic simulations for a CdTe nanohelix, illustrating the geometry of a three-dimensional (3D) nanohelix enantiomer model for electromagnetic calculations. [Figure 2B] Electromagnetic simulations for CdTe nanohelices. Λ-CdTe electric field profile maps under full-wave (range 300 nm–1500 nm) RCP (left) and LCP (right) illumination calculated by the finite difference time domain (FDTD) method. [Figure 2C] 1 shows electromagnetic simulations for a CdTe nanohelix, illustrating the radiation pattern of Λ-CdTe oriented perpendicular to the direction of electromagnetic wave incidence. The 3D radiation pattern was obtained from electromagnetic waves with a wavelength of 1095 nm. [Figure 2D]1 shows electromagnetic simulations for a CdTe nanohelix, illustrating the two-dimensional (2D) (x-normal) radiation pattern of Λ-CdTe oriented parallel to the electromagnetic wave incidence direction. The data was acquired by setting the reference direction, which is the electromagnetic wave incidence direction, as -z. [Figure 2E] 1 shows electromagnetic simulations for a CdTe nanohelix, illustrating the two-dimensional (2D) (x-normal) radiation pattern of Λ-CdTe oriented perpendicular to the electromagnetic wave incidence direction. The data was acquired by setting the reference direction, which is the electromagnetic wave incidence direction, as -z. [Figure 3A] Demonstration of third harmonic Mie scattering (THMS) optical activity. The third harmonic (TH) intensity in the forward direction (through the sample and in the forward direction relative to the light source generating the incident laser light) is shown from Λ-CdTe as a function of incident laser power at wavelength λ=1095 nm for LCP and RCP light. Symbols are experimental data points (each is the median value from 50 measurements) and lines are fits to a third order power law. A schematic of the experiment is shown as an inset. [Figure 3B] Demonstration of third harmonic Mie scattering (THMS) optical activity. The third harmonic (TH) intensity in the forward direction (through the sample and in the forward direction relative to the light source generating the incident laser light) is shown from Δ-CdTe as a function of incident laser power at wavelength λ=1095 nm for LCP and RCP light. Symbols are experimental data points (each is the median value from 50 measurements) and lines are fits to a third order power law. [Figure 3C] Demonstration of third harmonic Mie scattering (THMS) optical activity is shown, showing multiphoton forward emission from a Λ-CdTe nanohelix upon illumination at 1095 nm. The TH signal (at 365 nm) clearly dominates the nearby emission wavelengths of linearly polarized LCP and RCP light. [Figure 3D]Demonstration of third harmonic Mie scattering (THMS) optical activity is shown in Figure 3A and 3B, which shows the THMS ellipticity at three different wavelengths calculated from the power dependence curves from Λ- and Δ-CdTe as in Figure 3B. The kill optical response is well resolved, as demonstrated by the error bars indicating the standard deviation. [Figure 4A] Demonstration of third harmonic Mie scattering (THMS) optical activity: orthogonal third harmonic (TH) intensity from a left-handed CdTe nanohelix (Λ-CdTe) (orthogonal or perpendicular to the direction of the laser light from the source after leaving the sample) is shown as a function of incident laser power at wavelength λ=1095 nm for LCP and RCP light. [Figure 4B] Demonstration of third harmonic Mie scattering (THMS) optical activity. Showing the THMS ellipticity at three different wavelengths calculated from the power dependence curves for Λ- and Δ-CdTe. The kill optical response is well resolved as demonstrated by the error bars (representing standard deviation). This kill optical response is on the opposite side to that in Figure 3D. [Figure 4C] Demonstration of third harmonic Mie scattering (THMS) optical activity, showing the TH intensity in the forward direction (through the sample and in the forward direction relative to the light source generating the laser light) as a function of analyzing quarter-wave plate (AWP) rotation angle for Λ-CdTe. LCP and RCP incident light produces LCP and RCP TH light, respectively. [Figure 4D] Demonstration of third harmonic Mie scattering (THMS) optical activity, showing TH intensity in the 90° direction as a function of AWP rotation angle for Λ-CdTe and Δ-CdTe. LCP and RCP incident light produces linearly polarized TH light. All measurements were performed with incident 1095 nm light. A schematic of the experiment is shown in the inset. [Figure 5A]FIG. 1 illustrates the application of THMS to characterize chiral nanostructures in ultra-small volumes, showing proof-of-principle data demonstrating that a method according to certain embodiments of the present disclosure can clearly distinguish between Λ-CdTe and Δ-CdTe in a 1 mm thick optical cuvette (as opposed to a standard 1 cm cell). THMS ellipticity was calculated from power dependence curves measured at three different wavelengths. [Figure 5B] An example of the application of THMS to characterize chiral nanostructures in ultrasmall volumes is shown in Figure 1. In the same 1 mm cuvette, the TH intensity follows a clear third-order dependence as a function of laser power at a wavelength of 1095 nm. Despite the small dimensions of the cuvette, the kill optical effects for LCP and RCP, respectively, are clearly opposite in sign due to the symmetry of the samples, indicating the potential for very small volume applications. [Figure 5C] FIG. 1 shows an example of the application of THMS to characterize chiral nanostructures in ultra-small volumes, and is a schematic diagram illustrating an example of the application of techniques according to certain embodiments of the present disclosure as an analytical tool for parallel combinatorial chemical synthesis. [Figure 5D] An example application of THMS to characterize chiral nanostructures in ultrasmall volumes is shown, enabling high-throughput applications by scanning a laser beam within an optical objective to probe reaction conditions that generate nanomolar amounts of a desired compound in minute volumes (e.g., <1 μL) arrayed across a microplate. The red arrow indicates the direction of the incident light. [Figure 5E] Figure 1 shows the application of THMS for characterizing chiral nanostructures in ultra-small volumes and shows a schematic diagram for in-line reaction monitoring in a microreactor. [Figure 6A] Figure 1 shows third harmonic (TH) Mie forward scattering optical activity at two wavelengths, 1065 nm and 1125 nm. The TH intensity was measured at 1065 nm as a function of incident power on a Λ-CdTe nanohelix in a forward scattering setup (schematic diagram of the experimental setup is included in the inset). [Figure 6B] FIG. 1 shows third harmonic (TH) Mie forward scattering optical activity at two wavelengths, 1065 nm and 1125 nm, where the TH intensity was measured at 1065 nm as a function of incident power on a Δ-CdTe nanohelix in a forward scattering setup. [Figure 6C] FIG. 1 shows the optical activity of third harmonic (TH) Mie forward scattering at two wavelengths, 1065 nm and 1125 nm. [Figure 6D] FIG. 1 shows the optical activity of third harmonic (TH) Mie forward scattering at two wavelengths, −1065 nm and 1125 nm. [Figure 7A] FIG. 13 shows emission with 1065 nm light and simultaneous clear emission at the third harmonic wavelength, as shown in the inset, of forward multiphoton emission by the Λ-CdTe nanohelix. [Figure 7B] FIG. 13 shows emission with 1065 nm light and simultaneous clear emission at the third harmonic wavelength, as shown in the inset, in a right angle scattering setup. [Figure 8A] Scanning electron microscopy (SEM) images of CdTe nanoribbons at varying magnifications showing that in the case of comparative achiral CdTe nanoribbons no third harmonic (TH) Mie optical activity is observed. In the nonlinear experiments, the incident light is left circularly polarized (LCP) or right circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 8B] Scanning electron microscopy (SEM) images of CdTe nanoribbons at varying magnifications showing that in the case of comparative achiral CdTe nanoribbons no third harmonic (TH) Mie optical activity is observed. In the nonlinear experiments, the incident light is left circularly polarized (LCP) or right circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 8C]Scanning electron microscopy (SEM) images of CdTe nanoribbons at varying magnifications showing that in the case of comparative achiral CdTe nanoribbons no third harmonic (TH) Mie optical activity is observed. In the nonlinear experiments, the incident light is left circularly polarized (LCP) or right circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 8D] Figure 2 shows two measurements of third harmonic (TH) intensity as a function of incident power in a forward scattering setup, showing that no third harmonic (TH) Mie optical activity is observed in the comparative case of achiral CdTe nanoribbons. In the nonlinear experiment, the incident light is left-handed circularly polarized (LCP) or right-handed circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 8E] Figure 2 shows two measurements of third harmonic (TH) intensity as a function of incident power in a forward scattering setup, showing that no third harmonic (TH) Mie optical activity is observed in the comparative case of achiral CdTe nanoribbons. In the nonlinear experiment, the incident light is left-handed circularly polarized (LCP) or right-handed circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 8F] In the comparative case of achiral CdTe nanoribbons, third harmonic (TH) Mie optical activity is not observed, and the TH ellipticity is calculated from the results in Figures 8D and 8E. Inset: Schematic of the experimental setup. In the nonlinear experiments, the incident light is left-handed circularly polarized (LCP) or right-handed circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 8G]Figure 2 shows two measurements of the third harmonic (TH) intensity as a function of incident power in a 90° scattering setup, showing that no third harmonic (TH) Mie optical activity is observed in the comparative case of achiral CdTe nanoribbons. In the nonlinear experiment, the incident light is left-handed circularly polarized (LCP) or right-handed circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 8H] Figure 2 shows two measurements of the third harmonic (TH) intensity as a function of incident power in a 90° scattering setup, showing that no third harmonic (TH) Mie optical activity is observed in the comparative case of achiral CdTe nanoribbons. In the nonlinear experiment, the incident light is left-handed circularly polarized (LCP) or right-handed circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 8I] In the comparative case of achiral CdTe nanoribbons, third harmonic (TH) Mie optical activity is not observed, showing the TH ellipticity calculated from the results in Figures 8G and 8H. Inset: Schematic of the experimental setup. In the nonlinear experiments, the incident light is left-handed circularly polarized (LCP) or right-handed circularly polarized (RCP). The sample is illuminated with 1095 nm light. Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 9A] FIG. 1 shows third harmonic super-Mie scattering optical activity at right angle scattering. TH intensity is shown in the right angle direction from a right-handed CdTe nanohelix (Δ-CdTe) as a function of incident laser power at wavelength (λ)=1095 nm for LCP and RCP light. [Figure 9B] FIG. 1 shows third harmonic super-Mie scattering optical activity in orthogonal scattering. Multiphoton orthogonal emission from a Λ-CdTe nanohelix is ​​shown simultaneously with 1095 nm illumination. [Figure 10A]Figure 1 shows optical activity in third harmonic (TH) Mie right-angle scattering at two wavelengths, showing a Λ-CdTe nanohelix in a right-angle scattering setup (schematic diagram of the experimental setup in the inset) and the measured TH intensity at 1065 nm as a function of incident power. [Figure 10B] FIG. 1 shows optical activity in third harmonic (TH) Mie right-angle scattering at two wavelengths. Δ-CdTe nanohelices in the right-angle scattering setup. TH intensity at 1065 nm measured as a function of incident power. [Figure 10C] FIG. 1 shows optical activity in third harmonic (TH) Mie right-angle scattering at two wavelengths; similar measurements at 1125 nm are presented for Λ-CdTe. [Figure 10D] FIG. 1 shows optical activity in third harmonic (TH) Mie right-angle scattering at two wavelengths; similar measurements at 1125 nm are presented for Δ-CdTe. [Figure 11A] Figure 1 shows THMS polarization, where the forward TH intensity is shown as a function of the rotation angle of the quarter-wave plate (AWP) relative to the Δ-CdTe. LCP and RCP incident light produces LCP and RCP TH light, respectively. [Figure 11B] FIG. 13 shows THMS polarization, where TH intensity in the 90° direction is shown as a function of AWP rotation angle for Δ-CdTe. [Figure 12] 1 shows a multipolar spectral decomposition of the nanohelix scattering cross section. The curves correspond to the electric dipole (ED), magnetic dipole (MD), electric quadrupole (EQ), and magnetic quadrupole (QD), as well as the total scattering cross section upon illumination with right- and left-circularly polarized light (LCP and RCP, respectively). The circular difference (CD) corresponds to the difference (Δ) in the scattering cross section. [Figure 13A]The third harmonic (TH) scattering was determined in a liquid medium containing 0.2% sodium dodecyl sulfate (SDS) and shows the TH intensity as a function of incident laser power for 0.2% SDS illuminated with left circularly polarized (LCP) and right circularly polarized (RCP) light. The inset shows a schematic of the setup for measuring the TH forward emission. In the plot, the sample was illuminated with 1095 nm light. The line is fitted to y=Ax+B. [Figure 13B] The third harmonic (TH) scattering was determined in a liquid medium containing 0.2% sodium dodecyl sulfate (SDS) and shows the TH intensity as a function of incident laser power for 0.2% SDS illuminated by LCP and RCP light. The inset shows a schematic of the setup for measuring TH emission at right angles. In the plot, the sample was illuminated by 1095 nm light. The line is fitted to y=Ax+B. [Figure 14A] Figure 1. Determining whether third harmonic (TH) light arises from the 10 mm cuvette interface. TH intensity as a function of focus lens position for illumination with linear and left-handed circularly polarized (LCP) 1095 nm light (incident power = 15 mW). The position of the cuvette containing Λ-CdTe was fixed. Measurements were performed in forward scattering geometry. [Figure 14B] Figure 1. Determining whether third harmonic (TH) light arises from the 10 mm cuvette interface. TH intensity as a function of incident power measured for an empty cuvette in forward scattering geometry. The focusing lens was placed at 89.5 mm. A line is fitted to y=Ax+B. [Figure 15A] FIG. 1 shows that no third harmonic (TH) optical rotation is observed. A schematic diagram of the setup is depicted. [Figure 15B] 1 shows that no third harmonic (TH) optical rotation is observed. TH intensity is shown as a function of analyzer angle (distinguishing between Λ-CdTe and Δ-CdTe) for both chiral forms of nanoparticles prepared according to the present disclosure. [Figure 16]It shows the absence of third harmonic (TH) light from the 1 mm cuvette interface, and more specifically, the TH intensity as a function of focus lens position for illumination with linear and left circularly polarized (LCP) 1095 nm light (incident power = 15 mW). Measurements were performed in forward scattering geometry. [Figure 17A] Third harmonic (TH) Mie forward scattering optical activity at two wavelengths when the sample was measured in a cuvette containing a 1 mm path length. TH intensity was measured at 1065 nm as a function of incident power on the Λ-CdTe nanohelix in the forward scattering setting. In this measurement, the incident light is left circularly polarized (LCP) or right circularly polarized (RCP). Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 17B] Third harmonic (TH) Mie forward scattering optical activity at two wavelengths when the sample was measured in a cuvette containing a 1 mm path length. TH intensity was measured at 1065 nm as a function of incident power on a Δ-CdTe nanohelix in forward scattering configuration. In this measurement, the incident light was left circularly polarized (LCP) or right circularly polarized (RCP). Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 17C] Third harmonic (TH) Mie forward scattering optical activity at two wavelengths when the sample was measured in a cuvette containing a 1 mm path length. A similar measurement at 1125 nm is presented for Λ-CdTe. In this measurement, the incident light is left circularly polarized (LCP) or right circularly polarized (RCP). Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. [Figure 17D]Third harmonic (TH) Mie forward scattering optical activity at two wavelengths when the sample was measured in a cuvette containing a 1 mm path length. A similar measurement at 1125 nm is presented for Δ-CdTe. In this measurement, the incident light is left circularly polarized (LCP) or right circularly polarized (RCP). Each data point is the median of 50 measurements. The data set is fitted with a function of the form y=Ax3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0034] Corresponding reference numerals indicate corresponding parts throughout the several views of the drawings.

[0035] The example embodiments are provided so that the disclosure will be thorough and fully convey the scope to those skilled in the art. Many specific details, such as examples of specific compositions, components, devices, and methods, are set forth in order to provide a thorough understanding of the embodiments of the present disclosure. It will be apparent to those skilled in the art that it is not necessary to employ specific details, that the example embodiments can be embodied in many different forms, and that none of these should be construed as limiting the scope of the present disclosure. In some example embodiments, well-known processes, well-known device structures, and well-known techniques are not described in detail.

[0036] The terminology used herein is for the purpose of describing particular example embodiments only and is not intended to be limiting. As used herein, the singular forms "a", "an" and "the" may be intended to include the plural forms as well, unless the context clearly indicates otherwise. The terms "comprise", "comprises", "includes" and "having" are inclusive and thus specify the presence of stated features, elements, compositions, steps, integers, operations and / or components, but do not preclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or groups thereof. The open-ended term "comprises" should be understood as a non-limiting term used to describe and claim various embodiments in certain aspects described herein, although the term may alternatively be understood as a more restrictive and limiting term such as "consisting of" or "consisting essentially of". Thus, for any given embodiment that recites compositions, materials, components, elements, features, integers, operations, and / or process steps, the disclosure also expressly includes embodiments that consist of or consist essentially of such recited compositions, materials, components, elements, features, integers, operations, and / or process steps. In the "consisting of" case, alternative embodiments exclude any additional compositions, materials, components, elements, features, integers, operations, and / or process steps, while in the "consisting essentially of" case, any additional compositions, materials, components, elements, features, integers, operations, and / or process steps that affect the materially basic and novel characteristics are excluded from such embodiment, but any compositions, materials, components, elements, features, integers, operations, and / or process steps that do not affect the materially basic and novel characteristics may be included in the embodiment.

[0037] Any method steps, processes, and operations described herein should not be construed as necessarily requiring performance in the particular order discussed or illustrated, unless specifically identified as such. It should be further understood that additional or alternative steps may be utilized, unless otherwise indicated.

[0038] When a component, element, or layer is referred to as being "on", "engaged with", "connected to", or "coupled to" another element or layer, it may be directly on, engaged with, connected to, or coupled to the other component, element, or layer, or there may be intervening elements or layers. In contrast, when an element is referred to as being "directly on", "directly engaged with", "directly connected to", or "directly coupled to" another element or layer, there may not be an intervening element or layer. Other words used to describe relationships between elements should be interpreted in a similar manner (e.g., "between" vs. "directly between", "adjacent" vs. "directly adjacent", etc.). As used herein, the term "and / or" includes any and all combinations of one or more of the associated listed items.

[0039] Although terms such as first, second, third, etc. may be used herein to describe various steps, elements, components, regions, layers, and / or sections, these steps, elements, components, regions, layers, and / or sections should not be limited by these terms unless otherwise indicated. These terms may be used only to distinguish one step, element, component, region, layer, or section from another step, element, component, region, layer, or section. Terms such as "first", "second", and other numerical terms, when used herein, do not imply any sequence or order unless clearly indicated by the context. Thus, a first step, element, component, region, layer, or section discussed below could be referred to as a second step, element, component, region, layer, or section without departing from the teachings of the example embodiments.

[0040] Spatial or temporal relative terms such as "before," "after," "inside," "outside," "below," "below," "below," "above," "above" and the like may be used herein for ease of description to describe the relationship of one element or feature to another element(s) or feature(s) as illustrated in the drawings. Spatial or temporal relative terms may be intended to encompass different orientations of a device or system during use or operation in addition to the orientation depicted in the drawings.

[0041] Throughout this disclosure, numerical values ​​represent approximate magnitudes or range limits to encompass minor deviations from a given value and embodiments with approximate values ​​as well as embodiments with exact values ​​as stated. Except in the working examples provided at the end of the detailed description, all numerical values ​​of parameters (e.g., amounts or conditions) in this specification, including the appended claims, should be understood to be modified in all instances by the term "about", regardless of whether "about" actually appears before the numerical value. "About" indicates that the stated numerical value allows for some slight ambiguity (somewhat close to the precision of the value; approximately or fairly close to the value; approximately). If the ambiguity realized by "about" is not otherwise understood in the art in this ordinary sense, "about" as used herein indicates at least the variation that may result from ordinary methods of measuring and using such parameters. For example, "about" can include a variation of less than or equal to 5%, optionally less than or equal to 4%, optionally less than or equal to 3%, optionally less than or equal to 2%, optionally less than or equal to 1%, optionally less than or equal to 0.5%, and in certain embodiments, optionally less than or equal to 0.1%.

[0042] Moreover, disclosure of a range includes disclosure of all values ​​within that entire range, including the endpoints and subranges given in the range, and any further divided ranges.

[0043] Example embodiments will now be described more fully with reference to the accompanying drawings, in which:

[0044] In various embodiments, the present disclosure contemplates the use of novel kill optical effects in certain chiral nanoparticle structures that can be used for characterization of particularly small volume samples, e.g., samples having a volume of approximately 1 microliter (μL) or less. In certain embodiments, the sample volume is 10 -5The volume of the light can be as small as 1 μL. Thus, nonlinear kill optical characterization of small volumes of inorganic nanostructures is contemplated by using circularly polarized Mie scattering spectroscopy. Light is a TEM wave, whereas natural light is generally unpolarized and all planes of propagation are of equal probability. In general, circularly polarized light (CPL) typically has two perpendicular electromagnetic waves of equal amplitude and phase difference of 90°, and can have either a left-handed orientation (the electric vector of the light originating from the source appears to rotate clockwise) or a right-handed orientation (the electric vector of the light originating from the source appears to rotate counterclockwise). Elliptical polarized light is light with two perpendicular waves of unequal amplitude with a phase difference of 90°, and can be used similarly to circularly polarized light.

[0045] Nanoparticle chirality means that the nanoparticle or nanostructure exhibits asymmetric optical activity with different symmetries, clockwise to form left-handed chirality (S, L, or Λ orientation) and counterclockwise to form right-handed chirality (R, D, or Δ orientation). The nanoparticles can be provided, for example, in a mixture with enantiomeric nanoparticle species of either left (Λ) or right (Δ) symmetry of about 99% or more enantiomeric purity, or, optionally, with a relatively pure enantiomeric mixture with an enantiomeric purity of 99.5% or more. The nanoparticle component(s) is preferably a dispersion of chiral nanoparticle(s) in a liquid medium, such as an aqueous medium. Such nanoparticle dispersions are preferably stable at ambient conditions.

[0046] A "nanoparticle" is a solid or semi-solid material that may have a variety of shapes or morphologies and may include nanostructures or aggregates of nanoparticles. However, nanoparticles are generally understood by those skilled in the art to mean that the particle / structure has at least one spatial dimension that is about 10 micrometers (μm) (10,000 nm) or less. In certain aspects, the nanoparticles have at least one spatial dimension, such as a thickness or diameter, that is about 2 nm to about 5 μm, optionally about 2 nm to about 3 μm, optionally about 2 nm to about 1 μm, optionally about 2 nm to about 500 nm, optionally about 2 nm to about 100 nm, optionally about 2 nm to about 50 nm, optionally about 5 nm to about 30 nm, and optionally about 25 nm with certain variations. It should be noted that other dimensions may be larger than these ranges. In certain embodiments, the nanoparticles used according to the present disclosure are nanohelices, nanoribbons, nanorods, or nanoaggregates of any of these nanoparticles. In certain embodiments, the chiral nanoparticles are nanoassemblies of nanohelices or nanoribbons, such as assemblies of nanostructured helices.

[0047] Thus, the chiral nanoparticles may include or be formed from light absorbing materials. The chiral nanoparticles may include semiconductor materials, including direct and indirect band gap semiconductors. In certain embodiments, the chiral nanoparticles formed according to certain embodiments of the present disclosure are selected from the group consisting of CdTe, CdSe, CdS, gold, silver, copper, nickel, iron, carbon, platinum, silicon, HgTe, HgSe, HgS, PbTe, PbSe, PbS, MoS2, FeS2, FeS, FeSe, and combinations thereof. In further embodiments, the chiral nanoparticles include semiconductor materials such as cadmium telluride (CdTe).

[0048] In various embodiments, methods are provided according to the present disclosure for experimentally examining chiral optical properties in ultra-small volumes using third harmonic Mie scattering (THMS) from chiral nanoscale particles. THMS optical activity arises when three circularly polarized photons at the fundamental frequency create a single photon at triple frequency. More specifically, in certain embodiments, the methods can use third harmonic Mie scattering (THMS) optical activity observed in suspensions of CdTe nanostructured helices in volumes several orders of magnitude smaller than 1 μL. As described herein, when CdTe helices are illuminated with laser beams having wavelengths of 1065 nm, 1095 nm, and 1125 nm, kill optical third harmonic emissions have been recorded, with THMS intensity approximately 10 times higher in the forward direction (traveling away from the laser source) than in the sideways direction. The third harmonic ellipticity was as high as approximately 3°. This is believed to be due to the effect of interference between chiral and achiral effective nonlinear susceptibility tensor components. THMS for semiconductor helices according to certain embodiments of the present disclosure can be, for example, from volumes of about 1 microliter or less to 10 -5 It provides rapid high-throughput kill optical characterization of sample volumes ranging from as small as 1 µL.

[0049] Furthermore, as in the background art, new optical tools need to be developed for rapid characterization of chiral nanocompounds in ultra-small volumes. Nonlinear chiral optical spectroscopy could potentially characterize nanocompounds in volumes of tens of cubic micrometers (µm 3 ) and are well suited for microplates containing the highest number of wells. Nonlinear kill optical effects applicable in isotropic liquids have been reported, but they are technically too complex to require combinatorial nanochemistry and high-throughput synthesis. For example, in the case of super-Rayleigh scattering optical activity, the geometry of well plates is not favorable for nonlinear Rayleigh scattering registration, and therefore typically 4π integrating spheres centered on each individual sample would be required to reduce artifacts and crosstalk between adjacent samples.

[0050] Nonlinear kill optical characterization of small volumes of inorganic nanostructures may be possible by circularly polarized Mie scattering spectroscopy. This scattering modality has advantages over Rayleigh scattering because Mie scattering occurs within a small continuous angle. The smaller scattering continuous angle simplifies the registration and polarimetry of scattered photons and is compatible with the requirements of microplate geometry. Mie scattering from chiral metallic particles and their assemblies can exceptionally result in strong dependence on light polarization, torque transfer, and spin-polarized electron emission. Despite the wide interest that chiral nonmetallic particles attract in relation to ultrafast and miniaturized devices, their Mie scattering properties are poorly known. Interactions of light materials with nonmetallic particles can include electric and magnetic dipole and multipole, as well as anapole resonances. Compared to their plasmonic counterparts, the electric and magnetic contributions in these nonmetallic nanoparticles can become comparable, thereby resulting in enhanced kill optical properties. The nonlinear kill optical properties of such individual particles are currently unknown.

[0051] In the context of the present disclosure, the nonlinear scattering process of CdTe semiconductor helices is explored, and a new kill optical effect is discovered and demonstrated that can be used to characterize samples of interest, particularly very small sample sizes (e.g., volumes of about 1 microliter (μL) or less). In certain embodiments, the nanoparticles are CdTe nanoparticles that form self-assembled nanostructured helices. The nanostructured helices may be about 5 to about 8 micrometers (μm) in length, thereby resulting in Mie scattering. For brevity, these nanoparticles will be referred to as nanohelices because they not only exhibit some nanoscale dimensions (e.g., have a thickness of approximately 25 nm), but also largely retain the nanoscale dimensions of the individual self-assembled, interwoven nanowires. Semiconductor nanohelices can be obtained with 99.5% enantiomeric purity in both left-handed (Λ) and right-handed (Δ) symmetries. The semiconductor nanohelices are randomly dispersed in an isotropic liquid environment in all samples described herein. Their dispersion reveals strong kill-optical third-harmonic Mie scattering (THMS) observed at three different wavelengths in the near-infrared range of the electromagnetic spectrum.

[0052] THMS of nanohelices is characterized by third harmonic (TH) emission that is roughly 10 times stronger in the forward direction than at a 90° angle to the incident light. The nonlinear ellipticity can be as high as 3°, thereby changing sign for Λ and Δ-CdTe nanohelices. The kill optical contrast is inverted between forward and 90° angle emission, thereby revealing a phase relationship between the chiral and achiral effective tensor components of the TH susceptibility. Furthermore, the kill optical effect can be observed in both forward-emitting circularly polarized TH light and transverse-emitting linearly polarized TH light. Finally, successful kill optical characterization of CdTe nanohelices is demonstrated in small (<1 μL) volumes using THMS.

[0053] As discussed above, with reference to Figures 1A-1E, THMS optical activity occurs when three circularly polarized photons at the fundamental frequency create a single photon at triple frequency, as shown in Figure 1A, with the conversion efficiency depending on the chirality of the CdTe helix and the symmetry of the incident circularly polarized light. This effect is a manifestation of optical activity in the general sense of the term, e.g., in this case it refers to any change in the intensity or polarization of light due to the chirality of the material. Prior to the present invention, it is believed that THMS optical activity has not previously been observed for any semiconductor, metal, dielectric, or biological sample.

[0054] As described in the examples below, CdTe nanohelices can be synthesized using the method of J. Yan et al., "Self-Assembly of Chiral Nanoparticles into Semiconductor Helices with Tunable near-Infrared Optical Activity," Chem. Mater. 32(1), pp. 476-488 (2020), the relevant portions of which are incorporated herein by reference, to create helicoids with a geometry approaching that of twisted ribbons. By analyzing SEM microscopy images and geometric parameters of the nanohelices (140±20 nm thick, 453±70 nm wide, and 302±45 nm pitch in one batch), their uniformity appears to arise from a self-limited assembly of nanoparticles controlled by electrostatic repulsion. Further reference to FIG. 2A shows the width, thickness, and pitch of the nanohelix (thickness is 25 nm, and pitch is approximately 550 nm, from the first apex of the first twist to the second apex of the adjacent twist). The circular dichroism (CD) spectra of the Λ- and Δ-nanohelices have two similar, but opposite polarities, singular shapes. The differential extinction cross section spectra of the 3D helix models (FIG. 2B-2E), calculated by the finite difference time domain (FDTD) method, match well with the experimental CD spectrum (FIG. 1C). The difference in amplitude of the experimental CD peaks is due to the difference in the concentration of the prepared suspensions. FIG. 1D shows the scattering patterns of the Λ-CdTe nanohelix at the same wavelength as that of the incident beam illuminated along the principal axis for LCP and RCP light (further details on these simulations can be found in FIG. 2A-2E). Clearly, the patterns are characteristic of Mie scattering.

[0055] CdTe nanohelices exhibit multiple scales of organization, including microscale lengths comparable to the wavelengths of visible and near-infrared light and submicron scale pitch lengths, making them useful candidates not only for observing linear Kirk optical activity during scattering, but also for observing super-Mie scattering rather than super-Rayleigh scattering. The TH experimental setup to evaluate super-Mie scattering activity is shown in Figure 1E, which includes a laser source, a chopper, a polarizer, various lenses (designated L) and filters (designated F), as well as a cuvette containing CdTe samples to be tested. TH scattered light was measured both in the forward direction and at right angles to the direction of the incident light. Briefly, femtosecond laser pulses at wavelengths of 1065 nm, 1095 nm, and 1125 nm were circularly polarized by an achromatic quarter-wave plate and focused into a fused silica cuvette containing an aqueous dispersion of CdTe nanohelices. The scattered light is then collimated and filtered to select only TH wavelengths, as described in the examples.

[0056] Working Example Example A All chemicals used in this example were analytical grade or of the highest purity available. Aluminum telluride (Al2Te3), used as a source of hydrogen telluride gas, was purchased from Materion (product number: 122704). Cadmium perchlorate hexahydrate was purchased from Alfa Aesar (product number: 12936). L- and D-cysteine ​​hydrochloride monohydrate (product numbers: C7880 and C8005, respectively), thioglycolic acid (product number: 528056), sodium hydroxide (NaOH), hydrochloric acid (HCl), and methanol were purchased from Sigma Aldrich. Deionized water (DI water) was prepared using a Milli-Q water purification system (Millipore).

[0057] Cadmium telluride nanoparticles (CdTe NPs) were synthesized by following the method from a previous publication (N. Gaponik et al., "Thiol-Capping of CdTe Nanocrystals: An Alternative to Organometallic Synthetic Routes", J. Phys. Chem. B, 106(29), 7177-7185 (2002)) (the relevant parts of this publication are incorporated herein by reference after some modifications). For chiral CdTe NPs, an aqueous solution of a mixture of cadmium perchlorate hexahydrate (Cd(ClO4)2·6H2O) and L- or D-cysteine ​​(L- / D-Cys) hydrochloride monohydrate was prepared at final concentrations of 18.75 mM and 45 mM in 125 mL of deionized water (DI water). The pH of the mixture was then adjusted to 11.2 by adding 1 M sodium hydroxide (NaOH). The mixture was placed in a 250 mL three-neck round-bottom flask and connected to another 50 mL three-neck round-bottom flask containing 0.1 g of aluminum telluride powder (Al2Te). These synthesis reaction vessels were purged with nitrogen gas for 30 minutes while being vigorously stirred for thorough mixing of the solution.

[0058] Hydrogen telluride gas was generated by introducing 0.5 M hydrogen sulfide into a small flask containing AlTe powder and slowly purging it into the mixed solution of cadmium precursor and ligand. The solution was then refluxed under nitrogen purging for approximately 10 h to obtain chiral CdTe NPs.

[0059] Achiral CdTe NPs were prepared following the same method described above, but by using thioglycolic acid (TGA) as the surface ligand source (18.75 mM) for the cadmium precursor mixed solution. After slowly purging hydrogen telluride gas, the solution was refluxed for 1 h. The as-prepared NP dispersion was stored in a dark bottle prior to the integration process, which included the aging requirement as described below.

[0060] Example B Colloids of CdTe nanohelices and achiral CdTe nanoribbons are prepared in this example. Self-assembly of nanohelices is as follows. CdTe NPs carrying L- or D-Cys, such as those described in Example A, were assembled into helical structures by a modified method described in J. Yan et al., Chem. Mater. 32, p. 476 (2020) and W. Feng et al., "Assembly of mesoscale helices with near-unity enantiomeric excess and light-matter interactions for chiral semiconductors", Sci. Adv. 3(3), e1601159 (2017), the relevant portions of which are incorporated herein by reference. The dispersions of synthesized chiral CdTe NPs were aged at room temperature in the dark for 3 to 5 days prior to self-assembly. 20 μL of 0.1 M Cd(ClO4)2·6H2O was injected into 500 μL of aged chiral NPs, and the pH was adjusted to 8 with 1 M hydrochloric acid solution. Depending on the batch, the solution was then mixed with 1 mL or 1.5 mL of methanol and kept for 3 days under room light conditions. The self-assembled colloids were centrifuged at 6,000 rpm for 3 min, and the black precipitate was redispersed in DI water. The resulting solution was treated three times with the same washing steps to ensure obtaining purified nanohelix colloids. To avoid aggregation of the nanohelices, the final precipitate was redispersed in 0.05 wt% sodium dodecyl sulfate (SDS) solution and sonicated for approximately 1 min.

[0061] Self-assembly of achiral nanoribbons is as follows. TGA-covered CdTe NPs were assembled into achiral nanoribbons by modifying the method described above for nanohelix assembly. Without adding Cd(ClO4)2·6H2O, the pH of 500 μL of aged TGA-CdTe NPs was directly adjusted to 8 by 1 M HCl solution, mixed with 1.5 mL of methanol, and kept for 3 days under room light conditions. The nanoribbon solution treated with the same washing steps of nanohelices was redispersed in 0.05 wt% SDS solution and sonicated for approximately 1 min.

[0062] Example C Characterization of nanoparticle assemblies is explored in this example, such as CdTe nanohelices and achiral CdTe nanoribbons in Example B.

[0063] Linear optical characterization. A suspension of CdTe nanohelices in a quartz glass cuvette was characterized in an Applied Photoelectron Physics Kirascan CD spectrometer. Two photomultiplier tubes (PMTs) were used as detectors, each of which was designed for measurements in a different spectral region. The measured CD spectrum of a reference sample (cuvette containing 0.2% SDS) was extracted from the spectrum of the investigated sample. The path length in the cuvette was 10 mm. The time per point was set to 0.5 s and the step to 1 nm. Each spectrum was measured three times before averaging. The bandwidth was set to 2 nm in the 300–600 nm spectral region and 40 nm in the 600–1130 nm region.

[0064] Nonlinear experiments were performed as follows. A Radiantis Inspire optical parametric oscillator (OPO) pumped by a Ti:sapphire laser was used as the laser source for the nonlinear experiments. Laser pulses were produced by the OPO at a repetition rate of 80 MHz and had a width of 200 fs. An optical chopper with a 50% duty cycle tuned the laser beam to a frequency of 246 Hz. An achromatic half-wave plate designed to work in the 690-1200 nm spectral range was placed in front of an uncoated Glan-Laser calcite polarizer to achieve power control. After passing through the polarizer (with its transmission axis oriented vertically), an achromatic quarter-wave plate (with a design wavelength range of 690-1200 nm) controlled the polarization state of the laser beam. Left-handed circularly polarized light is defined to appear along the direction of propagation from the source's perspective such that the electric field of the light follows a helix in space that rotates and propagates in a positive trigonometric direction. A pair of long-pass filters removed light with wavelengths below the cut-on wavelength (1000 nm) from the beam. A coated achromatic doublet lens (design wavelength range 1050-1700 nm, focal length 30 mm) focused the beam into a fused silica cuvette containing the sample.

[0065] In experiments measuring scattering at right angles, an anti-reflective coated 25.4-mm lens was used to collect the scattered light. Another anti-reflective coated lens (focal length 200 nm) focused the collected light onto the photocathode of the PMT. In experiments performed in transmission geometry, a 25.4-mm focal length lens was placed after the cuvette, followed by a colored glass bandpass filter (transmission in the 335-610 nm region), three UV-enhanced Al mirrors, and a 200-mm focal length lens that focused the light onto the photoelectrode of the PMT.

[0066] To investigate the polarization of THMS light, a superachromatic quarter-wave plate (design wavelength range 325–1100 nm) and an uncoated Glan-Laser calcite polarizer were added to the experimental setup.

[0067] In all experiments, a hard-coated bandpass filter with a full width at half maximum of the transmission peak of 10 nm was placed in front of the detector to isolate the scattered light in the desired wavelength range. The signal from the PMT was pre-amplified five times before entering the photon counter. The photon counter was used in the gated regime, and the signal was measured for a uniform period of time with the laser beam blocked and unblocked by an optical chopper to obtain an evaluation of noise and environmental counts.

[0068] Electromagnetic simulations were performed as follows. To compute the linear optical activity of CdTe nanohelices, a three-dimensional CdTe nanohelix structure was modeled and Maxwell's equations were solved using two different techniques. The range of geometric parameters (pitch, width, and thickness) of the three-dimensional CdTe nanohelix model structure in Figure 2A was determined based on the electron microscope images (Figure 1B). The model structure was placed in a dielectric medium with a refractive index equal to 1.33, which represents water for colloidal samples. The refractive index for CdTe was adopted from the paper by Treharne et al., Phys. Conf. Ser., 286, 012038 (2011), the relevant parts of which are incorporated herein by reference. Thanks to a simple implementation of the finite difference time domain (FDTD) technique as a full-wavelength solver, the spectra for the kill optical activity of CdTe nanohelices were calculated using the commercially available software package Lumerical. Two linearly polarized total-field scattered-field (TFSF) sources, perpendicular to each other, were used to generate CPL by setting uniform amplitude and differing in phase by 90° (or −90°).

[0069] The FDTD simulation domain was defined by a larger box monitor with a stretched coordinate perfect match layer and a non-uniform mesh type. Focusing tests with different mesh sizes were performed to determine the best balance between computational time constraints and simulation accuracy. Frequency profile and movie monitors were inserted in the full field domain to calculate the electric field enhancement in 2D. Absorption and scattering cross sections of the model structures under opposing CPLs were acquired by the two analysis groups using box output monitors, and the difference of the complete extinction cross section (the sum of the absorption and scattering cross sections) was calculated to compare with the ellipticity observed in the experimental spectra. The nanohelix model was rotated along the Cartesian axis in steps of 45° to consider the random orientation of the objects as a colloidal dispersion. To account for the variation of the geometric parameters of the internal objects due to the sharpening of the nanohelix edges, calculations were performed for nanohelices with various widths (50, 150, and 350 nm) and the obtained spectra were averaged.

[0070] The differential extinction cross section of the nanohelix model is in good agreement with the experimental observations, see Figure 1C. The 2D (x-normal) electric field profiles for Λ-CdTe oriented parallel to the incident direction of right-handed circularly polarized (RCP) and left-handed circularly polarized (LCP) light sources clearly showed the different interactions of the model for waves with opposite polarities (Figure 2B). Movies of Λ-CdTe oriented parallel or perpendicularly show information of the electric and magnetic field distributions under opposite CPL.

[0071] To investigate more deeply the optical activity of the nanohelix model at three different excitation wavelengths (1065 nm, 1095 nm, and 1125 nm), the frequency domain form of Maxwell's equations is solved by the finite element method using the COMSOL Multiphysics 5.5 software package (Radio Frequency Module). The radiation patterns for both the nanohelix models oriented perpendicular and parallel to the light propagation direction exhibited typical Mie scattering behavior (Figures 2C-2E).

[0072] Third harmonic (TH) scattering has found increasing application as a fast and sensitive method to screen for second hyperpolarized states. Due to their strong forward directionality, the attributions in these cases clearly indicate Mie scattering processes, rather than Rayleigh scattering. Computational models establish that the emission patterns from CdTe nanohelices with the same geometric scale show typical Mie scattering behavior for electromagnetic waves with all three excitation wavelengths (Fig. 2C-2F). Correctly considering the different scattering contributions further leads to a good agreement between the calculated and experimental CD spectra (Fig. 1C). Multipolar decomposition of the linear optical spectrum (Fig. 12) shows that for circularly polarized excitation, electric and magnetic dipole and quadrupole resonances can exist at both the fundamental and third harmonic wavelengths. The spectral positions of these resonances depend on the direction of the incident light for each helix, and all are accessible since the particle is freely rotating. As demonstrated in Fig. 4B, circularly polarized fundamental light produces a circularly polarized third harmonic signal. It is therefore reasonable to view the nonlinear conversion process as an energy coupling channel between the resonances identified in FIG. 12 at both the fundamental and third harmonic.

[0073] Being cautious about assigning the physical properties of the observed optical phenomena to THMS, other competing mechanisms are explored. One possibility is that the results here are not due to Mie scattering but to TH generation (THG). Both effects are coherent and both will produce strong forward directed radiation. Furthermore, THG followed by the linear optical scattering process by the nanohelix will redirect a small amount of light at right angles, which may explain the large difference in intensity between Figures 3A-3D and 4A-4B. However, THG becomes impossible in isotropic media with circularly polarized light. One reason is that while focusing a Gaussian beam in an isotropic medium, as a result of the Gouy phase shift, the THG on one side of the focal spot cancels the THG on the other side by destructive interference. Another reason is that in the CPL case, the axial spin angular momentum of each photon is (depending on the CPL orientation)

number

number

number

[0074] Furthermore, any THG from the solvent or from the glass interface can be ruled out, as demonstrated in Figures 13A-13B and 14A-14B, respectively. Furthermore, THG followed by linear optical Mie scattering should have the same sign as the measured ellipticity, which is clearly not the case (in Figures 3D and 4B). Furthermore, THG followed by linear kill optical effects such as CD could also exhibit optical rotation. As discussed in more detail below, the sample was illuminated with linearly polarized light and tested for any such optical rotation, and none was found. See Figures 15A-15B. THG can be ruled out, and further, Figures 3C and 4C demonstrate the absence of any competing multiphoton luminescence or supercontinuum effects.

[0075] Mie scattering occurs at scales that lie between those of point scatterers (Rayleigh scattering) and geometric optics. On a microscopic scale, the dielectric dipole moment is μ i = α ij E j +β ijk E j E k +γ ijkl Ej E k E l +··· (2) can be written as where i, j, k, and l may represent any of the Cartesian directions in the x, y, z coordinate system of the helix, α is the polarizability tensor, β is the first hyperpolarizability tensor, γ is the second hyperpolarizability tensor, E j is the electric field component at the fundamental frequency of light along the j Cartesian direction of the helical coordinate system (which can take on x, y, or z values). Thus, the dielectric dipole moment per unit volume at TH is P I (3ω)=χ IJKL E J (ω)E K (ω)E L (ω) (3) can be written as However, χ IJKL is the macroscopic third-order susceptibility, and I, J, K, and L represent any of the Cartesian directions in the laboratory's X, Y, Z coordinate system (Figure 1D). The expressions at the microscopic and macroscopic scales are

number

[0076] In an isotropic chiral medium, such as an enantiopure suspension of nanohelices, χ IJKL is nonzero. The isotropic chiral symmetry group belongs to one of the seven Curie limit groups for anisotropic materials. It is denoted by ∞∞ in Hermann-Morgan, ∞ / ∞ in Shubnikov, K in Schönfries, and ∞ / ∞2 in international notation. It has three independent tensor components χ IIJJ , χIJJI , χ IJIJ and they have IIII =χ IIJJ +χ IJJI +χ IJIJ where the indices I, J can be either the Lab frame coordinates X, Y, or Z, where I ≠ J.

[0077] The intensity at TH is then I(3ω)∝N〈|χ THS | 2 〉I 3 (ω) (4) It is. In general, in forward X-ray detection, the TH scattering intensity is expressed as 〈|χ THS | 2 〉=〈|χ ZJKL | 2 〉+〈|χ YJKL | 2 〉, where J, K, and L can be either Y or Z, but not X, for CPL incident light. In an isotropic chiral medium, 〈|χ ZJKL | 2 〉 and 〈|χ YJKL | 2 〉, thus TH polarization is possible along both Z and Y, resulting in the TH intensity observed in FIG. 4C, where the CPL TH light has both Z and Y components.

[0078] In contrast, in the Y direction (perpendicular to the incident beam), 〈|χ THS | 2 〉=〈|χ XJKL | 2 〉+〈|χ ZJKL | 2 〉, but again, for CPL illumination, J, K, and L can take on Y or Z values ​​instead of X. As a result, in an isotropic chiral medium, 〈|χ ZJKL | 2 > term can contribute, which means that TH can only be vertically polarized, as can be seen in FIG. 4D.

[0079] Next, we consider the microscopic hyperpolarized state. The symmetry group of the nanohelix is ​​D2 in Schönfries notation and 222 in Hermann-Morgan notation. It has 21 independent tensor components, 3 with equal indices and 18 with equal indices in pairs. In the laboratory coordinate system X, Y, Z, μ i To express this, we use the angle

number

number

number

number

number

number

number

number

[0080] therefore,

number

[0081] Similar values ​​can be calculated for other macroscopic sensitivities, but since there are 21 microscopic hyperpolarization tensor elements, each of which is complex, the number of parameters is too large to be intuitively understood.

[0082] For simplicity, we adopt here an alternative notation using the effective chiral and achiral fractions of the macroscopic sensitivity. The achiral fraction includes contributions from either the solvent or from degraded achiral CdTe particles. In the following representation, as the chirality of the sample is inverted, the chiral fraction changes sign, but the achiral fraction does not (changing the direction of the CPL has the same effect).

number

number

number

number

number

[0083] Third Harmonic Super Mie Scattering Optical Activity-Forward Scattering at 1065 nm and 1125 nm. As mentioned above, power dependent measurements of third harmonic (TH) forward scattering were presented for illumination with 1095 nm light. Figures 6A-6D show similar measurements at two other wavelengths, 1065 nm and 1125 nm, for Λ-CdTe and Δ-CdTe. A schematic of the experimental setup is shown in the inset of Figure 6A. In all measurements, the incident light is left circularly polarized (LCP) or right circularly polarized (RCP). Each data point is the median of 50 measurements. The data set includes the equation y=Ax 3 A clear optical activity is observed at both wavelengths. The sign of the optical activity is opposite to the symmetry of the CdTe nanohelix.

[0084] Figures 7A-7B show the multiphoton emission for illumination at 1065 nm. More specifically, Figures 7A-7B show the emission spectrum of a suspension of Λ-CdTe nanohelices when it is illuminated with 1065 nm light. The incident light is left circularly polarized (LCP), linearly polarized, or right circularly polarized (RCP). The incident power was 18.5 mW. For both forward and right-angle scattering, the signal detected at the TH wavelength stands out clearly in the multiphoton luminescence background.

[0085] Figures 8A-8I show comparative third harmonic super-Mie scattering for achiral CdTe nanoribbons. Achiral CdTe nanoribbons with the geometry shown in Figures 8A-8C were measured with an identical setup as used for CdTe nanohelices. The TH intensity in forward scattering geometry detected simultaneously with illumination with 1095 nm light is shown in Figures 8D, 8E. The data in the two plots originate from two separate measurements made under the same conditions. Presumably due to the large variance in the size of the nanoribbons, the results are noisier compared to the nanohelices. No optical activity is observed, as evidenced by the fit and by the calculated TH ellipticity in Figure 8F as well. Figures 8G, 8H show two separate measurements of TH intensity in right angle scattering. In the first measurement, the fit shows a larger signal for the incident LCP light. On the other hand, in the second measurement, the fit shows a larger signal for the incident RCP light. Thus, there is no consistent indication of optical activity. Indeed, when the TH ellipticity is calculated (FIG. 8I), the ellipticity is scattered around zero.

[0086] Figures 9A-9B show third harmonic super-Mie scattering optical activity at right angle scattering demonstrating THMS optical activity. In Figure 9A, TH intensity is shown in the orthogonal direction from a right-handed CdTe nanohelix (Δ-CdTe) as a function of incident laser power at a wavelength (λ) of 1095 nm for LCP and RCP light. In Figure 9B, multiphoton orthogonal emission from a Λ-CdTe nanohelix is ​​shown simultaneously with 1095 nm illumination. The TH signal (at 365 nm) clearly dominates the nearby emission wavelengths of the incident linearly polarized LCP and RCP light.

[0087] The third harmonic super-Mie scattering optical activity at 1065 nm and 1125 nm for the right-angle scattering experiments at 1065 nm and 1125 nm is shown in Figures 10A-10D. The TH intensity was measured at 1065 nm as a function of incident power. Figure 10A shows a Λ-CdTe nanohelix in the right-angle scattering setup, and Figure 10B shows a Δ-CdTe nanohelix in the right-angle scattering setup. The experimental setup is shown in the inset of Figure 10A. Similar measurements at 1125 nm are presented in Figure 10C for Λ-CdTe and Figure 10D for Δ-CdTe. In all measurements, the incident light was left-handed circularly polarized (LCP) or right-handed circularly polarized (RCP). Each data point is the median of 50 measurements. The data set includes the equation y=Ax 3 Fit the function.

[0088] The detected TH intensity is significantly lower than in the forward scattering geometry, which is consistent with the results presented for illumination at 1095 nm discussed above. Furthermore, optical activity is observed, the sign of which varies with the symmetry of the CdTe nanohelices. However, for each sample, the sign of the optical activity is opposite to that in forward scattering.

[0089] The third harmonic Mie scattering polarization is shown in Figures 11A-11B. In Figure 11A, the TH intensity in the forward direction is shown as a function of the rotation angle of the quarter wave plate (AWP) relative to the Δ-CdTe. LCP and RCP incident light produces LCP and RCP TH light, respectively. In Figure 11B, the TH intensity in the 90° direction is shown as a function of the AWP rotation angle relative to the Δ-CdTe. LCP and RCP incident light produces linearly polarized TH light. All measurements were performed for incident 1095 nm light.

[0090] Figure 12 shows the multipolar spectral decomposition of the nanohelix scattering cross section. The curves correspond to the electric dipole (ED), magnetic dipole (MD), electric quadrupole (EQ), and magnetic quadrupole (QD) as well as the total scattering cross section upon illumination with right- and left-circularly polarized light (LCP and RCP, respectively). The circular difference (CD) corresponds to the difference (Δ) in the scattering cross section.

[0091] To determine the contribution of the solvent to the third harmonic scattering (TH) signal, experiments were performed with a liquid medium containing 0.2% sodium dodecyl sulfate (SDS) in an aqueous medium (water) at forward and 90° emission. Figure 13A shows the measured TH intensity as a function of laser power for left circularly polarized (LCP) and right circularly polarized (RCP) incidence. A schematic of the experimental setup is provided in the inset in Figure 13A. Clearly, there is no TH forward emission from the solvent. Figure 13B shows the TH intensity as a function of incident laser power for 0.2% SDS illuminated by LCP and RCP light. Clearly, there is no TH scattering from the solvent. The inset in Figure 13B shows a schematic of the setup for measuring TH emission at right angles. In both plots, the sample was illuminated by 1095 nm light.

[0092] The lines represent linear fits to y = Ax + B. For LCP, the coefficients A and B are 10 -3 and 3 x 10 -2 For the RCP, these coefficients are -6.1×10 -3 and 5.6 x 10 -2 Therefore, it can be concluded that the contribution of the solvent to the results is negligible. Figure 13B shows the TH intensity emitted at right angles from SDS. The figure is constructed similarly to Figure 10A. For LCP, the coefficients A and B are -1.1 x 10 -2 and 4.4 x 10 -2 For the RCP, these coefficients are 2.4×10 -3 and -5.8 x 10 -2Therefore, again, the contribution of the solvent to the results can be neglected. These results unequivocally demonstrate that the TH results are due to the nonlinear optical properties of the CdTe nanohelices.

[0093] Determination of third harmonic scattering / generation at 10 mm cuvette interfaces. All samples are measured in quartz glass cuvettes. Breaking of symmetry at interfaces can lead to strong nonlinearities. Therefore, determine whether TH generation at air / quartz, quartz / solvent, solvent / quartz, and quartz / air interfaces contributes to the measured TH intensity.

[0094] The TH intensity measured in the forward scattering setup for various positions of the focus lens are presented in Figure 14A-14B. For incident linearly polarized light, four peaks of TH intensity are observed. These peaks correspond to the four interfaces of the cuvette. When the focus lens is placed between approximately 86 mm and 92 mm, the peaks are narrow, so there is no contribution from the interfaces. For incident LCP light, the TH intensity generated at the interfaces of the cuvette is much lower than for linearly polarized light. For the measurements on the CdTe nanohelices, the incident light is circularly polarized and the focus lens is placed at 89.5 mm, clearly far from any interfaces. Therefore, there is no contribution from TH generation at the glass interfaces in any of the measurements. To verify this observation, power-dependent measurements with an empty cuvette are presented in Figure 14B. The filled circles and triangles correspond to LCP and RCP illumination, respectively. The lines are fitted to the equation y=Ax+B. For LCP, coefficients A and B are -4.1×10 -4 and 3.3 x 10 -3 For RCP, coefficients A and B are 1.1×10 -3 and -2.3 x 10 -2 Therefore, the contribution from the glass interface can be neglected.

[0095] Moreover, the results in Fig. 14B are important because they demonstrate that there is no TH generation from any of the optical components in the setup, regardless of the illumination power. Furthermore, these same results show that the detector is not affected by any external light sources, such as the instrument LEDs and displays in the lab.

[0096] Next, a test for the presence of optical rotation is performed. Figure 15A shows a schematic diagram of the setup. The fundamental is linearly polarized along the vertical (S) direction. The quarter-wave plate is not removed to avoid significantly changing the setup, however its fast axis is set parallel to the direction of the incident polarization. The analyzing polarizer (analyzer) is placed on a rotation stage in front of the detector. An angular position of 90° corresponds to the vertical direction of polarization. The third harmonic signal is then measured as a function of the analyzer angle. For both chiral forms of the sample, the data are shown in Figure 15B. As can be seen, the third harmonic light is vertically polarized and there is no measurable optical rotation.

[0097] Third harmonic scattering / generation at the 1 mm cuvette interface is determined in Figure 16. More specifically, Figure 16 shows the TH intensity as a function of focus lens position for illumination with linear and left circularly polarized (LCP) 1095 nm light (incident power = 15 mW). Measurements were performed in forward scattering geometry. No third harmonic (TH) light is observed from the 1 mm cuvette interface.

[0098] Figures 17A-17D show the optical activity of third harmonic super-Mie scattering at 1065 nm and 1125 nm when the sample was measured in a cuvette with a 1 mm path length. Measurements of TH intensity as a function of power for Λ-CdTe and Δ-CdTe nanohelices placed in a cuvette with a 1 mm path length are presented in Figures 17A-17D. These power-dependent curves were used to calculate the ellipticity in Figure 5A.

[0099] 5A-5E show an example application of THMS to characterize chiral nanostructures in ultra-small volumes. FIG. 5A shows proof-of-principle data showing that the method according to certain embodiments of the present disclosure can clearly distinguish between Λ-CdTe and Δ-CdTe in a 1 mm thick optical cuvette (as opposed to a standard 1 cm cell). THMS ellipticity was calculated from power dependence curves measured at three different wavelengths. FIG. 5B shows that in the same 1 mm cuvette, the TH intensity follows a clear third-order dependence as a function of laser power at a wavelength of 1095 nm. Despite the small dimensions of the cuvette, the kill optical effects for LCP and RCP, respectively, are clearly opposite in sign due to the symmetry of the samples, indicating the potential for very small volume applications. FIG. 5C shows a schematic diagram showing an example application of the technique according to certain embodiments of the present disclosure as an analytical tool for parallel combinatorial chemical synthesis. Figure 5D shows that high-throughput applications can be enabled by scanning a laser beam within an optical objective to probe reaction conditions that generate nanomolar amounts of a desired compound in minute volumes (e.g., <1 μL) arrayed across a microplate. The red arrow indicates the direction of the incident light. Figure 5E shows a schematic diagram for in-line reaction monitoring within a microreactor.

[0100] These examples therefore demonstrate the fundamental capability of nonlinear kill optical activity for Mie scattering represented by THMS. As determined above, contributions from THG, multiphoton luminescence and supercontinuum generation were carefully excluded and this effect was observed for semiconductor CdTe nanohelices at three different wavelengths. The magnitude of THMS is large, approximately 4.56 × 10 -14 m 3 V focusThe illumination volume as small as 1000 nm exhibits a TH ellipticity of approximately 3°. In accordance with the physics of Mie scattering, the effect is highly directional, with approximately 10 times more TH light detected in the forward direction compared to the sideways direction. The TH radiation in the forward direction is circularly polarized, whereas in the orthogonal direction, the TH radiation is linearly polarized (vertically). In both cases, a clear kill optical response with inverted sign is observed. The inverted sign indicates that the forward and orthogonal radiation are due to different sets of TH effective susceptibility tensor components, whereby the phase between the chiral and achiral parts changes sign depending on the direction of radiation. These results suggest that a novel achiral scattering technique, potentially 10 -17 m 3 This paves the way for the chiral optical characterization of semiconductor and other chiral non-metallic particles of orders of magnitude in volume. The ability to characterize such miniaturized reaction volumes provides a technological link between chemical synthesis and exploring the data science requirements of chiral nanostructures. Furthermore, the capability could potentially be extended to multi-scale tissues and chiral nanostructured particles such as extracellular vesicles, which have similar dimensions and are widely investigated today for cancer detection. By labeling with inorganic nanoparticles, the high THMS intensity provides a route to detect and enumerate the presence of rare extracellular vesicles containing microfluidics.

[0101] Thus, the present disclosure contemplates the use of Kir optical spectroscopy to provide new optical dimensions and informative data sets for structural analysis of nanostructured particles. Kir optical spectroscopy can be utilized for robotic optimization of nanophotonic materials, but these spectroscopy methods typically require sample volumes that are incompatible with generating large chemical libraries. These new optical tools can characterize chirality in ultra-small volumes such as 1 μL droplets, which are necessary for high-throughput synthesis and analysis stations for chiral compounds. We experimentally demonstrated that a novel photonic effect that enables such capabilities - third harmonic Mie scattering optical activity - is observed in suspensions of CdTe nanostructured helices in volumes several orders of magnitude smaller than 1 μL. Kir optical third harmonic emission was recorded when CdTe helices were illuminated with 1065 nm, 1095 nm, and 1125 nm laser beams, and the THMS intensity was roughly 10 times higher in the forward direction than in the transverse direction. The third harmonic ellipticity was approximately 3° high. This is attributed to the effect of interference between the chiral and achiral effective nonlinear susceptibility tensor components. Therefore, the THMS for the semiconductor helix is ​​10 -5 It provides the capability for rapid high-throughput kill optical characterization of sample volumes as small as 1 μL.

[0102] The preceding description of the embodiments has been provided for purposes of illustration and description. The preceding description of the embodiments is not intended to be an exhaustive disclosure or to limit the disclosure. Individual elements or features of a particular embodiment are generally not limited to that particular embodiment, but may be interchangeable, where applicable, and may be used in selected embodiments even if not specifically shown or described. Moreover, the same may vary in many ways. Such variations should not be considered as departures from the present disclosure, and all such modifications are intended to be included within the scope of the present disclosure.

Claims

1. 1. A method for detecting a chiral feature in a sample, the method comprising: directing light towards a sample in contact with chiral nanoparticles; detecting third harmonic Mie scattering (THMS) optical activity generated by the chiral nanoparticles in contact with the sample.

2. 2. The method of claim 1, wherein the third harmonic Mie scattering (THMS) optical activity is third harmonic (TH) radiation in a forward direction that is circularly polarized.

3. The method of claim 1 , wherein the sample has a volume of about 1 microliter or less.

4. The sample is about 10 -5 10. The method of claim 1, having a volume of at least a microliter and no more than about 1 microliter.

5. The method of claim 1 , wherein the chiral nanoparticles comprise a semiconductor material.

6. The method of claim 1 , wherein the chiral nanoparticles comprise cadmium telluride (CdTe).

7. The method of claim 1 , wherein the chiral nanoparticles comprise a plurality of chiral nanoparticles self-assembled together to define at least one self-assembled nanostructured helix.

8. 2. The method of claim 1, wherein the chiral nanoparticles comprise a plurality of chiral nanoparticles integrated together, each chiral nanoparticle being in the form of a nanohelix having a length of about 5 micrometers to about 8 micrometers and a thickness of about 10 nm to about 50 nm.

9. The method of claim 1 , wherein the light is circularly polarized light.

10. 1. An apparatus for detecting a chiral property of a sample, said apparatus comprising: at least one microwell having a volume of about 1 microliter or less configured to hold chiral nanoparticles capable of generating third harmonic Mie scattering (THMS) optical activity and a sample to be analyzed; a light source configured to generate light and direct the light to the at least one microwell containing the chiral nanoparticles and the sample; and at least one detector configured to detect third harmonic Mie scattering (THMS) generated by the chiral nanoparticles in the at least one microwell.

11. The device of claim 10 , wherein the chiral nanoparticles are provided within the sample in the microwell.

12. The device of claim 10 , wherein the chiral nanoparticles are associated with a surface of the microwell.

13. The microwells are about 10 -5 The device of claim 10 having a volume of at least a microliter and up to about 1 microliter.

14. The device of claim 10 , wherein the chiral nanoparticles comprise a semiconductor material.

15. The device of claim 10 , wherein the chiral nanoparticles comprise cadmium telluride (CdTe).

16. The apparatus of claim 10 , wherein the chiral nanoparticles comprise a plurality of chiral nanoparticles self-assembled together to define at least one self-assembled nanostructured helix.

17. 11. The device of claim 10, wherein the chiral nanoparticles comprise a plurality of chiral nanoparticles integrated together, each chiral nanoparticle in the form of a nanohelix having a length of about 5 micrometers to about 8 micrometers and a thickness of about 10 nm to about 50 nm.

18. The apparatus of claim 10 , wherein the light source is configured to generate circularly polarized light and to guide the circularly polarized light.

19. 11. The device of claim 10, wherein the at least one microwell comprises an array of microwells.

Citation Information

Patent Citations

  • Preparation method of ordered chiral copper iron selenide nano-film with near-infrared light response

    CN111994883A

  • Medium measuring surface plasmon resonance sensor having circular dichroism, and method and device for measuring circular dichroism

    JP2009210495A

  • Production of chiral gold nanorod organization body using serum protein

    JP2015155824A

  • Method for detecting amino acid using chiral gold NANO rod structure

    JP2016142699A

  • Apparatuses and methods for up-converting electromagnetic radiation

    US20080258079A1