Power module with patterned sintered connections and method for producing the power module - Patents.com
Patterned sintered connection layers in power modules address the issue of internal thermomechanical stresses by distributing and reducing stress, improving reliability and durability through partial coverage and flexible design.
Patent Information
- Application Number
- JP2024600002U
- Authority / Receiving Office
- JP · JP
- Patent Type
- Utility models
- Current Assignee / Owner
- Priority Date
- 2021-07-05
- Filing Date
- 2022-06-30
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2032-06-30
AI Technical Summary
Existing power modules experience undesirable deformations and potential damage due to internal thermomechanical stresses caused by temperature fluctuations, particularly in sintered connections that are not patterned, leading to issues like internal cracks and delamination.
The implementation of patterned sintered connection layers in power modules, where the area covered by sintered material is partially uncovered, with a ratio of uncovered surface to covered area ranging from 10% to 75%, allowing for improved flexibility and stress distribution, reducing internal thermomechanical stresses.
The patterned sintered connection layers significantly reduce internal stresses, enhancing the reliability and durability of power modules by minimizing deformation and damage from thermal cycling, while maintaining mechanical stability.
Smart Images

Figure 0003248739000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a power module with at least one patterned sintered connection and a method for manufacturing the power module. [Background technology]
[0002] Sintering is a preferred method for establishing mechanically strong and reliable bonded connections. With respect to the thermomechanical stresses typically occurring in thermal cycling, the reliability of sintered connections, illustratively silver sintered connections, can significantly exceed that of soldered connections. Sintered bonded connections, for example prepared from silver or copper fine particles or nanoparticles, can be used not only for die bonding, but also for clips or other planar contacts that can be fixed, for example, to the upper contact surface of a chip, or to bond a substrate with a base plate.
[0003] US Patent Application Publication No. 2019 / 043791 describes a sintering metal paste used to form a sintering metal bond. The sintering metal paste is, for example, a sintering silver paste. The sintering metal paste is applied to a predetermined portion of a first pad portion, and a coating area and a non-coating area are preset in the first pad portion. The coating area is an area to which the sintering metal paste is applied. The non-coating area is an area to which the sintering metal paste is not applied. The coating area and the non-coating area 62 may have different continuous or discontinuous shapes.
[0004] JP 2014-029964 A provides a bonding method for joining an aluminum member to another member using a joining material containing silver oxide. In particular, the method includes a base layer forming step of forming a base layer and an uncovered portion of the base layer on the surface of the joining surface of the aluminum member, and forming the uncovered portion of the base layer so as to extend to the peripheral portion of the joining surface. A joining material disposing step is performed to dispose the joining material between the aluminum member and the other member. A sintering step is also performed to sinter the joining material to form the uncovered portion and the joining layer, thereby joining the aluminum member to the other member via the uncovered portion and the joining layer.
[0005] US Patent Application Publication No. 2012 / 211764A1 describes a nano-Ag paste that is applied around a solder sheet in the area of a lead frame, and a semiconductor element is mounted in a face-up manner on the solder sheet and the nano-Ag paste. The nano-Ag paste and the solder sheet are heated to form the solder sheet. At this time, the Ag particles contained in the nano-Ag paste are sintered before the solder sheet melts, forming a film-like porous metal material. When the solder sheet melts, the molten solder flows into the pores of the porous metal material, and the remaining molten solder remains in the center part. When the solder solidifies in the subsequent cooling process, a composite material is formed, and a solder layer is formed inside the composite material.
[0006] SUMMARY OF THE DISCLOSURE An embodiment of the present disclosure relates to a power module having reduced internal thermo-mechanical stresses. Further embodiments of the present disclosure relate to a simplified yet efficient method for manufacturing a power module having low internal thermo-mechanical stresses. Summary of the Invention [Problem to be solved by the invention]
[0007] SUMMARY OF THE DISCLOSURE Embodiments of the present disclosure address, in whole or in part, the above-mentioned shortcomings in the art. Further embodiments of the power module and the method for manufacturing the power module are the subject of further claims. [Means for solving the problem]
[0008] According to an embodiment of the power module, it comprises at least two module components and at least one connection layer, which is formed along the vertical direction between the at least two module components for mechanically connecting the at least two module components. The at least one connection layer is a sintered connection layer forming a sintered connection between the at least two module components. The at least one connection layer is patterned, such that, in a top view, the area of the sintered connection is only partially covered by the sintered material and the sub-areas of the area not covered by the sintered material are bounded by one or several outer edges of the area. Furthermore, the ratio of the surface of the non-covered sub-area to the respective area of the sintered connection is ≧10% and ≦75%. For example, the power module is a power semiconductor module. Furthermore, the at least one connection layer can also be used to electrically connect the at least two module components.
[0009] In the case of power modules in which the module components are mechanically joined to each other by non-patterned or non-structured sintered layers, undesirable deformations may occur during the manufacture or operation of the power module due to internal thermomechanical stresses, for example caused by the effects of temperature fluctuations. Such undesirable deformations may form internal cracks in the power module, for example in the joint connections, peeling of module components, or other damage to the power module. In contrast, using a patterned sintered connection layer, a very high reliability of the power module with respect to thermomechanical stresses can be achieved, since the patterned sintered connection layer does not cover the entire area of the sintered connection, and is therefore less rigid and in this sense more flexible, and may act as a compensation layer to distribute or reduce internal thermomechanical stresses in the power module, for example in the joint connections and at the corresponding interfaces with the joint partners.
[0010] It has been found that a significant reduction of the internal thermomechanical stresses in the connection layer and the power module can be achieved using a ratio of the surface of the non-coated sub-area to the respective area of the sintered connection of ≧10% and ≦75%. For example, the ratio is 15%-75%, 15%-65%, 15%-55%, 15%-45%, 15%-35%, or 25%-75%, 35%-75%, 45%-75%, or 55%-75%. If the ratio is less than 15%, for example less than 10%, less than 7%, less than 5% or less than 3%, the effect of reducing the internal thermomechanical stresses is very low or almost non-existent. If the ratio is more than 75%, a mechanically stable connection between at least two module parts may not always be guaranteed.
[0011] Furthermore, the area ratio of the surface of the uncovered subregion to the surface of the area of the connection covered by the sintered material can be 0.25 to 4, 0.5 to 2, 0.75 to 1.5, 1 to 1.5, or 0.75 to 1.25.
[0012] Furthermore, since sub-regions of the area of the sintered connection that are not covered with sintering material are bounded by one or several outer edges of the area of the sintered connection, these sub-regions can be used, for example, to improve the removal of gases or organics during the sintering process, thereby improving the quality of the sintered connection.
[0013] In the present disclosure, the area of sintered connection or the area of connection can be considered as the overlapping surfaces or vertical intermediate spaces between at least two modular parts, which intermediate spaces are filled by sintered material in some places and not filled by sintered material in other places. The area of sintered connection can also be defined by the rear side or the front side of one of the at least two modular parts. The vertical direction is understood to mean a direction oriented perpendicular to the main extension plane of one or both of the at least two modular parts. The lateral direction is understood to mean a direction parallel to the main extension plane of one or both of the at least two modular parts. The vertical direction and the lateral direction are perpendicular to each other.
[0014] According to a further embodiment, the at least two module components are elements from the group comprising base plate, substrate, electronic component and electrical connection. Here, the power module can comprise three or more module components. It is also possible that the power module comprises at least two substrates arranged vertically above one another. Furthermore, it is also possible that the power module comprises at least two substrates arranged laterally adjacent to one another and mechanically and / or electrically connected to one another by a third module component, for example an electrical connection in the form of a clip.
[0015] The base plate can be used, for example, to receive and carry a substrate. The base plate can be made of a metal or metal alloy, for example, including or made of CU or Al, or a corresponding alloy. Alternatively, the base plate can be made of a composite material, for example a composite material including SiC. Such materials can be filled with a metallic material such as Al or Mg, resulting in AlSiC or MgSiC. However, the base plate is not limited to the above materials.
[0016] The substrate can be used to receive one electronic component or several electronic components. For example, the substrate comprises a front metallization and a rear metallization, the front metallization being vertically separated from the rear metallization by an insulating layer. The insulating layer can be made of a ceramic material such as AlN, Si3N4, Al2O3, or a resin material with inorganic fillers. The front metallization can comprise one first metallization layer and one second metallization layer, which is electrically and spatially separated from the first metallization layer, for example by an isolation trench. The first metallization layer and the second metallization layer can be assigned to different electrical polarities of the power module or electronic component. For example, the electronic component is arranged on the front metallization and is electrically connected to both the first metallization layer and the second metallization layer. The front metallization can comprise multiple first metallization layers and / or multiple second metallization layers. The substrate can be a printed circuit board.
[0017] The electronic components may be, but are not limited to, electronic chips, semiconductor chips, e.g. sensors for measuring temperature, switching devices such as IGBTs, power MOSFETs made of silicon, silicon carbide, gallium nitride or other semiconductor materials, diodes, resistors, capacitors, inductive components or discrete devices such as transistors.
[0018] The electrical connection can be a clip, a terminal, e.g. a terminal leg, or a planar contact structure, e.g. a platelet, to which another connection element is attached. For example, the electrical connection is used to electrically connect an electronic component with a second metallization of a substrate. For example, an electronic component is placed on a first metallization layer, and the electrical connection electrically connects the front side of the electronic component with the second metallization layer. It is also possible that the electrical connection is configured to interconnect two chip surfaces, e.g. two surfaces of two electronic components, or two metallization patterns of a substrate. At least one patterned sintered connection layer can be applied, for example, in the form of a terminal leg or other planar contact to the chip surface or to the metallization of the substrate, to join the electrical connection. Furthermore, at least one patterned sintered connection layer can be applied, for example, to join contact platelets that can be used for copper wire bonds, or to join terminals on the chip surface, so that no additional sintered connection on the substrate is required.
[0019] According to further embodiments, the at least one patterned sintered connection layer is arranged along the vertical direction between the electrical connection and the electronic component, between the electrical connection and the substrate, between the electronic component and the substrate, or between the substrate and the base plate. Depending on the position of the at least one patterned sintered connection layer, the at least one patterned sintered connection layer can be directly adjacent to the base plate, the substrate, the electronic component, and / or the electrical connection.
[0020] Therefore, some joint connections that can be realized by the sintered connection layer are: between the upper surface of the chip and an electrical connection, for example in the form of a clip, another type of planar contact element of the terminal, for example a contact platelet, between the substrate metallization and an electrical connection in the form of, for example, clips, terminals or other types of planar contact elements, - Between the substrate metallization and the chip backside (die bond) and / or - Between the base plate and the substrate (substrate bond), can be placed in
[0021] Some specific types of bonding connections on the top surface of the chip may include clips interconnecting the chip surface and the substrate surface, terminals with legs for the interconnection, the latter may be associated with external terminals attached directly to the chip surface, or other types of planar contacts. The electrical connections may be contact elements in the form of clips, terminals, or another type of planar contact, for example contact platelets to facilitate wire bonding with thick copper bonding wires, the contact elements being made of copper, silver, aluminum, or corresponding alloys. The contact elements and / or bonding surfaces of the electronic component or substrate may be coated with one additional metal layer, for example a noble metal such as gold or silver, to improve the bonding process.
[0022] The module component may comprise multiple connection layers, for example one connection layer between the electrical connection and the electronic component, one connection layer between the electrical connection and the substrate, one connection layer between the electronic component and the substrate, and / or one connection layer between the substrate and the base plate, at least one of the connection layers being sintered. If the power module comprises two or more substrates, at least one connection layer, for example at least one sintered connection layer, may also be formed between the two substrates.
[0023] At least one, two, three or all of these connection layers can be patterned sintered connection layers. The sintered connection layers can be patterned in the same way so that the patterned sintered connection layers show a similar structure or design when viewed from above. However, different sintered connection layers at different positions can be patterned in different ways so that the different sintered connection layers at different positions can show different structures or designs when viewed from above. It is also possible that one, two or three connection layers are not patterned sintered connection layers and / or sintered connection layers. Instead of sintered connection layers, the non-patterned one, two or three connection layers can be normal connection layers such as solder layers.
[0024] According to a further embodiment, at least one connection layer is continuous. In other words, all sub-regions of at least one connection layer are connected to each other. Viewed from above, at least one patterned sintered connection layer can have, but is not limited to, a comb, cross, star or zigzag shape. Locally, at least one connection layer can show a striped pattern, and different sub-regions of the connection layer can have the form of a number of stripes, for example parallel stripes, connected to each other.
[0025] Subregions of the area of the sintered connection that are not covered by the sintering material can form local intermediate spaces or gaps between different subregions of the connection layer. Such intermediate spaces or gaps can be seen as grooves or trenches that can reach at least one edge or several edges of the sintered connection. In other words, such intermediate spaces or gaps can be bounded by one or several outer edges of the area of the sintered connection.
[0026] However, it is also possible that at least one connecting layer is discontinuous. In this case, at least one connecting layer can comprise spatially separated sub-regions. Viewed from above, the spatially separated sub-regions can form a stripe-like or dot-like layout. Some or all of the spatially separated sub-regions can have stripe shapes of the same or different sizes, or dot shapes of the same or different sizes. The dot shapes can be of any geometric form. For example, a dot shape or dot pattern can comprise a plurality of circular, square, rectangular and / or hexagonal dots. The connecting layer comprises spatially separated sub-regions, intermediate spaces or gaps between the separated sub-regions of the connecting layer. As in the case of adjacent connecting layers, the intermediate spaces or gaps can reach at least one edge or several edges of the sintered connection, i.e. one or several outer edges of the area of the sintered connection.
[0027] In both cases, in the case of discontinuous connection layers as well as in the case of continuous connection layers, the non-covered sub-regions of the connection area can form channel-like grooves that can extend laterally from the inner sub-regions of the connection area towards one or several outer edges of the connection area. Some of the non-covered sub-regions can be located next to the edges of the connection area. The non-covered sub-regions can be empty spaces, e.g. at least some or all of the non-covered sub-regions can be filled with a gaseous medium, such as the surrounding air, which can be used to remove gases or organic matter during the sintering process. This can improve the quality of the sintered connection. However, in some cases, the non-covered sub-regions can also be filled with an electrically insulating material, e.g. a mechanically flexible or soft rigid insulating material for compensating internal thermomechanical stresses in the power module, e.g. in the connection layer. The non-covered sub-regions can also be filled with an electrically conductive material different from the sintering material.
[0028] The lateral width, e.g., average lateral width, of the gap, space, or channel-like groove can be greater than 0.1 mm, 0.2 mm, 0.5 mm, 0.7 mm, or 1 mm, for example, but not limited to, 0.1 mm to 3 mm, 0.5 mm to 3 mm, 1 mm to 3 mm, or 0.1 mm to 2 mm, 0.5 mm to 2 mm, or 1 mm to 2 mm.
[0029] The thickness of at least one patterned sintered connection layer may be 100 μm or less, for example, 10 μm to 100 μm, 10 μm to 80 μm, 10 μm to 70 μm, or 20 μm to 50 μm. When the layout of the patterned sintered connection layer comprises stripes or dots, the width of the stripes or the diameter or side length of the dots can be in the range of 0.1 mm to 2.0 mm, for example, in the range of 0.1 mm to 1.5 mm, 0.1 mm to 1.0 mm, 0.1 mm to 0.5 mm, or in the range of 0.3 mm to 2.0 mm, 0.5 mm to 2.0 mm, 1 mm to 2.0 mm, or 1.5 mm to 2.0 mm.
[0030] For example, in the case of a substrate bonding connection between a substrate and a base plate, the gaps, spaces or channel-like grooves and / or patterns or stripes or dots may have a width or length or diameter greater than 2 mm, 3 mm, 5 mm, or greater than 10 mm. The thickness of the connection layer in this case may be greater than 100 μm, 150 μm, or 200 μm.
[0031] According to one embodiment of a method for producing a power module, such as a power module as described in the present disclosure, the method comprises a step of forming at least one sintered connection layer, the sintering material being applied on one or both surfaces of the two module parts, for example by stencil printing, by evaporation or sputtering using a mask for patterning the at least one connection layer, or by another method for applying the sintering material. This can also be achieved by structuring an originally homogeneous layer.
[0032] As the material of the sintered material, silver or copper can be used. For example, nano-sized and / or micron-sized silver or copper particles can be used. During the sintering process, pressure can be applied, for example, a certain pressure can be applied to adjust the porosity or denseness of at least one connecting layer. Such a procedure can be called pressure sintering or pressureless sintering method. In other words, the sintering process can be performed with high pressure, low pressure or without pressure. The application of pressure is related to the desired porosity or denseness of the final sintered layer. A higher pressure during the process usually leads to a lower porosity and, as a result, a higher mechanical strength of the sintered layer.
[0033] The present disclosure includes several aspects of power modules and methods for manufacturing power modules based on their embodiments and examples. All features described with respect to one of the aspects are also disclosed herein with respect to the other aspects, even if each feature is not explicitly mentioned in the context of a particular aspect. For example, the method described in the present disclosure relates to the manufacture of any of the embodiments of the power modules described herein. Thus, features and advantages described in relation to the power module can be used in the method, and vice versa.
[0034] While the present disclosure is susceptible to various modifications and alternative forms, details of which have been shown by way of example in the drawings and will be described in detail. It should be understood, however, that the intention is not to limit the disclosure to the specific described embodiments and examples. On the contrary, the intention is to cover all modifications, equivalents, and alternatives falling within the scope of the disclosure as defined by the appended claims.
[0035] The accompanying drawings are included to provide a further understanding. In the drawings, elements of the same structure and / or function may be assigned the same reference numerals. It should be understood that the examples shown in the figures are illustrative representations and are not necessarily drawn to scale. [Brief description of the drawings]
[0036] [Figure 1] FIG. 1 illustrates a general concept of a power module according to an example. [Figure 2A] FIG. 2 illustrates a specific implementation of a power module according to an example. [Figure 2B] 11A-11C show different layouts of the connection layer according to different examples. [Figure 2C] 11A-11C show different layouts of the connection layer according to different examples. [Figure 3A] 11A-11C show different layouts of the connection layer according to different examples. [Figure 3B] 11A-11C show different layouts of the connection layer according to different examples. [Figure 3C] 11A-11C show different layouts of the connection layer according to different examples. [Figure 3D] 11A-11C show different layouts of the connection layer according to different examples. [Figure 3E] 11A-11C show different layouts of the connection layer according to different examples. [Figure 3F] 11A-11C show different layouts of the connection layer according to different examples. [Figure 4A] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 4B] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 4C] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 4D] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 4E] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 4F] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 4G]FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 5A] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 5B] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 5C] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 6A] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 6B] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 6C] FIG. 13 shows a power module according to another example and some simulations using "von Mises stress" showing the distribution of thermomechanical stresses in different connection layers and different module components of the power module. [Figure 7A] 2D simulation of a cross section according to the length direction of the clip, a cross section of a power module in a patterned sintered connecting layer having a stripe layout with stripes of different sizes including a stress distribution obtained by the "von Mises stress". [Figure 7B] 7A shows a 2D simulation of a cross section of the clip along its length, illustrating the distribution of thermomechanical stresses in a power module including a connecting layer with two stripe layouts of different sizes, where the thermomechanical stresses are obtained along the dashed line shown in FIG. 7A. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0037] FIG. 1 shows a power module 10 comprising at least two module components M and at least one connection layer 5. The module components M can be a base plate 1, a substrate 2, an electronic component 3 or an electrical connection 4. The at least one connection layer 5 is formed along the vertical direction between the two module components M in order to mechanically connect the two module components. The at least one connection layer 5 can also be used to thermally and possibly electrically connect the two module components. The at least one connection layer 5 can be one connection layer 5 in the form of a lower connection layer 5A formed between the base plate 1 and the substrate 2, one connection layer 5 in the form of a first connection layer 5B formed between the substrate 2 and the electronic component 3, one connection layer 5 in the form of a second connection layer 5C formed between the electronic component 3 and the electrical connection 4 or one connection layer 5 in the form of a third connection layer 5D formed between the substrate 2 and the electrical connection 4.
[0038] For example, as shown for example in FIG. 2A, the connection layer 5A mechanically and / or thermally connects the base plate 1 with the substrate 2. The connection layer 5B mechanically, electrically and / or thermally connects the electronic component 3 with the substrate 2. The connection layer 5C mechanically, electrically and / or thermally connects the electronic component 3 with the electrical connection 4, which may be a clip, a terminal or a planar contact element. The connection layer 5D mechanically, electrically and / or thermally connects the electrical connection 4 with the substrate 2, for example when the electrical connection 4 is a clip. However, when the electrical connection 4 is a terminal or a planar contact element, the connection layer 5D may not be present. The terminal or the planar contact element may be mechanically and electrically connected with the electronic component 3 by the connection layer 5C. Furthermore, the terminal or the planar contact element may be electrically connected to the metallization layer 22 of the substrate 2, for example by using a bond wire.
[0039] Exactly or at least one, two, three or all of the connection layers 5, 5A, 5B, 5C, 5D can be formed as sintered connection layers forming a sintered connection between two respective module parts M, 1, 2, 3 and 4. The sintered connection can be patterned such that, viewed from above, an area 50 of the sintered connection is only partially covered by the sintered material. The area 50 can be an area 50A between the base plate 1 and the substrate 2, an area 50B between the electronic component 3 and the substrate 2, an area 50C between the electronic component 3 and the electrical connection 4 or an area 50D between the electrical connection 4 and the substrate 2.
[0040] For example, area 50A may be defined by joining a surface of base plate 1 and substrate 2. Area 50B may be defined by joining a surface of electronic component 3 and substrate 2. Area 50C may be defined by joining a surface of electronic component 3 and electrical connection 4. Area 50D may be defined by joining a surface of electrical connection 4 and substrate 2.
[0041] If any of the connection layers 5, 5A, 5B, 5C and 5D are patterned, the corresponding area of connection 50, 50A, 50B, 50C or 50D may comprise sub-regions 50U, 5AU, 5BU, 5CU or 5DU that are not covered by sintered material. As shown in Figures 1 and 2A, any of the connection layers 5A, 5B, 5C and 5D may have a striped layout. In this case, the sub-regions 5AU, 5BU, 5CU or 5DU are the lateral spaces between or surrounding the stripes. The sub-regions 50U, 5AU, 5BU, 5CU and 5DU may be bounded by one or several outer edges 50E, 5AE, 5BE, 5CE and 5DE of the connection area 50A, 50B, 50C, 50D, respectively. It is also possible that one or several of the connection layers 5A, 5B, 5C and 5D are not sintered and / or patterned.
[0042] The non-covered sub-regions 50U may thus form channel-like grooves extending laterally from the inner sub-regions of the connection area 50 towards one or several outer edges 50E of the connection area 50. The channel-like grooves can be used to remove gases or organic matter during the sintering process. On the connection area 50, the non-covered sub-regions 50U may form a continuous structure. In this case, the connection area 50 may be a void of the non-covered inner sub-region completely surrounded by the connection layer 5. The connection area 50 therefore does not comprise an inner sub-region in which gases or organic matter may be trapped. However, it is also possible that the connection area 50 comprises at least one non-covered inner sub-region completely surrounded by the connection layer 5 in the laterally direction.
[0043] Furthermore, the non-coated sub-area 50U can act as a compensation area to distribute or reduce internal thermomechanical stresses in the power module. The non-coated sub-area 50U, i.e. 5AU, 5BU, 5CU or 5DU, may be empty and filled with ambient air. However, in some cases, the non-coated sub-area 50U can also be partially filled with an electrically insulating material, for example an encapsulating material. The non-coated sub-area 50U can also be filled with an electrically insulating material, for example a mechanically flexible, elastic or soft rigid insulating material for compensating internal thermomechanical stresses, or filled with a conductive material different from the sintered material. For example, at least one or all of the connection layers 5A, 5B, 5C or 5D are silver or copper sintered connection layers. Due to the high mechanical strength, the silver or copper sintered bonded connection offers very high reliability with respect to thermomechanical stresses. As a result, the silver or copper sintered connection has a strong potential to significantly improve the product life.
[0044] However, silver or copper sintered connections offer significantly higher stiffness than soldered connections, which can lead to higher thermomechanical stresses not only in the sintered connection itself, but also in the mating connections and corresponding interface-bonded mating materials due to the mismatch in thermal expansion coefficients of mating materials such as silver at 18.9 ppm / K, copper at 16.4 ppm / K, silicon at 2.49 ppm / K, and aluminum at 24 ppm / K.
[0045] Thus, the interconnection connections between the electronic component 3, for example in the form of an electronic chip, the electrical connection 4, for example in the form of a clip, the connection between the substrate 2 and the connection between the substrate 2 and the base plate 1, can be subject to high thermomechanical stresses due to the different thermal expansion coefficients of silicon and copper. Furthermore, the relatively soft metallization layers, for example made of aluminum, used as contact metallization of the electronic component 3, should also be taken into account, which are not very suitable for high mechanical stresses. In the case of solder connections, this stress can be partially compensated for by the relatively soft solder material, but this limits the reliability of the solder connection itself.
[0046] In the case of the more robust silver or copper sintered connections, a clearly higher reliability of the bonded connection itself is achieved. By structuring the sintered connection layers 5A, 5B, 5C and / or 5D, potential weak points in the connection layers 5A, 5B, 5C and / or 5D can be improved and stresses reduced, so that the risk of peeling or other damage to the contact metallization, the connection layers or the bonded partners during long-term operation can be minimized.
[0047] 2A is a perspective view of a power module 10 according to one embodiment. The power module 10 comprises four module components: a base plate 1, a substrate 2, an electronic component 3, and an electrical connection 4. The power module 10 comprises one lower sintered connection layer 5A directly adjacent to the base plate 1 and the substrate 2. The base plate 1 is thereby mechanically connected to the substrate 2 via the lower sintered connection layer 5A.
[0048] The substrate 2 has a first metallization layer 21 and a second metallization layer 22, which is spatially and electrically separated from the first metallization layer 21 by an isolation trench 2T. The first and second metallization layers 21 and 22 are assigned to different electrical polarities / voltage potentials of the power module 10. The substrate 2 further comprises a rear metallization 23 and an insulating layer 20, which is arranged along the vertical direction between the rear metallization 23 and the first and second metallization layers 21 and 22. In the isolation trench 2T, the insulating layer 20 may be exposed. The first and second metallization layers 21 and 22 and the rear metallization may be made of the same material or of different materials. The substrate metallizations 21, 22, and / or 23 may be made of copper or aluminum, or corresponding alloys. Coating with a metal layer, such as nickel, gold, silver or other metals, is also possible. The insulating layer 20 may be a ceramic material such as Si3N4, AlN, Al2O3, or a resin that may contain inorganic fillers.
[0049] One first sintered connection layer 5B is disposed between the substrate 2 and the electronic component 3. Thus, the first sintered connection layer 5B can electrically and thermally connect the electronic component 3 to the first metallization layer 21. The electronic component 3 can be, but is not limited to, a semiconductor chip.
[0050] One second sintered connection layer 5C is formed between the electronic component 3 and the electrical connection 4. In Fig. 2A, the electrical connection 4 is a clip. One third sintered connection layer 5D is formed between the substrate 2 and the electrical connection 4.
[0051] In this disclosure, the terms "first," "second," "third," and "fourth" are intended to distinguish between similar parts, but do not necessarily indicate a particular sequence or order. For example, the lower sintered connection layer 5A may be assigned as the fourth sintered connection layer 5A. It is understood that these terms are interchangeable in appropriate circumstances.
[0052] According to the present disclosure, at least one, two, three or all of the connection layers 5A, 5B, 5C and 5D are patterned sintered connection layers. In Fig. 2A, only the sintered connection layers 5A, 5C and 5D are patterned. It is also possible to deviate from this and have exactly one or exactly three of the sintered connection layers 5A, 5B, 5C and 5D be patterned and the remaining connection layers not be patterned.
[0053] According to Fig. 2A, the second sintered connection layer 5C and the third sintered connection layer 5D are patterned and have a striped layout with a plurality of stripes. The stripes are oriented parallel to the separation trench 2T, i.e. perpendicular to the main extension direction of the clip, as shown in Fig. 2B, for example. Alternatively, it is also possible that the second sintered connection layer 5C and the third sintered connection layer 5D have a plurality of stripes oriented perpendicular to the separation trench 2T, i.e. parallel to the main extension direction of the clip, as shown in Fig. 2C.
[0054] 2B and 2C show top views of the patterned sintered connecting layer 5. Any of the patterned sintered connecting layers 5A, 5B, 5C and 5D can have a striped layout with multiple parallel stripes. In the case of the connecting layers 5C and 5D, the stripes can be oriented parallel or perpendicular to the separation trenches 2T. In the case of the connecting layers 5A and 5B, the separation trenches 2T are not present.
[0055] The stripes are formed by isolated sub-regions of the connection layer 5. These sub-regions partially cover the area 50 of the connection. In other words, these sub-regions correspond to sub-areas of the area 50A, 50B, 50C or 50D of the connection covered by the sintered material. In Fig. 2B and Fig. 2C, the sub-regions of the connection layer 5A, 5B, 5C or 5D have a lateral width W. The width W can be between 0.1 mm and 2.0 mm or more.
[0056] The area of connection 50 comprises sub-regions or sub-areas 50U that are not covered by sintered material. The sub-regions or sub-areas 50U are bounded by two opposite edges 50E of the corresponding area 50. The non-covered sub-regions or sub-areas 50U have a lateral width S. The width S can be greater than 0.1 mm, greater than 0.3 mm or greater than 0.5 mm. For example, the width S is equal to, less than or greater than the width W. According to Fig. 2B and Fig. 2C, the non-covered sub-regions or sub-areas 50U form a channel-like groove that extends laterally from one outer edge of the area of connection 50 across the inner sub-region to another opposite outer edge.
[0057] FIG. 3A shows a top view of a patterned sintered connection layer 5, which may be one of the connection layers 5A, 5B, 5C and 5D. Any of the patterned sintered connection layers 5A, 5B, 5C and 5D may have a so-called dot-like layout with a plurality of dots. In FIG. 3A, the sub-regions of the sintered connection layer 5 and the non-covered sub-regions 50U of the area of connection 50 have an irregular structure. The dots may have a circular, square, rectangular, hexagonal or other geometric shape. The dots may have equal or different geometric sizes. The diameter or side length of the dots may be 0.1 mm to 2.0 mm or more. The dots may be distributed uniformly or non-uniformly in the area of connection 50.
[0058] Further examples of discontinuous connecting layers 5, which can be any of connecting layers 5A, 5B, 5C, and 5D, are shown in Figure 3B. Such connecting layers can comprise multiple dots and multiple stripes.
[0059] Figures 3C, 3D, 3E and 3F show exemplary layouts of successive connecting layers 5A, 5B, 5C or 5D, which according to Figure 3C have a cross or fence-like shape, according to Figure 3D have a comb-like shape, according to Figure 3E have a zigzag or serpentine shape and according to Figure 3F have a star-shaped shape.
[0060] FIG. 4A shows the power module 10 of FIG. 2A without the base plate 1 and the connection layer 5A. FIG. 4B, FIG. 4C and FIG. 4D illustrate simulations obtained by "von Mises stress" showing the distribution of thermomechanical stresses in the module parts 2, 3 and 4 of the power module 10 in the presence of the unpatterned first connection layers 5B, 5C and 5D as shown in FIG. 4A. FIG. 4E, FIG. 4F, FIG. 4G, FIG. 5A, FIG. 5B, FIG. 5C, FIG. 6A, FIG. 6B and FIG. 6C illustrate several simulations showing the distribution of thermomechanical stresses in the module parts 2, 3 and 4 of the power module 10 in the presence of the unpatterned first connection layer 5B and the patterned sintered connection layers 5C and 5D as shown in FIG. 4A. The simulations were performed for half of the clip 4.
[0061] 4B shows the results of a simulation for the setup of a power module 10 with an electronic component 3 which is a chip, where the electronic component 3 is bonded to a first metallization layer 21 of a substrate 2. The second metallization layer 22 of the substrate and the chip surface are electrically interconnected by an electrical connection 4 which is a copper clip bonded on the surface of the second metallization layer 22 on the one hand and on the other hand bonded onto the upper contact of the electronic component 3 by silver sintering.
[0062] As shown in Fig. 4B, if the sintered connection layers 5B, 5C and 5D are not patterned, a large stress accumulation occurs not only on the chip and on the clip. Fig. 4C and Fig. 4D show local stress maxima on the edges of the sintered connection layers 5B and 5C. This large stress accumulation can lead to damage or peeling of the contact metallization, which is made, for example, of soft aluminum, and can also damage the sintered layers.
[0063] Figure 4C shows in a top view the calculated distribution of thermomechanical stresses on the side of the electronic component 3, i.e. the stress distribution at the interface between the sintered connection layer 5C and the clip 4. Figure 4D shows in a top view the calculated distribution of thermomechanical stresses on the side of the substrate 2, here at the interface between the sintered connection layer 5D and the clip 4.
[0064] As shown in Fig. 4B, large stresses occur not only in the sintered connection but also in the bonded partner. Improvement of the mechanical strength of the setup can be obtained by the use of harder and / or stronger contact metallization of the chip or the need for stress reduction of the bonded connection resulting in improved reliability against thermal cycling. Stress reduction of the sintered bonded connection has been found to be very effective in terms of improving the reliability of the power module against thermal cycling.
[0065] Stress reduction is achieved by patterned sintered connections. While the bonded connections of the copper clips interconnecting the chip and substrate surfaces shown in Figures 4B-4D were prepared by a homogenous layer of sintered silver, the present disclosure proposes patterning such a homogenous layer, where the area of the connection is not completely covered by the sintered material such as silver.
[0066] As shown in Fig. 4A, the connection layers 5C and 5D comprise a number of stripes of sintered silver interrupted by a number of spaces, which are sub-regions 5CU and 5DU of the connection areas 50C and 50D, respectively, that are not covered by sintered material and are bounded by one or several outer edges 5CE or 5DE of the connection areas 50C or 50D (see also Fig. 2B or 2C).
[0067] Figure 4E shows the results of a finite element (FEM) simulation with the setup shown in Figure 4A. Except for the patterned structure of the sintered connection layers 5C and 5D, the setup is identical to the setup used for the stress simulation shown in Figure 4B. Here, a striped layout according to Figure 2B is used, with the stripes parallel to the trenches 2T or perpendicular to the main direction of the clip.
[0068] The patterned connection layer 5C or 5D comprises three stripes of sintered material with a width of 500 μm, which are separated by non-covered sub-areas 5CU or 5DU forming gaps or spaces with a width of 200 μm. The stripes have their length direction perpendicular to the main orientation of the clips, i.e. the electrical connections 4, or parallel to the separating trenches 2T. The results show a significant reduction of stresses in the sintered bonded connections of the patterned structures compared to homogeneous sintered layers, i.e. about three times less. Here, the stresses in both bonding partners and in the sintered layer are also significantly reduced. This can be expected to significantly improve the reliability of the power module 10 against thermal cycles.
[0069] Similar to Figures 4C and 4D, Figure 4F shows the calculated distribution of thermomechanical stresses on the interface between sintered connection layer 5C and clip 4 in a top view, and Figure 4G shows the calculated distribution of thermomechanical stresses on the interface between sintered connection layer 5D and clip 4 in a top view.
[0070] 5A, 5B and 5C essentially correspond to 4E, 4F and 4G, respectively. In contrast, according to 5A, 5B and 5C, the sintered connection layers 5C and 5D are prepared with stripes oriented parallel to the main extension direction of the clip, i.e. the main extension direction of the electrical connection 4, or orthogonal to the main extension direction of the separation trench 2T. Moreover, the different stripes have different widths. This layout results in a different distribution of thermomechanical stresses in the sintered connection layers 5C and 5D, compared to the use of a homogeneous sintered connection layer. Here, the local stress maxima at the edges of the clip are stronger compared to the homogeneous case, while the stresses in the center of the sintered connection are reduced. It is, however, assumed that the stresses that occur are concentrated, but also limited to a relatively small area of the stripes.
[0071] Figures 6A, 6B, and 6C essentially correspond to Figures 5A, 5B, and 5C, or Figures 4E to 4G, respectively. In contrast, according to Figures 6A, 6B, and 6C, the patterned sintered connection layers 5C and 5D are prepared by dots, i.e., are dot-shaped (see also Figure 3A for an example).
[0072] In Figures 4E-5C, the non-covered sub-regions 5CU or 5DU are separated from each other and in each case form channel-like grooves extending laterally from one outer edge of the area of connection 50C or 50D to another opposite outer edge. In contrast, in Figures 6A, 6B and 6C, the non-covered sub-regions 5CU or 5DU form channel-like grooves and form a connected network, i.e. they are continuous. The connected network channel-like grooves are adjacent to all outer edges 5CE and 5DE of the respective area of connection 50C or 50D (see also Figures 3A and 3B).
[0073] Compared to Figures 5A, 5B and 5C, according to the setup described in Figures 6A, 6B and 6C, even less sintering material is required, since it is only present in the areas of dots or dot-like structures separated from each other by horizontal and vertical gaps. Figure 6A shows the results of a finite element simulation for a clip, where the sintering connection is prepared as an area of several dots. This layout also results in an overall stress reduction compared to the use of a homogeneous sintering layer. The local stress maxima at the edges of the clip are stronger compared to the homogeneous case, but the stresses in the center of the sintering connection are reduced. However, the stresses that occur are considered to be concentrated in the relatively small area of the dots.
[0074] A striped layout with stripe orientation as shown in Figure 4E appears to be most suitable for the bonding connection of clips. Nevertheless, alternative layouts such as dot patterns or striped layouts with other orientations are also well suited for the bonding connection of terminals or other types of planar contacts on the surface of a chip or substrate. Here, layouts are possible in which the homogeneous sintered layer is only partially interrupted by grooves, as occurs, for example, in star or cross shapes or other shapes shown, for example, in Figures 3A-3F.
[0075] Moreover, further improvements of the exfoliated layout can be achieved by selecting an appropriate width and / or distance of the stripes. FIG. 7A shows a 2D simulation of the stress distribution referring to a cross section of a clip 4 sintered to a substrate 2. FIG. 7B shows the stress distribution along the inner line of the sintered layer (dashed line in FIG. 7A). The patterned sintered connection layer has a striped layout with stripes parallel to the separation trenches 2T or perpendicular to the main orientation of the clips 4, where on the one hand a stripe width W=W1 and a gap width S of 100 μm were selected, and on the other hand a stripe width W=W2 and a gap width S of 200 μm were selected. In FIG. 7B the distribution of the thermomechanical stress T in a non-patterned homogeneous connection layer, thus a single "stripe" with a maximum width W=W0, is also shown for comparison.
[0076] The stress curve shown in FIG. 7B is determined in a two-dimensional simulation at the center of the sintered connection layer 5D, ie along the dashed line in FIG. 7A.
[0077] For example, FIG. 7A shows the stress distribution on the substrate side. FIG. 7B also shows the distribution of stress on the substrate side, i.e. in the connection layer 5D between the clip 4 and the substrate 2, as a function of D, the distance from the edge of the stripe. It was found that for smaller stripe widths W=W1 and distances, a stronger stress reduction is achieved. The results show that a smaller stripe width of 100 μm leads to an even greater stress reduction compared to a stripe width and distance of 200 μm. Thus, the use of smaller stripes is advantageous with regard to the reduction of thermomechanical stresses in the patterned sintered connection.
[0078] Similar patterned sintered connection layers 5B and 5A may be applied to the bonding connection between the substrate 2 and the electronic component 3, and the bonding connection between the substrate 2 and the base plate 1, respectively. For these bonding connections as well, it is expected that the reliability of the connection layers 5A, 5B or the power module 10 against thermomechanical stress will be improved.
[0079] Further aspects of the disclosure are provided below, and the numbering used below is intended to facilitate reference to features of the other aspects.
[0080] Aspect 1: A power module comprising at least two module components and at least one connection layer, the at least one connection layer being formed along the vertical direction between the at least two module components to mechanically connect the at least two module components. The at least one connection layer is a sintered connection layer that forms a sintered connection between the at least two module components. The at least one connection layer is patterned such that, in a top view, the area of the sintered connection is only partially covered by the sintered material, and the subregions of the area that are not covered by the sintered material are bounded by one or several outer edges of the area. The ratio of the surface of the uncovered subregion to the respective area of the sintered connection is ≧10% and ≦75%.
[0081] Aspect 2: A power module as described in aspect 1, wherein the uncovered subregions of the area form channel-like grooves extending laterally from an inner subregion of the area towards one or more outer edges of the area.
[0082] Aspect 3: A power module according to any one of the preceding aspects, wherein at least some or all of the non-covered sub-regions of the area are empty spaces filled with air, or with an insulating material, or with a conductive material different from the sintered material.
[0083] Aspect 4: A power module according to any one of the preceding aspects, wherein at least one connection layer is continuous.
[0084] Aspect 5: A power module according to the preceding aspect, wherein at least one connecting layer has a comb-shaped, cross-shaped, star-shaped, zigzag-shaped or serpentine-shaped shape.
[0085] Aspect 6: The power module of any one of Aspects 1 to 3, wherein at least one connection layer is discontinuous.
[0086] Aspect 7: A power module according to the preceding aspect, wherein at least one connection layer comprises spatially separated sub-regions forming a striped or dotted pattern.
[0087] Embodiment 8: A power module according to any one of the preceding embodiments, wherein the at least two module components are elements from the group including a base plate, a substrate, an electronic component, and an electrical connection.
[0088] Aspect 9: A power module according to any one of the preceding aspects, comprising at least three module components, which are a substrate, an electronic component, and an electrical connection, the substrate having a first metallization layer and a second metallization layer spatially separated from the first metallization layer by an isolation trench. The electronic component is a semiconductor chip electrically and thermally connected to the first metallization layer by one connection layer in the form of the first connection layer. The electrical connection is a metal clip or a planar contact or terminal electrically connected to the electronic component by one connection layer in the form of the second connection layer. At least one or both of the connection layers are patterned sintered connection layers.
[0089] Aspect 10: The power module according to aspect 9, wherein the electrical connection is a metal clip and is electrically connected to the second metallization layer by one connection layer in the form of a third connection layer. At least one of the second connection layer and the third sintered connection layer is a patterned sintered connection layer.
[0090] Aspect 11: A power module as described in aspect 10, wherein at least one of the second connection layer and the third sintered connection layer has a striped layout including multiple stripes, the stripes being oriented parallel or perpendicular to the separation trenches.
[0091] Aspect 12: A power module according to any one of the preceding aspects, comprising at least four module parts, which are a base plate, a substrate, an electronic component and an electrical connection, and one connection layer in the form of a lower sintered connection layer is formed between the base plate and the substrate. One connection layer in the form of a first connection layer is formed between the substrate and the electronic component. One connection layer in the form of a second connection layer is formed between the electronic component and the electrical connection. At least one, two or all of the connection layers are patterned sintered connection layers.
[0092] Aspect 13: A power module according to any one of the preceding aspects, wherein at least one connection layer is a sintered connection layer of silver or copper.
[0093] Aspect 14: A power module according to any one of the preceding aspects, wherein the uncovered subregion has a lateral width (W) greater than 0.1 mm.
[0094] Aspect 15: A method for manufacturing a power module described in any one of the preceding aspects, comprising applying a sintering material onto one or more surfaces of one or both of at least two module components to form at least one sintered connecting layer, and applying a predetermined pressure during the formation of the at least one sintered connecting layer to adjust the porosity or density of the at least one connecting layer.
[0095] The embodiments shown in the above figures represent exemplary embodiments of the improved configuration of the power module, and therefore do not constitute an exhaustive list of all embodiments according to the improved configuration of the power module. The actual arrangement of the power module may differ from the exemplary embodiments described above.
[0096] This application claims priority from European Patent Application No. 21 183 737.2, the disclosure of which is incorporated herein by reference. [Explanation of symbols]
[0097] Reference sign 10 Power Module M module parts 1 module part, base plate 2 Module components, boards 20 Insulating layer 21 First Metallization Layer 22 Second Metallization Layer 23 Rear Metallization 2T Isolation Trench 3. Module components, electronic components 4 Module components, electrical connections 5. Connection Layer 5A Lower / 4th connection layer, the connection layer between the base plate and the substrate 5B First connection layer, connection layer between substrate and electronic component 5C Second connection layer, connection layer between electronic components and electrical connections 5D third connection layer, a connection layer between the electrical connection and the substrate W, W0, W1, W2 Widths of the sub-regions of the connection layer 50 Connection Areas 50A Area of connection between base plate and board 50B Area of connection between board and electronic component 50C Area of connection between electronic components and electrical connections 50D The area of the connection between the board and the electrical connection Uncovered sub-area of area 50 with 50U connection Uncovered sub-area of area 50A with 5AU connection 5BU Uncovered sub-area of area 50B with connection Uncovered sub-area of area 50C with 5CU connection Uncoated sub-area of area 50D with 5DU connection S is the width of the channel-like groove formed by the subregion of the uncovered subregion 50E Outer edge of Area 50 Outer edge of area 50A of 5AE connection Outer edge of area 50B of 5BE connection Outer edge of area 50C of 5CE connection Outer edge of area 50D of 5DE connection
Claims
1. A power module (10) comprising at least three module components (M) which are substrates (2), an electronic component (3) and an electrical connection (4), further comprising at least a first connection layer (5, 5B) and a second connection layer (5, 5C), said substrate (2) comprises a first metallization layer (21) and a second metallization layer (22) spatially separated from said first metallization layer (21) by an isolation trench (2T); the first connection layer (5, 5B) is formed vertically between the substrate (2) and the electronic component (3) for mechanically connecting the electronic component (3) to the substrate (2), the electronic component (3) being a semiconductor chip electrically and thermally connected to the first metallization layer (21) by the first connection layer (5, 5B); said first connection layer (5, 5B) is a sintered connection layer which forms a sintered connection between said substrate (2) and said electronic component (3); said first connection layer (5, 5B) is patterned, in a top view, such that the areas (50) of the sintered connections are only partially covered by sintering material and that the sub-areas (50U) of said areas (50) that are not covered by sintering material are bounded by one or several outer edges (50E) of said areas (50), the ratio of the surface of said non-covered sub-areas (50U) to said respective areas (50) of the sintered connections being between 10% and 75%, - said electrical connection (4) is electrically connected to said electronic component (3) by said second connection layer (5C), said second connection layer (5, 5C) being another patterned sintered connection layer; A power module (10).
2. 2. The power module (10) of claim 1, wherein the non-covered sub-regions (50U) of the area (50) form channel-like grooves extending laterally from an inner sub-region of the area (50) towards one or several outer edges (50E) of the area (50).
3. 10. The power module (10) according to any one of the preceding claims, wherein at least some or all of the non-covered sub-areas (50U) of the area (50) are empty spaces filled with air, or with an insulating material, or with a conductive material different from the sintered material.
4. 10. A power module (10) according to any one of the preceding claims, wherein the first or second connection layer (5, 5B, 5C) is continuous.
5. 10. The power module (10) according to the preceding claim, wherein the first or second connection layer (5, 5B, 5C) has a comb, cross, star, zigzag or serpentine shape.
6. The power module (10) according to any one of claims 1 to 3, wherein the first or second connection layer (5, 5B, 5C) is discontinuous.
7. 10. A power module (10) according to the preceding claim, wherein the first or second connection layer (5, 5B, 5C) comprises spatially separated sub-regions forming a striped or dotted pattern.
8. 10. The power module (10) according to any one of the preceding claims, wherein the electrical connections (4) are metal clips or flat contacts or terminals electrically connected to the electronic components (3) by means of the second connection layer (5C).
9. - said electrical connection (4) is a metal clip, electrically connected to said second metallization layer (22) by a third connection layer (5, 5D); - said third sintered connection layer (5D) is a patterned sintered connection layer; A power module (10) according to claim 8.
10. 10. The power module (10) of claim 9, wherein at least one of the second connection layer (5C) and the third sintered connection layer (5D) has a striped layout comprising a plurality of stripes, the stripes being oriented parallel to the separation trenches (2T).
11. 10. The power module (10) of claim 9, wherein at least one of the second connection layer (5C) and the third sintered connection layer (5D) has a striped layout comprising a plurality of stripes, the stripes being oriented perpendicular to the separation trenches (2T).
12. The device comprises at least four module components, which are a base plate (1), the substrate (2), the electronic components (3) and the electrical connections (4), - one further connection layer (5) in the form of a lower sintered connection layer (5A) is formed between said base plate (1) and said substrate (2), - said lower connection layer (5, 5A) is another patterned sintered connection layer, A power module (10) according to any one of the preceding claims.
13. 10. Power module (10) according to any one of the preceding claims, wherein the first or second connection layer (5, 5B, 5C) is a sintered connection layer of silver or copper.
14. 10. The power module (10) according to any one of the preceding claims, wherein the non-covered sub-area (50U) has a lateral width (W) greater than 0.1 mm.
15. A method for manufacturing a power module (10) according to any one of the preceding claims, comprising the steps of: - applying a sintering material onto one or more surfaces of one or both of said substrate (2) and said electronic component (3) to form said first sintered connection layer (5, 5B); - applying a pressure during the formation of the first sintered connection layer (5, 5B) in order to adjust the porosity or density of the first connection layer (5, 5B); A method comprising: