Semiconductor Device
The semiconductor device with a silicon carbide epitaxial layer and junction Schottky barrier diode structure addresses the high source-drain voltage drop in MOSFETs by reducing VFSD and Rds(on), improving reliability and maintaining chip area efficiency.
Patent Information
- Application Number
- JP2024003016U
- Authority / Receiving Office
- JP · JP
- Patent Type
- Utility models
- Current Assignee / Owner
- Priority Date
- 2023-09-27
- Filing Date
- 2024-09-06
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2034-09-06
AI Technical Summary
The source-drain forward voltage drop (VFSD) in metal oxide field effect transistors (MOSFETs) is higher than that of junction Schottky barrier diodes, and this issue is exacerbated when the gate-source voltage changes from 0V to -5V, necessitating the development of new semiconductor devices.
The semiconductor device incorporates a silicon carbide epitaxial layer with a junction Schottky barrier diode structure comprising a first metal layer, a barrier layer, and a heavily doped p-type region, which reduces the source-drain forward voltage drop and drain-source on-resistance by forming a recess in the silicon carbide epitaxial layer and using a barrier layer on its surfaces.
The solution effectively reduces the source-drain forward voltage drop and drain-source on-resistance, enhancing device reliability while maintaining a compact chip area without increasing the overall size.
Smart Images

Figure 0003249108000001_ABST
Abstract
Description
[Technical field]
[0001] This utility model relates to a semiconductor device, and in particular to a power MOSFET (MOSFET field effect transistor). [Background technology]
[0002] Usually, the source-drain forward voltage drop (VFSD) of a metal oxide field effect transistor (MOSFET) is higher than the forward voltage drop of a junction Schottky barrier diode. In a metal oxide field effect transistor, when the gate-source voltage goes from 0V to -5V, the source-drain forward voltage drop becomes high. To overcome these problems, a new semiconductor device is required. Summary of the Invention
[0003] In view of the above, the semiconductor device of the present invention includes a silicon carbide epitaxy layer, a gate electrode oxide layer, a polysilicon layer, an interlayer dielectric layer, a recess, a barrier layer, and a first metal layer, the silicon carbide epitaxy layer having a junction field effect region in the gate electrode region, a p-type well region contacting the junction field effect region, a first heavily doped p-type region in the p-type well region, and a second heavily doped p-type region outside the p-type well region. the gate anodization layer is on the silicon carbide epitaxy layer, the polysilicon layer is on the gate anodization layer, the interlevel dielectric layer is on the polysilicon layer, the recess is formed in the silicon carbide epitaxy layer through the interlevel dielectric layer, the polysilicon layer and the gate anodization layer in a source pole region, the barrier layer is on lower and side surfaces of the recess and on the second heavily doped p-type region, and the first metal layer is on the barrier layer. In summary, the junction Schottky barrier diode (composed of the first metal layer, the barrier layer and the second heavily doped p-type region) in the semiconductor device can reduce the source-drain forward voltage drop VFSD and the drain-source on-resistance Rds(on) of a metal oxide field effect transistor, overcome the technical problem of a high source-drain forward voltage drop VFSD when the gate-source voltage goes from 0V to -5V, and improve the reliability of the device. [Brief description of the drawings]
[0004] [Figure 1] 1 is a cross-sectional view of a semiconductor device 100 according to the present invention. [Diagram 2] 4 is a flowchart of a method for manufacturing a semiconductor device in the present utility model. [Diagram 3] 2 is another cross-sectional view of the semiconductor device 100. FIG. [Figure 4] 2 is another cross-sectional view of the semiconductor device 100. FIG. [Diagram 5] 2 is another cross-sectional view of the semiconductor device 100. FIG. [Figure 6] 2 is another cross-sectional view of the semiconductor device 100. FIG. [Figure 7] 2 is another cross-sectional view of the semiconductor device 100. FIG. [Figure 8] 2 is another cross-sectional view of the semiconductor device 100. FIG. [Figure 9] 2 is another cross-sectional view of the semiconductor device 100. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0005] FIG. 1 is a cross-sectional view of a semiconductor device 100 in the present invention. As shown in FIG. 1, the semiconductor device 100 has a unit cell region UC, a junction Schottky barrier diode region JBS outside the unit cell region UC, and a guard ring region GR. In detail, the semiconductor device 100 has a silicon carbide epitaxy layer 101, a gate anodization layer 102, a polysilicon layer 103, an interlayer dielectric layer 104, a contact spacer 105, a metal layer 110, a barrier layer 116, a field oxide layer FOX, a passivation layer 114, and a polyimide layer 115. The silicon carbide epitaxy layer 101 also has a p-type well region 106, a heavily doped n region 107, a silicide SC, a junction field effect region JF, and a heavily doped p region PP. The heavily doped p regions PP include a heavily doped p region PP1 in the unit cell region UC, a heavily doped p region PP2 in the junction Schottky barrier diode region JBS, and a heavily doped p region PP3 in the guard ring region GR. The heavily doped p regions PP1, PP2, PP3 and other heavily doped p regions PP can be completed in the same process.
[0006] Specifically, within unit cell region UC in silicon carbide epitaxy layer 101, junction field effect region JF is in the gate pole region, p-type well region 106 is between and in contact with two junction field effect regions JF, heavily doped p region PP1 is below heavily doped n region 107 and in p-type well region 106, heavily doped n region 107 is at the surface of p-type well region 106 and partially overlaps heavily doped p region PP1, the depth of heavily doped p region PP1 is greater than the depth of heavily doped n region 107. Gate anodization layer 102 is on silicon carbide epitaxy layer 101, and gate anodization layer 102 overlaps a portion of heavily doped n region 107 and a portion of p-type well region 106. A polysilicon layer 103 overlies the gate electrode layer 102, and the polysilicon layer 103 is formed as the gate electrode of the transistor. An interlevel dielectric layer 104 overlies the polysilicon layer 103, and a contact spacer 105 overlies the heavily doped n-type region 107 and contacts the gate electrode layer 102, the polysilicon layer 103, and the interlevel dielectric layer 104.
[0007] The semiconductor device 100 further includes a recess 109. A first recess 109 is formed in the silicon carbide epitaxial layer 101 at the source pole region CTS, penetrating the interlevel dielectric layer 102, the polysilicon layer 103 and the gate pole oxide layer 104. A barrier layer 116 is formed on the lower and side surfaces of the recess 109, so that the barrier layer 116 contacts the interlevel dielectric layer 104 and the contact spacer 105, and also contacts the heavily doped n-type region 107 and the heavily doped p-type region PP1 through silicide SC. Note that a metal layer 110 is formed on the barrier layer 116, and the metal layer 110 is used to form the source pole contact and the gate pole contact. The metal layer 110 is in the first recess 109, and contacts the barrier layer 116, the heavily doped p-type region PP1 and the heavily doped n-type region 107 through silicide SC. Metal layer 110 contacts polysilicon layer 103 in the gate pole region (not shown). Barrier layer 116 can be a stack of titanium (Ti) and titanium nitride (TiN). In some embodiments, an optional field oxide layer FOX can be provided on silicon carbide epitaxy layer 101 in unit cell region UC.
[0008] Within the junction Schottky barrier diode region JBS in the silicon carbide epitaxy layer 101, the heavily doped p-type region PP2 is outside the p-type well region 106 and directly contacts the silicon carbide epitaxy layer 101. The barrier layer 116 is on the silicon carbide epitaxy layer 101 and on the heavily doped p-type region PP2. Thus, the barrier layer 116 contacts the silicon carbide epitaxy layer 101 and the heavily doped p-type region PP2, and the metal layer 110 contacts the heavily doped p-type region PP2 through the barrier layer 116. In some embodiments, there is a silicide SC between the barrier layer 116 and the heavily doped p-type region PP2. The metal layer 110, the barrier layer 116, and the second heavily doped p-type region PP2 form a junction Schottky barrier diode. In some embodiments, an optional field oxide layer FOX may be provided on the silicon carbide epitaxial layer 101 in the junction Schottky barrier diode region JBS.
[0009] Within the guard ring region GR in the silicon carbide epitaxy layer 101, the heavily doped p-type region PP3 is directly in contact with the silicon carbide epitaxy layer 101, and a field oxide layer FOX is provided on and in contact with the silicon carbide epitaxy layer 101. A passivation layer 114 may be provided on the metal layer 110 and the field oxide layer FOX, and a polyimide layer 115 may be provided on the passivation layer 114.
[0010] In addition, on the backside of the silicon carbide epitaxial layer 101, the semiconductor device 100 has a silicon carbide substrate (not shown) below the silicon carbide epitaxial layer 101 and a metal layer (not shown) below the silicon carbide substrate. The metal layer below the silicon carbide substrate is used to form a drain electrode contact, and the composition of the metal layer 110 and the metal layer below the silicon carbide substrate includes, but is not limited to, Ni, Ti, TiN, AlCu, etc. In a preferred embodiment of the present invention, the metal layer 110 is an aluminum copper alloy.
[0011] Fig. 2 is a flow chart of the method for manufacturing a semiconductor device in the present utility model, and Figs. 3 to 9 are cross-sectional views of a semiconductor device 100 for explaining steps S1 to S8 of the method for manufacturing a semiconductor device. First, in step S1, as shown in Fig. 3, a silicon carbide epitaxy layer 101 is provided, which includes a p-type well region 106, a heavily doped n-type region 107, a junction field effect region JF, and a heavily doped p-type region PP. The heavily doped p-type region PP further includes a heavily doped p-type region PP1 used in the unit cell region UC, a heavily doped p-type region PP2 used in the junction Schottky barrier diode region JBS, and a heavily doped p-type region PP3 used in the guard ring region GR.
[0012] In step S2, a field oxide layer FOX is formed. In detail, the field oxide layer FOX is deposited on the silicon carbide epitaxial layer 101, and the photomask pattern of the field oxide layer FOX is transferred to the field oxide layer FOX, and then the field oxide layer FOX is wet-etched. As shown in FIG. 4, by retaining the field oxide layer FOX in the guard ring region GR and the junction Schottky barrier diode region JBS, damage caused by the subsequent etching process to the silicon carbide epitaxial layer 101 and the elements therein can be avoided.
[0013] In step S3, a gate electrode oxide layer 102, a polysilicon layer 103, and an interlayer dielectric layer 104 are formed. In detail, as shown in Fig. 5, the gate electrode oxide layer 102, the polysilicon layer 103, and the interlayer dielectric layer 104 are deposited in this order, and a photomask pattern of the polysilicon layer 103 is transferred, and the interlayer dielectric layer 104, the polysilicon layer 103, and the gate electrode oxide layer 102 are dry etched.
[0014] In step S4, a recess 109 is formed in the unit cell region UC. In particular, as shown in FIG. 6, a contact spacer 105 is deposited, the contact spacer 105 is etched back, and a blanket etch of silicon carbide is performed to make the depth of the recess 109 greater than the depth of the heavily doped n-type region 107.
[0015] In step S5, a recess 111 is formed in the junction Schottky barrier diode region JBS. In detail, as shown in FIG. 7, a photomask pattern of silicide of the junction Schottky barrier diode region JBS is transferred, and the junction Schottky barrier diode region JBS is etched.
[0016] In step S6, as shown in FIG. 8, silicide is formed in the recess 109 in the unit cell region UC and in the recess 111 in the junction Schottky barrier diode region JBS.
[0017] In step S7, the field oxide layer FOX in the junction Schottky barrier diode region JBS is patterned. In detail, as shown in Fig. 9, a photomask pattern of the contact of the junction Schottky barrier diode region JBS is transferred, and the junction Schottky barrier diode region JBS is wet-etched.
[0018] 1, a barrier layer 116, a metal layer 110, a passivation layer 114, and a polyimide layer 115 are formed. In detail, the barrier layer 116 and the metal layer 110 are deposited in this order, a photomask pattern of the metal layer 110 is transferred, and the metal layer 110 is etched. The passivation layer 114 is deposited, a photomask pattern of the passivation layer 114 is transferred, and the passivation layer 114 is etched. The polyimide layer 115 is deposited, a photomask pattern of the polyimide layer 115 is transferred, and the polyimide layer 115 is etched.
[0019] To sum up, the above configuration and method can reduce the source-drain forward voltage drop VFSD and drain-source on-resistance Rds(on) of a metal oxide field effect transistor, overcome the technical problem of high source-drain forward voltage drop when the gate-source voltage changes from 0 V to -5 V, and increase the reliability of the device. In addition, this configuration reduces the area of the unit element by the source pole self-alignment process, so there is no increase in the chip area due to an increase in the junction Schottky barrier diode region JBS.
[0020] As above, the features of some embodiments have been outlined so that those skilled in the art can better understand the present specification. It is understood by those skilled in the art that other processes and structures can be designed or modified based on the contents presented in the present application to achieve the same purpose and / or the same advantages as those in the above application. It is also understood by those skilled in the art that equivalent structures that do not depart from the spirit and scope of the present application can be modified, substituted, and altered in various ways without departing from the spirit and scope of the present application. [Explanation of symbols]
[0021] 100: Semiconductor device 101: Silicon carbide epitaxy layer 102: Gate anodization layer 103: Polysilicon layer 104: Interlayer dielectric layer 105: Contact spacer 106: p-type well region 107: Heavily doped n region 109: Dent 110: Metal layer 111: Dent 114: Passivation layer 115: Polyimide layer 116: Barrier layer SC: Silicide JF: Junction field effect region PP, PP1, PP2, PP3: heavily doped p-type regions UC: Unit cell domain JBS: Junction Schottky Barrier Diode Region GR: Protection Ring Region FOX: Field oxide layer S1, S2, S3, S4, S5, S6, S7, S8: Step
Claims
1. a junction field effect region within the gate electrode region; a p-type well region in contact with the junction field effect region; a first heavily doped p-type region within the p-type well region; a second heavily doped p-type region outside the p-type well region; and a gate anodization layer overlying the silicon carbide epitaxial layer; a polysilicon layer overlying the gate oxide layer; an interlevel dielectric layer overlying the polysilicon layer; a recess formed in the silicon carbide epitaxy layer through the interlevel dielectric layer, the polysilicon layer and the gate oxide layer in a source pole region; a barrier layer overlying a lower surface and a side surface of the recess and overlying the second heavily doped p-type region; a first metal layer overlying the barrier layer.
2. 2. The semiconductor device of claim 1 , wherein the silicon carbide epitaxial layer further comprises: a heavily doped n-type region overlying a surface of the p-type well region; the heavily doped p-type region underlies the heavily doped n-type region; The depth of the recess is greater than the depth of the heavily doped n-type region.
3. The semiconductor device according to claim 2, further comprising: A contact spacer overlies a surface of the heavily doped n-type region and contacts the gate oxide layer, the polysilicon layer and the interlevel dielectric layer.
4. 4. The semiconductor device of claim 3, wherein said first metal layer is in said recess and contacts said barrier layer, said first heavily doped p-type region and said heavily doped n-type region through silicide.
5. 4. The semiconductor device as recited in claim 3, wherein said barrier layer contacts said interlevel dielectric layer, said contact spacer and said silicon carbide epitaxy layer.
6. 2. The semiconductor device of claim 1, wherein there is a silicide between said barrier layer and said second heavily doped p-type region.
7. 2. The semiconductor device according to claim 1, further comprising: A silicon carbide substrate is provided below the silicon carbide epitaxial layer.
8. The semiconductor device according to claim 7, further comprising: A second metal layer underlying the silicon carbide substrate.
9. 2. The semiconductor device as recited in claim 1, wherein said first metal layer, said barrier layer and said second heavily doped p-type region form a junction Schottky barrier diode.
10. 2. The semiconductor device according to claim 1, wherein the first metal layer is an aluminum-copper alloy, and the barrier layer is a laminate of titanium and titanium nitride.