Manufacturing method and drilling device for liquid transport pipe

The integrated perforation process during extrusion and winding of liquid transport pipes addresses inefficiencies in existing methods by enhancing production efficiency, hole consistency, and surface quality, ensuring mechanical and chemical resistance.

JP7553392B2Active Publication Date: 2024-09-18C I TAKIRONCIVIL CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2021056866
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-30
Publication Date
2024-09-18
Estimated Expiration
2041-03-30

AI Technical Summary

Technical Problem

The existing methods for manufacturing perforated liquid transport pipes require a separate drilling process after molding, which reduces production efficiency and introduces inefficiencies.

Method used

A method and device for manufacturing liquid transport pipes that integrate a perforation process during the extrusion and winding of molten thermoplastic resin around a core material, forming through holes in the thickness direction and supporting the resin to control hole dimensions and shape, allowing for efficient production of pipes with through holes on their circumferential surfaces.

Benefits of technology

This approach improves production efficiency by eliminating the need for post-molding drilling, ensures consistent hole shape and size, reduces burrs, and enhances the smoothness and durability of the inner surface, while maintaining mechanical and chemical resistance properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007553392000001
    Figure 0007553392000001
  • Figure 0007553392000006
    Figure 0007553392000006
  • Figure 0007553392000007
    Figure 0007553392000007
Patent Text Reader

Abstract

To provide a method of manufacturing a liquid transport pipe that has a through hole on a peripheral surface, and can improve production efficiency, and a punching device.SOLUTION: There is provided a method for manufacturing a liquid transport pipe in which a liquid transport pipe is molded from a molten resin 20 that is a thermoplastic resin in a molten state, comprising: an extrusion step of extruding the molten resin 20 into a band shape; a punching step of forming a through hole 20a that penetrates the band-shaped molten resin 20 in a thickness direction; and a winding step of spirally winding the band-shaped molten resin 20 having the through hole 20a formed around an outer peripheral surface of a core material 14a so that the through hole 20a communicates with an inside and outside of the liquid transport pipe.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a manufacturing method and a drilling device for a liquid transport pipe. [Background technology]

[0002] A known method for manufacturing a liquid transport pipe made of thermoplastic resin is to extrude molten thermoplastic resin, then wrap the resin in a spiral shape around the outer circumference of a core material and solidify the resin to form the thermoplastic resin into a tubular shape (see, for example, Patent Document 1).

[0003] As an example of a liquid transport pipe, a perforated pipe having through holes formed in a peripheral surface of the liquid transport pipe is known. The perforated pipe is used, for example, as a drainage pipe buried in a landfill at a waste disposal site. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2020-133742 A Summary of the Invention [Problem to be solved by the invention]

[0005] The through holes in the perforated pipe are formed in a factory, etc., by an operator using a tool such as a drill to drill holes in the peripheral surface of the molded liquid transport pipe. Further improvement in production efficiency is also desired in the manufacturing method of the perforated pipe. [Means for solving the problem]

[0006] A manufacturing method for a liquid transport tube to solve the above problem is a manufacturing method for a liquid transport tube in which a liquid transport tube is formed from molten resin, which is a thermoplastic resin in a molten state, and includes an extrusion process in which the molten resin is extruded in a strip shape, a drilling process in which through holes are formed through the strip of molten resin in the thickness direction, and a winding process in which the strip of molten resin with the through holes formed therein is spirally wound around the outer peripheral surface of a core material so that the through holes connect the inside and outside of the liquid transport tube.

[0007] According to the above manufacturing method, by performing the drilling process in the limited period between the process of extruding the molten resin and the process of winding the molten resin around a core material, the drilling work that was previously performed after molding can be reduced, thereby improving the production efficiency of liquid transport pipes having through holes on their peripheral surface.

[0008] In the above-mentioned method for manufacturing a liquid transport tube, it is preferable that the through hole in the perforation step has a dimension in the extension direction of the molten resin smaller than a dimension in the width direction of the molten resin perpendicular to the extension direction. According to the above-mentioned manufacturing method, in the winding step, tension in the winding direction, which is the direction in which the molten resin is wound and along the extension direction of the molten resin, acts on the molten resin, so that the through hole provided in the molten resin is stretched in the winding direction. Therefore, since the dimension of the through hole formed in the perforation step in the extension direction of the molten resin is smaller than the dimension in the width direction of the molten resin, the shape of the opening of the through hole in the liquid transport tube can be made closer to a perfect circle by the tension in the winding direction acting on the molten resin in the winding step.

[0009] In the above-mentioned method for manufacturing a liquid transport pipe, it is preferable that in the perforation step, the molten resin is supported on a receiving stand while the molten resin is punched in the thickness direction by a perforation pin, thereby forming the through hole in the molten resin. According to the above-mentioned manufacturing method, the receiving stand supports the molten resin when the perforation pin forms the through hole in the molten resin. This allows the punching load of the perforation pin to be suitably applied to the molten resin, which is in a state where it is easily deformed.

[0010] In the above-mentioned method for manufacturing a liquid transport pipe, in the perforation step, it is preferable that the perforation pin and the receiving base move following the movement of the molten resin transported toward the core material, and the perforation pin punches the molten resin while moving following the molten resin. According to the above-mentioned manufacturing method, the perforation pin punches the molten resin while moving following the transported molten resin, thereby preventing the molten resin transported from upstream from being blocked by the perforation pin. Therefore, it is easier to control the shape of the through hole than when the perforation pin is simply driven perpendicular to the molten resin.

[0011] In the above-mentioned method for manufacturing a liquid transport tube, in the piercing step, it is preferable that the piercing pin forms the through hole by punching the molten resin from a first surface of the molten resin that faces the outer circumferential surface of the core material toward a second surface that is the opposite surface to the first surface. According to the above-mentioned manufacturing method, the first surface that faces the core material becomes the inner surface of the liquid transport tube, and the second surface that is the opposite surface to the first surface becomes the outer surface of the liquid transport tube. By forming the through hole from the first surface to the second surface, burrs and the like are less likely to occur on the first surface when the through hole is formed. This makes it possible to smooth the inner surface of the liquid transport tube, thereby reducing resistance to a fluid passing through the inside of the liquid transport tube.

[0012] In the above-mentioned manufacturing method of the liquid transport pipe, the receiving base has an escape portion into which the piercing pin is inserted when the piercing pin punches out the molten resin, and the inner diameter of the escape portion is larger than the outer diameter of the piercing pin, and the clearance between the escape portion and the piercing pin is preferably 0.01 mm or more and 0.3 mm or less. According to the above-mentioned manufacturing method, by setting the clearance between the escape portion and the piercing pin to 0.01 mm or more and 0.3 mm or less, it is possible to prevent the molten resin from being caught in the gap between the escape portion and the piercing pin while preventing interference between the piercing pin and the escape portion when the piercing pin punches out the molten resin. As a result, it is possible to suppress the generation of burrs on the surface facing the receiving base. This makes it possible to suppress the deterioration of the appearance of the liquid transport pipe.

[0013] In the above-mentioned method for manufacturing a liquid transport pipe, the nominal diameter of the liquid transport pipe is preferably 300 mm or more and 3000 mm or less. According to the above-mentioned manufacturing method, since the nominal diameter of the liquid transport pipe is 300 mm or more and 3000 mm or less, the liquid transport pipe can be suitably used as a gas vent pipe or a drainage pipe.

[0014] In the above-mentioned method for manufacturing a liquid transport pipe, the thermoplastic resin is preferably selected from at least one of high-density polyethylene, low-density polyethylene, glass fiber reinforced polyethylene, and polypropylene. According to the above-mentioned manufacturing method, since the thermoplastic resin is a resin selected from at least one of high-density polyethylene, low-density polyethylene, glass fiber reinforced polyethylene, and polypropylene, it is possible to achieve mechanical properties such as pressure resistance and chemical properties such as chemical resistance and corrosion resistance required for a liquid transport pipe.

[0015] A perforating device for solving the above problem is a perforating device that forms through holes that penetrate the thickness direction of molten resin, which is a molten thermoplastic resin, before the molten resin is extruded in a band shape and wrapped around a core material, and is equipped with a perforating pin that forms the through hole by punching the molten resin, a receiving base that supports the molten resin when the perforating pin forms the through hole in the molten resin, and a movable part that moves the perforating pin and the receiving base to follow the molten resin moving toward the core material, and the perforating pin punches the molten resin while moving in accordance with the molten resin.

[0016] According to the above-mentioned configuration, through holes can be formed in the molten resin extruded in a strip shape. Then, by winding the molten resin with the through holes formed therein around the core material, a process of forming through holes using a drill or the like after molding is not required. Therefore, the production efficiency of the liquid transport pipe with the through holes on the circumferential surface can be improved. Effect of the Invention

[0017] According to the present invention, it is possible to improve the production efficiency of a liquid transport pipe having a through hole on its circumferential surface. [Brief description of the drawings]

[0018] [Figure 1] Schematic diagram of a liquid transport pipe manufacturing system. [Diagram 2] FIG. [Diagram 3] Schematic diagram of a drilling device. [Figure 4] FIG. 4 is a front view of a through hole in the molten resin before winding. [Diagram 5] FIG. 4 is a cross-sectional view of a through hole in the molten resin immediately after winding. [Figure 6] FIG. 4 is a cross-sectional view of a through hole in the molten resin after cooling. [Figure 7] FIG. 4 is a cross-sectional view of a through hole in the molten resin after cooling. [Figure 8] FIG. 4 is a front view of the through holes in the molten resin after cooling, as viewed from the second surface. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, one embodiment of the present invention will be described with reference to FIGS. [Liquid transport pipe manufacturing system] 1, the liquid transport pipe manufacturing system 10 is a system for manufacturing a perforated pipe, which is an example of a liquid transport pipe. The liquid transport pipe manufacturing system 10 includes an extrusion device 11, a perforation device 12, a cooling device 13, a winding device 14, and a control device 15.

[0020] The extrusion device 11 is the device located most upstream in the liquid transport pipe manufacturing system 10. The extrusion device 11 is an extrusion molding machine that melts a thermoplastic resin input as a raw material and then extrudes molten resin 20, which is a thermoplastic resin in a molten state, into a strip shape. The molten resin 20 extruded from the extrusion device 11 passes through a punching device 12 and a cooling device 13, and is transported downstream by being wound up by a winding device 14.

[0021] The punching device 12 is a device located downstream of the extrusion device 11 in the liquid transport pipe manufacturing system 10. The punching device 12 includes a punching pin 12a and a receiving stand 12b. The punching pin 12a punches out a part of the molten resin 20 to form through holes 20a penetrating the molten resin 20 in the thickness direction. In this embodiment, the punching pin 12a forms the through holes 20a at a constant pitch in the molten resin 20 in the extension direction of the molten resin 20. The receiving stand 12b supports the molten resin 20 extruded from the extrusion device 11.

[0022] Cooling device 13 is a device located downstream of extrusion device 11 and punching device 12 in liquid transport pipe manufacturing system 10. Cooling device 13 includes a conveying table 13a, a pressure bonding portion 13b, and a support portion 13c.

[0023] The conveying table 13a supports the molten resin 20 extruded from the extrusion device 11. The conveying table 13a is made of a metal such as iron or aluminum to improve the cooling efficiency of the molten resin 20. The punching device 12 is disposed upstream of the conveying table 13a. The upper surface of the conveying table 13a is located on the same plane as the upper surface of the receiving table 12b. In addition, the winding device 14 is disposed downstream of the conveying table 13a. The molten resin 20 extruded from the extrusion device 11 is wound up by the winding device 14 while being supported by the conveying table 13a through the upper part of the receiving table 12b.

[0024] The pressure-bonding portion 13b presses the molten resin 20 passing over the conveyance table 13a toward the core material 14a provided in the winding device 14. The support portion 13c is a portion that supports the pressure-bonding portion 13b and serves as a fulcrum when the pressure-bonding portion 13b presses the molten resin 20.

[0025] The winding device 14 is provided downstream of the conveyor 13a. The winding device 14 includes a core material 14a. The core material 14a is a cylindrical mold called a mandrel. In this embodiment, the core material 14a rotates around the central axis of the cylindrical shape. The rotation axis of the core material 14a is not limited to the central axis of the cylindrical shape, and may be, for example, an axis parallel to the central axis of the cylindrical shape and not overlapping with the central axis of the cylindrical shape.

[0026] Molten resin 20 supported by conveyor 13a is pressed against the outer circumferential surface of core 14a by pressure bonding unit 13b. With molten resin 20 pressed against core 14a by pressure bonding unit 13b, core 14a rotates, whereby molten resin 20 is wound around core 14a. At this time, molten resin 20 is wound in a spiral shape with a predetermined pitch in a direction along the rotation axis of core 14a, thereby forming a tubular molten resin 20 on the outer circumferential surface of core 14a. Thereafter, molten resin 20 is cooled and solidified to produce liquid transport pipe 21 (see FIG. 2).

[0027] The control device 15 is a computer that controls each device included in the liquid transport pipe manufacturing system 10. That is, the control device 15 controls the extrusion device 11, the punching device 12, the cooling device 13, and the winding device 14.

[0028] The control device 15 includes a control unit, a storage unit, and a touch panel. The control unit is, for example, a CPU. The control unit executes a process of controlling each device included in the liquid transport pipe manufacturing system 10 according to a control program stored in the storage unit. The storage unit is, for example, a storage medium such as an SSD or an HDD. The storage unit has a control program installed therein for the control unit to control each device. In addition, the storage unit stores various manufacturing conditions such as the rotation speed of the core material 14a, the pitch at which the through holes 20a are provided in the extension direction of the molten resin 20, and the pitch in the direction along the rotation axis of the molten resin 20 wound in a spiral shape. The touch panel is an operation unit that inputs an operation signal to the control unit based on the operation of the worker, and is also a display unit that displays the status of each device, the set manufacturing conditions, and the like. In addition, the control device 15 may be configured to control each device included in the liquid transport pipe manufacturing system 10 by, for example, a relay circuit.

[0029] [Liquid transport pipe] 2, liquid transport pipe 21 is a perforated pipe manufactured by cooling and solidifying molten resin 20 in liquid transport pipe manufacturing system 10. Liquid transport pipe 21 is used, for example, as a drainage pipe, which is a buried pipe buried in a landfill at a waste disposal site, a gas vent pipe, etc.

[0030] The liquid transport pipe 21 comprises a pipe body 22, a socket 23, and a spigot 24. The pipe body 22 is the central region of the liquid transport pipe 21. The socket 23 is formed at one end of the pipe body 22. The spigot 24 is formed at the other end of the pipe body 22. A plurality of liquid transport pipes 21 are connected to form a pipeline by inserting the spigot 24 of another liquid transport pipe 21 into the socket 23.

[0031] The pipe body 22 includes a through hole 20a and a rib 22a. The through hole 20a is formed by a drilling device 12 in the state of molten resin 20. The through hole 20a communicates between the inside and the outside of the liquid transport pipe 21. The through hole 20a is provided at an arbitrary position in the pipe body 22, taking into consideration the mechanical properties of the liquid transport pipe 21, such as pressure resistance.

[0032] The ribs 22a are ridges formed in a spiral shape on the outer circumferential surface of the pipe body 22. Providing the ribs 22a on the pipe body 22 can increase the resistance to external pressure acting on the liquid transport pipe 21. The ribs 22a are provided at any position that does not overlap with the through holes 20a and does not block the through holes 20a. In this embodiment, the through holes 20a are provided at a constant pitch along the circumferential direction of the pipe body 22 in the recesses between adjacent ribs 22a.

[0033] Socket 23 is configured so that its outer and inner diameters are larger than those of pipe body 22. The inner surface of socket 23 faces the outer surface of spigot 24. Spigot 24 is configured so that its inner diameter matches the inner diameter of pipe body 22 and its outer diameter is larger than the outer diameter of an area of ​​pipe body 22 where ribs 22a are not provided. The inner surface of spigot 24 is flush with the inner surface of pipe body 22. The outer surface of spigot 24 faces the inner surface of socket 23.

[0034] A circumferentially extending groove 24a is provided in the tip end region of the outer surface of the spigot 24. A water-stopping rubber 24b, which is an example of a water-stopping material, is provided in the groove 24a. The water-stopping rubber 24b is, for example, styrene-butadiene rubber or ethylene-propylene-diene rubber. The water-stopping rubber 24b provides water-stopping between the inner surface of the socket 23 and the outer surface of the spigot 24 by its rubber elasticity and sealing properties. This allows the liquid transport pipes 21 to be connected together by the simple task of simply inserting the spigot 24 into the socket 23.

[0035] A marked line 24c is provided on the outer surface of the spigot 24 in an area closer to the pipe body 22 than the recessed groove 24a and the water-stop rubber 24b. The marked line 24c is an indicator that indicates how far the spigot 24 should be inserted into the socket 23. Here, the spigot 24 is inserted to a position where the marked line 24c is covered by the socket 23 of another liquid transport pipe 21.

[0036] Furthermore, the nominal diameter of the liquid transport pipe 21 is preferably 300 mm or more and 3000 mm or less. When the nominal diameter of the liquid transport pipe 21 is 300 mm or more and 3000 mm or less, the liquid transport pipe 21 can be suitably used as a gas vent pipe or a drainage pipe.

[0037] The thermoplastic resin constituting the liquid transport pipe 21 is preferably at least one selected from the group consisting of high-density polyethylene, low-density polyethylene, glass fiber reinforced polyethylene, and polypropylene. The above-mentioned materials can achieve the mechanical properties, such as pressure resistance, and chemical properties, such as chemical resistance and corrosion resistance, required for the liquid transport pipe 21.

[0038] [Drilling device] The punching device 12 will now be described in detail with reference to FIG. As shown in Fig. 3, the punching device 12 includes a first movable part 12c and a second movable part 12d in addition to the punching pin 12a and the receiving base 12b described above. The punching pin 12a has a cylindrical shape that is elliptical in cross section. The punching pin 12a is disposed perpendicular to the receiving base 12b above the molten resin 20 conveyed on the receiving base 12b. One end of the punching pin 12a that faces the receiving base 12b has a conical shape with a pointed tip.

[0039] The piercing pin 12a punches the molten resin 20 from a first surface 20b that faces the outer peripheral surface of the core material 14a toward a second surface 20c that is the surface opposite to the first surface 20b, thereby forming a through hole 20a. The first surface 20b is the surface that becomes the inner surface of the liquid transport pipe 21. The second surface 20c is the surface that becomes the outer surface of the liquid transport pipe 21, and is the surface that faces the receiving table 12b and the transfer table 13a.

[0040] By forming the through-hole 20a from the first surface 20b toward the second surface 20c, burrs are less likely to occur on the first surface 20b, which becomes the inner surface of the liquid transport tube 21, when the through-hole 20a is formed. This makes it possible to make the inner surface of the liquid transport tube 21 smooth, thereby reducing resistance to the fluid passing through the inside of the liquid transport tube 21.

[0041] The piercing pin 12a preferably has an elliptical shape in cross section, with the extension direction of the molten resin 20 being the short side and the width direction perpendicular to the extension direction of the molten resin 20 being the long side. The molten resin 20 is formed with a through hole 20a having a shape corresponding to the shape of the piercing pin 12a. Therefore, the molten resin 20 is formed with an elliptical through hole 20a, with the extension direction of the molten resin 20 being the short side and the width direction of the molten resin 20 being the long side. In addition, in the winding process in which the molten resin 20 is wound around the core material 14a, tension acts on the molten resin 20 in the winding direction, which is the direction in which the molten resin 20 is wound around the core material 14a and along the extension direction of the molten resin 20. Therefore, in the winding process, the tension in the winding direction acting on the molten resin 20 causes the through hole 20a to be stretched in the winding direction and open so as to approach a perfect circle. This allows the through hole 20a to be formed in the liquid transport pipe 21 in a shape closer to a perfect circle, improving the appearance of the liquid transport pipe 21. Note that, since there is little change in the dimension of the through hole 20a in the width direction of the molten resin 20 during the winding process, the longitudinal dimension of the piercing pin 12a may be set to the target dimension of the through hole 20a.

[0042] The receiving table 12b is, for example, a rectangular plate. The molten resin 20 extruded from the extrusion device 11 is placed on the upper part of the receiving table 12b. Therefore, the molten resin 20 extruded from the extrusion device 11 passes over the conveyance table 13a through the upper part of the receiving table 12b.

[0043] The receiving base 12b supports the molten resin 20 when the piercing pins 12a form the through holes 20a in the molten resin 20. This allows the punching load of the piercing pins 12a to be appropriately applied to the molten resin 20, which is in a state where it is easily deformed.

[0044] The receiving base 12b has an escape portion 12e. The escape portion 12e is a through hole that penetrates the receiving base 12b in the thickness direction. The escape portion 12e is provided coaxially with the piercing pin 12a. When the piercing pin 12a punches out the molten resin 20, the tip of the piercing pin 12a is inserted into the escape portion 12e. The molten resin 20 punched out by the piercing pin 12a is discharged through the escape portion 12e. The discharged molten resin 20 can be reused as a raw material.

[0045] Conventionally, after the thermoplastic resin is molded into a tube, an operator forms a through hole in the circumferential surface of the tube using a drill or the like. In this case, the thermoplastic resin cut to form the through hole falls into the inside of the liquid transport pipe 21, and is then collected and discarded. It is difficult to reuse the cut thermoplastic resin because foreign matter is easily mixed in during collection. In this regard, by manufacturing the liquid transport pipe 21 with the through hole 20a by the liquid transport pipe manufacturing system 10, which is a series of manufacturing equipment rows, as in the present embodiment, the molten resin 20 punched by the boring pin 12a can be reused as a raw material.

[0046] The inner diameter of the relief portion 12e is configured to be larger than the outer diameter of the piercing pin 12a to prevent interference with the piercing pin 12a. In addition, if the clearance between the relief portion 12e and the piercing pin 12a is excessively large, the molten resin 20 is likely to be caught in the gap between the relief portion 12e and the piercing pin 12a when the piercing pin 12a punches the molten resin 20. Then, the caught molten resin 20 is stretched so as to protrude beyond the second surface 20c, and burrs are generated on the second surface 20c. If burrs are generated on the second surface 20c, the resistance increases when the crimping portion 13b presses the second surface 20c toward the core material 14a. In addition, since the second surface 20c is the outer surface of the liquid transport pipe 21, the appearance of the liquid transport pipe 21 may be deteriorated. Therefore, it is preferable that the inner diameter of the escape portion 12e is large enough so as not to interfere with the piercing pin 12a, and also large enough so that the molten resin 20 is not caught in the gap between the escape portion 12e and the piercing pin 12a.

[0047] Specifically, the clearance between the relief portion 12e and the piercing pin 12a is preferably 0.01 mm or more and 0.3 mm or less, and more preferably 0.01 mm or more and 0.05 mm or less. By setting the clearance between the relief portion 12e and the piercing pin 12a within the above range, it is possible to prevent the molten resin 20 from being caught in the gap between the relief portion 12e and the piercing pin 12a while preventing interference between the piercing pin 12a and the relief portion 12e. As a result, the generation of burrs on the second surface 20c can be suppressed, and the second surface 20c can be suitably pressed toward the core material 14a by the crimping portion 13b. In addition, it is possible to suppress deterioration of the appearance of the liquid transport pipe 21.

[0048] The first movable part 12c is, for example, a rectangular plate. The piercing pin 12a is fixed to the first movable part 12c. The second movable part 12d is, for example, a member having a prismatic shape extending perpendicularly to the receiving stand 12b. The first movable part 12c is attached to the upper part of the second movable part 12d so as to be movable in the extending direction of the second movable part 12d, i.e., in the direction perpendicular to the receiving stand 12b. The receiving stand 12b is fixed to the lower part of the second movable part 12d. The second movable part 12d is configured to be movable parallel to the conveying direction of the molten resin 20.

[0049] The first movable part 12c is driven relative to the second movable part 12d in the extension direction of the second movable part 12d, whereby the piercing pin 12a is driven in a direction perpendicular to the receiving stand 12b. The second movable part 12d is moved parallel to the conveying direction of the molten resin 20, whereby the piercing pin 12a and the receiving stand 12b are moved parallel to the conveying direction of the molten resin 20. The driving of the first movable part 12c and the second movable part 12d is controlled by the control device 15.

[0050] [Method of manufacturing liquid transport pipes] The following describes a method for manufacturing the liquid transport pipe 21 in the liquid transport pipe manufacturing system 10. The manufacturing process for the liquid transport pipe 21 is roughly divided into an extrusion process, a perforation process, a winding process, and a cooling process.

[0051] First, with reference to Fig. 1, an extrusion process in which a thermoplastic resin is extruded as a molten resin 20 will be described. First, a thermoplastic resin is fed as a raw material into an extrusion device 11. The extrusion device 11 melts the fed thermoplastic resin and then extrudes it as a strip-shaped molten resin 20. The extruded molten resin 20 is transported downstream by being wound up by a rotating core material 14a while being placed on a transport table 13a via an upper portion of a receiving table 12b.

[0052] Next, a description will be given of a punching process for forming through holes 20a in molten resin 20 with reference to Fig. 3. In the punching process, control device 15 forms through holes 20a in molten resin 20 by driving first movable part 12c and second movable part 12d.

[0053] Specifically, the control device 15 drives the first movable part 12c to descend vertically relative to the receiving table 12b until the tip of the punching pin 12a is inserted into the inside of the relief part 12e. As a result, a part of the molten resin 20 is punched in the thickness direction by the punching pin 12a while the molten resin 20 is supported by the receiving table 12b, thereby forming a through hole 20a in the molten resin 20. Thereafter, the control device 15 drives the first movable part 12c to ascend vertically relative to the receiving table 12b.

[0054] In addition to the process of lowering and raising the first movable part 12c described above, the control device 15 also executes a process of driving the second movable part 12d to follow the movement of the molten resin 20 at the same speed as the conveying speed of the molten resin 20. This causes the piercing pins 12a and the receiving base 12b to move to follow the molten resin 20 conveyed downstream. Therefore, the piercing pins 12a punch the molten resin 20 to form the through holes 20a while moving to follow the molten resin 20 conveyed downstream. The conveying speed of the molten resin 20 depends on the winding speed of the core material 14a in the winding device 14, i.e., the rotation speed of the core material 14a.

[0055] If the second movable part 12d is not driven and the first movable part 12c is simply driven in a vertical direction relative to the conveying platform 13a, the molten resin 20 conveyed from the upstream is blocked to a certain extent when the drilling pin 12a punches the molten resin 20. In this case, the molten resin 20 located around the drilling pin 12a, especially on the upstream side, is deformed, making it difficult to control the shape of the through hole 20a. If the molten resin 20 defining the through hole 20a is deformed, for example, the through hole 20a becomes larger than necessary, and when the liquid transport pipe 21 is buried in the ground, crushed stones or the like may easily enter, or cracks may occur around the through hole 20a. In addition, the load of the molten resin 20 conveyed from the upstream is applied to the drilling pin 12a, making the drilling pin 12a more likely to break.

[0056] Also, for example, when the rotation of the core material 14a is stopped and the transport of the molten resin 20 is stopped when the piercing pin 12a punches out the molten resin 20, the core material 14a may rotate excessively due to inertia. In this case, the molten resin 20 may be unintentionally stretched, which may cause the width of the molten resin 20 to be partially narrowed or the molten resin 20 to break. In addition, the molten resin 20 may be pushed out from the extrusion device 11 due to inertia, which may cause the width of the molten resin 20 to be partially narrowed. For this reason, when the transport of the molten resin 20 is stopped when the piercing pin 12a punches out the molten resin 20, it is difficult to stably produce the liquid transport pipe 21.

[0057] In this respect, as in the present embodiment, by punching the molten resin 20 while moving following the transported molten resin 20, the shape of the through hole 20a can be easily controlled compared to the case where the piercing pin 12a is simply driven in a direction perpendicular to the molten resin 20. Also, the load applied to the piercing pin 12a by the molten resin 20 transported from upstream can be reduced. Also, more stable production can be achieved and production efficiency can be improved compared to the case where the rotation of the core material 14a is stopped and the transport of the molten resin 20 is stopped when the piercing pin 12a punches the molten resin 20.

[0058] Here, the shape of the through hole 20a formed in the molten resin 20 in the perforation process will be described with reference to Fig. 4. As described above, the through hole 20a formed in the perforation process has an elliptical shape with the extension direction of the molten resin 20 as the short side and the width direction of the molten resin 20 as the long side. More specifically, the through hole 20a formed in the perforation process preferably has a dimension D1 in the extension direction of the molten resin 20 of 20% to 80% of the dimension D2 in the width direction of the molten resin 20. By forming the through hole 20a having such dimensions D1 and D2 in the perforation process, the through hole 20a can be stretched in the winding direction by the tension in the winding direction acting on the molten resin 20 in the winding process, and opened so as to approach a perfect circle.

[0059] Next, referring again to FIG. 3, the winding process of winding the molten resin 20 around the core material 14a will be described. In the winding process, the control device 15 drives the pressure bonding unit 13b to press the molten resin 20 against the core material 14a, and drives the core material 14a to rotate. The molten resin 20 is wound around the outer circumferential surface of the core material 14a in a spiral shape with a predetermined pitch in a direction along the rotation axis, thereby forming a tubular shape. In the winding process, the through hole 20a is stretched in the winding direction by the tension acting on the molten resin 20 in the winding direction, and opens so as to approach a perfect circle.

[0060] The predetermined pitch here is a pitch at which adjacent molten resins 20 are spirally wound around each other without gaps when the molten resin 20 is pressed against the core material 14a by the pressure bonding portion 13b. The predetermined pitch here is a pitch at which the through holes 20a provided in the molten resin 20 are not blocked by adjacent molten resins 20 and face the outer surface, that is, the through holes 20a open on the outer surface of the liquid transport pipe 21. In this embodiment, a single layer of molten resin 20 is wound around the core material 14a.

[0061] In the winding process, the molten resin 20 formed into a tubular shape has spiral ribs 22a formed in a region corresponding to the pipe body 22 of the liquid transport pipe 21. The ribs 22a are formed, for example, by winding a hollow core tube (not shown) wrapped with molten thermoplastic resin in a molten state in a spiral shape around the molten resin 20 formed into a tubular shape. The ribs 22a are provided at an arbitrary pitch in a position that does not overlap the through hole 20a and does not block the through hole 20a.

[0062] Finally, the molten resin 20 formed into a tubular shape is cooled in a cooling process for cooling the molten resin 20. Then, the cooled and solidified molten resin 20 is removed from the core material 14a, thereby producing the liquid transport pipe 21.

[0063] As described above, in the past, in addition to the process of molding the thermoplastic resin into a tubular shape, a drilling operation was required in which an operator formed a through hole using a drill or the like. In this case, advance preparation such as marking the position where the through hole is to be provided on the tube body based on strength calculations or the like is also required. In this regard, by performing the drilling process in a limited period between the extrusion process and the winding process, the drilling operation after molding and the advance preparation process are not required. Therefore, the production efficiency of the liquid transport pipe 21 having the through hole 20a on the circumferential surface can be improved. In addition, the variation in the position where the through hole 20a is provided is reduced compared to the case where an operator forms the through hole using a drill or the like.

[0064] [Changes in shape of through holes due to cooling of molten resin] Next, the change in shape of the through hole 20a during the cooling process will be described with reference to FIGS.

[0065] 5, the molten resin 20 immediately after being wound around the core material 14a and before being cooled is in a state where the first surface 20b, which becomes the inner surface of the liquid transport pipe 21, is stuck to the core material 14a. In this state, the molten resin 20 that defines the through hole 20a on the first surface 20b side sticks to the core material 14a, so that the diameter of the through hole 20a on the first surface 20b side becomes slightly larger than the diameter of the second surface 20c side. Note that the through hole 20a in the molten resin 20 before being cooled has a shape close to a perfect circle on both the first surface 20b side and the second surface 20c side.

[0066] 6, the molten resin 20 is wound around the core material 14a, and then cooled and solidified in a state in which the molten resin 20 defining the through-hole 20a on the first surface 20b side is stuck to the core material 14a. Therefore, the shape of the molten resin 20 defining the through-hole 20a on the first surface 20b side hardly changes before and after cooling.

[0067] In contrast, the molten resin 20 defining the through hole 20a on the second surface 20c side shrinks in the extension direction of the molten resin 20 as shown by the arrow in Fig. 6 due to the influence of residual stress of the tension acting on the molten resin 20 in the winding process and the like as it cools. Furthermore, the molten resin 20 defining the through hole 20a on the second surface 20c side forms a protruding portion 20d in the extension direction of the molten resin 20 due to shrinkage caused by cooling. The protruding portion 20d is a region where the molten resin 20 protrudes from the second surface 20c.

[0068] As shown in FIG. 7, the molten resin 20 that defines the through hole 20a on the second surface 20c side contracts with cooling to form an inclined portion 20e on the inner peripheral surface of the through hole 20a that reduces the diameter of the through hole 20a. The inclined portion 20e is a region where the molten resin 20 sinks toward the first surface 20b side from the second surface 20c and protrudes inward of the through hole 20a. The inclined portion 20e is, for example, a straight inclined surface, a curved surface that bulges upward, a curved surface that is recessed downward, or a combination of these. The inclined portion 20e reduces the diameter of the through hole 20a most in the width direction at the edge that defines the through hole 20a. The position of the edge that defines the through hole 20a in the inclined portion 20e slightly moves up and down in the depth direction of the through hole 20a depending on the manufacturing conditions such as the cooling rate and the thickness of the molten resin 20.

[0069] As shown in FIG. 8, the shape of the through hole 20a in the cooled molten resin 20 is expanded in the extension direction of the molten resin 20 on the second surface 20c side due to contraction caused by cooling, and is reduced in the width direction of the molten resin 20. However, on the first surface 20b side, as described above, the shape of the through hole 20a hardly changes before and after cooling, and is maintained in a state close to a perfect circle. Therefore, the through hole 20a after cooling has a smaller dimension on the second surface 20c side than the first surface 20b side in the width direction of the molten resin 20, and has a smaller dimension on the first surface 20b side than the second surface 20c side in the extension direction of the molten resin 20. This makes it difficult for crushed stones and the like to enter through the through hole 20a while securing the area required for the through hole 20a.

[0070] [Effects of the embodiment] According to the above embodiment, the following effects can be obtained. (1) In the drilling process, by forming the through holes 20a in the molten resin 20, the drilling work after molding the thermoplastic resin into a tubular shape is not required. Therefore, the production efficiency of the liquid transport pipe 21 having the through holes 20a on the circumferential surface can be improved. Also, the variation in the position where the through holes 20a are provided is reduced compared to the case where an operator forms the through holes using a drill or the like.

[0071] (2) After cooling, through hole 20a has a smaller dimension on the second surface 20c side than on the first surface 20b side in the width direction of molten resin 20, and has a smaller dimension on the first surface 20b side than on the second surface 20c side in the extension direction of molten resin 20. Therefore, by forming through hole 20a in molten resin 20 in the drilling step and winding molten resin 20 around core material 14a in the winding step, it is possible to ensure an area required for through hole 20a while making it difficult for crushed stone or the like to enter through through hole 20a.

[0072] (3) Through hole 20a formed in the perforation process is configured so that dimension D1 in the extension direction of molten resin 20 is smaller than dimension D2 in the width direction of molten resin 20. As a result, in the winding process, through hole 20a is stretched in the winding direction by tension in the winding direction acting on molten resin 20, so that the shape of through hole 20a can be made closer to a perfect circle.

[0073] (4) When the piercing pin 12a forms the through hole 20a in the molten resin 20, the molten resin 20 is supported by the receiving base 12b, so that the punching load of the piercing pin 12a can be applied appropriately to the molten resin 20, which is in a state where it is easily deformed.

[0074] (5) The piercing pin 12a punches the molten resin 20 while moving in accordance with the molten resin 20 being transported, thereby preventing the molten resin 20 being transported from upstream from being blocked by the piercing pin 12a. This makes it easier to control the shape of the through hole 20a than when the piercing pin 12a is simply driven in a direction perpendicular to the molten resin 20. This reduces the load applied to the piercing pin 12a by the molten resin 20 being transported from upstream. In addition, since the through hole 20a can be formed while the molten resin 20 is being transported, production can be more stable and production efficiency can be improved compared to a manufacturing method in which the rotation of the core material 14a is stopped and the transport of the molten resin 20 is stopped when the piercing pin 12a punches the molten resin 20.

[0075] (6) By forming the through-holes 20a from the first surface 20b facing the core 14a toward the second surface 20c, which is the surface opposite the first surface 20b, burrs are less likely to occur when forming the through-holes 20a on the first surface 20b, which is the inner surface of the liquid transport tube 21. This makes it possible to make the inner surface of the liquid transport tube 21 smooth, thereby reducing resistance to the fluid passing through the inside of the liquid transport tube 21.

[0076] (7) The clearance between the relief portion 12e and the piercing pin 12a is set to 0.01 mm or more and 0.3 mm or less, more preferably 0.01 mm or more and 0.05 mm or less. This prevents the piercing pin 12a from interfering with the relief portion 12e when the piercing pin 12a punches the molten resin 20, while preventing the molten resin 20 from being caught in the gap between the relief portion 12e and the piercing pin 12a. As a result, the generation of burrs on the second surface 20c is suppressed, and therefore the resistance when the crimping portion 13b presses the second surface 20c toward the core material 14a is prevented from increasing. Therefore, the crimping portion 13b can suitably press the second surface 20c toward the core material 14a. In addition, the deterioration of the appearance of the liquid transport pipe 21 can be suppressed.

[0077] (8) Since the nominal diameter of the liquid transport pipe 21 is 300 mm or more and 3000 mm or less, the liquid transport pipe 21 can be suitably used as a gas vent pipe or a drainage pipe. (9) The thermoplastic resin constituting the liquid transport pipe 21 is selected from at least one of high density polyethylene, low density polyethylene, glass fiber reinforced polyethylene, and polypropylene. By using the above-mentioned material as the thermoplastic resin constituting the liquid transport pipe 21, the mechanical properties such as pressure resistance and chemical properties such as chemical resistance and corrosion resistance required for the liquid transport pipe 21 can be achieved.

[0078] The liquid transport pipe manufacturing system 10 as described above can be further modified as necessary as follows. High density polyethylene, low density polyethylene, glass fiber reinforced polyethylene, and polypropylene are given as examples of the thermoplastic resin that constitutes the liquid transport pipe 21. However, the present invention is not limited to these, and polyvinyl chloride (PVC), ABS resin (acrylonitrile butadiene styrene resin), acrylic resin (PMMA), and the like may also be used as the thermoplastic resin that constitutes the liquid transport pipe 21. Furthermore, the thermoplastic resin that constitutes the liquid transport pipe 21 may contain additives such as pigments, antioxidants, and stabilizers, as well as coupling materials.

[0079] The configuration in which the nominal diameter of the liquid transport pipe 21 is 300 mm or more and 3000 mm or less has been exemplified. However, the present invention is not limited to this, and as long as the mechanical properties required for the liquid transport pipe 21 can be achieved, for example, the nominal diameter of the liquid transport pipe 21 may be less than 300 mm or more than 3000 mm.

[0080] The configuration in which the clearance between the relief portion 12e and the piercing pin 12a is 0.01 mm or more and 0.3 mm or less, or 0.01 mm or more and 0.05 mm or less, is exemplified. However, the present invention is not limited to this. For example, if the piercing pin 12a and the relief portion 12e do not interfere with each other, the clearance between the relief portion 12e and the piercing pin 12a may be less than 0.01 mm. Also, for example, if the molten resin 20 is not caught in the gap between the relief portion 12e and the piercing pin 12a, the clearance between the relief portion 12e and the piercing pin 12a may be more than 0.3 mm.

[0081] The configuration in which the piercing pin 12a forms the through hole 20a from the first surface 20b toward the second surface 20c has been exemplified. However, the present invention is not limited to this, and for example, the piercing pin 12a may form the through hole 20a from the second surface 20c toward the first surface 20b as long as the burrs generated when the piercing pin 12a forms the through hole 20a are of a size that does not cause resistance to the fluid passing through the liquid transport pipe 21.

[0082] The configuration in which the piercing pin 12a punches out the molten resin 20 while moving following the transported molten resin 20 has been exemplified. However, the present invention is not limited to this, and as long as the shape of the through hole 20a can be controlled when the rotation speed of the core material 14a is low, for example, the second movable part 12d may not be driven, and the first movable part 12c may simply be driven in a vertical direction relative to the transport table 13a. Also, as long as stable production of the liquid transport pipe 21 is possible, for example, the piercing pin 12a may form the molten resin 20 in a state in which the rotation of the core material 14a is stopped and the transport of the molten resin 20 is stopped.

[0083] In the through hole 20a formed in the punching step, a configuration has been exemplified in which the dimension D1 in the extension direction of the molten resin 20 is smaller than the dimension D2 in the width direction of the molten resin 20. However, this is not limited thereto, and the dimensions D1 and D2 of the through hole 20a formed in the punching step may be appropriately determined depending on the type of thermoplastic resin and the tension in the winding direction acting on the molten resin 20 in the winding step, and for example, the dimension D1 may be the same as the dimension D2. Also, the dimension D1 may be larger than the dimension D2.

[0084] In the punching step, the through holes 20a are formed at a constant pitch. However, the present invention is not limited to this, and the through holes 20a may be provided at any position in the extension direction of the molten resin 20, taking into consideration mechanical properties such as pressure resistance.

[0085] In the winding step, a configuration in which one layer of molten resin 20 is wound around core material 14a has been exemplified. However, the present invention is not limited to this, and for example, multiple layers of molten resin 20 may be wound around core material 14a. In this case, the second and subsequent layers of molten resin 20 are wound at a pitch that does not block the through holes 20a formed in the first layer of molten resin 20. This allows the strength of liquid transport pipe 21 to be increased by partially increasing the thickness.

[0086] The configuration has been exemplified in which the liquid transport pipes 21 are provided with a water stop rubber 24b, and the spigot 24 of the liquid transport pipe 21 is inserted into the socket 23 of the other liquid transport pipe 21, thereby connecting the liquid transport pipes 21 to each other. However, the present invention is not limited to this, and the water stop rubber 24b may be a water-expanding rubber. Furthermore, the liquid transport pipes 21 may be connected to each other by, for example, electric fusion or butt fusion. In this case, the liquid transport pipe 21 does not need to be provided with the water stop rubber 24b. Furthermore, in order to connect the liquid transport pipes 21 to each other, a member that serves as a joint for connecting the liquid transport pipes 21 to each other, such as a flange joint, may be used.

[0087] The number of the marked lines 24c may be two or more. Also, if the insertion depth is determined by the length of the socket 23 and the spigot 24, the marked lines 24c do not have to be provided. Although the liquid transport pipe 21 is provided with the ribs 22a in the above example, the liquid transport pipe 21 does not necessarily need to have the ribs 22a as long as the liquid transport pipe 21 can achieve the mechanical properties required for the liquid transport pipe 21. [Explanation of symbols]

[0088] 10...Liquid transport pipe manufacturing system 11...Extrusion device 12...Drilling device 12a…Piercing pin 12b…Pedestal 12c...first movable part 12d…Second movable part 12e…Relief section 13…Cooling device 13a...Transport platform 13b… Crimping section 13c...Support part 14…Wrapping device 14a…Core material 15...Control device 20...Molten resin 20a...Through hole 20b…Side 1 20c…Second side 21…Liquid transport pipe 22...Liquid transport pipe manufacturing system 22a…Rib 23…Socket 24…Outlet 24a…groove 24b…Shisui Yuna 24c… marking line

Claims

1. A method for manufacturing a liquid transport pipe, comprising the steps of: forming a liquid transport pipe from a molten resin that is a thermoplastic resin in a molten state, the method comprising the steps of: an extrusion step of extruding the molten resin into a strip shape; a perforation step of forming a through hole penetrating the band-shaped molten resin in a thickness direction; a winding step of spirally winding the strip-shaped molten resin having the through hole formed therein around an outer circumferential surface of a core material so that the through hole communicates with the inside and outside of the liquid transport pipe and so that tension acts on the molten resin in a winding direction along the extension direction of the molten resin, In the perforating step, the through hole is formed so that a dimension of the through hole in the extension direction is smaller than a dimension of the through hole in a width direction of the molten resin perpendicular to the extension direction. A method for manufacturing a liquid transport tube.

2. In the perforation step, the molten resin is punched in the thickness direction by a perforation pin while the molten resin is supported on a receiving stand, so that the through hole is formed in the molten resin. A method for manufacturing the liquid transport pipe according to claim 1.

3. In the perforation step, the piercing pin and the receiving base move in accordance with the movement of the molten resin transported toward the core material, The piercing pin punches out the molten resin while moving in accordance with the molten resin. A method for manufacturing the liquid transport pipe according to claim 2.

4. In the perforation step, The piercing pin forms the through hole by punching the molten resin from a first surface of the molten resin facing the outer circumferential surface of the core material toward a second surface that is the opposite surface to the first surface. A method for manufacturing the liquid transport pipe according to claim 2 or 3.

5. the receiving base includes a relief portion into which the piercing pin is inserted when the piercing pin punches out the molten resin, The inner diameter of the relief portion is larger than the outer diameter of the piercing pin, The clearance between the relief portion and the piercing pin is 0.01 mm or more and 0.3 mm or less. A method for manufacturing the liquid transport pipe according to any one of claims 2 to 4.

6. The nominal diameter of the liquid transport pipe is 300 mm or more and 3000 mm or less. A method for manufacturing the liquid transport pipe according to any one of claims 1 to 5.

7. The thermoplastic resin is selected from at least one of high density polyethylene, low density polyethylene, glass fiber reinforced polyethylene, and polypropylene. A method for manufacturing the liquid transport pipe according to any one of claims 1 to 6.

8. A method for manufacturing a liquid transport pipe, comprising molding a liquid transport pipe from a molten resin that is a thermoplastic resin in a molten state, comprising: an extrusion step of extruding the molten resin into a strip shape; a perforation step of forming a through hole penetrating the band-shaped molten resin in a thickness direction; a winding step of spirally winding the strip-shaped molten resin having the through hole formed therein around an outer circumferential surface of a core material so that the through hole communicates with the inside and outside of the liquid transport tube; In the perforation step, the molten resin is punched in the thickness direction by a piercing pin while the molten resin is supported on a receiving stand, thereby forming the through hole in the molten resin; the piercing pin and the receiving base move in accordance with the movement of the molten resin transported toward the core material, The piercing pin punches out the molten resin while moving in accordance with the molten resin. A method for manufacturing a liquid transport tube.

9. A punching device for forming through holes penetrating a thickness direction of a molten resin, the molten resin being a thermoplastic resin in a molten state, before the molten resin is extruded in a strip shape and wound around a core material, the punching device comprising: a piercing pin that forms the through hole by punching the molten resin; a receiving base for supporting the molten resin when the piercing pin forms the through hole in the molten resin; a movable portion that moves the piercing pin and the receiving base so as to follow the molten resin moving toward the core material, The piercing pin punches out the molten resin while moving in accordance with the molten resin. perforation device.

Citation Information

Patent Citations

  • JP1967011519Y1

  • Production of perforated pipe

    JP1978134883A

  • Corrugated pipe, pressing member, and core die

    JP1990134484A

  • Method and device for processing thermoplastic resin tubular body

    JP2001062913A

  • Float and fish preserve using the same

    JP2005143458A