Valve body and manufacturing method thereof

By positioning the neck transversely and thickening the wall thickness between the sprue and neck in the valve body, directional solidification is promoted, effectively preventing shrinkage cavities and reducing manufacturing costs.

JP7556710B2Active Publication Date: 2024-09-26KITZ CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2020112885
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-06-30
Publication Date
2024-09-26
Estimated Expiration
2040-06-30

AI Technical Summary

Technical Problem

Casting defects, particularly shrinkage cavities, frequently occur at the intersection of the neck and cylindrical body in valve bodies, especially in stainless steel cast products, leading to increased manufacturing costs due to additional processing steps required to remove sprues and prevent defects.

Method used

The neck part of the valve body is positioned transversely to the cylindrical body with the sprue located closer to the base of the neck, and the wall thickness between the sprue mark and neck is made thicker than other regions, gradually thinning towards the base, promoting directional solidification and minimizing shrinkage cavities.

Benefits of technology

This design suppresses the occurrence of shrinkage cavities by ensuring faster solidification of molten metal, reducing the need for additional processing and maintaining the integrity of the valve body.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007556710000004
    Figure 0007556710000004
  • Figure 0007556710000005
    Figure 0007556710000005
  • Figure 0007556710000001
    Figure 0007556710000001
Patent Text Reader

Abstract

To provide the body of a valve that is produced by casting, excellent in castability by suitably controlling a solidification step from a sprue to a neck part for casting, thus suppressing the generation of shrinkage cavities.SOLUTION: In the body 1 of a valve, a gate part 6 as a molten metal pouring port upon casting is formed in a state of being bulged to the cylindrical surface 2 of the body, also, the wall thickness of a first region 7 as a part in a space from the gate part 6 to a neck part 3 is formed so as to be thicken than the wall thickness of regions other than the body, and further, the wall-thickness of the first region 7 in a thickly formed state is formed so as to be gradually thinned from the gate part 6 toward the part 8 of the root of the neck part, and also, a method for producing the same is provided.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a valve body capable of suppressing the occurrence of casting defects and a method for manufacturing the valve body. [Background technology]

[0002] Since the valve body is a pressure-resistant vessel, it is mainly manufactured by metal casting.

[0003] In particular, when the main body of this type of valve, such as a ball valve or butterfly valve, which has a substantially cylindrical body with a neck protruding from it to form a mounting portion and has a packing, handle, etc. attached to it to open and close the valve, is manufactured by casting, a casting defect called a shrinkage cavity is likely to occur at the base of the neck, which causes a decrease in yield when the main body is cast.

[0004] In casting, the molten metal poured into the mold shrinks in volume as it cools and begins to solidify, and the molten metal that makes up for this shrinkage is solidified from the surrounding area to make up for the shrinkage, but the final solidification area (the area that cools and solidifies last) cannot make up for the shrinkage from the surrounding area, so the shrinkage remains as a gap and becomes a shrinkage cavity. In a valve body having a neck protruding from a roughly cylindrical body and a mounting part, the upper part of the body and the base of the neck form an intersection with an L-shaped cross section, but such an intersection is difficult to cool and solidify, so it is likely to become the final solidification area, and as a result, shrinkage cavities are likely to occur at this intersection.

[0005] It is difficult to completely prevent the occurrence of shrinkage cavities, no matter what metal material is used to cast the body, but in bodies made of stainless steel castings (SCS) made from stainless steel, shrinkage cavities are particularly likely to occur, because stainless steel has almost no volume expansion due to graphite crystallization when cooled and solidified.

[0006] As a technique for casting a main body having a mounting part with a neck protruding from a substantially cylindrical body while preventing the occurrence of casting defects such as shrinkage cavities, for example, Patent Document 1 discloses an as-cast ball valve body in which a sprue is provided directly on the mounting part located approximately in the center of the body, and the thickness of the mounting part is kept equal to or greater than the minimum thickness of the body, thereby directionally solidifying the molten metal and preventing the occurrence of shrinkage cavities at the intersection formed by the top of the body and the base of the mounting part. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Japanese Patent Application Publication No. 5-50209 Summary of the Invention [Problem to be solved by the invention]

[0008] However, in the as-cast ball valve body disclosed in Patent Document 1, the sprue is provided directly on the mounting portion located approximately in the center of the body, so that when removed from the mold (as-cast state), the sprue remains above the mounting portion, and the mounting portion is formed in a solid state.

[0009] Therefore, after removal from the mold, it is not possible to obtain a usable body without not only cutting out the sprue portion that is directly attached to the mounting portion, but also forming an insertion hole in the mounting portion for inserting the valve stem and steps and grooves for attaching gaskets, etc., which increases the number of processing steps and therefore increases manufacturing costs.

[0010] The present invention has been developed to solve the above problems, and an object of the present invention is to provide a valve body manufactured by casting that has excellent castability by appropriately controlling the solidification process from the casting gate to the neck, thereby suppressing the occurrence of shrinkage cavities. [Means for solving the problem]

[0011] In order to achieve the above object, the invention according to claim 1 provides a shaft mounting part by projecting a neck part in a direction perpendicular to a cylindrical body. Established A body main body, When casting this body, The remains of the gate used for pouring during casting The dam is located closer to the base of the neck than the position rotated 90 degrees in the circumferential direction of the cylinder of the body from the base of the neck. Formed in a raised state on the cylindrical surface of the body death The body of the valve is characterized in that the thickness of a first region, which is the area from the dam mark to the neck portion, is formed to be thicker than the thickness of other regions of the body, and the thickness of the first region in this thick state is gradually thinner from the dam mark to the area at the base of the neck portion.

[0012] The invention according to claim 2 is a valve body, in which the wall thickness of the body in the first region is formed to be thicker than at least the base of the neck portion.

[0013] The invention according to claim 3 is as follows: A body main body having a cylindrical body with a neck portion protruding in a direction perpendicular to the body and a mounting portion provided therewith, the trace of a dam portion, which is a pouring port during casting, is formed in a raised state on the cylindrical surface of the body, and the thickness of a first region, which is a region between the trace of the dam portion and the neck portion, is formed to be thicker than the thickness of other regions of the body, and the thickness of the first region in the thick state is formed to be gradually thinner from the trace of the dam portion toward the region at the base of the neck portion, and further, The width of the first region is gradually narrowed from the dam portion toward the base of the neck portion. Characterized by This is the body of the valve.

[0014] The invention according to claim 4 is A body main body having a cylindrical body with a neck portion protruding in a direction perpendicular to the body and a mounting portion provided therewith, the trace of a dam portion, which is a pouring port during casting, is formed in a raised state on the cylindrical surface of the body, and the thickness of a first region, which is a region between the trace of the dam portion and the neck portion, is formed to be thicker than the thickness of other regions of the body, and the thickness of the first region in the thick state is formed to be gradually thinner from the trace of the dam portion toward the base of the neck portion, and further, The mark of the dam is wider than the base of the neck. Characterized by This is the body of the valve.

[0015] The invention according to claim 5 is a cylindrical body having a neck portion protruding in a direction perpendicular to the cylindrical body. hand The mounting part Established A method for manufacturing a valve body, comprising the steps of: The base of the neck is located closer to the position rotated 90 degrees around the circumference of the body cylinder than the base of the neck. The position is offset from the neck portion, Furthermore, the pouring spout is formed in a raised state on the cylindrical surface of the body,The height of the molten metal passage in a first region from the pouring port to the base of the neck is made higher than the height of other regions, and the height of the molten metal passage is made gradually lower from the pouring port to the base of the neck, thereby suppressing shrinkage cavities from occurring in the valve body during casting in a mold. Effect of the Invention

[0016] According to the invention of claim 1, the trace of the gate, which is the pouring port during casting, The dam is located closer to the base of the neck than the position rotated 90 degrees in the circumferential direction of the cylinder of the body from the base of the neck. Formed in a raised state on the cylindrical surface of the body death The thickness of the first region between the dam mark and the neck is made thicker than the thickness of other regions of the body, and the thickness of the first region in the thick state is gradually reduced from the dam mark to the base of the neck. The molten metal is quickly pumped from the gate into the casting space at the base of the neck, allowing the molten metal to solidify faster than in other areas. Since the base of the neck portion is less likely to reach the final solidification point during casting, it is possible to suppress the occurrence of casting defects such as shrinkage cavities that have traditionally been prone to occur at the base of the neck portion of the main body.

[0017] In addition, since the thickness of the first region is formed to be thicker than the thickness of the surrounding cylindrical surface of the body, directional solidification of the molten metal from the base of the neck toward the trace of the dam (pouring port) during casting is promoted, and the occurrence of casting defects such as shrinkage cavities at the base of the neck can be suppressed.

[0018] According to the invention of claim 2, the thickness of the body in the first region is formed to be thicker than the thickness of at least the base of the neck portion. Therefore, during casting, the molten metal in at least the base of the neck portion solidifies earlier than the molten metal in the first region. This prevents the base of the neck portion from becoming the final solidification point, thereby suppressing the occurrence of casting defects such as shrinkage cavities in the base of the neck portion.

[0019] According to the invention of claim 3, the width of the first region is formed so as to gradually narrow from the trace of the dam portion toward the base of the neck portion. This makes it easier to promote directional solidification of the molten metal from the base of the neck portion toward the dam portion during casting, and makes it possible to more effectively suppress the occurrence of casting defects such as shrinkage cavities at the base of the neck portion.

[0020] According to the invention of claim 4, the mark of the dam portion is formed wider than the base of the neck portion. Therefore, the solidification of the molten metal at the dam portion is delayed compared to the body portion, and the final solidification of the molten metal is likely to occur at the dam portion. As a result, casting defects such as shrinkage cavities are less likely to occur not only at the base of the neck portion but also throughout the entire body. In addition, the molten metal can be efficiently sent from the dam portion into the mold for the valve body during casting.

[0021] According to the invention of claim 5, the pouring port during casting of the mold is: The base of the neck is located closer to the position rotated 90 degrees around the circumference of the body cylinder than the base of the neck. The position is offset from the neck portion, Furthermore, the pouring spout is formed in a raised state on the cylindrical surface of the body, In addition, the height of the molten metal passage in the first region from the pouring port to the base of the neck is higher than the height of the other regions, and the height of the molten metal passage is gradually lowered from the pouring port to the base of the neck. The molten metal can be quickly sent from the gate to the casting space at the base of the neck, allowing the molten metal to solidify faster than in other areas. This makes it easier to directionally solidify the molten metal from the base of the neck portion toward the dam portion, and makes it possible to more effectively suppress the occurrence of shrinkage cavities at the base of the neck portion.

[0022] Furthermore, when the valve body is cast using this manufacturing method, a sound body can be obtained by performing only minimal processing, such as cutting off the main body portion at the dam portion after casting, without increasing the number of processing steps. [Brief description of the drawings]

[0023] [Figure 1] FIG. 1 is an external perspective view showing an embodiment of a body of a valve according to the present invention. [Diagram 2] FIG. 2 is a cross-sectional view perpendicular to the flow passage of the body of the valve of FIG. 1. [Diagram 3]FIG. 2 is a diagram showing an example of a wax tree when the body of the valve in FIG. 1 is cast by the lost wax method. [Figure 4] FIG. 1(a) is a diagram of a body mold used in a conventional method for casting a valve body, and FIG. 1(b) is a diagram of a body mold used in the method for casting a valve body of the present invention. [Diagram 5] FIG. 2 is a schematic diagram for explaining a process in which molten metal poured into a body mold used in the casting method for the valve body of the present invention solidifies. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0024] An embodiment of the valve body of the present invention and a method for manufacturing the same will be described in detail below with reference to the drawings. Figure 1 is a perspective view showing the appearance of a main body of a ball valve, which is an embodiment of the valve body of the present invention, and Figure 2 is a cross-sectional view perpendicular to the flow path of the main body of the ball valve of Figure 1.

[0025] According to Figure 1, the main body 1 has a mounting portion 4 with a cylindrical neck portion 3 protruding in a direction perpendicular to a cylindrical body 2, and a dam portion 6, which is the mark of a pouring spout used during casting (for convenience in the following description, referred to as "dam portion 6"), is formed in a raised state on the cylindrical surface 5 of the body 2, and a first region 7, which is raised from the cylindrical surface 5, is formed between the dam portion 6 and the neck portion 3.

[0026] In addition, the dam portion 6 is formed wider than the base portion 8 of the neck portion 3, and the width of the first region 7 is formed so as to gradually increase from the dam portion 6 toward the base portion 8 of the neck portion 3.

[0027] Furthermore, according to Figure 2, the thickness of the body 2 in the first region 7 between the dam portion 6 and the neck portion 3 is formed to be thicker than the thickness of other regions of the body 2, at least the thickness of the region 8 at the base of the neck portion 3, and the thickness of the body in the first region 7 in this thickened state is formed so as to gradually increase from the region 8 at the base of the neck portion 3 toward the dam portion 6.

[0028] Furthermore, by providing the first region 7, as shown in FIG. 2, the thickness of the body 2 in the area of ​​the first region 7 is thicker than the thickness of other areas of the body 2, and gradually increases from the area 8 at the base of the neck portion 3 toward the dam portion 6, and as shown in FIG. 1, the width of the first region 7 also gradually increases from the area 8 at the base of the neck portion 3 toward the dam portion 6.

[0029] Therefore, the thickness of the first region 7 gradually increases from the region 8 at the base of the neck portion 3 toward the dam portion 6, and the width of the first region 7 gradually increases from the region 8 at the base of the neck portion 3 toward the dam portion 6. Note that the dam portion 6 shown in Fig. 2 is the remaining portion when the body 1 is separated from the runner at the dam portion after casting, and therefore the thickness of the dam portion 6 at the time of casting is even thicker than the thickness of the first region 7.

[0030] In this manner, in the body of the valve of the present invention, as shown in FIG. 2, the thickness of the body in the first region 7 is formed to be thicker than the thickness of the region 8 at the base of the neck portion 3. As a result, the portion of the body in the first region 7 is more difficult to cool during casting than other portions. Therefore, at least the region 8 at the base of the neck portion 3 is not cooled faster than the body portion including the first region 7. Therefore, the region 8 at the base of the neck portion 3 becomes the final solidification portion, thereby suppressing the generation of shrinkage cavities.

[0031] In addition, the first region 7 is provided and connected to the dam portion 6 in a state in which the thickness and width gradually increase from the base portion 8 of the neck portion 3 toward the dam portion 6. Therefore, when the molten metal is cooled, directional solidification is promoted from the base portion 8 of the neck portion 3 toward the dam portion 6, making it easier for the final solidification portion of the molten metal to occur in the dam portion 6. This makes it possible to suppress the occurrence of shrinkage cavities not only in the base portion 8 of the neck portion 3 but throughout the entire body 1.

[0032] Next, a method for manufacturing the valve body of the present invention will be described with reference to the drawings, in which the body of the ball valve described above is cast by the lost wax method.

[0033] In the manufacturing method of the valve body of the present invention, the pouring port used during casting is positioned offset from the position that will become the neck, and the height of the molten metal passage in a first region from the pouring port to the position that will become the base of the neck is formed higher than the height of the other regions, and a body mold for body casting is used in which the height of the molten metal passage is gradually decreased from the pouring port toward the position that will become the base of the neck.

[0034] When manufacturing a valve body using such a body mold by the lost wax process, first, a wax prototype 14 for the body is manufactured. The wax prototype 14 has the same shape as the body to be manufactured, except for a gate provided on the surface of the body that serves as a pouring port during casting, and is manufactured from pattern wax using a specified mold and core.

[0035] After producing the required number of these wax patterns 14, a wax tree 11 is manufactured as shown in Fig. 3. The wax tree 11 is prepared by previously producing a portion 12 that will become the sprue gate during casting and a portion 13 that will become the runner using pattern wax, and the wax pattern 14 is joined to the portion 13 that will become the runner via a dam (not shown) using an electric heating iron or adhesive wax to form a tree shape.

[0036] Next, the surface of the wax tree 11 is coated with a material (such as ceramic) that will become the mold, and then dried. The wax tree inside is melted and dewaxed at high temperature to form a mold with a space of the same shape as the wax tree inside. The mold is then fired as necessary to complete the casting mold. The casting mold contains the same number of body molds as the wax master patterns 14 used.

[0037] Molten metal made from the raw materials for the body (stainless steel, cast iron, brass alloy, etc.) is poured into the casting mold obtained in this way through the sprue, and then the molten metal is poured into each of the multiple body molds through the runner and the weir. After that, when the molten metal cools and solidifies, the casting mold is broken by applying vibration or impact, and the casting inside is taken out, and a casting with the same shape as the wax tree is obtained, and the cast body is separated from this casting at the weir to obtain the main body of the ball valve cast into the specified shape.

[0038] In the casting of the main body including the lost wax method, the molten metal is introduced from a sprue into a runner in a casting mold, and the molten metal is poured into the body mold via a dam. In a conventional body mold 15 shown in Fig. 4(a), a casting space 16 is formed so that the wall thickness of the cylindrical body is approximately constant, and a casting space 17 is formed so that the wall thickness of the cylindrical mounting part is also approximately constant, and the connection part between the casting space 16 and the casting space 17 is an intersection part 18 with an L-shaped cross section. In addition, a dam part 19 is provided at a position rotated 90 degrees in the circumferential direction of the cylinder of the body from a position 20 which is the base of the neck part.

[0039] As described above, in casting, such intersections 18 are difficult to cool and solidify and tend to become the final solidification part, so that the final solidification part tends to have casting defects such as shrinkage cavities 21. This is because when the molten metal is cooled and starts to solidify, its volume shrinks and the amount of shrinkage is compensated for by the surrounding molten metal, but as the solidification of the molten metal progresses, the same phenomenon occurs sequentially, so that the final solidification part, which solidifies last, cannot compensate for the molten metal from the surroundings and the amount of shrinkage remains as a void.

[0040] In contrast, in the manufacturing method of the valve body of the present invention, as shown in FIG. 4(b), the pouring port (dam portion 26) used during casting is positioned offset from position 27 which becomes the base of the neck, and the height of the molten metal passage (casting space) 31 in the first region 30 from the pouring port to position 27 which becomes the base of the neck is formed higher than the height of the casting space in other regions, so that the height of the molten metal passage 31 gradually decreases from the pouring port toward position 27 which becomes the base of the neck.

[0041] Therefore, when the molten metal is poured from the weir portion 26 into the casting space in the body mold 25 and then sequentially cooled and solidified, directional solidification of the molten metal can be promoted from the part 27 which becomes the base of the neck portion toward the weir portion 26. As a result, the intersection, which was likely to be the final part to solidify in the past, does not become the final part to solidify, making it possible to suppress the occurrence of casting defects such as shrinkage cavities which were likely to occur in this part.

[0042] In addition, in the body mold 25 used in the manufacturing method of the valve body of the present invention, the dam portion 26 is provided closer to the position 27 of the base of the neck portion than a position rotated 90 degrees in the circumferential direction of the cylinder of the body from the position 27 of the base of the neck portion. By providing the dam portion 26 closer to the position 27 of the base of the neck portion in this manner, the molten metal can be quickly fed from the dam portion 26, which is the pouring port into the body mold 25, into the casting space of the position 27 of the base of the neck portion, so that the molten metal can be solidified faster than in other parts, and since it is advantageous to replenish the molten metal from the dam portion 26 to the neck portion during shrinkage due to solidification, it becomes easier to suppress the occurrence of shrinkage cavities at the position 27 of the base of the neck portion.

[0043] In particular, in the body mold 25 used in the manufacturing method of the valve body of the present invention, there are no noticeable intersections other than at the portion 27 which becomes the base of the neck portion, and therefore the dam portion 26, which has the greatest thickness, is likely to become the portion that solidifies last, and casting defects such as shrinkage cavities can occur in the dam portion 26. For this reason, when the casting is removed from the casting mold after the molten metal has completely solidified and each body main body is separated from the casting, if the separation is performed at the dam portion so that no shrinkage cavities remain in the dam portion remaining in the body main body, a body main body cast with high precision can be obtained.

[0044] In the lost wax process, the same mold or other tools are used to produce the wax model, and the dam portions of all of the wax models are therefore positioned closer to the base of the neck than the position rotated 90 degrees circumferentially around the cylinder of the body from the position that would be the base of the neck. This allows the molten metal to be delivered quickly to the base of the neck of all bodies to be cast, and to solidify faster than in other areas, making it easier to suppress the occurrence of shrinkage cavities at the base of the neck.

[0045] 5(a) to 5(e), the process by which the molten metal poured into the body mold 25 solidifies will be described in more detail below. In the drawings, the area hatched with diagonal lines from the upper right to the lower left indicates an area where the molten metal has not yet solidified, and the area hatched with diagonal lines from the upper left to the lower right indicates an area where the molten metal has been cooled and solidified.

[0046] As shown in (a), when molten metal is poured into body mold 25 as shown by arrow 32 from a runner in a casting mold (not shown) through weir section 26, which is a pouring port to body mold 25, the molten metal flows through molten metal passages 31 and 33 in body mold 25 toward the bottom side of body mold 25 as shown by arrows 34 and 35.

[0047] Next, as shown in (b), the molten metal 37 flowing into the bottom side of the body mold 25 is cooled and solidified, so that it gradually shrinks toward the bottom side of the mold as shown diagrammatically by the arrow 38.

[0048] As shown in (c), when the molten metal has been poured into all of the casting space and weir portion 26 in body mold 25, the height of molten metal path 31 in body mold 25 is formed to be higher than the height of other areas, and the height of molten metal path 31 is gradually decreased from weir portion 26, which is the pouring port, toward portion 27 at the base of the neck portion. As a result, directional solidification of the molten metal poured into body mold 25 is promoted from portion 27 at the base of the neck portion toward weir portion 26.

[0049] In particular, when viewed in the thickness direction, the molten metal solidifies from the vicinity of the front and back surfaces (the surfaces in contact with the mold), and the vicinity of the center in the thickness direction solidifies last. Therefore, at the intersection of the region 27 at the base of the neck, solidification proceeds from the outside first, and the vicinity of the center may become closed. When this happens, it becomes impossible to replenish the molten metal from the dam portion 26 to the vicinity of the center, and shrinkage cavities occur. In contrast, in the present invention, the height of the molten metal passage 31 gradually increases from the region 27 at the base of the neck toward the dam portion 26, so that the vicinity of the center of the intersection is less likely to be closed in the solidification region, and the occurrence of shrinkage cavities is easily suppressed.

[0050] As a result, unsolidified molten metal 40 remains in the upper casting space of the body mold 25 including the weir portion 26, but as the molten metal 41 in the casting space below it solidifies sequentially, it shrinks toward the bottom of the mold as shown diagrammatically by arrow 43. In this way, the molten metal solidifies most slowly in the weir portion 26, which becomes the last part to solidify, so that the molten metal 40 in the weir portion 26 moves from the weir portion 26 to the solidified part in the body mold 25 to make up for the shrinkage.

[0051] As shown in (d), when the molten metal in the body mold 25 is cooled and completely solidified, the weir portion 26, which has become the last solidified part, cannot be replenished with molten metal from the surrounding area, and as a result, casting defects such as shrinkage cavities 45 and blowholes 46 occur in the upper part of the weir portion 26.

[0052] However, by cutting the cast body at the dam portion 26 along the cutting line 47, the area where the casting defect occurred is no longer included in the body, so that a sound body without casting defects can be obtained, as shown in (e).

[0053] As described above, according to the method for manufacturing a valve body of the present invention, a conventional problem in which casting defects such as shrinkage cavities were likely to occur at the base of the neck (intersection) because the molten metal solidified more slowly during casting at the base of the neck than at the surrounding area has been solved by providing a first region on the cylindrical surface of the body that promotes directional solidification from the base of the neck toward the dam section. Therefore, it is possible to obtain a highly precisely cast body by simply cutting the body at the dam section after casting without any additional processing.

[0054] The metallic material for manufacturing the valve body of the present invention is not particularly limited as long as it is a castable metallic material. In particular, stainless steel is particularly effective as a metallic material for applying the valve body and manufacturing method of the present invention, since it is necessary to cast stainless steel at high temperatures among metallic materials, it is easily cooled and solidified in the mold, and there is almost no volume expansion due to graphite crystallization during cooling and solidification, and therefore stainless steel is a metallic material in which shrinkage cavities are likely to occur in the final solidified portion.

[0055] In the explanation of the manufacturing method of the present invention, casting by the lost wax method has been taken as an example. However, the manufacturing method of the present invention is equally effective in preventing the occurrence of shrinkage cavities at the base of the neck when the valve body is manufactured by a casting method other than the lost wax method.

[0056] Furthermore, the shape of the valve body is not limited to the one-piece type as in this embodiment, but may also be two or more pieces. In order to prevent the intersection from becoming the final solidification part, the thickness from the pouring spout to the intersection is gradually reduced toward the intersection, making it possible to similarly suppress the occurrence of shrinkage cavities.

[0057] Furthermore, in the above example, the first region has a gradually thinner thickness and a gradually narrower width from the dam portion to the base of the neck portion, but it is not necessary to satisfy both of these conditions, and the thickness may be gradually thinner or the width may be gradually narrowed. Alternatively, as long as the cross-sectional area of ​​the first region satisfies the condition that it becomes gradually smaller from the dam portion to the neck portion, it may be possible to suppress the occurrence of shrinkage cavities in the base of the neck portion even if the thickness of the first region does not gradually become thinner or the width does not gradually become narrower. [Explanation of symbols]

[0058] 1. Body 2 Body 3 Neck 4. Shaft mounting 5 Cylindrical Surface 6 Remains of the dam 7 First area 8. Base of neck

Claims

1. 1. A valve body comprising a cylindrical body having a neck portion protruding in a transverse direction relative to the body and provided with an axle mounting portion, wherein, during casting of the body, a trace of a dam portion which serves as a pouring port during casting is disposed closer to the root of the neck portion than a position rotated 90 degrees circumferentially around the cylinder of the body from the root of the neck portion, and further, the trace of the dam portion is formed in a raised state on the cylindrical surface of the body, and the thickness of a first region which is the region from the trace of the dam portion to the neck portion is formed thicker than the thickness of other regions of the body, and the thickness of the first region in the thickened state is gradually reduced from the trace of the dam portion toward the root of the neck portion.

2. 2. The valve body according to claim 1, wherein the thickness of the body in the first region is greater than at least a portion of the base of the neck portion.

3. A valve body comprising a cylindrical body having a neck portion protruding in a transverse direction to provide an axle mounting portion, wherein, during casting of the body, a trace of a dam portion, which is a pouring port during casting, is formed in a raised state on the cylindrical surface of the body, and the thickness of a first region, which is the portion between the trace of the dam portion and the neck portion, is formed to be thicker than the thickness of other regions of the body, and the thickness of the first region in this thick state is formed so as to gradually become thinner from the trace of the dam portion toward the portion at the base of the neck portion, and further, the width of the first region is formed so as to gradually become narrower from the trace of the dam portion toward the base of the neck portion.

4. A valve body comprising a cylindrical body having a neck portion protruding in a transverse direction and provided with an axle mounting portion, wherein, during casting of the body, a trace of a dam portion, which is a pouring port during casting, is formed in a raised state on the cylindrical surface of the body, and the thickness of a first region, which is the portion between the trace of the dam portion and the neck portion, is formed to be thicker than the thickness of other regions of the body, and the thickness of the first region in its thick state is formed to gradually become thinner from the trace of the dam portion toward the portion at the base of the neck portion, and further, the trace of the dam portion is formed to be wider than the portion at the base of the neck portion.

5. 1. A method for manufacturing a valve body having a cylindrical body with a neck portion protruding in a transverse direction to the body and provided with a mounting portion, wherein a pouring port used in casting using a mold is positioned closer to the root of the neck portion than a position rotated 90 degrees circumferentially around the cylinder of the body from the root of the neck portion, and is offset from the position that will become the neck portion, and further, the pouring port is formed in a raised state on the cylindrical surface of the body, and the height of a molten metal path in a first region from the pouring port to the root of the neck portion is higher than the heights of other regions, and the height of the molten metal path from the pouring port to the root of the neck portion is gradually reduced from the pouring port toward the root of the neck portion, thereby suppressing shrinkage cavities from occurring in the valve body during casting using the mold.

Citation Information

Patent Citations

  • Manufacture of mold

    JP1981102347A

  • globe valve box

    JP1993028549U

  • As cast valve body in ball valve

    JP1993050209A