Per- and polyfluoroalkyl compound sampler

The sampler addresses the challenge of incomplete collection and quantification of volatile and semi-volatile per- and polyfluoroalkyl compounds by employing a multi-area design with optimized activated carbon filters, ensuring efficient and accurate measurement of these compounds in the atmosphere.

JP7560052B2Active Publication Date: 2024-10-02NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCE & TECHNOLOGY +1
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2020193453
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-12-05
Filing Date
2020-11-20
Publication Date
2024-10-02
Estimated Expiration
2040-11-20

AI Technical Summary

Technical Problem

Existing samplers are unable to efficiently collect and quantify volatile and semi-volatile per- and polyfluoroalkyl compounds in the atmosphere due to limitations in adsorption and desorption capabilities, leading to incomplete and inaccurate measurements.

Method used

A sampler with multiple collection areas: particle-adsorbing, semi-volatile, and volatile compound collection areas, utilizing inertial impactors, urethane foam filters, and activated carbon filters, optimized for BET surface area, pore volume, and surface oxide amounts to separate and collect per- and polyfluoroalkyl compounds effectively.

Benefits of technology

The sampler achieves comprehensive collection and accurate quantification of per- and polyfluoroalkyl compounds in various forms by minimizing co-elution and improving adsorption performance, allowing for precise measurement of each compound form.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007560052000032
    Figure 0007560052000032
  • Figure 0007560052000033
    Figure 0007560052000033
  • Figure 0007560052000034
    Figure 0007560052000034
Patent Text Reader

Abstract

To provide a per- and polyfluoroalkyl compound collection sampler that can collect per- and polyfluoroalkyl compounds existing in the air in various forms efficiently and generally.SOLUTION: A per- and polyfluoroalkyl compound collection sampler includes: a suction part for sucking sample air; a particle-adsorbing compound collection area connected to the suction part, and including an inertial impactor part for collecting particle-adsorbing per- and polyfluoroalkyl compounds; a semi-volatile compound collection area connected to the particle-adsorbing compound collection area, and including an urethane foam filter part for collecting semi-volatile per- and polyfluoroalkyl compounds; a volatile compound collection area connected to the semi-volatile compound collection area, and including a filter part comprising absorptive activated carbon where the BET specific surface area for collecting volatile per- and polyfluoroalkyl compounds is 900 m2 / g or more; and an exhaust part connected to the volatile compound collection area, and exhausting the air ventilating each area.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a sampler for collecting per- and polyfluoroalkyl compounds, which collects various forms of per- and polyfluoroalkyl compounds present in the atmosphere. [Background technology]

[0002] Per- and polyfluoroalkyl compounds are fluorine-substituted aliphatic compounds that have high thermal stability, high chemical stability, and high surface modification activity. Taking advantage of these properties, per- and polyfluoroalkyl compounds are widely used in industrial and chemical applications such as surface treatment agents, packaging materials, and liquid fire extinguishing agents.

[0003] Some per- and polyfluoroalkyl compounds are very stable chemical substances and are difficult to decompose under natural conditions after being released into the environment. For this reason, in recent years, per- and polyfluoroalkyl compounds have been recognized as persistent organic pollutants (POPs), and the production and use of perfluorooctane sulfonate (PFOS) (IUPAC name: 1,1,2,2,3,3,4,4,5,5,6,6,7,7,8,8,8-heptadecafluorooctane-1-sulfonic acid) has been restricted since 2010 under the Stockholm Convention on Persistent Organic Pollutants (POPs Convention).

[0004] Perfluoroalkyl compounds have a completely fluorinated linear alkyl group and are represented by the chemical formula (ii). Examples include perfluorooctane sulfonic acid (PFOS) and perfluorooctanoic acid (PFOA) (IUPAC name: 2,2,3,3,4,4,5,5,6,6,7,7,8,8,8-pentadecafluorooctanoic acid).

[0005]

number

[0006] A polyfluoroalkyl compound is a compound in which some of the hydrogen atoms in an alkyl group are replaced with fluorine, and is represented by the chemical formula (iii). For example, there is fluorotelomer alcohol.

[0007]

number

[0008] Thus, since per- and polyfluoroalkyl compounds continue to remain in nature (in water, soil, and air), the establishment of a quantitative test method for per- and polyfluoroalkyl compounds is being considered. The challenge in the study of a quantitative test method is the development of a sampler with high collection, adsorption, and desorption performance for per- and polyfluoroalkyl compounds. Air, which is a sample containing trace amounts of per- and polyfluoroalkyl compounds, is ventilated, and various forms of per- and polyfluoroalkyl compounds (particle-adsorbing, semi-volatile, volatile) contained in the sample air are collected or adsorbed, and the compounds are desorbed from the collector or adsorbent into an extract by an extraction process and concentrated. After concentration, quantitative measurement is performed using a measuring device such as LC-MS or GC-MS, making it possible to measure the concentration of per- and polyfluoroalkyl compounds contained in the sample.

[0009] A method using a high-volume air sampler is known for measuring per- and polyfluoroalkyl compounds in the air (see, for example, Non-Patent Document 1). In this method, a filter paper made of fine fibers such as quartz fiber filter paper is attached inside the high-volume air sampler, and the sampler is allowed to circulate for a certain period of time to collect airborne particles, thereby measuring the PFOS contained in the airborne particles.

[0010] However, the substances that can be collected by passing air through the filter paper are limited to non-volatile ionic compounds such as PFOS and PFOA, which are perfluoroalkyl compounds that adsorb to airborne particles. Per- and polyfluoroalkyl compounds that cannot be collected by this sampler include volatile compounds. Volatile per- and polyfluoroalkyl compounds pass through the filter paper, making it impossible to perform quantitative measurements.

[0011] For this reason, there was a demand for a collection sampler that could collect per- and polyfluoroalkyl compounds that exist in other forms, such as volatile polyfluoroalkyl compounds that are not contained in airborne particles and cannot be collected by the sampler.

[0012] In addition, silica gel-based collectors and the like are used as collectors for volatile per- and polyfluoroalkyl compounds. For example, an organic fluorine-based compound adsorbent made of cyclodextrin polymer has been proposed (Patent Document 1). This adsorbent is specialized only for adsorption and cannot desorb the compounds, so it is not suitable for use as a collector for quantitative measurement. In addition, cyclodextrin polymers are powdery or particulate, which makes them difficult to handle, and has high resistance when passing liquid or air, resulting in problems such as the risk of fine powder leaking to the secondary side. As such, there was a problem that existing adsorbents could not sufficiently collect volatile per- and polyfluoroalkyl compounds, making it impossible to perform accurate quantitative measurement. [Prior art documents] [Patent documents]

[0013] [Patent Document 1] JP 2012-101159 A [Non-patent literature]

[0014] [Non-Patent Document 1] Michiko Kotani et al., "Weekly Changes in Perfluorooctane Sulfonate (PFOS) Concentrations in Urban Air," Journal of the Japan Society for Atmospheric Environment, Vol. 45, No. 6, November 10, 2010, pp. 279-282 Summary of the Invention [Problem to be solved by the invention]

[0015] The present invention has been made in consideration of the above points, and provides a per- and polyfluoroalkyl compound collection sampler that can efficiently and comprehensively collect per- and polyfluoroalkyl compounds present in the atmosphere in various forms. [Means for solving the problem]

[0016] That is, the first invention is a sampler for collecting per- and polyfluoroalkyl compounds in a sample air, comprising an intake section for sucking in the sample air, a particle-adsorbent compound collection area connected to the intake section and having an inertial impactor section for collecting particle-adsorbent per- and polyfluoroalkyl compounds in the air, a semi-volatile compound collection area connected to the particle-adsorbent compound collection area and having a urethane foam filter section for collecting semi-volatile per- and polyfluoroalkyl compounds in the air, and a filter section having a BET specific surface area of ​​900 m2 connected to the semi-volatile compound collection area for collecting volatile per- and polyfluoroalkyl compounds in the air. 2 The present invention relates to a per- and polyfluoroalkyl compound collection sampler, comprising: a volatile compound collection area having a filter section made of activated carbon with an adsorption capacity of 1000 mPa (1 / g) or more; and an exhaust section connected to the volatile compound collection area, through which the atmospheric air that has been ventilated through each of the areas is exhausted.

[0017] The second invention relates to a per- and polyfluoroalkyl compound collection sampler according to the first invention, in which the particle-adsorbing compound collection area is composed of multiple layers of the inertial impactor section which sequentially collects particulate per- and polyfluoroalkyl compounds in the atmosphere in multiple particle sizes in descending order of particle diameter.

[0018] A third invention relates to a sampler for collecting per- and polyfluoroalkyl compounds according to the first or second invention, wherein the amount of surface oxides on the adsorbent activated carbon is 0.10 meq / g or more.

[0019] The fourth invention is the method according to any one of the first to third inventions, further comprising: mic) is 0.35 cm 3 / g or more for per- and polyfluoroalkyl compound collection samplers.

[0020] The fifth invention is the first to 3 In any one of the above-mentioned inventions, the sum of the mesopore volumes of 2 to 60 nm of the adsorbent activated carbon (V met ) is 0.02 cm 3 / g or more for per- and polyfluoroalkyl compound collection samplers.

[0021] The sixth invention relates to the fourth invention, wherein the sum of the mesopore volumes of 2 to 60 nm of the adsorbent activated carbon (V met ) is 0.02 cm 3 / g or more for per- and polyfluoroalkyl compound collection samplers.

[0022] No. 7 The invention is 6 In the invention of the present invention, the sum of the micropore volumes (V mic ) and the sum of the mesopore volume (V met ) and the volume difference (V s ) is 0.45 or more.

[0023]

number

[0024] According to the first invention, the per- and polyfluoroalkyl compound collection sampler is a sampler for collecting per- and polyfluoroalkyl compounds in a sample air, the sampler comprising an intake section for sucking in the sample air, a particle-adsorbent compound collection area having an inertial impactor section connected to the intake section for collecting particle-adsorbent per- and polyfluoroalkyl compounds in the air, a semi-volatile compound collection area having a urethane foam filter section connected to the particle-adsorbent compound collection area for collecting semi-volatile per- and polyfluoroalkyl compounds in the air, and a filter section having a BET specific surface area of ​​900 m2 connected to the semi-volatile compound collection area for collecting volatile per- and polyfluoroalkyl compounds in the air. 2 The apparatus includes a volatile compound collection area having a filter section made of activated carbon with an adsorption capacity of 10000 ppm or more and an exhaust section connected to the volatile compound collection area and through which the air that has been ventilated through each area is exhausted, so that per- and polyfluoroalkyl compounds present in the air in various forms can be efficiently and comprehensively collected. In addition, since per- and polyfluoroalkyl compounds are selectively collected in each area according to their various forms, by collecting them separately from other forms of per- and polyfluoroalkyl compounds, analytical errors due to co-elution in the measuring device can be minimized, and highly accurate quantitative measurement can be performed.

[0025] According to the per- and polyfluoroalkyl compound collection sampler of the second invention, in the first invention, the particle-adsorbing compound collection area is composed of multiple layers of the inertial impactor section which sequentially collects particulate per- and polyfluoroalkyl compounds in the atmosphere in multiple particle sizes in descending order of particle diameter, so that particulate per- and polyfluoroalkyl compounds in the atmosphere can be efficiently collected in any particle size.

[0026] According to the per- and polyfluoroalkyl compound collection sampler of the third invention, in the first or second invention, the surface oxide amount of the adsorbent activated carbon is 0.10 meq / g or more, so that it not only has the adsorption performance due to the pores of the activated carbon, but also has chemical adsorption ability, thereby further improving the adsorption performance of per- and polyfluoroalkyl compounds.

[0027] According to the fourth aspect of the present invention, in any one of the first to third aspects of the present invention, the sum of the micropore volumes of the adsorbent activated carbon of 1 nm or less (V mic ) is 0.35 cm 3 / g or more, the adsorption performance of the per- and polyfluoroalkyl compounds by the pores of the adsorbent activated carbon can be improved.

[0028] According to the fifth aspect of the present invention, the per- and polyfluoroalkyl compound collection sampler is 3 In any one of the above-mentioned inventions, the sum of the mesopore volumes of 2 to 60 nm of the adsorbent activated carbon (V met ) is 0.02 cm 3 / g or more, the adsorption performance of the per- and polyfluoroalkyl compounds by the pores of the adsorbent activated carbon can be improved.

[0029] According to the sixth aspect of the present invention, there is provided a per- and polyfluoroalkyl compound collection sampler, which is the same as the fourth aspect of the present invention, except that the sum of the mesopore volumes of the adsorbent activated carbon having a diameter of 2 to 60 nm (V met ) is 0.02 cm 3 / g or more, the adsorption performance of the per- and polyfluoroalkyl compounds by the pores of the adsorbent activated carbon can be improved.

[0030] No. 7 According to the per- and polyfluoroalkyl compound collection sampler of the present invention, 6 Inventions In the above, the sum of the micropore volumes (V mic ) and the sum of the mesopore volume (V met ) and the volume difference (V s ) is 0.45 or more, the adsorption performance of the per- and polyfluoroalkyl compounds by the pores of the adsorbent activated carbon can be improved. [Brief description of the drawings]

[0031] [Figure 1] FIG. 1 is a perspective view showing one embodiment of a per- and polyfluoroalkyl compound collection sampler of the present invention. [Diagram 2] FIG. 2 is a central cross-sectional view of the sampler of FIG. 1. [Diagram 3] FIG. 3 is an enlarged view of the upper part of FIG. [Figure 4] FIG. 2 is a plan view showing an example of the shape of an impactor plate. [Diagram 5] FIG. 3 is an enlarged view of the lower part of FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0032] The purpose of the per- and polyfluoroalkyl compound collection sampler is to comprehensively collect per- and polyfluoroalkyl compounds that exist in various forms in the atmosphere. Per- and polyfluoroalkyl compounds present in the atmosphere are roughly classified into three types. One type is particle-adsorbed per- and polyfluoroalkyl compounds that adhere to the surface of fine particles (e.g., dust such as pollen and soil particles) suspended in the air, and most of these are ionic compounds.

[0033] The second type is semi-volatile per- and polyfluoroalkyl compounds such as N-ethylperfluorooctanesulfonic acid amidoethanol (hereinafter referred to as "N-EtFOSE") and N-methylperfluorooctanesulfonic acid amidoethanol (hereinafter referred to as "N-MeFOSE"). According to the definition of the World Health Organization (WHO), semi-volatile organic compounds are compounds with a boiling point of 260 to 380°C. It is known that PFOS and PFOA are produced by the decomposition of semi-volatile per- and polyfluoroalkyl compounds. N-EtFOSE is a substance represented by the following chemical formula (iv), and N-MeFOSE is a substance represented by the chemical formula (v).

[0034]

number

[0035]

number

[0036] The third type is volatile per- and polyfluoroalkyl compounds that exist as gases in the atmosphere, such as fluorotelomer alcohols (hereinafter referred to as "FTOHs") as shown in the above-mentioned chemical formula (iii). Volatile organic compounds are defined by the World Health Organization (WHO) as compounds with a boiling point of 50 to 160°C.

[0037] As described above, the per- and polyfluoroalkyl compounds, which are the subject of the present invention, exist in the atmosphere mainly in three forms. For this reason, the sampler of the present invention is formed by dividing it into areas for collecting per- and polyfluoroalkyl compounds in each form, as shown in Figures 1 and 2.

[0038] The sampler 10 of the present invention is formed by arranging a particle-adsorbent compound collection area 20, a semi-volatile compound collection area 30, and a volatile compound collection area 40 in this order from the upstream where the sample air is sucked in to the downstream where the air is discharged. The sample air is sucked in from the intake section 12 by a suction pump or the like arranged on the downstream side of the sampler, passes through the particle-adsorbent compound collection area 20 that collects particle-adsorbent per- and polyfluoroalkyl compounds, then passes through the semi-volatile compound collection area 30 that collects semi-volatile per- and polyfluoroalkyl compounds, and then passes through the volatile compound collection area 40 that collects volatile per- and polyfluoroalkyl compounds, before being discharged from the exhaust section 13.

[0039] First, the particle-adsorbent compound collection area 20 will be described with reference to Figures 3 and 4. The particle-adsorbent compound collection area 20 includes an inertial impactor portion 21 that collects particle-adsorbent per- and polyfluoroalkyl compounds in the atmosphere.

[0040] An inertial impactor is used to collect fine particles (aerosols) suspended in gas, by passing particles from a nozzle toward an impactor plate (collection plate) and collecting the particles on the impactor plate by colliding them with the impactor plate by inertial force. Also, by connecting inertial impactors with different nozzle diameters in multiple stages, it becomes possible to collect particles of different particle diameters on the impactor plate of each stage.

[0041] The inertial impactor section 21 is provided with a collecting filter paper 22 in the center of a disk-shaped object, an impactor plate 23 with a plurality of through holes 24 formed on its outer periphery, a clearance section 25 on the upstream side of the impactor plate 23, and a connecting hole 27 on the downstream side. The inertial impactor section 21 classifies and collects fine particles (aerosols) by using inertial force. By suddenly changing the direction of the airflow of the sample air flowing in from the upstream side, particles with a certain particle size or larger are collided with the collecting filter paper by utilizing the particle size dependency of the inertial motion of the fine particles, and the fine particles are collected. In the inertial impactor section, the fine particles and gas do not pass through the filter paper, so that the material exchange between the collected particles on the filter paper and the gas being aerated, which is a concern in the existing method where the particles pass through the filter paper, is minimized.

[0042] In addition, it is preferable that the inertial impactor section 21 is arranged in a plurality of layers. The size of the fine particles that can be collected can be appropriately adjusted by the shape, diameter size, distance to the lower plate, etc. of the through-hole 24 formed in the impactor plate 23. For example, the shape of the through-hole 24 formed in the impactor plate 23 can be a shape as shown in FIG. 4. Therefore, it is possible to collect fine particles of different particle sizes in each layer. In this case, if the inertial impactor section 21 is arranged in a plurality of layers so that the fine particles are collected in order of the particle diameter from the upstream side to the downstream side, the collection efficiency is increased. Furthermore, it is preferable that the downstream side of the impactor plate 23 has an acceleration nozzle 26 that accelerates the airflow formed on a taper toward the downstream side.

[0043] The sample air that flows into the clearance section from the upstream side flows toward the through-holes 24 formed in the impactor plate 23. Because the through-holes 24 in the impactor plate 23 are not arranged in a straight line from the air inflow direction, the flow path of the gas bends outward toward the through-holes 24. Particles above a certain size cannot ride the airflow that bends outward due to inertia, and collide with the collection filter paper 22 and are collected. By connecting multiple layers of inertial impactor sections, each with a modified shape of the through-hole, it is possible to collect fine particles of any particle size. A publicly known inertial impactor section 21 can be used.

[0044] In the particle-adsorbing compound collection area 20 of this embodiment, three or four inertial impactors 21 are provided, and particle-adsorbing perfluoroalkyl compounds with particle diameters of 10 μm or more, 2.5 to 10 μm, and 1.0 to 2.5 μm are collected from the upstream by the inertial impactor of each layer. In addition, in the lowest layer, a very small particle collection section 29 equipped with a collection filter paper 22 is formed on the upper surface of a disk-shaped object 28 having a plurality of through holes 24 in order to collect particle-adsorbing perfluoroalkyl compounds with particle diameters smaller than 1.0 μm. Note that the very small particle collection section 29 may be omitted depending on the purpose.

[0045] Next, the semivolatile compound collection area 30 connected to the particle-adsorbing compound collection area 20 will be described. As shown in Fig. 5, the semivolatile compound collection area 30 includes a urethane foam filter section 31 made of a urethane foam 32 that collects semivolatile per- and polyfluoroalkyl compounds. In this embodiment, the urethane foam 32 is a cylindrical polyurethane foam having a diameter of 47 mm and a length of 50 mm, which is filled in the sampler cylinder.

[0046] Next, the volatile compound collection area 40 connected to the semivolatile compound collection area 30 will be described. As shown in Fig. 5, the volatile compound collection area 40 includes a filter section 41 made of adsorbent activated carbon C that collects volatile per- and polyfluoroalkyl compounds present in a gaseous state in the atmosphere. The filter section 41 may be arranged in multiple layers.

[0047] By collecting semi-volatile per- and polyfluoroalkyl compounds in the semi-volatile compound collection area 30, which is arranged in the stage preceding the volatile compound collection area 40, it is possible to prevent the micropores of the adsorbent activated carbon C in the filter section 41 provided in the volatile compound collection area 40 from being blocked, and it is expected that deterioration of the adsorption performance will be reduced. In addition, since the urethane foam filter section 31 can remove fine particles that have slipped through the particle-adsorbing compound collection area 20, deterioration of the performance of the filter section 41 of the volatile compound collection area 40 is further suppressed.

[0048] In this way, by collecting particles (compounds adsorbed to particles), semi-volatile compounds, and volatile compounds in different areas, particle-adsorbed per- and polyfluoroalkyl compounds, semi-volatile per- and polyfluoroalkyl compounds, and volatile per- and polyfluoroalkyl compounds can be collected separately, making it possible to analyze each form of per- and polyfluoroalkyl compounds independently, preventing co-elution, reducing analytical errors in the measurement device, and improving measurement accuracy.

[0049] The per- and polyfluoroalkyl compound-adsorbing activated carbon is made of fibrous activated carbon or powdered activated carbon. The fibrous activated carbon is activated carbon obtained by carbonizing and activating appropriate fibers, such as phenol resin-based, acrylic resin-based, cellulose-based, and coal pitch-based. The fiber length and cross-sectional diameter are appropriate. If the fiber cross-sectional diameter is too large, the surface area is reduced and the contact efficiency is reduced, so from the viewpoint of improving the adsorption capacity, the fiber cross-sectional diameter is preferably 30 μm or less.

[0050] The raw materials for powdered activated carbon include wood (waste wood, thinned wood, sawdust), coffee bean residue, rice husks, coconut shells, bark, and fruit. These naturally derived raw materials are prone to developing pores through carbonization and activation. In addition, since it is a secondary use of waste, it can be procured at low cost. Other raw materials that can be used include tires, petroleum pitch, burned products derived from synthetic resins such as urethane resins and phenolic resins, and even coal. If the particle size of the activated carbon is small, the density of the filter body is high, and the adsorption performance of per- and polyfluoroalkyl compounds is improved. On the other hand, if the particle size is large, the density of the filter body is small, and the breathability is improved. For these reasons, the average particle size of the powdered activated carbon can be appropriately adjusted according to the conditions of use, and the adsorption performance of per- and polyfluoroalkyl compounds can be improved while ensuring breathability.

[0051] The activated carbon raw material is heated and carbonized at a temperature range of 200°C to 600°C as necessary to form micropores. The activated carbon raw material is then exposed to steam and carbon dioxide gas at a temperature range of 600°C to 1200°C for activation. As a result, activated carbon with various types of developed pores is produced. Other activation methods include activation with zinc chloride. Sequential washing is also performed.

[0052] The physical properties of the activated carbon thus produced determine the adsorption performance of the adsorbent. The adsorption performance of the activated carbon for adsorbing per- and polyfluoroalkyl compounds, which are the target adsorbents of the present invention, is determined by the specific surface area, which is an index showing the amount of pores formed in the activated carbon. In this specification, the specific surface area of ​​each prototype is measured by the BET method (Brunauer, Emmett and Teller method).

[0053] Activated carbon is also defined by the pore size. In the case of an adsorbent such as activated carbon, there are micropores, mesopores, and macropores. The adsorption target and performance of activated carbon change depending on which range of pores is developed more. The activated carbon desired in the present invention is one that effectively adsorbs molecules of per- and polyfluoroalkyl compounds in a desorbable manner.

[0054] In addition, acidic functional groups are present on the surface of the activated carbon. The acidic functional groups that increase due to the surface oxidation of the activated carbon are mainly hydrophilic groups such as carboxyl groups and phenolic hydroxyl groups. The acidic functional groups on the surface of the activated carbon affect the collection capacity. The amount of these acidic functional groups can be understood as the amount of surface oxide. It is believed that an increase in the amount of surface oxide of the activated carbon increases the hydrophilicity of the surface of the activated carbon, and thus improves the collection performance of per- and polyfluoroalkyl compounds, particularly fluorotelomer compounds having hydrophilic groups.

[0055] The following methods can be used to increase the amount of surface oxides in activated carbon. One method is to promote the oxidation of surface residues by undergoing a heating process again, thereby increasing acidic functional groups. That is, oxidation in an air or oxygen atmosphere. Alternatively, air at a temperature of 25 to 40°C and a humidity of 60 to 90% is also introduced at the same time in an air atmosphere. There, activated carbon with an increased amount of surface oxides can be obtained by heating at 150 to 900°C for 1 to 10 hours. It is believed that the acidic functional groups increase when the activated carbon is heated with moist air, as a result of which hydrocarbon groups such as alkyl groups present on the surface of the activated carbon being oxidized, or hydroxyl groups of water being introduced to the surface.

[0056] Another method is to oxidize the surface of activated carbon with an oxidizing agent to increase the amount of surface oxide. Examples of oxidizing agents include hypochlorous acid and hydrogen peroxide. Activated carbon with an increased amount of surface oxide can be obtained by immersing activated carbon in a liquid containing such an oxidizing agent and then drying it. The amount of acidic functional groups on the surface of the activated carbon can be measured as the amount of surface oxide, as shown in each prototype example described below.

[0057] The adsorption performance of activated carbon that adsorbs volatile per- and polyfluoroalkyl compounds in a desorbable manner is determined by the specific surface area of ​​the activated carbon being 900 m2 or more, as will be explained in the examples below. 2 / g or more. By forming a certain number of pores in the activated carbon, the adsorption performance of the compound is ensured.

[0058] It was also found that the pore distribution formed in the activated carbon also contributes to the adsorption of volatile per- and polyfluoroalkyl compounds. In this specification, the term "micropore" refers to a pore having a diameter of 1 nm or less, and as will be derived from the examples described later, the pore volume (V mic ) total is 0.35cm 3 / g or more, the adsorption performance of volatile per- and polyfluoroalkyl compounds is improved. In this specification, the micropore volume of 1 nm or less in each prototype is measured by the MP method (Micropore method). It is considered that the formation of a certain number of micropores makes it easier for the compounds to be captured in the pores.

[0059] In this specification, the term "mesopores" refers to pores having a pore diameter in the range of 2 to 60 nm, and as will be explained in the examples below, the pore volume (V met ) is 0.02cm 3 / g or more, the adsorption performance of volatile per- and polyfluoroalkyl compounds is improved. In this specification, the mesopore volume in the range of 2 to 60 nm in each prototype is measured by the DH method (Dollimore-Heal method). Since the measurement is by the DH method, the measurement targets were pores of 2.43 to 59.72 nm. It is considered that the formation of a certain number of mesopores or more allows the compound to easily penetrate into the micropores.

[0060] In addition, the difference between the pore volume of the micropores and the pore volume of the mesopores is also thought to contribute to the efficient adsorption of per- and polyfluoroalkyl compounds. As will be explained in the examples below, the sum of the micropore volumes (V mic ) and the sum of the mesopore volume (V met ) and the volume difference (V s ) is 0.45 or more, volatile per- and polyfluoroalkyl compounds can be adsorbed efficiently and desorbably. By making the activated carbon have well-developed micropores in addition to not overdeveloping mesopores, it is believed that the adsorption performance of per- and polyfluoroalkyl compounds can be improved while the compounds can be smoothly desorbed during the subsequent extraction operation, thereby enabling good quantitative measurement.

[0061] Next, by making the surface oxide amount 0.10 meq / g or more, the hydrophilicity of the activated carbon surface is increased, enabling per- and polyfluoroalkyl compounds to be adsorbed efficiently. EXAMPLES

[0062] [Study on collection performance of atmospheric per- and polyfluoroalkyl compounds 1] [Create a sampler] In order to prepare a sampler for collecting per- and polyfluoroalkyl compounds, the inventors prepared a sampler using polypropylene resin with the following composition.

[0063] Air intake section Intake hole: Inner diameter 11.0mm -Particle adsorbent collection area 1st stage: Particle adsorbent compound collection area that collects particles of 10 μm or more Clearance: Inner diameter 40mm Collection filter paper: Quartz fiber filter, diameter 25 mm Impactor plate: Shape shown in Fig. 4(a), diameter 47 mm Connection hole: Inner diameter (diameter) 4.3mm Second stage: Particle-adsorbent compound collection area that collects fine particles of 2.5 to 10 μm Clearance: Inner diameter 40mm Collection filter paper: Quartz fiber filter, diameter 25 mm Impactor plate: Shape shown in Fig. 4(a), diameter 47 mm Connection hole: Inner diameter (diameter) 2.2mm 3rd stage: Particle adsorbent compound collection area for collecting fine particles of 1.0 to 2.5 μm Clearance: Inner diameter 40mm Collection filter paper: Quartz fiber filter, diameter 25 mm Impactor plate: Shape shown in Fig. 4(a), diameter 47 mm Connection hole: Inner diameter (diameter) 40mm 4th stage: Particle adsorbent compound collection area that collects particles of 1.0 μm or less Clearance: Inner diameter 40mm Collection filter paper: Quartz fiber filter, diameter 47 mm Impactor plate: Shape shown in Fig. 4(b), diameter 47 mm Connection hole: Inner diameter (diameter) 40mm

[0064] A quartz fiber filter manufactured by Shibata Scientific Co., Ltd. was used as the collection filter paper for each particle-adsorbing compound collection area.

[0065] Semi-volatile compound collection area Urethane foam filter part: Polyurethane foam (manufactured by Shibata Scientific Co., Ltd.), diameter 47 mm, height 50 mm

[0066] Volatile Compounds Area The following adsorbent activated carbon samples 1 to 5 were used to prepare circular sheets (diameter 47 mm, thickness 2 mm), which were used as the filter section and were arranged in pairs.

[0067] [Activated carbon adsorbent used] The inventors used the following raw materials to prepare per- and polyfluoroalkyl compound-adsorbing activated carbon: · Fibrous activated carbon Futamura Chemical Co., Ltd.: Fibrous activated carbon "CF" (average fiber diameter: 15 μm) {Hereafter, this will be referred to as C1.} Futamura Chemical Co., Ltd.: Fibrous activated carbon "FE3010" (average fiber diameter: 15 μm) {Hereafter, this will be referred to as C2.} Futamura Chemical Co., Ltd.: Fibrous activated carbon "FE3012" (average fiber diameter: 15 μm) {Hereafter, this will be referred to as C3.} Futamura Chemical Co., Ltd.: Fibrous activated carbon "FE3013" (average fiber diameter: 15 μm) {Hereafter, this will be referred to as C4.} Futamura Chemical Co., Ltd.: Fibrous activated carbon "FE3015" (average fiber diameter: 15 μm) {Hereafter, this will be referred to as C5.} Futamura Chemical Co., Ltd.: Fibrous activated carbon "FE3018" (average fiber diameter: 15 μm) {Hereafter, this will be referred to as C6.} ·Granular activated carbon Futamura Chemical Co., Ltd.: Coconut shell activated carbon "CW480SZ" (average particle size: 250 μm) {Hereafter, this will be referred to as C7.} Futamura Chemical Co., Ltd.: Phenolic resin activated carbon "QW250" (average particle size: 250 μm) {Hereafter, this will be referred to as C8.}

[0068] [Activated carbon treatment] <Prototype 1> The activated carbon for prototype 1 was fibrous activated carbon "CF" (C1), which was made by carbonizing phenolic resin fiber, the same raw material as FE3010, at 600°C.

[0069] <Prototype Example 2> The fibrous activated carbon "FE3015" (C5) manufactured by Futamura Chemical was used as the activated carbon for Prototype Example 2.

[0070] <Prototype 3> 10 g of fibrous activated carbon "FE3010" (C2) manufactured by Futamura Chemical was immersed in 500 ml of a 6% hydrogen peroxide solution, left to stand for 150 hours, then taken out and dried to obtain the activated carbon of prototype 3.

[0071] <Prototype 4> 10 g of fibrous activated carbon "FE3015" (C5) manufactured by Futamura Chemical was immersed in 500 ml of a 6% hydrogen peroxide solution, left to stand for 70 hours, then removed and dried to obtain the activated carbon of prototype 4.

[0072] <Prototype 5> 10 g of fibrous activated carbon "FE3018" (C6) manufactured by Futamura Chemical was immersed in 500 ml of a 6% hydrogen peroxide solution, left to stand for 50 hours, then removed and dried to obtain the activated carbon of prototype 5.

[0073] [Measurement of adsorbent activated carbon] The amount of surface oxide (meq / g) was determined by applying the Boehm method, in which the adsorbent activated carbon of each example was shaken in a 0.05N aqueous solution of sodium hydroxide, filtered, and the filtrate was neutralized and titrated with 0.05N hydrochloric acid to obtain the amount of sodium hydroxide.

[0074] Specific surface area (m 2 / g) was determined by measuring the nitrogen adsorption isotherm at 77K using an automatic specific surface area / pore distribution analyzer "BELSORP-miniII" manufactured by Microtrack-BEL Corporation and using the BET method (BET specific surface area).

[0075] The average pore diameter (nm) is calculated by multiplying the pore volume (ml / g) and specific surface area (m2) obtained from the above measurement, assuming that the pores are cylindrical. 2 / g) according to formula (vi).

[0076]

number

[0077] The physical properties of the adsorbent activated carbon of each prototype are shown in Table 1. From the top to the bottom of Table 1, the surface oxide amount (meq / g), BET specific surface area (m 2 / g), average pore diameter (nm), and average fiber diameter (μm).

[0078] [Table 1]

[0079] [Measurement of collection efficiency of atmospheric per- and polyfluoroalkyl compounds 1] Experiments were conducted to collect atmospheric particle-adsorbent per- and polyfluoroalkyl compounds in a particle-adsorbent compound collection area, as well as semi-volatile per- and polyfluoroalkyl compounds in a semi-volatile compound collection area and volatile per- and polyfluoroalkyl compounds in a volatile compound collection area.

[0080] [Experiment 1: Collection of particulate-adsorbed per- and polyfluoroalkyl compounds] A sampler consisting of the particle-adsorbent compound collection area described in the Examples was installed outdoors and aerated for 48 hours at an airflow rate of 20 L / min, and the amount of fine particles collected on the collection filter paper at each stage of the particle-adsorbent compound collection area was measured. Table 2 shows the month of measurement and the amount of collected fine particles (μg / m) for each particle size (at each stage). 3 ) is shown.

[0081] [Table 2]

[0082] After calculating the amount of fine particles, the amounts of PFOS and PFOA attached to the fine particles collected in November 2017 were quantitatively evaluated using the following procedure.

[0083] After aeration, the collection filter papers at each stage were thoroughly contacted and stirred with 15 ml of a mixed solvent mainly composed of dichloromethane and ethyl acetate, then centrifuged to separate the solid and liquid, and the extract was collected.

[0084] The extract was quantitatively measured in MRM mode using GC-MS / MS (Waters QuatrimicroGC) to confirm the collection performance.

[0085] Table 3 shows the amount of PFOS and PFOA recovered from fine particles of each particle size (pg / m 3 ) was shown. Quantitative measurements were performed four times.

[0086] [Table 3]

[0087] [Results and considerations of particle-adsorbed per- and polyfluoroalkyl compound collection experiments 1] As shown in Tables 2 and 3, the particle adsorption compound collection area was confirmed to have the ability to collect fine particles in the air, and it was also confirmed that it was possible to quantify the PFOS and PFOA adsorbed to the fine particles.

[0088] [Experiment 1 for the collection of semi-volatile per- and polyfluoroalkyl compounds and experiment 1 for the collection of volatile per- and polyfluoroalkyl compounds] Using the above-mentioned semi-volatile compound collection area and a volatile compound collection area equipped with a filter section made of activated carbon of each prototype example, collection experiments were conducted on semi-volatile per- and polyfluoroalkyl compounds and volatile per- and polyfluoroalkyl compounds.

[0089] As per- and polyfluoroalkyl compounds, this time, FTOHs and ethyl perfluorooctanesulfamide (IUPAC name: N-ethyl-1,1,2,2,3,3,4,4,5,5,6,6,7,7,8,8,8-heptadecafluorooctane-1-sulfamide) (hereafter referred to as "N-EtFOSA") were used for the evaluation. The substance names of FTOHs vary depending on the number of carbon atoms. For example, C8F 17 In the case of CH2CH2OH, it is named 8:2FTOH (IUPAC name: 3,3,4,4,5,5,6,6,7,7,8,8,9,9,10,10,10-heptadecafluoro-1-decanol). N-EtFOSA is the substance represented by the following chemical formula (vii).

[0090]

number

[0091] Each standard substance (4:2FTOH (IUPAC name: 3,3,4,4,5,5,6,6,6-nonafluoro-1-hexanol), 6:2FTOH (IUPAC name: 3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluoro-1-octanol), 8:2FTOH, 10:2FTOH (IUPAC name: 3,3,4,4,5,5,6,6,7,7,8,8,9,9,10,10,11,11,12,12,12-heneicosafluoro-1-dodecanol), N-EtFOSA and N-EtFOSE) was diluted with methanol to 100 ppb and added in an amount of 100 μl to the urethane foam filter in the semivolatile compound collection area. Subsequently, air at 22 to 24° C. was passed through the semivolatile compound collection area and the volatile compound collection area at a rate of 20 l / min for 48 hours.

[0092] After aeration, the urethane foam filter part and the filter part made of activated carbon of each prototype were removed and thoroughly contacted and stirred with 15 ml of a mixed solvent mainly composed of dichloromethane and ethyl acetate, then centrifuged to separate the solid and liquid, and the extract was collected.

[0093] The extract was quantitatively measured in MRM mode using GC-MS / MS (Waters QuatrimicroGC) to confirm the collection performance.

[0094] Table 4 shows the recovery rate (%) for each target substance in the urethane foam filter. Quantitative measurements were performed four times. In the table, "ND" indicates that the value was below the lower limit of quantification.

[0095] [Table 4]

[0096] The recovery rate (%) of each target substance in the filter part made of activated carbon for each prototype is shown in Table 5. Quantitative measurements were performed four times.

[0097] In the table, "ND" indicates that the value was below the lower limit of quantification. In addition, there were cases where the recovery rate was 150% or more due to the coelution phenomenon in which the mass number affects the same fragment.

[0098] [Table 5]

[0099] [Results and considerations of collection experiments for semi-volatile per- and polyfluoroalkyl compounds and volatile per- and polyfluoroalkyl compounds 1] As shown in Table 4, N-EtFOSE was specifically captured in the urethane foam filter of the semivolatile compound collection area, and the recovery rate was approximately 100% in all prototype samplers. In addition, all fluorotelomer alcohols were below the detection limit in the urethane foam filter, demonstrating that the semivolatile compound collection area and volatile compound collection area are capable of selectively capturing compounds according to their physical properties.

[0100] As shown in Table 5, Prototypes 3 to 5 showed good results in terms of the collection rate of all FTOHs. In Prototype 1, the results showed that 4:2FTOH and 10:2FTOH were below the detection limit, and adsorption was not possible. In addition, the collection rates of 6:2FTOH and 8:2FTOH were both less than 10%, indicating that the adsorption performance was insufficient. In Prototype 2, the collection performance of 10:2FTOH was sufficient, but the collection performance of 4:2FTOH, 6:2FTOH, and 8:2FTOH was less than 50%, indicating that the adsorption performance was insufficient.

[0101] It is believed that Prototype 1 did not exhibit sufficient collection performance because it did not have the pores and specific surface area necessary to capture the target substances. As for Prototype 2, although the specific surface area may have been sufficient, it is believed that the various hydrophilic FTOHs could not be sufficiently captured because the surface was hydrophobic.

[0102] For prototypes 3 to 5, the collection rates of 4:2FTOH, 6:2FTOH, 8:2FTOH, and 10:2FTOH were all 50% or more, demonstrating excellent collection performance. These are all test examples in which the surface of the activated carbon was oxidized, and it is presumed that the high collection performance was achieved due to the presence or absence of the oxidation treatment, i.e., the large amount of oxide on the surface of the activated carbon.

[0103] Among them, Prototype 4 had a high collection rate of 70% or more for all of 4:2FTOH, 6:2FTOH, 8:2FTOH, and 10:2FTOH, and was confirmed to have the best collection performance.

[0104] Concerning the collection efficiency of N-EtFOSA, it was found that the collection efficiency of prototype 1 was below 50%, and it did not have sufficient collection performance. Although the collection efficiency of prototype 2 was above 50%, it was still not enough.

[0105] In all of the prototypes 3 to 5, the collection rate of N-EtFOSA exceeded 100%, and they had sufficient collection performance. The prototype 4, which has the same specific surface area as the prototype 2, suggests that the collection performance is greatly improved by oxidizing the activated carbon surface. In other words, for N-EtFOSA, the specific surface area of ​​the prototype 3 is necessary, and the increased acidic groups on the activated carbon surface make it possible to provide sufficient collection performance.

[0106] Considering each prototype overall, the collection performance of prototype 1 is insufficient for 4:2FTOH, 6:2FTOH, 8:2FTOH, and 10:2FTOH, and is not suitable as a collection material. Prototype 2 has excellent collection performance for 10:2FTOH, and may be used as a collection material exclusively for 10:2FTOH. However, from the viewpoint of collecting 4:2FTOH, 6:2FTOH, 8:2FTOH, 10:2FTOH, and N-EtFOSA in a well-balanced manner, prototypes 3 to 5 have excellent collection performance for per- and polyfluoroalkyl compounds.

[0107] As described above, the semi-volatile per- and polyfluoroalkyl compound N-EtFOSA was efficiently collected in the semi-volatile compound collection area, and the recovery rate of the compound was nearly 100%. And, since the compound was not detected in the filter part of the volatile compound collection area, it was found that the semi-volatile per- and polyfluoroalkyl compounds and the volatile per- and polyfluoroalkyl compounds can be separated and efficiently collected in each collection area.

[0108] By separating and collecting semi-volatile per- and polyfluoroalkyl compounds in the semi-volatile compound collection area arranged in front of the volatile compound collection area, clogging of the micropores of the adsorption activated carbon in the filter part of the volatile compound collection area can be prevented, and the deterioration of the adsorption performance can be reduced. In addition, by separating and collecting the compounds, it is possible to prevent the co-elution phenomenon during measurement, reduce the analytical error in the measurement device, and improve the measurement accuracy.

[0109] In this way, by collecting per- and polyfluoroalkyl compounds adsorbed to particles, semi-volatile per- and polyfluoroalkyl compounds, and volatile per- and polyfluoroalkyl compounds in different collection areas, it is possible to separate and collect each compound, and it has been found that all forms of per- and polyfluoroalkyl compounds can be measured satisfactorily.

[0110] [Study on collection performance of volatile per- and polyfluoroalkyl compounds 2] Next, the inventors used the following activated carbon prototypes 6 to 21 to reexamine the optimal transitions and collision energies for the MRM mode of GC-MS / MS ("GCMS-TQ8050", manufactured by Shimadzu Corporation), and conducted Experiment 2 on the collection of per- and polyfluoroalkyl compounds in air samples under more accurate analytical conditions.

[0111] [Activated carbon treatment 2] <Prototype Example 6> 10 g of fibrous activated carbon "CF" (C1) manufactured by Futamura Chemical Co., Ltd. was used as the activated carbon of Prototype Example 6.

[0112] <Prototype 7> 10 g of fibrous activated carbon "CF" (C1) manufactured by Futamura Chemical was immersed in 500 ml of a 4.2% hydrogen peroxide solution, left to stand for 220 hours, then removed and dried to obtain the activated carbon of Prototype Example 7.

[0113] <Prototype Example 8> 10 g of fibrous activated carbon "FE3010" (C2) manufactured by Futamura Chemical was used as the activated carbon of Prototype Example 8.

[0114] <Prototype Example 9> 10 g of fibrous activated carbon "FE3010" (C2) manufactured by Futamura Chemical was immersed in 500 ml of a 4.2% hydrogen peroxide solution, left to stand for 150 hours, then removed and dried to obtain the activated carbon of prototype 9.

[0115] <Prototype Example 10> 10 g of fibrous activated carbon "FE3012" (C3) manufactured by Futamura Chemical was used as the activated carbon of Prototype Example 10.

[0116] <Prototype Example 11> 10 g of fibrous activated carbon "FE3012" (C3) manufactured by Futamura Chemical was immersed in 500 ml of a 4.2% hydrogen peroxide solution, left to stand for 100 hours, then removed and dried to obtain the activated carbon of Prototype Example 11.

[0117] <Prototype Example 12> 10 g of fibrous activated carbon "FE3013" (C4) manufactured by Futamura Chemical was immersed in 500 ml of a 1.5% hydrogen peroxide solution, left to stand for 70 hours, then removed and dried to obtain the activated carbon of prototype 12.

[0118] <Prototype Example 13> 10 g of fibrous activated carbon "FE3015" (C5) manufactured by Futamura Chemical was used as the activated carbon for Prototype Example 13.

[0119] <Prototype Example 14> 10 g of fibrous activated carbon "FE3015" (C5) manufactured by Futamura Chemical was immersed in 500 ml of a 1.5% hydrogen peroxide solution, left to stand for 40 hours, then removed and dried to obtain the activated carbon of prototype 14.

[0120] <Prototype Example 15> 10 g of fibrous activated carbon "FE3015" (C5) manufactured by Futamura Chemical was immersed in 500 ml of a 4.2% hydrogen peroxide solution, left to stand for 70 hours, then removed and dried to obtain the activated carbon of prototype 15.

[0121] <Prototype Example 16> 10 g of fibrous activated carbon "FE3015" (C5) manufactured by Futamura Chemical was immersed in 500 ml of a 14.0% hydrogen peroxide solution, left to stand for 350 hours, then removed and dried to obtain the activated carbon of prototype 16.

[0122] <Prototype Example 17> 10 g of fibrous activated carbon "FE3015" (C5) manufactured by Futamura Chemical was immersed in 500 ml of a 18.9% hydrogen peroxide solution, left to stand for 480 hours, then removed and dried to obtain the activated carbon of prototype 17.

[0123] <Prototype Example 18> 10 g of fibrous activated carbon "FE3018" (C6) manufactured by Futamura Chemical was used as the activated carbon of Prototype Example 18.

[0124] <Prototype Example 19> 10 g of fibrous activated carbon "FE3018" (C6) manufactured by Futamura Chemical was immersed in 500 ml of a 4.2% hydrogen peroxide solution, left to stand for 50 hours, then removed and dried to obtain the activated carbon of prototype 19.

[0125] <Prototype Example 20> 10 g of coconut shell activated carbon "CW480SZ" (C7) manufactured by Futamura Chemical was immersed in 500 ml of a 4.2% hydrogen peroxide solution, left to stand for 70 hours, then removed and dried to obtain the activated carbon of prototype 20.

[0126] <Prototype Example 21> 10 g of Futamura Chemical's phenolic resin activated carbon "QW250" (C8) was immersed in 500 ml of a 4.2% hydrogen peroxide solution, left to stand for 70 hours, then removed and dried to obtain the activated carbon of Prototype Example 21.

[0127] [Measurement of adsorbent activated carbon 2] The surface oxide, specific surface area and average pore diameter of each of Prototype Examples 6 to 21 were determined in the same manner as in "Measurement of adsorbent activated carbon 1" above.

[0128] [Micropore volume] The pore volume was measured by nitrogen adsorption using an automatic specific surface area / pore distribution measuring device ("BELSORP-miniII", manufactured by Microtrack Bell Co., Ltd.). The sum of the micropore volumes (V mic )(cm 3 / g) was calculated by analyzing the dV / dD value in the range of pore diameters of 1 nm or less from the t-plot of the nitrogen gas adsorption isotherm using the MP method.

[0129] [Mesopore volume] The value of dV / dD in the range of pore diameters from 2 to 60 nm was analyzed by the DH method from the nitrogen gas adsorption isotherm. The diameter range of pore diameters from 2 to 60 nm in the analysis software is 2.43 to 59.72 nm. From the analysis results, the sum of the mesopore volumes (V met )(cm 3 / g) was calculated.

[0130] [Volume difference] Volume difference between prototypes 6 to 21 (V s ) is the sum of the micropore volumes (V mic )(cm 3 / g) to the sum of mesopore volumes (V met )(cm 3 / g) and was calculated using the above formula (i).

[0131] The physical properties of the activated carbons of Experimental Examples 6 to 21 are shown in Tables 6 to 8. In order from the top of Table 6, the surface oxide amount (meq / g), BET specific surface area (m2 / g), average pore diameter (nm), micropore volume (V mic )(cm 3 / g), mesopore volume (V met )(cm 3 / g), volume difference (V s )(cm 3 / g).

[0132] [Table 6]

[0133] [Table 7]

[0134] [Table 8]

[0135] [Volatile per- and polyfluoroalkyl compound collection experiment 2] As in the above-mentioned Collection Experiment 1, FTOHs was used as the per- and polyfluoroalkyl compound, and evaluation was carried out for Prototype Examples 6 to 21.

[0136] Each standard substance was diluted with methanol to 100ng / ml (100ppb), and 100μl of the diluted solution was added to a flexible polyurethane foam (PUF) and placed in the first stage. Next, the second stage was filled with the prototype activated carbon so that the thickness of the filled case was about 2mm in a 47mmφ case, and air at 22-24℃ was passed through the PUF in the first stage and the adsorbent activated carbon in the second stage at a rate of 20L / min for 48 hours.

[0137] After aeration, the activated carbon of the prototype was transferred to a PP centrifuge tube (volume 15 ml) and 10 ml of a mixed solvent mainly composed of dichloromethane and ethyl acetate was added. The centrifuge tube was shaken at 225 rpm for 10 minutes, and the extract was collected. This extraction process was repeated twice, and a total of 30 ml of extract was collected.

[0138] The collected extract was concentrated to 1 ml using a nitrogen blowing concentrator, and then the extract was quantitatively measured in MRM mode using GC-MS / MS ("GCMS-TQ8050", Shimadzu Corporation) to confirm the collection performance.

[0139] Tables 9 to 11 show the recovery rates (%) of fluorotelomer alcohols (FTOHs) for each target substance for the activated carbon of prototypes 6 to 21. The target substances are 4:2FTOH (IUPAC name: 3,3,4,4,5,5,6,6,6-nonafluoro-1-hexanol), 6:2FTOH (IUPAC name: 3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluoro-1-octanol), 8:2FTOH, and 10:2FTOH (IUPAC name: 3,3,4,4,5,5,6,6,7,7,8,8,9,9,10,10,11,11,12,12,12-heneicosafluoro-1-dodecanol).

[0140] [Table 9]

[0141] [Table 10]

[0142] [Table 11]

[0143] In the table, "ND" indicates that the value was below the lower limit of quantification. Compared to collection experiment 1, the variation in the measured values ​​by mass spectrometry was reduced.

[0144] [Results and considerations of the collection experiment of volatile per- and polyfluoroalkyl compounds 2] In the prototypes 6 to 9, the recovery rate was below the lower limit of quantification for all FTOHs, and the adsorption of the target substances was insufficient. It is presumed that the adsorption performance was not achieved because the pores or specific surface area required for the adsorption of the target substances were not present.

[0145] In the prototypes 10 to 21, all FTOHs were recoverable. 2 It was shown that the target substance can be adsorbed when the specific surface area of ​​the activated carbon is set to 1 / g or more. It is presumed that the parameter of the specific surface area of ​​the activated carbon has a certain effect on the adsorption performance of each FTOH. Furthermore, in particular, prototypes 10 to 19, which are fibrous activated carbon, showed good results with a recovery rate of 50% or more for each FTOH. From the standpoint of the contact efficiency between the target substance and activated carbon, it is thought that FTOH can be adsorbed more efficiently when fibrous activated carbon is used.

[0146] It was also shown that activated carbon with developed micropores and mesopores exhibits high adsorption performance for all FTOH. In prototypes 6 and 7, neither the micropores nor the mesopores were developed, and it is believed that none of the FTOH was adsorbed. In prototypes 8 and 9, the micropores were developed but the mesopores were not developed, so there were few mesopores on the inlet side of the activated carbon pores, and it is believed that the FTOH molecules were not smoothly introduced into the micropores, resulting in no adsorption.

[0147] In prototypes 10 to 21, the pore volumes of both the micropores and mesopores are large, and it is believed that both pores are sufficiently developed, so that FTOH molecules are smoothly introduced into the pores of the activated carbon, and excellent adsorption performance is demonstrated. Prototypes 12 to 19 showed particularly excellent FTOH recovery performance. Prototypes 12 to 19 are all characterized by a large micropore volume and the fact that although the mesopores are well developed, the mesopore volumes are not that large. After the FTOH molecules are adsorbed into the micropores, they are easily desorbed out of the pores during the extraction operation, which is thought to be why a particularly good recovery rate was demonstrated.

[0148] In contrast, since the pore volumes of both micropores and mesopores in prototypes 20 and 21 are large, it can be said that these are activated carbons with complexly developed pores ranging from large pores to small pores. It is presumed that the FTOH molecules adsorbed in the complexly developed pores are less likely to be smoothly desorbed during the extraction operation, resulting in a slightly lower FTOH recovery rate compared to prototypes 12 to 19. In view of these results, the sum of the pore volumes of the micropores in the activated carbon (V mic ), the sum of the pore volumes of the mesopores (V met ) and the difference between them, the volume difference (V s It is understood that the recovery rate of FTOH is affected by the above.

[0149] In addition to the pore conditions of the activated carbon, we also investigated whether the adsorption performance of FTOH could be improved by improving the affinity with FTOH having a hydrophilic group by improving the amount of surface oxide. As a result, between Prototype 13 and Prototypes 14 to 17, which are made of the same activated carbon raw material, Prototypes 14 to 17, which had an increased amount of surface oxide, showed better adsorption performance. Similarly, in Prototype 18 and Prototype 19, Prototype 19, which had a larger amount of surface oxide, showed better adsorption performance. Therefore, it is understood that the adsorption performance of FTOH can be further improved by increasing the amount of surface oxide of the activated carbon.

[0150] As shown in the above volatile per- and polyfluoroalkyl compound collection experiments 1 and 2, it was understood that the adsorption performance of volatile per- and polyfluoroalkyl compounds can be greatly improved by setting the BET specific surface area, pore conditions, and surface oxide amount of the adsorbent activated carbon to a certain level or higher. This allows the adsorption of volatile per- and polyfluoroalkyl compounds by the adsorbent activated carbon in the filter part of the volatile compound collection area to be effectively performed, thereby further improving the accuracy of comprehensive quantitative analysis of all forms of per- and polyfluoroalkyl compounds.

[0151] [Study on collection performance of atmospheric per- and polyfluoroalkyl compounds 2] The above experiments showed that it was possible to collect all forms of per- and polyfluoroalkyl compounds in the atmosphere, and therefore the inventors conducted a quantitative evaluation experiment of per- and polyfluoroalkyl compounds in an actual environment.

[0152] [Creating a sampler 2] In order to prepare a sampler for collecting per- and polyfluoroalkyl compounds, the inventors prepared a sampler using polypropylene resin with the following composition.

[0153] Air intake section Intake hole: Inner diameter 11.0mm -Particle adsorbent collection area 1st stage: Particle adsorbent compound collection area that collects particles of 10 μm or more Clearance: Inner diameter 40mm Collection filter paper: Quartz fiber filter, diameter 25 mm Impactor plate: Shape shown in Fig. 4(a), diameter 47 mm Connection hole: Inner diameter (diameter) 4.3mm Second stage: Particle-adsorbent compound collection area that collects fine particles of 2.5 to 10 μm Clearance: Inner diameter 40mm Collection filter paper: Quartz fiber filter, diameter 25 mm Impactor plate: Shape shown in Fig. 4(a), diameter 47 mm Connection hole: Inner diameter (diameter) 2.2mm 3rd stage: Particle adsorbent compound collection area for collecting fine particles of 1.0 to 2.5 μm Clearance: Inner diameter 40mm Collection filter paper: Quartz fiber filter, diameter 25 mm Impactor plate: Shape shown in Fig. 4(a), diameter 47 mm Connection hole: Inner diameter (diameter) 40mm

[0154] A quartz fiber filter manufactured by Shibata Scientific Co., Ltd. was used as the collection filter paper for each particle-adsorbing compound collection area.

[0155] Semi-volatile compound collection area Urethane foam filter part: Polyurethane foam (manufactured by Shibata Scientific Co., Ltd.), diameter 47 mm, height 50 mm

[0156] Volatile Compounds Area A circular sheet (diameter 47 mm, thickness 2 mm) was made using Prototype 10 of adsorbent activated carbon, and two sheets were placed on top of each other to form the filter section.

[0157] [Treatment experiments of per- and polyfluoroalkyl compounds in real environments] Samplers with the above configuration were installed outdoors in Tsukuba City, Ibaraki Prefecture (April 2020) and Minokamo City, Gifu Prefecture (May 2020), and were ventilated at an airflow rate of 20 l / min for 72 hours to conduct experiments on the collection of per- and polyfluoroalkyl compounds in the air under real-world conditions.

[0158] First, the collection experiment in Tsukuba city, Ibaraki prefecture was conducted under conditions of temperature 2-21°C (average 11°C) and relative humidity 31-100% (average 71%), and the experimental results are shown in Tables 12-15. Next, the collection experiment in Minokamo city, Gifu prefecture was conducted under conditions of temperature 16-27°C (average 22°C) and relative humidity 43-88% (average 65%), and the experimental results are shown in Tables 16-19.

[0159] In the particle adsorbent compound collection area, per- and polyfluoroalkyl compounds were measured, including perfluorocarboxylic acids (hereinafter referred to as "PFCAs"): 6:2FTUCA (IUPAC name: 3,4,4,5,5,6,6,7,7,8,8,8-dodecafluoro-2-octenoic acid), PFBA, PFPeA, PFHxA, PFOA, PFNA, PFUnDA, PFDoDA, PFTrDA, PFTeDA, PFHxDA, 8:2diPAP, HFPODA, and perfluoroacids (hereinafter referred to as "PFSAs"): PFBS, PFOS, PFDS, 6:2FTSA (all from ISO21675:2019).

[0160] In the semi-volatile compound collection area, in addition to the PFCAs and PFSAs mentioned above, perfluorooctanoic acids (hereafter referred to as "FOSAs"), such as FOSA and N-MeFOSA (above, from ISO21675:2019), and perfluorooctane sulfonic acids (hereafter referred to as "FOSEs"), such as N-MeFOSE and N-EtFOSE, were measured. Note that recovery rates (%) were also measured using N-MeFOSE and N-EtFOSE as surrogates.

[0161] In the volatile compound collection area, 4:2FTOH, 6:2FTOH, 8:2FTOH, and 10:2FTOH were used as FTOHs, and 6:2FTI, 8:2FTI, and 10:2FTI were measured as fluorotelomer iodines (hereinafter referred to as "FTIs"). FTI is a substance represented by the following chemical formula (viii). In addition, recovery rates (%) were also measured using 4:2FTOH, 6:2FTOH, 8:2FTOH, and 10:2FTOH as surrogates.

[0162]

number

[0163] The sampler was collected after ventilation, and the collection filter paper from each stage of the particle-adsorbent compound collection area was placed in a PP test tube, 4 ml of methanol was added, and the mixture was shaken for 20 minutes. The process of transferring the permeate to another PP test tube was repeated three times to collect the extract. The extract was concentrated with nitrogen to a constant volume of 1 ml, and the per- and polyfluoroalkyl compounds collected in the particle-adsorbent compound collection area were quantitatively measured using an LC-MS / MS ("LCMS-8030", Shimadzu Corporation) in MRM mode.

[0164] In addition, the urethane foam filter part of the semi-volatile compound collection area was packed into a PP syringe, and 18 ml of a mixed solvent of dichloromethane and ethyl acetate was passed through at a rate of 1 drop / second, and extract A-1 was obtained in a PP test tube. Furthermore, 15 ml of methanol was passed through at a rate of 1 drop / second, and extract B was obtained in a PP test tube. Extracts A-1 and B were concentrated by nitrogen blowing to a constant volume of 1 ml. Extract A-1 was separated into another PP test tube, and the solvent was replaced with methanol to obtain extract A-2. Extract A-1 was quantitatively analyzed for per- and polyfluoroalkyl compounds collected in the semi-volatile compound collection area using GS-MS / MS, and extracts A-2 and B were quantitatively analyzed in MRM mode using LC-MS / MS, and all values ​​were added together to calculate the total.

[0165] The filter part made of adsorbent activated carbon from the volatile compound collection area was placed in a PP test tube, 10 ml of a mixed solvent of dichloromethane and ethyl acetate was added, and the mixture was shaken for 10 minutes. The process of transferring the permeate to another PP test tube was repeated twice to collect an extract. The extract was concentrated by blowing nitrogen to a constant volume of 1 ml, and the per- and polyfluoroalkyl compounds collected in the volatile compound collection area were quantitatively analyzed using GS-MS / MS in MEM mode.

[0166] Tables 12 and 16 show the concentrations (pg / m) of per- and polyfluoroalkyl compounds in sample air in the particle adsorbent collection area. 3 ), and Tables 13 and 17 show the amount (mg) and particle concentration (μg / m 3 ), and the concentration of per- and polyfluoroalkyl compounds in particles (μg / g). Tables 14 and 18 show the concentrations of per- and polyfluoroalkyl compounds in sample air in the semivolatile compound collection area (pg / m 3 ), and Tables 15 and 19 show the concentrations (pg / m) of volatile per- and polyfluoroalkyl compounds in the sample air in the volatile compound collection area. 3 ) is shown.

[0167] [Concentration of per- and polyfluoroalkyl compounds in sample air] Tables 12, 14 to 16, 18, and 19 show the concentrations (pg / m) of per- and polyfluoroalkyl compounds in the sample air. 3 The concentration of per- and polyfluoroalkyl compounds is calculated by multiplying the amount (pg) of per- and polyfluoroalkyl compounds (target substances) collected in each collection area by the cumulative flow rate (m 3 ) and was calculated using the following formula (ix). In the table, "BLANK" indicates the value detected by performing the same measurement on the collection filter paper, the urethane foam filter part, and the filter part before the experiment, and "LOQ" indicates the lower limit at which each substance can be quantitatively measured by the measuring device. "-" indicates that it is below the lower limit of quantification.

[0168]

number

[0169] [Collected amount] Tables 13 and 17 show the particles and particle-adsorbent per- and polyfluoroalkyl compounds collected in the particle-adsorbent compound collection area. The amount of particles collected (mg) was calculated as the difference between the filter weight after the experiment and the filter weight before the collection experiment. The weight of the filter was measured to the nearest 1μg using a precision balance (Micro Electronic Balance "BM-20" manufactured by A&D Co., Ltd.) in a space adjusted to a temperature of 25±1℃ and humidity of 35-40%.

[0170] [Particle concentration] Particle concentration (μg / m 3 ) is the cumulative flow rate (m 3 ) and was calculated using the following formula (x):

[0171]

number

[0172] [Concentration of per- and polyfluoroalkyl compounds in collected particles] The concentration of per- and polyfluoroalkyl compounds attached to the collected particles is referred to as PFAS concentration in Tables 13 and 17. The PFAS concentration (μg / g) is a value that indicates the ratio of detected per- and polyfluoroalkyl compounds (PFAS) to the amount of collected particles. The sum of the concentrations of per- and polyfluoroalkyl compounds in the particle-adsorbed compound collection area (pg / m 3 ) to particle concentration (μg / m 3 ) and was calculated using the following formula (xi).

[0173]

number

[0174] [Table 12]

[0175] [Table 13]

[0176] [Table 14]

[0177] [Table 15]

[0178] [Table 16]

[0179] [Table 17]

[0180] [Table 18]

[0181] [Table 19]

[0182] [Results and considerations of collection experiments of per- and polyfluoroalkyl compounds in real environments] As shown in Figures 12 to 19, even in collection experiments conducted in actual environments in different regions, it was shown that per- and polyfluoroalkyl compounds in the target form could be successfully collected in each collection area.

[0183] In the particle-adsorbent compound collection areas shown in Tables 12, 13, 16, and 17, particle-adsorbent per- and polyfluoroalkyl compounds were detected, and it can be said that good collection was achieved. In addition, although the types of particle-adsorbent per- and polyfluoroalkyl compounds detected tended to be similar in each area, differences were found, such as different types of particle-adsorbent per- and polyfluoroalkyl compounds being collected, the particle sizes of the particles to which the per- and polyfluoroalkyl compounds were attached being different, and characteristics were also observed in the concentrations and amounts of the per- and polyfluoroalkyl compounds, demonstrating the significance of the sampler as a sampler used for quantitative measurement of particle-adsorbent per- and polyfluoroalkyl compounds.

[0184] It can also be said that semivolatile per- and polyfluoroalkyl compounds were successfully captured in the semivolatile compound collection areas shown in Tables 14 and 18. Since particle-adsorbent per- and polyfluoroalkyl compounds were detected in the semivolatile compound collection areas in each region, it is believed that the accuracy of collection of per- and polyfluoroalkyl compounds by form can be further improved by setting a particle-adsorbent compound collection area capable of capturing particles with smaller particle diameters in the particle-adsorbent compound collection area.

[0185] As with the particle-adsorbent compound collection areas, differences in the types and amounts of semivolatile per- and polyfluoroalkyl compounds detected in each region were observed, demonstrating the significance of the sampler for quantitative measurement of semivolatile per- and polyfluoroalkyl compounds. In addition, the good measurement of N-MeFOSE and N-EtFose used as surrogates indicates the high accuracy of the sampler for semivolatile per- and polyfluoroalkyl compounds.

[0186] Volatile per- and polyfluoroalkyl compounds were also successfully captured in the volatile compound capture areas shown in Tables 15 and 19. As with the other forms of per- and polyfluoroalkyl compounds listed above, there were regional differences in the captured per- and polyfluoroalkyl compounds, demonstrating the significance of the sampler for quantitative measurement of volatile per- and polyfluoroalkyl compounds. The recovery of FTOHs used as a surrogate was also good, indicating the high accuracy of the sampler for volatile per- and polyfluoroalkyl compounds.

[0187] As described above, by using the sampler according to the present invention, good results were obtained for the collection of per- and polyfluoroalkyl compounds by form in each collection area. In other words, it was shown that the per- and polyfluoroalkyl compound collection sampler according to the present invention can efficiently and comprehensively collect per- and polyfluoroalkyl compounds present in the atmosphere, and can also separate and collect them by form, and can perform highly accurate quantitative measurement. [Industrial Applicability]

[0188] The per- and polyfluoroalkyl compound collection sampler of the present invention can comprehensively collect per- and polyfluoroalkyl compounds present in the atmosphere in various forms, and therefore enables quantitative measurement of the compounds, which was impossible with existing collection materials, and by controlling the physical properties of the activated carbon as a collection material, the adsorption performance of per- and polyfluoroalkyl compounds is improved, enabling more accurate and effective quantitative measurement. This makes it possible to contribute to the quantitative evaluation of per- and polyfluoroalkyl compounds as environmental persistent organic pollutants that may be subject to regulation. [Explanation of symbols]

[0189] 10. Sampler 20 Particulate Adsorbent Collection Area 21 Inertial impactor section 22 Collection filter paper 23 Impactor Plate 24 Through hole 25 Clearance section 26 Accelerating Nozzle 27 Connection hole 28 Discoid 29 Ultra-fine particle collection section 30 Semi-volatile Compound Collection Area 31 Urethane foam filter section 32 Urethane foam 40 Volatile Compound Collection Area 41 Filter section C Adsorbent activated carbon

Claims

1. A sampler for collecting per- and polyfluoroalkyl compounds in a sample air, comprising: an intake section for sucking in the sample air; a particle-adsorbent compound collection area connected to the air intake and including an inertial impactor for collecting particle-adsorbent per- and polyfluoroalkyl compounds in the air; a semi-volatile compound collection area connected to the particle-adsorbent compound collection area and including a urethane foam filter section for collecting semi-volatile per- and polyfluoroalkyl compounds in the air; a BET specific surface area of ​​900 m for collecting volatile per- and polyfluoroalkyl compounds in the air connected to the semi-volatile compound collection area; 2 A volatile compound collection area having a filter portion made of adsorbent activated carbon having a molecular weight of at least 10000 / g; an exhaust section connected to the volatile compound collection area and through which the atmospheric air that has ventilated each of the areas is exhausted; A sampler for collecting per- and polyfluoroalkyl compounds.

2. The per- and polyfluoroalkyl compound collection sampler of claim 1, wherein the particle-adsorbent compound collection area comprises a plurality of layers of the inertial impactor section which sequentially collects particle-adsorbent per- and polyfluoroalkyl compounds in the atmosphere in the order of particle diameter from largest to smallest.

3. 3. The sampler for collecting per- and polyfluoroalkyl compounds according to claim 1, wherein the amount of surface oxides of the adsorbent activated carbon is 0.10 meq / g or more.

4. The sum of the micropore volumes of the adsorbent activated carbon of 1 nm or less (V mic ) is 0.35 cm 3 4. The per- and polyfluoroalkyl compound collection sampler according to claim 1, wherein the concentration of said per- and polyfluoroalkyl compounds is 1 / g or more.

5. The sum of the mesopore volumes of 2 to 60 nm of the adsorbent activated carbon (V met ) is 0.02 cm 3 4. The per- and polyfluoroalkyl compound collection sampler according to claim 1, wherein the concentration of said per- and polyfluoroalkyl compounds is 1 / g or more.

6. The per- and polyfluoroalkyl compound collection sampler according to claim 4, wherein the sum of the volumes of mesopores of 2 to 60 nm in the adsorbent activated carbon (V met ) is 0.02 cm 3 / g or more.

7. The sum of the micropore volumes of the adsorbent activated carbon defined by the following formula (i) (V mic ) and the sum of the mesopore volume (V met ) and the volume difference (V s 7. The per- and polyfluoroalkyl compound collection sampler according to claim 6, wherein the ratio of the fluorocarbon content to the total fluorocarbon content is 0.45 or more. [0010]

Citation Information

Patent Citations

  • Active sampling system of persistent organic pollutants PAHs in atmosphere

    CN105445061A

  • Passive sampling device for sampling long-lasting organic pollutants in atmosphere

    CN106053152A

  • Active sampling sleeve for persistent organic pollutant in atmosphere

    CN107843463A

  • Method for collecting residual organic pollutant and sampler

    JP2005189025A

  • Organic fluorine compound adsorbent

    JP2012101159A