Anode for magnesium battery and method of making same
The magnesium battery anode with a protective layer addresses the boundary layer issue, enhancing stability and performance by preventing direct electrolyte contact, thus improving cycle life and kinetics.
Patent Information
- Application Number
- JP2022577292
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-07-15
- Filing Date
- 2021-07-05
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-07-05
AI Technical Summary
Magnesium batteries suffer from a boundary layer formation on the anode that reduces service life and performance, particularly impedance and cycle stability, due to exposure to air.
A magnesium battery anode with a core element coated in magnesium and a protective layer of metal, ceramic, or metal sulfide, which prevents direct contact between the electrolyte and the magnesium coating, using materials like aluminum, copper, or ceramic oxides to enhance stability and reduce interfacial resistance.
The protective layer prevents boundary layer formation, improving the anode's lifespan and performance by reducing impedance and enhancing the kinetics of dissolution and deposition processes.
Smart Images

Figure 0007566935000001 
Figure 0007566935000002
Abstract
Description
[Technical field]
[0001] The present invention relates to an anode for a magnesium battery and a method for producing an anode for a magnesium battery. A magnesium battery is an electrochemical power storage device, the anode of which is essentially made of magnesium. [Background technology]
[0002] US 2020 / 0112028 A1 discloses an anode for a magnesium battery. The anode is formed from magnesium foam with a polymer layer covering the magnesium foam on all surfaces.
[0003] US 2016 / 0254541 describes an electrode active material for magnesium batteries that includes a λ-MnO2 phase.
[0004] US Patent Application Publication No. 2018 / 0190981 discloses a device having a first electrode made of magnesium metal and a coating including a first polymer.
[0005] JP 2014-143191 A describes a magnesium battery having a negative electrode comprising magnesium, a positive electrode comprising copper or a copper alloy, and an electrolyte comprising citric acid, sodium chloride, and water. The face of the negative electrode opposite the positive electrode is coated with a coating comprising tin.
[0006] Generally, it is known that a magnesium battery includes a plurality of battery cells, each of which has a plurality of anodes and cathodes disposed in an electrolyte. During the operation of the magnesium battery, an interface layer is formed on the magnesium anode between the electrolyte and the magnesium anode, which reduces the service life and performance of the magnesium battery, especially the impedance and cycle stability. This interface layer can be formed as soon as the magnesium anode is exposed to the surrounding air. Summary of the Invention [Problem to be solved by the invention]
[0007] The object of the present invention is to provide a long-life anode for magnesium batteries. Furthermore, the anode should be cheap to manufacture and increase the performance of magnesium batteries. This object is achieved by the subject matter of claims 1 and 7. Preferred embodiments can be found in the dependent claims, the description and the drawings. [Means for solving the problem]
[0008] The magnesium battery anode according to the present invention comprises a core element made from a core material, a magnesium coating disposed at least partially on a surface of the core element, and a protective layer disposed on a surface of the magnesium coating, the protective layer comprising: Designated as a metal and consisting of one of the following elements: aluminum, copper, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver, or An alloy of at least two of the following elements: Made of aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, or silver; or Designated as a ceramic and consisting of elements from the group including aluminium, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver, carbon, nitrogen and oxygen; or the protective layer consists of a metal sulfide, at least one of the elements from the group consisting of aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver forming a metal sulfide, or the protective layer consists of carbon or doped carbon; Either:
[0009] In other words, at least a part of the surface of the core element or the entire surface of the core element is coated with a magnesium coating, the magnesium of the magnesium coating preferably having a purity of at least 99.9%. The magnesium coating is the active material of the anode. The active material is intended to interact with the cathode. The protective layer is arranged on the entire surface of the magnesium coating. In particular, the protective layer is formed on the surface of the magnesium coating such that the electrolyte of the magnesium battery does not directly, i.e. directly, come into contact with the magnesium coating of the anode, but merely comes into contact with the protective layer arranged on the surface of the magnesium coating or, by interacting with the magnesium coating, positively influences the operation of the anode. This has the advantage that no spontaneous boundary layer to the electrolyte is formed on the magnesium coating, which reduces the service life and performance, in particular the impedance and cycle stability of the magnesium battery. In particular, the protective layer protects the magnesium coating from oxidation during manufacture. Furthermore, the protective layer allows a reduction of the interface resistance and an improvement of the kinetics of the dissolution and deposition processes. Furthermore, the protective layer optimizes the cyclability of the anode.
[0010] To achieve these advantages, the protective layer is designed as a metal and is preferably formed from one of the following elements: aluminum, copper, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver. Alternatively, the protective layer is formed from an alloy of at least two of the following elements: aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver.
[0011] For example, the protective layer is made of aluminum or an aluminum alloy. For example, the protective layer is made of copper or a copper alloy. For example, the protective layer is made of a tin alloy. For example, the protective layer is made of silicon or a silicon alloy. For example, the protective layer is made of titanium or a titanium alloy. For example, the protective layer is made of tantalum or a tantalum alloy. For example, the protective layer is made of niobium or a niobium alloy. For example, the protective layer is made of nickel or a nickel alloy. For example, the protective layer is made of molybdenum or a molybdenum alloy. For example, the protective layer is made of silver or a silver alloy.
[0012] In an alternative embodiment, the protective layer is designed as a ceramic and consists of elements from the group including aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver, carbon, nitrogen, oxygen.
[0013] In particular, the ceramic protective layer is a metal oxide layer. For example, the protective layer is at least partially or entirely made of aluminum oxide. For example, the protective layer is at least partially or entirely made of copper oxide. For example, the protective layer is at least partially or entirely made of tin oxide. For example, the protective layer is at least partially or entirely made of silicon oxide. For example, the protective layer is at least partially or entirely made of titanium oxide. For example, the protective layer is at least partially or entirely made of tantalum oxide. For example, the protective layer is at least partially or entirely made of niobium oxide. For example, the protective layer is at least partially or entirely made of nickel oxide. For example, the protective layer is at least partially or entirely made of molybdenum oxide. For example, the protective layer is at least partially or entirely made of silver oxide.
[0014] In further preferred embodiments, the ceramic protective layer is formed from a carbide and / or nitride compound. For example, the protective layer is formed at least partially or entirely from silicon nitride. For example, the protective layer is formed at least partially or entirely from titanium nitride. For example, the protective layer is formed at least partially or entirely from niobium nitride. For example, the protective layer is formed at least partially or entirely from tantalum nitride.
[0015] In a further alternative embodiment, the protective layer is made of a metal sulfide, and at least one of the elements selected from the group including aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, and silver forms the metal sulfide, for example, the protective layer is at least partially or entirely made of molybdenum sulfide.
[0016] According to a further preferred embodiment, the protective layer may comprise a sulfide compound and / or a nitride compound.
[0017] In a further alternative embodiment, the protective layer consists of carbon or doped carbon. The doping of the doped carbon layer, i.e. the protective layer formed predominantly from carbon, reaches up to 45 atomic %. Preferably, one or more elements from the group comprising aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver, hydrogen are used here as doping elements.
[0018] According to a preferred embodiment of the invention, the protective layer has a thickness of at least 0.5 nm and at most 5 μm. In particular, it has been found that a protective layer thickness of at least 5 nm and at most 250 nm contributes particularly well to maintaining the energy density of the anode.
[0019] Preferably, the core element, also known as conductor, is at least partially made of aluminum, copper, steel or polymer material. For example, the core element is made of aluminum or an aluminum alloy. For example, the core element is made of copper or a copper alloy. For example, the core element is made of steel or a steel alloy. In particular, the steel alloy is a stainless steel, i.e. a steel with a purity such that the sulfur and phosphorus content is at most 0.025 wt%. In particular, the steel alloy is corrosion resistant and has at least chromium and / or nickel as alloying elements. The alloy composition of the steel alloy can be determined, for example, by optical emission spectroscopy (OES) or X-ray fluorescence analysis (XRF). wt% stands for weight percent.
[0020] To manufacture the anode according to the invention, the following method steps are carried out: first, a core element is provided. The core element is preferably formed from a core material of aluminum, copper, steel or a polymer material. This is followed by applying a magnesium coating to at least a part of the surface of the core element. This is followed by applying a protective layer to the surface of the magnesium coating.
[0021] According to a preferred embodiment of the invention, the magnesium coating is applied to at least a portion or all of the surface of the core element by a galvanic process, a lamination process, a PVD process, a CVD process, an ALD process, a plating process, a thermal spray process, or a melting process.
[0022] The magnesium coating preferably has a layer thickness in the range from 50 nm to 200 μm, in particular from 1 μm to 50 μm.
[0023] In the galvanic process, electrochemistry of magnesium on the core element is carried out, for example, in a deposition bath. In the lamination process, coated materials, for example magnesium coatings and protective layers, are transferred or laminated onto the structured core element. In the plating process, also known as cladding, a metal layer is formed on the substrate or core element by pressure and temperature, in particular by subsequent heat treatment. In the thermal spray process, liquefied magnesium is sprayed onto the substrate, i.e. the core element.
[0024] PVD is an abbreviation for the term "Physical Vapor Deposition". The PVD process is a process carried out under vacuum at temperatures ranging from 150 °C to 500 °C. A physical process is used to convert the starting material for the magnesium coating into the gas phase. The gaseous material is then directed to the surface of the core element, where it condenses to form the magnesium coating. For example, in the PVD process, particles are extracted from a magnesium target by sputtering and transported in a plasma to the surface of the core element. The PVD process can be used to produce particularly pure and uniform coatings.
[0025] CVD is an abbreviation for the term "Chemical Vapor Deposition". In the CVD process, a chemical reaction from the gas phase causes a layer deposition on the heated surface of the core element. The CVD process is characterized by at least one reaction at the surface of the core element. This reaction involves at least one gaseous starting compound and at least two reaction products, at least one of which is in the solid phase. The CVD process can be used to produce particularly uniform coatings.
[0026] ALD is an abbreviation of the term "Atomic Layer Deposition". The ALD process is a highly modified CVD process, involving at least two cyclically performed self-limiting surface reactions. The material to be deposited is bound in chemical form to one or more carrier gases. The carrier gases are alternately delivered to a reaction chamber, where they are reacted with the surface of the core element, and the magnesium bound in the gas is deposited on the surface of the core element. The ALD process can be used to produce particularly thin coatings.
[0027] In the melt process, magnesium is melted and applied to the core element, for example by dipping or spraying. The melt process offers the advantages of high speed and large area coating formation, as well as cost advantages.
[0028] According to a preferred embodiment of the present invention, a protective layer is applied to the entire surface of the magnesium coating by a PVD process, a CVD process, or an ALD process.
[0029] It is also possible to coat a protective layer on the magnesium foil, which is applied to the core element. The magnesium foil is preferably manufactured using a rolling process.
[0030] According to a preferred embodiment of the present invention, a protective layer is applied to the surface of the magnesium coating during operation of the anode. In other words, the battery cell is designed such that a protective layer is generated on the magnesium coating of the anode during operation of the magnesium battery, which protects the magnesium coating from oxidation, optimizes the cyclability of the anode, reduces the interfacial resistance, and improves the kinetics of the dissolution and deposition process. For example, the electrolyte is formed such that one of the following elements is deposited on the magnesium coating of the anode as a protective layer. Alternatively, an alloy of at least two elements from the group including aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, and silver is deposited.
[0031] The present invention further relates to a magnesium battery comprising an anode according to the present invention, in particular a magnesium battery having a plurality of battery cells, each battery cell having a plurality of anodes and cathodes disposed in a liquid or solid electrolyte.
[0032] Cathodes made of cathode materials containing sulfur components have proven to be suitable with the anodes according to the invention. V2O5 or MgMn2O4 have proven to be particularly suitable as base materials for the intercalation reaction to form the cathode. Sulfur-permeated carbon, sulfur-carbon compounds or SPAN (sulfurized poly(acrylonitrile)) have proven to be particularly suitable as base materials for the conversion reaction to form the cathode.
[0033] The following electrolyte salts have proven suitable for forming the electrolyte of magnesium batteries:
[0034] MgTFSI2 Magnesium bis(trifluoromethanesulfonimide) Mg(B(hfip)4)2 Magnesium tetrakis(hexafluoroisopropyloxy)borate Mg(BH4)2 Magnesium borohydride Also, a mixture of Mg(BH4)2 and Li(BH4) (= lithium borohydride) or a mixture of Mg(B(hfip)4)2 and Li(B(hfip)4) (= lithium tetrakis(hexafluoroisopropyloxy)borate) has been shown to improve performance.
[0035] Furthermore, the use of electrolyte salts based on Mg(HMDS)2 (=magnesium bis(hexamethyldisilazide)) has proven suitable.
[0036] Glymes, in particular TEG (= tetraethylene glycol dimethyl ether, tetraglyme), DEG (= diethylene glycol dimethyl ether, diglyme), DME (= 1,2-dimethoxyethane, ethylene glycol dimethyl ether, monoglyme), or a mixture of TEG and DME, have proven to be suitable solvents for dissolving the electrolyte salts.
[0037] Other solvents that have been demonstrated are THF (tetrahydrofuran) or Pyrrolo. 14 Ionic liquids such as TFSI (=1-butyl-1-methylpyrrolidinium bis(trifluoromethylsulfonyl)imide).
[0038] Further means for improving the invention are presented in more detail below in conjunction with a description of a preferred exemplary embodiment of the invention based on two figures, in which like elements are given the same reference numbers. FIG. [Brief description of the drawings]
[0039] [Figure 1] FIG. 1 shows a highly simplified schematic cross-sectional view of a magnesium battery according to the invention, only partially shown. [Diagram 2] FIG. 1 shows a highly simplified schematic cross-sectional view of an anode according to the invention, only partially shown. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0040] 1 shows a highly simplified magnesium battery 2 according to the present invention. The magnesium battery 2 has a plurality of battery cells 8, but for simplicity, only a portion of a single battery cell 8 is shown here. The battery cell 8 has a plurality of anodes 1 and cathodes 7, which are disposed in an electrolyte 6. The surface of each anode 1 is completely covered with a protective layer 5.
[0041] FIG. 2 shows a cross section of the anode 1 according to FIG. 1. The anode 1 has a core element 3, which here is formed from the core material aluminum. A magnesium coating 4 is arranged on the surface of the core element 3 as the active material of the anode 1, the magnesium coating 4 being formed, for example, by a melting process. A protective layer 5 is arranged on the surface of the magnesium coating 4. For example, the protective layer 5 is metallic and formed from aluminum or ceramic and formed from copper oxide. In particular, a PVD process is suitable for forming the protective layer 5. The protective layer 5 preferably has a layer thickness of at least 0.5 nm and a maximum of 5 μm. The electrolyte 6 does not adjoin the magnesium coating 4, but only the protective layer 5. This increases the life of the anode 1 and improves the performance of the magnesium battery 2. [Explanation of symbols]
[0042] 1 Anode 2 Magnesium batteries 3 Core Elements 4. Magnesium coating 5 Protective layer 6 Electrolytes 7 Cathode 8 Battery Cells
Claims
1. An anode (1) for a magnesium battery (2), comprising a core element (3) made from a core material, a magnesium coating (4) disposed at least partially on a surface of said core element (3), and a protective layer (5) disposed on a surface of said magnesium coating (4), The protective layer (5) Designated as a metal and one of the following elements: Aluminum, silicon, titanium, tantalum, niobium, molybdenum, silver, or It is made of an alloy of at least two of the following materials: aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, and silver; or Designated as a ceramic and consisting of elements from the group including aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver, carbon, nitrogen, oxygen, or the protective layer (5) consists of a metal sulfide, at least one of the elements from the group including aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver forming said metal sulfide, or said protective layer (5) consisting of carbon doped with one or more elements from the group including aluminum, copper, tin, silicon, titanium, tantalum, niobium, nickel, molybdenum, silver, hydrogen; The anode (1) is characterized in that it is either
2. 2. The anode (1) according to claim 1, characterized in that the ceramic protective layer (5) is a metal oxide layer.
3. 2. Anode (1) according to claim 1, characterized in that the ceramic protective layer (5) is formed from a carbide and / or nitride compound.
4. Anode (1) according to any one of claims 1 to 3, characterized in that the protective layer (5) has a layer thickness of at least 0.5 nm and at most 5 μm.
5. Anode (1) according to any one of the preceding claims, characterized in that the magnesium coating (4) has a layer thickness in the range of 50 nm to 200 μm.
6. Anode (1) according to any one of the preceding claims, characterized in that the core material is made from at least one material from the group comprising aluminium, copper, steel and polymeric materials.
7. A method for producing an anode (1) according to any one of claims 1 to 6, comprising the steps of: - a method step of providing said core element (3); - a method step of application of said magnesium coating (4) to at least a part of the surface of said core element (3); - the method step of application of said protective layer (5) to said surface of said magnesium coating (4).
8. 8. The method according to claim 7, characterized in that the magnesium coating (4) is applied to at least a part of the surface of the core element (3) by a galvanic process, a lamination process, a PVD process, a CVD process, an ALD process, a plating process, a thermal spraying process or a melting process.
9. 9. The method according to claim 7 or 8, characterized in that the protective layer (5) is applied to the surface of the magnesium coating (4) by a galvanic process, a PVD process, a CVD process, a plating process or an ALD process.
10. A magnesium battery (2) comprising at least one anode (1) according to any one of claims 1 to 6 and at least one cathode (7) made of a cathode material containing a sulfur component.
Citation Information
Patent Citations
Negative electrode for battery and manufacture thereof
JP1999345610A
Negative electrode for battery and its manufacture
JP2000012016A
Electrodes for magnesium secondary batteries and magnesium secondary batteries equipped therewith
JP2012531725A
Battery pack
JP2013168351A
Magnesium fuel electrode manufacturing method and magnesium fuel electrode manufacturing apparatus
JP2019186026A