Semiconductor wafer manufacturing method

The semiconductor wafer with grooves and structural enhancements addresses the issue of surface area limitations, ensuring uniform film formation and etching, enhancing manufacturing reliability.

JP7566966B2Active Publication Date: 2024-10-15KK TOSHIBA +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023066092
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-03-20
Filing Date
2023-04-14
Publication Date
2024-10-15
Estimated Expiration
2040-03-10

AI Technical Summary

Technical Problem

Existing semiconductor wafers lack a sufficient surface area for effective film formation and etching processes, leading to variations and potential warping during repeated use.

Method used

The semiconductor wafer is designed with grooves having a specific aspect ratio and directionality to increase surface area, incorporating features like grooves, partition walls, and porous regions to enhance stability and facilitate easy film removal.

Benefits of technology

The increased surface area and structural design minimize warping and variations, enabling uniform film formation and etching, thereby improving the reliability and efficiency of semiconductor device manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007566966000001
    Figure 0007566966000001
  • Figure 0007566966000002
    Figure 0007566966000002
  • Figure 0007566966000003
    Figure 0007566966000003
Patent Text Reader

Abstract

To provide a semiconductor wafer with a larger surface area and a manufacturing method for the semiconductor wafer.SOLUTION: A manufacturing method for a semiconductor wafer 1 includes the steps for forming a catalyst layer 2 containing at least one precious metal element selected from the group consisting of gold, silver, platinum, iridium, and palladium on a surface 10a of a semiconductor substrate, immersing the semiconductor substrate on which the catalyst layer is formed in a first chemical solution, partially etching the semiconductor substrate to form grooves 11 on the surface, and removing the catalyst layer from the surface.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing a semiconductor wafer. [Background technology]

[0002] In the manufacture of semiconductor devices, a non-product wafer (NPW) on which no semiconductor devices are formed is sometimes used. Also, a semiconductor device in which memory cells are arranged three-dimensionally on a semiconductor wafer is known. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] International Publication No. 2015 / 012874 [Patent Document 2] International Publication No. 2010 / 114887 Summary of the Invention

[0004] The problem to be solved by the invention of the embodiment is to provide a semiconductor wafer having a larger surface area.

[0005] A semiconductor wafer according to an embodiment has a surface having at least one groove including an inner wall surface. The groove has an exposed inner wall surface. [Brief description of the drawings]

[0006] [Figure 1] FIG. 1 is a schematic view showing the appearance of a semiconductor wafer. [Diagram 2] 1 is a schematic top view illustrating an example of a structure of a semiconductor wafer. [Diagram 3] 1 is a schematic cross-sectional view showing an example of a structure of a semiconductor wafer. [Figure 4] 1 is a schematic top view illustrating an example of a structure of a semiconductor wafer. [Diagram 5] 1 is a schematic top view showing the boundary between region 101 and region 102. FIG. [Figure 6]1A to 1C are schematic diagrams for explaining an example of a method for manufacturing a semiconductor wafer. [Figure 7] 1A to 1C are schematic diagrams for explaining an example of a method for manufacturing a semiconductor wafer. [Figure 8] 1A to 1C are schematic diagrams for explaining an example of a method for manufacturing a semiconductor wafer. [Figure 9] 10A to 10C are schematic diagrams for explaining another example of a method for manufacturing a semiconductor wafer. [Figure 10] 11 is a schematic cross-sectional view showing another example of the structure of a semiconductor wafer. FIG. [Figure 11] 11 is a schematic cross-sectional view showing another example of the structure of a semiconductor wafer. FIG. [Figure 12] 11 is a schematic cross-sectional view showing another example of the structure of a semiconductor wafer. FIG. [Figure 13] 11 is a schematic cross-sectional view showing another example of the structure of a semiconductor wafer. FIG. [Figure 14] 11 is a schematic cross-sectional view showing another example of the structure of a semiconductor wafer. FIG. [Figure 15] 1 is a schematic cross-sectional view showing a structural example of a semiconductor device; [Figure 16] FIG. 1 is a schematic diagram showing a configuration example of a semiconductor manufacturing apparatus. [Figure 17] 1 is a schematic diagram illustrating a structural example of a semiconductor device. [Figure 18] 1A to 1C are schematic diagrams for explaining an example of a method for manufacturing a semiconductor device. [Figure 19] 1A to 1C are schematic diagrams for explaining an example of a method for manufacturing a semiconductor device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Hereinafter, the embodiments will be described with reference to the drawings. The relationship between the thickness and planar dimensions of each component, the thickness ratio of each component, etc. shown in the drawings may differ from the actual product. In addition, in the embodiments, substantially the same components are given the same reference numerals and the description will be omitted as appropriate.

[0008] (Example of semiconductor wafer structure) Fig. 1 is a schematic diagram of the appearance of a semiconductor wafer, Fig. 2 is a schematic top view showing an example of the structure of a semiconductor wafer, showing a part of an XY plane including an X axis of the semiconductor wafer and a Y axis perpendicular to the X axis, Fig. 3 is a schematic cross-sectional view showing an example of the structure of a semiconductor wafer, showing a part of an XZ cross section including an X axis and a Z axis perpendicular to the X axis and the Y axis.

[0009] The semiconductor wafer 1 is an NPW, and is a wafer used to evaluate and measure in advance various processes in semiconductor manufacturing, such as film formation, etching, and the like. For example, it is used for evaluation and measurement of film formation processes such as CVD (Chemical Vapor Deposition) and ALD (Atomic Layer Deposition), which form a thin film by reacting a raw material gas with the wafer surface, or etching processes such as CDE (Chemical Dry Etching), which supplies plasma to the wafer surface to etch a thin film, ALE (Atomic Layer Etching), which supplies raw material gas to the surface to etch a thin film, and wet etching, which supplies a liquid. It is also used for reproducibility tests thereof. It may be processed in the same processing chamber as a wafer on which a semiconductor device is formed. The semiconductor wafer 1 of the embodiment may also be called a dummy wafer or a test piece.

[0010] The semiconductor wafer 1 includes a surface 10a extending in the X-axis direction and the Y-axis direction, and a surface 10b opposite to the surface 10a. The surface area of ​​the surface 10a is preferably approximately the same as the surface area of ​​a device formation surface of a semiconductor wafer on which a semiconductor device has been formed or is in the process of being formed. The semiconductor wafer 1 may be, for example, a silicon wafer, a silicon carbide wafer, a glass wafer, a quartz wafer, a sapphire wafer, or a compound semiconductor wafer such as a GaAs substrate. The shape of the semiconductor wafer 1 is not limited to the shape shown in FIG. 1, and may be, for example, a shape having an orientation flat.

[0011] The surface 10a has a pattern including at least one groove 11. The groove 11 includes an inner wall surface 11a. The inner wall surface 11a is exposed to the surface 10a. When a plurality of grooves 11 are provided, the plurality of grooves 11 are arranged in parallel along the X-axis direction of the surface 10a and extend in a line along the Y-axis direction of the surface 10a, as shown in FIG. 2. The length L of the long side of the groove 11 is, for example, 4 μm or more, preferably 40 μm or more. The interval between adjacent grooves 11 along the X-axis direction is, for example, 0.4 μm or more and 14 μm or less, preferably 1 μm or less. The ends of adjacent grooves 11 along the X-axis direction may be shifted from each other along the Y-axis direction.

[0012] The aspect ratio of the groove 11 is, for example, 50 or more and 1750 or less. The aspect ratio is defined by the ratio of the depth D of the groove 11 to the width W of the groove 11 shown in FIG. 3. The width W of the groove 11 is, for example, 0.4 μm or more and 14 μm or less. The depth D of the groove 11 is, for example, 20 μm or more and the thickness of the semiconductor wafer 1 or less, and the groove 11 may penetrate through the semiconductor wafer 1. The surface area of ​​the surface 10a is, for example, 50 times or more, preferably 100 times or more, compared to the surface area in the case where the groove 11 is not formed. In other words, when no grooves or the like are formed on the surface 10b, it can be said that the surface area is 50 times or more, preferably 100 times or more, of the surface 10b.

[0013] It is preferable that the groove 11 has a depth D from the surface 10a of, for example, 20 μm or more and an aspect ratio of 50 or more. This makes it possible to realize the groove 11 that increases the surface area of ​​the surface 10a and makes it easy to remove the film formed on the surface 10a.

[0014] Groove 11 may be formed via partition walls 12. When the length L, depth D, and aspect ratio of groove 11 are large, groove 11 is likely to collapse and deform. In contrast, by providing partition walls 12, the partition walls 12 function as beams to support groove 11, so that deformation of groove 11 can be suppressed.

[0015] In order to suppress deformation of the grooves 11, the partitions 12 are preferably provided at intervals of, for example, 100 μm or more in the Y-axis direction. Moreover, it is preferable that the lengths of the partitions 12 in the Y-axis direction are the same. Furthermore, the positions of the partitions 12 of grooves 11 adjacent to each other along the X-axis direction may be shifted from each other along the Y-axis direction as shown in FIG. 2, and the regions between the adjacent grooves 11 may be connected via the partitions 12.

[0016] The groove 11 may include a plurality of grooves extending along different directions. FIG. 4 is a schematic top view showing a structural example of the semiconductor wafer 1, showing a part of the XY plane. The surface 10a of the semiconductor wafer 1 shown in FIG. 4 includes a region 101 and a region 102. The regions 101 and 102 are alternately arranged along, for example, the X-axis direction and the Y-axis direction. The interval between the regions 101 and 102 is, for example, 2 μm or more. Note that FIG. 4 shows one shot region out of a plurality of shot regions formed on the surface 10a.

[0017] FIG. 5 is a schematic top view showing the boundary between the region 101 and the region 102. The region 101 has a groove 111, and the region 102 has a groove 112. The grooves 111 are arranged side by side along the X-axis direction and extend along the Y-axis direction. The grooves 112 are arranged side by side along the Y-axis direction and extend along the X-axis direction. The extension directions (length L direction) of the grooves 111 and the extension directions (length L direction) of the grooves 112 are not limited to being perpendicular to each other, but may be in any directions intersecting each other. The grooves 111 and 112 are included in the groove 11. Therefore, the description of the groove 11 can be used as appropriate for other descriptions of the grooves 111 and 112. The structure of the surface 10a described above may be formed on the surface 10b.

[0018] As described above, the semiconductor wafer 1 can be used as a test piece for forming a film on the semiconductor wafer 1 and evaluating the film. Alternatively, the semiconductor wafer 1 can be used as a test piece for forming a film on the semiconductor wafer 1 and then etching the same for evaluation. In this case, the semiconductor wafer 1 is prone to warping because it has a pair of surfaces with different surface areas and the difference in the amount of film formed on the pair of surfaces is large. Therefore, if all of the multiple grooves 11 extend in the same direction, stress is applied in one direction, which tends to cause the semiconductor wafer 1 to warp significantly. In contrast, by extending the multiple grooves 11 in multiple directions, the direction in which stress is applied can be dispersed, thereby suppressing the warping of the semiconductor wafer 1.

[0019] The semiconductor wafer 1 can be repeatedly used as a test piece. In other words, it is possible to perform a film formation process continuously on the semiconductor wafer 1, or to perform a film formation process and an etching process continuously on the semiconductor wafer 1. Since the grooves 11 increase the surface area, even in the case of continuous film formation, the change in the surface area can be suppressed, and even in the case of etching, the film can be easily removed.

[0020] As shown in FIG. 4, the surface 10a may further include a region 103. The region 103 is preferably a flat surface without a groove 11. By being a flat surface, the region 103 can be used to measure, for example, the thickness, density, and composition of a film formed on the surface 10a using a measuring instrument such as a spectroscopic ellipsometer, an X-ray photoelectron spectroscopy (XPS), an X-ray fluorescence analysis, or a Fourier transform infrared spectroscopy (FTIR) having a larger minimum measurement area than the flat portion provided between the grooves 11. The area of ​​the region 103 may be smaller than, for example, the area of ​​the region 101 or the area of ​​the region 102. The region 103 is formed, for example, for each of the multiple shot regions of the surface 10a.

[0021] As described above, by controlling the shape of the grooves for increasing the surface area, the semiconductor wafer 1 can realize the grooves 11 that are less likely to deform. This makes it possible to suppress changes in the surface area when the semiconductor wafer 1 is used repeatedly. This makes it possible to provide a semiconductor wafer with a larger surface area. The dimensions of the grooves 11 described above are preferably set according to the type and thickness of the film to be formed.

[0022] (Example of semiconductor wafer manufacturing method) The semiconductor wafer 1 can be manufactured by, for example, metal-assisted chemical etching (MACE). MACE is a technique in which a substrate having a catalyst layer formed on its surface is immersed in a chemical solution to etch only the area in contact with the catalyst layer in a substantially vertical direction.

[0023] 6 to 8 are diagrams for explaining an example of a method for manufacturing a semiconductor wafer. The example of the method for manufacturing a semiconductor wafer includes a catalyst layer forming step, an etching step, and a catalyst layer removing step.

[0024] In the catalyst layer forming step, as shown in Fig. 6, a catalyst layer 2 is formed on the surface 10a of the semiconductor wafer 1. The catalyst layer 2 contains a catalyst of a precious metal such as gold, silver, platinum, iridium, or palladium. The catalyst layer 2 can be formed by using, for example, sputtering, a CVD method, or a plating method. The catalyst layer 2 may contain a catalyst of a carbon material such as graphene.

[0025] In the etching step, the semiconductor wafer 1 is immersed in a first chemical liquid (etchant) as shown in Fig. 7. As the first chemical liquid, for example, a mixture of hydrofluoric acid and hydrogen peroxide can be used.

[0026] When the semiconductor wafer 1 is immersed in the first chemical solution, the material of the surface 10a (e.g., silicon) dissolves in the etching solution at the contact portion between the surface 10a and the catalyst layer 2. This reaction is repeated, and the semiconductor wafer 1 is etched approximately vertically. As a result, the grooves 11 can be formed. The shape of the grooves 11 can be controlled by adjusting, for example, the size of the catalyst layer 2, the etching time, etc.

[0027] In the catalyst layer removal step, the catalyst layer 2 is removed from the surface 10a as shown in Fig. 8. The catalyst layer 2 is removed, for example, by immersing the semiconductor wafer 1 in a second chemical liquid. As the second chemical liquid, for example, a mixed liquid of hydrochloric acid and nitric acid (aqua regia) can be used.

[0028] As described above, by manufacturing the semiconductor wafer 1 using the MACE, even a groove 11 having a large length L, depth D, and aspect ratio can be easily formed.

[0029] (Another example of a method for manufacturing semiconductor wafers) 9 is a diagram for explaining another example of a method for manufacturing a semiconductor wafer 1. In this example, a surface 10a is formed along the (110) plane of the semiconductor wafer 1, a mask layer 3 is formed on the surface 10a, and the semiconductor wafer 1 is etched along the (111) plane of the semiconductor wafer 1 to form a groove 11.

[0030] The (111) surface of the semiconductor wafer 1 made of silicon or the like is more stable than the (110) surface. Therefore, the semiconductor wafer 1 can be etched substantially vertically along the (111) surface by, for example, alkaline etching using an alkaline chemical solution, and the grooves 11 can be easily formed even when the grooves 11 have a large length L, depth D, and aspect ratio.

[0031] (Another example of a semiconductor wafer structure) 10 to 14 are schematic cross-sectional views showing other structural examples of the semiconductor wafer 1. Note that the above description of the semiconductor wafer 1 can be appropriately applied to the same parts as those described above.

[0032] The surface 10a of the semiconductor wafer 1 shown in FIG. 10 further has protrusions 13 formed at the bottom of the grooves 11. The protrusions 13 are provided in the grooves 11 and extend, for example, in the Z-axis direction from the bottom surface of the grooves 11. The protrusions 13 are, for example, needle-shaped. The protrusions 13 are formed, for example, by forming through holes in the catalyst layer 2 along the Z-axis direction and then etching the semiconductor wafer 1. By forming through holes in the catalyst layer 2, it is possible to make it easier to etch the areas facing the openings of the contact areas between the surface 10a and the catalyst layer 2. On the other hand, the areas of the surface 10a that do not face the openings are difficult to etch and remain, forming the needle-shaped protrusions 13. By forming the protrusions 13, it is possible to further increase the surface area of ​​the surface 10a.

[0033] 11 further includes a porous region 14. The porous region 14 is formed, for example, by etching the region between adjacent grooves 11 in the semiconductor wafer 1 with a first chemical liquid or a second chemical liquid. By forming the porous region 14, the surface area of ​​the surface 10a can be further increased.

[0034] As shown in Fig. 12, the pores 14a of the porous region 14 may be blocked by filling the pores of the porous region 14 with a filler 4a. Alternatively, as shown in Fig. 13, a protective film 4b may be formed on the entire surface 10a including the porous region 14. This makes it possible to prevent the porous region 14 from being further etched by repeated use of the semiconductor wafer 1. As the filler 4a and the protective film 4b, a material having heat resistance and chemical resistance, such as carbon, silicon, silicon nitride, silicon oxide, etc., is preferable, and silicon carbide and silicon carbonitride are more preferable.

[0035] The pores 14a of the porous region 14 may be filled by dissolving the porous region 14 by annealing in a hydrogen atmosphere. The surface 10a after dissolution has a curved surface, as shown in Fig. 14. Dissolving the porous region 14 can prevent the porous region 14 from being etched.

[0036] (Example of the structure of a semiconductor device) FIG. 15 is a schematic cross-sectional view showing a structural example of a semiconductor device using a semiconductor wafer 1. The semiconductor device shown in FIG. 15 includes a film 5 provided on a semiconductor wafer 1. The film 5 is formed on a surface 10a using a film forming apparatus such as a CVD apparatus. The film 5 functions, for example, as a base film for film formation evaluation, or as a film to be etched for etching. The thickness of the film 5 is set according to the application. The film 5 may be a laminated film, and may be formed on a protective film 4b shown in FIG. 13.

[0037] (Example of how semiconductor wafers are used) As an example of a method of using the semiconductor wafer of the embodiment, an example in which the semiconductor wafer 1 is used as a dummy wafer in a manufacturing process of a semiconductor device will be described with reference to FIGS.

[0038] Fig. 16 is a schematic diagram showing a configuration example of a semiconductor manufacturing apparatus. Fig. 16 shows a configuration example of an LP-CVD (Low Pressure Chemical Vapor Deposition) apparatus. The semiconductor manufacturing apparatus 20 shown in Fig. 16 includes a processing chamber 21 and a pipe 23 for supplying a source gas 22 into the processing chamber 21. The semiconductor manufacturing apparatus 20 further includes a vacuum pump, a heater, an exhaust system, a power supply, a control circuit, etc., which are not shown.

[0039] There is a case where a semiconductor wafer 1 as a dummy wafer is carried into the same processing chamber 21 together with a device wafer 9, which is a semiconductor wafer on which a semiconductor device has been formed or is in the process of being formed, and the semiconductor wafer 1 and the device wafer 9 are processed simultaneously. In this case, an example of a method for manufacturing a semiconductor device includes a step of placing the device wafer 9 in the processing chamber 21, a step of placing the semiconductor wafer 1 of the embodiment in the processing chamber 21, and a step of processing the device wafer 9 and the semiconductor wafer 1 simultaneously in the processing chamber 21. The device wafer 9 and the semiconductor wafer 1 are placed in the processing chamber 21 in the same step or in different steps.

[0040] 16 shows an example in which, when a plurality of device wafers 9 are processed in the processing chamber 21, at least one semiconductor wafer 1 is placed in the processing chamber 21 together with the plurality of device wafers 9, and film formation processing is performed simultaneously. At least one semiconductor wafer 1 may be placed, but it is preferable to place a plurality of semiconductor wafers 1 as shown in Fig. 16. Also, it is preferable to place the semiconductor wafer 1 at least in the upper or lower region of the processing chamber 21 as shown in Fig. 16.

[0041] Here, a description will be given of an example of the structure of the device wafer 9. The semiconductor device formed on the device wafer 9 is, for example, a three-dimensional NAND flash memory. Hereinafter, a film formation process in the manufacture of the three-dimensional NAND flash memory will be described.

[0042] FIG. 17 is a schematic diagram showing a structural example of a semiconductor device. The semiconductor device shown in FIG. 17 includes a core insulating film 91, a semiconductor channel layer 92, a memory film 93 including a tunnel insulating film 931, a charge storage layer 932, and a block insulating film 933, an electrode material layer 94, a metal layer 95, and an insulating layer 96. The electrode material layer 94 functions as a gate electrode (word line). The core insulating film 91, the semiconductor channel layer 92, and the memory film 93 are formed in a memory hole H and constitute a memory cell. The block insulating film 933 is, for example, a SiO2 film (silicon oxide film). The charge storage layer 932 is, for example, a SiN film (silicon nitride film). The tunnel insulating film 931 is, for example, a laminated film including a SiO2 film and a SiON film (silicon oxynitride film). The semiconductor channel layer 92 is, for example, a polysilicon layer. The core insulating film 91 is, for example, a SiO2 film. The electrode material layer 94, the metal layer 95, and the insulating layer 96 are, for example, a W layer (tungsten layer), a TiN film (titanium nitride film), and an Al2O3 film (aluminum oxide film), respectively. In this case, the metal layer 95 functions as a barrier metal layer in the electrode layer described above, and the insulating layer 96 functions as a block insulating film together with the block insulating film 933 described above.

[0043] Next, an example of a method for manufacturing the semiconductor device shown in Fig. 17 will be described with reference to Fig. 18 and Fig. 19. In Fig. 18, a laminated film is formed on a semiconductor wafer 90 such as a silicon wafer, in which a plurality of sacrificial layers 97 and a plurality of insulating layers 98 are alternately laminated, and a memory hole H, which is a groove, is provided in these sacrificial layers 97 and insulating layers 98. The sacrificial layers 97 are regions in which electrode material layers will be formed later. The memory holes H are regions in which memory films 93 will be formed later.

[0044] The semiconductor wafer 1 is used, for example, in the formation of a memory film 93, a semiconductor channel layer 92, and a core insulating film 91 in the manufacture of a semiconductor device, or in the formation of an electrode material layer 94, a metal layer 95, and an insulating layer 96, as well as in the modification and etching of those thin films including a sacrificial layer 97 and an insulating layer 98 that constitute the side surface of a memory hole H.

[0045] The memory film 93 is formed by loading the device wafer 9, in which a memory hole H is formed in a stack of alternating sacrificial layers 97 and insulating layers 98 as shown in FIG. 18, into the processing chamber 21, and depositing a block insulating film 933, a charge storage layer 932, and a tunnel insulating film 931 in this order in the memory hole H.

[0046] The metal layer 95 and the insulating layer 96 are formed by removing the multiple sacrificial layers after the memory film 93 is formed, carrying the device wafer 9 having the cavity C between the multiple insulating layers 98 into the processing chamber 21, and depositing the insulating layer 96 and the metal layer 95 in this order in the cavity C as shown in Fig. 19. (This is called a replacement process.)

[0047] The modification process includes, for example, oxidation by performing a process with a gas containing oxygen after or during the formation of each layer or film in the process of forming the sacrificial layer 97, the insulating layer 98, the block insulating film 933, the charge storage layer 932, the tunnel insulating film, and the semiconductor channel layer 92 in Figures 18 and 19, nitridation by a gas phase process using a nitrogen-containing gas such as ammonia, and crystallization by performing a heat treatment. It also includes a process of forming a sacrificial layer containing a desired impurity such as boron, phosphorus, or metal after the formation of a layer or film, diffusing the impurity into the target layer or film by performing a heat treatment, and then etching and removing the sacrificial layer. The same applies to the electrode material layer 94, the metal layer 95, and the insulating layer 96.

[0048] The etching process includes a process of thinning a layer or film by using an etching gas containing a halogen such as fluorine, chlorine, or bromine after the formation of the layer or film, for example, for the sacrificial layer 97 and insulating layer 98 in Fig. 18, and the block insulating film 933, charge storage layer 932, tunnel insulating film, and semiconductor channel layer 92 formed in Fig. 19. The same is true for the electrode material layer 94, metal layer 95, and insulating layer 96.

[0049] In either example, at least one semiconductor wafer 1 is loaded into the processing chamber 21 together with multiple device wafers 9, and similar processing is performed. In this way, when a desired processing result cannot be obtained at a specific position in the processing chamber 21, the semiconductor wafer 1 can be used as a dummy wafer. Note that multiple processes may be performed.

[0050] As described above, the semiconductor wafer 1 has a plurality of grooves 11 formed therein so as to increase the surface area. This makes the semiconductor wafer 1 a dummy wafer having a surface area similar to that of the device wafer 9. This makes it possible to further reduce the variation in film formation in the processing chamber 21, which is caused by differences in surface area, for example, and to further improve the uniformity of the film thickness, film composition, film density, and the like between the device wafers 9 or within the surface of the device wafer 9. In other words, it becomes possible to manufacture semiconductor devices with improved reliability.

[0051] In this example of the method of use, the LP-CVD apparatus has been described as an example, but the semiconductor wafer 1 can also be applied to other semiconductor manufacturing apparatuses. Also, the semiconductor device is not limited to a 3D NAND flash memory, and other semiconductor devices can also be applied.

[0052] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims.

Claims

1. forming a catalyst layer containing at least one precious metal element selected from the group consisting of gold, silver, platinum, iridium, and palladium on a surface of a semiconductor substrate; immersing the semiconductor substrate on which the catalyst layer is formed in a first chemical solution, and partially etching the semiconductor substrate to form grooves on the surface; After forming the grooves, removing the catalyst layer from the surface with a second chemical solution; The grooves are provided in a plurality, and a porous region is formed on the surface by etching a region between adjacent grooves with the first chemical liquid or the second chemical liquid. A method for manufacturing semiconductor wafers.

2. The method of claim 1 , wherein the semiconductor substrate comprises silicon.

3. The method for producing a semiconductor wafer according to claim 1 , wherein the semiconductor substrate is a silicon wafer.

4. The method of claim 1 , wherein the at least one noble metal element comprises platinum.

5. The method for manufacturing a semiconductor wafer according to claim 1 , further comprising forming a through hole in the catalyst layer, and forming a protrusion in the groove by the etching.

6. The method for producing a semiconductor wafer according to claim 1 , further comprising forming a film containing silicon carbide or silicon carbonitride on the surface.

Citation Information

Patent Citations

  • Etching method, manufacturing method of article and semiconductor device, and etchant

    JP2016058647A

  • Method for forming hole in semiconductor substrate and mask structure used therein

    JP2017201660A

  • Capacitance reduction for pillar structured devices

    US20160356901A1

  • Self-Anchored Catalyst Metal-Assisted Chemical Etching

    US20170243751A1

  • Metal-assisted chemical etching of substrates

    WO2010114887A1