Wiring Board

The wiring board design with roughened conductor pads and coating films enhances adhesion and prevents peeling, addressing defects caused by chemical film dissolution and stress, ensuring high-quality performance.

JP7569743B2Active Publication Date: 2024-10-18IBIDEN CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021070663
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-04-19
Publication Date
2024-10-18
Estimated Expiration
2041-04-19

AI Technical Summary

Technical Problem

The chemical conversion film on the surface of metal wiring layers in existing printed wiring boards can be dissolved during subsequent treatments, leading to unintended defects and quality deterioration.

Method used

A wiring board design featuring a core substrate with laminated insulating and conductor layers, including stacked via conductors with roughened surfaces and conductor pads covered by a coating film to enhance adhesion, preventing separation and peeling between connection conductors and conductor pads.

Benefits of technology

The design provides a high-quality wiring board with improved adhesion and resistance to peeling, maintaining transmission characteristics and preventing defects due to liquid infiltration and stress-induced cracks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007569743000001
    Figure 0007569743000001
  • Figure 0007569743000002
    Figure 0007569743000002
  • Figure 0007569743000003
    Figure 0007569743000003
Patent Text Reader

Abstract

To provide a wiring board improved in quality.SOLUTION: A wiring board of an embodiment includes a core substrate and a laminate laminated on the core substrate, the laminate including: insulating layers and conductor layers laminated alternately; and a connection conductor 4 penetrating through the insulating layers. The laminate includes a stacked via conductor comprising the connection conductors 4 and conductor pads respectively included in the conductor layers, the connection conductors and the conductor pads being laminated alternately. The stacked via conductor includes at least one first conductor pad 11a having a roughened surface 110 and at least one second conductor pat 12a having a surface 120 which is covered with a coating film 5 to be roughened, the coating film improving adhesion between the insulating layers and the conductor layers. The first conductor pad 11a is laminated closer to a core substrate 3 side than the second conductor pad 12a.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wiring board. [Background technology]

[0002] Patent Document 1 discloses that, with respect to a printed wiring board, a chemical conversion coating is formed on the surface of a low-roughness or non-roughness metal wiring layer, and an insulating resin layer is formed on the metal wiring layer via this chemical conversion coating. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2018-172759 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the method disclosed in Patent Document 1, the chemical conversion film formed on the surface of the metal wiring layer may be dissolved by various treatments in later steps, which may cause unintended defects in the printed wiring board manufactured by the method of Patent Document 1 due to the dissolving liquid of the chemical conversion film, leading to deterioration in the quality of the printed wiring board. [Means for solving the problem]

[0005] The wiring board of the present invention includes a core substrate, and a laminate including insulating layers and conductor layers alternately laminated on the core substrate, and a connection conductor penetrating the insulating layers. The laminate includes a stack via conductor formed by alternately laminating the connection conductor and a conductor pad included in the conductor layer, the stack via conductor includes at least one first conductor pad having a roughened surface, and at least one second conductor pad having a roughened surface covered with a coating film that improves adhesion between the insulating layer and the conductor layer, the first conductor pad being laminated closer to the core substrate than the second conductor pad.

[0006] According to the embodiments of the present invention, it is possible to provide a high-quality wiring board that is believed to be less susceptible to problems such as peeling between the connection conductors connecting the conductor layers and the conductor pads in contact with the connection conductors. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a cross-sectional view showing an example of a wiring board according to an embodiment of the present invention. [Diagram 2] An enlarged view of part II in Figure 1. [Figure 3A] FIG. 4 is a cross-sectional view showing another example of the wiring board according to an embodiment of the present invention. [Figure 3B] FIG. 11 is a cross-sectional view showing still another example of the wiring board according to an embodiment of the present invention. [Figure 3C] 5A to 5C are cross-sectional views showing an example of a manufacturing process for the wiring board according to the embodiment of the present invention. [Figure 3D] 5A to 5C are cross-sectional views showing an example of a manufacturing process of the wiring board according to the embodiment of the present invention. [Figure 3E] 5A to 5C are cross-sectional views showing an example of a manufacturing process for the wiring board according to the embodiment of the present invention. [Figure 3F] 5A to 5C are cross-sectional views showing an example of a manufacturing process of the wiring board according to the embodiment of the present invention. [Figure 3G] 5A to 5C are cross-sectional views showing an example of a manufacturing process of the wiring board according to the embodiment of the present invention. [Figure 3H] 5A to 5C are cross-sectional views showing an example of a manufacturing process for the wiring board according to the embodiment of the present invention. [Figure 3I] 5A to 5C are cross-sectional views showing an example of a manufacturing process of the wiring board according to the embodiment of the present invention. [Figure 3J] 5A to 5C are cross-sectional views showing an example of a manufacturing process of the wiring board according to the embodiment of the present invention. [Figure 3K] 5A to 5C are cross-sectional views showing an example of a manufacturing process of the wiring board according to the embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] A wiring board according to an embodiment of the present invention will be described with reference to the drawings. Fig. 1 is a cross-sectional view showing a wiring board 100, which is an example of a wiring board according to an embodiment. Note that the wiring board 100 is merely an example of a wiring board according to the present embodiment. The laminated structure of the wiring board according to the embodiment and the number of each of the conductor layers and the insulating layers are not limited to the laminated structure of the wiring board 100 shown in Fig. 1 and the number of each of the conductor layers and the insulating layers included in the wiring board 100.

[0009] 1, wiring board 100 includes a core substrate 3 and a laminate including insulating layers and conductor layers alternately laminated on each of two main surfaces (first surface 3a and second surface 3b) opposing each other in the thickness direction of core substrate 3. Core substrate 3 includes insulating layer 32 and conductor layers 31 formed on both surfaces of insulating layer 32.

[0010] In the description of the embodiment, the side of the wiring board 100 farther from the insulating layer 32 in the thickness direction is also referred to as the "upper side," "upper," or "outer side," or simply "upper" or "outer," and the side closer to the insulating layer 32 is also referred to as the "lower side," "lower," or "inner side," or simply "lower" or "inner." Furthermore, in each conductor layer and each insulating layer, the surface facing the side opposite the insulating layer 32 is also referred to as the "upper surface," and the surface facing the insulating layer 32 is also referred to as the "lower surface."

[0011] The wiring board 100 includes a first insulating layer 21, a first conductor layer 11, a second insulating layer 22, a second conductor layer 12, a third insulating layer 23, a third conductor layer 13, a fourth insulating layer 24, and a fourth conductor layer 14, which are laminated on the first surface 3a of the core substrate 3 in this order from the first surface 3a side. The first insulating layer 21 covers the first surface 3a of the core substrate 3, and the second insulating layer 22 covers the first conductor layer 11 and the first insulating layer 21 that is not covered by the first conductor layer 11 and is exposed. The wiring board 100 further includes four insulating layers 25 and four conductor layers 15, which are alternately laminated on the second surface 3b of the core substrate 3.

[0012] In each insulating layer, a connection conductor is formed which penetrates the insulating layer and connects adjacent conductor layers via the insulating layer. The first insulating layer 21, the second insulating layer 22, the third insulating layer 23, the fourth insulating layer 24, and the four insulating layers 25 each include a connection conductor 4. The insulating layer 32 of the core substrate 3 includes a connection conductor 33. The connection conductor 33 is a so-called through-hole conductor which connects the conductor layers 31 on both sides of the core substrate 3 to each other.

[0013] The connection conductor 4 is a so-called via conductor formed in each insulating layer that is built up in sequence. The connection conductor 4 included in the first insulating layer 21 connects the conductor layer 31 and the first conductor layer 11. The connection conductor 4 included in the second insulating layer 22 connects the first conductor layer 11 and the second conductor layer 12. The connection conductor 4 included in the third insulating layer 23 connects the second conductor layer 12 and the third conductor layer 13, and the connection conductor 4 included in the fourth insulating layer 24 connects the third conductor layer 13 and the fourth conductor layer 14. The connection conductor 4 included in each of the four insulating layers 25 connects the conductor layer 31 and the conductor layer 15, or connects the conductor layers 15 together.

[0014] The first to fourth insulating layers 21, 22, 23, 24, insulating layer 25, and insulating layer 32 are formed of any insulating resin. Examples of insulating resins include epoxy resin, bismaleimide triazine resin (BT resin), and phenol resin. In the example of FIG. 1, insulating layer 32 includes a core material (reinforcing material) 32a formed of glass fiber, aramid fiber, or the like. Although not shown in FIG. 1, each insulating layer other than insulating layer 32 may also include a core material made of glass fiber or the like. Each insulating layer may further include an inorganic filler (not shown) made of fine particles such as silica (SiO2), alumina, or mullite.

[0015] The first to fourth conductor layers 11, 12, 13, 14, conductor layer 15, and conductor layer 31, as well as the connecting conductor 4 and connecting conductor 33, are formed using any metal such as copper or nickel. In the example of Fig. 1, the conductor layer 31 includes a metal foil 31a, a metal film 31b, and a plating film 31c. The connecting conductor 33 is formed integrally with the conductor layer 31, and is composed of the metal film 31b and the plating film 31c.

[0016] On the other hand, the first to fourth conductor layers 11, 12, 13, 14, and conductor layer 15, and the connecting conductor 4 are each composed of a metal film 10b and a plating film 10c. Each connecting conductor 4 is formed integrally with the first to fourth conductor layers 11, 12, 13, 14, or conductor layer 15. The plating films 31c and 10c are, for example, electrolytic plating films. The metal films 31b and 10b are, for example, electroless plating films or sputtering films, and function as power supply layers when the plating films 31c and 10c are formed by electrolytic plating, respectively.

[0017] A solder resist 6 is formed on the fourth insulating layer 24 and the fourth conductor layer 14. A solder resist 6 is also formed on the outer insulating layer 25 and conductor layer 15 on the second surface 3b side of the core substrate 3. The solder resist 6 has an opening 6a that exposes a part of the fourth conductor layer 14 or the conductor layer 15. The solder resist 6 is formed of, for example, a photosensitive epoxy resin or a polyimide resin.

[0018] Each of the first to fourth conductor layers 11, 12, 13, 14, the four conductor layers 15, and the two conductor layers 31 includes a predetermined conductor pattern. The first conductor layer 11 includes a first conductor pad 11a and a first wiring pattern 11b. The second conductor layer 12 includes a second conductor pad 12a and a second wiring pattern 12b.

[0019] The first conductive pad 11a is in contact with the connection conductor 4 penetrating the second insulating layer 22. That is, the first conductive pad 11a is a conductive pad on which the connection conductor 4 is formed, and is a so-called receiving pad for the connection conductor 4 penetrating the second insulating layer 22. Therefore, a part of the surface of the first conductive pad 11a on the second insulating layer 22 side is covered by the connection conductor 4 penetrating the second insulating layer 22. In other words, a part of the surface of the first conductive pad 11a on the second insulating layer 22 side faces the bottom surface of the connection conductor 4 penetrating the second insulating layer 22. And the second conductive pad 12a is a receiving pad for the connection conductor 4 penetrating the third insulating layer 23, and a part of the surface of the second conductive pad 12a on the third insulating layer 23 side faces the bottom surface of the connection conductor 4 penetrating the third insulating layer 23.

[0020] 1, the connection conductor 4 penetrating the first insulating layer 21, the connection conductor 4 penetrating the second insulating layer 22, the connection conductor 4 penetrating the third insulating layer 23, and the connection conductor 4 penetrating the fourth insulating layer 24 are stacked to form a so-called stacked via conductor. Therefore, the first conductive pad 11a is provided as a so-called via pad of the connection conductor 4 (via conductor) penetrating the first insulating layer 21. And the second conductive pad 12a is provided as a via pad of the connection conductor 4 (via conductor) penetrating the second insulating layer 22.

[0021] The first wiring pattern 11b and the second wiring pattern 12b are conductor patterns that function as conductive paths used for transmitting any electric signal or supplying power. The first wiring pattern 11b is covered with a second insulating layer 22 on the surface other than the surface facing the first insulating layer 21. The second wiring pattern 12b is covered with a third insulating layer 23 on the surface other than the surface facing the second insulating layer 22. The first wiring pattern 11b and the second wiring pattern 12b may be transmission paths for high-frequency signals, for example, exceeding several GHz, but are not limited thereto.

[0022] FIG. 2 shows an enlarged view of part II in FIG. 1. Although omitted in FIG. 1 referred to so far, as shown in FIG. 2, a coating film 5 is formed on the surface of the second conductor layer 12 facing the third insulating layer 23. That is, the wiring board 100 further includes a coating film 5 interposed between the second conductor layer 12 and the third insulating layer 23. Note that "the surface of the second conductor layer 12 facing the third insulating layer 23" means the area of ​​the surface of the second conductor layer 12 facing the third insulating layer 23. Similarly, "the surface of the second conductor pad 12a and the second wiring pattern 12b facing the third insulating layer 23" of each of the second conductor pad 12a and the second wiring pattern 12b described later means the area of ​​the surface of each of the second conductor pad 12a and the second wiring pattern 12b facing the third insulating layer 23.

[0023] 2, the coating film 5 is formed on the entire surface of the second conductor layer 12 facing the third insulating layer 23. However, the coating film 5 may be formed on only a portion of the surface of the second conductor layer 12 facing the third insulating layer 23. It is sufficient that the coating film 5 is formed on at least a portion of the surface of the second conductor pad 12a facing the third insulating layer 23. Note that the "surface of the second conductor layer 12 facing the third insulating layer 23" does not include the portion of the surface of the second conductor pad 12a that is covered by the connection conductor 4 that penetrates the third insulating layer 23.

[0024] The coating film 5 improves the adhesion between the second conductor layer 12 and the third insulating layer 23. The coating film 5 is formed of a material that can bond with both an organic material such as a resin constituting the third insulating layer 23 and an inorganic material such as a metal constituting the second conductor layer 12. The coating film 5 is formed of a material that includes both a reactive group that can chemically bond with an organic material and a reactive group that can chemically bond with an inorganic material. Therefore, each conductor pattern of the second conductor layer 12 covered with the coating film 5 and the third insulating layer 23 are adhered with sufficient strength. An example of the material of the coating film 5 is a silane coupling agent containing an azole silane compound such as a triazole compound. Note that the material of the coating film 5 is not limited to a silane coupling agent as long as it can increase the adhesion strength between the second conductor layer 12 and the third insulating layer 23 compared to the case where the third insulating layer 23 is directly formed on the second conductor layer 12.

[0025] 2, in this embodiment, the surface 121 of the second wiring pattern 12b of the second conductor layer 12 that faces the third insulating layer 23 is covered with the coating film 5. That is, the adhesion between the second wiring pattern 12b and the third insulating layer 23 is improved compared to the case where there is no coating film 5. Therefore, it is considered that the third insulating layer 23 is less likely to lift or peel off from the second wiring pattern 12b.

[0026] In this embodiment, the surface 120 of the second conductive pad 12a facing the third insulating layer 23 is covered with the coating film 5. That is, the adhesion between the second conductive pad 12a and the third insulating layer 23 is also improved compared to the case where there is no coating film 5. Therefore, it is considered that the third insulating layer 23 is less likely to lift or peel off from the second conductive pad 12a.

[0027] 2, each conductor pattern (second conductor pad 12a, second wiring pattern 12b, etc.) of second conductor layer 12 has different degrees of unevenness on the surface not in contact with second insulating layer 22. In other words, second conductor layer 12 has a plurality of regions with different surface roughness on the surface (surface 120 and surface 121) facing third insulating layer 23 and on surface 124 covered by connecting conductor 4. In the example of FIG. 2, the concave portions of the unevenness of surface 120 and surface 121 are filled with coating film 5.

[0028] In the second conductor layer 12 shown in FIG. 2, the height difference of the unevenness on the surface 120 of the second conductor pad 12a facing the third insulating layer 23 is larger than the height difference of the unevenness on the surface 121 of the second wiring pattern 12b facing the third insulating layer 23. The surface 120 of the second conductor pad 12a has a surface roughness (first surface roughness) higher than the surface roughness (second surface roughness) of the surface 121 of the second wiring pattern 12b. The surface 120 of the second conductor pad 12a is roughened to have a first surface roughness higher than the second surface roughness. As described later, the surface 120 of the second conductor pad 12a is roughened by, for example, microetching.

[0029] On the other hand, the surface 121 of the second wiring pattern 12b does not have to be roughened by a process specifically provided for roughening the surface 121. The unevenness of the surface 121 may be caused by grain boundaries of the plating film 10c or unevenness on the surface of the plating resist when the plating film 10c is formed.

[0030] In the wiring board 100 of this embodiment, the surface 120 of the second conductive pad 12a is roughened to have a relatively high surface roughness (first surface roughness). Therefore, peeling between the second conductive pad 12a and the third insulating layer 23 may be suppressed. Specifically, the unevenness of the surface 120 of the second conductive pad 12a, which has a relatively high first surface roughness, prevents unintended liquid from penetrating the interface between the second conductive pad 12a and the third insulating layer 23. As a result, peeling between the second conductive pad 12a and the third insulating layer 23, which may be caused by such liquid penetration, may be suppressed.

[0031] More specifically, in the manufacturing process of the wiring board 100, the inner wall of the through hole 4a provided in the third insulating layer 23 for forming the connection conductor 4 may be exposed to various processing solutions, plating solutions, and the like. These liquids may penetrate from the inner wall of the through hole 4a into the interface between the second conductive pad 12a and the third insulating layer 23, causing peeling between the second conductive pad 12a and the third insulating layer 23. However, in this embodiment, the intrusion of unintended liquid that may cause such peeling is prevented by the unevenness of the surface 120 of the second conductive pad 12a, which has a relatively high first surface roughness.

[0032] In the example shown in FIG. 2, the surface 121 of the second wiring pattern 12b has a surface roughness (second surface roughness) lower than the first surface roughness of the surface 120 of the second conductive pad 12a. For example, if the wiring pattern has a highly roughened surface, it is considered that the substantial impedance increases due to the influence of the skin effect in the transmission of high-frequency signals, and the transmission characteristics deteriorate. In addition, in a fine wiring pattern of, for example, about 10 μm / 10 μm (wiring width / wiring spacing) or less, if the surface is highly roughened, a desired shape may not be obtained after roughening for the designed wiring width and thickness. As in this embodiment, if the surface 121 of the second wiring pattern 12b has a relatively low surface roughness, at least a second surface roughness lower than the first surface roughness, it is considered that problems such as deterioration of high-frequency transmission characteristics due to high surface roughness are unlikely to occur.

[0033] 2, the surface 121 of the second wiring pattern 12b is also covered with a coating film 5 that improves the adhesion between the second wiring pattern 12b and the third insulating layer 23. In general, the so-called anchor effect is not sufficiently obtained between a conductor layer having a surface with a relatively low surface roughness and an insulating layer formed on the surface of the conductor layer, and as a result, peeling between the conductor layer and the insulating layer may occur. However, since the surface 121 of the second wiring pattern 12b of this embodiment is covered with the coating film 5, it is considered that peeling between the second wiring pattern 12b and the third insulating layer 23 is unlikely to occur.

[0034] Furthermore, in this embodiment, the unevenness of the surface 120 of the second conductive pad 12a may prevent quality deterioration due to dissolution of the coating film 5 formed on the surface 120 of the second conductive pad 12a. As described above, in the manufacturing process of the wiring board 100, the inner wall of the through hole 4a provided in the third insulating layer 23 may be exposed to various liquids. When the liquid penetrates into the interface between the second conductive pad 12a and the third insulating layer 23, the penetrating liquid may dissolve the coating film 5 formed on the surface 120 of the second conductive pad 12a. In that case, the coating film 5 may dissolve into the through hole 4a, causing a connection failure between the connection conductor 4 and the second conductive pad 12a, or peeling may occur between the second conductive pad 12a and the third insulating layer 23 at the point where the coating film 5 is dissolved. However, in this embodiment, the unevenness of the surface 120 of the second conductive pad 12a, which has a relatively high first surface roughness, prevents the intrusion of unintended liquid that may cause the dissolution of the coating film 5.

[0035] As shown in FIG. 2, in this embodiment, the coating film 5 is not formed on the surface of the first conductor layer 11, which is laminated on an inner layer than the second conductor layer 12, facing the second insulating layer 22. Here, "the surface of the first conductor layer 11 facing the second insulating layer 22" means the area of ​​the surface of the first conductor layer 11 facing the second insulating layer 22. That is, the surfaces of the first conductor pad 11a and the first wiring pattern 11b included in the first conductor layer 11 facing the second insulating layer 22 are not covered with the coating film 5. However, the coating film 5 may be formed on a part of the surface of the first conductor layer 11 facing the second insulating layer 22. For example, the first conductor layer 11 may include any conductor pattern whose surface facing the second insulating layer 22 is covered with the coating film 5 in addition to the first wiring pattern 11b not covered with the coating film 5.

[0036] 2, the surface 110 of the first conductive pad 11a and the second insulating layer 22 are in direct contact without the intermediation of the coating film 5. Also, the surface 111 of the first wiring pattern 11b and the second insulating layer 22 are in direct contact without the intermediation of the coating film 5. On the other hand, both the surface 110 of the first conductive pad 11a and the surface 111 of the first wiring pattern 11b have a surface roughness substantially equal to the surface roughness (first surface roughness) of the surface 120 of the second conductive pad 12a included in the second conductive layer 12. That is, in the first conductive layer 11, the surface 110 of the first conductive pad 11a and the surface 111 of the first wiring pattern 11b are roughened by, for example, microetching.

[0037] In a wiring board on which a stack via conductor is formed, thermal stress or the like may cause stress to the stack via conductor or distortion of the stack via conductor. These stresses may concentrate at the bottom of the via, causing cracks at the via connection of the stack via conductor, or the cracks may cause peeling at the interface with the insulating layer. However, in this embodiment, since the first conductor layer 11, which is an inner layer on which stress tends to concentrate, is formed to have a high surface roughness, it is considered that a sufficient anchor effect that can suppress peeling can be obtained between the first conductor pad 11a and the second insulating layer 22. Similarly, a sufficient anchor effect can be obtained between the first wiring pattern 11b and the second insulating layer 22. It is considered that the anchor effect brought about by the surface having the first surface roughness is greater than the improved adhesion between the conductor layer and the insulating layer that can be provided by the coating film 5. A highly reliable wiring board 100 that is less likely to crack or peel at the interface can be provided.

[0038] When the wiring board 100 has a core board such as the core board 3 as shown in FIG. 1, it is considered that the insulating layer and the conductor layer on the inner layer side close to the core board 3 have a lower degree of freedom in terms of displacement and deformation than the outer layer side far from the core board 3. For this reason, it is considered that stress is difficult to be relaxed on the inner layer side, and stress from the outer layer side is also easily applied. However, it is presumed that substantial defects such as interfacial peeling and cracks are unlikely to occur at the interface between the conductor layer 31 of the core board 3 and the connection conductor 4 penetrating the insulating layer 21 because the rigidity of the core board 3 itself is high. Therefore, among the multiple connection conductors 4 constituting the stack via conductor, the connection conductor 4 penetrating the insulating layer 22, which is the second closest to the core board 3 after the connection conductor 4 penetrating the insulating layer 21, may be most likely to cause substantial defects due to concentrated stress. Therefore, as in the wiring board 100 of FIG. 1, it may be preferable that the connection conductor 4 penetrating the insulating layer 22, which is the second closest to the core board 3, is connected to the first conductor pad 11a. As mentioned above, the surface 110 of the first conductor pad 11a has a high surface roughness and a sufficient anchor effect is obtained between the surface 110 and the second insulating layer 22, so that it is considered that interfacial peeling between the connecting conductor 4 and the first conductor layer 11 to which the connecting conductor 4 is connected and cracks near the interface are effectively prevented.

[0039] In this way, in the wiring board 100, quality deterioration due to peeling between the first conductor pad 11a, which is in contact with the connecting conductor 4 of the stack via conductor, and the second insulating layer 22, and peeling between the second conductor pad 12a and the third insulating layer 23, etc. can be suppressed, and it is believed that good transmission characteristics and sufficient adhesion to the third insulating layer 23 can be obtained in the second wiring pattern 12b.

[0040] For example, the surface roughness (first surface roughness) of the surface 110 of the first conductive pad 11a, the surface 120 of the second conductive pad 12a, and the surface 111 of the first wiring pattern 11b may be, for example, 0.3 μm or more and 0.6 μm or less in arithmetic mean roughness (Ra). With this level of surface roughness, a good anchor effect that can suppress the occurrence of peeling between the first conductive pad 11a and the second insulating layer 22 can be obtained.

[0041] 2, the surface of the coating film 5 covering the surface 120 of the second conductive pad 12a, which faces the third insulating layer 23, has undulations due to the unevenness of the surface 120. When the surface 120 of the second conductive pad 12a has the above-mentioned degree of surface roughness, the contact area between the coating film 5 and the third insulating layer 23 increases compared to when the surface of the coating film 5 is flat, and in addition to the adhesion improving effect of the coating film 5, an adhesion improving effect due to the increased contact area may be obtained.

[0042] For example, the first surface roughness of the surface 110 of the first conductive pad 11a, the surface 120 of the second conductive pad 12a, and the surface 111 of the first wiring pattern 11b is 100% or more higher than the surface roughness (second surface roughness) of the surface 121 of the second wiring pattern 12b. For example, the first surface roughness can be 200% or more and 1200% or less of the second surface roughness. It is considered that while almost completely preventing the infiltration of liquid into the interface between the second conductive pad 12a and the third insulating layer 23, good transmission characteristics for high-frequency signals of the order of several GHz can be obtained in the second wiring pattern 12b as necessary. Since the surface roughness of the surface 121 of the second wiring pattern 12b is small, it is presumed that the anchor effect obtained on the surface 121 of the second wiring pattern 12b is small, but the surface 121 of the second wiring pattern 12b is covered with the coating film 5 as described above. It is believed that interfacial peeling between the second wiring pattern 12b and the third insulating layer 23, the adhesion of which is enhanced by the coating film 5, is unlikely to occur.

[0043] 2, there is no coating film 5 between the surface 124 of the second conductive pad 12a covered by the connection conductor 4 and the connection conductor 4. That is, the second conductive pad 12a and the connection conductor 4 are in direct contact with each other. For example, without an organic material such as a silane coupling agent, the metal such as copper constituting the second conductive pad 12a and the metal such as copper constituting the connection conductor 4 are in direct contact with each other at the interface between the second conductive pad 12a and the connection conductor 4. Therefore, it is considered that a mechanically strong metal-metal bond with low electrical resistance is obtained at the interface between the second conductive pad 12a and the connection conductor 4.

[0044] Of the surface of the second conductive pad 12a, the region 124 covered by the connection conductor 4 may have a surface roughness (third surface roughness) lower than the first surface roughness of the surface 120 of the second conductive pad 12a facing the third insulating layer 23. The third surface roughness is higher than the second surface roughness of the surface 121 of the second wiring pattern 12b. The third surface roughness may be any surface roughness between the first surface roughness and the second surface roughness. As described above, since the second conductive pad 12a and the connection conductor 4 are firmly bonded to each other by metals, it is considered that even if the third surface roughness is lower than the first surface roughness, interfacial peeling is unlikely to occur between the second conductive pad 12a and the connection conductor 4. Similarly, of the surface of the first conductive pad 11a, the surface 114 covered by the connection conductor 4 may have a surface roughness (third surface roughness) lower than the first surface roughness of the surface 110 facing the second insulating layer 22.

[0045] Up to now, with reference to FIG. 1, a stack via conductor formed by stacking connection conductors 4 on the first surface 3a side of the core substrate 3 has been described as an example of a stack via conductor, but the stack via conductor is not limited to this example. A stack via conductor having a structure including an inner layer via pad having a roughened surface and an outer layer via pad having a roughened surface covered with a coating film as shown in FIG. 2 may also be formed on the second surface 3b side of the core substrate 3. In other words, the stack via conductor having the structure of the embodiment may be formed on the component mounting surface side of the wiring substrate 100, or may be formed on the opposite surface side to the component mounting surface. In addition, the stack via conductor referred to in FIG. 1 is formed at a position overlapping in a plan view with a stack via conductor formed by stacking connection conductors 4 on the second surface 3b side of the core substrate 3. Here, "plan view" means that the wiring substrate 100 is viewed along its thickness direction. However, each stack via conductor formed on the first surface 3a of the core substrate 3 and the stack via conductor formed on the second surface 3b may be formed at different positions in a plan view, and may be formed at positions overlapping or different from the through-hole conductors (connection conductors 33) in a plan view. Any stack via conductor may be formed as a stack via conductor having the structure of the embodiment shown in FIG.

[0046] In the example shown in FIG. 1, the first conductor layer 11 is a conductor layer including a conductor pad having a high first surface roughness that is not covered by the coating film 5, and the second conductor layer 12 directly above it is a conductor layer including a conductor pad having a high first surface roughness that is covered by the coating film 5. However, the stacked via conductor of this embodiment only needs to include at least one conductor pad having a high first surface roughness that is not covered by the coating film 5 in the inner layer, and at least one conductor pad having a high first surface roughness that is covered by the coating film 5 in the outer layer. It is considered that cracks at the interface between the insulating layer and the conductor pad due to stress that tends to concentrate on the inner layer side and peeling of the insulating layer are suppressed by a good anchor effect due to the large unevenness of the first surface roughness that is exposed without being covered by the coating film 5. For example, a conductor pad having a high first surface roughness that is not covered by the coating film 5 and that forms the stacked via conductor may be included in the first conductor layer 11, and a conductor pad having a high first surface roughness that is covered by the coating film 5 and that forms the stacked via conductor may be included in the third conductor layer 13 or even an outer conductor layer. Furthermore, the stacked via conductor may include a plurality of conductor pads that are not covered with the covering film 5 and have a high first surface roughness and / or a plurality of conductor pads that are covered with the covering film 5 and have a high first surface roughness.

[0047] Next, a method for manufacturing a wiring board according to an embodiment will be described with reference to FIGS. 3A to 3K using wiring board 100 of FIG. 1 as an example.

[0048] As shown in FIG. 3A, a starting substrate (e.g., a double-sided copper-clad laminate) is prepared, which includes an insulating layer that will become the insulating layer 32 of the core substrate 3 and metal foils 31a laminated on both surfaces of the insulating layer, and the conductor layer 31 and the connection conductor 33 of the core substrate 3 are formed. For example, a through hole is formed at the formation position of the connection conductor 33 by drilling or irradiation with a carbon dioxide laser beam, and a metal film 31b is formed in the through hole and on the metal foil 31a by electroless plating or sputtering. Then, a plating film 31c is formed by electrolytic plating using the metal film 31b as a power supply layer. As a result, a three-layered conductor layer 31 and a two-layered connection conductor 33 are formed. Thereafter, the conductor layer 31 is patterned by a subtractive method to obtain a core substrate 3 having a predetermined conductor pattern.

[0049] 3A, the first insulating layer 21 and the insulating layer 25 are formed on the first surface 3a and the second surface 3b of the core substrate 3, respectively. In forming the first insulating layer 21 and the insulating layer 25, for example, a film-like epoxy resin is laminated on the core substrate 3, and heated and pressurized. As a result, the first insulating layer 21 and the insulating layer 25 are formed. The first insulating layer 21 and the insulating layer 25 may be formed of any resin, such as BT resin or phenol resin, and are not limited to a film-like epoxy resin. In the first insulating layer 21 and the insulating layer 25, a through hole 4a for forming the connection conductor 4 is formed, for example, by irradiation with a carbon dioxide laser beam.

[0050] A first conductor layer 11 having a first conductor pad 11a and a first wiring pattern 11b is formed. A conductor layer 15 is formed on the second surface 3b side of the core substrate 3. A connection conductor 4 is formed on each of the first insulating layer 21 and the insulating layer 25. The first conductor layer 11, the conductor layer 15, and the connection conductor 4 are formed by using, for example, a semi-additive method. That is, a metal film 10b is formed in the through hole 4a and on the surfaces of the first insulating layer 21 and the insulating layer 25 by, for example, electroless plating or sputtering.

[0051] A plating resist (not shown) having openings corresponding to the first conductive pad 11a and the first wiring pattern 11b, or openings corresponding to the conductive pattern to be included in the conductive layer 15, is provided on the metal film 10b. Then, a plating film 10c is formed in the openings of the plating resist by electrolytic plating using the metal film 10b as a power supply layer. As a result, the first conductive layer 11 and the conductive layer 15 each made of the metal film 10b and the plating film layer 10c are formed. A connection conductor 4 made of the metal film 10b and the plating film layer 10c is formed in the through hole 4a. Thereafter, the plating resist is removed using an alkaline stripping agent such as sodium hydroxide, and then the exposed part of the metal film 10b that is not covered by the plating film 10c is removed by etching or the like.

[0052] Next, as shown in Fig. 3B, the exposed surface of first conductor layer 11, which is a region of the surface of first conductor layer 11 that is not in contact with first insulating layer 21, is roughened. Fig. 3B is an enlarged view of the exposed surface of first conductor layer 11 in part IIIB of Fig. 3A after roughening treatment.

[0053] The exposed surface of the first conductor layer 11 may be roughened by any method, for example, a surface oxidation treatment called blackening or browning, or a microetching treatment using an acidic solvent.

[0054] The roughening treatment roughens the exposed surfaces of the first conductive pads 11a and the first wiring pattern 11b of the first conductive layer 11. The exposed surfaces of the first conductive pads 11a and the first wiring pattern 11b are roughened to have a surface roughness of, for example, 0.3 μm or more and 0.6 μm or less in arithmetic mean roughness (Ra).

[0055] Next, as shown in FIG. 3C, a second insulating layer 22 is formed to cover the first conductor layer 11. An insulating layer 25 having two levels is further formed on the second surface 3b side of the core substrate 3. The "levels" are the numbers given to each insulating layer or conductor layer when the multiple insulating layers or conductor layers laminated on the first surface 3a side and the second surface 3b side are sequentially given numbers that increase by one from the core substrate 3 side, starting from 1. The second insulating layer 22 and the insulating layer 25 having two levels are formed, for example, by laminating film-like epoxy resin and applying heat and pressure, similar to the first insulating layer 21 and the insulating layer 25 having one level.

[0056] In the second insulating layer 22 and the insulating layer 25 with the number of floors being two, a through hole 4a for forming the connecting conductor 4 is formed, for example, by irradiation with a carbon dioxide laser beam. For example, the second conductor layer 12 and the conductor layer 15 with the number of floors being two may be formed in the same manner as in the formation of the first conductor layer 11 and the conductor layer 15 with the number of floors being one described above. In the through hole 4a, for example, the connecting conductor 4 penetrating the second insulating layer 22 is formed in the same manner as in the formation of the connecting conductor 4 penetrating the first conductor layer 11 and the first insulating layer 21 described above.

[0057] As shown in Figures 3D and 3E, the exposed surface of the second conductor layer 12, which is a region not in contact with the second insulating layer 22, is roughened. However, the exposed surface of the second wiring pattern 12b is not roughened. On the other hand, the exposed surface of the second conductor pad 12a is roughened. Therefore, as shown in Figures 3D and 3E, a resist film R1 having an opening R1a exposing the second conductor pad 12a is provided on the second insulating layer 22 and the second conductor layer 12.

[0058] The exposed surface of the second conductor layer 12 may be roughened by any method. For example, the exposed surface of the second conductor layer 12 may be roughened by the same treatment as that for roughening the exposed surface of the first conductor layer 11. By the treatment, the portion of the exposed surface of the second conductor layer 12 that is not covered by the resist film R1, i.e., the exposed surface of the second conductor pad 12a, is roughened.

[0059] The resist film R1 is formed by laminating films containing, for example, photosensitive resin. The resist film R1 is provided with an opening R1a that exposes the second conductive pad 12a by using a photolithography technique such as exposure and development. The resist film R1 may be formed of the same material as the plating resist (not shown) used to form the first conductive layer 11 described above.

[0060] Fig. 3E shows an enlarged view of the exposed surface of the second conductor layer 12 in part IIIE of Fig. 3D after roughening treatment. The exposed surface of the second conductor pad 12a is roughened to have a surface roughness at least higher than the surface roughness (second surface roughness) of the unroughened surface 121 of the second wiring pattern 12b. The exposed surface of the second conductor pad 12a is roughened to have a surface roughness of, for example, 0.3 μm or more and 0.6 μm or less in arithmetic mean roughness (Ra).

[0061] After removing the resist film R1, as shown in Fig. 3F, a coating film 5 is provided on the exposed surface of the second conductor layer 12. Fig. 3F shows a state after the coating film 5 has been formed for a portion similar to that of Fig. 3E.

[0062] The coating film 5 improves adhesion between the second conductor layer 12 and a third insulating layer 23 (see FIG. 3G) formed in a later process. The coating film 5 is formed, for example, by immersing the second conductor layer 12 in a liquid containing a material capable of bonding with both organic and inorganic materials, such as a silane coupling agent, or by spraying such a liquid. However, the method of forming the coating film 5 is arbitrary and is not limited to immersion in a material constituting the coating film 5 or spraying such a material.

[0063] As shown in FIG. 3G and FIG. 3H, a third insulating layer 23 is formed to cover the second conductor layer 12. An insulating layer 25 having three layers is further formed on the second surface 3b side of the core substrate 3. FIG. 3H shows an enlarged view of the IIIH portion in FIG. 3G. As shown in FIG. 3H, the third insulating layer 23 also covers the coating film 5. The third insulating layer 23 and the insulating layer 25 having three layers are formed, for example, by laminating a film-like epoxy resin and applying heat and pressure, similar to the first and second insulating layers 21 and 22 and the insulating layers 25 having one and two layers.

[0064] Through holes 4a for forming connection conductors 4 (see FIG. 3I) in a later process are formed in the second insulating layer 22 and the third insulating layer 23, for example, by irradiation with a carbon dioxide laser beam. The through holes 4a are formed in the third insulating layer 23 in regions above the second conductive pads 12a. A portion of the surface (surface 124) of the second conductive pads 12a is exposed by the through holes 4a.

[0065] In the example of FIG. 3H, the coating film 5 formed on the surface 124 of the second conductive pad 12a exposed in the through hole 4a by the formation of the through hole 4a is removed. The coating film 5 formed on the surface 124 is melted and vaporized or sublimated, for example, by irradiation with a laser beam when the through hole 4a is formed. As a result, the coating film 5 formed on the surface 124 can be removed. By removing the coating film 5 from the surface 124, the connection conductor 4 formed on the conductive pad in a later process and the second conductive pad 12a can be firmly joined between metals with low electrical resistance.

[0066] In addition, when removing the coating film 5, the penetration of the dissolving solution of the coating film 5 into the interface between the second conductive pad 12a and the third insulating layer 23 is prevented by the unevenness of the surface 120 of the second conductive pad 12a, which has been roughened to have a relatively high surface roughness as described above. This may prevent interfacial peeling between the second conductive pad 12a and the third insulating layer 23.

[0067] After the through-hole 4a is formed, a desmear process is preferably performed to remove resin residue (smear) caused by the formation of the through-hole 4a. For example, the smear in the through-hole 4a is removed by exposing the inner wall of the through-hole 4a to a treatment liquid such as an alkaline permanganate solution. The intrusion of the treatment liquid for this desmear process into the interface between the second conductor pad 12a and the third insulating layer 23 is prevented by the unevenness of the roughened surface 120 of the second conductor pad 12a. It is believed that this prevents the dissolution of the coating film 5 on the surface 120 by the treatment liquid and the associated problems such as interface peeling.

[0068] Preferably, a soft etching process is performed before the formation of the third conductor layer 13 and the connection conductor 4 (see FIG. 3I) in a later process. The soft etching process removes oxide films and the like from the surfaces (exposed portions of the surface 120 of the second conductor pad 12a and the surface of the third insulating layer 23) on which the third conductor layer 13 and the connection conductor 4 are formed. This soft etching process reduces the surface roughness of the connection region 124 exposed in the through hole 4a of the surface 120 of the second conductor pad 12a to a surface roughness (third surface roughness) lower than the first surface roughness of the surface 120 facing the third insulating layer 23. An example of this is shown in FIG. 3H.

[0069] Although not shown in Fig. 3C, a soft etching process may also be performed before the formation of the second conductor layer 12 and the connection conductor 4. This soft etching process may also reduce the surface roughness of the connection region 114, which is the region of the surface 110 of the first conductor pad 11a that is exposed in the through hole 4a and connected to the connection conductor 4, below the surface roughness of the surface 110 facing the second insulating layer 22 (see Figs. 2 and 3H).

[0070] As shown in Figures 3I and 3J, a third conductor layer 13 is formed on the third insulating layer 23, and a connection conductor 4 is formed to penetrate the third insulating layer 23 and connect the second conductor pad 12a and the third conductor layer 13. A conductor layer 15 and a connection conductor 4 are further formed on the second surface 3b side of the core substrate 3. Figure 3J shows an enlarged view of part IIIJ in Figure 3I.

[0071] The connection conductor 4 penetrating the third conductor layer 13 and the third insulating layer 23 is formed, for example, by a method similar to the method for forming the connection conductor 4 penetrating the first conductor layer 11 and the first insulating layer 21 described above. For example, the connection conductor 4 penetrating the third conductor layer 13 and the third insulating layer 23, and the conductor layer 15 of the third layer further formed on the second surface 3b side of the core substrate 3 and the connection conductor 4 are formed by a semi-additive method.

[0072] In forming the connection conductor 4 on the third insulating layer 23 by the semi-additive method, as shown in Fig. 3J, a metal film 10b is formed in the through hole 4a by, for example, electroless plating, and a plating film 10c is further formed by electrolytic plating. In the method for manufacturing a wiring board of this embodiment, the intrusion of a plating solution into the interface between the second conductor pad 12a and the third insulating layer 23 during the formation of the metal film 10b is prevented by the unevenness of the roughened surface 120 of the second conductor pad 12a. It is believed that this prevents the dissolution of the coating film 5 on the surface 120 by the plating solution and the resulting problems such as interface peeling.

[0073] Next, in the same manner as the formation of the first conductor layer 11, the conductor layer 15, and the connection conductor 4 described above, a fourth insulating layer 24 covering the third conductor layer 13 and a fourth conductor layer 14 on the fourth insulating layer 24 are formed, for example, by using a semi-additive method. An insulating layer 25 having four levels is further formed on the second surface 3b side of the core substrate 3, and a conductor layer 15 having four levels is formed on the insulating layer 25 having four levels. A connection conductor 4 connecting the fourth conductor layer 14 and the third conductor layer 13 is formed on the fourth insulating layer 24. A connection conductor 4 connecting the upper and lower conductor layers 15 is also formed on the insulating layer 25 having four levels. A solder resist 6 is formed on the outermost layer on the first surface 3a side and the second surface 3b side of the core substrate 3. An opening 6a is provided in the solder resist 6 to expose a part of the fourth conductor layer 14 or the conductor layer 15 having four levels. The solder resist 6 and the openings 6a are formed by forming a resin layer containing, for example, a photosensitive epoxy resin or polyimide resin, and exposing and developing it using a mask having an appropriate opening pattern.

[0074] 1 is completed through the above steps. A surface protective film (not shown) may be formed on the surface of the fourth conductor layer 14 or the portion of the conductor layer 15 having the fourth hierarchical level that is exposed in the opening 6a of the solder resist 6 by electroless plating, a solder leveler, spray coating, or the like.

[0075] The wiring board of the embodiment is not limited to those having the structure illustrated in each drawing, and the structure, shape, and material illustrated in this specification. As described above, the wiring board of the embodiment may have any laminated structure. For example, the wiring board of the embodiment may be a coreless substrate that does not include a core substrate. The wiring board of the embodiment may include any number of conductor layers and insulating layers. As described above, the first conductor layer 11 and the second conductor layer 12 may be present at any layer on the laminated structure of the wiring board, as long as the first conductor layer 11 is present on the inner layer side and the second conductor layer 12 is present on the outer layer side. The first conductor layer 11 and the second conductor layer 12 may not include the plating film 10c made of an electrolytic plating film, and may include only the metal film 10b made of an electroless plating film, for example.

[0076] The method for manufacturing the wiring board of the embodiment is not limited to the method described with reference to the drawings. For example, the first to fourth conductor layers 11, 12, 13, 14 and the conductor layer 15 may be formed by a full additive method. The first to fourth insulating layers 21, 22, 23, 24 and the insulating layer 25 may be formed using resin in any form, not limited to a film-like resin. The method for manufacturing the wiring board of the embodiment may include any process other than the above-mentioned processes, or some of the above-mentioned processes may be omitted. [Explanation of symbols]

[0077] 100 Wiring board 11 First conductor layer 11a First conductor pad 110 Surface facing the second insulating layer 114 Surface covered by connecting conductor 11b First wiring pattern 111 Surface facing the second insulating layer 12 Second conductor layer 12a Second conductor pad 120 Surface facing the third insulating layer 124 Surface covered by connecting conductor 12b Second wiring pattern 121 Surface facing the third insulating layer 13 Third conductor layer 14 4th conductor layer 15 Conductor layer 21 First insulating layer 22 Second insulating layer 23 Third insulating layer 24 Fourth insulating layer 25 Insulating layer 4 Connecting conductor (via conductor) 5 Coating film R1 resist film

Claims

1. A core substrate; a laminate including insulating layers and conductor layers alternately laminated on the core substrate, and connecting conductors penetrating the insulating layers; A wiring board comprising: the laminate includes a stacked via conductor formed by alternately stacking the connection conductor and a conductor pad included in the conductor layer, The stacked via conductor is at least one first conductive pad having a roughened surface; At least one second conductive pad having a roughened surface covered with a coating film that improves adhesion between the insulating layer and the conductive layer; Including, The first conductive pad is laminated closer to the core substrate than the second conductive pad.

2. 2. The wiring board according to claim 1, The laminate comprises: a first conductor layer including the first conductor pad; and a second insulating layer covering the first conductor layer; a second conductor layer including the second conductor pad; and a third insulating layer covering the second conductor layer; Including, The roughened surface of the first conductive pad has a first surface roughness, and faces the second insulating layer so as to be in direct contact with the second insulating layer without the coating film therebetween.

3. 3. The wiring board according to claim 2, wherein the coating film is interposed between the second conductive pad and the third insulating layer.

4. 4. The wiring board according to claim 3, wherein the surface of the second conductor pad facing the third insulating layer is roughened to have a surface roughness substantially equal to the first surface roughness.

5. 4. The wiring board according to claim 3, wherein the third insulating layer includes the connection conductor that penetrates the third insulating layer and the coating film and contacts the second conductive pad.

6. 3. The wiring board according to claim 2, the first conductor layer further includes a first wiring pattern covered with the second insulating layer, The surface of the first wiring pattern facing the second insulating layer is roughened to have a surface roughness approximately equal to the first surface roughness, and is in direct contact with the second insulating layer without the intermediary of the coating film.

7. 5. The wiring board according to claim 4, the second conductor layer further includes a second wiring pattern covered with the third insulating layer, The coating film is interposed between the second wiring pattern and the third insulating layer.

8. 8. The wiring board according to claim 7, wherein the surface of the second wiring pattern facing the third insulating layer has a second surface roughness lower than the first surface roughness.

9. 9. A wiring board as described in claim 8, wherein a surface of the first conductor pad covered by the connecting conductor and a surface of the second conductor pad covered by the connecting conductor have a third surface roughness lower than the first surface roughness and higher than the second surface roughness.

10. 2. A wiring board as described in claim 1, wherein the metal constituting the connection conductor and the metal constituting the conductor pad facing the bottom surface of the connection conductor are in direct contact at the interface between the connection conductor and the conductor pad without a coating film therebetween.

Citation Information

Patent Citations

  • Method of manufacturing wiring board

    JP2009277905A

  • Wiring board and manufacturing method of the same

    JP2010067887A

  • Wiring board and manufacturing method of the same

    JP2014067941A

  • Wiring board and method for manufacturing wiring board

    JP2015015285A