Method for manufacturing a microelement and a microelement

Vacuum deposition of self-assembled electrets through micropores in MEMS structures addresses the destruction issue, allowing electret integration without charging, improving device performance and functionality.

JP7571995B2Active Publication Date: 2024-10-23THE RITSUMEIKAN TRUST +1
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2020132954
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-08-05
Publication Date
2024-10-23
Estimated Expiration
2040-08-05

AI Technical Summary

Technical Problem

Forming electrets on integrated MEMS devices requires high temperature and high voltage charging, which can destroy semiconductor integrated circuits and MEMS structures, preventing electrets from being formed in these devices.

Method used

A method involving vacuum deposition of self-assembled electrets through micropores in the MEMS structure, avoiding the need for charging treatment and using a low-temperature process to integrate electrets into integrated MEMS devices.

Benefits of technology

Prevents damage to semiconductor integrated circuits and MEMS structures while enabling the formation of electrets, enhancing sensor sensitivity and reducing power consumption, and adding new functions like energy harvesting.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007571995000001
    Figure 0007571995000001
  • Figure 0007571995000002
    Figure 0007571995000002
  • Figure 0007571995000003
    Figure 0007571995000003
Patent Text Reader

Abstract

To provide a fine element manufacturing method capable of forming an electret in an integrated MEMS element.SOLUTION: A self-organization electret 11 is arranged in an MEMS structure 4 formed on a semiconductor integrated circuit 3 by vacuum deposition of the self-organization electret 11 onto the MEMS structure 4. When the self-organization electret 11 is arranged in the MEMS structure 4, fine holes 4 are formed in the MEMS structure 4 by removing sacrifice layers G, and the self-organization electret 11 is arranged in the MEMS structure 4 by vapor deposition of the self-organization electret 11 using the fine holes 4a.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a microelement and a microelement. [Background technology]

[0002] In recent years, integrated MEMS elements in which a semiconductor integrated circuit (LSI) and a MEMS structure are formed on a single chip have become known as elements produced using MEMS (Micro Electro Mechanical Systems) technology (see, for example, Patent Document 1).

[0003] Incidentally, if an electret, which is a dielectric that semi-permanently retains an electric charge, is formed on such an integrated MEMS element, the performance of the integrated MEMS element can be improved, such as by improving sensor sensitivity, reducing power consumption, and providing a power generation function. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2008-140867 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, because the formation of electrets requires charging treatment such as high temperature and high voltage application, forming electrets on integrated MEMS elements has the problem that it may destroy semiconductor integrated circuits (LSIs) and MEMS structures, which has led to the problem that electrets cannot be formed on integrated MEMS elements.

[0006] In view of the above problems, an object of the present invention is to provide a manufacturing method for a microelement that can form an electret in an integrated MEMS element, and the microelement. [Means for solving the problem]

[0007] The above object of the present invention can be achieved by the following means. Note that the parentheses indicate reference symbols of the embodiments described below, but the present invention is not limited thereto.

[0008] The method for producing a microelement according to claim 1 comprises: Capacitive elements, resistive elements, memory cells, etc. are formed on the substrate (2). On semiconductor integrated circuit (3) The movable electrode (movable electrode portion 41) is supported so as to be able to swing at a distance from the fixed electrode (fixed electrode portion 40) and has a micro hole (4a). MEMS Structures (4) A method for manufacturing a microdevice comprising the steps of: A self-assembled electret (11) that does not require charging and can be vacuum-deposited is passed through the micropores (4a) and deposited inside the MEMS structure (4). It is characterized by the following.

[0009] request The method for producing a microelement according to claim 2 is the method for producing a microelement according to claim 1, A first step of forming a first layer (first layer wiring M1) on which a first sacrificial layer (G) is formed; a second step of stacking a plurality of layers (second-layer wiring M2 to seventh-layer wiring M7) each having a second sacrificial layer (G) formed thereon on the first layer (first-layer wiring M1); a third step of selectively etching and removing the first sacrificial layer and the second sacrificial layer to form the fixed electrode (fixed electrode portion 40) in the first layer and to form the movable electrode (movable electrode portion 41) having micropores (4a) in the layers formed on the first layer; and a fourth step of depositing the self-assembled electret (11) inside the MEMS structure (4) by passing it through the micropores (4a). It is characterized by the following.

[0010] request Claim 3 The method for producing a microelement according to claim 2 further comprises a fifth step of forming an adhesion layer (Ti layer 40a) on the semiconductor integrated circuit (3) and then forming a seed layer (Au layer 40b); and a sixth step of forming a sacrificial layer (G) of a mask pattern (P) having an opening on the seed layer (Au layer 40b), In the first step, the seed layer (Au layer 40b) exposed in the opening in the sixth step is grown to increase its thickness, thereby forming the first layer (first-layer wiring M1); In the second step, a second layer (second layer wiring M2) formed only of the second sacrificial layer (G) is formed, and then, the fifth step and the sixth step are performed on the second layer (second layer wiring M2) to laminate a third layer (third layer wiring M3) on which the second sacrificial layer (G) is formed; In the third step, the first sacrificial layer and the second sacrificial layer are selectively etched and removed to form the fixed electrode (fixed electrode portion 40) in the first layer (first layer wiring M1), and form the movable electrode (movable electrode portion 41) having a microhole (4a) in the second layer (second layer wiring M2) and the third layer (third layer wiring M3) formed on the first layer (first layer wiring M1). It is characterized by the following. The method for manufacturing a micro-element of claim 4 is characterized in that, in the method for manufacturing a micro-element as described in claim 3, in the second step, a plurality of layers (fourth layer wiring M4 to seventh layer wiring M7) in which the second sacrificial layer (G) is formed are formed on the third layer (third layer wiring M3) by repeatedly performing the fifth step and the sixth step. Effect of the Invention

[0011] Next, the effects of the present invention will be described with reference to the drawings. Note that the reference symbols in the parentheses are those of the embodiments described below, but the present invention is not limited thereto.

[0012] Claim 1 According to the invention The self-assembled electret (11) is passed through the micropores (4a) of the movable electrode (movable electrode portion 41), MEMS structures fabricated by vacuum deposition (4) Because it is evaporated insideThis can prevent the semiconductor integrated circuit 3 and the MEMS structure 4 from being destroyed. This makes it possible to form an electret in the integrated MEMS element. Furthermore, it is possible to prevent the function of the electret from being deteriorated.

[0013] In the method for producing a microelement according to the present invention, the production methods described in claims 2 to 4 are preferable. [Brief description of the drawings]

[0014] [Figure 1] 1 is a perspective view showing a microelement according to an embodiment of the present invention. [Diagram 2] 5(a) to 5(c) are partial vertical cross-sectional views showing a process of forming a MEMS structure on a semiconductor integrated circuit formed on a substrate according to the embodiment. [Diagram 3] 3(a) to (b) are partial cross-sectional views showing a continuation of the process of forming a MEMS structure on a semiconductor integrated circuit formed on a substrate according to the embodiment shown in FIG. 2, and FIG. 3(c) is a partial cross-sectional view showing a process of forming an electret in the MEMS structure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] The method for producing a microelement and the microelement according to the present invention will be described in detail below with reference to the drawings. In the following description, when directions such as up, down, left, and right are indicated, they refer to up, down, left, and right when viewed from the front in the drawings.

[0016] As shown in Fig. 1, a microelement 1 according to this embodiment is an integrated MEMS element 10 on which a self-organized electret 11 is formed. To explain in more detail, the integrated MEMS element 10 is mainly composed of a substrate 2, a semiconductor integrated circuit 3, and a MEMS structure 4. The substrate 2 is formed in a rectangular shape as shown in Fig. 1, and is formed of, for example, a silicon substrate.

[0017] On the other hand, the semiconductor integrated circuit 3 is formed on a substrate 2 as shown in FIG. 1, and has various elements such as capacitance elements, resistance elements, and memory cells.

[0018] As shown in Fig. 1, the MEMS structure 4 is formed on a semiconductor integrated circuit 3, and is a microstructure formed by microfabrication using semiconductor manufacturing technology. This MEMS structure 4 can constitute mechanical elements such as a pressure sensor, an acceleration sensor, a gyroscope, an optical scanner, a digital mirror device, and an optical modulator. To explain in more detail, as shown in Fig. 1, the MEMS structure 4 is composed of a fixed electrode portion 40 fixed on the semiconductor integrated circuit 3 and a movable electrode portion 41 provided at an interval from the fixed electrode portion 40, and although not shown, the movable electrode portion 41 is supported by a support portion so as to be swingable, as is well known in the art.

[0019] Thus, the integrated MEMS element 10 constructed as described above is generally known.

[0020] However, when attempting to form an electret, which is a dielectric that semi-permanently holds an electric charge, in such an integrated MEMS element 10, a charging process such as high temperature and high voltage application is required. Therefore, when attempting to form an electret in the integrated MEMS element 10, the semiconductor integrated circuit 3 and the MEMS structure 4 may be destroyed. do Therefore, there is a problem that it is not possible to form an electret in the integrated MEMS element 10.

[0021] Therefore, in this embodiment, an electret is formed on the integrated MEMS element 10 by using a self-organized electret 11. That is, the self-organized electret 11 was invented by one of the present inventors, Ariya Tanaka, does not require charging processing, and can be vacuum-deposited. For more information about the self-organized electret 11, see the joint announcement made by the Japan Science and Technology Agency and Chiba University on April 20, 2020 (https: / / www.jst.go.jp / pr / announce / 20200420 / index.html). Therefore, a detailed explanation will be omitted here.

[0022] Hereinafter, a method for forming an electret by using the self-assembled electret 11 on the integrated MEMS element 10 as described above will be described in detail.

[0023] First, as shown in FIG. 2(a), a thin Ti layer 40a serving as an adhesion layer is formed on a semiconductor integrated circuit 3 formed on a substrate 2 by, for example, a vapor deposition method, and then a thin Au layer 40b serving as a seed layer is formed.

[0024] Next, as shown in FIG. 2(b), the first layer wiring M1 is formed. To explain in more detail, a mask pattern P having openings at the locations to be each pattern is formed by a known photolithography technique. Sacrificial layer G Then, the thickness of the Au layer 40b is made thicker than the seed layer exposed in the opening by electrolytic plating (the Au layer 40b is grown). .death Thus, the first-layer wiring M1 is formed as shown in Fig. 2(b). The sacrificial layer G is formed by applying photosensitive polyimide to form a coating film, and then patterning the coating film by photolithography.

[0025] Next, on the first layer wiring M1, After forming the second layer wiring M2 consisting only of the sacrificial layer G, The processes in FIGS. 2(a) and 2(b) are repeated to form the second layer wiring M2 as shown in FIG. 2(c). On top of that, A third-layer wiring M3 and a fourth-layer wiring M4 are formed. Then, the processes of Fig. 2(a) and (b) are repeated on the fourth-layer wiring M4 to form a fifth-layer wiring M5, a sixth-layer wiring M6, and a seventh-layer wiring M7, as shown in Fig. 3(a).

[0026] Incidentally, when the second-layer wiring M2 to the seventh-layer wiring M7 are formed, they are formed as shown in Fig. 3(a) so that release holes, which are micropores 4a as shown in Fig. 1, are formed. Note that, when the seventh-layer wiring M7 is formed, the sacrificial layer G is not formed.

[0027] Next, as shown in Fig. 3(b), the sacrificial layer G is removed. As a result, the MEMS structure 4 in which the first-layer wiring M1 becomes the fixed electrode portion 40 and the second-layer wiring M2 to the seventh-layer wiring M7 become the movable electrode portion 41 is formed on the semiconductor integrated circuit 3. Thus, the integrated MEMS element 10 is formed in this manner. Note that the sacrificial layer G can be removed by selectively etching the organic material using, for example, a dry etching process using oxygen gas.

[0028] 3(c), the self-assembled electret 11 is disposed on the upper surface of the MEMS structure 4 by a low-temperature process (at about room temperature) using vacuum deposition. Furthermore, since the movable electrode portion 41 has micropores 4a formed therein, the self-assembled electret 11 is disposed in the MEMS structure 4 by passing the self-assembled electret 11 through the micropores 4a.

[0029] Thus, in this manner, an electret can be formed in the integrated MEMS element 10 by using the self-organized electret 11.

[0030] According to the present embodiment described above, the self-assembled electret 11 is arranged on the MEMS structure 4 only by a low-temperature process (about room temperature) using vacuum deposition, so that the semiconductor integrated circuit 3 and the MEMS structure 4 are not destroyed. do This can prevent a situation where the electret is damaged, and thus an electret can be formed in the integrated MEMS element 10. This improves the performance of the integrated MEMS element 10 due to the self-bias effect of the electret. For example, it becomes possible to improve the sensitivity of physical and chemical sensors and reduce the power consumption of electrostatic actuators. It is also possible to add new functions to the integrated MEMS element 10. For example, it becomes possible to realize an energy harvesting function in which the integrated MEMS element can generate power from environmental vibrations.

[0031] The shapes and the like shown in this embodiment are merely examples, and various modifications and changes are possible within the scope of the gist of the present invention described in the claims. For example, in this embodiment, after removing the sacrificial layer G, the self-organized electret 11 is arranged on the MEMS structure 4 by a low-temperature process (about room temperature) by vacuum deposition, but the present invention is not limited to this. The self-organized electret 11 may be arranged on the MEMS structure 4 by a low-temperature process (about room temperature) by vacuum deposition, and then the sacrificial layer G may be removed. However, in such a method, there is a risk that the function of the electret may be reduced when the sacrificial layer G is removed. Therefore, if the self-organized electret 11 is arranged on the upper surface of the MEMS structure 4 by a low-temperature process (about room temperature) by vacuum deposition after removing the sacrificial layer G as in this embodiment, the situation in which the function of the electret is reduced can be prevented.

[0032] In addition, in this embodiment, the electret is formed using the self-assembled electret 11, but the present invention is not limited to this. Any electret may be used as long as it does not require charging processing and can be vacuum deposited. [Explanation of symbols]

[0033] 1 Microelements 2. Board 3. Semiconductor Integrated Circuits 4. MEMS Structure 4a Micropore 10 Integrated MEMS elements 11 Self-organized electrets (electrets) G Sacrificial layer

Claims

1. A method for manufacturing a microelement on a semiconductor integrated circuit on which capacitive elements, resistive elements, memory cells, etc. are formed on a substrate, the method comprising forming a MEMS structure on the semiconductor integrated circuit, the MEMS structure comprising a fixed electrode and a movable electrode having a micropore, the movable electrode being supported so as to be capable of swinging at a distance from the fixed electrode, the method comprising the steps of: A method for manufacturing a microelement, in which a self-organized electret that does not require a charging process and can be vacuum-deposited is passed through the micropores and deposited within the MEMS structure.

2. A first step of forming a first layer having a first sacrificial layer formed thereon; A second step of stacking a plurality of layers, each of which has a second sacrificial layer formed on the first layer; a third step of selectively etching and removing the first sacrificial layer and the second sacrificial layer to form the fixed electrode in the first layer and to form the movable electrode having a microhole in the layers formed on the first layer; 2. The method for producing a microelement according to claim 1, further comprising a fourth step of depositing the self-assembled electret inside the MEMS structure by passing the self-assembled electret through the micropores.

3. A fifth step of forming an adhesion layer on the semiconductor integrated circuit, followed by forming a seed layer; and a sixth step of forming a sacrificial layer of a mask pattern having an opening on the seed layer, In the first step, the seed layer exposed in the opening in the sixth step is grown to a thickness to form the first layer; In the second step, a second layer formed only of the second sacrificial layer is formed, and then a third layer formed with the second sacrificial layer is laminated on the second layer by carrying out the fifth step and the sixth step; 3. The method for manufacturing a microelement as described in claim 2, wherein in the third step, the first sacrificial layer and the second sacrificial layer are selectively etched and removed to form the fixed electrode in the first layer, and the movable electrode having a microhole in the second layer and the third layer formed on the first layer.

4. A method for manufacturing a micro-element as described in claim 3, wherein in the second step, the fifth step and the sixth step are repeatedly performed on the third layer to form a plurality of layers in which the second sacrificial layer is formed.

Citation Information

Patent Citations

  • A micro generator and its preparation method

    CN102290968A

  • Production of semiconductor device

    JP1978096761A

  • Semiconductor device mixedly mounted with micro electro mechanical system sensor

    JP2008140867A

  • Oscillating power-generation element and manufacturing method thereof

    JP2011036089A

  • Electret and method for manufacturing electret

    JP2017099208A