Polishing pad and wafer notch polishing method

The annular polishing pad with a porous base and diamond abrasive particles addresses notch polishing issues by reducing waste and processing time, preventing chips or cracks, and enhancing cleaning efficiency.

JP7577288B1Active Publication Date: 2024-11-05NORITAKE MACHINE TECHNO CO LTD +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2024057062
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2024-03-29
Publication Date
2024-11-05
Estimated Expiration
2044-03-29

AI Technical Summary

Technical Problem

Conventional polishing pads fail to effectively polish the notches on wafers without causing chips or cracks, leading to waste and increased processing time, especially for large-diameter wafers with orientation flats.

Method used

A polishing pad with an annular shape and specific properties, including a base material with pores and diamond abrasive particles, is used to polish the notch by rotating around a perpendicular axis, minimizing pressure concentration and enhancing flexibility.

Benefits of technology

The solution reduces wafer waste, shortens processing time, and prevents chipping or cracking near the notch, while using a polishing liquid without abrasive particles for improved cleaning efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007577288000001_ABST
    Figure 0007577288000001_ABST
Patent Text Reader

Abstract

To provide a polishing pad capable of minimizing waste of a wafer having a notch, shortening the processing time, and preventing chipping of the notch, and a method for polishing the notch of such a wafer. [Solution] The polishing pad 1 of the present invention has a polishing surface 3 that contains a binder resin and is composed of an abrasive body including a base material 13 in which a plurality of pores 15a, 15b are formed, and abrasive particles 11 held in the base material 13 or the pores 15a, 15b. The binder resin is polyvinylidene fluoride or thermoplastic polyurethane, and the abrasive grains 11 are diamond and have a density of 0.9 to 1.2 g / cm. 3 The durometer hardness (D) is 26 to 47, and the compressive elastic modulus is 1645.1 to 3241.7 MPa.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a polishing pad and a method for polishing a wafer notch. [Background technology]

[0002] Patent Documents 1 to 4 disclose conventional polishing pads. The polishing pads of Patent Documents 1 to 3 are made by impregnating a nonwoven fabric with a paste and removing the solvent in the paste. The paste of Patent Document 1 is made of urethane, a solvent such as dimethylformamide, abrasive particles such as SiO2, and alkaline fine particles such as sodium carbonate. The paste of Patent Document 2 is made of an ether-based urethane and a solvent such as N,N-dimethylformamide. The paste of Patent Document 3 is made of urethane, a solvent, and a water repellent. By removing the solvent by drying or the like, the urethane is solidified in a state bonded to the nonwoven fabric. The polishing pad of Patent Document 4 is manufactured using a paste in which a binder resin, abrasive particles, and a solvent are mixed.

[0003] The polishing pad of Patent Document 1 is used to polish the outer peripheral edge of a disk-shaped wafer made of silicon or the like used to manufacture semiconductor elements. That is, the wafer is held on a rotating table that can rotate around the center of rotation. At this time, the central axis of the wafer is positioned at the center of rotation of the rotating table. Meanwhile, a polishing pad is provided on the upper end of a spindle so that the outer peripheral end face of the polishing pad abuts against the outer peripheral edge of the wafer. Then, a polishing liquid is supplied between the outer peripheral edge of the wafer and the outer peripheral end face of the polishing pad, and the rotating table and spindle are rotated while applying a predetermined load. This allows the outer peripheral edge of the wafer to be polished. This makes it possible to suppress the occurrence of defects in semiconductor devices due to the outer peripheral edge of the wafer. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2019-46838 A [Patent Document 2] JP 2019-118981 A [Patent Document 3] JP 2020-49639 A [Patent Document 4] Patent No. 5511266 Summary of the Invention [Problem to be solved by the invention]

[0005] However, in addition to the central axis that forms the center of the arc, a wafer may have a notch that indicates the direction of the crystal axis. This is because with a general orientation flat that is used to indicate the direction of the crystal axis, the area to be cut out from a large-diameter wafer becomes large, resulting in a waste of the wafer.

[0006] In the case of a wafer having such a notch, if the front or back surface is polished without taking any measures for the notch, chipping or cracking will occur near the notch during polishing, resulting in waste of the wafer.

[0007] In addition, while shortening the processing time is desirable in consideration of mass production, there is also a demand for preventing chipping or the like from occurring in the notch.

[0008] The present invention has been made in consideration of the above-mentioned conventional situation, and has as its object to provide a polishing pad that can minimize waste of a wafer having a notch, shorten the processing time, and prevent chipping of the notch, as well as a method for polishing the notch of such a wafer. [Means for solving the problem]

[0009] The polishing pad of the present invention is formed in an annular shape centered on a first rotation axis, a first surface having an annular shape extending in a direction substantially perpendicular to the first axis of rotation, a second surface having an annular shape extending in a direction substantially perpendicular to the first axis of rotation and positioned opposite the first surface, and a polished surface connecting the first surface and the second surface on an outer circumferential side, A polishing pad that polishes a notch formed in a disk-shaped wafer and indicates a direction of a crystal axis by rotating the pad around the first rotation axis while pressing the polishing surface against the notch, the polishing surface is constituted by an abrasive body including a base material containing a binder resin and having a plurality of pores formed therein, and abrasive particles held within the base material or the pores; the binder resin is polyvinylidene fluoride or thermoplastic polyurethane; Polishing particle is a diamond, Density: 0.9~1.2g / cm 3 and Durometer hardness (D) is 26 to 47; It is characterized by having a compressive elastic modulus of 1645.1 to 3241.7 MPa.

[0010] The present invention also provides a method for polishing a wafer notch, comprising: a first step of preparing a wafer, a polishing pad, and a polishing liquid; a second step of polishing the wafer with the polishing pad while supplying the polishing liquid between the wafer and the polishing pad; the wafer has a central axis, a front surface extending in a direction substantially perpendicular to the central axis, a back surface located opposite to the front surface and extending in a direction substantially perpendicular to the central axis, and a notch cut from the front surface to the back surface and indicating a direction of a crystal axis; The polishing pad is formed in an annular shape centered on a first rotation axis, the polishing pad has an annular first surface extending in a direction substantially perpendicular to the first rotation axis, an annular second surface extending in a direction substantially perpendicular to the first rotation axis and positioned opposite the first surface, and a polishing surface connecting the first surface and the second surface on an outer circumferential side; the polishing surface is constituted by an abrasive body including a base material containing a binder resin and having a plurality of pores formed therein, and abrasive particles held within the base material or the pores; the binder resin is polyvinylidene fluoride or thermoplastic polyurethane; Polishing particle is a diamond, Density: 0.9~1.2g / cm 3 and Durometer hardness (D) is 26 to 47; The compressive elastic modulus is 1645.1 to 3241.7 MPa. The second step is characterized in that the first rotation axis is perpendicular to the central axis, and the polishing pad is rotated around the first rotation axis while pressing the polishing surface against the notch using the polishing liquid that does not contain the abrasive particles.

[0011] The polishing pad of the present invention is composed of an abrasive body whose polishing surface contains a base material and abrasive particles. The base material contains a binder resin and has a plurality of pores formed therein. The abrasive particles are held in the base material or in the pores. Therefore, by using the notch polishing method of the present invention to polish a notch of a wafer with the polishing pad of the present invention, excellent followability can be exhibited when pressed against the notch, and good polishing can be performed.

[0012] In addition, the polishing pad of the present invention has a binder resin of polyvinylidene fluoride or thermoplastic polyurethane, and particle The diamond has a specific density, durometer hardness (D) and compressive modulus. Test results by the inventors have shown that these properties reduce the processing time while reducing or eliminating chipping or cracking near the notch. Effect of the Invention

[0013] According to the present invention, the amount of waste of a wafer having a notch can be minimized, the processing time can be shortened, and chipping does not occur in the notch. Furthermore, according to the present invention, since a polishing liquid that does not contain abrasive particles or has a small amount of abrasive particles can be used, the amount of particles that are abrasive particles remaining on the wafer after polishing is small, and the wafer after polishing has excellent cleanability. [Brief description of the drawings]

[0014] [Figure 1] FIG. 1 relates to polishing pads of Examples 1 to 10, where FIG. 1A is a plan view and FIG. 1B is a cross-sectional view. [Diagram 2] FIG. 2 is an enlarged cross-sectional view of the polishing pads of Examples 1 to 10. [Diagram 3] FIG. 3 is a SEM photograph of the polishing pad of Example 1 at 500 times magnification. [Figure 4] FIG. 4 is a SEM photograph of the polishing pad of Example 1 at 2000 times magnification. [Diagram 5] FIG. 5 is a SEM photograph of the polishing pad of Example 1 at 5000 times magnification. [Figure 6] FIG. 6 is a 500x SEM photograph of the polishing pad of Example 1 showing some large pores. [Figure 7] FIG. 7 is a 500x SEM photograph of the polishing pad of Example 1 showing other large pores. [Figure 8] FIG. 8 relates to a wafer before polishing used in the notch polishing methods of Examples 1 to 6, where FIG. 8A is a plan view and FIG. 8B is a cross-sectional view. [Figure 9] FIG. 9 is a partially enlarged side view of a wafer before polishing used in the notch polishing method of the embodiment. [Figure 10] FIG. 10 is a schematic plan view showing the notch polishing methods of Examples 1 to 6. [Figure 11] FIG. 11 is a schematic side view showing the notch polishing methods of Examples 1 to 6. [Figure 12] FIG. 12 is a partially enlarged plan view of the wafer after being polished by the notch polishing methods of Examples 1 to 6. [Figure 13] FIG. 13 is a partially enlarged side view of the wafer after being polished by the notch polishing methods of Examples 1 to 6. [Figure 14] FIG. 14 is a schematic enlarged cross-sectional view of the polishing pads of Examples 1 to 6 during polishing. [Figure 15] FIG. 15 is a schematic enlarged cross-sectional view of the polishing pads of Examples 1 to 6. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] The polishing pad of the present invention has a polishing surface formed of an abrasive body, which contains a base material and abrasive particles. The base material contains a binder resin and has a plurality of pores. The abrasive particles are held within the base material or within the pores. This polishing pad is an abrasive-containing type polishing pad, also known as an LHA (Loosely Held Abrasive) pad.

[0016] As the binder resin, polyvinylidene fluoride or thermoplastic polyurethane is adopted. As the binder resin of the LHA pad, in addition to polyether, rigid foamed polyurethane, epoxy resin, polyethersulfone resin, polyvinyl fluoride, vinyl fluoride-hexafluoropropylene copolymer, polyvinylidene fluoride, vinylidene fluoride-hexafluoropropylene copolymer, polyethylene resin, polymethyl methacrylate, etc. can be adopted. However, according to the test results of the inventors, polyvinylidene fluoride or thermoplastic polyurethane is preferable for the polishing pad of the present invention in terms of followability, flexibility, etc.

[0017] Diamond is used as the abrasive particles. The LHA pad can use silica, ceria, alumina, zirconia, titania, manganese oxide, barium carbonate, chromium oxide, boron carbide, iron oxide, etc. as abrasive particles, but according to the inventors' test results, diamond is preferable for the polishing pad of the present invention because of its high Knoop hardness and good polishing durability.

[0018] According to the results of the inventors' tests, the polishing pad of the present invention has a density of 0.9 to 1.2 g / cm 3 It is preferable that the durometer hardness (D) is 26 to 47 and the compressive elastic modulus is 1645.1 to 3241.7 MPa.

[0019] According to the results of the inventors' tests, it is particularly preferable that the polishing body contains silica particles held within the matrix or pores. Silica particles are softer than diamond, which is an abrasive particle, and flexibly support the diamond.

[0020] It is particularly preferable that the pores consist of fine pores forming a three-dimensional network structure and large pores having a larger volume than the fine pores and communicating with the fine pores while opening on the polishing surface. The large pores suppress the processing resistance during polishing of the notch and reduce chipping at the notch.

[0021] According to the inventors' test results, the fine pores are 46.8 to 57.7% by volume, and the large pores are 0. Beyond 13.8% by volume below It is preferable that:

[0022] When a polishing liquid is used, the polishing liquid may be pure water, may be oil-based, or may contain an acidic or alkaline chemical.

[0023] The polishing surface may have a third surface that is continuous with the first surface and has a tapered shape that becomes larger in diameter as it approaches the second surface, and a fourth surface that is continuous with the second surface and has a tapered shape that becomes larger in diameter as it approaches the first surface. It is preferable that the third surface and the fourth surface have an interior angle that matches the opening angle of the notch.

[0024] In the polishing method of the present invention, in the second step, it is preferable to move the polishing pad along the first rotation axis. In this case, the entire notch, including the boundary between the fifth and sixth faces of the notch, can be polished by the ridge of the polishing pad. Therefore, chipping or cracking is less likely to occur or does not occur in the vicinity of the notch on the wafer after notch polishing.

[0025] In the polishing method of the present invention, in the second step, the polishing pad is rotated so that the central axis thereof oscillates around the first rotation axis. For wafer In this case, the edge portion between the notch and the front or back surface can also be polished appropriately. Therefore, chipping or cracking is less likely to occur or does not occur at all in the vicinity of the notch in the wafer after notch polishing.

[0026] (Examples and Comparative Examples) Examples 1 to 6 embodying the present invention and Comparative Examples 1 and 2 will be described below.

[0027] First, the following binder resin, abrasive particles, and solvent were prepared. (binder resin) PVDF (Polyvinylidene Fluoride) (abrasive particles) Diamond (average grain size: 5 μm) (solvent) NMP (N-methyl-2-pyrrolidone) (Filler) Silica particles (average particle size: 200 nm) (pore forming agent) Granulated sugar (average particle size 200 μm)

[0028] The binder resin, abrasive particles, solvent, filler and pore-forming agent were mixed in the mass percentages shown in Table 1 to form pastes. Each of the resulting pastes was used to obtain a sheet-shaped molded body using a T-die. The solvent was removed from each molded body, and the binder resin was solidified.

[0029] [Table 1]

[0030] Thus, each polishing body was prepared. The outer peripheral portion and the inner peripheral portion of each polishing body were cut away around the first rotation axis P to obtain the polishing pads 1 of Examples 1 to 6. As shown in Figs. 1 and 2, each polishing pad 1 has an inner diameter φ1 of 152 mm, an outer diameter φ2 of 200 mm, and a thickness t of 4.5 mm. The inner diameter, outer diameter, and thickness can be changed depending on the polishing device described below.

[0031] 1, each polishing pad 1 is formed in an annular shape centered on a first rotation axis P. Each polishing pad 1 has an annular first surface 1a extending in a direction substantially perpendicular to the first rotation axis P, an annular second surface 1b extending in a direction substantially perpendicular to the first rotation axis P and positioned opposite the first surface 1a, and a polishing surface 3 connecting the first surface 1a and the second surface 1b on the outer periphery.

[0032] As shown in Fig. 2, the polished surface 3 has a third surface 3a that is continuous with the first surface 1a and that tapers from the first rotation axis P toward the second surface 1b, and a fourth surface 3b that is continuous with the second surface 1b and that tapers from the first rotation axis P toward the first surface 1a. The third surface 3a and the fourth surface 3b have an interior angle θ1 of 110°±20°. The third surface 3a and the fourth surface 3b form a ridge line L. The interior angle θ1 is formed in accordance with the opening angle θ2 of a notch 7 described later.

[0033] An SEM photograph of polishing pad 1 of Example 1 at 500x magnification is shown in Figure 3, an SEM photograph of it at 2000x magnification is shown in Figure 4, and an SEM photograph of it at 5000x magnification is shown in Figure 5. In addition, an SEM photograph of a large pore in polishing pad 1 of Example 1 at 500x magnification is shown in Figure 6, and an SEM photograph of another large pore at 500x magnification is shown in Figure 7.

[0034] As shown in Figs. 3 and 4, the polishing pads 1 of Examples 1 to 6 have a base material 13 and abrasive particles 11, as shown in Figs. 14 and 15. The base material 13 is made of a binder resin, and has a plurality of pores 15a and 15b formed therein. The abrasive particles 11 are held in the base material 13 or in the pores 15a. Each polishing pad 1 also includes a filler 12 held in the base material 13 or in the pores 15a. As shown in Figs. 5 and 6, the pores 15a and 15b of each polishing pad 1 are composed of pores 15a forming a three-dimensional network structure and large pores 15b having a larger volume than the pores 15a, which are open to the polishing surface 3 and communicate with the pores 15a.

[0035] The physical properties of the polishing pads 1 of Examples 1 to 6 thus obtained were durometer hardness (D), density (g / cm 3 The results are shown in Table 2.

[0036] [Table 2]

[0037] The binder resin content (volume %), abrasive particle content (volume %), filler content (volume %) and pore content (volume %) were also measured. The results are shown in Table 3.

[0038] [Table 3]

[0039] The pore content breakdown, i.e., the volume percent of fine pores and the volume percent of large pores, was also measured, and the results are shown in Table 4.

[0040] [Table 4]

[0041] (test) As shown in FIG. 8, an unpolished wafer 5 made of SiC was prepared. The wafer 5 was disk-shaped with a diameter of 8 inches. The wafer 5 had a central axis Q forming the center of an arc, a front surface 5a extending in a direction substantially perpendicular to the central axis Q, and a back surface 5b located opposite the front surface 5a and extending in a direction substantially perpendicular to the central axis Q. In addition, the wafer 5 had a notch 7 cut from the front surface 5a to the back surface 5b at one location on the outer periphery thereof, indicating the direction of the crystal axis.

[0042] As shown in FIG. 9, the notch 7 is formed by a fifth surface 7a extending from one point on the outer peripheral edge toward the central axis Q, and a sixth surface 7b extending from another point on the outer peripheral edge toward the central axis Q at an opening angle θ2.

[0043] A polishing apparatus shown in FIG. 10 was prepared. The polishing apparatus was a "FINE SURFACE E-200" manufactured by BBS Kinmei Co., Ltd., and was equipped with a bracket (not shown) that could rotate the polishing pad 1 around a first rotation axis P. The first rotation axis P is perpendicular to a central axis Q of a wafer 5 held on a drum (not shown). The bracket can press the polishing pad 1 against the drum. The polishing apparatus can also move the polishing pad 1 within a certain range T along the first rotation axis P. This allows the entire notch 7, including the boundary between the fifth surface 7a and the sixth surface 7b of the notch 7, to be polished by the ridge L of the polishing pad 1.

[0044] 11, the wafer 5 is adapted to oscillate at an angle of S° up and down with respect to the polishing pad 1 so that the central axis Q oscillates around the first rotation axis P. The center of oscillation is an intersection X between an imaginary line extending from the central axis Q toward the center of the notch 7 at the center in the thickness direction of the wafer 5 and the outer circumferential surface of the wafer 5. This allows the notch 7 to be polished at the boundary portion with the front surface 5a of the wafer 5 and the boundary portion with the back surface 5b of the wafer 5.

[0045] Then, using the polishing pads 1 of Examples 1 to 6 or the polishing pads 1 of Comparative Examples 1 and 2, the notches 7 of 200 wafers 5 were polished under the following conditions. The polishing pad 1 of Comparative Example 1 was a commercially available hard urethane pad (hardness D: 60), and the polishing pad 1 of Comparative Example 2 was a commercially available nonwoven fabric pad (hardness D: 30). For the polishing pads 1 of Examples 1 to 6, water containing no abrasive particles was used as the polishing liquid. For the polishing pads 1 of Comparative Examples 1 and 2, silica was used as the abrasive particles, and a permanganate-based slurry with a different concentration of the abrasive particles was used as the polishing liquid. Polishing pad 1 rotation speed: 600 (rpm) Pressing load of polishing surface 3 against notch 7: 0.8 (kgf)

[0046] A partially enlarged plan view of the notch 7 after polishing is shown in Fig. 12, and a partially enlarged side view is shown in Fig. 13. As shown in Fig. 12 and Fig. 13, the surface of the notch 7 after polishing is smoothed, and chamfers 9 are formed at the tip, the boundary with the front surface 5a, and the boundary with the back surface 5b, making it difficult for chipping or cracking to occur in the vicinity of the notch 7 in the polished wafer 5.

[0047] The polishing time, the presence or absence of unpolished areas, particles, and the polishing liquid were evaluated. In this case, the unpolished areas were evaluated at the tip of the notch 7 (TOP-VN), the surface 5a portion of the notch 7 (A-VN), and the back surface 5b portion of the notch 7 (B-VN).

[0048] Regarding the polishing time and the presence or absence of unpolished areas, if the polishing time was within 90 seconds and there was no unpolished area, it was rated as ◎, if the polishing time was within 120 seconds and there was no unpolished area, it was rated as ○, if the polishing time was within 180 seconds and there was no unpolished area, it was rated as △, and if the polishing time was 180 seconds or more and there was an unpolished area, it was rated as ×. However, in notch 7, if there were grinding marks (scratches) from previous processing in the horizontal direction and horizontal grinding marks were confirmed by microscope observation, it was determined that there was an unpolished area.

[0049] Regarding particles, within a 5 μm x 5 μm area, the number of particles was judged as 0 (◎), 5 or less (◯), 5 or more but less than 10 (△), and 10 or more (×) based on observation with an electron microscope.

[0050] Regarding the polishing liquid, if polishing was possible with an abrasive particle concentration of 0 ppm, it was marked with an ◎; if polishing was not possible unless the abrasive particle concentration was 1 ppm or more and less than 1000 ppm, it was marked with an ◯; if polishing was not possible unless the abrasive particle concentration was 1000 ppm or more and less than 5000 ppm, it was marked with a △; and if polishing was not possible unless the abrasive particle concentration was 5000 ppm or more and 10000 ppm or less, it was marked with an ×.

[0051] Overall, if there was even one × or △ for the polishing time, the presence or absence of unpolished areas, particles, and polishing liquid, it was marked as ×, if all were ○ or above and ◎ was 2 or less, it was marked as ○, and if all were ○ or above and ◎ was 3 or more, it was marked as ◎. The results are shown in Table 5.

[0052] [Table 5]

[0053] From Table 5, the polishing pads 1 of Examples 1 to 4 were given the rating of ⊚, and the polishing pads 1 of Examples 5 and 6 were given the rating of ◯. According to the inventors' test results, the same effect was obtained when TPU (thermoplastic polyurethane) was used instead of PVDF. In contrast, the polishing pads 1 of Comparative Examples 1 and 2 had some areas left unpolished, and were poorly evaluated in terms of particles and polishing liquid. It is presumed that this is due to the following reasons.

[0054] That is, as shown in FIG. 14 and FIG. 15, the polishing pad 1 of Examples 1 to 6 has pores 15 consisting of fine pores 15a and large pores 15b. The fine pores 15a have a three-dimensional network structure. The large pores 15b have a larger volume than the fine pores 15a, and are open to the polishing surface 2 while communicating with the fine pores 15a. The diamond abrasive particles 11 are contained within the fine pores 15a of the base material 13 and are fixed to the base material 13 by point or surface contact. During polishing, if an excessively large load is concentrated on a certain abrasive particle 11, the abrasive particle 11 falls off from the base material 13 and polishes while having a degree of freedom locally within the fine pores 15a. At this time, the filler 12 flexibly supports the abrasive particle 11 within the fine pores 15a, suppressing the concentration of an excessively large load on the abrasive particle 11. Therefore, deep scratches or scratches are not formed in the notch 7 of the wafer 5.

[0055] Furthermore, it is presumed that the polishing pads 1 of Examples 1 to 6 have improved flexibility due to the presence of large pores 15b, and are therefore more likely to deform during processing, polishing while following the notch 7. Thus, in the polishing pads 1 of Examples 1 to 6, the large pores 15b suppress the processing resistance during polishing of the notch 7, and reduce chipping at the notch 7.

[0056] In particular, the polishing pads of Examples 1 to 6 have a binder resin of polyvinylidene fluoride or thermoplastic polyurethane, and particle The diamond 11 has a specific density, durometer hardness (D) and compressive modulus. These characteristics reduce the processing time, and chipping or cracking is unlikely or does not occur near the notch 7.

[0057] Therefore, it is understood that the polishing pads 1 of Examples 1 to 6 and the notch polishing methods using them can minimize waste of the wafer 5 having the notch 7.

[0058] Furthermore, according to the polishing pads 1 of Examples 1 to 10 and the notch polishing methods using these, a polishing liquid that does not contain abrasive particles or has a small amount of abrasive particles can be used, and since there are few particles that are abrasive particles remaining on the wafer 5 after polishing, the wafer 5 has excellent cleaning properties after polishing.

[0059] In the above, the present invention has been described based on Examples 1 to 6. However, the present invention is not limited to the above Examples 1 to 6, and it goes without saying that the present invention can be modified and applied as appropriate without departing from the spirit of the present invention.

[0060] For example, in Examples 1 to 6, the notch 7 of the wafer 5 made of SiC was polished, but the polishing pad and wafer polishing method of the present invention can also be applied to polishing notches of wafers made of semiconductors in general, such as Si and GaN. [Industrial Applicability]

[0061] The present invention can be used in semiconductor device manufacturing equipment and the like. [Explanation of symbols]

[0062] P…1st rotation axis center 1a…First page 1b…Second side 3…Polished surface 5…Wafer 7…Notch 1...Polishing pad 15a, 15b...pores (15a...small pores, 15b...large pores) 13...Base material 11...Abrasive particles 12...Silica particles (filler)

Claims

1. The first rotation axis is a first axis of rotation. a first surface having an annular shape extending in a direction substantially perpendicular to the first axis of rotation, a second surface having an annular shape extending in a direction substantially perpendicular to the first axis of rotation and positioned opposite the first surface, and a polished surface connecting the first surface and the second surface on an outer circumferential side, a polishing pad for polishing a notch formed in a disk-shaped wafer and indicating a direction of a crystal axis by rotating the pad around the first rotation axis while pressing the polishing surface against the notch, the pad comprising: the polishing surface is constituted by an abrasive body including a base material containing a binder resin and having a plurality of pores formed therein, and abrasive particles held within the base material or the pores; the binder resin is polyvinylidene fluoride or thermoplastic polyurethane; the abrasive particles are diamond; Density: 0.9 to 1.2 g / cm 3 and Durometer hardness (D) is 26 to 47; A polishing pad having a compressive elastic modulus of 1645.1 to 3241.7 MPa.

2. 2. The polishing pad of claim 1, wherein the polishing body comprises silica particles held within the matrix or within the pores.

3. 3. The polishing pad according to claim 1, wherein the pores are composed of fine pores forming a three-dimensional network structure and large pores having a larger volume than the fine pores, opening onto the polishing surface and communicating with the fine pores.

4. The pores are 46.8 to 57.7% by volume; 4. The polishing pad of claim 3, wherein the large pores are greater than 0 and less than or equal to 13.8% by volume.

5. A first step of preparing a wafer, a polishing pad, and a polishing liquid; a second step of polishing the wafer with the polishing pad while supplying the polishing liquid between the wafer and the polishing pad; the wafer has a central axis, a front surface extending in a direction substantially perpendicular to the central axis, a back surface located opposite to the front surface and extending in a direction substantially perpendicular to the central axis, and a notch cut from the front surface to the back surface and indicating a direction of a crystal axis; The polishing pad is formed in an annular shape centered on a first rotation axis, the polishing pad has an annular first surface extending in a direction substantially perpendicular to the first rotation axis, an annular second surface extending in a direction substantially perpendicular to the first rotation axis and positioned opposite the first surface, and a polishing surface connecting the first surface and the second surface on an outer circumferential side; the polishing surface is constituted by an abrasive body including a base material containing a binder resin and having a plurality of pores formed therein, and abrasive particles held within the base material or the pores; the binder resin is polyvinylidene fluoride or thermoplastic polyurethane; the abrasive particles are diamond; Density: 0.9 to 1.2 g / cm 3 and Durometer hardness (D) is 26 to 47; The compressive elastic modulus is 1645.1 to 3241.7 MPa; The second step of the method for polishing a notch of a wafer comprises rotating the polishing pad around the first rotation axis while pressing the polishing surface against the notch and orthogonalizing the first rotation axis to the central axis and using the polishing liquid that does not contain the abrasive particles.

6. 6. The method for polishing a wafer notch according to claim 5, wherein in the second step, the polishing pad is moved along the first rotation axis.

7. 7. The method for polishing a wafer notch according to claim 5, wherein in the second step, the wafer is oscillated relative to the polishing pad so that the central axis oscillates around the first rotation axis.

Citation Information

Patent Citations

  • Production of photo molding material for making stencil

    JP1980011266A

  • Edge polishing method

    JP2019046838A

  • Polishing pad

    JP2019118981A

  • Polishing pad

    JP2020049639A

  • Polishing pad, manufacturing method for the same, and manufacturing method for polishing-processed product

    JP2021041483A