High temperature forming mold
The high-temperature molding mold addresses the challenge of workpiece removal by using inner and outer molds with differing thermal expansion coefficients, facilitating easy release and improving accuracy while reducing management complexity.
Patent Information
- Application Number
- JP2023209323
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-12-12
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2043-12-12
AI Technical Summary
High-temperature molding molds face challenges in removing workpieces due to thermal expansion and elastic deformation, leading to difficulties in achieving accuracy and increased processing costs, particularly with tapered molds that require complex assembly and management.
A high-temperature molding mold design with an inner mold and outer mold having different thermal expansion coefficients, where the inner mold expands more than the outer mold during heating and contracts more during cooling, allowing for easy release and improved accuracy without the need for complex assembly or management.
The mold design enables easy removal of workpieces and simplifies mold management by leveraging differential thermal expansion to enhance accuracy and reduce processing time and effort.
Smart Images

Figure 0007577825000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a die for forming a workpiece at high temperatures. [Background technology]
[0002] In high-temperature molding using a mold, the effect of thermal expansion can make it difficult to remove the workpiece from the mold. During high-temperature molding, the mold expands thermally and becomes larger than its initial dimensions due to elastic deformation caused by the molding load. When the high-temperature environment is removed by cooling after molding, if the thermal contraction and elastic deformation of the mold are greater than the thermal contraction of the workpiece, the workpiece cannot be removed from the mold. For this reason, a tapered mold structure is known in which the mold has a two-layer structure of an inner mold and an outer mold, the inner mold is a split mold, and the inner mold and the outer mold are fitted together at a taper (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 3050866 Summary of the Invention [Problem to be solved by the invention]
[0004] However, tapered dies require machining into a tapered shape during production, which makes it difficult to achieve precision and tends to be expensive. Also, it may be necessary to actually assemble the inner and outer dies and perform a finish machining process to match them. In this case, it is essential to use and store the inner and outer dies as a set after adjusting the fit. Therefore, in forming devices that use many dies to perform hot forming, there is a problem that the effort required to manage and store the dies increases.
[0005] An object of the present invention is to provide a mold for high-temperature molding which is easy to remove the workpiece from and which is easy to manage. [Means for solving the problem]
[0006] A high-temperature molding die according to one aspect of the present invention comprises an outer mold including a holding surface, an outer side surface at least partially adjacent to the holding surface, and an inner mold including an inner side surface that defines a molding chamber; the inner mold is a split-type inner mold formed by an assembly of a plurality of split molds, the holding surface is an inner wall surface surrounding the inner mold, The temperature of the outer mold and the inner mold before high-temperature molding is T, the temperature rise due to high-temperature molding is ΔT, the thermal expansion coefficient of the inner mold in the temperature range from temperature T to temperature T+ΔT is α, and the thermal expansion coefficient of the outer mold is β. In the high-temperature molding die, when the outer dimension of the inner mold in a direction along a center line passing through the center of the molding chamber is A and the inner dimension of the outer mold is B, the relationship of the following formula (2) is satisfied; the multiple split molds include a pair of first split molds arranged opposite each other across the center line of the molding chamber, and a pair of second split molds arranged opposite each other so as to intersect the center line and be adjacent to one end and the other end of the pair of first split molds, and when the dimension of the first split mold along the center line is A1 and one dimension of the second split mold along the center line is A2, the relationship of the following formula (3) is satisfied; and when the thermal expansion coefficient of the first split mold in a temperature range from temperature T to temperature T+ΔT is α1 and the thermal expansion coefficient of the second split mold is α2, the relationship of the following formula (4) is satisfied; and the molding chamber has a shape such that the thermal expansion coefficient of a molded product molded in the molding chamber differs between the direction along the center line and the direction perpendicular to the center line. (1) α>β (2) α×A×ΔT>β×B×ΔT (3) α×A1×ΔT+2×(α×A2×ΔT)>β×B×ΔT (4)α1×A1×ΔT+2×(α2×A2×ΔT)>β×B×ΔT (however, α1>β, α2>β)
[0007] According to this embodiment, since the thermal expansion coefficient α of the inner mold is larger than the thermal expansion coefficient β of the outer mold, the inner mold expands while being restrained by the outer mold during hot working. Therefore, when the workpiece is placed in the molding chamber and heated and pressed, the pressing force of the workpiece against the inner wall surface of the inner mold increases, and processing with high accuracy can be performed. In other words, the inner shape of the molding chamber can be well transferred to the workpiece. On the other hand, when the temperature is lowered from hot to cold, the inner mold has a larger degree of thermal contraction than the outer mold. For this reason, a gap is easily generated between the inner mold and the outer mold, and the inner mold can be easily released from the outer mold. In addition, since the difference in the thermal expansion coefficient between the inner mold and the outer mold is utilized to improve the molding accuracy and to remove the workpiece, there is no need for a finishing process of the inner mold and the outer mold in place, as in the case of a tapered mold. Therefore, there is no need to manage and store the inner mold and the outer mold as a set, and management of the mold can be simplified.
[0008] In the above-mentioned high-temperature molding die, when the holding surface is an inner wall surface surrounding the inner mold, and the outer dimension of the inner mold in a direction along a center line passing through the center of the molding chamber is A and the inner dimension of the outer mold is B, it is desirable to satisfy the relationship of the following formula (2). (2) α×A×ΔT>β×B×ΔT
[0009] According to this embodiment, the outer dimensions of the inner mold are larger than the inner dimensions of the outer mold with respect to the amount of thermal expansion and contraction in the temperature range of ΔT. Therefore, when hot, the inner mold is pressed against the outer mold to form an interference fit, improving the strength of the mold. On the other hand, when the temperature is reduced from hot to cold, the inner mold shrinks more than the outer mold, so that the inner mold can be reliably released from the outer mold.
[0010] In the above-mentioned high-temperature molding die, it is preferable that the inner die is a split-type inner die formed by an assembly of a plurality of split dies.
[0011] According to this embodiment, since the inner mold is of a split type, the molded product after the workpiece is molded at high temperature can be easily released from the inner mold.
[0012] In the above-mentioned high-temperature molding die, the multiple split dies include a pair of first split dies arranged opposite each other across the center line of the molding chamber, and a pair of second split dies arranged opposite each other so as to intersect with the center line and be adjacent to one end and the other end of the pair of first split dies, respectively, and may be configured to satisfy the relationship of the following formula (3), where A1 is the dimension of the first split dies along the center line and A2 is one dimension of the second split dies along the center line. (3) α×A1×ΔT+2×(α×A2×ΔT)>β×B×ΔT
[0013] According to this embodiment, the inner mold is composed of a pair of first split molds and a pair of second split molds. With respect to the amount of thermal expansion and contraction in the temperature range of ΔT, the total outer dimensions of the split mold pair constituting the inner mold are greater than the inner dimensions of the outer mold. This improves molding accuracy and allows the inner mold composed of the split mold pair to be reliably released from the outer mold.
[0014] In the above-mentioned high-temperature molding die, when the thermal expansion coefficient of the first split die in the temperature range from temperature T to temperature T+ΔT is α1 and the thermal expansion coefficient of the second split die is α2, the die may be configured to satisfy the relationship of the following formula (4). (4)α1×A1×ΔT+2×(α2×A2×ΔT)>β×B×ΔT (however, α1>β, α2>β)
[0015] According to this embodiment, even if the inner mold is composed of a pair of a first split mold and a second split mold and the thermal expansion coefficients of the two are different, the molding accuracy is improved and the inner mold consisting of the split mold pair can be reliably released from the outer mold.
[0016] In the above-mentioned high-temperature molding die, the multiple split molds are arc-shaped split molds obtained by dividing a cylindrical inner mold with its circular center at the center of the molding chamber into multiple parts in the circumferential direction, and may include a pair of arc-split molds facing each other along the center line of the molding chamber, and may be configured to satisfy the relationship of the following formula (5), where A3 is the distance between the pair of arc-split molds on the center line and A4 is the dimension of one of the arc-split molds along the center line. (5)α×(A3+2×A4)×ΔT>β×B×ΔT
[0017] According to this embodiment, when the inner mold is constructed by combining arc-shaped split molds, the outer dimensions of the inner mold are larger than the inner dimensions of the outer mold in terms of the amount of thermal expansion and contraction in the temperature range of ΔT. This improves molding accuracy and allows the inner mold consisting of the split mold pair to be reliably released from the outer mold.
[0018] In the above-mentioned high-temperature molding die, the multiple split dies are arranged along an inner wall surface partitioned by the pair of first split dies and the pair of second split dies, and further include a pair of third split dies and a pair of fourth split dies that partition the molding chamber, the pair of third split dies are arranged opposite each other across the center line of the molding chamber, and the pair of fourth split dies are arranged opposite each other so as to intersect with the center line and be adjacent to one end and the other end of the pair of third split dies, respectively, and the configuration may be such that the relationship of the following formula (6) or (7) is satisfied, where γ is the thermal expansion coefficient of the third split dies and the fourth split dies in the temperature range from temperature T to temperature T+ΔT, C1 is the dimension of the third split dies along the center line, and C2 is one dimension of the fourth split dies along the center line. (6) α×A1×ΔT+2×(α×A2×ΔT)>β×B×ΔT (where α>γ) (7) 2×(α×A2×ΔT)+γ×C1×ΔT+2×(γ×C2×ΔT)>β×B×ΔT(where α<γ)
[0019] According to this embodiment, the inner mold has a multi-layer structure in which an inner mold consisting of a pair of third split molds and a pair of fourth split molds is disposed within an outer mold consisting of a pair of first split molds and a pair of second split molds. In addition, taking into consideration the difference in thermal expansion coefficient between the outer mold and the inner mold, the total outer dimensions of the inner mold are set to be larger than the inner dimensions of the outer mold with respect to the amount of thermal expansion and contraction in the temperature range of ΔT. This improves molding accuracy and ensures that the inner mold consisting of the first to fourth split molds can be reliably released from the outer mold.
[0020] The above-mentioned high-temperature molding die may further include a partition plate disposed inside the molding chamber for dividing the molding chamber into a plurality of compartments.
[0021] According to this aspect, one molding chamber can be divided into a plurality of compartments by the partition plates, thereby improving the production efficiency of molded products. Effect of the Invention
[0022] According to the present invention, it is possible to provide a high-temperature molding die which allows easy removal of the workpiece and is easy to manage. [Brief description of the drawings]
[0023] [Figure 1] FIG. 1 is a schematic diagram of a molding apparatus to which a high-temperature molding die according to the present invention is applied. [Diagram 2] FIG. 2 is a cross-sectional view showing a high-temperature molding die having a molding chamber with a rectangular cross section according to a first embodiment of the present invention. [Diagram 3] FIG. 3 is a cross-sectional view showing a high-temperature molding die having a molding chamber with a circular cross section, which is a modified example of the first embodiment. [Figure 4] FIG. 4 is a cross-sectional view showing a high-temperature molding die in which a partition plate is arranged in a molding chamber, which is a modified example of the first embodiment. [Diagram 5]FIG. 5 is a cross-sectional view showing a high-temperature molding die according to a second embodiment, in which a molding chamber having a rectangular cross section is partitioned by a split inner die. [Figure 6] FIG. 6 is a cross-sectional view showing a high-temperature molding die in a modified example of the second embodiment, in which a molding chamber having a circular cross section is partitioned by a split inner die. [Figure 7] FIG. 7 is a cross-sectional view showing a high-temperature molding die that uses a split inner die having a different thermal expansion coefficient, which is a modified example of the second embodiment. [Figure 8] FIG. 8 is a cross-sectional view showing a high-temperature molding die in which a partition plate is arranged in the molding chamber, which is a modified example of the second embodiment. [Figure 9] FIG. 9 is a cross-sectional view showing a high-temperature molding die according to a third embodiment, in which a molding chamber having a rectangular cross section is partitioned by two layers of split inner dies. [Figure 10] FIG. 10 is a cross-sectional view showing a high-temperature molding die that uses a split inner die having a different thermal expansion coefficient, which is a modified example of the third embodiment. [Figure 11] FIG. 11 is a cross-sectional view showing a high-temperature molding die that uses a split inner die having a different thermal expansion coefficient, which is a modified example of the third embodiment. [Figure 12] FIG. 12(A) is a top view showing a modified example of the outer mold, and FIG. 12(B) is a cross-sectional view taken along line XIIB-XIIB of FIG. 12(A). [Figure 13] FIG. 13(A) is a top view showing a modified example of the outer mold, and FIG. 13(B) is a cross-sectional view taken along line XIIIB-XIIIB of FIG. 13(A). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. The die according to the present invention is a die for high-temperature molding used at high temperatures of several hundred degrees Celsius for sintering, which heats and pressurizes sintered materials such as powders and solid pieces of metals and ceramics, die casting, which pressurizes and molds molten metal, diffusion bonding, which bonds different materials or the same materials, etc. In other words, it is a die for high-temperature molding used in applications in which a heated workpiece contained in the die is pressed to transfer the shape of the inner wall surface of the die to the workpiece, thereby producing a molded product with high precision.
[0025] 1 is a vertical cross-sectional view showing a molding apparatus 1 used for molding sintered products, etc., and is a diagram showing a preferred application of a high-temperature molding die 2 according to the present invention. The die 2 has a molding chamber 20 for molding a workpiece MP. The die 2 has a two-layer structure of at least an inner die and an outer die in the direction from the molding chamber 20 toward the outside. The details of the die structure will be described later.
[0026] The molding apparatus 1 includes an upper punch 11 that presses the workpiece MP in the molding chamber 20, and a lower punch 12 that receives the workpiece MP to be pressed. An upper backing 13 that applies a pressing force is attached to the upper punch 11. The lower punch 12 may use a backing that receives the press load, or may be attached with a lower backing 14 that is supported by a cushion mechanism that controls the load applied to the workpiece, as shown in FIG. 1. The molding apparatus 1 further includes a heating means for the die 2. The heating means is, for example, an electric current heating or induction heating device for the die 2, or a heating furnace that houses the molding apparatus 1.
[0027] In the case of high-temperature molding using the die 2 as described above, in which the workpiece MP is pressed against the inner wall surface of the molding chamber 20, the die 2 expands thermally and becomes larger than its initial dimensions due to elastic deformation caused by the molding load of the press. When cooled after molding, the dimensions of the die 2 and the workpiece MP become smaller than in the high-temperature environment. However, if the amount of thermal contraction of the die 2 is larger than the amount of thermal contraction of the workpiece MP, it becomes impossible to remove the workpiece MP from the die 2.
[0028] One way to solve this problem is to use a tapered die, but as mentioned above, this requires fitting and finishing, which is problematic as it requires a lot of effort in die management. In the present invention, by providing a difference in thermal expansion coefficient between the constituent materials of the inner and outer dies, a die 2 for high-temperature molding is provided that can easily achieve precision and remove the workpiece MP, and can also simplify the effort of die management. Various specific examples of such a die 2 are described below.
[0029] [First embodiment] 2 is a horizontal cross-sectional view showing a high-temperature molding die 2A with a molding chamber having a rectangular cross section according to a first embodiment of the present invention. The die 2A has a molding chamber 20 having a rectangular cross section that contains a workpiece MP that will eventually become a molded product. The die 2A is composed of an outer die 3 and an inner die 4 whose periphery is surrounded by the outer die 3.
[0030] The outer mold 3 has a rectangular frame shape in cross section and has a rectangular inner wall surface 301 that serves as a holding surface for the inner mold 4. The inner mold 4 includes an outer side surface 401 adjacent to the inner wall surface 301 of the outer mold 3 and an inner side surface 402 that defines the molding chamber 20. The inner wall surface 301 surrounds the four sides of the inner mold 4. The inner mold 4 also has a rectangular frame shape in cross section. Examples of the mold material constituting the outer mold 3 and the inner mold 4 include metal-based materials, nonmetal-based materials, composite materials of metal-based materials and nonmetal-based materials, cermet-based materials, and ceramic-based materials. Examples of the metal-based materials include, for example, cemented carbide, tool steel, aluminum alloy, copper alloy, and magnesium alloy. Examples of the nonmetal-based materials include graphite, plastic formed carbon, CFRP, and carbon composites. Examples of the cermet-based materials include titanium carbonitride, and examples of the ceramic-based materials include alumina, silicon nitride, and zirconia.
[0031] Of the above mold materials, the material for the inner mold 4 is selected to have a larger thermal expansion and contraction than the material for the outer mold 3 in a specified temperature range. Here, the temperature of the outer mold 3 and inner mold 4 before high-temperature molding is T, and the temperature rise associated with high-temperature molding is ΔT. Temperature T is also the temperature when the molded product is removed from the mold 2A. ΔT is the temperature difference between the temperature during high-temperature molding and the temperature when the molded product is removed. Also, the thermal expansion coefficient of the inner mold 4 in the temperature range from temperature T to temperature T+ΔT is α, and the thermal expansion coefficient of the outer mold 3 is β. In this case, the mold 2A satisfies the relationship of the following formula (1). (1) α>β
[0032] Furthermore, the outer dimension of the inner die 4 in the direction along one center line CL passing through the center of the molding chamber 20 is defined as A, and the inner dimension of the outer die 3 is defined as B. In this case, it is desirable that the mold 2A satisfy the relationship of the following formula (2). (2) α×A×ΔT>β×B×ΔT
[0033] According to the above-mentioned mold 2A, as shown in formula (1), the thermal expansion coefficient α of the inner mold 4 is larger than the thermal expansion coefficient β of the outer mold 3, so that in the hot state where high-temperature molding is performed, the inner mold 4 expands inward while the outer mold 3 is restraining the periphery. Therefore, when the workpiece MP (FIG. 1) is placed in the molding chamber 20 and heated and pressed, the pressing force of the workpiece MP against the inner surface 402 of the inner mold 4 increases. Therefore, the inner shape of the molding chamber 20 can be well transferred to the workpiece MP, and processing can be performed with high precision. In addition, in the hot state, the inner mold 4 presses against the outer mold 3 to form an interference fit, which has the advantage of improving the strength of the mold 2A.
[0034] On the other hand, in the cold state after the mold is cooled, the degree of thermal contraction of the inner mold 4 is greater than that of the outer mold 3. That is, as shown in formula (2), the outer dimension A of the inner mold 4 is greater than the inner dimension B of the outer mold 3 in terms of the amount of thermal expansion and contraction in the temperature range of ΔT. That is, when the temperature is lowered from hot to cold, the inner mold 4 contracts more than the outer mold 3. Therefore, a gap is easily generated between the outer surface 401 of the inner mold 4 and the inner wall surface 301 of the outer mold 3, and the inner mold 4 can be easily released from the outer mold 3. If the thermal expansion coefficient α of the inner mold 4 is set to be smaller than the thermal expansion coefficient of the workpiece MP, the workpiece MP contracts more than the inner mold 4 in the molding chamber 20. Therefore, even if the inner mold 4 is a non-split type, the molded product of the workpiece MP can be easily removed from the inner mold 4.
[0035] As described above, the mold 2A utilizes the difference in thermal expansion coefficient between the inner mold 4 and the outer mold 3 to improve molding accuracy and remove the processed material MP. This eliminates the need for matching finish processing as with tapered molds. This makes it unnecessary to manage and store the inner mold 4 and outer mold 3 as a set, which simplifies mold management.
[0036] 3 is a cross-sectional view showing a high-temperature molding die 2B, which is a modified example of the first embodiment and has a molding chamber 20 that is circular in a horizontal cross-sectional view. The die 2B is composed of an outer die 3 having a frame shape with a circular cross section, and an inner die 4 whose periphery is surrounded by the outer die 3. The inner die 4 includes a cylindrical outer surface 401 adjacent to the cylindrical inner wall surface 301 of the outer die 3, and a cylindrical inner surface 402 that defines the molding chamber 20.
[0037] In the mold 2B, the relationship between the thermal expansion coefficient α of the inner mold 4 and the thermal expansion coefficient β of the outer mold 3 is as shown in the above formula (1). In addition, the relationship between the outer dimension of the inner mold 4 and the inner dimension of the outer mold 3 along the center line CL passing through the center of the molding chamber 20, that is, the relationship between the amount of thermal expansion and contraction in the temperature range of ΔT when the diameter of the inner mold 4 is A and the inner diameter of the outer mold is B, is as shown in the above formula (2). Even in a mold with a circular cross section such as the mold 2B, by satisfying the relationship of formula (1) and further formula (2), the inner mold 4 shrinks more than the outer mold 3 in the cold state. Therefore, the ease of removing the molded product of the workpiece MP from the mold 2B can be improved.
[0038] FIG. 4 is a cross-sectional view showing a high-temperature molding die 2C according to another modified example of the first embodiment. The structure itself of the outer die 3 and the inner die 4 of the die 2C is the same as that of the die 2A previously shown in FIG. 2. The difference is that a partition plate 5 is arranged in the molding chamber 20 of the inner die 4. FIG. 4 shows an example in which two partition plates 5 are arranged at equal intervals in the direction of the center line CL. The two partition plates 5 divide the molding chamber 20 into three small chambers 20A. The workpiece MP is loaded into each small chamber 20A, and high-temperature molding is performed. In other words, the die 2C can simultaneously produce three molded products in one molding.
[0039] [Second embodiment] FIG. 5 is a horizontal cross-sectional view showing a high-temperature molding die 2D according to the second embodiment, in which a molding chamber 20 having a rectangular cross section is partitioned by a split inner die. The die 2D is composed of an outer die 3 and an inner die 4A whose periphery is surrounded by the outer die 3. The inner die 4A has an outer side surface 401 adjacent to the inner wall surface 301 of the outer die 3 and an inner side surface 402 that partitions the molding chamber 20 having a rectangular cross section. The above points are the same as those of the die 2A of the first embodiment. The die 2D differs from the die 2A of the first embodiment in that the inner die 4A of the die 2D is a split die formed by an assembly of a pair of first split dies 41 and a pair of second split dies 42. By adopting the split inner die 4A, the molded product after high-temperature molding of the workpiece MP can be easily removed from the inner die 4A.
[0040] The pair of first split molds 41 are mold halves each having a rectangular cross section, and are arranged opposite each other across the center line CL of the molding chamber 20. The pair of second split molds 42 are mold halves each having a rectangular cross section, and are arranged in a direction intersecting the center line CL, more specifically, in a direction perpendicular to the center line CL. One second split mold 42 is arranged adjacent to one end 411 of the first split mold 41, and closes the space between the pair of one ends 411. The other second split mold 42 is arranged adjacent to the other end 412 of the first split mold 41, and closes the space between the pair of other ends 412.
[0041] The first split mold 41 and the second split mold 42 are formed from the same mold material. That is, the thermal expansion coefficients of the first split mold 41 and the second split mold 42 in the temperature range from temperature T to temperature T+ΔT are α. The thermal expansion coefficient of the outer mold 3 is β, and is set to have the relationship α>β as shown in formula (1). Regarding the amount of thermal expansion, the mold 2D satisfies the relationship of the following formula (3), where A1 is the dimension of the first split mold 41 along the center line CL and A2 is one dimension of the second split mold 42 along the center line CL. (3) α×A1×ΔT+2×(α×A2×ΔT)>β×B×ΔT
[0042] According to the mold 2D of the second embodiment, an inner mold 4A is used, which is made up of a pair of first split molds 41 and a pair of second split molds 42. In the temperature range of ΔT, the amount of thermal expansion and contraction of the total outer dimension A1+2×A2 of the split mold pair constituting the inner mold 4A is greater than the amount of thermal expansion and contraction of the inner dimension B of the outer mold 3. This improves the molding accuracy of the workpiece MP, and also makes it possible to reliably release the inner mold 4A made up of the split mold pair from the outer mold 3. It also makes it easier to remove the molded product from the inner mold 4A.
[0043] FIG. 6 is a horizontal cross-sectional view showing a high-temperature molding die 2E in which a molding chamber 20 having a circular cross section is partitioned by a split inner die 4B, which is a modified example of the second embodiment. The die 2E is composed of an outer die 3 having a circular cross-sectional frame shape and an inner die 4B having a circular cross-sectional frame shape surrounded by the outer die 3. The split inner die 4B is composed of arc-shaped divided pieces obtained by dividing a cylinder having the center of the molding chamber 20 as a circular center into a plurality of parts in the circumferential direction. FIG. 6 shows an inner die 4B divided equally into four parts in the circumferential direction. The inner die 4B includes a cylindrical outer surface 401 adjacent to the cylindrical inner wall surface 301 of the outer die 3, and a cylindrical inner surface 402 that partitions the molding chamber 20. The division of the inner die 4B is arbitrary, and may be divided into three or less, five or more, or may not be divided equally.
[0044] Specifically, the inner mold 4B is composed of a pair of first arc-shaped divided dies 45 facing each other along one center line CL that passes through the center of the molding chamber 20, and a pair of second arc-shaped divided dies 46 arranged facing each other across the center line CL. The annular inner mold 4B is configured in such a manner that two circumferential gaps between the pair of first arc-shaped divided dies 45 are closed by the pair of second arc-shaped divided dies 46, respectively.
[0045] The first arc-segmented mold 45 and the second arc-segmented mold 46 are formed of the same mold material. That is, the thermal expansion coefficient of the first arc-segmented mold 45 and the second arc-segmented mold 46 in the temperature range from temperature T to temperature T+ΔT is α. The thermal expansion coefficient of the outer mold 3 is β, and is set to have the relationship α>β as shown in formula (1). Regarding the amount of thermal expansion and contraction, the mold 2E satisfies the relationship of formula (5) below, where A3 is the distance between the first arc-segmented molds 45 on the center line CL, and A4 is one dimension (thickness) of the first arc-segmented mold 45 along the center line CL. (5) α×(A3+2×A4)×ΔT>β×B×ΔT
[0046] According to the mold 2E in Fig. 6, when the inner mold 4B is formed by combining the first arc-shaped split mold 45 and the second arc-shaped split mold 46, the amount of thermal expansion and contraction of the outer dimension A3+2×A4 of the inner mold 4B is larger than the amount of thermal expansion and contraction of the inner dimension B of the outer mold in the temperature range of ΔT. This improves the molding accuracy of the workpiece MP, and also enables the inner mold 4B consisting of a split mold pair to be reliably released from the outer mold 3. In addition, because the inner mold 4B is a split mold, it is easy to remove the molded product from the inner mold 4B.
[0047] FIG. 7 is a horizontal cross-sectional view showing a high-temperature molding die 2F using a split inner die 4A having a different thermal expansion coefficient, which is a modified example of the second embodiment. The structure itself of the outer die 3 and the split inner die 4A of the die 2F is the same as that of the die 2D shown in FIG. 5. The difference is that the thermal expansion coefficient of the first split die 41 and the thermal expansion coefficient of the second split die 42 are different. For example, depending on the shape of the molded product, that is, the shape of the molding chamber 20, the amount of thermal expansion may be significantly different between the direction along the center line CL and the direction perpendicular to the center line CL. In this case, in the split inner die 4A, the thermal expansion coefficients of the first split die 41 and the second split die 42 are adjusted to improve the ease of removal of the molded product.
[0048] Regarding the amount of thermal expansion and contraction, when the thermal expansion coefficient of first split mold 41 in the temperature range from temperature T to temperature T+ΔT is α1 and the thermal expansion coefficient of second split mold 42 is α2, mold 2F satisfies the relationship of the following formula (4). (4)α1×A1×ΔT+2×(α2×A2×ΔT)>β×B×ΔT (however, α1>β, α2>β)
[0049] FIG. 8 is a cross-sectional view showing a high-temperature molding die 2G according to another modified example of the second embodiment. The structure itself of the outer die 3 and the split inner die 4A of the die 2G is the same as that of the die 2D previously shown in FIG. 5. The difference is that two partition plates 5 are arranged in the molding chamber 20 of the inner die 4A. The molding chamber 20 is divided into three small chambers 20A by the two partition plates 5. The workpiece MP is loaded into each small chamber 20A, and high-temperature molding is performed. In other words, the die 2G can simultaneously produce three molded products in one molding.
[0050] In the mold 2G, the thermal expansion coefficient of the contents in the molding chamber 20 may be taken into consideration. In the mold 2G, the partition plate 5 and the workpiece MP loaded in the small chamber 20A are the contents. If the amount of thermal expansion and contraction of the contents along the center line CL is smaller than the amount of thermal expansion and contraction of the first split mold 41 along the center line CL, it may hinder the release of the inner mold 4A from the outer mold 3. For example, when the heat is transferred from hot to cold, if the amount of thermal contraction of the contents is smaller than the amount of thermal contraction of the first split mold 41, the contents may press the second split mold 42 against the inner wall surface 301 of the outer mold 3. In this case, it is desirable to set the amount of thermal expansion and contraction of the inner mold 4A including the contents to be larger than the amount of thermal expansion and contraction of the outer mold. In other words, in addition to the amount of thermal expansion and contraction of the first split mold 41 along the center line CL, the amount of thermal expansion and contraction of the contents may be taken into consideration.
[0051] Here, assuming that the thermal expansion coefficient of the partition plate 5 is δ, the thermal expansion coefficient of the workpiece MP loaded into the small chamber 20A is ε, the dimension of the partition plate 5 along the center line CL is D, the dimension of the small chamber 20A along the center line CL is E, the number of parallel partition plates 5 is N1, and the number of parallel chambers 20A is N2, the configuration may further satisfy the relationship of the following formula (3-1) in addition to the above formula (3). (3-1) 2×(α×A2×ΔT)+δ×D×ΔT×N1+ε×E×ΔT×N2>β×B×ΔT
[0052] [Third embodiment] 9 is a cross-sectional view showing a high-temperature molding die 2H according to the third embodiment, in which a molding chamber 20 having a rectangular cross section is partitioned by two layers of split inner dies. The die 2H is composed of an outer die 3 and an inner die 4C whose periphery is surrounded by the outer die 3. The inner die 4C is a split frame body and has a two-layer structure of a first inner die layer 40A and a second inner die layer 40B whose periphery is surrounded by the first inner die layer 40A. The die 2H is an embodiment in which a split inner die is further disposed inside the inner die 4A of the die 2D shown in FIG. 5.
[0053] The first inner mold layer 40A of the inner mold 4C is formed by an assembly of a pair of first split molds 41 and a pair of second split molds 42. The pair of first split molds 41 are arranged opposite each other across the center line CL of the molding chamber 20. The pair of second split molds 42 are arranged in a direction perpendicular to the center line CL. One of the second split molds 42 is arranged adjacent to one end 411 of the first split mold 41 and closes the space between the pair of one ends 411. The other of the second split molds 42 is arranged adjacent to the other end 412 of the first split mold 41 and closes the space between the pair of other ends 412.
[0054] The second inner mold layer 40B defines the molding chamber 20. The second inner mold layer 40B is formed by an assembly of a pair of third split molds 43 and a pair of fourth split molds 44 arranged along the inner side 402 of the area defined by the first inner mold layer 40A. The pair of third split molds 43 are mold pieces each having a rectangular cross section, and are arranged opposite each other across the center line CL of the molding chamber 20. The pair of second split molds 42 are mold pieces each having a rectangular cross section, and are arranged in a direction perpendicular to the center line CL. One fourth split mold 44 is arranged adjacent to one end 431 of the third split mold 43 and closes the space between the pair of one ends 431. The other fourth split mold 44 is arranged adjacent to the other end 432 of the third split mold 43 and closes the space between the pair of other ends 432. The outer side 403 of the second inner mold layer 40B abuts against the inner side 402 of the first inner mold layer 40A. The inner surface 404 of the second inner mold layer 40B becomes an inner wall surface that defines the molding chamber 20.
[0055] In the hot mold 2H, the first inner layer 40A, whose outward expansion is restricted by the outer mold 3, expands inward and pushes the second inner layer 40B inward. In the direction of extension of the center line CL, one end 431 and the other end 432 of the third split mold 43 of the second inner layer 40B abut against the fourth split mold 44. In the direction intersecting with the center line CL, the side of the second inner layer 40B abuts against the inner side surface 402 of the first inner layer 40A. Therefore, according to the mold 2H having the split inner mold 4C with a two-layer structure, the dimensions inside the molding chamber 20 are as designed, and there is an advantage in that no gap occurs between the split molds, so that the generation of burrs can be suppressed.
[0056] In the mold 2H, the thermal expansion coefficients of the first split mold 41 and the second split mold 42 in the temperature range from temperature T to temperature T+ΔT are both α. The thermal expansion coefficients of the third split mold 43 and the fourth split mold 44 in the temperature range from temperature T to temperature T+ΔT are both γ. It is also possible for α=γ. The thermal expansion coefficient of the outer mold 3 is β, and is set to at least the relationship α>β as shown in formula (1). Regarding the amount of thermal expansion, the mold 2H is set to satisfy the relationship of the following formula (6) or (7), where A1 is the dimension of the first split mold 41 along the center line CL, A2 is one dimension of the second split mold 42 along the center line CL, C1 is the dimension of the third split mold 43 along the center line CL, and C2 is one dimension of the fourth split mold 44 along the center line CL. (6) α×A1×ΔT+2×(α×A2×ΔT)>β×B×ΔT (where α>γ) (7) 2×(α×A2×ΔT)+γ×C1×ΔT+2×(γ×C2×ΔT)>β×B×ΔT(where α<γ)
[0057] According to the mold 2H, the inner mold 4C has a multi-layer structure in which a second inner mold layer 40B composed of a pair of third split molds 43 and a pair of fourth split molds 44 is arranged in a first inner mold layer 40A composed of a pair of first split molds 41 and a pair of second split molds 42. In addition, taking into account the difference in thermal expansion coefficient between the first inner mold layer 40A and the second inner mold layer 40B, the total outer dimension of the inner mold 4C is set larger than the inner dimension of the outer mold 3 for the amount of thermal expansion and contraction in the temperature range of ΔT. Therefore, the molding accuracy is improved, and the inner mold 4C formed of two split mold layers can be reliably released from the outer mold 3. In the third embodiment, a partition plate 5 may be arranged in the molding chamber 20 to partition a plurality of small chambers 20A as in the modified example of the second embodiment in FIG. 8. This allows a plurality of molded products to be produced simultaneously in one molding.
[0058] Fig. 10 is a cross-sectional view showing a high-temperature molding die 2I having an inner die 4C formed using split dies with different thermal expansion coefficients, which is a modified example of the third embodiment. The structure itself of the outer die 3 and split inner die 4C of the die 2I is the same as that of the die 2H shown in Fig. 9. The difference is that the thermal expansion coefficient of the first split die 41 of the first inner die layer 40A is different from that of the second split die 42. The thermal expansion coefficients of the third split die 43 and the fourth split die 44 of the second inner die layer 40B are the same value = γ.
[0059] Regarding the amount of thermal expansion and contraction, when the thermal expansion coefficient of the first split mold 41 is α1 and the thermal expansion coefficient of the second split mold 42 is α2 in the temperature range from temperature T to temperature T+ΔT, the mold 2I is set so as to satisfy the relationship of equation (6-1) or (7-1), which is obtained by rewriting the above equations (6) and (7) as follows. (6-1) α1×A1×ΔT+2×(α2×A2×ΔT)>β×B×ΔT (where α1>γ) (7-1) 2×(α2×A2×ΔT)+γ×C1×ΔT+2×(γ×C2×ΔT)>β×B×ΔT (where α1<γ) In this modification, a partition plate 5 may be disposed in the molding chamber 20 to partition the chambers 20A into a plurality of small chambers as in the modification of the second embodiment shown in Fig. 8. This allows a plurality of molded products to be produced simultaneously in one molding run.
[0060] Fig. 11 is a cross-sectional view showing a high-temperature molding die 2J having an inner die 4C formed using split dies with different thermal expansion coefficients, which is another modified example of the third embodiment. The structure itself of the outer die 3 and split inner die 4C of the die 2J is the same as that of the die 2H shown in Fig. 9. The differences are that the thermal expansion coefficients of the first split die 41 and the second split die 42 of the first inner die layer 40A are different, the thermal expansion coefficients of the third split die 43 and the fourth split die 44 of the second inner die layer 40B are different, and further, two partition plates 5 are arranged in the molding chamber 20.
[0061] In mold 2J, the thermal expansion coefficient of first split mold 41 in the temperature range from temperature T to temperature T+ΔT is α1, the thermal expansion coefficient of second split mold 42 is α2, the thermal expansion coefficient of third split mold 43 is γ1, and the thermal expansion coefficient of fourth split mold 44 is γ2. In this case, mold 2J is set with respect to the amount of thermal expansion so as to satisfy the relationship of formula (6-2) or (7-2) obtained by rewriting the above formulas (6) and (7) as follows: (6-2) α1×A1×ΔT+2×(α2×A2×ΔT)>β×B×ΔT (where α1×A1 > γ1×C1+2×γ2×C2) (7-2) 2×(α2×A2×ΔT)+γ1×C1×ΔT+2×(γ2×C2×ΔT)>β×B×ΔT (where α1×A1 < γ1×C1+2×γ2×C2)
[0062] As yet another modified example of the third embodiment, a high-temperature molding die may be used in which the thermal expansion coefficients of the first split die 41 and the second split die 42 in the temperature range from temperature T to temperature T+ΔT are the same value (α), the thermal expansion coefficient of the third split die 43 is γ1, and the thermal expansion coefficient of the fourth split die 44 is γ2 (γ1 ≠ γ2). In addition, by disposing the partition plate 5 in the molding chamber 20 to divide the small chamber 20A, multiple molded products can be produced simultaneously in one molding run.
[0063] [Variations of external shape] Next, modified examples of the outer mold 3 will be described. In the above embodiment, the outer mold 3 completely surrounds the four sides of the inner mold 4. The outer mold 3 does not have to be of the completely surrounding type as described above, and it is sufficient if it has a holding surface that holds the inner mold 4.
[0064] Fig. 12(A) is a top view showing a high-temperature molding die 2K having an outer die 3A according to a modified example, and Fig. 12(B) is a cross-sectional view taken along line XIIB-XIIB in Fig. 12(A). The die 2K is composed of an outer die 3A and an inner die 4D held by the outer die 3A. The outer die 3A includes an outer die base 31 formed of a rectangular parallelepiped having a substantially square shape when viewed from above, and a restricting plate 32 erected from the outer die base 31. The restricting plate 32 is a rectangular parallelepiped having a rectangular cross section, and is erected from the central regions of the four sides of the outer die base 31. The inner surface of the restricting plate 32 is a holding surface 32A that holds the inner die 4.
[0065] The inner mold 4D is formed by a pair of first split molds 41A and a pair of second split molds 42A, and defines the molding chamber 20. The outer surfaces of the first split mold 41A and the second split mold 42A are adjacent to the holding surfaces 32A of the regulating plates 32 that are arranged correspondingly. The first split mold 41A and the second split mold 42A are each smaller in size than the regulating plates 32, and spacers 6 that fill the size difference between them are disposed at the four corners of the inner mold 4D.
[0066] In the mold 2K, the thermal expansion coefficient of the first split mold 41A and the second split mold 42A of the inner mold 4D in the temperature range from temperature T to temperature T+ΔT is α, and the thermal expansion coefficient of the outer mold 3A is β. In this case, the relationship α>β is set as shown in formula (1). The amount of thermal expansion and contraction can be mutatis mutandis with the relationship of the mold 2D shown in Figure 5. In other words, when the dimension of the first split mold 41A is A1, one dimension of the second split mold 42A is A2, and the dimension between the holding surfaces 32A of a pair of opposing regulating plates 32 is B, the mold 2K satisfies the relationship of formula (3) shown above.
[0067] Fig. 13(A) is a top view showing a high-temperature molding die 2L having an outer die 3B according to another modified example, and Fig. 13(B) is a cross-sectional view taken along line XIIIB-XIIIB in Fig. 13(A). The die 2L is composed of an outer die 3B and an inner die 4E held by the outer die 3B. The outer die 3B includes an outer die base 310 formed of a rectangular parallelepiped having a substantially square shape in top view, and a regulating rod 33 erected from the outer die base 310. The regulating rod 33 is a cylindrical body, and two of them are erected from each of the four sides of the outer die base 310.
[0068] The inner mold 4E is formed by a pair of first split molds 41B and a pair of second split molds 42B, and defines the molding chamber 20. The outer surfaces of the first split mold 41B and the second split mold 42B are adjacent to the inner peripheral surfaces of the correspondingly arranged regulating rods 33. In this modification, the inner peripheral surfaces of the regulating rods 33 are the holding surfaces of the inner mold 4E.
[0069] In the mold 2L, the thermal expansion coefficient of the first split mold 41B and the second split mold 42B of the inner mold 4E in the temperature range from temperature T to temperature T+ΔT is α, and the thermal expansion coefficient of the outer mold 3B is β. In this case, the relationship α>β is set as shown in formula (1). The relationship of the mold 2D shown in Figure 5 can be applied mutatis mutandis to the amount of thermal expansion and contraction. In other words, when the dimension of the first split mold 41B is A1, one dimension of the second split mold 42B is A2, and the dimension between the inner peripheral surfaces of a pair of opposing regulating rods 33 is B, the mold 2L satisfies the relationship of formula (3) shown above.
[0070] In the above embodiments, the molding chamber 20 has been described as being rectangular or circular in horizontal cross section, but the cross-sectional shape is not limited to these. The cross-sectional shape of the molding chamber 20 is appropriately set according to the contour of the molded product. Therefore, the cross-sectional shape of the inner mold exemplified in each of the above embodiments is appropriately set according to the contour of the molded product. [Explanation of symbols]
[0071] 1 Molding equipment 1 2, 2A~2L mold 20 Molding room 20A Small Room (Multiple Compartments) 3, 3A, 3B external type 301 Inner wall surface (retaining surface) 4, 4A~4E inner mold 401 External surface 402 Inner surface 40A 1st inner mold layer 40B 2nd inner mold layer 41 1st split type 411 one end 412 Other end 42 Second split type 43 Third division type 44 4th division type 45 1st arc division type 46 Second arc division type 5 Partition
Claims
1. an outer mold including a retaining surface; An inner mold including an outer surface at least partially adjacent to the holding surface and an inner surface defining a molding chamber, the inner mold is a split-type inner mold formed by an assembly of a plurality of split molds, the holding surface is an inner wall surface surrounding the inner mold, The temperature of the outer mold and the inner mold before high-temperature molding is T, the temperature rise due to high-temperature molding is ΔT, the thermal expansion coefficient of the inner mold in the temperature range from temperature T to temperature T+ΔT is α, and the thermal expansion coefficient of the outer mold is β. The relationship of the following formula (1) is satisfied: In a high-temperature molding die, when an outer dimension of the inner die is A and an inner dimension of the outer die is B in a direction along a center line passing through the center of the molding chamber, the relationship of the following formula (2) is satisfied: The plurality of split molds are: A pair of first split dies arranged opposite each other across a center line of the molding chamber; a pair of second split dies arranged opposite each other so as to intersect with the center line and be adjacent to one end and the other end of the pair of first split dies, When a dimension of the first split mold along the center line is A1 and a dimension of one of the second split molds along the center line is A2, the relationship of the following formula (3) is satisfied, When the thermal expansion coefficient of the first split mold is α1 and the thermal expansion coefficient of the second split mold is α2 in a temperature region from temperature T to temperature T+ΔT, the relationship of the following formula (4) is satisfied: The molding chamber has a shape such that the thermal expansion coefficient of a molded product molded in the molding chamber differs between a direction along the center line and a direction perpendicular to the center line. (1)α>β (2) α×A×ΔT>β×B×ΔT (3) α×A1×ΔT+2×(α×A2×ΔT)>β×B×ΔT (4) α1×A1×ΔT+2×(α2×A2×ΔT)>β×B×ΔT (however, α1>β, α2>β)
2. In the high-temperature molding die according to claim 1, the plurality of split dies are arranged along an inner wall surface partitioned by the pair of first split dies and the pair of second split dies, and further include a pair of third split dies and a pair of fourth split dies which partition the molding chamber; The pair of third split dies are disposed opposite to each other across a center line of the molding chamber, the pair of fourth split dies are disposed opposite each other so as to intersect with the center line and to be adjacent to one end and the other end of the pair of third split dies, A high-temperature molding die, which satisfies the relationship of the following formula (6) or (7), where γ is the thermal expansion coefficient of the third split die and the fourth split die in the temperature range from temperature T to temperature T+ΔT, C1 is a dimension of the third split die along the center line, and C2 is one dimension of the fourth split die along the center line. (6) α×A1×ΔT+2×(α×A2×ΔT)>β×B×ΔT (where α<γ) (7) 2×(α×A2×ΔT)+γ×C1×ΔT+2×(γ×C2×ΔT)>β×B×ΔT (where α>γ)
3. In the high-temperature molding die according to claim 1 or 2, The high-temperature molding die further comprises a partition plate disposed inside the molding chamber and dividing the molding chamber into a plurality of compartments.
Citation Information
Patent Citations
Hot press die
JP1979118408A
Mold for hot press
JP1981141998A
Jig and molding tool
JP2016168676A
JP2553811U
Molding die for electric sintering