SUBSTRATE PROCESSING SYSTEM AND SUBSTRATE PROCESSING METHOD
The substrate processing system improves throughput by using independent thickness measurement devices before and after grinding, optimizing chuck table inclination for uniformity, addressing inefficiencies in conventional systems.
Patent Information
- Application Number
- JP2022565233
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-11-27
- Filing Date
- 2021-11-15
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-11-15
AI Technical Summary
Conventional wafer processing systems face decreased throughput due to the integration of thickness measurement and grinding processes, which prolongs the working time at the secondary grinding position, leading to inefficiencies in substrate processing.
A substrate processing system that includes separate thickness measuring devices before and after grinding, allowing independent measurement and adjustment of wafer thickness, coupled with a control system to optimize the inclination of the chuck table for uniform grinding, thereby separating the measurement process from the grinding operation.
This approach enhances throughput by reducing the time spent on thickness measurement within the grinding equipment, ensuring uniformity of wafer thickness, and maintaining cleanliness across processing stages.
Smart Images

Figure 0007581374000001 
Figure 0007581374000002 
Figure 0007581374000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a substrate processing system and a substrate processing method. [Background technology]
[0002] Patent Document 1 discloses a grinding device that adjusts the wafer thickness by adjusting the tilt angle of a chuck table. In this grinding device, a finishing thickness measuring device is disposed near the secondary grinding position to measure the thickness of only the secondary ground wafer at multiple points in the radial direction, and the radial thickness distribution of the wafer is determined from the wafer thickness measured by the device. Then, based on the determined radial thickness distribution, the tilt angle adjustment mechanism tilts the chuck table to adjust the angle of the wafer relative to the grindstone, thereby adjusting the wafer thickness after secondary grinding. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japan Patent Publication No. 2008-264913 Summary of the Invention [Problem to be solved by the invention]
[0004] The techniques disclosed herein improve the throughput of substrate processing, including substrate grinding. [Means for solving the problem]
[0005] A substrate processing system for processing a laminated substrate in which a first substrate and a second substrate are bonded together, the system comprising: a processing device for grinding the first substrate; Located outside of a first thickness measuring device for measuring a thickness of the first substrate before grinding and a total thickness of the laminated substrate including the first substrate; and Located outside of and a second thickness measuring device that measures the thickness of the first substrate after grinding. Effect of the Invention
[0006] According to the present disclosure, the throughput of substrate processing, including substrate grinding, can be improved. [Brief description of the drawings]
[0007] [Figure 1] 1 is a side view showing a configuration example of a laminated wafer processed in a wafer processing system. [Diagram 2] FIG. 1 is a plan view showing a configuration example of a wafer processing system. [Diagram 3] 1 is a side view showing an example of an internal configuration of a wafer processing system. [Figure 4] 4 is an explanatory diagram showing the thickness of an upper wafer, the thickness of a lower wafer, and the total thickness of an overlapping wafer. FIG. [Diagram 5] 4 is a side view showing a configuration example of each grinding unit. FIG. [Figure 6] FIG. 2 is a plan view showing a configuration example of a first thickness measurement device. [Figure 7] FIG. 2 is a side view showing a configuration example of a first thickness measurement device. [Figure 8] FIG. 2 is a perspective view showing a configuration example of a first thickness measuring device. [Figure 9] FIG. 4 is an explanatory diagram showing an example of a thickness measurement position in a plan view. [Figure 10] 11 is a plan view showing an example of a state in which a thickness is measured by an entire thickness measuring unit. FIG. [Figure 11] FIG. 11 is a plan view showing an example of a state in which thickness is measured by a partial thickness measuring unit. [Figure 12] FIG. 4 is an explanatory diagram showing an air current generated inside the first thickness measurement device. [Figure 13] FIG. 4 is a plan view showing a configuration example of a second thickness measurement device. [Figure 14] FIG. 4 is a side view showing a configuration example of a second thickness measuring device. [Figure 15] FIG. 2 is a flow diagram showing an example of main steps of wafer processing. [Figure 16] 4A to 4C are explanatory views showing an example of main steps in a first thickness measuring device. [Figure 17]5A to 5C are explanatory views showing an example of main steps in a second thickness measuring device. [Figure 18] FIG. 13 is a plan view showing a configuration example of a wafer processing system according to another embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] In recent years, in the manufacturing process of semiconductor devices, a laminated wafer in which a semiconductor substrate (hereinafter referred to as an "upper wafer") having a plurality of devices such as electronic circuits formed on its surface and a lower wafer are bonded together is produced by grinding the back surface of the upper wafer to thin it.
[0009] The upper wafer is thinned by bringing a grinding wheel into contact with the back surface of the upper wafer while the back surface of the lower wafer is held by a chuck, and grinding the back surface of the upper wafer. However, when grinding the upper wafer in this manner, the flatness (total thickness variation (TTV)) of the upper wafer after grinding may be deteriorated due to the relative inclination between the grinding wheel that is in contact with the back surface of the upper wafer and the chuck that holds the lower wafer.
[0010] In the grinding apparatus disclosed in the above-mentioned Patent Document 1, the tilt angle of the chuck table is adjusted to adjust the thickness of the wafer, for example to make it uniform. Specifically, after the secondary grinding (finish grinding) is completed, the thickness of the wafer is measured at multiple points in the radial direction to grasp the radial thickness distribution of the wafer, and based on this thickness distribution, the chuck table is tilted to adjust the angle of the wafer relative to the grindstone. In addition, in this grinding apparatus, a finish thickness measuring device is provided near the secondary grinding position, and the thickness is measured while the wafer is held in the chuck. This shortens the work time required to grasp the radial thickness distribution, thereby improving production efficiency.
[0011] However, in the grinding device disclosed in Patent Document 1, the secondary grinding of the wafer and the measurement of the wafer thickness are performed at the secondary grinding position. If the tendency after the secondary grinding is used to adjust the tilt of the chuck table when grinding the next wafer, the operation time at the secondary grinding position of the grinding device will be longer, resulting in a decrease in the throughput of the entire wafer processing. Therefore, there is room for improvement in conventional wafer processing.
[0012] The technology disclosed herein improves the throughput of substrate processing, including substrate grinding. Hereinafter, a wafer processing system as a substrate processing system and a wafer processing method as a substrate processing method according to the present embodiment will be described with reference to the drawings. In this specification and the drawings, elements having substantially the same functional configurations are denoted by the same reference numerals, and duplicated descriptions will be omitted.
[0013] In a wafer processing system 1 according to this embodiment, which will be described later, a process is performed on an overlapped wafer T, which is an overlapped substrate in which an upper wafer W as a first substrate and a lower wafer S as a second substrate are bonded together, as shown in Fig. 1. Then, in the wafer processing system 1, the upper wafer W is thinned. Hereinafter, the surface of the upper wafer W that is bonded to the lower wafer S is referred to as the front surface Wa, and the surface opposite the front surface Wa is referred to as the back surface Wb. Similarly, the surface of the lower wafer S that is bonded to the upper wafer W is referred to as the front surface Sa, and the surface opposite the front surface Sa is referred to as the back surface Sb.
[0014] The upper wafer W is a semiconductor wafer such as a silicon substrate, and has a device layer Dw including a plurality of devices formed on its surface Wa. A surface film Fw is further formed on the device layer Dw, and the upper wafer W is bonded to the lower wafer S via the surface film Fw. Examples of the surface film Fw include an oxide film (SiO2 film, TEOS film), a SiC film, a SiCN film, or an adhesive.
[0015] The lower wafer S has, for example, the same configuration as the upper wafer W, and a device layer Ds and a surface film Fs are formed on the surface Sa. The lower wafer S does not need to be a device wafer on which a device layer Ds is formed, and may be, for example, a support wafer that supports the upper wafer W. In such a case, the lower wafer S functions as a protective material that protects the device layer Dw of the upper wafer W.
[0016] In the drawings used in the following description, the device layers Dw, Ds and the surface films Fw, Fs may be omitted in order to avoid complication of the illustration.
[0017] 2 and 3, the wafer processing system 1 has a configuration in which a loading / unloading station 2 and a processing station 3 are integrally connected. The loading / unloading station 2 loads / unloads a cassette C capable of accommodating a plurality of overlapped wafers T, for example, between the outside and the loading / unloading station 2. The processing station 3 is equipped with various processing devices that perform desired processing on the overlapped wafers T.
[0018] The loading / unloading station 2 serving as a loading / unloading area is provided with a cassette mounting table 10. In the illustrated example, a plurality of cassettes C, for example, two cassettes C, can be freely mounted in a line in the Y-axis direction on the cassette mounting table 10. The number of cassettes C mounted on the cassette mounting table 10 is not limited to the present embodiment and can be determined arbitrarily.
[0019] The processing station 3 is provided with, for example, three processing blocks G1 to G3. The first processing block G1, the second processing block G2, and the third processing block G3 are arranged in this order from the negative side of the X-axis (the loading / unloading station 2 side) to the positive side. The processing blocks G1 to G3 are spatially separated from each other by partitions, and the laminated wafer T is transported between the processing blocks G1 to G3 through loading / unloading ports formed in the various processing devices. The loading / unloading ports formed in the various processing devices are provided with shutters (not shown) for opening and closing the loading / unloading ports.
[0020] The first processing block G1 is provided with an etching processing device 30 and a wafer transport device 40. The etching processing device 30 is provided, for example, stacked in two stages in the vertical direction. The wafer transport device 40 is disposed on the Y-axis positive side of the etching processing device 30. Note that the number and arrangement of the etching processing devices 30 and the wafer transport devices 40 are not limited to this.
[0021] The etching processing device 30 etches the back surface Wb of the upper wafer W and the back surface Sb of the lower wafer S after grinding. At this time, cleaning processes such as removing particles and metal components are also performed. For example, an etching solution is supplied to the back surfaces Wb and Sb, and the back surfaces Wb are wet-etched. For example, FPM, HF, HNO3, H3PO4, TMAH, Choline, KOH, etc. are used as the etching solution.
[0022] The wafer transfer device 40 as a first substrate transfer device has, for example, two transfer arms 41 that hold and transfer the overlapped wafer T. Each transfer arm 41 is configured to be movable horizontally, vertically, around a horizontal axis, and around a vertical axis. The wafer transfer device 40 is configured to be able to transfer the overlapped wafer T to the cassette C on the cassette mounting table 10, the etching device 30, a first cleaning device 50 (described later), a second cleaning device 51 (described later), a first thickness measuring device 52 (described later), and a second thickness measuring device 53 (described later).
[0023] The first processing block G1 is also provided with a fan filter unit (FFU) (not shown), which keeps the interior of the first processing block G1 highly clean and maintains the internal pressure higher than that of the second processing block G2.
[0024] In the second processing block G2 as a processing region, a first cleaning device 50, a second cleaning device 51, a first thickness measuring device 52, a second thickness measuring device 53, and a wafer transport device 60 are provided. The first cleaning device 50, the second cleaning device 51, the first thickness measuring device 52, and the second thickness measuring device 53 are stacked in this order from above. The wafer transport device 60 is disposed on the Y-axis negative side of the first cleaning device 50, the second cleaning device 51, the first thickness measuring device 52, and the second thickness measuring device 53. The number and arrangement of the first cleaning device 50, the second cleaning device 51, the first thickness measuring device 52, the second thickness measuring device 53, and the wafer transport device 60 are not limited to this.
[0025] The first cleaning device 50 cleans the back surface Wb of the upper wafer W and the back surface Sb of the lower wafer S before grinding in the processing device 70 described later. For example, a cleaning liquid is supplied to the back surface Wb to spin-clean the back surface Wb, and a brush is brought into contact with the back surface Sb to scrub-clean the back surface Sb.
[0026] The second cleaning apparatus 51 cleans the back surface Wb of the upper wafer W and the back surface Sb of the lower wafer S after grinding in the processing apparatus 70 described later. Similarly to the first cleaning apparatus 50, the second cleaning apparatus 51 also supplies a cleaning liquid to the back surface Wb to spin-clean the back surface Wb, and brings a brush into contact with the back surface Sb to scrub-clean the back surface Sb.
[0027] The first thickness measuring device 52 measures a thickness Hw (see FIG. 4) of the upper wafer W before grinding in a processing device 70 described later, and a total thickness Ht (see FIG. 4) of the overlapped wafer T including the upper wafer W. The first thickness measuring device 52 also adjusts the horizontal orientation and position of the overlapped wafer T before grinding. The detailed configuration of the first thickness measuring device 52 and a detailed method of thickness measurement will be described later.
[0028] The second thickness measuring device 53 measures the thickness Hw (see FIG. 4) of the upper wafer W after grinding in the processing device 70 described later. The second thickness measuring device 53 also adjusts the horizontal orientation and position of the laminated wafer T after grinding. The detailed configuration of the second thickness measuring device 53 and the detailed method of thickness measurement will be described later.
[0029] The wafer transfer device 60 as the second substrate transfer device has, for example, two transfer arms 61 that adsorb and hold the overlapped wafer T by an adsorption holding surface (not shown) and transfer the overlapped wafer T. Each transfer arm 61 is configured to be movable in the horizontal direction, the vertical direction, around a horizontal axis, and around a vertical axis. The wafer transfer device 60 is configured to be able to transfer the overlapped wafer T to the second cleaning device 51, the first thickness measuring device 52, and a processing device 70 described later.
[0030] In this embodiment, an example will be described in which the wafer transport device 60 does not transport the overlapped wafer T to the first cleaning device 50 and the second thickness measuring device 53 based on the wafer processing steps described below. However, the overlapped wafer T may be configured to be transportable to the first cleaning device 50 and the second thickness measuring device 53 based on the wafer processing steps.
[0031] The third processing block G3 as a processing region is provided with one processing device 70. Note that the number and arrangement of the processing devices 70 are not limited to this.
[0032] The processing device 70 has a rotary table 71. On the rotary table 71, four chucks 72 are provided as third substrate holding parts for adsorbing and holding the overlapped wafer T. For example, a porous chuck is used for the chucks 72, and the chucks adsorb and hold the back surface Sb of the lower wafer S of the overlapped wafer T. The surface of the chucks 72, i.e., the holding surface of the overlapped wafer T, has a convex shape in which the center protrudes compared to the ends in a side view. Note that since this protrusion of the center is minute, the convex shape of the chucks 72 is omitted in the illustrations in the following description.
[0033] As shown in FIG. 5, the chuck 72 is held by a chuck base 73. The chuck base 73 is provided with an inclination adjustment unit 74 for adjusting the relative inclination between the grinding wheel and the chuck 72 provided in each grinding unit (rough grinding unit 80, medium grinding unit 90, and finish grinding unit 100) described later. The inclination adjustment unit 74 has a fixed shaft 75 provided on the lower surface of the chuck base 73 and a plurality of, for example, two, lifting shafts 76. Each lifting shaft 76 is configured to be freely expandable and contractible, and lifts and lowers the chuck base 73. The inclination adjustment unit 74 can tilt the chuck 72 and the chuck base 73 by vertically lifting and lowering one end of the outer periphery of the chuck base 73 (the position corresponding to the fixed shaft 75) using the lifting shaft 76 as a base point. This makes it possible to adjust the relative inclination between the surface of the grinding wheel and the surface of the chuck 72 provided in each grinding unit 80, 90, 100 at the processing positions A1 to A3.
[0034] The configuration of the inclination adjustment unit 74 is not limited to this, and can be selected arbitrarily as long as it can adjust the relative angle (parallelism) of the surface of the chuck 72 with respect to the surface of the grinding wheel.
[0035] 2, the four chucks 72 can be moved to a delivery position A0 and processing positions A1 to A3 by rotation of the rotary table 71. In addition, each of the four chucks 72 is configured to be rotatable about a vertical axis by a rotation mechanism (not shown).
[0036] At the delivery position A0, the overlapped wafer T is delivered by the wafer transport device 60. At the processing position A1, a rough grinding unit 80 is disposed and performs rough grinding of the upper wafer W. At the processing position A2, a medium grinding unit 90 is disposed and performs medium grinding of the upper wafer W. At the processing position A3, a finish grinding unit 100 is disposed and performs finish grinding of the upper wafer W.
[0037] 5, the rough grinding unit 80 has a rough grinding wheel 81 equipped with an annular rough grinding stone on its underside, a mount 82 supporting the rough grinding wheel 81, a spindle 83 rotating the rough grinding wheel 81 via the mount 82, and a drive section 84 incorporating, for example, a motor (not shown). The rough grinding unit 80 is configured to be movable in the vertical direction along a support column 85 shown in FIG.
[0038] The medium grinding unit 90 has a similar configuration to the rough grinding unit 80. That is, the medium grinding unit 90 has a medium grinding wheel 91 equipped with an annular medium grinding stone, a mount 92, a spindle 93, a drive unit 94, and a support 95. The grain size of the abrasive grains of the medium grinding stone is smaller than the grain size of the abrasive grains of the rough grinding stone.
[0039] The finish grinding unit 100 has a configuration similar to that of the rough grinding unit 80 and the medium grinding unit 90. That is, the finish grinding unit 100 has a finish grinding wheel 101 equipped with an annular finish grinding stone, a mount 102, a spindle 103, a drive unit 104, and a support column 105. The grain size of the abrasive grains of the finish grinding stone is smaller than the grain size of the abrasive grains of the medium grinding stone.
[0040] In addition, the third processing block G3 is provided with an exhaust unit (not shown). This allows particles and the like generated by the grinding process in the processing device 70 to be exhausted, and the internal pressure of the third processing block G3 is kept lower than the internal pressure of the second processing block G2. That is, in the wafer processing system 1, the internal pressures of the first processing block G1, the second processing block G2, and the third processing block G3 are controlled to increase in this order.
[0041] 2, the wafer processing system 1 is provided with a control device 110. The control device 110 is, for example, a computer equipped with a CPU, a memory, and the like, and has a program storage unit (not shown). The program storage unit stores a program for controlling the wafer processing in the wafer processing system 1. The program may be recorded in a computer-readable storage medium H and installed in the control device 110 from the storage medium H.
[0042] Next, a detailed configuration of the above-mentioned first thickness measuring device 52 will be described.
[0043] 6 and 7, the first thickness measurement device 52 has a chuck 300 as a first substrate holding unit that holds the overlapped wafer T. The chuck 300 suction-holds a central portion of the back surface Sb of the lower wafer S of the overlapped wafer T. The diameter of the chuck 300 is, for example, half or less of the diameter of the overlapped wafer T.
[0044] The chuck 300 is formed with a notch 301 extending in the radial direction (Y-axis direction) from the center to the outer end of the chuck 300. The notch 301 is formed so that a lower sensor 332 of the total thickness measuring unit 330 described later can advance and retreat.
[0045] The chuck 300 is configured to be rotatable around a vertical axis and movable in a horizontal direction. A rotation mechanism 310 for rotating the chuck 300 is provided below the chuck 300. A drive unit (not shown), such as a motor, is built into the rotation mechanism 310. The rotation mechanism 310 is supported by a support member 311. The support member 311 is attached to a rail 312 extending in the horizontal direction (Y-axis direction). The support member 311 is configured to be movable along the rail 312 by a movement mechanism 313 provided on the rail 312. A drive unit (not shown), such as a motor, is built into the movement mechanism 313. In this embodiment, the rotation mechanism 310 and the movement mechanism 313 for driving the chuck 300 constitute a "first drive unit" according to the technology of the present disclosure.
[0046] The side of the chuck 300 (X axis Positive direction The position detector 320 is provided on the side of the chuck 300 as a first position detector. The position detector 320 detects the horizontal position of the overlapped wafer T before grinding. The position detector 320 irradiates light onto the outer periphery of the lower wafer S held by the chuck 300 and has a sensor that receives the light. Alternatively, the position detector 320 may have a sensor that captures an image of the outer periphery of the lower wafer S. Then, while rotating the overlapped wafer T held by the chuck 300, the position detector 320 detects the position of the notch of the lower wafer S and further detects the position (eccentricity) of the center of the overlapped wafer T (upper wafer W). The detection result of the position detector 320 is output to the control device 110. Then, based on this detection result, the horizontal orientation of the overlapped wafer T is adjusted (θ alignment) and the horizontal position is adjusted (XY alignment). Note that, although the position of the notch of the lower wafer S is detected in this embodiment, the present invention is not limited to this. For example, the position of the orientation flat of the lower wafer S may be detected, and the horizontal orientation and position of the overlapped wafer T may be adjusted.
[0047] An overall thickness measuring unit 330 is provided above and below the chuck 300. The overall thickness measuring unit 330 measures the overall thickness Ht of the overlapped wafer T shown in FIG. 4. The overall thickness Ht of the overlapped wafer T measured by the overall thickness measuring unit 330 is output to the control device 110.
[0048] As shown in FIGS. 6 to 8, the total thickness measuring unit 330 includes an upper sensor 331, a lower sensor 332, and a calculation unit (not shown). The upper sensor 331 is disposed above the overlapped wafer T held by the chuck 300, and measures the distance from the upper sensor 331 to the back surface Wb of the upper wafer W. The lower sensor 332 is disposed below the overlapped wafer T held by the chuck 300, and measures the distance from the lower sensor 332 to the back surface Sb of the lower wafer S. The upper sensor 331 and the lower sensor 332 are disposed opposite to each other on the same coordinate axis, and the measurement point of the upper sensor 331 and the measurement point of the lower sensor 332 are at the same position in a plan view. In the total thickness measuring unit 330, the calculation unit derives the total thickness Ht of the overlapped wafer T based on the distance between the upper sensor 331 and the back surface Wb of the upper wafer W and the distance between the lower sensor 332 and the back surface Sb of the lower wafer S. Any known sensor that measures distance may be used for the upper sensor 331 and the lower sensor 332. For example, a confocal sensor is used. A calculation unit (not shown) may be provided inside the first thickness measurement device 52 or outside the first thickness measurement device 52.
[0049] The upper sensor 331 and the lower sensor 332 each move relative to the chuck 300 as the chuck 300 moves in the horizontal direction. The lower sensor 332 is configured to be able to move forward and backward relative to the cutout portion 301. That is, as the chuck 300 moves in the horizontal direction, the lower sensor 332 moves forward and backward from the cutout portion 301. The total thickness measuring unit 330 can measure the total thickness Ht of the overlapped wafer T at a plurality of points.
[0050] The upper sensor 331 and the lower sensor 332 are positioned so that when the overlapped wafer T is rotated in detecting the horizontal position by the position detection unit 320 described above, the lower sensor 332 does not interfere with the cutout portion 301, i.e., on the positive Y-axis side of the position detection unit 320.
[0051] A partial thickness measuring section 340 is further provided above the chuck 300 as a first measuring section. The partial thickness measuring section 340 measures the thickness Hw of the upper wafer W shown in FIG. 4. The partial thickness measuring section 340 measures the thickness of the upper wafer W without contacting the upper wafer W. The thickness Hw of the upper wafer W measured by the partial thickness measuring section 340 is output to the control device 110. The control device 110 calculates the thickness Hs of the parts other than the upper wafer W by subtracting the thickness Hw of the upper wafer W from the total thickness Ht of the overlapped wafer T measured by the total thickness measuring section 330. This thickness Hs includes the thickness of the lower wafer S, the thickness of the device layers Dw, Ds, and the thickness of the surface films Fw, Fs, but may be referred to as the thickness Hs of the lower wafer S for simplicity in the following description.
[0052] The calculated thickness Hs of the lower wafer S is output to the control device 110. Then, based on the thickness Hs of the lower wafer S, the relative angle (parallelism) of the surface of the chuck 72 with respect to the surface of the grinding wheel in the processing device 70 is adjusted.
[0053] As shown in FIGS. 6 to 8, the partial thickness measuring unit 340 has a sensor 341 and a calculation unit (not shown). The sensor 341 irradiates the upper wafer W with light, and receives the reflected light reflected from the front surface Wa and the back surface Wb of the upper wafer W. In the partial thickness measuring unit 340, the calculation unit measures the thickness Hw of the upper wafer W based on both reflected lights. The sensor 341 is disposed at the same position as the position detection unit 320 in the Y-axis direction. The sensor 341 can be any known sensor that measures thickness, and may be, for example, a spectroscopic interference sensor. The calculation unit (not shown) may be provided inside the first thickness measuring device 52 or outside the first thickness measuring device 52.
[0054] As the chuck 300 moves in the horizontal direction, the sensor 341 moves relatively to the chuck 300. The partial thickness measuring unit 340 can measure the thickness Hw of the upper wafer W at a plurality of points.
[0055] The total thickness measuring unit 330 and the partial thickness measuring unit 340 each measure the total thickness Ht of the overlapped wafer T and the thickness Hw of the upper wafer W at the same measurement point in a plan view. That is, as shown in Fig. 9, the total thickness measuring unit 330 and the partial thickness measuring unit 340 each measure the total thickness Ht of the overlapped wafer T and the thickness Hw of the upper wafer W at, for example, three points in the radial direction. Measurement point P1 is the center of the upper wafer W. Measurement point P2 is the middle part of the upper wafer W, and is located at a position R / 2 from the center, where R is the radius of the upper wafer W. Measurement point P3 is the outer periphery of the upper wafer W.
[0056] 10(a), when measuring the total thickness Ht at the measurement point P1 by the total thickness measuring unit 330, the total thickness Ht of the overlapped wafer T is measured with the rotation of the chuck 300 (overlapping wafer T) stopped. At this time, the lower sensor 332 enters the cutout portion 301. Therefore, in order to avoid interference between the lower sensor 332 and the chuck 300, the chuck 300 is not rotated. On the other hand, as shown in FIG. 11(a), when the partial thickness measuring unit 340 measures the thickness Hw of the upper wafer W at the measurement point P1, since there is no interference between the sensor 341 and the chuck 300, the chuck 300 (superimposed wafer T) may be rotated or may be stopped from rotating.
[0057] 10(b), when measuring the total thickness Ht at measurement point P2 by total thickness measuring unit 330, the total thickness Ht of overlapped wafer T is measured at multiple points in the circumferential direction while rotating chuck 300. At this time, since the diameter of chuck 300 is half or less of the diameter of overlapped wafer T and lower sensor 332 is retracted from cutout portion 301, even if chuck 300 is rotated, lower sensor 332 and chuck 300 do not interfere with each other. Also, as shown in FIG. 11(b), when the partial thickness measuring unit 340 measures the thickness Hw of the upper wafer W at the measurement point P2, the thickness Hw of the upper wafer W is measured at multiple points in the circumferential direction while rotating the chuck 300. Then, at the measurement point P2, a moving average value of the measured multiple points in the circumferential direction is calculated and set as the total thickness Ht of the overlapped wafer T or the thickness Hw of the upper wafer W at the measurement point P2. The measured thickness at the measurement point P2 may be a moving median value of the measured multiple points in the circumferential direction.
[0058] As shown in FIGS. 10(c) and 11(c), the total thickness Ht of the overlapping wafer T and the thickness Hw of the upper wafer W are also measured at the measurement point P3 in the same manner as at the measurement point P2.
[0059] In this embodiment, the moving average or moving median of multiple points in the circumferential direction is used as the measured thickness at the measurement points P2 and P3, but thickness measurement may be performed at, for example, designated coordinates. For example, at the measurement points P2 and P3, the total thickness Ht of the overlapped wafer T or the thickness Hw of the upper wafer W is measured with the rotation of the overlapped wafer T stopped. Then, at the measurement points P2 and P3, the total thickness Ht or the thickness Hw of the upper wafer W is measured at one point in the circumferential direction. Then, the thickness measured at such designated coordinates may be used as the thickness of the measurement points P2 and P3 as a representative point.
[0060] In this embodiment, the measurement result of the thickness Hw of the upper wafer W is used to adjust the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 as described later, but the use is not limited to this. For example, the thickness Hw of the upper wafer W may be measured at a specified measurement point in order to grasp the tendency of the thickness Hw of the upper wafer W.
[0061] In the first thickness measuring device 52 of the present embodiment, the chuck 300 moves in the horizontal direction (Y-axis direction), and the upper sensor 331 and the lower sensor 332 of the total thickness measuring unit 330 and the sensor 341 of the partial thickness measuring unit 340 are fixed, but the chuck 300 and the total thickness measuring unit 330 or the partial thickness measuring unit 340 may move relatively in the horizontal direction. For example, the chuck 300 may be fixed, and the upper sensor 331 and the lower sensor 332, or the sensor 341 may move in the horizontal direction. Alternatively, the chuck 300 may move in the horizontal direction, and further the upper sensor 331 and the lower sensor 332, or the sensor 341 may also move in the horizontal direction.
[0062] 6, a first shutter 350 is provided on a side wall surface on the negative X-axis direction side of first thickness measurement device 52. First shutter 350 is configured so that a first transfer port can be opened and closed by a drive mechanism 351. When first shutter 350 is opened, first thickness measurement device 52 communicates with the inside of first processing block G1, and the wafer transfer device 40 transfers the overlapped wafer T in and out.
[0063] A second shutter 360 is provided on a side wall surface on the negative Y-axis direction side of first thickness measurement device 52. Second shutter 360 is configured so that a second transfer port can be opened and closed by a drive mechanism 361. When second shutter 360 is opened, first thickness measurement device 52 and the inside of second processing block G2 communicate with each other, and the wafer transfer device 60 transfers the overlapped wafer T in and out.
[0064] An exhaust unit 370 is connected to the lower part of the first thickness measurement device 52. The exhaust unit 370 has an exhaust path 371 provided below a driving part such as the rail 312, and an exhaust mechanism 372 such as a vacuum pump connected to the exhaust path 371. The exhaust unit 370 exhausts particles and the like generated by driving such as the rotation and movement of the chuck 300 to the outside of the first thickness measurement device 52 by the operation of the exhaust mechanism 372.
[0065] Further, the exhaust unit 370 is configured to be able to exhaust (reducing pressure) the processing space of the first thickness measurement device 52. The internal pressure of the first thickness measurement device 52 is controlled to be kept lower than the internal pressure of the first processing block G1 and higher than the internal pressure of the second processing block G2. In other words, in the first thickness measurement device 52, an airflow flows in from the first processing block G1 when the first shutter 350 is opened, and an airflow flows out to the second processing block G2 when the second shutter 360 is opened. This prevents particles and the like generated by the grinding process in the processing device 70 from flowing into the inside of the first thickness measurement device 52, as shown in FIG. 12, and prevents particles and the like from flowing out to the first processing block G1 (cassette C) side, which is a clean space.
[0066] Specifically, for example, as shown in Fig. 12(a), when the first shutter 350 and the second shutter 360 are closed, no airflow flows out from the first thickness measurement device 52, and the airflow is exhausted only from the exhaust section 370. Even when the first shutter 350 is thus closed, as shown in Fig. 12(a), a small amount of airflow flows in from the first processing block G1, which is a clean space, through a small gap formed on the first shutter 350 side. Furthermore, as shown in FIG. 12(b), when the first shutter 350 is opened, the airflow is discharged only from the exhaust section 370. Furthermore, as shown in FIG. 12(c), when the second shutter 360 is opened, no airflow flows in from the second shutter 360 side into the first thickness measuring device 52, and no airflow flows out from the first shutter 350 side to the outside of the first thickness measuring device 52.
[0067] In this way, airflow flows into the first thickness measurement device 52 only from the first shutter 350 (first processing block G1) side, and airflow does not flow into the first thickness measurement device 52 from the second shutter 360 (processing device 70) side. That is, the inflow of particles and the like from the processing device 70 is suppressed. Moreover, airflow from first thickness measuring device 52 flows out only from second shutter 360 (processing device 70) side and exhaust section 370, and does not flow out to first shutter 350 (first processing block G1) side. That is, particles and the like are prevented from flowing out into first processing block G1, which is a clean space. 12, in the first thickness measurement device 52, the first shutter 350 and the second shutter 360 are not opened simultaneously. This further prevents particles and the like from flowing out from the processing device 70 to the first processing block G1.
[0068] Next, a detailed configuration of the second thickness measurement device 53 will be described. In the second thickness measurement device 53, elements having substantially the same functional configuration as those of the first thickness measurement device 52 are denoted by the same reference numerals and will not be described again.
[0069] 13 and 14, the second thickness measurement device 53 has a chuck 400 as a second substrate holding unit that holds the overlapped wafer T. The chuck 400 suction-holds a central portion of the back surface Sb of the lower wafer S of the overlapped wafer T. The diameter of the chuck 400 is larger than the diameter of the chuck 300 included in the first thickness measurement device 52, for example, and may be half or more of the diameter of the overlapped wafer T.
[0070] The second thickness measuring device 53 measures the thickness Hw of the upper wafer W after grinding, in other words, the thickness Hw that is smaller than the thickness Hw of the upper wafer W before grinding in the first thickness measuring device 52. Thus, by suction-holding the overlapped wafer T with the chuck 400 having a larger diameter than the chuck 300 in this manner, warping of the overlapped wafer T thinned by grinding is suppressed.
[0071] The chuck 400 is configured to be rotatable about a vertical axis by the rotation mechanism 310 and to be movable in the horizontal direction along the rail 312. Positive directionA position detection unit 320 as a second position detection unit is provided on the upper wafer W (on the upper side) to adjust the horizontal orientation and position of the laminated wafer T after grinding, and detect the position (amount of eccentricity) of the center of the upper wafer W. In this embodiment, the rotation mechanism 310 and the movement mechanism 313 that drive the chuck 400 constitute a "second drive unit" according to the technology of the present disclosure.
[0072] A partial thickness measuring unit 440 is provided above the chuck 400 as a second measuring unit for measuring the thickness Hw of the upper wafer W after grinding. The partial thickness measuring unit 440 measures the thickness of the upper wafer W without contacting the upper wafer W. As described above, the second thickness measuring device 53 measures the thickness Hw of the upper wafer W after grinding, in other words, a thickness Hw smaller than the thickness Hw of the upper wafer W before grinding in the first thickness measuring device 52. For this reason, the partial thickness measuring unit 440 is provided with a sensor 441 capable of measuring a thickness smaller than that of the partial thickness measuring unit 340 included in the first thickness measuring device 52.
[0073] The thickness Hw of the upper wafer W measured by the partial thickness measuring unit 440 is output to the control device 110. Then, based on the thickness Hw of the upper wafer W, the relative angle (parallelism) of the surface of the chuck 72 with respect to the surface of the grinding wheel is adjusted during grinding processing of the overlapped wafer T to be subsequently processed in the wafer processing system 1.
[0074] The partial thickness measuring unit 440 measures the thickness Hw of the upper wafer W at the same measurement points as the entire thickness measuring unit 330 and the partial thickness measuring unit 340 in the first thickness measuring device 52 in a plan view. That is, the partial thickness measuring unit 440 measures the thickness Hw of the upper wafer W at, for example, three points in the radial direction shown in Fig. 9. Note that the method of measuring the thickness Hw of the upper wafer W by the partial thickness measuring unit 440 is similar to the method of measuring the thickness Hw of the upper wafer W by the partial thickness measuring unit 340 shown in Fig. 11.
[0075] In addition, in the second thickness measuring device 53, as in the first thickness measuring device 52, when measuring the thickness at measurement points P2 and P3, instead of calculating a moving average or moving median of multiple points in the circumferential direction, the thickness measured at a specified coordinate may be used as a representative point and used as the thickness of measurement points P2 and P3.
[0076] In this embodiment, the measurement result of the thickness Hw of the upper wafer W is used to adjust the relative angle of the surface of the chuck 72 with respect to the surface of the grinding wheel during the grinding process of the overlapped wafer T to be subsequently processed, but the use is not limited to this. For example, the thickness Hw of the upper wafer W may be measured at a specified measurement point in order to grasp the tendency of the thickness Hw of the upper wafer W.
[0077] As described above, the second thickness measurement device 53 does not measure the total thickness Ht of the laminated wafer T. Therefore, the second thickness measurement device 53 is not provided with the total thickness measurement unit 330 as in the first thickness measurement device 52. Furthermore, since the second thickness measurement device 53 is not provided with the total thickness measurement unit 330 (lower sensor 332) as described above, the chuck 400 is not formed with a notch for inserting the lower sensor 332.
[0078] 13, a first shutter 350 is provided on a side wall surface on the negative X-axis direction side of second thickness measurement device 53. First shutter 350 is configured so that a first transfer port can be opened and closed by a drive mechanism 351. When first shutter 350 is opened, second thickness measurement device 53 and the inside of first processing block G1 communicate with each other, and the wafer transfer device 40 transfers the overlapped wafer T in and out.
[0079] As described above, in the second thickness measurement device 53, the overlapped wafer T is not loaded / unloaded by the wafer transport device 60 in the second processing block G2, but is loaded / unloaded only by the wafer transport device 40 in the first processing block G1. For this reason, the second thickness measurement device 53 does not have a second transport port on the second processing block G2 side, that is, the second shutter 360 is not provided. As described above, the second thickness measurement device 53 measures the thickness Hw of the overlapped wafer T (upper wafer W) after grinding, but by omitting the second shutter 360 on the second processing block G2 side and loading / unloading the overlapped wafer T only by the wafer transport device 40, particles generated by the grinding process in the processing device 70 are prevented from flowing into the second thickness measurement device 53.
[0080] Further, an exhaust unit 370 is provided below the second thickness measurement device 53. This allows particles and the like generated by, for example, the rotation or horizontal movement of the chuck 400 to be exhausted to the outside of the second thickness measurement device 53, and also allows the internal pressure of the second thickness measurement device 53 to be reduced. The internal pressure of the second thickness measurement device 53 is controlled so as to be kept lower than the internal pressure of the first processing block G1, for example.
[0081] The first thickness measuring device 52 and the second thickness measuring device 53 according to this embodiment are configured as described above. Next, a description will be given of wafer processing performed using the wafer processing system 1 configured as described above. In this embodiment, the upper wafer W and the lower wafer S are bonded in a bonding device (not shown) provided outside the wafer processing system 1 to form an overlapped wafer T in advance.
[0082] First, a cassette C storing a plurality of overlapped wafers T is placed on the cassette placement stage 10 of the carry-in / out station 2. Next, the overlapped wafers T are removed from the cassette C by the wafer transfer device 40 and transferred to the first cleaning device 50. In the first cleaning device 50, a cleaning liquid is supplied to the back surface Wb of the upper wafer W while rotating the overlapped wafer T, and the back surface Wb is spin-cleaned. Also, a cleaning liquid is supplied while a cleaning brush (not shown) is in contact with the back surface Sb of the lower wafer S, and the back surface Sb is scrubbed (step E1 in FIG. 15).
[0083] Next, the first shutter 350 of the first thickness measurement device 52 is opened, and the overlapped wafer T is transported to the first thickness measurement device 52 by the wafer transport device 40. At this time, since the internal pressure of the first thickness measurement device 52 is controlled to be lower than the internal pressure of the first processing block G1, the first processing block G1, which is a clean space, is prevented from being contaminated by opening the first shutter 350. In the first thickness measurement device 52, first, the overlapped wafer T is adsorbed and held by the chuck 300 at the load / unload position (home position).
[0084] Next, the chuck 300 is moved to the alignment position as shown in Fig. 16(a). Then, while rotating the overlapped wafer T as shown in Fig. 16(b), the position detector 320 detects the horizontal position of the overlapped wafer T and further detects the position (amount of eccentricity) of the center of the upper wafer W. Based on the detection result, the horizontal orientation of the overlapped wafer T is adjusted (θ alignment), and the horizontal position is also adjusted (XY alignment) (step E2 in Fig. 15).
[0085] At the alignment position, the thickness Hw of the upper wafer W before grinding is measured by the partial thickness measuring unit 340 using the method shown in FIG. 11 (step E3 in FIG. 15). That is, first, the thickness Hw at the center (measurement point P1) of the upper wafer W is measured. When measuring the thickness Hw of the upper wafer W at the measurement point P1, the chuck 300 (overlapped wafer T) may be rotated or may be stopped from rotating. Moreover, the measurement of the thickness Hw of the upper wafer W at the measurement point P1 may be performed simultaneously with the detection of the horizontal position of the overlapped wafer T (step E2). The thickness Hw of the upper wafer W measured in this manner (distribution of thickness Hw) is output to the control device 110.
[0086] 16(c), the chuck 300 is sequentially moved and rotated in the negative Y-axis direction to measure the thickness Hw at multiple points (measurement points P2, P3) in the radial direction of the upper wafer W. When measuring the thickness Hw of the upper wafer W at the measurement points P2, P3, the thickness Hw of the upper wafer W is measured at multiple points in the circumferential direction while rotating the chuck 300, and a moving average or moving median of the measured multiple points in the circumferential direction is calculated.
[0087] 16(d), the chuck 300 is moved toward the total thickness measuring unit 330, and the total thickness Ht of the overlapped wafer T is measured by the method shown in FIG. 10 (step E4 in FIG. 15). That is, first, the total thickness Ht is measured at the center (measurement point P1) of the overlapped wafer T. At the measurement point P1, the lower sensor 332 has entered the cutout portion 301, and therefore, with the rotation of the overlapped wafer T stopped, the total thickness Ht of the overlapped wafer T at the measurement point P1 is measured by the total thickness measuring unit 330.
[0088] Next, as shown in FIG. 16(e), the Y axis of the chuck 300 negative directionThe chuck 300 is moved and rotated sideways in sequence to measure the total thickness Ht at multiple points (measurement points P2, P3) in the radial direction of the overlapped wafer T. When measuring the total thickness Ht of the overlapped wafer T at measurement points P2 and P3, the total thickness Ht of the overlapped wafer T is measured at multiple points in the circumferential direction while rotating the chuck 300, and a moving average or moving median of the measured multiple points in the circumferential direction is calculated. The total thickness Ht of the overlapped wafer T measured in this manner (distribution of the total thickness Ht) is output to the control device 110.
[0089] After the alignment in step E2 and the thickness measurements in steps E3 and E4 are completed as described above, the chuck 300 is moved to the carry-in / out position as shown in Fig. 16(f). At this time, the chuck 300 is rotated to align the horizontal position of the upper wafer W measured in step E2 to a desired position.
[0090] The control device 110 calculates the thickness Hs of the lower wafer S by subtracting the thickness Hw of the upper wafer W measured in step E3 from the thickness Ht of the overlapped wafer T measured in step E4 (step E5 in FIG. 15). As described above, this thickness Hs includes the thickness of the lower wafer S, the thicknesses of the device layers Dw, Ds, and the thicknesses of the surface films Fw, Fs. The thickness Hs of the lower wafer S is calculated at each of the measurement points P1, P2, and P3, thereby obtaining the distribution of the thickness Hs of the lower wafer S.
[0091] Furthermore, the control device 110 controls the tilt adjustment unit 74 at the processing position A3 of the processing device 70 based on the distribution of the thickness Hs of the lower wafer S calculated in step E5. Specifically, based on the distribution of the thickness Hs of the lower wafer S, the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 is adjusted so that the in-plane thickness of the upper wafer W bonded to the lower wafer S after finish grinding becomes uniform (step E6 in FIG. 15). In the following description, this adjustment of the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 may be referred to as tilt correction.
[0092] Next, the second shutter 360 of the first thickness measurement device 52 is opened, and the laminated wafer T is transported by the wafer transport device 60 to the processing device 70 and delivered to the chuck 72 at the delivery position A0. At this time, since the internal pressure of the first thickness measurement device 52 is controlled to be higher than the internal pressure of the second processing block G2, the intrusion of particles and the like from the processing device 70 into the first thickness measurement device 52 is suppressed.
[0093] Next, the rotary table 71 is rotated to move the overlapped wafer T to the processing position A1. Then, the back surface Wb of the upper wafer W is roughly ground by the rough grinding unit 80 (step E7 in FIG. 15). At this time, the upper wafer W is ground to a desired thickness while measuring the total thickness Ht of the overlapped wafer T using a contact-type thickness measuring device (not shown).
[0094] Next, the turntable 71 is rotated to move the overlapped wafer T to the processing position A2. Then, the intermediate grinding unit 90 performs intermediate grinding on the back surface Wb of the upper wafer W (step E8 in FIG. 15). At this time, the upper wafer W is ground while measuring the total thickness Ht of the overlapped wafer T using a contact-type thickness gauge (not shown), and then the upper wafer W is ground while measuring the thickness Hw of the upper wafer W using a non-contact-type thickness gauge (not shown).
[0095] Next, the rotary table 71 is rotated to move the overlapped wafer T to the processing position A3. Then, the finish grinding unit 100 finish-grinds the back surface Wb of the upper wafer W (step E9 in FIG. 15). In this finish grinding, the chuck 72 and the finish grinding wheel 101, which have been subjected to tilt correction in step E6, are used. At this time, the upper wafer W is ground to a desired thickness while measuring the thickness Hw of the upper wafer W using a non-contact thickness measuring device (not shown).
[0096] Next, the rotary table 71 is rotated to move the overlapped wafer T to the transfer position A0. At the transfer position A0, the back surface Wb of the upper wafer W after grinding may be cleaned by a cleaning unit (not shown).
[0097] After the processing in the processing apparatus 70, the overlapped wafer T is then transferred by the wafer transfer apparatus 60 to the second cleaning apparatus 51. In the second cleaning apparatus 51, cleaning similar to that in step E1 is performed. That is, while rotating the overlapped wafer T, a cleaning liquid is supplied to the back surface Wb of the upper wafer W to spin-clean the back surface Wb, and a cleaning brush (not shown) is brought into contact with the back surface Sb of the lower wafer S to supply a cleaning liquid to scrub-clean the back surface Sb (step E10 in FIG. 15).
[0098] Next, the first shutter 350 of the second thickness measurement device 53 is opened, and the overlapped wafer T is transported to the second thickness measurement device 53 by the wafer transport device 40. At this time, since the internal pressure of the second thickness measurement device 53 is controlled to be lower than the internal pressure of the first processing block G1, the first processing block G1, which is a clean space, is prevented from being contaminated by opening the first shutter 350. In the second thickness measurement device 53, first, the overlapped wafer T is adsorbed and held by the chuck 400 at the load / unload position (home position).
[0099] Next, the chuck 400 is moved to the alignment position as shown in Fig. 17(a). Then, while rotating the overlapped wafer T as shown in Fig. 17(b), the position detector 320 detects the horizontal position of the overlapped wafer T and further detects the position (amount of eccentricity) of the center of the upper wafer W. Based on the detection result, the horizontal orientation of the overlapped wafer T is adjusted (θ alignment), and the horizontal position is also adjusted (XY alignment) (step E11 in Fig. 15).
[0100] At the alignment position, the thickness Hw of the upper wafer W after grinding is measured by the partial thickness measuring unit 440 using the method shown in FIG. 11 (step E12 in FIG. 15). That is, first, the thickness Hw at the center (measurement point P1) of the upper wafer W is measured. When measuring the thickness Hw of the upper wafer W at the measurement point P1, the chuck 400 (overlapping wafer T) may be rotated or may be stopped from rotating. Note that the measurement of the thickness Hw of the upper wafer W at the measurement point P1 may be performed simultaneously with the detection of the horizontal position of the overlapping wafer T (step E11).
[0101] 17(c), the chuck 400 is sequentially moved and rotated in the negative Y-axis direction to measure the thickness Hw at multiple points (measurement points P2, P3) in the radial direction of the upper wafer W. When measuring the thickness Hw of the upper wafer W at the measurement points P2 and P3, the thickness Hw of the upper wafer W is measured at multiple points in the circumferential direction while rotating the chuck 400, and a moving average or moving median of the measured multiple points in the circumferential direction is calculated. The thickness Hw of the upper wafer W measured in this manner (distribution of thickness Hw) is output to the control device 110.
[0102] When the alignment in step E11 and the measurement of the thickness Hw of the upper wafer W in step E12 are completed as described above, the chuck 400 is moved to the carry-in / out position as shown in Fig. 17(d). At this time, the chuck 400 is rotated to align the horizontal position of the overlapped wafer T measured in step E11 to a desired position.
[0103] The control device 110 controls the inclination adjustment unit 74 at the processing position A3 of the processing device 70 based on the distribution of the thickness Hw of the upper wafer W measured in step E12. Specifically, based on the distribution of the thickness Hw of the upper wafer W after grinding, the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 is adjusted so that the in-plane thickness of the upper wafer W to be processed next after finish grinding becomes uniform (step E13 in FIG. 15). That is, in step E13, after steps E1 to E12 are performed on the nth (n is an integer equal to or greater than 1) overlapped wafer T, the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 is adjusted at the processing position A3 in order to grind the n+1th overlapped wafer T (upper wafer W).
[0104] Next, the second thickness measuring device 53 First shutter 350 The upper wafer W is opened, and the overlapped wafer T is transported by the wafer transport device 40 to the etching processing device 30. In the etching processing device 30, a wet etching process (cleaning process) is performed on the back surface Wb of the upper wafer W and the back surface Sb of the lower wafer S (Step E14 in FIG. 15).
[0105] Thereafter, the laminated wafer T on which all the processes have been performed is transferred by the wafer transfer device 40 to the cassette C on the cassette mounting table 10. In this manner, a series of wafer processes in the wafer processing system 1 is completed.
[0106] In the wafer processing system 1, the processing for the n-th overlapped wafer T and the processing for the n+1-th overlapped wafer T may be performed in parallel. In such a case, steps E1 to E12 are performed for the n-th overlapped wafer T, and tilt correction for grinding the n+1-th upper wafer W is performed in step E13. On the other hand, steps E1 to E5 are performed for the n+1-th overlapped wafer T, and tilt correction for grinding the n+1-th upper wafer W is performed in step E6. In this way, in step E13 for the n-th wafer and step E6 for the n+1-th wafer, tilt correction for grinding the same n+1-th upper wafer W is performed. Therefore, in such a case, the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 at the processing position A3 is adjusted based on the thickness Hw of the n-th upper wafer W measured in step E12 and the thickness Hs of the n+1-th lower wafer S calculated in step E5.
[0107] According to the above embodiment, the thickness Hw of the upper wafer W before and after grinding in the processing apparatus 70 is measured by the first thickness measuring device 52 and the second thickness measuring device 53 that are provided independently outside the processing apparatus 70. Therefore, in this embodiment, the wafer processing time in the processing apparatus 70 can be shortened compared to the conventional case where thickness measurement is performed in the processing apparatus 70. As a result, the throughput of the wafer processing can be improved.
[0108] In addition, since the first thickness measuring device 52 and the second thickness measuring device 53 are provided independently of the other processing devices in the wafer processing system 1, Wafer Processing System 1 The wafer processing time in other processing apparatuses (for example, the first cleaning apparatus 50 and the second cleaning apparatus 51) in the wafer processing system is not affected, and the wafer processing throughput can be further improved.
[0109] Furthermore, in this embodiment, the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 is adjusted in step E13 based on the thickness Hw of the upper wafer W measured in step E12, so that the in-plane thickness of the upper wafer W to be processed next after finish grinding can be made uniform.
[0110] In this embodiment, the measurement of the thickness Hw of the upper wafer W before grinding in step E3 and the measurement of the total thickness Ht of the overlapped wafer T before grinding in step E4 are performed by the first thickness measuring device 52. Since the two thickness measurements before grinding are performed in the same device in this manner, the wafer processing time in the wafer processing system 1 can be further shortened and the throughput can be further improved.
[0111] Furthermore, in this embodiment, the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 is adjusted in step E6 based on the thickness Hs of the lower wafer S calculated in step E5, so that the in-plane thickness of the upper wafer W after finish grinding can be made uniform.
[0112] In this embodiment, the measurement of the thickness Hw in step E3, the measurement of the total thickness Ht in step E4, and the measurement of the thickness Hw in step E12 are performed at the same measurement points P1, P2, and P3, respectively. Therefore, the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 can be appropriately determined.
[0113] In this embodiment, the position detection unit 320 and the sensors 341, 441 of the partial thickness measurement units 340, 440 are provided at the same positions in the Y-axis direction (the driving direction of the chucks 300, 400) in the first thickness measurement device 52 and the second thickness measurement device 53. This allows the position detection unit 320 to detect the horizontal position and the partial thickness measurement units 340, 440 to measure the thickness Hw at the center of the upper wafer W at the same positions, thereby shortening the wafer processing time in the first thickness measurement device 52 and the second thickness measurement device 53.
[0114] In this embodiment, the internal pressures of the first to third processing blocks G1 to G3 in the wafer processing system 1 are controlled to be higher in this order, and the internal pressure of the first thickness measuring device 52 is controlled to be lower than the internal pressure of the first processing block G1 and higher than the internal pressure of the third processing block G3. In other words, in the wafer processing system 1, an air flow is formed that flows sequentially from the first processing block G1 through the first thickness measuring device 52 to the second, third processing blocks G2, and G3. This prevents particles and the like generated in the processing device 70 of the third processing block G3 from flowing into the first processing block G1 and the first thickness measuring device 52, which are clean spaces, and thus prevents the overlapped wafer T that has been subjected to a series of processes in the wafer processing system 1 from being contaminated.
[0115] Furthermore, in this embodiment, the first shutter 350 and the second shutter 360 of the first thickness measurement device 52 are not opened simultaneously during a series of wafer processing. In other words, the first processing block G1 and the second processing block G2 are not directly connected to each other during alignment and thickness measurement of the overlapped wafer T, which further prevents particles and the like from flowing into the first processing block G1.
[0116] In this embodiment, the overlapped wafer T is not transported by the wafer transport device 60 to the second thickness measuring device 53 that measures the thickness of the upper wafer W after grinding in the processing device 70, and no second shutter 360 is provided. As a result, the second processing block G2 that communicates with the processing device 70 does not communicate with the second thickness measuring device 53, which further prevents contamination of the overlapped wafer T that has been subjected to a series of processes.
[0117] In the above embodiment, as shown in steps E1 and E10 of FIG. 15, the overlapped wafer T is cleaned prior to alignment of the overlapped wafer T. However, this cleaning of the overlapped wafer T may be omitted as appropriate.
[0118] 15, alignment of the overlapped wafer T after the grinding process is performed in the second thickness measurement device 53. However, for example, when no deviation occurs in the horizontal position of the overlapped wafer T during the grinding process (steps E7 to E9) or when the overlapped wafer T is transported, such alignment of the overlapped wafer T may be omitted.
[0119] 15, the overlapped wafer T is cleaned prior to alignment of the overlapped wafer T, but the order of cleaning and alignment of the overlapped wafer T may be reversed. In such a case, alignment of the overlapped wafer T may be performed inside the thickness measuring device, or an alignment device for aligning the overlapped wafer T may be further provided outside the thickness measuring device.
[0120] In addition, when the order of the cleaning (steps E1, E10) and alignment (steps E2, E11) of the overlapped wafer T is changed in this way, ,cormorant By the wafer transport device 60 Number The overlapped wafer T may be transportable to the first cleaning apparatus 50 and the second thickness measuring apparatus 53. In other words, the second thickness measuring apparatus 53 may be provided with a second shutter 360 for transferring the overlapped wafer T to and from the wafer transport apparatus 60.
[0121] In the above embodiment, the first thickness measuring device 52 and the second thickness measuring device 53 are provided with partial thickness measuring units 340, 440, respectively, and the first thickness measuring device 52 is provided with an overall thickness measuring unit 330, to collect information (thickness) necessary for tilt correction at the processing position A3, but information (thickness) used for purposes other than tilt correction may also be collected.
[0122] In the above embodiment, thickness measurements are performed at three radial points (measurement points P1, P2, and P3) of the overlapped wafer T (upper wafer W) in steps E3, E4, and E12, but the number of measurement points P may be four or more. The more measurement points there are, the more appropriately the distribution of the thickness Hw of the upper wafer W and the thickness Hs of the lower wafer S can be grasped, and as a result, the parallelism between the surface of the chuck 72 and the surface of the finish grinding wheel 101 can be appropriately adjusted in step E6.
[0123] The position of the measurement point of the thickness Hw of the upper wafer W is not limited to this embodiment. For example, when a position where unevenness occurs in the thickness Hw of the upper wafer W after grinding, i.e., a singular point, is known in advance, the singular point may be used as the measurement point of the thickness Hw. Also, for example, after the thickness measurement at the measurement points P1 to P3 in step E12, the thickness Hw of the upper wafer W at the singular point may be further measured.
[0124] Specifically, for example, when the thickness Hw of the upper wafer W at a singular point is measured in the second thickness measuring device 53, the chuck 400 (superimposed wafer T) is rotated and moved horizontally while the superimposed wafer T is held by the chuck 400, and the singular point is moved directly below the sensor 441 of the partial thickness measuring unit 440. As a result, the thickness Hw of the upper wafer W is measured by the partial thickness measuring unit 440. Note that, when multiple singular points occur within the surface of the upper wafer W, the thickness measurements at each singular point can be performed sequentially by repeatedly rotating and moving the chuck 400 (superimposed wafer T).
[0125] In addition, when the thickness Hw of the upper wafer W at the singular point is measured by the second thickness measuring device 53 in this manner, the installation position of the second thickness measuring device 53 is not limited to this embodiment. Since this measurement may be performed after the wet etching process in step E14, the second thickness measuring device 53 may be provided in, for example, the first processing block G1.
[0126] In the above embodiment, as shown in Figures 2 and 3, the wafer processing system 1 has a configuration in which the load / unload station 2 and the first to third processing blocks G1 to G3 are arranged in this order in the X-axis direction, but the configuration of the wafer processing system 1 is not limited to this.
[0127] 18, the first processing block G1 may be omitted. More specifically, the etching processing device 30 and the wafer transport device 40 may be omitted as in the wafer processing system 500, and the ground overlapped wafer T may be subjected to an etching process outside the wafer processing system 500. In this case, the second processing block G2 is provided with a wafer transport device 510 configured to transport the overlapped wafer T to the cassette C on the cassette mounting table 10, the first cleaning device 50, the second cleaning device 51, the first thickness measuring device 52, the second thickness measuring device 53, and the processing device 70.
[0128] In such a case, the wafer transport device 510 has, for example, a transport arm 41 that holds and transports the overlapped wafer T, and is capable of transferring the overlapped wafer T between the cassette C, and a transport arm 61 that has an adsorption holding surface (not shown) for the overlapped wafer T, and is capable of transferring the overlapped wafer T between the first cleaning device 50, the second cleaning device 51, the first thickness measuring device 52, the second thickness measuring device 53, and the processing device 70.
[0129] In the wafer processing system 500, the wafer transfer device 40 is omitted, and therefore the first cleaning device 50, the second cleaning device 51, the first thickness measuring device 52, and the second thickness measuring device 53 are not provided with a wafer transfer device. 510 In other words, in the wafer processing system 500, the first shutter 350 and the drive mechanism 351 on the side surface on the negative side of the X-axis are omitted in the first thickness measurement device 52 and the second thickness measurement device 53, and the second shutter 360 and the drive mechanism 361 on the side surface on the negative side of the Y-axis are provided.
[0130] Note that the wafer transfer device 510 may be provided with two transfer arms 61, one for transferring the overlapped wafer T before grinding and the other for transferring the overlapped wafer T after grinding.
[0131] The embodiments disclosed herein should be considered as illustrative and not restrictive in all respects. The above-described embodiments may be omitted, substituted, or modified in various forms without departing from the scope and spirit of the appended claims. [Explanation of symbols]
[0132] 1. Wafer Processing System 52 First thickness measuring device 53 Second thickness measuring device 70 Processing equipment Ht Overall thickness Hw (top wafer) thickness S Lower Wafer T Polymer Wafer W Upper wafer
Claims
1. A substrate processing system for processing a laminated substrate in which a first substrate and a second substrate are bonded together, comprising: a processing device that grinds the first substrate; a first thickness measuring device provided outside the processing apparatus and configured to measure a thickness of the first substrate before grinding and a total thickness of the laminated substrate including the first substrate; a second thickness measuring device provided outside the processing apparatus and configured to measure a thickness of the first substrate after grinding, the substrate processing system comprising:
2. The first thickness measuring device is a first substrate holding part for holding the laminated substrate; a first measuring unit that measures a thickness of the first substrate held by the first substrate holding unit; an overall thickness measuring unit that measures an overall thickness of the laminated substrate held by the first substrate holding unit, a notch portion is formed in the first substrate holding portion, the notch portion extending radially from a center portion to an outer end portion of the first substrate holding portion and allowing the total thickness measuring portion to relatively move forward and backward; The second thickness measuring device is a second substrate holding part for holding the laminated substrate; The substrate processing system according to claim 1 , further comprising: a second measuring unit configured to measure a thickness of the first substrate held by the second substrate holding unit.
3. The substrate processing system of claim 2 , wherein a diameter of the first substrate holding part is smaller than a diameter of the second substrate holding part.
4. The first thickness measuring device is A first drive unit that moves and rotates the first substrate holding unit in a horizontal direction; a first position detection unit that detects a horizontal position of the laminated substrate before grinding by the processing device; 4. The substrate processing system according to claim 2, wherein the first position detection unit is disposed at the same position as the first measurement unit in a moving direction of the first substrate holding unit.
5. The second thickness measuring device is A second drive unit that moves and rotates the second substrate holding unit in a horizontal direction; a second position detection unit that detects a horizontal position of the laminated substrate after grinding; 5. The substrate processing system according to claim 2, wherein the second position detection unit is disposed at the same position as the second measurement unit in a moving direction of the second substrate holding unit.
6. a first substrate transfer device that transfers the laminated substrate to a cassette that can accommodate a plurality of the laminated substrates; a second substrate transport device that transports the laminated substrate to the processing device, The first thickness measuring device includes: a first transfer opening through which the first substrate transfer device enters; a second transfer opening through which the second substrate transfer device enters is formed; The second thickness measuring device includes: a first transfer opening through which the first substrate transfer device enters is formed; 6. The substrate processing system according to claim 1, wherein a second transfer opening through which the second substrate transfer device enters is not formed.
7. a loading / unloading area in which a cassette capable of accommodating a plurality of the laminated substrates is placed; a processing area in which the first thickness measurement device and the second thickness measurement device are provided; A processing area in which the processing device is provided is formed, The substrate processing system according to any one of claims 1 to 6, further comprising a control device that controls the internal pressure of the loading / unloading region to be higher than the internal pressure of the processing region and to be higher than the internal pressure of the processing region.
8. The substrate processing system according to claim 7 , wherein the control device controls internal pressures of the first thickness measuring device and the second thickness measuring device to be lower than an internal pressure of the loading / unloading region and higher than an internal pressure of the processing region.
9. a first cleaning device that cleans the laminated substrate before it is ground by the processing device; a second cleaning device that cleans the laminated substrate after grinding by the processing device, 9. The substrate processing system according to claim 1, wherein the first cleaning device, the second cleaning device, the first thickness measuring device, and the second thickness measuring device are arranged in a stacked manner.
10. A substrate processing method for processing a laminated substrate in which a first substrate and a second substrate are bonded together in a substrate processing system, comprising: measuring a thickness of the first substrate before grinding with a first thickness measuring device; measuring an overall thickness of the laminated substrate before grinding with a first thickness measuring device; grinding the first substrate with a processing device; measuring the thickness of the first substrate after grinding with a second thickness measuring device; A substrate processing method, wherein the first thickness measuring device and the second thickness measuring device are provided outside the processing device.
11. Calculating a thickness of the second substrate based on a total thickness of the laminated substrate before grinding and a thickness of the first substrate before grinding; 11. The substrate processing method according to claim 10, further comprising: adjusting, prior to grinding the first substrate, a relative inclination between a holding surface of the laminated substrate of a third substrate holding portion in the processing apparatus and a grinding surface of a grinding wheel based on the calculated thickness of the second substrate.
12. In the substrate processing system, a plurality of laminated substrates are continuously processed, 12. The substrate processing method according to claim 10, further comprising the steps of: adjusting a relative inclination between a holding surface of the third substrate holding part of the processing apparatus for holding the laminated substrate and a grinding surface of a grinding wheel based on a thickness of the first substrate measured after grinding of one substrate prior to grinding of the first substrate in the laminated substrate to be processed next.
13. Detecting a horizontal position of the laminated substrate before grinding with a first thickness measuring device; 13. The substrate processing method according to claim 10, further comprising: detecting a horizontal position of the laminated substrate after grinding with a second thickness measuring device.
14. The first thickness measuring device and the second thickness measuring device measure the thickness of the first substrate at a plurality of points in a radial direction; The substrate processing method according to claim 13 , wherein the measurement of the thickness at the center of the first substrate is performed at the same position as the detection of the horizontal position.
15. The substrate processing system includes: a first substrate transfer device that transfers the laminated substrate to a cassette that can accommodate a plurality of the laminated substrates; a second substrate transport device that transports the laminated substrate to the processing device, The first substrate transport device and the second substrate transport device are inserted into the first thickness measuring device; The substrate processing method according to any one of claims 10 to 14, wherein only the first substrate transport device enters the second thickness measurement device, and the second substrate transport device does not enter the second thickness measurement device.
16. The substrate processing system includes: a loading / unloading area in which a cassette capable of accommodating a plurality of the laminated substrates is placed; a processing area in which the first thickness measurement device and the second thickness measurement device are provided; A processing area in which the processing device is provided is formed, The substrate processing method according to any one of claims 10 to 15, wherein the internal pressure of the loading / unloading region is controlled to be higher than the internal pressure of the processing region, and the internal pressure of the processing region is controlled to be higher than the internal pressure of the processing region.
17. The substrate processing method according to claim 16 , further comprising controlling an internal pressure of the first thickness measurement device and the second thickness measurement device to be lower than an internal pressure of the loading / unloading region and higher than an internal pressure of the processing region.
18. cleaning the laminated substrate before grinding in a first cleaning device prior to measuring the thickness of the first substrate with the first thickness measuring device; The substrate processing method according to any one of claims 10 to 17, further comprising: cleaning the ground laminated substrate in a second cleaning device prior to measuring the thickness of the first substrate with the second thickness measuring device.
Citation Information
Patent Citations
Grinding device
JP2008264913A
Method and apparatus for grinding, and control program for the apparatus
JP2009274139A
Polishing device and polishing method
JP2012033585A
Grinding method
JP2014226749A
Grinding device
JP2017056523A