Metal-resin composite molding and method for producing metal-resin composite molding
The metal-resin composite molded body with controlled grooves formed by stamping and coining processes addresses material escape issues, ensuring sealing integrity and adaptability to thermal expansion.
Patent Information
- Application Number
- JP2024109098
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-11-28
- Estimated Expiration
- 2044-07-05
AI Technical Summary
Existing methods for forming grooves in metal terminals during press molding risk material escape, leading to wall formation that compromises sealing performance.
A metal-resin composite molded body with grooves formed by stamping concave and convex portions, using molds with specific coining processes to control underfill and fillet formation, ensuring the grooves maintain sealing integrity.
The solution effectively maintains sealing performance by controlling material escape and fillet height, allowing the grooves to adapt to thermal expansion and contraction of the resin, preventing cross-sectional obstruction.
Smart Images

Figure 0007591332000001_ABST
Abstract
Description
[Technical field]
[0001] This specification discloses a metal-resin composite molded product and a method for producing the same.
[0002] Patent Document 1 discloses a metal resin composite molding. For example, a metal terminal serves as an insert part, and the metal resin composite molding is insert-molded.
[0003] Both ends of the metal terminal are exposed from the resin, and the middle part is embedded in the resin. One end of the metal terminal is connected to a substrate, for example. The other end of the metal terminal is placed in an environment exposed to liquid, such as the stator of a motor. In the embedded part of the metal terminal (i.e., the middle part), multiple grooves are formed along the longitudinal direction to provide sealing properties. The grooves are formed around the entire circumference of the metal terminal. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 5667652 Summary of the Invention [Problem to be solved by the invention]
[0005] However, when attempting to form a groove in a metal terminal by coining using a press molding machine, there is a risk of material loss occurring during the press process. This material loss forms a wall in the groove, blocking the entire cross section of the groove, making it difficult to maintain the sealing performance of the groove.
[0006] Therefore, this specification discloses a metal-resin composite molded product and a manufacturing method thereof that can maintain the sealing properties of a groove when the groove is formed in a metal terminal by coining. [Means for solving the problem]
[0007] This specification discloses a metal-resin composite molded product. The molded product includes a flat metal terminal and a resin part. The resin part exposes both ends of the metal terminal and embeds a middle portion of the metal terminal. A groove is formed in the middle portion of the metal terminal by forming recesses and protrusions all around the circumference by stamping, and a plurality of grooves are arranged along the longitudinal direction of the middle portion. The recesses are recessed from the non-coined surface of the middle portion. The protrusions protrude from the non-coined surface of the middle portion.
[0008] According to the above-mentioned configuration, the excess material generated when the recess is formed can be used to increase the height of the protrusion.
[0009] In the above configuration, the side surface of the groove formed by the recessed and protruding portions may extend perpendicularly to the non-coining surface.
[0010] According to the above-described configuration, when the resin filled in the recess undergoes thermal expansion and contraction, the interface between the resin and the metal terminal is sealed by the side surface and the resin.
[0011] In the above configuration, the protruding height of the protruding portion from the non-coining surface may be smaller than the recessed depth of the recessed portion from the non-coining surface.
[0012] According to the above-mentioned configuration, the amount of material lost to the protrusions can be reduced compared to the amount of material lost when the recesses are stamped. The material lost to the protrusions is densely packed to increase the height of the protrusions, so that the shape of the die in the protrusions is transferred to the material lost with high precision.
[0013] In the above configuration, the groove may be formed around the entire circumference of the metal terminal by a first groove portion and a second groove portion. The first groove portion is formed on both sides of the metal terminal in the thickness direction. The second groove portion is formed on both sides of the metal terminal in the width direction and is connected to the first groove portion. One of the first groove portion and the second groove portion is deeper than the other.
[0014] There is a risk that the coining process will cause material to escape into the groove, forming a plate-like portion. If one of the first groove portion and the second groove portion is coined and then the other is coined, a plate-like portion due to material escape may be formed in the one groove that was coined first. Therefore, the relatively deep groove is coined first, and then the relatively shallow groove is coined. At this time, a relatively small amount of material escapes into the relatively deep groove to form a plate-like portion. As a result, the entire cross section of the deep groove is prevented from being blocked by a relatively small amount of material escape.
[0015] In the above configuration, the first groove may be deeper than the second groove. In this case, the plate-shaped portion is disposed at the end of the first groove in the longitudinal direction with the bottom surface of the plate-shaped portion laid flat.
[0016] According to the above configuration, even if a plate-like portion is formed in the first groove portion of the deep groove, blocking of the first groove portion is suppressed by arranging the plate-like portion in a lying position.
[0017] In the above configuration, at least some of the grooves may be arranged at different pitches.
[0018] According to the above-mentioned configuration, it is possible to exhibit a sealing property in response to various modes of expansion and contraction of the resin part and the metal terminal.
[0019] This specification also discloses a method for manufacturing a metal resin composite molded body. The metal resin composite molded body includes a flat metal terminal and a resin part. The resin part exposes both ends of the metal terminal and embeds a middle portion of the metal terminal. In the method for manufacturing a metal resin composite molded body, a die having a concave-convex shape formed on the pressing surface is used to coin both thickness-wise and width-wise sides of the middle portion of the metal terminal. As a result, a groove is formed around the entire circumference of the middle portion. In addition, in the coining process, a position where the bottom surface of the recess on the pressing surface of the die is retracted from the non-coined surface of the middle portion of the metal terminal along the coining direction is set as the coining stop position.
[0020] According to the above-mentioned configuration, the excess material generated when the recess is formed can be used to increase the height of the protrusion.
[0021] In the above configuration, at the coining stop position, the distance between the bottom surface of the recess and the non-coining surface may be shorter than the distance between the non-coining surface and the top surface of the protrusion on the pressing surface.
[0022] According to the above-mentioned configuration, the amount of material lost to the protrusions can be reduced compared to the amount of material lost when the recesses are imprinted. The lost material is densely packed in the mold corresponding to the protrusions, so that the shape of the mold is transferred to the lost material with high accuracy.
[0023] In the above configuration, the mold may include a first mold, a second mold, and a third mold. The first mold forms an uneven shape on the pressing surface. The second mold and the third mold form uneven shapes with the same groove width and pitch as the first mold on the pressing surface. The coining process includes a first groove portion processing, a second groove portion processing, and a bending process. In the first groove portion processing, the first mold performs coining on both thickness direction sides of the middle part of the metal terminal to form a first groove portion in the middle part. In the second groove portion processing, after the first groove portion processing, the second mold performs coining on both width direction sides of the middle part of the metal terminal to form a second groove portion connected to the first groove portion in the middle part. In the bending process, after the second groove portion processing, the third mold folds the plate-shaped portion formed at the longitudinal end of the first groove portion so as to lie on the bottom surface of the first groove portion.
[0024] According to the above configuration, even if a plate-like portion is formed in the groove by the relief during groove processing, the plate-like portion is laid down in the groove by the bending process.
[0025] In the above configuration, the first mold may have deeper concave and convex grooves than the second mold.
[0026] According to the above configuration, by forming the plate-like portion in the groove of the metal terminal formed by the first mold, i.e., in a relatively deep groove, the cross section of the groove is prevented from being entirely blocked. Effect of the Invention
[0027] According to the metal-resin composite molded product and the manufacturing method thereof disclosed in this specification, when a groove is formed in a metal terminal by coining, the sealing properties of the groove can be maintained. [Brief description of the drawings]
[0028] [Figure 1] 1 is a perspective view illustrating a metal resin composite molded body according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a perspective view illustrating a metal terminal. [Diagram 3] FIG. 4 is a cross-sectional view illustrating the sealing effect of a groove. [Figure 4] FIG. 4 is a perspective view illustrating a mold used for forming a groove in a metal terminal. [Diagram 5] FIG. 11 is a cross-sectional view illustrating machining of a first groove portion. [Figure 6] FIG. 11 is a perspective view illustrating machining of a second groove portion. [Figure 7] FIG. [Figure 8] FIG. 2 is a partially sectional perspective view illustrating a groove structure. [Figure 9] FIG. 4 is a cross-sectional view illustrating an example of a non-uniform pitch groove. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0029] 1.Metal-resin composite molded body Fig. 1 illustrates a metal resin composite molded product 10 according to this embodiment, and Fig. 2 illustrates a metal terminal 30.
[0030] 1 to 9 show an orthogonal coordinate system, which is made up of a T axis, an L axis, and a W axis.
[0031] The T-axis is a thickness direction axis. The T-axis is set based on the thickness direction of the intermediate portion 36 of the metal terminal 30. For example, the T-axis extends perpendicular to the flat surface 31 of the intermediate portion 36. The W-axis is a width direction axis. The W-axis is set parallel to the width direction of the metal terminal 30. Furthermore, the L-axis is a longitudinal axis of the intermediate portion 36.
[0032] The metal resin composite molded body 10 includes a resin part 20 and a metal terminal 30. The metal resin composite molded body 10 is manufactured by, for example, insert molding. The resin part 20 is, for example, a plate-shaped part. The material of the resin part 20 is, for example, a highly heat-resistant crystalline thermoplastic resin such as PPS resin or PPA resin.
[0033] For example, a terminal block (not shown) is placed on the upper surface 22 of the resin part 20. Therefore, the upper surface 22 is an area that should not be exposed to water. On the other hand, the lower surface 24 is connected to, for example, a pump stator and is an area that is exposed to water.
[0034] The metal terminal 30 has ends exposed from the upper surface 22 and the lower surface 24 of the resin part 20. The metal terminal 30 has a flat plate shape and is also called a blank. The metal terminal 30 is made of a conductive material such as copper, brass, or iron.
[0035] 1 and 2, both ends of the metal terminal 30 in the longitudinal direction are bent into a substantially S-shape. The metal terminal 30 has a first end 32, a second end 34, and a middle portion 36.
[0036] A first end 32 at one longitudinal end of the metal terminal 30 is exposed from the upper surface 22 of the resin part 20. For example, the first end 32 is connected to a terminal block. A second end 34 at the other longitudinal end of the metal terminal 30 is exposed from the lower surface 24 of the resin part 20. For example, the second end 34 is connected to a stator of a motor.
[0037] An intermediate portion 36 is formed between the first end portion 32 and the second end portion 34. The intermediate portion 36 is embedded in the resin part 20. If a gap is formed at the interface between the intermediate portion 36 and the resin part 20, liquid may leak from the lower surface 24 (wet area) of the resin part 20 to the upper surface 22 (non-wet area). Therefore, a terminal groove 38 is formed in the intermediate portion 36.
[0038] 2.Groove shape The terminal groove 38 is formed around the entire circumference of the intermediate portion 36 of the metal terminal 30. The terminal groove 38 is formed in an annular shape with the longitudinal axis L as the central axis. Furthermore, a plurality of terminal grooves 38 are formed in the intermediate portion 36 along the longitudinal direction.
[0039] 8, the terminal groove 38 includes a first groove portion 40 and a second groove portion 50. The first groove portion 40 is formed on both thickness-wise surfaces of the metal terminal 30. The second groove portion 50 is formed on both width-wise surfaces of the metal terminal 30. The first groove portion 40 and the second groove portion 50 both extend in a straight line. The first groove portion 40 and the second groove portion 50 are connected to each other, so that the terminal groove 38 is formed around the entire circumference (i.e., annularly) of the intermediate portion 36.
[0040] 2 illustrates an enlarged cross-sectional view (AA cross-sectional view) of the terminal groove 38. A plurality of terminal protrusions 41 and terminal recesses 43 are formed in the terminal groove 38. The terminal protrusions 41 protrude from the flat plate surface 31 (non-coining surface) of the intermediate portion 36. The terminal recesses 43 are recessed from the flat plate surface 31 (non-coining surface).
[0041] For example, the protruding height H20 of the terminal protruding portion 41 is lower than the recessed depth H21 of the terminal recessed portion 43 (H20 < H21). As described later, the terminal protruding portion 41 is formed by a relief material generated when the terminal recessed portion 43 is coined.
[0042] 3 illustrates a TL cross section of the first groove portion 40. The TL cross section is the same cut surface as the AA cross section in FIG. 2. Except for the groove depth of the first groove portion 40, the second groove portion 50 has the same cross-sectional shape as that in FIG. 3. That is, the second groove portion 50 has the same groove width and pitch as the first groove portion 40. Here, even if there is a difference in the groove width or groove pitch, it is considered to be the same as long as the difference falls within the tolerance. In addition, the groove pitch refers to the distance between adjacent terminal grooves 38, 38.
[0043] The first groove portion 40 and the second groove portion 50 are both rectangular U-shaped grooves. That is, referring to Fig. 3 and Fig. 8, the first groove portion 40 has a bottom surface 46 and a pair of side surfaces 44, 44 erected from the bottom surface 46. Similarly, the second groove portion 50 has a bottom surface 56 and a pair of side surfaces 54, 54 erected from the bottom surface. Referring to Fig. 3, the adjacent terminal grooves 38, 38 are connected to the top surface 42.
[0044] The side surfaces 44, 44 and the side surfaces 54, 54 are all arranged to extend perpendicular to the flat plate surfaces 31, 35 (non-pressing surfaces, see FIG. 2). Note that perpendicular includes the case where the side surfaces 44, 44 and the side surfaces 54, 54 are substantially perpendicular. For example, if the angle of the side surfaces 44, 44 and the side surfaces 54, 54 with respect to the flat plate surfaces 31, 35 is within the range of 80° to 100°, the side surfaces 44, 44 and the side surfaces 54, 54 are considered to be perpendicular to the flat plate surfaces 31, 35.
[0045] The resin part 20 is filled in the terminal groove 38. A sealing effect is obtained at the interface between the resin part 20 and the metal terminal 30 by this filling portion 23 (indicated by 23A and 23B in FIG. 3).
[0046] The metal terminal 30 and the resin part 20 have different linear expansion coefficients. For example, the linear expansion coefficient of copper is 17.7×10 ―6 / ℃, whereas the linear expansion coefficient of PPS resin is 4.9×10 ―5 / ° C. In other words, in a high-temperature environment, the resin part 20 expands more than the metal terminal 30.
[0047] At this time, as the filling portion 23A expands thermally, it presses the side surfaces 44A, 44B of the terminal groove 38 as shown by the arrow (1). Then, due to the elasticity of the resin part 20, the side surfaces 44A, 44B are sealed.
[0048] Furthermore, in a low-temperature environment, the resin part 20 shrinks more than the metal terminal 30. At this time, as illustrated by the arrow (2), the filling parts 23A and 23B pressurize the side surfaces 44B and 44C. Then, based on the elasticity of the resin part 20, the side surfaces 44B and 44C are sealed.
[0049] In order to obtain such a sealing effect, the side surfaces 44, 54 (see FIG. 8) of the terminal groove 38 extend perpendicularly to the flat plate surfaces 31, 35 (see FIG. 2). As described above, the angle of the side surfaces 44, 44 and the side surfaces 54, 54 with respect to the flat plate surfaces 31, 35 is within the range of 80° to 100°.
[0050] In FIG. 3, the multiple terminal grooves 38 are formed with the same groove width and the same pitch. However, the groove width and groove pitch may be changed across the multiple terminal grooves 38. For example, FIG. 9 illustrates terminal grooves 38A, 38B, and 38C with different groove widths. The groove width W1 of terminal groove 38A, the groove width W2 of terminal groove 38B, and the groove width W3 of terminal groove 38C have a relationship of W1 > W2 > W3. For example, by providing multiple terminal grooves 38 with different groove widths and groove pitches, the above-mentioned sealing effect can be obtained in various temperature environments.
[0051] 8, the groove depths of the first groove portion 40 and the second groove portion 50 may be different. In other words, one of the first groove portion 40 and the second groove portion 50 is deeper than the other. For example, as shown by depths H5 and H6 in FIG. 8, the first groove portion 40 is deeper than the second groove portion 50.
[0052] As shown in Fig. 6 described later, when the terminal groove 38 is formed by coining, the plate-like portion 45 may be generated. By forming a relatively deep groove (first groove portion 40) and then forming a relatively shallow groove (second groove portion 50), the plate-like portion 45 is generated at the longitudinal end of the deep groove. Since only a small amount of material escape is required when coining the relatively shallow groove, the height of the plate-like portion 45 is suppressed to be less than the depth of the deep groove. Therefore, the deep groove (first groove portion 40) is prevented from being blocked by the plate-like portion 45 over the entire cross section.
[0053] Furthermore, the plate-like portion 45 is laid down by a bending process described later. By laying the plate-like portion 45 down on the bottom surface 46 of the relatively deep groove (first groove portion 40), a sufficient groove depth can be obtained even if the plate-like portion 45 adds height.
[0054] 3. Mold for forming grooves 4 illustrates a mold for forming the terminal groove 38 in the metal terminal 30. In the metal terminal 30 according to the present embodiment, the terminal groove 38 is formed by press molding. More specifically, the terminal groove 38 is formed by a coining process, which is also called coining.
[0055] As examples of dies for forming the terminal grooves 38, first dies 80A and 80B, second dies 60A and 60B, and third dies 70A-70D are shown in FIG.
[0056] The first dies 80A and 80B coin both sides in the thickness direction of the middle portion 36 of the metal terminal 30. A concave-convex shape (convex-concave groove) is formed on the pressing surfaces 82A and 82B of the first dies 80A and 80B. The concave-convex groove of the pressing surface 82A has the same groove width and pitch as the concave-convex groove of the pressing surface 82B.
[0057] Fig. 5 illustrates a TL cross section of the first mold 80A. The first mold 80B also has a cross-sectional shape similar to that of Fig. 5. In the following description of the first mold 80A, the structure of the first mold 80B will be described by replacing the suffix "A" with "B".
[0058] A plurality of die protrusions 81A and die recesses 83A are formed on the pressing surface 82A of the first die 80A. Fig. 5 illustrates a cross section of the first die 80A and the metal terminal 30 during the stamping process. The stroke of the stamping process is illustrated as coining stop positions L11 and L12. The top surface 84A of the die protrusion 81A is pressed in to the coining stop position L11. The bottom surface 85A of the die recess 83A moves to the coining stop position L12.
[0059] Here, the coining stop position L12 is located in front of the flat plate surface 31 (non-coining surface) of the middle portion 36 of the metal terminal 30. In other words, the coining stop position L12 is a position floating relative to the flat plate surface 31. That is, the bottom surface 85A of the die recess 83A is set at a position receding from the flat plate surface 31 (non-coining surface) of the middle portion 36 along the coining direction, so that the coining stop position L12 is set.
[0060] By setting the position in this way, as described later, the excess material caused by coining of the die protrusion 81A flows into the die recess 83A during coining. That is, the terminal protrusion 41 (see FIG. 2) is protruded from the middle portion 36. By using the excess material to raise the groove instead of as a wall that closes the inside of the groove, the sealing performance of the terminal groove 38 is improved.
[0061] At the coining stop positions L11 and L12, the distance H1 between the bottom surface 85A of the die recess 83A and the flat surface 31 (non-coining surface) may be shorter than the distance H2 between the top surface 84A of the die protrusion 81A and the flat surface 31 (non-coining surface) (H1 < H2). By setting such a positional relationship, the escape material that flows in is densely packed inside the die recess 83A. In other words, the shape of the die recess 83A is precisely transferred to the escape material.
[0062] 4, the second molds 60A, 60B coin both sides in the width direction of the middle portion 36 of the metal terminal 30. A concave-convex shape (convex-concave grooves) is formed on the pressing surfaces 62A, 62B of the second molds 60A, 60B. The concave-convex grooves of the pressing surfaces 62A, 62B have the same groove width and pitch as the concave-convex grooves of the pressing surfaces 82A, 82B.
[0063] Fig. 6 illustrates a pressing surface 62A of the second mold 60A. The second mold 60B also has a pressing surface shape similar to that of Fig. 6. In the following description of the second mold 60A, the structure of the second mold 60B will be described by replacing the suffix "A" with "B".
[0064] A plurality of die protrusions 61A and die recesses 63A are formed on the pressing surface 62A of the second die 60A. In the second die 60A as well, the coining stop position of the bottom surface 65A of the die recess 63A is located in front of the flat plate surface 35 (non-coining surface, see FIG. 2) of the intermediate portion 36 of the metal terminal 30. Furthermore, at the coining stop position, the separation distance between the bottom surface 85A of the die recess 83A and the flat plate surface 35 (non-coining surface) may be shorter than the separation distance between the top surface 84A of the die protrusion 81A and the flat plate surface 35 (non-coining surface).
[0065] Further, the depth H7 of the die recess 63A is shallower than the depth H8 (see FIG. 5) of the die recess 83A of the first die 80A. By performing coining using such a second die 60A, the second groove 50, which is shallower than the first groove 40, is formed.
[0066] 4, the third mold 70A-70D is an L-shaped mold when viewed from the side (when viewed in the L-axis direction). The third mold 70A-70D has first pressing surfaces 72A-72D and second pressing surfaces 74A-74D. The first pressing surfaces 72A-72D are disposed at right angles to the second pressing surfaces 74A-74D.
[0067] Fig. 7 illustrates a first pressing surface 72A and a second pressing surface 74A of the third mold 70A. The third molds 70B-70D also have the same pressing surface shape as that of Fig. 7. In the following description of the third mold 70A, the structures of the third molds 70B-70D will be described by replacing the suffix "A" with "B", "C", or "D".
[0068] A concave-convex shape (convex-convex grooves) is formed on the first pressing surface 72A of the third mold 70A. That is, a plurality of mold convex portions 71A and mold concave portions 73A are formed on the first pressing surface 72A. The mold convex portions 71A and mold concave portions 73A have the same groove width and pitch as the mold convex portions 61A and mold concave portions 63A formed on the pressing surface 62A of the second mold 60A (see FIG. 6), for example.
[0069] In addition, a concave-convex shape (convex-convex grooves) is also formed on the second pressing surface 74A of the third mold 70A. That is, a plurality of mold convex portions 75A and mold concave portions 77A are formed on the second pressing surface 74A. The mold convex portions 75A and mold concave portions 77A have the same groove width and pitch as the mold convex portions 81A and mold concave portions 83A formed on the pressing surface 82A of the first mold 80A (see FIG. 5).
[0070] As described later, the third dies 70A-70D are used in bending the plate-shaped portion 45 (see FIG. 7). Since the bending is an optional step and not an essential step, the third dies 70A-70D are optionally mounted on a press device.
[0071] 4. Groove formation process 4, first, first dies 80A and 80B are pressed against the middle portion 36 of the metal terminal 30 (first groove processing). Next, second dies 60A and 60B press the middle portion 36 (second groove processing). Furthermore, as an optional step, third dies 70A-70D press the middle portion 36 (bending process).
[0072] 5 illustrates the first groove processing. In the first groove processing, both sides in the thickness direction of the middle portion 36 are coined into the first mold 80A, 80B. At this time, the coining stop position L12 of the bottom surfaces 85A, 85B of the mold recesses 83A, 83B is located in front of the flat surface 31 (non-coined surface) of the middle portion 36 of the metal terminal 30. In other words, the coining stop position L12 is set at a position where the bottom surfaces 85A, 85B of the mold recesses 83A, 83B are retreated from the flat surface 31 (non-coined surface) of the middle portion 36 along the coining direction.
[0073] In the coining process, the metal (material) of the metal terminal 30 is pushed aside and moved by the die protrusions 81A, 81B of the first dies 80A, 80B, resulting in "material escape." At the coining stop position L12, a gap is provided between the flat plate surface 31 (non-pressed surface) of the middle portion 36 and the bottom surface 85A of the die recess 83A, so that the escaped material is guided into the gap. This makes it possible to raise the terminal protrusion 41 (see FIG. 2) of the first groove portion 40.
[0074] At the coining stop positions L11 and L12, the distance H1 between the bottom surfaces 85A and 85B of the die recesses 83A and 83B and the flat surface 31 (non-coining surface) may be shorter than the distance H2 between the top surfaces 84A and 84B of the die protrusions 81A and 81B and the flat surface 31 (non-coining surface) (H1 < H2). By adopting such a positional relationship, the escape material that flows in is densely packed into the die recesses 83A and 83B. In other words, the shape of the die recesses 83A and 83B is precisely transferred to the escape material.
[0075] Following the processing of the first groove portion, processing of the second groove portion is performed. Referring to Fig. 6, second dies 60A, 60B perform coining on both sides in the width direction of the middle portion 36. In this coining, the die protrusion 61A of the second die 60A is aligned with the first groove portion 40. For example, the metal terminal 30 and the second dies 60A, 60B are aligned by an alignment mechanism such as a ball screw (not shown).
[0076] 5, in coining the second groove portion 50, the coining stop positions of the bottom surfaces 65A, 65B of the die recesses 63A, 63B are located in front of the flat surface 35 (non-coined surface, see FIG. 2) of the middle portion 36 of the metal terminal 30. This makes it possible to raise the top surface 52 of the second groove portion 50 (see FIG. 8).
[0077] Furthermore, at the coining stop position, the distance between the bottom surfaces 65A, 65B of the die recesses 63A, 63B and the flat surface 35 (non-coining surface) may be shorter than the distance between the top surfaces 64A, 64B of the die protrusions 61A, 61B and the flat surface 31 (non-coining surface). This allows the escape material to be densely packed into the die recess 63A. In other words, the shape of the die recess 63A is transferred to the escape material with high accuracy.
[0078] Furthermore, by the coining process using the second molds 60A, 60B, the relief material enters into the first groove portion 40. More specifically, the remaining relief material that does not enter into the mold recesses 83A, 83B enters into the first groove portion 40. This relief material becomes a plate-shaped portion 45 and is provided in an upright position at the longitudinal end portion 39 of the first groove portion 40.
[0079] However, since the second groove portion 50 is shallower than the first groove portion 40, the stroke of the coining process is relatively short. That is, the amount of escape material generated in the first place is smaller than the amount of escape material generated during processing of the first groove portion 40. As a result, the height of the plate-shaped portion 45 is not so high as to block the entire cross section of the relatively deep first groove portion 40. That is, as exemplified by gap H4 in FIG. 6, even if the plate-shaped portion 45 is generated, the first groove portion 40 is sufficiently filled with resin, and the above-mentioned sealing effect is obtained.
[0080] After the second groove portion is processed, a bending process is performed as an optional process. In the bending process, the plate-like portion 45 is bent by the third molds 70A-70D. Referring to Fig. 4, the third molds 70A-70D press the middle portion 36 obliquely from the four corners of the cross section of the middle portion 36 toward the center of the cross section.
[0081] 7 and 8, by such pressing, the plate-like portion 45 formed at the longitudinal end 39 of the first groove portion 40 is bent so as to lie on the bottom surface 46 of the first groove portion 40. By bending the plate-like portion 45, the first groove portion 40 is opened to a sufficient depth over the entire circumference.
[0082] In the above embodiment, the first groove portion 40 is deeper than the second groove portion 50. Alternatively, the second groove portion 50 may be deeper than the first groove portion 40. For example, this alternative form is applicable when the height of the plate-shaped portion 45 is sufficiently smaller than the plate thickness of the intermediate portion 36.
[0083] In this alternative embodiment, the second groove portion is first processed, and then the first groove portion is processed. Then, the plate-shaped portion 45 is formed on the bottom surface 56 of the second groove portion 50. Furthermore, the plate-shaped portion 45 is laid on the bottom surface 56 by a bending process.
[0084] Furthermore, when the height of the plate-like portion 45 is sufficiently lower than the depths of the first groove portion 40 and the second groove portion 50, the first groove portion 40 and the second groove portion 50 may be made to have the same depth. For example, when most of the relief material is used to raise the height of the top surface 52 (see FIG. 8) in machining the second groove portion, the first groove portion 40 and the second groove portion 50 will have the same depth.
[0085] In the above embodiment, the terms "same" and "identical" include differences within a preset tolerance. In other words, even if there is a difference between the two (for example, the groove depth of the first groove portion 40 and the second groove portion 50), the two are considered to be identical as long as the difference falls within the tolerance. [Explanation of symbols]
[0086] 10 metal-resin composite molded body, 20 resin part, 30 metal terminal, 31, 35 flat surface (non-coined surface) of metal terminal, 32 first end, 34 second end, 36 middle portion, 38 terminal groove, 39 longitudinal end of first groove portion, 40 first groove portion, 41 terminal protrusion portion, 43 terminal recess portion, 44 side surface of terminal groove, 45 plate-shaped portion, 46 bottom surface of first groove portion, 50 second groove portion, 52A, 52B pressing surface of first mold, 60A, 60B second mold, 61, 71, 81 mold protrusion portion, 62A, 62B pressing surface of second mold, 63, 73, 83 mold recess portion, 70A-70D third mold, 72A-72D first pressing surface of third mold, 74A-74D second pressing surface of third mold, 80A, 80B first mold.
Claims
1. A flat metal terminal; a resin part in which both ends of the metal terminal are exposed and a middle portion of the metal terminal is embedded; A metal resin composite molding comprising: A groove is formed in the intermediate portion of the metal terminal, a first groove portion formed on each thickness direction surface of the metal terminal and a second groove portion formed on each width direction surface of the metal terminal and connected to the first groove portion, the groove being formed around the entire circumference of the metal terminal; The first groove portion is deeper than the second groove portion, At the longitudinal end of the first groove portion, a plate-shaped portion is disposed in a state where it is laid on a bottom surface. Metal-resin composite molded body.
2. The metal-resin composite molding according to claim 1, The groove is formed by forming recesses and protrusions over the entire circumference by coining, The grooves are arranged in a plurality of rows along the longitudinal direction of the intermediate portion, the recess is recessed from the non-coined surface of the middle portion; the protrusion protrudes from the non-coined surface of the middle portion; a side surface of the groove formed by the recess and the protrusion extends perpendicular to the non-coining surface; Metal-resin composite molded body.
3. The metal-resin composite molding according to claim 1 or 2, The plurality of grooves are arranged at least in part at different pitches. Metal-resin composite molded body.
4. A flat metal terminal; a resin part in which both ends of the metal terminal are exposed and a middle portion of the metal terminal is embedded; A method for producing a metal-resin composite molding comprising: A die having a concave-convex shape formed on a pressing surface is used to coin both thickness and width sides of the middle portion to form a groove around the entire circumference of the middle portion; The mold includes a first mold having a concave-convex shape formed on the pressing surface, and a second mold and a third mold having a concave-convex shape having the same groove width and pitch as the first mold formed on the pressing surface, The coining process is forming a first groove portion in the middle portion by coining both surfaces of the middle portion in a thickness direction with the first die; After the first groove portion is processed, a second groove portion is processed by coining both sides of the middle portion in the width direction with the second die to form a second groove portion connected to the first groove portion in the middle portion. a bending process in which, after the second groove portion is formed, a plate-shaped portion formed at an end portion in the longitudinal direction of the first groove portion is bent by the third mold so as to be laid on a bottom surface of the first groove portion; Including, A method for producing a metal-resin composite molded product.
5. The method for producing a metal-resin composite molding according to claim 4, The first mold has a deeper concave-convex groove than the second mold. A method for producing a metal-resin composite molded product.
6. A flat metal terminal; a resin part in which both ends of the metal terminal are exposed and a middle portion of the metal terminal is embedded; A method for producing a metal-resin composite molding comprising: A die having a concave-convex shape formed on a pressing surface is used to coin both thickness and width sides of the middle portion to form a groove around the entire circumference of the middle portion; The mold includes a first mold having a concave-convex shape formed on the pressing surface, and a second mold and a third mold having a concave-convex shape having the same groove width and pitch as the first mold formed on the pressing surface, The coining process is forming a second groove portion in the middle portion by coining both sides of the middle portion in the width direction with the second die; a first groove processing step in which, after the second groove processing, both surfaces in the thickness direction of the intermediate portion are coined with the first die to form a first groove portion connected to the second groove portion in the intermediate portion; a bending process in which, after the first groove portion is formed, a plate-shaped portion formed at an end portion in the longitudinal direction of the second groove portion is bent by the third mold so as to be laid on a bottom surface of the second groove portion; Including, A method for producing a metal-resin composite molded product.
7. A flat metal terminal; a resin part in which both ends of the metal terminal are exposed and a middle portion of the metal terminal is embedded; A metal resin composite molding comprising: A groove is formed in the intermediate portion of the metal terminal, a first groove portion formed on each thickness direction surface of the metal terminal and a second groove portion formed on each width direction surface of the metal terminal and connected to the first groove portion, the groove being formed around the entire circumference of the metal terminal; At the longitudinal end of the first groove portion or the second groove portion, a plate-shaped portion is disposed in a state where it is laid on a bottom surface. Metal-resin composite molded body.
8. A flat metal terminal; a resin part in which both ends of the metal terminal are exposed and a middle portion of the metal terminal is embedded; A metal resin composite molding comprising: A groove is formed in the intermediate portion of the metal terminal, a first groove portion formed on each thickness direction surface of the metal terminal and a second groove portion formed on each width direction surface of the metal terminal and connected to the first groove portion, the groove being formed around the entire circumference of the metal terminal; The second groove portion is deeper than the first groove portion, At the longitudinal end of the second groove portion, a plate-shaped portion is disposed in a state where it is laid on a bottom surface. Metal-resin composite molded body.
Citation Information
Patent Citations
Connector socket, vehicle-mounted equipment and vehicle
CN110492300A
Steering shaft lock
JP1981067652A
Connector
JP2014216165A
Waterproof connector
JP2016081737A
Method of manufacturing terminal and component for electrical circuit
JP2017147079A