Trench gate type semiconductor device and method for manufacturing the same

The semiconductor device addresses the challenge of balancing channel and contact resistance by employing trenches with a narrow depth and wider bottom distance, achieving low resistance through the FinFET effect and increased contact area.

JP7948847B2Active Publication Date: 2026-11-11DENSO CORP +2
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023006764
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-01-19
Publication Date
2026-11-11
Estimated Expiration
2043-01-19

AI Technical Summary

Technical Problem

Existing semiconductor devices with trench gates face challenges in balancing low channel resistance and high contact resistance due to the proximity of trenches, which limits the contact area between the source region and the upper electrode.

Method used

The semiconductor device design includes trenches with a maximum distance of less than 200 nm in the depth range where the body region is located, combined with a wider distance at the bottom, ensuring a large contact area between the source region and the upper electrode, while maintaining the FinFET effect for low channel resistance.

Benefits of technology

This design achieves both low channel resistance and low contact resistance by leveraging the FinFET effect and securing a sufficient contact area, enhancing electron mobility and reducing overall resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007948847000001
    Figure 0007948847000001
  • Figure 0007948847000002
    Figure 0007948847000002
  • Figure 0007948847000003
    Figure 0007948847000003
Patent Text Reader

Abstract

To provide a technique of reducing both the channel resistance and the contact resistance.SOLUTION: A trench gate type semiconductor device includes a semiconductor substrate, a first trench, a second trench, a gate insulating film, a gate electrode, and an upper electrode. The semiconductor substrate includes an n-type first semiconductor region in contact with the upper electrode, a p-type body region disposed below the first semiconductor region and extending from a position in contact with the gate insulating film in the first trench to a position in contact with the gate insulating film in the second trench, and an n-type second semiconductor region disposed below the body region and extending from the gate insulating film in the first trench to the position in contact with the gate insulating film in the second trench. A maximum value of the distance between the first trench and the second trench in a depth range where the body region is disposed is less than 200 nm. The distance between the first trench and the second trench on an upper surface of the semiconductor substrate is larger than the maximum value.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The technology disclosed herein relates to trench gate semiconductor devices and methods for manufacturing the same. [Background technology]

[0002] Patent Document 1 discloses a semiconductor device equipped with a trench gate. This semiconductor device has a semiconductor substrate having a plurality of trenches spaced apart on its upper surface, a gate insulating film and a gate electrode disposed within the trenches, and an upper electrode covering the upper surface of the semiconductor substrate. The semiconductor substrate also has an n-type source region, a p-type body region, and an n-type drift region. The source region is located between two trenches and is in contact with the upper electrode. The body region is located between two trenches and extends from a position in contact with the gate insulating film in one trench to a position in contact with the gate insulating film in the other trench. The drift region is located between two trenches, below the body region, and is separated from the source region by the body region.

[0003] In this semiconductor device, the distance between two adjacent trenches is relatively small, and when the semiconductor device is turned on, almost the entire body region located between the trenches inverts to form a channel. In this specification, the phenomenon in which almost the entire body region functions as a channel when the semiconductor device is turned on is called the FinFET effect. When the FinFET effect occurs, electrons flow even at positions far from the gate insulating film. Therefore, electrons are less affected by scattering caused by the interface between the gate insulating film and the body region. Consequently, electron mobility can be improved and channel resistance can be reduced. [Prior art documents] [Patent Documents]

[0004] [Patent Document 1] British Patent No. 2572442 [Overview of the project] [Problems that the invention aims to solve]

[0005] As described above, in the semiconductor device described in Patent Document 1, channel resistance can be reduced by reducing the distance between two adjacent trenches. However, in the semiconductor device described in Patent Document 1, because the distance between two adjacent trenches is small, it is difficult to secure a contact area between the source region and the upper electrode. Therefore, there is a problem of high contact resistance. This specification provides a technique for reducing both channel resistance and contact resistance. [Means for solving the problem]

[0006] The trench gate type semiconductor device (10) disclosed herein comprises a semiconductor substrate (12), a first trench (22a) provided on the upper surface (12a) of the semiconductor substrate, a second trench (22b) provided on the upper surface of the semiconductor substrate at a distance from the first trench, a gate insulating film (24) covering the inner surfaces of the first trench and the second trench, a gate electrode (26) disposed within the first trench and the second trench and insulated from the semiconductor substrate by the gate insulating film, and an upper electrode (70) covering the upper surface of the semiconductor substrate. The semiconductor substrate has an n-type first semiconductor region (30) located between the first trench and the second trench and in contact with the upper electrode; a p-type body region (32) located between the first trench and the second trench, below the first semiconductor region, and extending from a position in contact with the gate insulating film in the first trench to a position in contact with the gate insulating film in the second trench; and an n-type second semiconductor region (34) located between the first trench and the second trench, below the body region, extending from the gate insulating film in the first trench to a position in contact with the gate insulating film in the second trench, and separated from the first semiconductor region by the body region. The maximum distance between the first trench and the second trench in the depth range in which the body region is located is less than 200 nm. The distance between the first trench and the second trench on the upper surface of the semiconductor substrate is greater than the maximum value.

[0007] In the trench-gate type semiconductor device described above, the body region extends from the position in contact with the gate insulating film in the first trench to the position in contact with the gate insulating film in the second trench. Furthermore, the maximum distance between the first and second trenches in the depth range in which the body region is located is less than 200 nm, which is small enough to generate the FinFET effect. Therefore, when this semiconductor device is turned on, a channel is formed over almost the entire body region.

[0008] Furthermore, in the trench gate type semiconductor device described above, the distance between the first trench and the second trench on the upper surface of the semiconductor substrate is greater than the maximum value mentioned above. Therefore, the contact area between the first semiconductor region and the upper electrode is relatively large. As a result, the contact resistance between the first semiconductor region and the upper electrode is small. As explained above, this trench gate type semiconductor device can achieve low channel resistance and low contact resistance.

[0009] A method for manufacturing a trench gate semiconductor device (10) disclosed herein includes the steps of: preparing a first substrate (60) having an n-type first semiconductor region (30) provided on the upper surface of an n-type substrate (50), a p-type body region (32) provided on the upper surface of the first semiconductor region, and an n-type second semiconductor region (34) provided on the upper surface of the body region; forming an amorphous layer (40) near the upper surface of the second semiconductor region; and forming a first trench (22a) and a second trench (22b), respectively, which extend from the upper surface of the second semiconductor region to the first semiconductor region, wherein the maximum value of the distance between the first trench and the second trench in the depth range in which the body region is located is less than 200 nm, and the distance between the first trench and the second trench at the bottom of the first trench and the second trench is greater than the maximum value. The method comprises the steps of: forming the first trench and the second trench; forming a first insulating film (42, 44) covering the inner surfaces of the first trench and the second trench; a gate electrode (26) disposed in the first trench and the second trench; and a second insulating film (46) covering the upper surface of the gate electrode; flattening the upper surface of the second semiconductor region and the upper surface of the second insulating film so that the amorphous layer remains; preparing an n-type second substrate (62) having an amorphous layer (48) formed near its upper surface; joining the first substrate and the second substrate so that the amorphous layer of the first substrate and the amorphous layer of the second substrate face each other; exposing the first semiconductor region and the first insulating film by grinding the first substrate from the n-type substrate side; and forming an electrode (70) in contact with the exposed first semiconductor region.

[0010] Generally, it is relatively easy to form a trench where the lower part is narrower than the upper part, while it is difficult to form a trench where the lower part is wider than the upper part. In the above manufacturing method, trenches are formed on the first substrate such that the distance between the first and second trenches at the bottom of the first and second trenches is greater than the maximum distance between the first and second trenches in the depth range in which the body region is located. Then, the upper surface of the second substrate (the surface on which the amorphous layer is formed) and the trench-forming surface of the first substrate (i.e., the surface on the second semiconductor region side) are joined. That is, the first substrate with the trenches formed on it is joined to the second substrate inverted. After that, the surface opposite to the trench-forming surface (i.e., the surface of the joined substrate on the first substrate side) is ground to expose the first semiconductor region and the first insulating film in the trench. Then, electrodes are formed that are in contact with the exposed first semiconductor region. This makes it possible to obtain trenches in which the distance between the first and second trenches at the point of contact with the electrode (the bottom of the first and second trenches) is greater than the above-mentioned maximum value. Therefore, the contact area between the first semiconductor region and the electrode can be secured. Furthermore, the first and second trenches are formed so that the above-mentioned maximum value is less than 200 nm. As a result, it is possible to manufacture a semiconductor device that has low channel resistance due to the FinFET effect and low contact resistance. [Brief explanation of the drawing]

[0011] [Figure 1] Cross-sectional view of a trench gate type semiconductor device according to an embodiment. [Figure 2] A diagram illustrating the manufacturing process of a trench gate type semiconductor device. [Figure 3] A diagram illustrating the manufacturing process of a trench gate type semiconductor device. [Figure 4] A diagram illustrating the manufacturing process of trench gate type semiconductor devices. [Figure 5] A diagram illustrating the manufacturing process of trench gate type semiconductor devices. [Figure 6] A diagram for explaining a manufacturing process of a trench gate type semiconductor device. [Figure 7] A diagram for explaining a manufacturing process of a trench gate type semiconductor device. [Figure 8] A diagram for explaining a manufacturing process of a trench gate type semiconductor device. [Figure 9] A diagram for explaining a manufacturing process of a trench gate type semiconductor device. [Figure 10] A diagram for explaining a manufacturing process of a trench gate type semiconductor device. [Description of Embodiments]

[0012] In an example of the trench gate type semiconductor device disclosed in the present specification, the interval between the first trench and the second trench may decrease as it goes downward from the upper surface of the semiconductor substrate.

[0013] (Example) The trench gate type semiconductor device 10 (hereinafter simply referred to as semiconductor device 10) of the example shown in FIG. 1 is a MOSFET (metal-oxide-semiconductor field effect transistor). The semiconductor device 10 includes a semiconductor substrate 12. The semiconductor substrate 12 is composed of silicon carbide (SiC). However, the material of the semiconductor substrate 12 is not particularly limited, and may be, for example, silicon (Si), gallium nitride (GaN), diamond, or the like. Hereinafter, one direction parallel to the upper surface 12a of the semiconductor substrate 12 is referred to as the x direction, a direction parallel to the upper surface 12a and orthogonal to the x direction is referred to as the y direction, and the thickness direction of the semiconductor substrate 12 is referred to as the z direction.

[0014] Multiple trenches 22 are provided on the upper surface 12a of the semiconductor substrate 12. Each trench 22 extends long in the y direction. Each trench 22 extends parallel to each other with spacing in the x direction. The inner surface of each trench 22 is covered with a gate insulating film 24. A gate electrode 26, made of, for example, polysilicon, is placed inside each trench 22. The gate insulating film 24 also covers the upper surface of the gate electrode 26. That is, the gate electrode 26 is surrounded by the gate insulating film 24. The gate electrode 26 is insulated from the semiconductor substrate 12 by the gate insulating film 24. A portion of the gate insulating film 24 is exposed on the upper surface 12a of the semiconductor substrate 12. The width (i.e., length in the x direction) of each trench 22 increases as it moves downward from the upper surface 12a of the semiconductor substrate 12. Both sides of each trench 22 are inclined so as they move away from the center of the trench 22 towards the bottom surface. More specifically, each trench 22 has two sides, each consisting of a first side 23a connected to the upper surface 12a of the semiconductor substrate 12, and a second side 23b connected to the lower end of the first side 23a. The first side 23a extends with a slight curve, convex upwards. The second side 23b extends in a nearly planar shape. The angle between the second side 23b and the upper surface 12a is larger than the angle between the first side 23a and the upper surface 12a (i.e., the slope of the second side 23b is gentler than that of the first side 23a). The majority of the side of the trench 22 is made up of the second side 23b. For convenience of explanation, in the following, the trench 22 on the left in Figure 1 may be referred to as the first trench 22a, and the trench 22 on the right in Figure 1 may be referred to as the second trench 22b. Although not shown in the illustration, in Figure 1, multiple trenches similar to trench 22 are formed to the left of the first trench 22a and to the right of the second trench 22b.

[0015] An upper electrode 70 is positioned on the upper surface 12a of the semiconductor substrate 12. The upper electrode 70 has a source contact electrode 70a and a source electrode 70b. The source contact electrode 70a is made of, for example, nickel silicide (NiSi), titanium silicide (TiSi), etc. The source contact electrode 70a is provided in an area where the gate insulating film 24 is not exposed. The source electrode 70b is made of, for example, aluminum silicon (AlSi). The source electrode 70b covers the upper surface of the source contact electrode 70a and the gate insulating film 24. The upper electrode 70 is insulated from the gate electrode 26 by the gate insulating film 24. A lower electrode 72 is positioned on the lower surface 12b of the semiconductor substrate 12. The lower electrode 72 is in contact with substantially the entire area of ​​the lower surface 12b of the semiconductor substrate 12.

[0016] The semiconductor substrate 12 is provided with a source region 30, a body region 32, a drift region 34, and a drain region 36 inside.

[0017] The source region 30 is an n-type region. The source region 30 is positioned so as to be exposed on the upper surface 12a of the semiconductor substrate 12 and is in ohmic contact with the upper electrode 70 (source contact electrode 70a). The source region 30 extends from the gate insulating film 24 in the first trench 22a to a position where it is in contact with the gate insulating film 24 in the second trench 22b. The source region 30 is in contact with each gate insulating film 24 at the upper end of the first trench 22a and the upper end of the second trench 22b.

[0018] The body region 32 is a p-type region. The body region 32 is in contact with the source region 30. Below the source region 30, the body region 32 extends from the gate insulating film 24 in the first trench 22a to a position where it is in contact with the gate insulating film 24 in the second trench 22b. Below the source region 30, the body region 32 is in contact with the gate insulating films in each trench 22a and 22b. Although not shown, the body region 32 is in ohmic contact with the source contact electrode 70a in a different cross-section than that shown in Figure 1.

[0019] The drift region 34 is an n-type region. The drift region 34 is located below the body region 32. The drift region 34 extends from the gate insulating film 24 in the first trench 22a to a position where it touches the gate insulating film 24 in the second trench 22b. The drift region 34 is separated from the source region 30 by the body region 32. The drift region 34 is distributed to a depth range below the lower end of each trench 22. The drift region 34 covers the bottom of the first trench 22a and also covers the bottom of the second trench 22b.

[0020] The drain region 36 is an n-type region. The drain region 36 has a higher n-type impurity concentration than the drift region 34. The drain region 36 is located below the drift region 34. The drain region 36 is exposed on the lower surface 12b of the semiconductor substrate 12. The drain region 36 is in ohmic contact with the lower electrode 72.

[0021] As shown in Figure 1, the depth range D in which the body region 32 is located b So, what is the maximum value W of the distance W between the first trench 22a and the second trench 22b (the distance between the opposing sides of two adjacent trenches 22)? F However, it is less than 200 nm. In this embodiment, the width of each trench 22 increases towards the bottom, so the depth range D b Maximum value W F This becomes the upper end of the body region 32. Also, since the width of each trench 22 increases towards the bottom, the gap W between the first trench 22a and the second trench 22b on the upper surface 12a of the semiconductor substrate 12 T The maximum value is W F It is larger than that.

[0022] Next, the operation of the semiconductor device 10 will be described. When the semiconductor device 10 is in use, the semiconductor device 10, a load (for example, a motor) and a power supply are connected in series. A power supply voltage is applied to the series circuit of the semiconductor device 10 and the load. The power supply voltage is applied in such a direction that the drain side (lower electrode 72) of the semiconductor device 10 is at a higher potential than the source side (upper electrode 70). When turning on the semiconductor device 10, the potential of the gate electrode 26 is raised to a potential higher than the gate threshold. In the process of raising the potential of the gate electrode 26, first, the body region 32 in the range in contact with the gate insulating film 24 in the first trench 22a and the gate insulating film 24 in the second trench 22b is inverted to n-type. In the present embodiment, the depth range D where the body region 32 is arranged b The maximum value W of the interval W between the first trench 22a and the second trench 22b in F (that is, the maximum value of the width of the body region 32) is less than 200 nm. Since the width of the body region 32 is sufficiently narrow, when the potential of the gate electrode 26 is further increased, the FinFET effect occurs to expand the inversion layer, and substantially the entire body region 32 is inverted to n-type. As a result, a channel is formed in substantially the entire body region 32 between the first trench 22a and the second trench 22b. When the source region 30 and the drift region 34 are connected by the channel, electrons flow from the source region 30 to the drift region 34 via the channel. As a result, the semiconductor device 10 is turned on. When turning off the semiconductor device 10, the potential of the gate electrode 26 is made lower than the gate threshold. Then, the channel formed in the body region 32 disappears, and the semiconductor device 10 is turned off.

[0023] As described above, in the semiconductor device 10 of the present embodiment, the depth range D where the body region 32 is arranged b The maximum value W of the interval W between the first trench 22a and the second trench 22b in F is less than 200 nm, which is sufficiently small to enable the FinFET effect. Therefore, a channel can be formed in substantially the entire body region 32. Accordingly, the semiconductor device 10 has low channel resistance.

[0024] Furthermore, the gap W between the first trench 22a and the second trench 22b on the upper surface 12a of the semiconductor substrate 12. T However, the above maximum value W F It is larger than that. In other words, the source region 30 is exposed over a wide area of ​​the upper surface 12a of the semiconductor substrate 12. Therefore, a sufficient contact area can be secured between the source region 30 and the upper electrode 70 (source contact electrode 70a). Consequently, the semiconductor device 10 has low contact resistance.

[0025] As described above, the semiconductor device 10 of this embodiment can achieve low channel resistance and low contact resistance.

[0026] Next, a method for manufacturing the semiconductor device 10 will be described with reference to Figures 2 to 10. First, as shown in Figure 2, a first substrate 60 is prepared, which includes an n-type substrate 50, an n-type source region 30 provided on the n-type substrate 50, a p-type body region 32 provided on the source region 30, and an n-type drift region 34 provided on the body region 32. The first substrate 60 can be manufactured, for example, by forming the source region 30, the body region 32, and the drift region 34 on the n-type substrate 50 by appropriately combining known methods such as epitaxial growth and ion implantation.

[0027] Next, as shown in Figure 3, an amorphous layer 40 is formed near the upper surface of the drift region 34. Here, for example, argon atoms are irradiated onto the upper surface of the drift region 34. This disrupts the atomic arrangement near the upper surface of the drift region 34, and the amorphous layer 40 is formed.

[0028] Next, as shown in Figure 4, multiple trenches 22 are selectively formed on the upper surface of the drift region 34 by etching. Here, trenches 22 are formed that extend from the upper surface of the drift region 34, through the body region 32, to near the bottom surface of the source region 30. The sides of the trenches 22 formed by etching the first substrate 60 are inclined such that the width of the upper end of the trench 22 is wider than the width of the bottom of the trench 22. That is, the trenches 22 are formed so that their width gradually narrows towards the bottom. In addition, the trenches 22 are formed so that their bottom surface has a curved shape. Note that in this process, the depth range D in which the body region 32 is located b Each trench 22 is formed such that the maximum distance W between two adjacent trenches 22 (first trench 22a and second trench 22b) is less than 200 nm. Also, the distance W between the bottoms of two adjacent trenches 22 is B However, each trench 22 is formed such that it is greater than the maximum value of the interval W.

[0029] Next, as shown in Figure 5, an insulating film 42 is formed to cover the bottom surface of each trench 22. The insulating film 42 is formed such that its upper end is located below the upper end of the source region 30. Then, an insulating film 44 is formed on the side surface of each trench 22, and then a gate electrode 26 is formed by depositing polysilicon inside each trench 22. The gate electrode 26 is formed such that its upper end is located above the upper end of the body region 32. Then, an insulating film 46 is formed to cover the upper surface of the gate electrode 26.

[0030] Next, as shown in Figure 6, the upper surface of the drift region 34 and the upper surface of the insulating film 46 are planarized, for example, using CMP (Chemical Mechanical Polishing) technique, so that the amorphous layer 40 remains. The remaining insulating films 42, 44, and 46 become the gate insulating film 24.

[0031] Next, a second substrate 62, as shown in Figure 7, is prepared. The second substrate 62 has an n-type drain region 36 and an n-type drift region 34 provided on the drain region 36. The second substrate 62 can be manufactured, for example, by performing epitaxial growth on an n-type substrate that will become the drain region 36 to form the drift region 34. Then, an amorphous layer 48 is formed near the upper surface of the drift region 34. The amorphous layer 48 can be formed by the same process as the amorphous layer 40 in Figure 3.

[0032] Next, as shown in Figure 8, the first substrate 60 and the second substrate 62 are joined. Here, under a vacuum environment, the first substrate 60 and the second substrate 62 are brought into contact so that the amorphous layer 40 of the first substrate 60 and the amorphous layer 48 of the second substrate 62 face each other, and a heat treatment is performed at approximately 1000°C. This causes the disordered atoms in the amorphous layers 40 and 48 to flow in a direction that aligns them, and the amorphous layers 40 and 48 return to a crystalline state. In this process, the first substrate 60 and the second substrate 62 are joined. Note that in Figures 8 and later, the first substrate 60 shown in Figures 2 to 7 is depicted upside down.

[0033] Next, as shown in Figure 9, the n-type substrate 50 is removed. Specifically, the first substrate 60 is ground from the n-type substrate 50 side, for example using CMP technology, to expose the source region 30 and the gate insulating film 24 (insulating film 42). The first substrate 60 and the second substrate 62 after grinding become the semiconductor substrate 12.

[0034] Next, as shown in Figure 10, an upper electrode 70 is formed on the upper surface 12a of the semiconductor substrate 12, in contact with the source region 30. Specifically, a source contact electrode 70a is formed to cover the area where the source region 30 is exposed, and then a source electrode 70b is formed to cover the source contact electrode 70a and the gate insulating film 24.

[0035] Subsequently, the semiconductor device 10 shown in Figure 1 is completed by forming the lower electrode 72 on the lower surface 12b of the semiconductor substrate 12.

[0036] In the manufacturing method described above, the distance W between the first trench 22a and the second trench 22b at the bottom of the first trench 22a and the second trench 22b is B However, the depth range D in which the body region 32 is located b Each trench 22 is formed in the first substrate 60 such that it is greater than the maximum value of the distance W between the first trench 22a and the second trench 22b. Then, the upper surface of the second substrate 62 (the surface on which the amorphous layer 48 is formed) and the trench-forming surface of the first substrate 60 (i.e., the surface on the drift region 34 side) are joined. That is, the first substrate 60 with the trenches 22 formed on it is joined to the second substrate 62 inverted upside down. After that, the surface opposite to the trench-forming surface (i.e., the surface of the joined substrate on the first substrate side) is ground to expose the source region 30 and the gate insulating film 24 (insulating film 42) in the trench 22. Then, an upper electrode 70 is formed in contact with the exposed source region 30. This makes it possible to obtain trenches 22 such that the distance between the first trench 22a and the second trench 22b at the position in contact with the upper electrode 70 (the part that was the bottom of the first trench 22a and the second trench 22b) is greater than the above maximum value. Thus, in the above manufacturing method, by preparing two substrates 60 and 62, it is possible to obtain a trench 22 that is wider at the bottom than at the top, which was difficult to achieve conventionally. Therefore, the contact area between the source region 30 and the upper electrode 70 can be secured. Furthermore, the first trench 22a and the second trench 22b are formed so that the maximum value is less than 200 nm. As a result, a semiconductor device 10 having low channel resistance due to the FinFET effect and low contact resistance can be manufactured.

[0037] The source region 30 is an example of a "first semiconductor region," and the drift region 34 is an example of a "second semiconductor region." The insulating films 42 and 44 are examples of a "first insulating film," and the insulating film 46 is an example of a "second insulating film."

[0038] In the above-described embodiment, the side surface of the trench 22 was composed of a first side surface 23a and a second side surface 23b. However, the side surface of the trench 22 may be composed of, for example, only the second side surface 23b. Also, in the above-described embodiment, the trench 22 interval However, although it decreased from the upper surface 12a of the semiconductor substrate 12 downwards, the configuration is not limited to this. In the technology disclosed herein, the distance between the first trench 22a and the second trench 22b on the upper surface 12a of the semiconductor substrate 12 (in other words, the width of the source region 30 exposed between the two trenches 22) is the maximum value W F It is sufficient if it is larger than [the specified size], and the shape of the sides of the trench 22 is not particularly limited.

[0039] In the embodiment described above, the source region 30 was in contact with the gate insulating film 24. However, the source region 30 does not have to be in contact with the gate insulating film 24. In the art disclosed herein, a channel is formed over substantially the entire body region 32, so that electrons can flow even at positions within the body region 32 that are far from the gate insulating film 24. Therefore, even if the source region 30 is not in contact with the gate insulating film 24, electrons can flow from the upper electrode 70 to the lower electrode 72 via the source region 30, the channel, the drift region 34, and the drain region 36.

[0040] Furthermore, in the above-described embodiment, the case where the semiconductor device 10 is a MOSFET was explained. However, the semiconductor device 10 may also be an IGBT (Insulated Gate Bipolar Transistor). By changing the drain region 36 to a p-type region, an IGBT structure can be obtained.

[0041] Although embodiments have been described in detail above, these are merely illustrative and do not limit the scope of the claims. The technologies described in the claims include various modifications and changes to the specific examples illustrated above. The technical elements described in this specification or drawings exhibit technical usefulness individually or in various combinations, and are not limited to the combinations described in the claims at the time of filing. Furthermore, the technologies illustrated in this specification or drawings achieve multiple objectives simultaneously, and achieving even one of these objectives constitutes technical usefulness. [Explanation of symbols]

[0042] 10: Trench gate semiconductor device, 12: Semiconductor substrate, 22a: First trench, 22b: Second trench, 24: Gate insulating film, 26: Gate electrode, 30: Source region, 32: Body region, 34: Drift region, 36: Drain region, 70: Upper electrode, 72: Lower electrode

Claims

[Claim 1] A method for manufacturing a trench gate type semiconductor device (10), A step of preparing a first substrate (60) having an n-type first semiconductor region (30) provided on the upper surface of an n-type substrate (50), a p-type body region (32) provided on the upper surface of the first semiconductor region, and an n-type second semiconductor region (34) provided on the upper surface of the body region, A step of forming an amorphous layer (40) near the upper surface of the second semiconductor region, A step of forming a first trench (22a) and a second trench (22b) that each reach from the upper surface of the second semiconductor region to the first semiconductor region, wherein the maximum value of the distance between the first trench and the second trench in the depth range in which the body region is located is less than 200 nm, and the distance between the first trench and the second trench at the bottom of the first trench and the second trench is greater than the maximum value, The process involves forming a first insulating film (42, 44) covering the inner surfaces of the first trench and the second trench, a gate electrode (26) disposed within the first trench and the second trench, and a second insulating film (46) covering the upper surface of the gate electrode. A step of flattening the upper surface of the second semiconductor region and the upper surface of the second insulating film so that the amorphous layer remains, A step of preparing an n-type second substrate (62) having an amorphous layer (48) formed near the upper surface, A step of joining the first substrate and the second substrate such that the amorphous layer of the first substrate and the amorphous layer of the second substrate face each other, A step of exposing the first semiconductor region and the first insulating film by grinding the first substrate from the n-type substrate side, A step of forming an electrode (70) that is in contact with the exposed first semiconductor region, A manufacturing method that includes the following features.

Citation Information

Patent Citations

  • Power semiconductor device with a double gate structure

    GB2572442A

  • Method for manufacturing semiconductor device

    JP2002246554A

  • Semiconductor device manufacturing method and semiconductor device

    JP2008306047A

  • Semiconductor device and method of manufacturing the same

    JP2012248604A

  • Semiconductor device and insulated-gate bipolar transistor

    JP2015176927A