Electrode current collector, electrode assembly including the electrode current collector, and method for manufacturing the electrode current collector

The electrode current collector with a polymer and metal layer configuration addresses weldability and safety issues in secondary batteries, enhancing stability and reducing short circuit risks.

KR103045119B1Active Publication Date: 2026-11-06LG ENERGY SOLUTION LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
KR1020240108652
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Priority Date
2023-08-17
Filing Date
2024-08-13
Publication Date
2026-11-06
Estimated Expiration
2044-08-13

AI Technical Summary

Technical Problem

Secondary batteries face safety issues due to inadequate weldability and potential short circuits, which are not adequately addressed by existing technologies.

Method used

An electrode current collector with a polymer layer sandwiched between two metal layers, featuring a concave portion in at least one metal layer facing the polymer layer, and a narrowed spacing between the metal layers, enhancing weldability and thermal stability.

Benefits of technology

Improves weldability and thermal stability, reducing the risk of short circuits and fires, while maintaining high energy density and electrical conductivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 112024088356516-PAT00001_ABST
    Figure 112024088356516-PAT00001_ABST
Patent Text Reader

Abstract

The present invention relates to an electrode current collector, an electrode assembly including an electrode current collector, and a method for manufacturing an electrode current collector. The electrode current collector according to the present invention is an electrode current collector including an electrode tab extended at an end, comprising a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein a concave portion is formed in at least one of the first metal layer or the second metal layer at the electrode tab toward the polymer layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] The present invention relates to an electrode current collector, an electrode assembly including an electrode current collector, and a method for manufacturing an electrode current collector. Background Technology

[0003] Unlike primary batteries, secondary batteries are rechargeable and have been the subject of extensive research and development in recent years due to their potential for miniaturization and high capacity. As technological development and demand for electric vehicles, energy storage systems (ESS), and mobile devices increase, the demand for secondary batteries as an energy source is rapidly rising. However, the safety of secondary batteries is failing to keep pace with the speed of technological advancement. To address this, methods to improve safety include creating an electrical short circuit to drain energy or short-circuiting electrical connections before abnormal behavior occurs.

[0004] Secondary batteries are classified into coin batteries, cylindrical batteries, prismatic batteries, and pouch batteries according to the shape of the battery case. In secondary batteries, the electrode assembly mounted inside the battery case is a rechargeable power generation device consisting of a laminated structure of electrodes and separators.

[0005] Electrode assemblies can be roughly classified into a jelly-roll type, which is wound with a separator interposed between sheet-type positive and negative electrodes coated with an active material on a current collector; a stack type, which is sequentially stacked with a plurality of positive and negative electrodes interposed with a separator; and a stack / folding type, which is wound with stack-type unit cells into a long separating film. The problem to be solved

[0007] One aspect of the present invention is to provide an electrode current collector with improved weldability, an electrode assembly including the electrode current collector, and a method for manufacturing the electrode current collector. means of solving the problem

[0009] An electrode current collector according to an embodiment of the present invention is an electrode current collector comprising an electrode tab extended at an end, and comprises a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein a concave portion facing the polymer layer may be formed in at least one of the first metal layer or the second metal layer at the electrode tab.

[0010] Meanwhile, an electrode current collector according to an embodiment of the present invention is an electrode current collector including an electrode tab extended at an end, comprising a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein a portion of the first metal layer and the second metal layer at the electrode tab forms a narrow section with a narrowed spacing between them, and the spacing between the first metal layer and the second metal layer in the narrow section may be 72% or less with respect to the thickness of the polymer layer outside the narrow section.

[0011] In addition, an electrode assembly according to an embodiment of the present invention is an electrode assembly in which an electrode and a separator are alternately stacked, wherein the electrode includes an electrode current collector including an electrode tab extended at an end, and the electrode current collector includes a polymer layer in the stacking direction and a first metal layer and a second metal layer stacked on both sides of the polymer layer, and a concave portion facing the polymer layer may be formed in at least one of the first metal layer or the second metal layer at the electrode tab.

[0012] In addition, the method for manufacturing an electrode current collector according to an embodiment of the present invention may include: a lamination process of laminating a first metal layer and a second metal layer on both sides of a polymer layer to form a laminate; a tab forming process of notching an end portion of the laminate to form an electrode tab; and a concave portion forming process of forming a concave portion toward the polymer layer in at least one of the first metal layer or the second metal layer at the electrode tab. Effects of the invention

[0014] According to the present invention, in an electrode current collector in which metal layers are laminated on both sides of a polymer layer, a concave portion is formed in the metal layer located in the portion forming the electrode tab, so as to face the polymer layer, thereby significantly improving weldability. Brief explanation of the drawing

[0016] FIG. 1 is a perspective view showing an electrode current collector according to a first embodiment of the present invention. FIG. 2 is a cross-sectional view showing an electrode tab in an electrode current collector according to a first embodiment of the present invention. FIG. 3 is a perspective view showing an electrode current collector according to a second embodiment of the present invention. FIG. 4 is a cross-sectional view showing an electrode tab in an electrode current collector according to a second embodiment of the present invention. FIG. 5 is a cross-sectional view showing an electrode assembly according to an embodiment of the present invention. FIG. 6 is a side view showing an electrode assembly according to an embodiment of the present invention. FIG. 7 is a perspective view showing the electrode tab of the electrode current collector in an electrode assembly according to an embodiment of the present invention. FIG. 8 is a cross-sectional view showing a secondary battery including an electrode current collector according to an embodiment of the present invention. FIG. 9 is a perspective view showing the lamination process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 10 is a perspective view showing the tab formation process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 11 is a perspective view showing the process of forming a concave portion in a method for manufacturing an electrode current collector according to the first embodiment of the present invention. FIG. 12 is a cross-sectional view showing the process of forming a concave portion in the method for manufacturing an electrode current collector according to the first embodiment of the present invention. FIG. 13 is a cross-sectional view showing the process of forming a concave portion in the method for manufacturing an electrode current collector according to the second embodiment of the present invention. FIG. 14 is a cross-sectional view showing an additional lamination process in a method for manufacturing an electrode current collector according to a second embodiment of the present invention. FIG. 15 is a cross-sectional view showing an additional lamination process in a method for manufacturing an electrode current collector according to a second embodiment of the present invention. FIG. 16 is a perspective view showing an electrode current collector according to a third embodiment of the present invention. FIG. 17 is a cross-sectional view showing an electrode tab in an electrode current collector according to a third embodiment of the present invention. FIG. 18 is a perspective view showing an electrode current collector according to a fourth embodiment of the present invention. FIG. 19 is a cross-sectional view showing an electrode current collector according to a fourth embodiment of the present invention. FIG. 20 is a perspective view of a key part showing an example of an electrode current collector according to the fourth embodiment of the present invention. FIG. 21 is a perspective view of a key part showing another example of an electrode current collector according to the fourth embodiment of the present invention. Specific details for implementing the invention

[0017] The objects, specific advantages, and novel features of the present invention will become more apparent from the following detailed description and preferred embodiments in conjunction with the accompanying drawings. It should be noted that in assigning reference numerals to the components of each drawing in this specification, the same components are assigned the same number whenever possible, even if they are shown in different drawings. Furthermore, the present invention may be embodied in various different forms and is not limited to the embodiments described herein. Also, in describing the present invention, detailed descriptions of related known technologies that could unnecessarily obscure the essence of the invention are omitted.

[0019] Electrode current collector according to the first embodiment

[0020] FIG. 1 is a perspective view showing an electrode current collector according to a first embodiment of the present invention, and FIG. 2 is a cross-sectional view showing an electrode tab in an electrode current collector according to a first embodiment of the present invention.

[0021] Referring to FIG. 1 and FIG. 2, the electrode current collector (110) according to the first embodiment of the present invention is an electrode current collector (110) including an electrode tab (111) extended at the end, and includes a polymer layer (112) and a first metal layer (113) and a second metal layer (114) laminated on both sides of the polymer layer (112).

[0022] Additionally, a portion of the first metal layer (113) and the second metal layer (114) in the electrode tab (111) forms a narrow section (R1) with a narrow spacing between them, and the spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may be 72% or less of the thickness of the polymer layer (112).

[0023] In addition, a concave portion (115) facing the polymer layer (112) may be formed in at least one of the first metal layer (113) or the second metal layer (114) in the electrode tab (111).

[0025] More specifically, the electrode current collector (110) includes an electrode tab (111) extended at the end. That is, the electrode tab (111) may be formed by notching the end of the electrode current collector (110).

[0026] Additionally, the electrode current collector (110) includes a polymer layer (112) in the stacking direction and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112). Here, the polymer layer (112) is a layer containing a polymer material, and the first metal layer (113) and the second metal layer (114) are layers containing a metal material. Accordingly, the electrode current collector (110) is provided in a form in which the first metal layer (113) and the second metal layer (114) are stacked on both sides of the polymer layer (112), thereby preventing the occurrence of fire caused by excessive current density that occurs when the material is made only of metal. In addition, the electrode current collector (110) can have a first metal layer (113) and a second metal layer (114) formed thinly on both sides, so that when breaking occurs, the risk of a short circuit caused by metal burrs, etc. may be low.

[0027] In addition, for example, the thickness (t3) of the polymer layer (112) may be 4 to 20 µm. Specifically, for example, the thickness (t3) of the polymer layer (112) may be 4 to 14 µm.

[0028] And, for example, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114) may be 0.2 to 3 µm. Here, specifically, for example, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114) may be 0.2 to 2 µm.

[0029] Accordingly, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114) can be formed to be greater than or equal to a lower limit value of 0.2 µm, so that the electrical resistivity can be low. Accordingly, the function as an electrical connection, which is a required characteristic of the electric current collector foil, can be not limited. In other words, the function as a battery can be not weakened.

[0030] Meanwhile, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114) is formed to be less than or equal to an upper limit of 2 µm, so that the energy density can be high. In addition, the adverse effect on the enhancement of stability through electrical insulation during a nail test, which is a disadvantage of conventional metal foil, can be significantly reduced. Specifically, an electrode current collector (110) is provided in a form in which the first metal layer (113) and the second metal layer (114) are laminated on both sides of a polymer layer (112), so that the first metal layer (113) and the second metal layer (114) collapse due to the shrinkage of the polymer layer during a nail test, thereby enhancing safety through electrical insulation; however, if the first metal layer (113) and the second metal layer (114) are too thick, the polymer layer (112) cannot perform the stability enhancement function, and safety may deteriorate. Accordingly, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114) is formed to be less than or equal to an upper limit of 2 µm, so that the polymer layer (112) containing the polymer material can perform a stability enhancement function. Here, the nail test is a test of stability by penetrating with a nail.

[0032] Meanwhile, in the electrode tab (111), a portion of the first metal layer (113) and the second metal layer (114) forms a narrow section (R1) with a narrowed gap between them.

[0033] The mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may be, for example, 72% or less with respect to the thickness of the polymer layer (112). Accordingly, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) is formed to be, for example, 72% or less with respect to the thickness of the polymer layer (112), thereby improving weldability. Here, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may specifically be, for example, 50% or less with respect to the thickness of the polymer layer (112). At this time, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) can be more specifically, for example, 10 to 50% with respect to the thickness of the polymer layer (112).

[0034] Additionally, for example, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may be 2 to 10 μm. Here, the narrow section refers to a section where the mutual spacing between the first metal layer (113) and the second metal layer (114) is narrowed. Specifically, for example, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may be 2 to 8 μm. Accordingly, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) is formed to be greater than or equal to the lower limit value of 2 μm, thereby significantly improving thermal stability. one side, The mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) is formed to be less than or equal to an upper limit value of 10 µm, so that welding can be easy.

[0036] And, a concave portion (115) is formed toward the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (114) in the electrode tab (111). That is, in the narrow section (R1), a concave portion (115) can be formed toward the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (114) so ​​that the mutual gap (t0) between the first metal layer (113) and the second metal layer (114) is narrowed. Accordingly, the thickness of the polymer layer (112) portion in the welded part is reduced, and the gap between the first metal layer (113) and the second metal layer (114) is reduced, so that weldability can be improved.

[0037] The concave portion (115) may include a first concave portion (115a) formed in the first metal layer (113) and a second concave portion (115b) formed in the second metal layer (114).

[0038] The first concave portion (115a) and the second concave portion (115b) can be formed to face each other in the stacking direction.

[0039] Additionally, the first concave portion (115a) and the second concave portion (115b) may be provided at positions spaced apart from each other. Accordingly, the first metal layer (113) and the second metal layer (114) are provided in a spaced-apart manner, thereby maintaining the stability effect of the metalized electrode current collector (110) in which metal layers are laminated on both sides of the polymer layer (112).

[0040] And, for example, the mutually facing gap (t0) between the first metal layer (113) portion where the first concave portion (115a) is formed and the second metal layer (114) portion where the second concave portion (115b) is formed can be 2 to 10 μm. At this time, specifically, for example, the mutually facing gap (t0) between the first metal layer (113) portion where the first concave portion (115a) is formed and the second metal layer (114) portion where the second concave portion (115b) is formed can be 2 to 8 μm.

[0041] Accordingly, the mutually facing gap (t0) between the first metal layer (113) portion where the first concave portion (115a) is formed and the second metal layer (114) portion where the second concave portion (115b) is formed is formed to be greater than or equal to a lower limit value of 2 µm, so that thermal stability can be significantly improved. one side, The mutually facing gap (t0) between the first metal layer (113) portion in which the first concave portion (115a) is formed and the second metal layer (114) portion in which the second concave portion (115b) is formed is formed to be 8 µm or less, which is an upper limit value, so that welding can be significantly easier.

[0043] In addition, the first concave portion (115a) and the second concave portion (115b) may be formed in multiple numbers in the first metal layer (113) and the second metal layer (114), respectively.

[0044] Meanwhile, the depth (h1) in the stacking direction of the concave portion (115) can be formed to be, for example, 1 to 4 µm. Specifically, for example, the depth (h1) in the stacking direction of the first concave portion (115a) and the second concave portion (115b) can be formed to be 1 to 4 µm each.

[0046] Referring to FIG. 1 and FIG. 2, the electrode current collector (110) according to the first embodiment of the present invention configured as described above has the effect of significantly improving weldability by forming first and second concave portions (115a, 115b) facing the polymer layer (112) in the first and second metal layers located in the portion forming the electrode tab (111) of the metalized electrode current collector (110) in which metal layers are laminated on both sides of the polymer layer (112). That is, when electrode tabs (111) provided in each of the multiple electrode current collectors (110) are welded together to form an electrode assembly, first and second concave portions (115a, 115b) facing the polymer layer (112) are formed in the weld portion, so that the thickness of the polymer layer (112) located in the weld portion is formed thinly, and as the gap between the first and second metal layers is narrowed, the welding is performed significantly well. Ultimately, when welding with a laser or ultrasound, the laser or ultrasound cannot pass through the polymer layer (112), so the weldability can be prevented.

[0048] Electrode current collector according to the second embodiment

[0050] Hereinafter, an electrode current collector according to a second embodiment of the present invention will be described.

[0051] FIG. 3 is a perspective view showing an electrode current collector according to a second embodiment of the present invention, and FIG. 4 is a cross-sectional view showing an electrode tab in an electrode current collector according to a second embodiment of the present invention.

[0052] Referring to FIGS. 3 and 4, the electrode current collector (210) according to the second embodiment of the present invention is an electrode current collector (210) including an electrode tab (211) extended at the end, and includes a polymer layer (112) and a first metal layer (113) and a second metal layer (214) laminated on both sides of the polymer layer (112). In addition, a portion of the first metal layer (113) and the second metal layer (214) at the electrode tab (111) forms a narrow section (R2) in which the spacing between them is narrowed, and the spacing (t5) between the first metal layer (113) and the second metal layer (214) in the narrow section (R2) may be 72% or less of the thickness of the polymer layer (112).

[0053] In addition, a concave portion (215) is formed toward the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (214) in the electrode tab (211). At this time, an additional metal layer (216) may be further laminated.

[0054] The electrode current collector according to the second embodiment of the present invention differs from the electrode current collector according to the first embodiment of the present invention described above in that it is further provided with an additional metal layer (216) on the outer surface of the metal layer. Therefore, in this embodiment, details that overlap with the previously described embodiment are omitted or described briefly, and the description focuses on the differences.

[0056] More specifically, the electrode current collector (210) includes an electrode tab (211) extended at the end. That is, the electrode tab (211) may be formed by notching the end of the electrode current collector (210).

[0057] Additionally, the electrode current collector (210) includes a polymer layer (112) in the stacking direction and a first metal layer (113) and a second metal layer (214) stacked on both sides of the polymer layer (112). Here, the polymer layer (112) is a layer containing a polymer material, and the first metal layer (113) and the second metal layer (214) are layers containing a metal material.

[0058] In addition, for example, the thickness (t3) of the polymer layer (112) may be 4 to 20 µm. Specifically, for example, the thickness (t3) of the polymer layer (112) may be 4 to 14 µm.

[0059] And, for example, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (214) may be 0.2 to 3 µm. Here, specifically, for example, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (214) may be 0.2 to 2 µm.

[0061] Meanwhile, in the electrode tab (111), a portion of the first metal layer (113) and the second metal layer (214) forms a narrow section (R2) in which the spacing between them is narrowed. The spacing (t5) between the first metal layer (113) and the second metal layer (214) in the narrow section (R1) may be, for example, 72% or less with respect to the thickness of the polymer layer (112). Here, the spacing (t5) between the first metal layer (113) and the second metal layer (214) in the narrow section (R2) may specifically be, for example, 50% or less with respect to the thickness of the polymer layer (112). At this time, the spacing (t0) between the first metal layer (113) and the second metal layer (214) in the narrow section (R1) may more specifically be, for example, 10% to 50% with respect to the thickness of the polymer layer (112).

[0062] Additionally, for example, the mutual spacing (t5) between the first metal layer (113) and the second metal layer (214) in the narrow section (R2) may be 2 to 10 μm. Specifically, for example, the mutual spacing (t5) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may be 2 to 8 m.

[0064] And, a concave portion (215) is formed toward the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (214) in the electrode tab (211). That is, in the narrow section (R2), a concave portion (215) can be formed toward the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (214) so ​​that the mutual gap (t5) between the first metal layer (113) and the second metal layer (214) is narrowed.

[0065] At this time, a concave portion (215) may be formed in the first metal layer (113) at the electrode tab (211). Accordingly, the thickness of the polymer layer (112) portion in the welded portion is reduced, and the gap between the first metal layer (113) and the second metal layer (214) is reduced, thereby improving weldability. Also, the concave portion (215) and the second metal layer (214) may be provided at a position spaced apart from each other by a certain distance.

[0066] The mutually facing gap (t5) between the portion where the concave portion (215) is formed in the first metal layer (113) and the second metal layer (214) can be 2 to 10 μm.

[0067] Accordingly, the mutually facing gap (t5) between the portion where the concave portion (215) is formed in the first metal layer (113) and the second metal layer (214) is formed to be greater than or equal to the lower limit value of 2 µm, thereby enabling the effect of preventing fire caused by excessive current density in the electrode current collector (110) in which the first metal layer (113) and the second metal layer (114) are laminated on both sides of the polymer layer (112). That is, the mutually facing gap (t5) between the portion where the concave portion (215) is formed in the first metal layer (113) and the second metal layer (214) is formed to be greater than or equal to the lower limit value of 2 µm, so that thermal stability can be significantly improved.

[0068] one side,The mutually facing gap (t5) between the portion where the concave portion (215) is formed in the first metal layer (113) and the second metal layer (214) is formed to be less than or equal to an upper limit value of 8 µm, so that welding can be significantly easier.

[0069] In addition, the concave portion (215) can be formed in multiple numbers in the first metal layer (113).

[0070] Meanwhile, the depth in the stacking direction of the concave portion (215) can be formed to be 1 to 4 µm.

[0072] An additional metal layer (216) may be laminated on the outer surface of the first metal layer (113). Here, the additional metal layer (216) may be located on the electrode tab (211).

[0073] At this time, the thickness (t4) of the additional metal layer (216) can be formed to be 0.2 to 2 µm.

[0074] Additionally, the additional metal layer (216) may further include a protrusion (216a) protruding in correspondence with the concave portion (215). In this case, for example, the height (h2) of the protrusion (216a) in the stacking direction may be formed to be 1 to 4 μm.

[0075] Accordingly, when welding a metalized electrode current collector, an additional metal layer (216) can be laminated on the outer surface of the first metal layer (113) to significantly improve weldability. That is, weldability between electrode tabs (211) and weldability between electrode tabs (211) and electrode leads can be significantly improved.

[0077] Referring to FIG. 3 and FIG. 4, the electrode current collector (210) according to the second embodiment of the present invention configured as described above has the effect of improving weldability by forming a concave portion (215) toward the polymer layer (112) in the first metal layer (113) located in the portion forming the electrode tab (211) in the metalized electrode current collector (210) in which metal layers are laminated on both sides of the polymer layer (112). That is, when welding the electrode tabs (211) provided on each of the multiple electrode current collectors (210) to form an electrode assembly, and welding the electrode tabs (211) and the electrode lead, a concave portion (215) toward the polymer layer (112) is formed in the welding portion, so that the thickness of the polymer layer (112) located in the welding portion is formed thinly, and as the gap between the first and second metal layers is narrowed, the welding is performed significantly well. Ultimately, when welding using a laser or ultrasound, the laser or ultrasound cannot pass through the polymer layer (112), thereby preventing a decrease in weldability. In particular, by further laminating an additional metal layer (216) on the outer surface of the first metal layer (113), the weldability is significantly improved.

[0079] Electrode assembly according to the embodiment

[0081] Hereinafter, an electrode assembly according to an embodiment of the invention will be described.

[0082] FIG. 5 is a cross-sectional view showing an electrode assembly according to an embodiment of the present invention, and FIG. 6 is a side view showing an electrode assembly according to an embodiment of the present invention.

[0083] Referring to FIGS. 1, 2, 5 and 6, an electrode assembly (100) according to an embodiment of the present invention is an electrode assembly (100) in which an electrode (130) and a separator (140) are alternately stacked, wherein the electrode (130) includes an electrode current collector (110) including an electrode tab (111) extended at the end, and the electrode current collector (110) includes a polymer layer (112) in the stacking direction and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112), and a concave portion (115) is formed in at least one of the first metal layer (113) or the second metal layer (114) at the electrode tab (111) toward the polymer layer (112).

[0084] The electrode assembly (100) according to an embodiment of the present invention relates to an electrode assembly (100) comprising an electrode current collector according to the first embodiment and an electrode current collector (110) according to the second embodiment. Accordingly, the present embodiment will omit or briefly describe details that overlap with the previously described embodiment and focus on describing the differences.

[0086] More specifically, the electrode assembly (100) according to an embodiment of the present invention is a power generation device capable of charging and discharging, and forms a structure in which an electrode (130) and a separator (140) are assembled and alternately stacked.

[0087] The electrode (130) includes an electrode current collector (110) that includes an electrode tab (111) extended at the end.

[0088] Here, the electrode (130) may include an electrode current collector (110) and an electrode active material (120) coated on one or both sides of the electrode current collector (110). At this time, the electrode (130) may have a retaining region where the electrode active material (120) is coated on the electrode current collector (110) and an uncoated region where the electrode active material (120) is not coated on the electrode current collector (110). At this time, an electrode tab (111) may be positioned in the uncoated region of the electrode current collector (110).

[0089] The electrode current collector (110) may include a polymer layer (112) in the stacking direction and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112). At this time, a concave portion (115) is formed in at least one of the first metal layer (113) or the second metal layer (114) in the electrode tab (111) toward the polymer layer (112).

[0090] Meanwhile, the polymer layer (112) may be formed from a material including, for example, PET (polyethylene terephthalate), PI (polyimide), or EN (polyethylenenaphthalate).

[0092] FIG. 7 is a perspective view showing the electrode tab of the electrode current collector in an electrode assembly according to an embodiment of the present invention, and FIG. 8 is a cross-sectional view showing a secondary battery including the electrode current collector according to an embodiment of the present invention.

[0093] Meanwhile, referring to FIGS. 5 to 8, the electrode assembly (100) may have a plurality of electrodes (130) and a separator (140) stacked thereon. At this time, the electrode tabs (111) of the electrode current collectors (110) provided on each of the plurality of electrodes (130) are brought together and welded, and the concave portion (115) may be located at the welded portion (R) of the electrode tab (111). At this time, the electrode lead may be welded together at the welded portion (R). Accordingly, when welding the metalized electrode current collector (110), the concave portion (115) is located at the welded portion (R) of the electrode tab (111), so the weldability can be significantly improved. That is, the weldability between the electrode tabs (111) and the weldability between the electrode tab (111) and the electrode lead can be significantly improved.

[0095] Meanwhile, the electrode (130) may include an anode (130a) and a cathode (130b). And, the separator (140) separates the anode (130a) and the cathode (130b) to electrically insulate them.

[0096] The positive electrode (130a) may include a positive electrode current collector (110a) and a positive electrode active material (120a) provided on one side of the positive electrode current collector (110a). At this time, the positive electrode (130a) may include a positive electrode non-layer, which is an area where the positive electrode active material (120a) is not laminated.

[0097] The positive active material (120a) may be composed of lithium manganese oxide, lithium cobalt oxide, lithium nickel oxide, lithium iron phosphate, or compounds and mixtures containing one or more of these.

[0098] The negative electrode (130b) may include a negative electrode current collector (110b) and a negative electrode active material (120b) provided on one side of the negative electrode current collector (110b). At this time, the negative electrode (130b) may include a negative electrode non-layer, which is an area where the negative electrode active material (120b) is not laminated.

[0099] The negative electrode active material (120b) may be composed of, for example, artificial graphite, lithium metal, lithium alloy, carbon, petroleum coke, activated carbon, graphite, silicon compound, tin compound, titanium compound, or an alloy thereof. At this time, the negative electrode active material (120b) may further include, for example, non-graphite-based SiO (silica) or SiC (silicon carbide).

[0100] Meanwhile, the positive current collector (110a) and the negative current collector (110b) may include a polymer layer (112) and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112) in the stacking direction.

[0101] At this time, the first metal layer (113) and the second metal layer (114) located on the positive current collector (110a) may include aluminum material, and the first metal layer (113) and the second metal layer (114) located on the negative current collector (110b) may include copper material.

[0103] Meanwhile, referring to FIG. 2, for example, the concave portion (115) may be formed in the first metal layer (113) and the second metal layer. That is, the concave portion (115) may include a first concave portion (115a) formed in the first metal layer (113) and a second concave portion (115b) formed in the second metal layer.

[0104] Referring to FIG. 4, as another example, a concave portion (215) may be formed in the first metal layer (113). At this time, an additional metal layer (216) may be further laminated on the outer surface of the first metal layer (113). Here, the additional metal layer (216) may be located on the electrode tab (211).

[0106] Meanwhile, referring to FIG. 8, a secondary battery (10) can be manufactured by including an electrode assembly (100) according to an embodiment of the present invention configured as above. That is, the electrode assembly (100) can be housed in a pouch (20) to form a secondary battery (10). At this time, the secondary battery (10) can be formed by further including an electrode lead (30) that is connected to the electrode assembly (100) and electrically connected to the outside of the pouch (20).

[0108] Method for manufacturing an electrode current collector according to the first embodiment

[0110] Hereinafter, a method for manufacturing an electrode current collector according to the first embodiment of the present invention will be described.

[0111] FIG. 9 is a perspective view showing the lamination process in the method for manufacturing an electrode current collector according to an embodiment of the present invention, FIG. 10 is a perspective view showing the tab formation process in the method for manufacturing an electrode current collector according to an embodiment of the present invention, and FIG. 11 is a perspective view showing the concave portion formation process in the method for manufacturing an electrode current collector according to a first embodiment of the present invention.

[0112] Referring to FIGS. 9 to 11, the method for manufacturing an electrode current collector according to the first embodiment of the present invention comprises a lamination process of laminating a first metal layer (113) and a second metal layer (114) on both sides of a polymer layer (112) to form a laminate (S), a tab forming process of notching an end portion of the laminate (S) to form an electrode tab (111), and a concave portion forming process of forming a concave portion (115) facing the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (114) in the electrode tab (111). At this time, the concave portion forming process may form a narrow portion (R1) in which the spacing between the first metal layer (113) and the second metal layer (114) is narrowed in some sections of the electrode tab (111).

[0113] The method for manufacturing an electrode current collector according to the first embodiment of the present invention relates to a method for manufacturing an electrode current collector that includes the electrode current collector according to the first embodiment of the present invention described above and the electrode current collector included in the electrode assembly according to the embodiment of the present invention.

[0114] Accordingly, regarding the embodiment of the method for manufacturing an electrode current collector according to the first embodiment of the present invention, details that overlap with the previously described embodiments of the present invention are omitted or described briefly, and the description focuses on the differences.

[0116] More specifically, referring to FIG. 9, the lamination process forms a laminate (S) by laminating a first metal layer (113) and a second metal layer (114) on both sides of a polymer layer (112).

[0117] Additionally, the lamination process may laminate a first metal layer (113) and a second metal layer (114) on both sides of a polymer layer (112) through deposition or lamination.

[0119] Referring to FIG. 10, the tab forming process forms an electrode tab (111) by notching the end portion of the laminate (S).

[0121] That is, the tab forming process can form an electrode tab (111) in a protruding shape by cutting one side of a laminate (S) in which a first metal layer (113) and a second metal layer (114) are laminated on both sides of a polymer layer (112).

[0122] Additionally, the tab forming process can be notched so that an electrode tab (111) is formed in the laminate (S) through a punch die or a laser.

[0124] FIG. 12 is a cross-sectional view showing the process of forming a concave portion in the method for manufacturing an electrode current collector according to the first embodiment of the present invention.

[0125] Referring to FIGS. 2, 11, and 12, the concave formation process forms a concave portion (115) facing the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (114) in the electrode tab (111). Accordingly, the concave formation process can form a narrow section (R1) in which the spacing between the first metal layer (113) and the second metal layer (114) is narrowed in some sections of the electrode tab (111). At this time, the spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may be, for example, 72% or less of the thickness of the polymer layer (112). And, for example, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may be 2 to 10 μm. Specifically, for example, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) may be 2 to 8 m.

[0127] Additionally, the process of forming a concave portion may include a first pressing step of forming a first concave portion (115a) by pressing a portion of the first metal layer (113) with a pressing means (P), and a second pressing step of forming a second concave portion (115b) by pressing a portion of the second metal layer (114) with a pressing means (P). Here, the pressing means (P) may be, for example, a plunger. In this case, the process of forming a concave portion may form a concave portion (115) with a circular cross-section using a plunger whose end is formed in a cylindrical shape.

[0128] In addition, the process of forming the concave portions involves carrying out the first pressurization step and the second pressurization step together, and the first concave portion (115a) and the second concave portion (115b) can be formed to face each other at a certain distance apart from each other.

[0129] In addition, the concave portion formation process may form multiple first concave portions (115a) and second concave portions (115b) in the first metal layer (113) and the second metal layer (114), respectively.

[0130] Here, the process of forming the concave portion can, for example, form a depth (h1) of 1 to 4 µm in the stacking direction of the concave portion (115). Specifically, for example, the depth (h1) in the stacking direction of the first concave portion (115a) and the second concave portion (115b) can each be formed to 1 to 4 µm.

[0132] Method for manufacturing an electrode current collector according to the second embodiment

[0134] Hereinafter, a method for manufacturing an electrode current collector according to a second embodiment of the present invention will be described.

[0135] FIG. 13 is a cross-sectional view showing the process of forming a concave portion in the method for manufacturing an electrode current collector according to a second embodiment of the present invention, FIG. 14 is a cross-sectional view showing the additional stacking process in the method for manufacturing an electrode current collector according to a second embodiment of the present invention, and FIG. 15 is a cross-sectional view showing the additional stacking process in the method for manufacturing an electrode current collector according to a second embodiment of the present invention. Here, FIG. 13(a) shows the state before forming the concave portion, and FIG. 13(b) shows the state after the concave portion has been formed.

[0136] Referring to FIGS. 9, 10, and FIGS. 13 to 15, the method for manufacturing an electrode current collector according to the second embodiment of the present invention comprises a lamination process of laminating a first metal layer (113) and a second metal layer (214) on both sides of a polymer layer (112) to form a laminate (S); a tab forming process of notching an end portion of the laminate (S) to form an electrode tab (211); and a concave portion forming process of forming a concave portion (215) facing the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (214) in the electrode tab (211). Here, the concave portion forming process may allow a narrow portion (R2) to be formed in the electrode tab (211) such that a portion of the first metal layer (113) and the second metal layer (214) has a narrowed spacing from each other. Meanwhile, after the process of forming the concave portion, an additional lamination process may be further included to further laminate an additional metal layer (216).

[0137] The method for manufacturing an electrode current collector according to the second embodiment of the present invention relates to the electrode current collector (210) according to the second embodiment of the present invention described above and the method for manufacturing an electrode current collector included in an electrode assembly according to the embodiment of the present invention.

[0138] Accordingly, regarding the embodiment of the method for manufacturing an electrode current collector according to the second embodiment of the present invention, details that overlap with the previously described embodiments of the present invention are omitted or described briefly, and the description focuses on the differences.

[0140] More specifically, referring to FIG. 9, the lamination process forms a laminate (S) by laminating a first metal layer (113) and a second metal layer (214) on both sides of a polymer layer (112).

[0141] Additionally, the lamination process may laminate a first metal layer (113) and a second metal layer (214) on both sides of a polymer layer (112) through deposition or lamination. In this case, for example, the lamination process may form the first metal layer (113) and the second metal layer (214) by depositing them on both sides of the polymer layer (112).

[0143] Referring to FIG. 10, the tab forming process forms an electrode tab (211) by notching the end portion of the laminate (S).

[0144] That is, the tab forming process can form an electrode tab (211) in a protruding shape by cutting one side of a laminate (S) in which a first metal layer (113) and a second metal layer (214) are laminated on both sides of a polymer layer (112).

[0145] Additionally, the tab forming process can be notched so that an electrode tab (211) is formed in the laminate (S) through a punch die or a laser.

[0147] Referring to FIGS. 10 and 13, the concave formation process forms a concave portion (215) toward the polymer layer (112) in at least one of the first metal layer (113) or the second metal layer (214) in the electrode tab (211). Accordingly, the concave formation process can form a narrow section (R2) in which the spacing between the first metal layer (113) and the second metal layer (114) is narrowed in some sections of the electrode tab (211). At this time, the spacing (t5) between the first metal layer (113) and the second metal layer (114) in the narrow section (R2) may be, for example, 72% or less of the thickness of the polymer layer (112). And, for example, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (214) in the narrow section (R2) may be 2 to 10 μm. Specifically, for example, the mutual spacing (t0) between the first metal layer (113) and the second metal layer (214) in the narrow section (R2) may be 2 to 8 m.

[0149] Additionally, the process of forming the concave portion may include a pressurizing step of forming the concave portion (215) by pressing a part of the first metal layer (113) toward the polymer layer (112) with a pressurizing means (P).

[0150] The pressurization step can form a concave portion (215) such that the concave portion (215) and the second metal layer (214) are positioned at a certain distance from each other.

[0152] The additional lamination process may further laminate an additional metal layer (216) on the outer surface of the first metal layer (113) after the concave formation process.

[0153] Additionally, the additional stacking process can stack an additional metal layer (216) so that it is positioned on the electrode tab (211).

[0154] And, the additional lamination process can form the thickness (t4) of the additional metal layer (216) to 0.2 to 2 µm.

[0155] Additionally, the additional lamination process may further form a protrusion (216a) that protrudes in correspondence with the concave portion (215) in the additional metal layer (216). At this time, for example, the height of the protrusion (216a) in the lamination direction may be formed to be 1 to 4 μm.

[0157] Meanwhile, for example, an additional lamination process can be formed by applying heat and pressure to an additional metal layer (216) to laminate it with the first metal layer (113).

[0158] And, as another example, the additional lamination process can be formed by depositing an additional metal layer (216) on the outer surface of the first metal layer (113).

[0160] Although the present invention has been described in detail through specific embodiments, this is for the purpose of specifically explaining the invention and the invention is not limited thereto. It should be understood that various implementations are possible by those skilled in the art within the technical scope of the present invention.

[0161] In addition, the specific scope of protection of the invention will be clarified by the appended patent claims.

[0163] Electrode current collector according to the third embodiment

[0165] FIG. 16 is a perspective view showing an electrode current collector according to a third embodiment of the present invention, and FIG. 17 is a cross-sectional view showing an electrode tab in an electrode current collector according to a third embodiment of the present invention.

[0166] Referring to FIGS. 16 and 17, the electrode current collector (310) according to the third embodiment of the present invention is an electrode current collector (310) including an electrode tab (311) extended at the end, and includes a polymer layer (112) and a first metal layer (113) and a second metal layer (114) laminated on both sides of the polymer layer (112).

[0167] Additionally, in the electrode tab (311), a portion of the first metal layer (113) and the second metal layer (114) forms a narrow section (R3) with a narrow spacing between them, and the spacing (t0') between the first metal layer (113) and the second metal layer (114) in the narrow section (R3) may be 72% or less with respect to the thickness (t3') of the polymer layer (112).

[0168] In addition, at least one of the first metal layer (113) or the second metal layer (114) in the electrode tab (311) includes a metal wedge (315) that is inserted into the polymer layer (112).

[0169] The electrode current collector (310) according to the third embodiment of the present invention differs from the electrode current collector according to the first and second embodiments of the present invention described above in that a metal wedge (315) is positioned in at least one of the first metal layer (113) or the second metal layer (114). Accordingly, the present embodiment is described by omitting or briefly describing details that overlap with the previously described embodiments and focusing on the differences.

[0171] More specifically, the electrode current collector (310) includes an electrode tab (311) extended at the end. That is, the electrode tab (311) may be formed by notching the end of the electrode current collector (310).

[0172] Additionally, the electrode current collector (310) includes a polymer layer (112) in the stacking direction and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112). Here, the polymer layer (112) is a layer containing a polymer material, and the first metal layer (113) and the second metal layer (114) are layers containing a metal material. Accordingly, the electrode current collector (310) is provided in a form in which the first metal layer (113) and the second metal layer (114) are stacked on both sides of the polymer layer (112), thereby preventing the occurrence of fire caused by excessive current density that occurs when the material is made only of metal. In addition, the electrode current collector (310) can have a first metal layer (113) and a second metal layer (114) formed thinly on both sides, so that when breaking occurs, the risk of a short circuit caused by metal burrs, etc. may be low.

[0173] In addition, for example, the thickness (t3') of the polymer layer (112) may be 2 to 14 µm, and the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114) may be 0.2 to 3 µm.

[0175] A metal wedge (315) is positioned by being inserted into at least one of the first metal layer (113) or the second metal layer (114) from the electrode tab (311) to the polymer layer (112). At this time, the height (g1) of the metal wedge (315) inserted into the first metal layer (113) or the second metal layer (114) may be greater than the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114).

[0176] Additionally, the metal wedge (315) may include a metal material. Furthermore, the metal wedge (315) may include a material identical to that of the first metal layer (113) and the second metal layer (114), for example.

[0177] And, the metal wedge (315) may include a plurality of first metal wedges (315a) located in the first metal layer (113) and a plurality of second metal wedges (315b) located in the second metal layer (114).

[0178] Here, the first metal wedge (315a) and the second metal wedge (315b) may be positioned at a certain distance from each other.

[0179] In addition, the mutual spacing (t0') between the first metal wedge (315a) and the second metal wedge (315b) can be 2 to 10 μm. That is, the mutual spacing (t0') between the first metal layer (113) and the second metal layer (114) in the narrow section (R3) can be 2 to 10 μm.

[0180] Accordingly, the mutual spacing (t0') between the first metal wedge (315a) and the second metal wedge (315b) is formed to be greater than or equal to a lower limit value of 2 µm, thereby enabling the effect of preventing fire caused by excessive current density in the electrode current collector (310) in which the first metal layer (113) and the second metal layer (114) are laminated on both sides of the polymer layer (112). That is, the mutual spacing (t0') between the first metal wedge (315a) and the second metal wedge (315b) is formed to be greater than or equal to a lower limit value of 2 µm, thereby significantly improving thermal stability.

[0181] Meanwhile, the mutual spacing (t0') between the first metal wedge (315a) and the second metal wedge (315b) is formed to be less than or equal to the upper limit of 10 µm, so that welding is significantly easier and conductivity can be significantly increased.

[0183] Meanwhile, in the electrode tab (311), a portion of the first metal layer (113) and the second metal layer (114) forms a narrow section (R3) with a narrowed gap between them.

[0184] The mutual spacing (t0') between the first metal layer (113) and the second metal layer (114) in the narrow section (R3) may be, for example, 72% or less with respect to the thickness (t3') of the polymer layer (112). Accordingly, the mutual spacing (t0') between the first metal layer (113) and the second metal layer (114) in the narrow section (R3) is formed to be, for example, 72% or less with respect to the thickness (t3') of the polymer layer (112), thereby improving weldability. Here, the mutual spacing (t0') between the first metal layer (113) and the second metal layer (114) in the narrow section (R3) may specifically be, for example, 50% or less with respect to the thickness (t3') of the polymer layer (112). At this time, the mutual spacing (t0') between the first metal layer (113) and the second metal layer (114) in the narrow section (R1) can be more specifically, for example, 10 to 50% with respect to the thickness (t3') of the polymer layer (112).

[0186] In addition, as a first example of the electrode tab (311), the first metal wedge (315a) and the second metal wedge (315b) may be positioned parallel to each other in the stacking direction. Here, in one example of the electrode tab (311), the thicknesses (t1, t2) of the first metal layer (113) and the second metal layer (114) may be the same. At this time, for example, the thickness (t3') of the first metal layer (113) and the second metal layer (114) may be 0.5 to 1 µm.

[0187] Meanwhile, as a second example of the electrode tab (311), the first metal wedge (315a) and the second metal wedge (315b) in the metal wedge (315) may be positioned alternately with each other in the stacking direction.

[0188] Meanwhile, as a third example of the electrode tab (311), the thickness (t1) of the first metal layer (113) and the thickness (t2) of the second metal layer (114) may be formed differently from each other. At this time, a metal wedge (315) may be provided in the second metal layer (114).

[0190] Referring to FIGS. 16 and 17, the electrode current collector (310) according to the third embodiment of the present invention configured as described above has the effect of significantly improving weldability by inserting a metal wedge (315) into the polymer layer (112) in the metal layer located in the portion forming the electrode tab (311) in the metalized electrode current collector (310) in which a metal layer is laminated on both sides of the polymer layer (112). That is, when welding the electrode tabs (311) provided on each of the multiple electrode current collectors (310) to form an electrode assembly, and when welding the electrode tab (311) and the electrode lead, the metal wedge (315) is inserted into the polymer layer (112) in the welding portion, so that the thickness (t3') of the polymer layer (112) portion is formed thinly, and as the gap between the metal portions located on both sides of the polymer layer (112) is narrowed, the welding is significantly improved. Ultimately, when welding with a laser or ultrasound, the laser or ultrasound cannot pass through the polymer layer (112), so the weldability can be prevented.

[0192] Electrode current collector according to the fourth embodiment

[0194] FIG. 18 is a perspective view showing an electrode current collector according to a fourth embodiment of the present invention, and FIG. 19 is a cross-sectional view showing an electrode current collector according to a fourth embodiment of the present invention.

[0195] Referring to FIGS. 18 and 19, the electrode current collector (410) according to the fourth embodiment of the present invention is an electrode current collector (410) including an electrode tab (411) extended at the end, and includes a polymer layer (112) and a first metal layer (113) and a second metal layer (114) laminated on both sides of the polymer layer (112).

[0196] Additionally, in the electrode tab (411), a portion of the first metal layer (113) and the second metal layer (114) forms a narrow section (R4) with a narrow spacing between them, and the spacing (t0”) between the first metal layer (113) and the second metal layer (114) in the narrow section (R4) may be 72% or less with respect to the thickness (t3”) of the polymer layer (112).

[0197] In addition, at the electrode tab (411), the second metal layer (114) includes a metal rib (415) that extends into the polymer layer (112).

[0198] The electrode current collector (410) according to the fourth embodiment of the present invention differs from the electrode current collectors according to the first to third embodiments of the present invention described above in that it is provided with a metal rib (415) extending from the second metal layer (114) to a polymer layer. Accordingly, the present embodiment will omit or briefly describe details that overlap with the previously described embodiments and focus on describing the differences.

[0200] More specifically, the electrode current collector (410) includes an electrode tab (411) extended at the end. That is, the electrode tab (411) may be formed by notching the end of the electrode current collector (410).

[0201] Additionally, the electrode current collector (410) includes a polymer layer (112) in the stacking direction (D) and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112). Here, the polymer layer (112) is a layer containing a polymer material, and the first metal layer (113) and the second metal layer (114) are layers containing a metal material.

[0202] In addition, for example, the thickness (t3”) of the polymer layer (112) can be 2 to 14 µm.

[0203] And, for example, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114) may be 0.2 to 3 µm. Here, specifically, for example, the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114) may be 0.2 to 2 µm.

[0204] Meanwhile, the thickness (t1) of the first metal layer (113) may be the same as the thickness (t2) of the second metal layer (114), for example.

[0205] Additionally, the thickness (t1) of the first metal layer (113) may be thicker than the thickness (t2) of the second metal layer (114), as in another example. Accordingly, the manufacturing of the electrode current collector (410) may be easy.

[0207] The metal rib (415)(rib) may be provided to extend from the electrode tab to the second metal layer (114) to the polymer layer (112).

[0208] Additionally, the metal rib (415) may protrude from the inner surface of the second metal layer (114) into the polymer layer (112) and may be formed along the inner surface of the second metal layer (114).

[0209] In addition, the metal rib (415) may include the same material as the first metal layer (113) and the second metal layer (114).

[0211] FIG. 20 is a partial perspective view showing one example of an electrode current collector according to a fourth embodiment of the present invention, and FIG. 21 is a partial perspective view showing another example of an electrode current collector according to a fourth embodiment of the present invention.

[0212] Referring to FIG. 20, in the electrode tab (411) of the electrode current collector (410), the metal ribs (415) may be formed, for example, in the shape of a rectangular wall and provided in multiple numbers at regular intervals.

[0213] Referring to FIG. 21, in the electrode tab (411') of the electrode current collector (410'), the metal rib (415') may be provided in the form of a plurality of cylinders as another example.

[0215] Meanwhile, referring to FIG. 19, the end of the metal rib (415) may be spaced apart from the first metal layer (113) at a certain distance.

[0216] Accordingly, the end of the metal rib (415) is spaced apart from the first metal layer (113) at a certain distance, so that the first metal layer (113) and the second metal layer (114) are not connected, thereby maintaining the stability effect of the metalized electrode current collector (410) in which metal layers are laminated on both sides of the polymer layer (112).

[0218] Additionally, the spacing (t0”) between the end of the metal rib (415) and the first metal layer (113) can be 2 to 8 μm. That is, the mutual spacing (t0”) between the first metal layer (113) and the second metal layer (114) in the narrow section (R4) can be 2 to 10 μm. Accordingly, the mutual spacing (t0”) between the end of the metal rib (415) and the first metal layer (113) is formed to be greater than or equal to the lower limit value of 2 μm, thereby significantly improving thermal stability. Meanwhile, the mutual spacing (t0”) between the end of the metal rib (415) and the first metal layer (113) is formed to be less than or equal to the upper limit value of 8 μm, thereby making welding significantly easier.

[0220] Referring to FIG. 18 and FIG. 19, the electrode current collector (410) according to the fourth embodiment of the present invention configured as above is provided with a metal rib (415) extending toward the polymer layer (112) in the metal layer located in the portion forming the electrode tab (411) in the electrode current collector (410) in which a metal layer is laminated on both sides of the polymer layer (112), thereby having the effect of significantly improving weldability. That is, when welding the electrode tabs (411) provided on each of the multiple electrode current collectors (410) to form an electrode assembly, and welding the electrode tabs (411) and the electrode leads, the metal ribs (415) are extended toward the polymer layer (112) in the welding portion, so that the thickness (t3”) of the polymer layer (112) located in the welding portion is formed thinly, and as the gap between the first and second metal layers (113, 114) is narrowed, the welding is performed significantly well. Ultimately, when welding using a laser or ultrasound, it is possible to prevent the laser or ultrasound from failing to pass through the polymer layer (112), thereby preventing a decrease in weldability. Explanation of the symbols

[0222] 10: Secondary battery 20: Pouch 30: Electrode Lead 100: Electrode assembly 110,310,410: Electrode current collector 110a: Positive current collector 110b: Cathode current collector 111,211,311,411: Electrode tabs 112: Polymer layer 113: First metal layer 114, 214: Second metal layer 115, 215: Concave part 115a: First depression 115b: Second depression 120: Electrode active material 120a: Positive active material 120b: Cathode active material 130: Electrode 130a: Anode 130b: Cathode 140: Separator 216: Additional metal layer 216a: Protrusion 315: Metal wedge 315a: First metal wedge 315b: Second metal wedge 415, 415': Metal rib P: Pressurizing means R: Welding area S: Laminate

Claims

Claim 1 An electrode current collector comprising an electrode tab extended at an end, the electrode current collector comprising a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein at the electrode tab, the first metal layer and the second metal layer are provided in a spaced-apart manner, and at the electrode tab, a portion of the first metal layer and the second metal layer forms a narrow section with a narrowed spacing between them, wherein at least one of the first metal layer or the second metal layer forms a concave portion facing the polymer layer so as to narrow the spacing between the first metal layer and the second metal layer at the narrow section, and wherein the spacing between the first metal layer and the second metal layer at the narrow section is 2 to 10 μm. Claim 2 The electrode current collector according to claim 1, wherein the concave portion comprises a first concave portion formed in the first metal layer; and a second concave portion formed in the second metal layer. Claim 3 An electrode current collector according to claim 2, wherein the first concave portion and the second concave portion are formed to face each other in the stacking direction. Claim 4 In claim 3, the electrode current collector is provided at positions spaced apart from each other by a certain distance, wherein the first concave portion and the second concave portion. Claim 5 An electrode current collector according to claim 4, wherein the mutually facing distance between the first metal layer portion in which the first concave portion is formed and the second metal layer portion in which the second concave portion is formed is 2 to 8 μm. Claim 6 In claim 2, the first concave portion and the second concave portion are each formed as a plurality of electrode current collectors in the first metal layer and the second metal layer. Claim 7 An electrode current collector according to claim 1, wherein the depth in the stacking direction of the concave portion is 1 to 4 μm. Claim 8 An electrode current collector according to any one of claims 1 to 7, wherein the thickness of the polymer layer is 4 to 14 μm and the thickness of the first metal layer and the second metal layer is 0.2 to 2 μm. Claim 9 An electrode current collector according to claim 1, wherein the concave portion is formed in the first metal layer and further comprises an additional metal layer laminated on the outer surface of the first metal layer. Claim 10 An electrode current collector according to claim 9, wherein the thickness of the first metal layer and the second metal layer is formed to be 0.2 to 2 µm, and the thickness of the additional metal layer is formed to be 0.2 to 2 µm. Claim 11 In claim 9, the electrode current collector is provided such that the concave portion and the second metal layer are spaced apart from each other at a certain distance. Claim 12 An electrode current collector according to claim 11, wherein the mutually facing gap between the portion in which the concave portion is formed in the first metal layer and the second metal layer is 2 to 10 μm. Claim 13 In claim 9, the additional metal layer is an electrode current collector located on the electrode tab. Claim 14 The electrode current collector of claim 9, wherein the additional metal layer further comprises a protrusion protruding in correspondence with the concave portion. Claim 15 An electrode current collector according to claim 14, wherein the height of the protrusion in the stacking direction is formed to be 1 to 4 μm. Claim 16 An electrode current collector comprising an electrode tab extended at an end, the electrode current collector comprising a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein the first metal layer and the second metal layer are spaced apart from each other at the electrode tab, and a portion of the first metal layer and the second metal layer at the electrode tab forms a narrow section with a narrowed mutual spacing, wherein at least one of the first metal layer or the second metal layer forms a concave portion facing the polymer layer so as to narrow the mutual spacing of the first metal layer and the second metal layer at the narrow section, wherein the mutual spacing of the first metal layer and the second metal layer at the narrow section is 72% or less with respect to the thickness of the polymer layer outside the narrow section, and the mutual spacing of the first metal layer and the second metal layer at the narrow section is 2 to 10 μm. Claim 17 delete Claim 18 delete Claim 19 An electrode current collector according to claim 16, wherein, in the narrow section, at least one of the first metal layer or the second metal layer is inserted up to the polymer layer by a metal wedge such that the mutual spacing between the first metal layer and the second metal layer is narrowed. Claim 20 An electrode current collector according to claim 16, wherein, in the narrow section, the second metal layer includes a metal rib extending to the polymer layer so that the mutual spacing between the first metal layer and the second metal layer is narrowed. Claim 21 An electrode assembly having an electrode and a separator alternately stacked, wherein the electrode includes an electrode current collector including an electrode tab extended at an end, and the electrode current collector includes a polymer layer in the stacking direction and a first metal layer and a second metal layer stacked on both sides of the polymer layer, wherein the first metal layer and the second metal layer are provided in a spaced-apart manner at the electrode tab, and a portion of the first metal layer and the second metal layer at the electrode tab forms a narrow section with a narrowed mutual spacing, wherein at least one of the first metal layer or the second metal layer has a concave portion formed toward the polymer layer so as to narrow the mutual spacing of the first metal layer and the second metal layer at the narrow section, and wherein the mutual spacing of the first metal layer and the second metal layer at the narrow section is 2 to 10 μm, and the mutual spacing of the second metal layer is 2 to 10 μm. Claim 22 In claim 21, the electrode assembly comprises a plurality of electrodes and a separator, wherein the electrode tabs of the electrode current collectors provided on each of the plurality of electrodes are joined together and welded, and the concave portion is located at the welded portion of the electrode tab. Claim 23 In claim 21, the concave portion is formed in the first metal layer and further comprises an additional metal layer laminated on the outer surface of the first metal layer, wherein the additional metal layer is an electrode assembly located on the electrode tab. Claim 24 An electrode assembly according to claim 21, wherein the concave portion comprises a first concave portion formed in the first metal layer; and a second concave portion formed in the second metal layer, wherein the first concave portion and the second concave portion are formed to face each other in the stacking direction. Claim 25 A method for manufacturing an electrode current collector, comprising: a lamination process of laminating a first metal layer and a second metal layer on both sides of a polymer layer to form a laminate; a tab forming process of notching an end portion of the laminate to form an electrode tab; and a concave portion forming process of forming a concave portion toward the polymer layer in at least one of the first metal layer or the second metal layer in the electrode tab, wherein the first metal layer and the second metal layer in the electrode tab are provided in a spaced-apart manner, and the concave portion forming process forms a narrow portion in which the spacing between the first metal layer and the second metal layer in the electrode tab is narrowed, and the spacing between the first metal layer and the second metal layer in the narrow portion is 2 to 10 μm. Claim 26 A method for manufacturing an electrode current collector according to claim 25, wherein the concave portion forming process comprises: a first pressing step of forming a first concave portion by pressing a part of the first metal layer with a pressing means; and a second pressing step of forming a second concave portion by pressing a part of the second metal layer with a pressing means. Claim 27 A method for manufacturing an electrode current collector according to claim 26, wherein the concave portion forming process comprises the first pressing step and the second pressing step together, and the first concave portion and the second concave portion are formed to face each other at a position spaced apart from each other by a certain distance. Claim 28 A method for manufacturing an electrode current collector according to claim 27, wherein the concave portion forming process includes a pressing step of forming the concave portion by pressing a part of the first metal layer toward the polymer layer with a pressing means, and further includes an additional lamination process of laminating an additional metal layer on the outer surface of the first metal layer after the concave portion forming process. Claim 29 A method for manufacturing an electrode current collector according to claim 28, wherein the pressurizing step forms the concave portion such that the concave portion and the second metal layer are positioned at a certain distance from each other. Claim 30 A method for manufacturing an electrode current collector according to claim 28, wherein the lamination process forms the first metal layer and the second metal layer by depositing them on both sides of the polymer layer, and the additional lamination process forms the additional metal layer by laminating it with the first metal layer by applying heat and pressure. Claim 31 A method for manufacturing an electrode current collector according to claim 28, wherein the lamination process forms the first metal layer and the second metal layer by depositing them on both sides of the polymer layer, and the additional lamination process forms the additional metal layer by depositing it on the outer surface of the first metal layer. Claim 32 In claim 28, the additional lamination process is a method for manufacturing an electrode current collector in which the additional metal layer is laminated so as to be positioned on the electrode tab.

Citation Information

Patent Citations

  • Battery contacts and metallized film components of energy storage devices with internal fuses

    KR1020220122644A

  • Electrical collector body of secondary battery and secondary battery

    KR1020220145281A

  • Manufacturing Method of Electrode Assembly and Electrode Assembly By Using The Same

    KR1020230068521A

  • Current collectors comprising metallised films

    WO2022238713A1