Electrode current collector, electrode assembly including the electrode current collector, and method for manufacturing the electrode current collector
The electrode current collector with a polymer layer and metal wedge structure addresses weldability and safety issues in secondary batteries, enhancing thermal stability and preventing short circuits.
Patent Information
- Application Number
- KR1020240108650
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2023-08-17
- Filing Date
- 2024-08-13
- Publication Date
- 2026-11-06
- Estimated Expiration
- 2044-08-13
AI Technical Summary
Secondary batteries face safety issues due to inadequate weldability of electrode current collectors, leading to potential short circuits and fires from excessive current density.
An electrode current collector with a polymer layer sandwiched between two metal layers, featuring a metal wedge inserted into one of the metal layers at the electrode tab, enhancing weldability and thermal stability.
The design significantly improves weldability and thermal stability, preventing short circuits and fires by distributing current density effectively.
Smart Images

Figure 112024088356325-PAT00001_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to an electrode current collector, an electrode assembly including an electrode current collector, and a method for manufacturing an electrode current collector. Background Technology
[0003] Unlike primary batteries, secondary batteries are rechargeable and have been the subject of extensive research and development in recent years due to their potential for miniaturization and high capacity. As technological development and demand for electric vehicles, energy storage systems (ESS), and mobile devices increase, the demand for secondary batteries as an energy source is rapidly rising. However, the safety of secondary batteries is failing to keep pace with the speed of technological advancement. To address this, methods to improve safety include creating an electrical short circuit to drain energy or short-circuiting electrical connections before abnormal behavior occurs.
[0004] Secondary batteries are classified into coin batteries, cylindrical batteries, prismatic batteries, and pouch batteries according to the shape of the battery case. In secondary batteries, the electrode assembly mounted inside the battery case is a rechargeable power generation device consisting of a laminated structure of electrodes and separators.
[0005] Electrode assemblies can be roughly classified into a jelly-roll type, which is wound with a separator interposed between sheet-type positive and negative electrodes coated with an active material on a current collector; a stack type, which is sequentially stacked with a plurality of positive and negative electrodes interposed with a separator; and a stack / folding type, which is wound with stack-type unit cells into a long separating film. The problem to be solved
[0007] One aspect of the present invention is to provide an electrode current collector with improved weldability, an electrode assembly including the electrode current collector, and a method for manufacturing the electrode current collector. means of solving the problem
[0009] An electrode current collector according to an embodiment of the present invention is an electrode current collector comprising an electrode tab extended at an end, and comprises a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein a metal wedge inserted from the electrode tab to the polymer layer may be positioned in at least one of the first metal layer or the second metal layer.
[0010] In addition, an electrode assembly according to an embodiment of the present invention is an electrode assembly in which an electrode and a separator are alternately stacked, wherein the electrode includes an electrode current collector including an electrode tab extended at an end, and the electrode current collector includes a polymer layer in the stacking direction and a first metal layer and a second metal layer stacked on both sides of the polymer layer, and a metal wedge inserted from the electrode tab to at least one of the first metal layer or the second metal layer up to the polymer layer may be positioned.
[0011] In addition, the method for manufacturing an electrode current collector according to an embodiment of the present invention may include a lamination process of forming a laminate by laminating a first metal layer and a second metal layer on both sides of a polymer layer; a tab forming process of forming an electrode tab by notching an end portion of the laminate; and a wedge insertion process of inserting a metal wedge into at least one of the first metal layer or the second metal layer from the electrode tab to the polymer layer. Effects of the invention
[0013] According to the present invention, in an electrode current collector in which metal layers are laminated on both sides of a polymer layer, a metal wedge is inserted into the polymer layer in the metal layer located in the portion forming the electrode tab, thereby significantly improving weldability. Brief explanation of the drawing
[0015] FIG. 1 is a perspective view showing an electrode current collector according to an embodiment of the present invention. FIG. 2 is a cross-sectional view showing a first example of an electrode tab in an electrode current collector according to an embodiment of the present invention. FIG. 3 is a perspective view showing an example of an electrode wedge in an electrode current collector according to an embodiment of the present invention. FIG. 4 is a perspective view showing another example of an electrode wedge in an electrode current collector according to an embodiment of the present invention. FIG. 5 is a cross-sectional view showing a second example of an electrode tab in an electrode current collector according to an embodiment of the present invention. FIG. 6 is a cross-sectional view showing a third example of an electrode tab in an electrode current collector according to an embodiment. FIG. 7 is a cross-sectional view showing a fourth example of an electrode tab in an electrode current collector according to an embodiment. FIG. 8 is a cross-sectional view showing an electrode assembly according to an embodiment of the present invention. FIG. 9 is a side view showing an electrode assembly according to an embodiment of the present invention. FIG. 10 is a perspective view showing the electrode tab of the electrode current collector in an electrode assembly according to an embodiment of the present invention. FIG. 11 is a cross-sectional view showing a secondary battery including an electrode current collector according to an embodiment of the present invention. FIG. 12 is a perspective view showing the lamination process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 13 is a perspective view showing the tab formation process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 14 is a perspective view showing the process of inserting a tap wedge in a method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 15 is a perspective view showing the process of inserting a tap wedge through a roll in a method for manufacturing an electrode current collector according to an embodiment of the present invention. Specific details for implementing the invention
[0016] The objects, specific advantages, and novel features of the present invention will become more apparent from the following detailed description and preferred embodiments in conjunction with the accompanying drawings. It should be noted that in assigning reference numerals to the components of each drawing in this specification, the same components are assigned the same number whenever possible, even if they are shown in different drawings. Furthermore, the present invention may be embodied in various different forms and is not limited to the embodiments described herein. Also, in describing the present invention, detailed descriptions of related known technologies that could unnecessarily obscure the essence of the invention are omitted.
[0018] Electrode current collector according to the embodiment
[0020] FIG. 1 is a perspective view showing an electrode current collector according to an embodiment of the present invention, and FIG. 2 is a cross-sectional view showing a first example of an electrode tab in an electrode current collector according to an embodiment of the present invention.
[0021] Referring to FIGS. 1 and 2, an electrode current collector (110) according to an embodiment of the present invention is an electrode current collector (110) including an electrode tab (111) extended at an end, and includes a polymer layer (112) and a first metal layer (113) and a second metal layer (114) laminated on both sides of the polymer layer (112), and a metal wedge (115) is positioned on at least one of the first metal layer (113) or the second metal layer (114) at the electrode tab (111).
[0023] More specifically, the electrode current collector (110) includes an electrode tab (111) extended at the end. That is, the electrode tab (111) may be formed by notching the end of the electrode current collector (110).
[0024] Additionally, the electrode current collector (110) includes a polymer layer (112) in the stacking direction and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112). Here, the polymer layer (112) is a layer containing a polymer material, and the first metal layer (113) and the second metal layer (114) are layers containing a metal material. Accordingly, the electrode current collector (110) is provided in a form in which the first metal layer (113) and the second metal layer (114) are stacked on both sides of the polymer layer (112), thereby preventing the occurrence of fire caused by excessive current density that occurs when the material is made only of metal. In addition, the electrode current collector (110) can have a first metal layer (113) and a second metal layer (114) formed thinly on both sides, so that when breaking occurs, the risk of a short circuit caused by metal burrs, etc. may be low.
[0025] In addition, for example, the thickness of the polymer layer (112) may be 2 to 14 µm, and the thickness of the first metal layer (113) and the second metal layer (114) may be 0.2 to 3 µm.
[0027] A metal wedge (115) is positioned by being inserted into at least one of the first metal layer (113) or the second metal layer (114) from the electrode tab (111) to the polymer layer (112). At this time, the height (h1) of the metal wedge (115) inserted into the first metal layer (113) or the second metal layer (114) may be greater than the thickness (t1, t2) of the first metal layer (113) and the second metal layer (114).
[0028] Additionally, the metal wedge (115) may include a metal material. Furthermore, the metal wedge (115) may include a material identical to that of, for example, the first metal layer (113) and the second metal layer (114).
[0029] And, the metal wedge (115) may include a plurality of first metal wedges (115a) located in the first metal layer (113) and a plurality of second metal wedges (115b) located in the second metal layer (114).
[0030] Here, the first metal wedge (115a) and the second metal wedge (115b) may be positioned at a certain distance from each other.
[0031] In addition, the mutual spacing (t0) between the first metal wedge (115a) and the second metal wedge (115b) can be 2 to 10 μm.
[0032] Accordingly, the mutual spacing (t0) between the first metal wedge (115a) and the second metal wedge (115b) is formed to be greater than or equal to a lower limit value of 2 µm, thereby enabling the effect of preventing fire caused by excessive current density in the electrode current collector (110) in which the first metal layer (113) and the second metal layer (114) are laminated on both sides of the polymer layer (112). That is, the mutual spacing (t0) between the first metal wedge (115a) and the second metal wedge (115b) is formed to be greater than or equal to a lower limit value of 2 µm, so that thermal stability can be significantly improved.
[0033] Meanwhile, the mutual spacing (t0) between the first metal wedge (115a) and the second metal wedge (115b) is formed to be less than or equal to an upper limit of 10 µm, so that welding is significantly easier and conductivity can be significantly increased.
[0035] FIG. 3 is a perspective view showing one example of an electrode wedge in an electrode current collector according to an embodiment of the present invention, and FIG. 4 is a perspective view showing another example of an electrode wedge in an electrode current collector according to an embodiment of the present invention.
[0036] Meanwhile, referring to FIGS. 2 to 4, the metal wedge (115) may be provided in the shape of a pyramid or cone with its vertex facing the polymer layer (112). Here, the height (h1) and width (w1) of the metal wedge (115) may be formed to, for example, 1 to 5 μm.
[0037] Also, referring to FIG. 3, the metal wedge (115) can be formed in the shape of a pyramid, for example, having a polygonal base and a triangular side. Additionally, the metal wedge (115) can be formed specifically, for example, as a triangular pyramid or a square pyramid. Here, the metal wedge (115) can be formed more specifically, for example, as a square pyramid. At this time, the height and the width of one side (w1) of the metal wedge (115) can be formed to be, for example, 1 to 5 μm.
[0038] Additionally, referring to FIG. 4, the metal wedge (115') can be formed in the shape of a cone, having a three-dimensional shape with a circular base and a curved side. In this case, the height and diameter of the metal wedge (115) can be formed to, for example, 1 to 5 μm.
[0040] Meanwhile, referring to FIG. 2, in a first example of an electrode tab (111), a first metal wedge (115a) and a second metal wedge (115b) may be positioned parallel to each other in the stacking direction. Here, in the first example of the electrode tab (111), the thicknesses of the first metal layer (113) and the second metal layer (114) may be the same. At this time, for example, the thicknesses of the first metal layer (113) and the second metal layer (114) may be 0.5 to 1 μm.
[0042] FIG. 5 is a cross-sectional view showing a second example of an electrode tab in an electrode current collector according to an embodiment of the present invention.
[0043] Meanwhile, referring to FIG. 5, in a second example of the electrode tab (111), the first metal wedge (215a) and the second metal wedge (215b) in the metal wedge (215) may be positioned staggered relative to each other in the stacking direction. Here, in the second example of the electrode tab (111), the thicknesses of the first metal layer (113) and the second metal layer (114) may be the same. At this time, for example, the thicknesses of the first metal layer (113) and the second metal layer (114) may be 0.5 to 1 μm.
[0045] FIG. 6 is a cross-sectional view showing a third example of an electrode tab in an electrode current collector according to an embodiment, and FIG. 7 is a cross-sectional view showing a fourth example of an electrode tab in an electrode current collector according to an embodiment.
[0046] Referring to FIGS. 6 and 7, in the third and fourth examples of the electrode tab (111), the thickness (t3, t5) of the first metal layer (313, 413) and the thickness (t4, t6) of the second metal layer (314, 414) may be formed differently from each other. At this time, a metal wedge (315, 415) may be provided in the second metal layer (314, 414).
[0047] Also, referring to FIG. 6, in a third example of the electrode tab (111), the thickness (t3) of the first metal layer (313) may be formed to be thicker than the thickness (t4) of the second metal layer (314). Here, for example, the thickness (t3) of the first metal layer (313) may be 1 to 3 μm, and the thickness (t4) of the second metal layer (314) may be 0.2 to 0.5 μm. At this time, the height (h3) and width (w3) of the metal wedge (315) may be formed to be larger than the thickness (t4) of the second metal layer (314).
[0048] Meanwhile, referring to FIG. 7, as a fourth example of the electrode tab (111), the thickness (t5) of the first metal layer (413) may be formed thinner than the thickness (t6) of the second metal layer (414). Here, for example, the thickness (t5) of the first metal layer (413) may be 0.2 to 0.5 μm, and the thickness (t6) of the second metal layer (414) may be 1 to 3 μm. At this time, the height (h4) and width (w4) of the metal wedge (415) may be formed larger than the thickness (t6) of the second metal layer (414). Here, for example, the height (h4) and width (w4) of the metal wedge (415) may be 1.5 to 5 μm.
[0049] In addition, the mutual spacing (t7) between the metal wedge (415) and the first metal layer (413) can be 2 to 10 μm.
[0050] Accordingly, the mutual spacing (t7) between the metal wedge (415) and the first metal layer (413) is formed to be greater than or equal to a lower limit value of 2 µm, thereby enabling the effect of preventing fire caused by excessive current density in the electrode current collector (110) in which the first metal layer (113) and the second metal layer (114) are laminated on both sides of the polymer layer (112). That is, the mutual spacing (t7) between the metal wedge (415) and the first metal layer (413) is formed to be greater than or equal to a lower limit value of 2 µm, so that thermal stability can be significantly improved.
[0051] Meanwhile, the mutual spacing (t7) between the metal wedge (415) and the first metal layer (413) is formed to be less than or equal to an upper limit of 10 µm, so that welding is significantly easier and conductivity can be significantly increased.
[0053] Referring to FIG. 1 and FIG. 2, the electrode current collector (110) according to the embodiment of the present invention configured as described above has the effect of significantly improving weldability by inserting a metal wedge (115) into the polymer layer (112) in the metal layer located in the portion forming the electrode tab (111) in the metalized electrode current collector (110) in which a metal layer is laminated on both sides of the polymer layer (112). That is, when welding the electrode tabs (111) provided on each of the multiple electrode current collectors (110) to form an electrode assembly, and when welding the electrode tab (111) and the electrode lead, the metal wedge (115) is inserted into the polymer layer (112) in the welding portion, so that the thickness of the polymer layer (112) portion is formed thinly, and as the gap between the metal portions located on both sides of the polymer layer (112) is narrowed, the welding is significantly improved. Ultimately, when welding with a laser or ultrasound, the laser or ultrasound cannot pass through the polymer layer (112), so the weldability can be prevented.
[0055] Electrode assembly according to the embodiment
[0057] Hereinafter, an electrode assembly according to an embodiment of the invention will be described.
[0058] FIG. 8 is a cross-sectional view showing an electrode assembly according to an embodiment of the present invention, and FIG. 9 is a side view showing an electrode assembly according to an embodiment of the present invention.
[0059] Referring to FIGS. 1, 2, 8 and 9, an electrode assembly (100) according to an embodiment of the present invention is an electrode assembly (100) in which an electrode (130) and a separator (140) are alternately stacked, wherein the electrode (130) includes an electrode current collector (110) including an electrode tab (111) extended at the end, and the electrode current collector (110) includes a polymer layer (112) in the stacking direction and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112), and a metal wedge (115) is positioned from the electrode tab (111) to the polymer layer (112) by being inserted into at least one of the first metal layer (113) or the second metal layer (114).
[0060] The electrode assembly (100) according to an embodiment of the present invention relates to an electrode assembly (100) comprising an electrode current collector (110) according to the above-described embodiment. Accordingly, the present embodiment will omit or briefly describe details that overlap with the above-described embodiment and focus on describing the differences.
[0062] More specifically, the electrode assembly (100) according to an embodiment of the present invention is a power generation device capable of charging and discharging, and forms a structure in which an electrode (130) and a separator (140) are assembled and alternately stacked.
[0063] The electrode (130) includes an electrode current collector (110) that includes an electrode tab (111) extended at the end.
[0064] Here, the electrode (130) may include an electrode current collector (110) and an electrode active material (120) coated on one or both sides of the electrode current collector (110). At this time, the electrode (130) may have a retaining region where the electrode active material (120) is coated on the electrode current collector (110) and an uncoated region where the electrode active material (120) is not coated on the electrode current collector (110). At this time, an electrode tab (111) may be positioned in the uncoated region of the electrode current collector (110).
[0065] The electrode current collector (110) may include a polymer layer (112) in the stacking direction and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112). At this time, a metal wedge (115) is positioned in the electrode tab (111) and inserted into at least one of the first metal layer (113) or the second metal layer (114) up to the polymer layer (112).
[0066] Meanwhile, the polymer layer (112) may be formed from a material including, for example, PET (polyethylene terephthalate), PI (polyimide), or EN (polyethylenenaphthalate).
[0068] FIG. 10 is a perspective view showing the electrode tab of the electrode current collector in an electrode assembly according to an embodiment of the present invention.
[0069] Meanwhile, referring to FIGS. 8 to 10, the electrode assembly (100) may have a plurality of electrodes (130) and a separator (140) stacked thereon. At this time, the electrode tabs (111) of the electrode current collectors (110) provided on each of the plurality of electrodes (130) are gathered together and welded, and a metal wedge (115) may be positioned at the welded portion (P) of the electrode tabs (111). Accordingly, when welding the metalized electrode current collectors (110), the metal wedge (115) is positioned at the welded portion (P) of the electrode tabs (111), so weldability can be significantly improved. That is, weldability between the electrode tabs (111) and weldability between the electrode tabs (111) and the electrode leads can be significantly improved.
[0071] Meanwhile, the electrode (130) may include an anode (130a) and a cathode (130b). And, the separator (140) separates the anode (130a) and the cathode (130b) to electrically insulate them.
[0072] The positive electrode (130a) may include a positive electrode current collector (110a) and a positive electrode active material (120a) provided on one side of the positive electrode current collector (110a). At this time, the positive electrode (130a) may include a positive electrode non-layer, which is an area where the positive electrode active material (120a) is not laminated.
[0073] The positive active material (120a) may be composed of lithium manganese oxide, lithium cobalt oxide, lithium nickel oxide, lithium iron phosphate, or compounds and mixtures containing one or more of these.
[0074] The negative electrode (130b) may include a negative electrode current collector (110b) and a negative electrode active material (120b) provided on one side of the negative electrode current collector (110b). At this time, the negative electrode (130b) may include a negative electrode non-layer, which is an area where the negative electrode active material (120b) is not laminated.
[0075] The negative electrode active material (120b) may be composed of, for example, artificial graphite, lithium metal, lithium alloy, carbon, petroleum coke, activated carbon, graphite, silicon compound, tin compound, titanium compound, or an alloy thereof. At this time, the negative electrode active material (120b) may further include, for example, non-graphite-based SiO (silica) or SiC (silicon carbide).
[0076] Meanwhile, the positive current collector (110a) and the negative current collector (110b) may include a polymer layer (112) and a first metal layer (113) and a second metal layer (114) stacked on both sides of the polymer layer (112) in the stacking direction.
[0077] At this time, the first metal layer (113) and the second metal layer (114) located on the positive current collector (110a) may include aluminum material, and the first metal layer (113) and the second metal layer (114) located on the negative current collector (110b) may include copper material.
[0079] FIG. 11 is a cross-sectional view showing a secondary battery including an electrode current collector according to an embodiment of the present invention.
[0080] Meanwhile, referring to FIG. 11, a secondary battery (10) can be manufactured by including an electrode assembly (100) according to an embodiment of the present invention configured as above. That is, the electrode assembly (100) can be housed in a pouch (20) to form a secondary battery (10). At this time, the secondary battery (10) can be formed by further including an electrode lead (30) that is connected to the electrode assembly (100) and electrically connected to the outside of the pouch (20).
[0082] Method for manufacturing an electrode current collector according to an example
[0084] Hereinafter, a method for manufacturing an electrode current collector, which is an embodiment of the present invention, will be described.
[0085] FIG. 12 is a perspective view showing the lamination process in the method for manufacturing an electrode current collector according to an embodiment of the present invention, FIG. 13 is a perspective view showing the tab formation process in the method for manufacturing an electrode current collector according to an embodiment of the present invention, and FIG. 14 is a perspective view showing the tab wedge insertion process in the method for manufacturing an electrode current collector according to an embodiment of the present invention.
[0086] Referring to FIGS. 12 to 14, the method for manufacturing an electrode current collector according to an embodiment of the present invention comprises a lamination process of forming a laminate (S) by laminating a first metal layer (113) and a second metal layer (114) on both sides of a polymer layer (112); a tab forming process of forming an electrode tab (111) by notching an end portion of the laminate (S); and a wedge insertion process of inserting a metal wedge (115) into the polymer layer (112) from the electrode tab (111) to at least one of the first metal layer (113) or the second metal layer (114).
[0087] The method for manufacturing an electrode current collector according to an embodiment of the present invention relates to a method for manufacturing an electrode current collector that includes an electrode current collector according to the aforementioned embodiment of the present invention and an electrode assembly according to an embodiment of the present invention.
[0088] Accordingly, regarding the embodiment of the method for manufacturing an electrode current collector according to the embodiment of the present invention, details that overlap with the previously described embodiments of the present invention are omitted or described briefly, and the description focuses on the differences.
[0090] More specifically, referring to FIG. 12, the lamination process forms a laminate (S) by laminating a first metal layer (113) and a second metal layer (114) on both sides of a polymer layer (112).
[0091] Additionally, the lamination process may laminate a first metal layer (113) and a second metal layer (114) on both sides of a polymer layer (112) through deposition or lamination.
[0093] Referring to FIG. 13, the tab forming process forms an electrode tab (111) by notching the end portion of the laminate (S).
[0094] That is, the tab forming process can form an electrode tab (111) in a protruding shape by cutting one side of a laminate (S) in which a first metal layer (113) and a second metal layer (114) are laminated on both sides of a polymer layer (112).
[0095] Additionally, the tab forming process can be notched so that an electrode tab (111) is formed in the laminate (S) through a punch die or a laser.
[0097] FIG. 15 is a perspective view showing the process of inserting a tap wedge through a roll in a method for manufacturing an electrode current collector according to an embodiment of the present invention.
[0098] Referring to FIGS. 2, 14 and 15, the wedge insertion process involves inserting a metal wedge (115) into at least one of the first metal layer (113) or the second metal layer (114) from the electrode tab (111) to the polymer layer (112).
[0099] The metal wedge (115) may include a first metal wedge (115a) and a second metal wedge (115b).
[0100] Additionally, the wedge insertion process may involve inserting multiple first metal wedges (115a) into the first metal layer (113) and inserting multiple second metal wedges (115b) into the second metal layer (114).
[0101] In addition, the wedge insertion process can be performed by pressing the sheet (T) on which the metal wedge (115) is located through a roller (R) and inserting the metal wedge (115) located on the sheet (T) into at least one of the first metal layer (113) or the second metal layer (114).
[0103] Referring to FIGS. 2, FIGS. 5, and FIGS. 12, the lamination process can be performed such that the thickness (t1) of the first metal layer (113) and the thickness (t2) of the second metal layer (114) are equal to each other in the first example and the second example. Here, the lamination process can be formed by depositing the first metal layer (113) and the second metal layer (114) on both sides of the polymer layer (112).
[0104] At this time, referring to FIG. 2, the stacking process may, as a first example, position the first metal wedge (115a) and the second metal wedge (115b) side by side in the stacking direction.
[0105] Meanwhile, referring to FIG. 5, in the stacking process, as a second example, the first metal wedge (215a) and the second metal wedge (215b) can be positioned alternately in the stacking direction in the metal wedge (215).
[0107] Additionally, referring to FIGS. 6 and 7, the lamination process can be performed in the third and fourth examples such that the thickness (t3, t5) of the first metal layer (313, 413) and the thickness (t4, t6) of the second metal layer (314, 414) are different from each other. Additionally, the lamination process can form the layer with a relatively thin thickness among the first metal layer (313, 413) and the second metal layer (314, 414) through deposition, and the layer with a relatively thick thickness through lamination by applying heat and pressure.
[0108] Here, referring to FIG. 6, the lamination process is a third example in which the thickness (t3) of the first metal layer (313) can be formed thicker than the thickness (t4) of the second metal layer (314). At this time, the wedge insertion process can insert a metal wedge (315) into the second metal layer (314).
[0109] Meanwhile, referring to FIG. 7, the lamination process can be formed such that the thickness (t5) of the first metal layer (413) is thinner than the thickness (t6) of the second metal layer (414) as a fourth example. At this time, the wedge insertion process can insert a metal wedge into the second metal layer (414). Here, the wedge insertion process can be performed by using a metal wedge (415) that has a height (h4) greater than the thickness (t6) of the second metal layer (414) to insert it into the second metal layer (414).
[0111] Although the present invention has been described in detail through specific embodiments, this is for the purpose of specifically explaining the invention and the invention is not limited thereto. It should be understood that various implementations are possible by those skilled in the art within the technical scope of the present invention.
[0112] In addition, the specific scope of protection of the invention will be clarified by the appended patent claims. Explanation of the symbols
[0114] 10: Secondary battery 20: Pouch 30: Electrode Lead 100: Electrode assembly 110: Electrode current collector 110a: Positive current collector 110b: Cathode current collector 111: Electrode tab 112: Polymer layer 113, 313, 413: First metal layer 114, 314, 414: Second metal layer 115, 115', 215, 315, 415: Metal wedge 115a, 215a: First metal wedge 115b, 215b: Second metal wedge 120: Electrode active material 120a: Positive active material 120b: Cathode active material 130: Electrode 130a: Anode 130b: Cathode 140: Separator P: Welding area R: Roller S: Laminate T: Sheet
Claims
Claim 1 An electrode current collector comprising an electrode tab extended at an end, the electrode current collector comprising a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein a metal wedge is positioned at the electrode tab and inserted into at least one of the first metal layer or the second metal layer up to the polymer layer, the metal wedge comprises a plurality of first metal wedges positioned in the first metal layer and a plurality of second metal wedges positioned in the second metal layer, and the mutual spacing between the first metal wedges and the second metal wedges is 2 to 10 μm. Claim 2 An electrode current collector according to claim 1, wherein the thickness of the polymer layer is 2 to 14 μm, and the thickness of the first metal layer and the second metal layer is 0.2 to 3 μm. Claim 3 In claim 2, the first metal wedge and the second metal wedge are electrode current collectors positioned parallel to each other in the stacking direction. Claim 4 In claim 2, the first metal wedge and the second metal wedge are electrode current collectors positioned at a certain distance apart from each other. Claim 5 delete Claim 6 delete Claim 7 An electrode current collector according to claim 1, wherein the thickness of the first metal layer and the thickness of the second metal layer are formed differently from each other. Claim 8 delete Claim 9 delete Claim 10 delete Claim 11 In claim 1, the metal wedge is an electrode current collector provided in the shape of a pyramid or cone with a vertex facing the polymer layer. Claim 12 An electrode assembly having an electrode and a separator alternately stacked, wherein the electrode includes an electrode current collector including an electrode tab extended at an end, the electrode current collector includes a polymer layer in the stacking direction and a first metal layer and a second metal layer stacked on both sides of the polymer layer, and a metal wedge is positioned at the electrode tab to be inserted into at least one of the first metal layer or the second metal layer up to the polymer layer, the metal wedge includes a plurality of first metal wedges located in the first metal layer and a plurality of second metal wedges located in the second metal layer, and the mutual spacing between the first metal wedges and the second metal wedges is 2 to 10 μm. Claim 13 In claim 12, the electrode assembly comprises a plurality of electrodes and a separator stacked thereon, electrode tabs of the electrode current collectors each provided on the plurality of electrodes are gathered together and welded, and the metal wedge is positioned at the welded portion of the electrode tabs. Claim 14 A method for manufacturing an electrode current collector, comprising: a lamination process of laminating a first metal layer and a second metal layer on both sides of a polymer layer to form a laminate; a tab forming process of notching an end portion of the laminate to form an electrode tab; and a wedge insertion process of inserting a metal wedge into at least one of the first metal layer or the second metal layer from the electrode tab to the polymer layer, wherein the metal wedge comprises a first metal wedge and a second metal wedge, and the wedge insertion process involves inserting a plurality of the first metal wedges into the first metal layer and inserting a plurality of the second metal wedges into the second metal layer, wherein the mutual spacing between the first metal wedges and the second metal wedges is 2 to 10 μm. Claim 15 A method for manufacturing an electrode current collector according to claim 14, wherein the lamination process is formed by depositing the first metal layer and the second metal layer on both sides of the polymer layer. Claim 16 In claim 14, the lamination process is a method for manufacturing an electrode current collector in which the thicknesses of the first metal layer and the second metal layer are different from each other. Claim 17 A method for manufacturing an electrode current collector according to claim 16, wherein the lamination process forms a layer with a relatively thin thickness among the first metal layer and the second metal layer through deposition, and forms a layer with a relatively thick thickness through lamination by applying heat and pressure. Claim 18 delete Claim 19 A method for manufacturing an electrode current collector according to claim 14, wherein the wedge insertion process presses a sheet on which the metal wedge is located through a roller and inserts the metal wedge located on the sheet into at least one of the first metal layer or the second metal layer. Claim 20 A method for manufacturing an electrode current collector according to claim 14, wherein the thickness of the polymer layer is 2 to 14 μm, and the thickness of the first metal layer and the second metal layer is 0.2 to 3 μm.
Citation Information
Patent Citations
Method for preparing crude cell for lithium secondary battery
KR1020170052302A
Electrical collector body of secondary battery and secondary battery
KR1020220145281A
Manufacturing Method of Electrode Assembly and Electrode Assembly By Using The Same
KR1020230068521A
Current collectors comprising metallised films
WO2022238713A1