Electrode current collector, electrode assembly including the electrode current collector, and method for manufacturing the electrode current collector
The electrode current collector with a polymer-layered metal structure and metal rib improves weldability and safety in secondary batteries by addressing weldability and safety issues through enhanced electrical insulation and reduced short circuit risks.
Patent Information
- Application Number
- KR1020240108651
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2023-08-17
- Filing Date
- 2024-08-13
- Publication Date
- 2026-11-06
- Estimated Expiration
- 2044-08-13
AI Technical Summary
Existing electrode current collectors in secondary batteries face challenges with weldability and safety, particularly due to issues with electrical shorts and high current density, which can lead to safety hazards.
The electrode current collector is designed with a polymer layer sandwiched between two metal layers, featuring a metal rib extending from the first metal layer to the polymer layer, enhancing weldability and safety by reducing the risk of short circuits and improving electrical insulation.
This design significantly improves weldability between electrode tabs and leads, while maintaining high energy density and safety by preventing excessive current density and reducing the risk of fires, thus enhancing the overall stability of the battery.
Smart Images

Figure 112024088356471-PAT00002_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to an electrode current collector, an electrode assembly including an electrode current collector, and a method for manufacturing an electrode current collector. Background Technology
[0003] Unlike primary batteries, secondary batteries are rechargeable and have been the subject of extensive research and development in recent years due to their potential for miniaturization and high capacity. As technological development and demand for electric vehicles, energy storage systems (ESS), and mobile devices increase, the demand for secondary batteries as an energy source is rapidly rising. However, the safety of secondary batteries is failing to keep pace with the speed of technological advancement. To address this, methods to improve safety include creating an electrical short circuit to drain energy or short-circuiting electrical connections before abnormal behavior occurs.
[0004] Secondary batteries are classified into coin batteries, cylindrical batteries, prismatic batteries, and pouch batteries according to the shape of the battery case. In secondary batteries, the electrode assembly mounted inside the battery case is a rechargeable power generation device consisting of a laminated structure of electrodes and separators.
[0005] Electrode assemblies can be roughly classified into a jelly-roll type, which is wound with a separator interposed between sheet-type positive and negative electrodes coated with an active material on a current collector; a stack type, which is sequentially stacked with a plurality of positive and negative electrodes interposed with a separator; and a stack / folding type, which is wound with stack-type unit cells into a long separating film. The problem to be solved
[0007] One aspect of the present invention is to provide an electrode current collector with improved weldability, an electrode assembly including the electrode current collector, and a method for manufacturing the electrode current collector. means of solving the problem
[0009] An electrode current collector according to an embodiment of the present invention is an electrode current collector comprising an electrode tab extended at an end, and comprises a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein, in the electrode tab, the first metal layer may be provided with a metal rib extending to the polymer layer.
[0010] In addition, an electrode assembly according to an embodiment of the present invention is an electrode assembly in which an electrode and a separator are alternately stacked, wherein the electrode comprises an electrode current collector including an electrode tab extended at an end, and the electrode current collector comprises a polymer layer in the stacking direction and a first metal layer and a second metal layer stacked on both sides of the polymer layer, and a metal rib extending from the electrode tab to the first metal layer to the polymer layer may be provided.
[0011] In addition, the method for manufacturing an electrode current collector according to an embodiment of the present invention may include a rib forming process for forming a metal rib extending in a stacking direction on a first metal layer; a polymer stacking process for stacking a polymer layer on the first metal layer after the rib forming process; a second metal layer stacking process for forming a laminate by stacking a second metal layer on the polymer layer after the polymer stacking process; and a tab forming process for forming an electrode tab by notching an end portion of the laminate. Effects of the invention
[0013] According to the present invention, in an electrode current collector in which metal layers are laminated on both sides of a polymer layer, a metal layer located in the portion forming the electrode tab is provided with a metal rib extending toward the polymer layer, thereby having the effect of significantly improving weldability. Furthermore, as a result, the welding between the electrode tabs of the electrode current collector and the weldability between the electrode tab and the electrode lead are significantly improved. Brief explanation of the drawing
[0015] FIG. 1 is a perspective view showing an electrode current collector according to an embodiment of the present invention. FIG. 2 is a cross-sectional view showing a first example of an electrode current collector according to an embodiment of the present invention. FIG. 3 is a perspective view of a key part showing an example of an electrode current collector according to an embodiment of the present invention. FIG. 4 is a perspective view of a key part showing another example of an electrode current collector according to an embodiment of the present invention. FIG. 5 is a cross-sectional view showing a second example of an electrode current collector according to an embodiment of the present invention. FIG. 6 is a cross-sectional view showing an electrode assembly according to an embodiment of the present invention. FIG. 7 is a side view showing an electrode assembly according to an embodiment of the present invention. FIG. 8 is a cross-sectional view showing a secondary battery including an electrode current collector according to an embodiment of the present invention. FIG. 9 is a cross-sectional view showing the rib formation process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 10 is a cross-sectional view showing the polymer lamination process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 11 is a cross-sectional view showing the second metal layer stacking process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 12 is a perspective view showing an example of a rib formation process and a polymer lamination process in a method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 13 is a perspective view showing another example of the rib formation process and the polymer lamination process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 14 is a perspective view showing the second metal layer stacking process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 15 is a perspective view showing the tab formation process in the method for manufacturing an electrode current collector according to an embodiment of the present invention. Specific details for implementing the invention
[0016] The objects, specific advantages, and novel features of the present invention will become more apparent from the following detailed description and preferred embodiments in conjunction with the accompanying drawings. It should be noted that in assigning reference numerals to the components of each drawing in this specification, the same components are assigned the same number whenever possible, even if they are shown in different drawings. Furthermore, the present invention may be embodied in various different forms and is not limited to the embodiments described herein. Also, in describing the present invention, detailed descriptions of related known technologies that could unnecessarily obscure the essence of the invention are omitted.
[0018] Electrode current collector according to the embodiment
[0020] FIG. 1 is a perspective view showing an electrode current collector according to an embodiment of the present invention, and FIG. 2 is a cross-sectional view showing an electrode current collector according to an embodiment of the present invention.
[0021] Referring to FIG. 1 and FIG. 2, an electrode current collector (110) according to an embodiment of the present invention is an electrode current collector (110) including an electrode tab (111) extended at the end, and includes a polymer layer (112) and a first metal layer (114) and a second metal layer (113) laminated on both sides of the polymer layer (112), and in the electrode tab (111), the first metal layer (114) is provided with a metal rib (115) that extends to the polymer layer (112).
[0023] More specifically, the electrode current collector (110) includes an electrode tab (111) extended at the end. That is, the electrode tab (111) may be formed by notching the end of the electrode current collector (110).
[0024] Additionally, the electrode current collector (110) includes a polymer layer (112) in the stacking direction (D) and a first metal layer (114) and a second metal layer (113) stacked on both sides of the polymer layer (112). Here, the polymer layer (112) is a layer containing a polymer material, and the first metal layer (114) and the second metal layer (113) are layers containing a metal material. Accordingly, the electrode current collector (110) is provided in a form in which the first metal layer (114) and the second metal layer (113) are stacked on both sides of the polymer layer (112), thereby preventing the occurrence of fire caused by excessive current density that occurs when the material is made only of metal. In addition, the electrode current collector (110) can have a first metal layer (114) and a second metal layer (113) formed thinly on both sides, so that when breaking occurs, the risk of a short circuit caused by metal burrs, etc. may be low.
[0025] In addition, for example, the thickness (t3) of the polymer layer (112) can be 2 to 14 µm.
[0026] And, for example, the thickness (t1, t2) of the first metal layer (114) and the second metal layer (113) may be 0.2 to 3 µm. Here, specifically, for example, the thickness (t1, t2) of the first metal layer (114) and the second metal layer (113) may be 0.2 to 2 µm.
[0027] Accordingly, the thickness (t1, t2) of the first metal layer (114) and the second metal layer (113) can be formed to be greater than or equal to a lower limit value of 0.2 µm, so that the electrical resistivity can be low. Accordingly, the function as an electrical connection, which is a required characteristic of the electric current collector foil, can be not limited. In other words, the function as a battery can be not weakened.
[0028] Meanwhile, the thickness (t1, t2) of the first metal layer (114) and the second metal layer (113) is formed to be less than or equal to an upper limit of 2 µm, so that the energy density can be high. In addition, the adverse effect on safety enhancement through electrical insulation during a nail test, which is a disadvantage of conventional metal foil, can be significantly reduced. Specifically, an electrode current collector (110) is provided in a form in which the first metal layer (114) and the second metal layer (113) are laminated on both sides of a polymer layer (112), so that safety enhancement through electrical insulation can be enhanced by the collapse of the first metal layer (114) and the second metal layer (113) due to the shrinkage of the polymer layer during a nail test, but if the first metal layer (114) and the second metal layer (113) are too thick, the polymer layer (112) cannot perform the safety enhancement function, and safety may deteriorate. Accordingly, the thickness (t1, t2) of the first metal layer (114) and the second metal layer (113) is formed to be less than or equal to an upper limit of 2 µm, so that the polymer layer (112) containing the polymer material can perform a stability enhancement function. Here, the nail test is a test of stability by penetrating with a nail.
[0029] Meanwhile, the thickness (t1) of the first metal layer (114) may be the same as, for example, the thickness (t2) of the second metal layer (113).
[0030] Additionally, the thickness (t1) of the first metal layer (114) may be thicker than the thickness (t2) of the second metal layer (113), as in another example. Accordingly, the manufacturing of the electrode current collector (110) may be easy.
[0032] The metal rib (115)(rib) may be provided to extend from the first metal layer (114) to the polymer layer (112) at the electrode tab.
[0033] Additionally, the metal rib (115) may protrude from the inner surface of the first metal layer (114) into the polymer layer (112) and may be formed along the inner surface of the first metal layer (114).
[0034] In addition, the metal rib (115) may include the same material as the first metal layer (114) and the second metal layer (113).
[0036] FIG. 3 is a partial perspective view showing one example of an electrode current collector according to an embodiment of the present invention, and FIG. 4 is a partial perspective view showing another example of an electrode current collector according to an embodiment of the present invention.
[0037] Referring to FIG. 3, the metal ribs (115) may be formed in the shape of a rectangular wall, for example, and may be provided in multiple numbers at regular intervals.
[0038] Referring to FIG. 4, the metal ribs (115') may be provided in the form of multiple cylinders as another example.
[0040] Meanwhile, referring to FIG. 2, as a first example of an electrode current collector (110), the end of the metal rib (115) may be spaced apart from the second metal layer (113) at a certain distance.
[0041] Accordingly, the end of the metal rib (115) is spaced apart from the second metal layer (113) at a certain distance, so that the first metal layer (114) and the second metal layer (113) are not connected, thereby maintaining the stability effect of the metalized electrode current collector (110) in which metal layers are laminated on both sides of the polymer layer (112).
[0042] Additionally, the spacing between the end of the metal rib (115) and the second metal layer (113) can be 2 to 8 μm. Accordingly, the mutual spacing (t0) between the end of the metal rib (115) and the second metal layer (113) is formed to be greater than or equal to the lower limit value of 2 μm, thereby significantly improving thermal stability. Meanwhile, the mutual spacing (t0) between the end of the metal rib (115) and the second metal layer (113) is formed to be less than or equal to the upper limit value of 8 μm, thereby making welding significantly easier.
[0044] FIG. 5 is a cross-sectional view showing a second example of an electrode current collector according to an embodiment of the present invention.
[0045] Additionally, referring to FIG. 5, as a second example of the electrode current collector (210), the end of the metal rib (115) can come into contact with the second metal layer (113). Accordingly, the electrical resistivity can be lowered.
[0047] Meanwhile, referring to FIGS. 1 and 2, the electrode current collector (110) may include a body (116) on which an electrode active material is coated on the outer surface, and an electrode tab (111) extending from the body (116). At this time, a metal rib (115) may be further provided on the body (116). That is, a metal rib (115) may be provided so as to extend to a polymer layer (112) in a first metal layer (114) located on the body (116) and the electrode tab (111) in the electrode current collector (110).
[0049] Referring to FIG. 1 and FIG. 2, the electrode current collector (110) according to the embodiment of the present invention configured as described above is provided with a metal rib (115) extending toward the polymer layer (112) in the metal layer located in the portion forming the electrode tab (111) in the electrode current collector (110) in which a metal layer is laminated on both sides of the polymer layer (112), thereby having the effect of significantly improving weldability. That is, when welding the electrode tabs (111) provided on each of the multiple electrode current collectors (110) to each other and welding the electrode tab (111) and the electrode lead to form an electrode assembly, the metal rib (115) extends toward the polymer layer (112) in the welding portion, so that the thickness of the polymer layer (112) located in the welding portion is formed thinly, and as the gap between the first and second metal layers (114, 113) is narrowed, the effect of welding is significantly improved. Ultimately, when welding with a laser or ultrasound, the laser or ultrasound cannot pass through the polymer layer (112), so the weldability can be prevented.
[0051] Electrode assembly according to the embodiment
[0053] Hereinafter, an electrode assembly according to an embodiment of the invention will be described.
[0054] FIG. 6 is a cross-sectional view showing an electrode assembly according to an embodiment of the present invention, and FIG. 7 is a side view showing an electrode assembly according to an embodiment of the present invention.
[0055] Referring to FIGS. 1, FIGS. 2, FIGS. 5 and FIGS. 6, an electrode assembly (100) according to an embodiment of the present invention is an electrode assembly (100) in which an electrode (130) and a separator (140) are alternately stacked, wherein the electrode (130) includes an electrode current collector (110) including an electrode tab (111) extended at the end, and the electrode current collector (110) includes a polymer layer (112) and a first metal layer (114) and a second metal layer (113) stacked on both sides of the polymer layer (112) in the stacking direction (D), and a metal rib extending from the electrode tab (111) to the first metal layer (114) to the polymer layer (112) is provided.
[0056] The electrode assembly (100) according to an embodiment of the present invention relates to an electrode assembly (100) including an electrode current collector according to the above-described embodiment. Accordingly, the present embodiment will omit or briefly describe details that overlap with the above-described embodiment and focus on describing the differences.
[0058] More specifically, the electrode assembly (100) according to an embodiment of the present invention is a power generation device capable of charging and discharging, and forms a structure in which an electrode (130) and a separator (140) are assembled and alternately stacked.
[0059] The electrode (130) includes an electrode current collector (110) that includes an electrode tab (111) extended at the end.
[0060] Here, the electrode (130) may include an electrode current collector (110) and an electrode active material (120) coated on one or both sides of the electrode current collector (110). At this time, the electrode (130) may have a retaining region where the electrode active material (120) is coated on the electrode current collector (110) and an uncoated region where the electrode active material (120) is not coated on the electrode current collector (110). At this time, an electrode tab (111) may be positioned in the uncoated region of the electrode current collector (110).
[0061] The electrode current collector (110) may include a polymer layer (112) in the stacking direction (D) and a first metal layer (114) and a second metal layer (113) stacked on both sides of the polymer layer (112). At this time, a metal rib (115) extending from the electrode tab (111) to the polymer layer (112) in the first metal layer (114) is provided.
[0062] Meanwhile, the polymer layer (112) may be formed from a material including, for example, PET (polyethylene terephthalate), PI (polyimide), or EN (polyethylenenaphthalate).
[0064] FIG. 8 is a cross-sectional view showing a secondary battery including an electrode current collector according to an embodiment of the present invention.
[0065] Meanwhile, referring to FIGS. 5 to 8, the electrode assembly (100) may have a plurality of electrodes (130) and a separator (140) stacked thereon. At this time, the electrode tabs (111) of the electrode current collectors (110) provided on each of the plurality of electrodes (130) are gathered together and welded, and the metal ribs (115) may be positioned at the welded portion (R) of the electrode tabs (111). At this time, the electrode lead (30) may be welded together at the welded portion (R). Accordingly, when welding the metalized electrode current collectors (110), the metal ribs (115) are positioned at the welded portion (R) of the electrode tabs (111), so that weldability can be significantly improved. That is, the weldability between the electrode tabs (111) and the weldability between the electrode tabs (111) and the electrode lead (30) can be significantly improved.
[0067] Meanwhile, the electrode (130) may include an anode (130a) and a cathode (130b). And, the separator (140) separates the anode (130a) and the cathode (130b) to electrically insulate them.
[0068] The positive electrode (130a) may include a positive electrode current collector (110a) and a positive electrode active material (120a) provided on one side of the positive electrode current collector (110a). At this time, the positive electrode (130a) may include a positive electrode non-layer, which is an area where the positive electrode active material (120a) is not laminated.
[0069] The positive active material (120a) may be composed of lithium manganese oxide, lithium cobalt oxide, lithium nickel oxide, lithium iron phosphate, or compounds and mixtures containing one or more of these.
[0070] The negative electrode (130b) may include a negative electrode current collector (110b) and a negative electrode active material (120b) provided on one side of the negative electrode current collector (110b). At this time, the negative electrode (130b) may include a negative electrode non-layer, which is an area where the negative electrode active material (120b) is not laminated.
[0071] The negative electrode active material (120b) may be composed of, for example, artificial graphite, lithium metal, lithium alloy, carbon, petroleum coke, activated carbon, graphite, silicon compound, tin compound, titanium compound, or an alloy thereof. At this time, the negative electrode active material (120b) may further include, for example, non-graphite-based SiO (silica) or SiC (silicon carbide).
[0072] Meanwhile, the positive current collector (110a) and the negative current collector (110b) may include a polymer layer (112) and a first metal layer (114) and a second metal layer (113) stacked on both sides of the polymer layer (112) in the stacking direction (D).
[0073] At this time, the first metal layer (114) and the second metal layer (113) located on the positive current collector (110a) may include aluminum material, and the first metal layer (114) and the second metal layer (113) located on the negative current collector (110b) may include copper material.
[0075] Meanwhile, referring to FIG. 2, as a first example, the metal rib (115) extends from the first metal layer (114) to the polymer layer (112), and the end of the metal rib (115) may be spaced apart from the second metal layer (113) at a certain distance.
[0076] Referring to FIG. 5, in a second example, the metal rib (115) extends from the first metal layer (114) to the polymer layer (112), and the end of the metal rib (115) can come into contact with the second metal layer (113).
[0078] Meanwhile, referring to FIG. 8, a secondary battery (10) can be manufactured by including an electrode assembly (100) according to an embodiment of the present invention configured as above. That is, the electrode assembly (100) can be housed in a pouch (20) to form a secondary battery (10). At this time, the secondary battery (10) can be formed by further including an electrode lead (30) that is connected to the electrode assembly (100) and electrically connected to the outside of the pouch (20).
[0080] Method for manufacturing an electrode current collector according to an example
[0082] Hereinafter, a method for manufacturing an electrode current collector according to an embodiment of the present invention will be described.
[0083] FIG. 9 is a cross-sectional view showing the rib formation process in the method for manufacturing an electrode current collector according to an embodiment of the present invention, FIG. 10 is a cross-sectional view showing the polymer lamination process in the method for manufacturing an electrode current collector according to an embodiment of the present invention, and FIG. 11 is a cross-sectional view showing the second metal layer lamination process in the method for manufacturing an electrode current collector according to an embodiment of the present invention.
[0084] Referring to FIGS. 9 to 11, the method for manufacturing an electrode current collector according to an embodiment of the present invention is a method for manufacturing an electrode current collector and includes a rib forming process in which a metal rib (115) extending in the stacking direction (D) is formed on a first metal layer (114); a polymer stacking process in which a polymer layer (112) is stacked on the first metal layer (114) after the rib forming process; a second metal layer stacking process in which a second metal layer (113) is stacked on the polymer layer (112) after the polymer stacking process to form a stack (S); and a tab forming process in which an electrode tab (111) is formed by notching an end portion of the stack (S).
[0085] The method for manufacturing an electrode current collector according to an embodiment of the present invention relates to a method for manufacturing an electrode current collector that includes an electrode current collector included in an electrode assembly according to an embodiment of the present invention and an electrode current collector according to an embodiment of the present invention.
[0086] Accordingly, regarding the embodiment of the method for manufacturing an electrode current collector according to the embodiment of the present invention, details that overlap with the previously described embodiments of the present invention are omitted or described briefly, and the description focuses on the differences.
[0088] FIG. 12 is a perspective view showing an example of a rib formation process and a polymer lamination process in a method for manufacturing an electrode current collector according to an embodiment of the present invention. FIG. 13 is a perspective view showing another example of a rib formation process and a polymer lamination process in a method for manufacturing an electrode current collector according to an embodiment of the present invention.
[0089] More specifically, referring to FIGS. 9, 12, and 13, the rib forming process forms a metal rib (115) (rib) extending in the stacking direction (D) on the first metal layer (114).
[0090] Additionally, the rib formation process can form a metal rib (115) by etching one side of the first metal layer (114). At this time, the rib formation process can form a metal rib (115) having a cross-section corresponding to the pattern hole formed in the mask by stacking a mask with a pattern hole formed on one side of the first metal layer (114) and then pouring an etching solution onto the upper part of the mask so that the etching solution penetrates the part where the pattern hole is formed and etches one side of the first metal layer (114).
[0091] In addition, the rib forming process can form metal ribs (115, 115') into multiple wall-like or cylindrical shapes.
[0092] For example, the rib formation process can form a metal rib (115) in the area where the electrode tab (111) is formed on one side of the first metal layer (114).
[0093] As another example, the rib formation process can form metal ribs (115) over the entire surface of one side of the first metal layer (114).
[0095] Referring to FIG. 10, the polymer lamination process laminates a polymer layer (112) onto a first metal layer (114) after the rib formation process.
[0096] Referring to FIG. 2 and FIG. 10, the polymer lamination process can form a polymer layer (112) by pouring a polymer onto one side of a first metal layer (114) so that it has a thickness greater than the height (h1) in the lamination direction (D) of the metal rib (115) as a first example.
[0097] Referring to FIG. 5, the polymer lamination process can form a polymer layer (112) by pouring a polymer onto one side of the first metal layer (114) so that the polymer layer has a thickness corresponding to the height in the lamination direction (D) of the metal rib (115) as a second example. That is, the polymer lamination process can form the polymer layer (112) such that its thickness (t4) is equal to the height in the lamination direction (D) of the metal rib (115).
[0099] FIG. 14 is a perspective view showing the second metal layer stacking process in the method for manufacturing an electrode current collector according to an embodiment of the present invention.
[0100] Referring to FIGS. 11 and 14, the second metal layer lamination process forms a laminate (S) by laminating a second metal layer (113) onto a polymer layer (112) after the polymer lamination process.
[0101] Additionally, the second metal layer deposition process can deposit a second metal layer (113) by depositing metal on one surface of the polymer layer (112). Here, the second metal layer deposition process can deposit metal on one surface of the polymer layer (112) through a PVD (Physical Vapor Deposition) deposition method.
[0103] FIG. 15 is a perspective view showing the tab formation process in the method for manufacturing an electrode current collector according to an embodiment of the present invention.
[0104] Referring to FIG. 15, the tab forming process can form an electrode tab (111) by notching the end portion of the laminate (S).
[0105] That is, the tab forming process can form an electrode tab (111) in a protruding shape by cutting one side of a laminate (S) in which a first metal layer (114) and a second metal layer (113) are laminated on both sides of a polymer layer (112).
[0106] Additionally, the tab forming process can be notched so that an electrode tab (111) is formed in the laminate (S) through a punch die or a laser.
[0108] Although the present invention has been described in detail through specific embodiments, this is for the purpose of specifically explaining the invention and the invention is not limited thereto. It should be understood that various implementations are possible by those skilled in the art within the technical scope of the present invention.
[0109] In addition, the specific scope of protection of the invention will be clarified by the appended patent claims. Explanation of the symbols
[0111] 10: Secondary battery 20: Pouch 30: Electrode Lead 100: Electrode assembly 110,210: Electrode current collector 110a: Positive current collector 110b: Cathode current collector 111: Electrode tab 112: Polymer layer 113: Second metal layer 114: First metal layer 115, 115': Metal rib 116: Body 120: Electrode active material 120a: Positive active material 120b: Cathode active material 130: Electrode 130a: Anode 130b: Cathode 140: Separator D: Stacking direction R: Welding area S: Laminate
Claims
Claim 1 An electrode current collector comprising an electrode tab extending at an end, the electrode current collector comprising a polymer layer and a first metal layer and a second metal layer laminated on both sides of the polymer layer, wherein at the electrode tab, the first metal layer is provided with a metal rib extending to the polymer layer, the metal rib protrudes from the inner surface of the first metal layer into the polymer layer, is formed along the inner surface of the first metal layer, is formed in a rectangular wall shape, is provided in multiple numbers at regular intervals, and the end of the metal rib is spaced at a regular interval from the second metal layer. Claim 2 delete Claim 3 delete Claim 4 delete Claim 5 delete Claim 6 An electrode current collector according to claim 1, wherein the distance between the end of the metal rib and the second metal layer is 2 to 8 μm. Claim 7 delete Claim 8 The electrode current collector according to claim 1 or claim 6, wherein the electrode current collector comprises a body on which an electrode active material is coated on an outer surface; and the electrode tab extending from the body, and the metal rib further provided on the body. Claim 9 An electrode assembly having an electrode and a separator alternately stacked, wherein the electrode includes an electrode current collector having an electrode tab extended at an end, and the electrode current collector includes a polymer layer in the stacking direction and a first metal layer and a second metal layer stacked on both sides of the polymer layer, and a metal rib extending from the electrode tab to the first metal layer to the polymer layer is provided, wherein the metal rib protrudes from the inner surface of the first metal layer to the polymer layer, is formed along the inner surface of the first metal layer, is formed in a rectangular wall shape, is provided in multiple numbers at regular intervals, and the end of the metal rib is spaced at a regular interval from the second metal layer. Claim 10 A method for manufacturing an electrode current collector, comprising: a rib forming process for forming a metal rib extending in the stacking direction on a first metal layer; a polymer stacking process for stacking a polymer layer on the first metal layer after the rib forming process; a second metal layer stacking process for forming a laminate by stacking a second metal layer on the polymer layer after the polymer stacking process; and a tab forming process for forming an electrode tab by notching an end portion of the laminate. The rib forming process forms the metal rib in an area where the electrode tab is formed on one surface of the first metal layer, and forms the metal rib in the form of a plurality of walls. The metal rib protrudes from the inner surface of the first metal layer into the polymer layer, is formed along the inner surface of the first metal layer, and is provided in a plurality at regular intervals. The polymer stacking process forms the polymer layer by pouring the polymer onto one surface of the first metal layer so as to have a thickness greater than the height of the metal rib in the stacking direction. Claim 11 In claim 10, the rib forming process is a method for manufacturing an electrode current collector in which one surface of the first metal layer is etched to form the metal rib. Claim 12 delete Claim 13 delete Claim 14 delete Claim 15 In claim 10, the second metal layer lamination process is a method for manufacturing an electrode current collector by depositing metal on one surface of the polymer layer to laminate the second metal layer. Claim 16 delete Claim 17 delete
Citation Information
Patent Citations
Electrical collector body of secondary battery and secondary battery
KR1020220145281A
Manufacturing Method of Electrode Assembly and Electrode Assembly By Using The Same
KR1020230068521A
Current collectors comprising metallised films