Semiconductor memory device
A three-dimensional semiconductor memory device with a stacked structure and connected bonding pads addresses integration density and reliability issues, enhancing connectivity and simplifying wiring in semiconductor devices.
Patent Information
- Application Number
- KR1020220038356
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-03-28
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2042-03-28
AI Technical Summary
Existing two-dimensional semiconductor devices face limitations in integration density and reliability due to the need for expensive equipment for pattern miniaturization, while three-dimensional semiconductor memory devices offer a potential solution but require improved connectivity and wiring structures.
A semiconductor memory device with a stacked structure of word lines and interlayer insulating films, featuring a step structure and parallel sub-gate electrodes, along with a cell array and peripheral circuit structure connected by bonding pads, allowing for improved integration density and simplified wiring.
The solution enhances integration density and reliability by facilitating the connection of memory cells and peripheral circuits, simplifying the wiring structure, and improving the bonding process.
Smart Images

Figure 112022033436827-PAT00002_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a semiconductor device and a semiconductor memory device including the same, and more specifically, to a three-dimensional semiconductor memory device with improved reliability and integration density. Background Technology
[0002] In order to meet the superior performance and low price demands of consumers, it is required to increase the integration density of semiconductor devices. Since the integration density of semiconductor devices is a critical factor in determining product prices, particularly increased integration density is required. In the case of two-dimensional or planar semiconductor devices, the integration density is primarily determined by the area occupied by a unit memory cell, and thus is significantly influenced by the level of fine pattern formation technology. However, because ultra-expensive equipment is required for pattern miniaturization, the integration density of two-dimensional semiconductor devices is increasing but remains limited. Accordingly, three-dimensional semiconductor memory devices equipped with memory cells arranged in three dimensions are being proposed. The problem to be solved
[0003] The problem that the present invention aims to solve is to provide a semiconductor memory device with improved reliability and integration density.
[0004] The problems that the present invention aims to solve are not limited to those mentioned above, and other unmentioned problems will be clearly understood by those skilled in the art from the description below. means of solving the problem
[0005] To achieve the above-mentioned problem, a semiconductor memory device according to embodiments of the present invention comprises: a lower film including a first region and a second region; and a stacked structure including word lines and interlayer insulating films alternately stacked in a direction perpendicular to the upper surface of the lower film, wherein the stacked structure comprises having a step structure in the second region, the word lines extend along a first direction from the first region to the second region, and each of the word lines includes a pad in the second region, wherein each of the word lines may include sub-gate electrodes extending parallel to each other in the first region and a pad commonly connected to the sub-gate electrodes in the second region.
[0006] To achieve the above-mentioned problem, a semiconductor memory device according to embodiments of the present invention may include: a lower film comprising a first region and a second region; a stacked structure comprising word lines and interlayer insulating films alternately stacked in a direction perpendicular to the upper surface of the lower film, wherein each of the word lines has a pad in the second region, and the stacked structure has a step structure in the second region; channel patterns stacked in the vertical direction across the word lines; bit lines extending in the vertical direction across the word lines in the first region and connected to first ends of the channel patterns; data storage elements connected to second ends of the channel patterns in the first region; and cell contact plugs each connected to the pads of the word lines in the second region.
[0007] To achieve the above-mentioned problem, a semiconductor memory device according to embodiments of the present invention may include: a cell array structure including a memory cell array comprising memory cells arranged in three dimensions and first bonding pads connected to the memory cell array; and a peripheral circuit structure including peripheral circuits and second bonding pads connected to the peripheral circuits and bonded to the first bonding pads, wherein the cell array structure comprises: a lower film including a first region and a second region; a stacked structure including word lines and interlayer insulating films alternately stacked in a direction perpendicular to the upper surface of the lower film, wherein each of the word lines has a pad in the second region, and the stacked structure has a step structure in the second region; bit lines extending in the vertical direction across the word lines; and cell contact plugs each connected to the pads of the word lines in the second region, wherein the cell contact plugs are connected to the first bonding pads.
[0008] Specific details of other embodiments are included in the detailed description and drawings. Effects of the invention
[0009] According to embodiments of the present invention, the bonding pads of a first substrate on which memory cells are formed and the bonding pads of a second substrate on which peripheral circuits are formed can be joined to connect a cell array structure and a peripheral circuit structure. Accordingly, the integration density of the semiconductor memory device can be improved. In addition, since the pads of the word lines in the cell array structure are stacked in a stepped form, the wiring structure for connecting the word lines and the peripheral circuit structure can be simplified. Brief explanation of the drawing
[0010] FIG. 1 is a block diagram of a semiconductor memory device according to embodiments of the present invention. FIG. 2 is a perspective view showing a part of a semiconductor memory device according to embodiments of the present invention. FIG. 3 is a cross-sectional view of a semiconductor memory device according to embodiments of the present invention. FIG. 4 is a plan view showing a cell array structure of a semiconductor memory device according to embodiments of the present invention. FIG. 5a is a cross-sectional view of a cell array structure of a semiconductor memory device according to embodiments of the present invention, showing cross-sections cut along lines A-A' and B-B' of FIG. 4. FIG. 5b is a cross-sectional view of a cell array structure of a semiconductor memory device according to embodiments of the present invention, showing cross-sections cut along the CC' line of FIG. 4. Figure 6 is an enlarged view of the P1 portion of Figure 5a. Figures 7a and 7 are enlarged views of the P2 portion of Figure 5b. FIG. 8 is a flowchart illustrating a method for manufacturing a cell array structure of a semiconductor memory device according to embodiments of the present invention. FIGS. 9a to 18a are plan views for illustrating a method for manufacturing a cell array structure of a semiconductor memory device according to embodiments of the present invention. FIGS. 9b to 16b, and FIGS. 18b to 20b show cross-sections cut along the A-A' and B-B' lines of FIGS. 9a to 16a and FIGS. 18a to 20a. FIGS. 9c to 16c, FIGS. 16e, FIG. 16f, and FIGS. 17b, FIGS. 18c to 20c show cross-sections cut along the C-C' line of FIGS. 9a to 20a. FIG. 21 is a flowchart illustrating a method for manufacturing a cell array structure of a semiconductor memory device according to embodiments of the present invention. FIGS. 22a to 22f are perspective views illustrating a pad trimming process in a method for manufacturing a cell array structure according to embodiments of the present invention. FIGS. 23a and FIGS. 23b are perspective views illustrating a structure formed by a pad trimming process according to embodiments of the present invention. FIGS. 24a and FIGS. 24b are perspective views illustrating a structure formed by a pad trimming process according to embodiments of the present invention. FIGS. 25a to 25g are drawings for illustrating various arrangement structures of wordline pads in a cell array structure according to embodiments of the present invention. Specific details for implementing the invention
[0011] Hereinafter, a semiconductor device according to embodiments of the present invention and a semiconductor memory device including the same will be described in detail with reference to the drawings.
[0012] FIG. 1 is a block diagram of a semiconductor memory device according to embodiments of the present invention.
[0013] Referring to FIG. 1, a semiconductor memory device may include a memory cell array (1), a row decoder (2), a sensing amplifier (3), a column decoder (4), and control logic (5).
[0014] The memory cell array (1) includes a plurality of memory cells (MC) arranged in three dimensions. Each of the memory cells (MC) can be connected between a word line (WL) and a bit line (BL) that intersect each other.
[0015] Each memory cell (MC) includes a switching element (TR) and a data storage element (DS), and the switching element (TR) and the data storage element (DS) may be electrically connected in series. The switching element (TR) may be a field-effect transistor (FET), and the data storage element (DS) may be implemented as a capacitor or a variable resistor, etc. As an example, the switching element (TR) may include a transistor, the gate electrode of the transistor may be connected to the word line (WL), and the drain / source terminals of the transistor may be connected to the bit line (BL) and the data storage element (DS), respectively.
[0016] The row decoder (2) can decode an externally input address and select one of the word lines (WL) of the memory cell array (1). The address decoded by the row decoder (2) can be provided to a row driver (not shown), and the row driver can provide a predetermined voltage to the selected word line (WL) and the unselected word lines (WL), respectively, in response to the control of the control circuits.
[0017] The detection amplifier (3) can detect and amplify the voltage difference between the selected bit line (BL) and the reference bit line according to the address decoded from the column decoder (4) and output it.
[0018] The column decoder (4) can provide a data transmission path between the sensing amplifier (3) and an external device (e.g., a memory controller). The column decoder (4) can decode an externally input address and select any one of the bit lines (BL).
[0019] The control logic (5) can generate control signals that control operations for writing or reading data to or from the memory cell array (1).
[0020] FIG. 2 is a perspective view showing a part of a semiconductor memory device according to embodiments of the present invention. FIG. 3 is a cross-sectional view of a semiconductor memory device according to embodiments of the present invention.
[0021] Referring to FIGS. 2 and 3, a semiconductor memory device may include a cell array structure (CS) and a peripheral circuit structure (PS) on the cell array structure (CS).
[0022] In the embodiments, the semiconductor memory device may have a C2C (chip-to-chip) structure. A C2C structure may mean fabricating an upper chip including a cell array structure (CS) on a first wafer, fabricating a lower chip including a peripheral circuit structure (PS) on a second wafer different from the first wafer, and then connecting the upper chip and the lower chip to each other by a bonding method. For example, the bonding method may mean a method of electrically connecting a bonding metal formed on the uppermost metal layer of the upper chip and a bonding metal formed on the uppermost metal layer of the lower chip to each other. For example, if the bonding metal is formed of copper (Cu), the bonding method may be a Cu-to-Cu bonding method, and the bonding metal may also be formed of aluminum (Al) or tungsten (W).
[0023] The cell array structure (CS) may include a lower insulating film (300) having a first surface and a second surface facing each other, word lines (WL), bit lines (BL), a power capacitor (PC), an input / output contact plug (IOPLG), input / output pads (PAD) (IOPAD), and first bonding pads (PAD) (BP1a, BP1b, BP1c).
[0024] A cell array structure (CS) may include a cell array region (CAR) and a first peripheral region (PR1), and the cell array region (CAR) may include a first region (BCR; or bit line connection region) and a second region (WCR; or word line connection region).
[0025] A laminated structure (ST) may be disposed on a first surface of a lower insulating film (300). The laminated structure (ST) may include alternately stacked interlayer insulating patterns (ILD) and word lines (WL). The laminated structure (ST) may extend in a first direction (D1) parallel to the first surface of the lower insulating film (300) and may have a stepped structure in a second region (WCR).
[0026] Word lines (WL) can be extended from the first region (BCR) to the second region (WCR), and bit lines (BL) can be provided in the first region (BCR). Bit lines (BL) can be extended in a third direction (D3) perpendicular to the first surface of the lower insulating film (300).
[0027] Word lines (WL) may extend in a first direction (D1) parallel to a first surface of the lower insulating film (300). Word lines (WL) may include pads (PAD) connected to a cell contact plug (CPLG) in a second region (WCR). Word lines (WL) may be stacked to have a stepped structure in the second region (WCR). The pads (PAD) of the word lines (WL) may be located at different positions horizontally and vertically. In some examples, some of the word lines (WL) adjacent to the lower insulating film (300) may be provided as dummy word lines (DE).
[0028] Meanwhile, in the embodiments of the present invention, the word lines (WL) are described as being parallel to the first surface of the lower insulating film (300), but the present invention is not limited thereto, and the bit lines (BL) may be extended in a first direction (D1) parallel to the first surface of the lower insulating film (300), and the word lines (WL) may be extended in a third direction (D3).
[0029] According to the embodiments, each word line (WL) may have a double gate structure that crosses both sides of the channel pattern (SP), as shown in FIG. 2. Alternatively, each word line (WL) may have a structure that completely surrounds the channel pattern (SP) (i.e., a gate all around structure).
[0030] The first end of the channel pattern (SP) can be connected to the bit line (BL), and the second end of the channel pattern (SP) can be connected to the storage electrode (SE). The cell array region (CAR) of the cell array structure (CS) according to embodiments of the present invention will be described in more detail with reference to FIGS. 4, 5a, 5b, 6, 7a, and 7b.
[0031] A flat insulating film (110) may be disposed on the first surface of the lower insulating film (300) in the second region (WCR) and the first peripheral region (PR1). The flat insulating film (110) may cover the stepped structure of the laminated structure (ST). That is, the flat insulating film (110) of the word lines (WL) Pads It can cover.
[0032] A semiconductor memory device in the first peripheral region (PR1) Some of the core and peripheral circuits (see 2, 3, 4, and 5 in FIG. 1) may be provided. For example, A power capacitor (PC; or decoupling capacitor) that filters noise between operating power supplies input to a semiconductor memory device may be provided in the first peripheral region (PR1). The power capacitor (PC) may be configured as a voltage generator that receives a power supply voltage input to an input / output pad (IOPAD) and outputs operating voltages that operate a memory cell array. Additionally, the power capacitor (PC) may filter noise between operating power supplies input through the input / output pad (IOPAD). As an example, the power capacitor (PC) may be a Metal-Insulator-Metal (MIM) capacitor comprising first and second electrodes and a dielectric film between them.
[0033] The input / output contact plug (IOPLG) can penetrate the flat insulating film (110) in the first peripheral region (PR1). The input / output contact plug (IOPLG) can be connected to the first bonding pads (BP1a, BP1b, BP1c) through contact plugs and conductive lines.
[0034] Input / output pads (IOPAD) and dummy pads (PAD) (DPAD) may be disposed on a second surface of the lower insulating film (300). The input / output pads (IOPAD) may be connected to an input / output contact plug (IOPLG) through input / output vias (BVA) in a first peripheral region (PR1). Dummy pads (DPAD) may be provided in a first region (BCR) and a second region (WCR). The dummy pads (DPAD) may be connected to dummy vias (DVA). The dummy vias (DVA) may be surrounded by an insulating material and may be electrically floating, and the dummy pads (DPAD) and dummy vias (DVA) may be provided as a passage for supplying hydrogen during the manufacturing process of a semiconductor memory device. The input / output pads (PAD) (IOPAD) and dummy pads (PAD) (DPAD) may include a metallic material and may be made of, for example, aluminum.
[0035] A protective film (310) may be disposed on the second surface of the lower insulating film (300), and the protective film (310) may cover the input / output pads (IOPAD) and dummy pads (DPAD). The protective film (310) may be an oxide film containing hydrogen. The hydrogen concentration within the protective film (310) may be greater than the hydrogen concentration within the lower insulating film (300). The protective film (310) may be a High Density Plasma (HDP) oxide film or a Tetraethylortho Silicate (TEOS) film.
[0036] A capping insulating film (320) and a passivation film (330) may be formed sequentially on a protective film (310). The capping insulating film (320) and the passivation film (330) may have a pad opening (OP) that exposes a portion of the input / output pads (PAD) (IOPAD).
[0037] The capping insulating film (320) may be, for example, a silicon nitride film or a silicon oxynitride film. The passivation film (330) may be a polyimide-based material, for example, photosensitive polyimide (PSPI).
[0038] In the embodiments, the first bonding pads (BP1a, BP1b, BP1c) of the cell array structure (CS) may include first upper bonding pads (BP1a) provided in the first region (BCR), second upper bonding pads (BP1b) provided in the word line connection regions (WCR), and third upper bonding pads (BP1c) provided in the first peripheral region (PR1).
[0039] The first upper bonding pads (BP1a) can be electrically connected to bit lines (BL) through conductive lines and contact plugs, and the second upper bonding pads (BP1b) can be connected to pads (PAD) of word lines (WL) through conductive lines and cell contact plugs (CPLG). The third upper bonding pads (BP1c) can be connected to a power capacitor (PC) and an input / output contact plug (IOPLG) through conductive lines and contact plugs.
[0040] The peripheral circuit structure (PS) may include a semiconductor substrate (200), sense amplifiers (SA), subword line drivers (SWD), peripheral circuits (PTR), and second bonding pads (BP2a, BP2b, BP2c) on the semiconductor substrate (200).
[0041] In detail, the semiconductor substrate (200) of the peripheral circuit structure (PS) may include a first core region (CR1), a second core region (CR2), and a second peripheral region (PR2). The first and second core regions (CR1, CR2) may be vertically overlapped with the memory cell array region (CAR). The second peripheral region (PR2) may be vertically overlapped with the first peripheral region (PR1).
[0042] A plurality of sense amplifiers (SA) may be provided on the semiconductor substrate (200) of the first core region (CR1). A plurality of sub-word line drivers (SWD) may be provided on the semiconductor substrate (200) of the second core region (CR2). Peripheral circuits (PTR) may be provided on the semiconductor substrate (200) of the second peripheral region (PR2).
[0043] Peripheral interlayer insulating films (210, 220) may be provided on the upper surface of a semiconductor substrate (200). Peripheral interlayer insulating films (210, 220) may cover peripheral circuits (SA, SWD, PTR), peripheral contact plugs (PCP), and peripheral circuit wiring (PLP) on the semiconductor substrate (200). Peripheral contact plugs (PCP) and peripheral conductive lines may be electrically connected to peripheral circuits (SA, SWD, PTR). Peripheral interlayer insulating films (210, 220) may include silicon oxide, silicon nitride, silicon oxynitride, and / or low dielectric films.
[0044] The second bonding pads (BP2a, BP2b, BP2c) of the peripheral circuit structure (PS) may include first lower bonding pads (BP2a) provided in the first core region (CR1), second lower bonding pads (BP2b) provided in the second core region (CR2), and third lower bonding pads (BP2c) provided in the second peripheral region (PR2).
[0045] The first lower bonding pads (BP2a) can be electrically connected to sense amplifiers (SA) through conductive lines and contact plugs. The second lower bonding pads (BP2b) can be electrically connected to subword line drivers (SWD) through conductive lines and contact plugs. The third lower bonding pads (BP2c) can be electrically connected to peripheral circuits (PTR) through conductive lines and contact plugs.
[0046] In the embodiments, the first, second, and third lower bonding pads (BP2a, BP2b, BP2c) may be directly connected to the first, second, and third upper bonding pads (BP1a, BP1b, BP1c), respectively. The first, second, and third lower and upper bonding pads (BP1a, BP1b, BP1c, BP2a, BP2b, BP2c) may comprise the same metallic material and may have substantially the same size or area. The first, second, and third lower and upper bonding pads (BP1a, BP1b, BP1c, BP2a, BP2b, BP2c) may comprise, for example, copper (Cu), aluminum (Al), nickel (Ni), cobalt (Co), tungsten (W), titanium (Ti), tin (Sn), or alloys thereof.
[0047] FIG. 4 is a plan view showing a cell array structure of a semiconductor memory device according to embodiments of the present invention. FIG. 5a is a cross-sectional view of a cell array structure of a semiconductor memory device according to embodiments of the present invention, showing cross-sections cut along lines A-A' and B-B'' of FIG. 4. FIG. 5b is a cross-sectional view of a cell array structure of a semiconductor memory device according to embodiments of the present invention, showing cross-sections cut along line CC' of FIG. 4. FIG. 6 is an enlarged view of portion P1 of FIG. 5a. FIG. 7a and FIG. 7b are enlarged views of portion P2 of FIG. 5b.
[0048] Referring to FIGS. 4, FIGS. 5a, and FIGS. 5b, a semiconductor memory device may include stacked structures (ST) disposed on a substrate (100).
[0049] The substrate (100) may include a first region (BCR) and a second region (WCR) adjacent thereto. The substrate (100) may be one of a material having semiconductor properties (e.g., silicon wafer), an insulating material (e.g., glass), a semiconductor or a conductor covered by an insulating material.
[0050] In the embodiments, each of the stacked structures (ST) may include interlayer insulation patterns (ILD) and word lines (WLa, WLb) alternately stacked along a third direction on the substrate (100). The stacked structures (ST) may extend along a first direction (D1) from a first region (BCR) to a second region (WCR) and may have a stepped structure in the second region (WCR). Each of the stacked structures (ST) may include pads (PAD) of pad insulation patterns (ILD) and word lines (WLa, WLb) alternately stacked in the second region (WCR). The pad insulation patterns (PLD) are located at the same level as the interlayer insulation patterns (ILD), but the thickness of each pad insulation pattern (PLD) may be thicker than the thickness of each interlayer insulation pattern (ILD).
[0051] The stacked structures (ST) may include first and second stacked structures that are adjacent in a second direction (D2) and extend parallel to each other. The first stacked structure extends in a first direction (D1) and may include first word lines (WLa) stacked in a third direction (D3) with interlayer insulation patterns (ILD) interposed on the substrate (100). The second stacked structure may be spaced apart from the first stacked structure in the second direction (D2) and extend in the first direction (D1). The second stacked structure may include second word lines (WLb) stacked in a third direction (D3) with interlayer insulation patterns (ILD) interposed on the substrate (100). An upper insulating film (TIL) covering the first and second word lines (WLa, WLb) of the top layer may be disposed. The first and second word lines (WLa, WLb) may be any one of a doped semiconductor material (e.g., doped silicon, doped germanium, etc.), a conductive metal nitride (e.g., titanium nitride, tantalum nitride, etc.), a metal (e.g., tungsten, titanium, tantalum, etc.), and a metal-semiconductor compound (e.g., tungsten silicide, cobalt silicide, titanium silicide, etc.).
[0052] In one example, the staircase structure of each stacked structure (ST) may have pads (PAD) of two consecutively stacked word lines (WLa, WLb) forming a single stair, as illustrated in FIG. 5b. Accordingly, the two word lines (WLa, WLb) forming a single stair may have vertically aligned side walls. Alternatively, the staircase structure of the stacked structure (ST) may have pads (PAD) of three, four, or six consecutively stacked word lines (WLa, WLb) forming a single stair. The staircase structure of the stacked structure (ST) may be varied in many ways, which will be described in more detail with reference to FIG. 25a through 25g.
[0053] In each of the stacked structures (ST), pads (PADs) of the word lines (WLa, WLb) may be arranged along a first direction (D1), and the height of the pads (PADs) of the word lines (WLa, WLb) from the substrate may increase as they approach a first region (BCR). According to one example, the pads (PADs) of the odd-numbered word lines (WLa, WLb) among the word lines (WLa, WLb) may be arranged along the first direction (D1), and cell contact plugs (CPLG) may be connected to the pads (PADs) of the odd-numbered word lines (WLa, WLb), respectively.
[0054] Each of the stacked structures may be positioned between the first and second line separation insulation patterns (106, 113) in the second region (WCR). At least one of the first and second line separation insulation patterns (106, 113) may have a stepped structure substantially identical in form to the stacked structure (ST) (see 106 in FIG. 23b). As the height of the pads (PAD) from the substrate (100) decreases, the width of the first line separation insulation pattern (106) may decrease (see 106 in FIG. 23b). Additionally, as a result of the pad trimming process forming the stepped structure in the second region (WCR), as the height of the pads (PAD) of the word lines (WLa, WLb) from the substrate (100) decreases, the width of the pads (PAD) of the word lines (WLa, WLb) may decrease (see 20a, 20b in FIG. 24b).
[0055] According to the embodiments, in the first region (BCR), each of the word lines (WLa, WLb) may have a double gate structure provided on the upper and lower surfaces of the channel pattern (SP), as shown in FIG. 2.
[0056] More specifically, each of the first and second word lines (WLa, WLb) may include a pair of sub-gate electrodes extending in a first direction (D1) in a first region (BCR) and a pad (PAD) commonly connected to the sub-gate electrodes in a second region (WCR). Here, the sub-gate electrodes may be positioned between the first and second isolation patterns (STI1, STI2). Additionally, in the second direction (D2), the width of the sub-gate electrodes between the first and second isolation patterns (STI1, STI2) may be smaller than the width of the sub-gate electrodes on the channel patterns. In a planar view, the pair of first and second word lines (WLa, WLb) may be mirror-symmetric with respect to the plate electrode (PE).
[0057] Referring to FIGS. 7a and FIGS. 7b, in each of the word lines (WLa, WLb), the thickness of the pad (PAD) may be greater than the thickness of each sub-gate electrode.
[0058] Referring to FIG. 7a, a pad (PAD) of each word line (WLa, WLb) may be positioned between vertically adjacent pad insulation patterns (PLD). The upper and lower surfaces of the pad (PAD) may be in direct contact with the pad insulation patterns (PLD). In each word line (WLa, WLb), the pad (PAD) may have a protrusion extending between the sub-gate electrodes. The protrusion of the pad (PAD) may be in common contact with a pair of sub-gate electrodes. Additionally, in each word line (WLa, WLb), an interface may exist between the sub-gate electrodes and the pad (PAD).
[0059] Referring to FIG. 7b, in each word line (WLa, WLb), the sub-gate electrodes and the pad (PAD) may be formed as a single film without an interface between the sub-gate electrodes and the pad (PAD). In this case, a gate insulating film (Gox) may be interposed between the pad (PAD) and the pad insulating patterns (PLD).
[0060] Channel patterns (SP) can be stacked in a third direction (D3) in a first region (BCR) and can be spaced apart from each other in a first direction (D1) and a second direction (D2). That is, channel patterns (SP) can be arranged three-dimensionally on a substrate (100). Each of the channel patterns (SP) can have a bar shape with a major axis in the second direction (D2) across the word lines (WLa, WLb), as shown in FIG. 2.
[0061] When the word lines (WLa, WLb) are double gate structures, channel patterns (SP) can be spaced apart from each other in a first direction (D1) between a pair of sub-gate electrodes. Additionally, dummy insulation patterns (DIP) can be placed between adjacent channel patterns (SP) in the first direction (D1) and between a pair of sub-gate electrodes.
[0062] Channel patterns (SP) may include silicon (Si), germanium (Ge), or silicon-germanium (SiGe). For example, channel patterns (SP) may be made of single-crystal silicon. In some embodiments, channel patterns (SP) may have a bandgap energy greater than the bandgap energy of silicon. For example, channel patterns (SP) may have a bandgap energy of about 1.5 eV to 5.6 eV. For example, channel patterns (SP) may have optimal channel performance when having a bandgap energy of about 2.0 eV to 4.0 eV. For example, channel patterns (SP) may include an oxide semiconductor, and for example, the oxide semiconductor may include ZnxSnyO (ZTO), InxZnyO (IZO), ZnxO, InxGayZnzO (IGZO), InxGaySizO (IGSO), InxWyO (IWO), InxO, SnxO, TixO, ZnxONz, MgxZnyO, ZrxInyZnzO, HfxInyZnzO, SnxInyZnzO, AlxSnyInzZnaO, SixInyZnzO, AlxZnySnzO, GaxZnySnzO, ZrxZnySnzO, or a combination thereof.
[0063] Each of the channel patterns (SP) may include first and second source drain regions (SD1, SD2) spaced apart from each other, as shown in FIG. 6, and a channel region (CH) between the first and second source drain regions (SD1, SD2). Impurities may be doped within the first and second source drain regions (SD1, SD2) of each channel pattern (SP).
[0064] First spacer insulation patterns (SS1) can be placed between word lines (WL) and bit lines (BL), and between vertically adjacent interlayer insulation patterns (ILD). The first spacer insulation patterns (SS1) can surround the first dopant region (SD1) of the channel pattern (SP).
[0065] Second spacer insulation patterns (SS2) can be placed between word lines (WL) and data storage elements (DS), and between vertically adjacent interlayer insulation patterns (ILD), respectively. The second spacer insulation pattern (SS2) can surround the second dopant region (SD2) of the channel pattern (SP). In the second direction (D2), the width of the second spacer insulation patterns (SS2) can be greater than the width of the first spacer insulation patterns (SS1).
[0066] Gate insulating films (Gox) may be interposed between the channel regions (CH) and word lines (WLa, WLb) of the channel patterns (SP) in the first region (BCR), and between the interlayer insulating patterns (ILD) and word lines (WLa, WLb).
[0067] The gate insulating films (Gox) may be spaced apart from the pads (PAD) of each word line (WLa, WLb) as shown in FIG. 7a. Alternatively, the gate insulating films (Gox) may extend from the first region (BCR) to the second region (WCR) and conformally cover the surface of each word line as shown in FIG. 7b.
[0068] The gate insulating films (Gox) may include a single film selected from a high dielectric film, a silicon oxide film, a silicon nitride film, and a silicon oxynitride film, or a combination thereof. As an example, the high dielectric film may include at least one of hafnium oxide, hafnium silicon oxide, lanthanum oxide, zirconium oxide, zirconium silicon oxide, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, lithium oxide, aluminum oxide, lead scandium tantalum oxide, and lead zinc niobate.
[0069] The first end of the semiconductor pattern (SP) can be in contact with the bit line (BL), and the second end of the channel pattern (SP) can be connected to the data storage element (DS).
[0070] In the embodiments, the data storage element (DS) may be a capacitor, and the data storage element (DS) may include a storage electrode (SE), a plate electrode (PE), and a capacitor dielectric film (CIL) between them.
[0071] The storage electrodes (SE) can be in contact with the second end of each channel pattern (SP). The storage electrodes (SE) can be provided at substantially the same level as the channel patterns (SP). In other words, the storage electrodes (SE) can be stacked in a third direction (D3) and have a long axis in the second direction (D2). The storage electrodes (SE) can be placed between vertically adjacent interlayer insulation patterns (ILD).
[0072] The capacitor dielectric film (CIL) can conformally cover the surface of the storage electrodes (SE). The plate electrode (PE) can fill the interior of the storage electrodes (SE) on which the capacitor dielectric film (CIL) is formed.
[0073] Second separation insulation patterns (STI2) may be disposed between storage electrodes (SE) adjacent in a first direction (D1). The second separation insulation patterns (STI2) may extend in a third direction (D3). The second separation insulation patterns (STI2) may be one of insulating materials formed using SOG (Spin On Glass) technology, silicon oxide films, or silicon oxynitride films.
[0074] The first and second bit lines (BLa, BLb) may extend in a third direction (D3) perpendicular to the upper surface of the substrate (100). The first and second bit lines (BLa, BLb) may intersect with the first and second word lines (WLa, WLb). The first bit lines (BLa) may be spaced apart from each other in a first direction (D1), and first isolation insulation patterns (STI1) may be disposed between the first bit lines (BLa) adjacent in the first direction (D1). The first isolation insulation patterns (STI1) may extend in a third direction (D3). The first isolation insulation patterns (STI1) may be one of insulating materials formed using SOG (Spin On Glass) technology, silicon oxide films, and silicon oxynitride films.
[0075] The second bit lines (BLb) can be spaced apart from the first bit lines (BLa) in a second direction (D2) and can be spaced apart from each other in a first direction (D1). First isolation patterns (STI1) can be placed between the second bit lines (BLb) adjacent in the first direction (D1).
[0076] Each of the first and second bit lines (BLa, BLb) can come into contact with the first sides of the channel patterns (SP) that are spaced apart from each other in the third direction (D3). That is, each of the first and second bit lines (BLa, BLb) can be connected to the first dopant regions of the channel patterns (SP) stacked along the third direction (D3).
[0077] Line separation insulation patterns (120) may extend along a first direction (D1) on the substrate (100). The line separation insulation patterns (120) may cover the sidewalls of the first and second bit lines (BLa, BLb) and the sidewalls of the first separation insulation patterns (STI1). The line separation insulation patterns (120) may be one of insulating materials formed using SOG (Spin On Glass) technology, silicon oxide films, and silicon oxynitride films.
[0078] FIG. 8 is a flowchart illustrating a method for manufacturing a cell array structure of a semiconductor memory device according to embodiments of the present invention.
[0079] FIGS. 9a to 18a are plan views illustrating a method for manufacturing a cell array structure of a semiconductor memory device according to embodiments of the present invention. FIGS. 9b to 16b and FIGS. 18b to 20b show cross-sections cut along the A-A' and B-B' lines of FIGS. 9a to 16a and FIGS. 18a to 20a. FIGS. 9c to 16c, FIG. 16e, FIG. 16f, and FIGS. 17b, FIGS. 18c to 20c show cross-sections cut along the C-C' line of FIGS. 9a to 20a.
[0080] Referring to FIGS. 8, FIGS. 9a, FIGS. 9b, and FIGS. 9c, a first mold structure may be formed on a substrate (100) including a first region (BCR) and a second region (WCR) (S10).
[0081] The substrate (100) may be one of a material having semiconductor properties (e.g., silicon wafer), an insulating material (e.g., glass), a semiconductor or a conductor covered by an insulating material.
[0082] The first mold structure (MS1) may include first semiconductor films (10) and second semiconductor films (20) alternately stacked on a substrate (100).
[0083] The first semiconductor films (10) may be formed of a material having etch selectivity with respect to the second semiconductor films (20). The first semiconductor films (10) may be formed of at least one of, for example, silicon germanium, silicon oxide, silicon nitride, and silicon oxynitride. In one example, the first semiconductor films (10) may be a semiconductor material, for example, a silicon germanium film. When forming the first mold structure (MS1), the thickness of each first semiconductor film (10) may be smaller than the thickness of each second semiconductor film (20).
[0084] The second semiconductor films (20) may include, for example, silicon, germanium, silicon-germanium, or IGZO (Indium Gallium Zinc Oxide). In the embodiments, the second semiconductor films (20) may include the same semiconductor material as the substrate (100). For example, the second semiconductor films (20) may be a single-crystal silicon film or a polycrystalline silicon film.
[0085] The first semiconductor films (10) and the second semiconductor films (20) can be formed by performing an epitaxial growth process.
[0086] According to the embodiments, a buffer layer (BFL) may be interposed between the first mold structure (MS1) and the substrate (100). For example, the buffer layer (BFL) may include silicon-germanium (SiGe) and may have a different composition ratio from the first semiconductor films (10).
[0087] A first mask pattern (MP1) may be formed on a first mold structure (MS1). The first mask pattern (MP1) may cover the top layer second semiconductor film (20). The first mask pattern (MP1) may be made of an insulating material having etch selectivity for the first semiconductor films (10) and the second semiconductor films (20). For example, the first mask pattern (MP1) may be a silicon oxide film or a silicon nitride film.
[0088] Continuing with reference to FIGS. 9a, 9b, and 9c, first and second preliminary separation patterns (30, 40) penetrating the first mold structure (MS1) in the first region (BCR) may be formed. The first preliminary separation patterns (30) may be arranged spaced apart from each other in the first direction (D1), and the second preliminary separation patterns (40) may be arranged spaced apart from the first preliminary separation patterns (30) in the second direction (D2). Additionally, the first and second preliminary separation patterns (30, 40) may be formed repeatedly in a mirror-symmetric manner along the second direction (D2).
[0089] The first and second preliminary separation patterns (30, 40) may be spaced apart from each other by a first interval in the first direction (D1). The first preliminary separation patterns (30) may be spaced apart from the second preliminary separation patterns (40) by a second interval smaller than the first interval in the second direction (D2).
[0090] In the first direction (D1), the first and second preliminary separation patterns (30, 40) may each have a first width. In the second direction (D2), the length of each first preliminary separation pattern (PS1) may be smaller than the length of each second preliminary separation pattern (40).
[0091] Forming the first and second preliminary separation patterns (30, 40) may include forming first and second openings that penetrate the first mold structure (MS1) using the first mask pattern (MP1) and filling the first and second openings with an insulating material. Here, when forming the first and second openings, the bottom surfaces of the first and second openings may be spaced apart from the upper surface of the substrate (100). That is, at least one first semiconductor film (10) and at least one second semiconductor film (20) may remain between the bottom surfaces of the first and second preliminary separation patterns (30, 40) and the substrate (100).
[0092] Next, referring to FIG. 8, channel patterns and a second mold structure can be formed in a first region (BCR) (S20). A method for forming channel patterns and a second mold structure in the first region (BCR) is described in detail with reference to FIG. 10a to FIG. 15c.
[0093] Referring to FIGS. 10a, 10b, and 10c, first and second preliminary line patterns (103, 105) extending side by side in a first direction (D1) may be formed. The first and second preliminary line patterns (103, 105) may extend from a first region (BCR) to a second region (WCR).
[0094] The first preliminary line patterns (103) are adjacent to the first preliminary separation patterns (30) and can penetrate the first mold structure. The second preliminary line pattern (105) can penetrate the first mold structure between the second preliminary separation patterns (40) that are adjacent to each other.
[0095] Forming the first and second preliminary line patterns (103, 105) may include forming second mask patterns (MP2) in the form of lines on a first mask pattern (MP1), forming first and second trenches by anisotropically etching a first mold structure (MS1) using the second mask patterns (MP2) as an etching mask, and filling the first and second trenches with an insulating material. The first and second preliminary line patterns (103, 105) may include a silicon oxide film and / or a silicon nitride film.
[0096] Referring to FIGS. 11a, 11b, and 11c, a third mask pattern (MP3) may be formed on the first and second preliminary line patterns (103, 105) in the first region (BCR) and on the second mask pattern (MP2) in the second region (WCR). The third mask pattern (MP3) may have a line-shaped opening extending in the first direction (D1) in the first region (BCR).
[0097] After removing the first and second mask patterns (MP1, MP2) using the third mask pattern (MP3) as an etching mask, the first and second preliminary separation patterns (30, 40) can be removed. Accordingly, the first and second openings (OP1, OP2) can be re-formed in the first region (BCR). That is, the sidewalls of the first and second semiconductor films (10, 20) and the sidewalls of the first and second preliminary line patterns (103, 105) can be exposed in the first openings (OP1, OP2).
[0098] Referring to FIGS. 12a, 12b, and 12c, in the first region (BCR), first semiconductor films (10) exposed to the first and second openings (OP1, OP2) can be removed to form first horizontal regions (HR1) between vertically adjacent second semiconductor films (20). While forming the first horizontal regions (HR1) in the first region (BCR), the first semiconductor films (10) in the second region (WCR) may remain unetched.
[0099] Forming the first horizontal regions (HR1) may include isotropically etching the first semiconductor films (10) by performing an etching process having etch selectivity for the substrate (100), the second semiconductor films (20), and the first and second preliminary line patterns (103, 105). When the first semiconductor films (10) are removed, the second semiconductor films (20) can be vertically separated without collapsing due to the first and second preliminary line patterns (103, 105).
[0100] The vertical thickness of the first horizontal regions (HR1), that is, the vertical distance between adjacent second semiconductor films (20), can be substantially the same as the thickness of the first semiconductor film (10).
[0101] Referring to FIGS. 13a, 13b, and 13c, a trimming process may be performed to reduce the thickness of the second semiconductor films (20) exposed in the first horizontal regions (HR1). The trimming process may include etching the upper and lower surfaces of the second semiconductor films (20) exposed in the first horizontal regions (HR1). As an example, the trimming process may include performing an isotropic etching process having etch selectivity for the upper insulating film (TL) and the first and second sacrificial line patterns (103, 105).
[0102] As the trimming process is performed, the thickness of each of the second semiconductor films (20) is reduced so that preliminary channel films (21) can be formed. At the same time, the vertical thickness of the first horizontal regions (HR1) is increased so that second horizontal regions (HR2) can be formed between vertically adjacent preliminary channel films (21).
[0103] Referring to FIGS. 14a, FIGS. 14b, and FIGS. 14c, By forming sacrificial patterns (30) and interlayer insulation patterns (ILD) within the second horizontal regions (HR2), a second mold structure (MS2) can be formed in the first region (BCR).
[0104] The second mold structure (MS2) can be formed by sequentially depositing a sacrificial film and an interlayer insulating film on the surfaces of the preliminary channel films (21), and then sequentially performing a partial etching process on the interlayer insulating film and the sacrificial film.
[0105] More specifically, a sacrificial film and an interlayer insulating film may be deposited sequentially on the surfaces of the pre-channel films (21). Here, the sacrificial film may be deposited with a thickness less than half the vertical thickness of the second horizontal region (HR2). Accordingly, after depositing the sacrificial film, gap regions may be defined between vertically adjacent pre-channel films (21). Subsequently, an interlayer insulating film may be formed on the sacrificial film to fill the second horizontal region (HR2) where the sacrificial film is formed.
[0106] After forming an interlayer insulating film, portions of the interlayer insulating film exposed at the first and second openings (OP1, OP2) can be etched to form interlayer insulating patterns (ILD). The interlayer insulating patterns (ILD) may include isotropically etching the interlayer insulating film until a sacrificial film is exposed at the first and second openings (OP1, OP2). By the isotropic etching process, the interlayer insulating patterns (ILD) can be vertically separated from each other.
[0107] After forming interlayer insulation patterns (ILD), an isotropic etching process is performed on the sacrificial film so that the sidewalls of the pre-channel films (21) are exposed, thereby forming sacrificial patterns (30) between the interlayer insulation patterns (ILD) and the pre-channel films (21).
[0108] After forming the second mold structure (MS2), the sidewalls of the preliminary channel membranes (21), the sidewalls of the sacrificial patterns (30), and the sidewalls of the interlayer insulation patterns (ILD) can be exposed to the first and second openings (OP1, OP2).
[0109] Sacrificial patterns (30) can be formed by depositing a material having etch selectivity for the substrate (100) and the pre-channel films (21). The sacrificial patterns (30) can be formed, for example, from at least one of a silicon oxide film, a silicon nitride film, and a silicon oxynitride film.
[0110] The interlayer insulation patterns (ILD) can be formed of an insulating material having etch selectivity for the pre-channel films (21), sacrificial patterns (30), and substrate (100). As an example, the interlayer insulation patterns (ILD) may be silicon oxide.
[0111] Referring to FIGS. 15a, 15b, and 15c, in the first region (BCR), an etching process can be performed on portions of the preliminary channel films (21) exposed to the first and second openings (OP1, OP2). Accordingly, channel patterns (SP) separated from each other in the first direction (D1) can be formed.
[0112] Forming channel patterns (SP) may include isotropically etching the pre-channel films (21) exposed to the first and second openings (OP1, OP2). That is, an etching etchant may be supplied through the first and second openings (OP1, OP2) so that the pre-channel films (21) can be etched laterally along the first direction (D1) and the second direction (D2). At this time, since the spacing between the first openings (OP1) and the spacing between the second openings (OP2) is greater than the spacing between the first and second openings (OP1, OP2), parts of the pre-channel films (21) may be separated in the first direction (D1) to form channel patterns (SP). As a result of the isotropic etching process, the width in the first direction (D1) of each channel pattern (SP) may be greater in the center than in the sidewall portion. In contrast, each of the channel patterns (SP) can have a uniform width in the first direction (D1).
[0113] As the channel patterns (SP) are formed in this manner, gap regions can be formed between vertically adjacent sacrifice patterns (30) to expose the sidewalls of the channel patterns (SP). The gap regions may correspond to regions where the preliminary channel films (21) have been etched.
[0114] After forming channel patterns (SP), first and second separation insulation patterns (STI1, STI2) can be filled within the first and second openings (OP1, OP2), respectively, and an upper insulating film (TIL) can be formed on the second mold structure (MS2).
[0115] The upper insulating layer (TIL) and the first and second separation insulating patterns (STI1, STI2) may be one of insulating materials formed using SOG (Spin On Glass) technology, silicon oxide films, and silicon oxynitride films. The upper insulating layer (TIL) and the first and second separation insulating patterns (STI1, STI2) may be formed by depositing a separation insulating layer to fill the first and second openings (OP1, OP2), and then flattening the separation insulating layer so that the upper surface of the third mask pattern (MP3) is exposed.
[0116] When forming the upper insulating film (TIL) and the first and second separated insulating patterns (STI1, STI2), the insulating material can fill the gap regions. Accordingly, dummy insulating patterns (DIP) can be formed between adjacent channel patterns (SP) in the first region (BCR) in the first direction (D1).
[0117] Next, referring to FIG. 8, after forming channel patterns (SP) and a second mold structure (MS2) in a first region (BCR), a third mold structure (MS3) can be formed in a second region (WCR) (S30). Forming the third mold structure (MS3) is described with reference to FIG. 16a to 16e.
[0118] Referring to FIGS. 16a, 16b, and 16c, a fourth mask pattern (MP4) can be formed that exposes a portion of the second preliminary line pattern (105) in the second region (WCR).
[0119] A fourth mask pattern (MP4) can be used as an etching mask to etch a portion of the second preliminary line pattern (105) in the second region (WCR) to form a separation region (SR) that penetrates a portion of the second mold structure (MS2). The separation region (SR) can expose the sidewalls of the first and second semiconductor films (10, 20) in the second region (WCR).
[0120] Subsequently, the first semiconductor films (10) in the second region (WCR) can be selectively etched through the separation region (SR) to form third horizontal regions (HR3) between the second semiconductor films (20). Forming the third horizontal regions (HR3) may include isotropically etching the first semiconductor films (10) by performing an etching process having etch selectivity for the second semiconductor films (20), sacrificial patterns (30), and first and second pre-line patterns (103, 105), as previously formed the first horizontal regions (HR1). In one example, the third horizontal regions (HR3) It can expose parts of the sacrifice patterns (30) formed in the first region (BCR).
[0121] Next, referring to FIG. 16d, a trimming process to reduce the thickness of the second semiconductor films (20) exposed in the third horizontal regions (HR3) and a process to isotropically etch the sacrificial patterns (30) exposed in the third horizontal regions (HR3) may be performed. Accordingly, the vertical thickness of the third horizontal regions may be increased, and the interlayer insulation patterns (ILD) of the first region (BCR) may be exposed in the third horizontal regions.
[0122] Referring to FIG. 16e, a third mold structure (MS3) can be formed in the second region (WCR) by filling the third horizontal regions (HR3) with an insulating material. The third mold structure may include pad insulating patterns (PLD) between each of the second semiconductor films (20). The pad insulating patterns (PLD) may be vertically separated from each other by the second semiconductor films (20) and may come into contact with the interlayer insulating patterns (ILD) of the first region (BCR). The pad insulating patterns (PLD) may be formed of an insulating material having etch selectivity for the second semiconductor films (20) and the sacrificial patterns (30). For example, the pad insulating patterns (PLD) may be silicon oxide.
[0123] When forming pad insulation patterns (PLD), a first line insulation pattern (106) may be formed within the separation region (SR). The first line insulation pattern (106) may include the same insulating material as the pad insulation patterns (PLD) or may include a different insulating material from the pad insulation patterns (PLD).
[0124] Referring to FIG. 8, FIG. 17a, FIG. 17b, and FIG. 17c, a pad trimming process for a third mold structure can be performed in a second region (WCR) (S40).
[0125] The pad trimming process can form a stepped structure by repeating the patterning process for the third mold structure (MS3) in the second region (WCR). During the pad trimming process, a thick trimming mask pattern (TPR) may be formed on the fourth mask pattern (MP4), and the first, second, third, and fourth mask patterns may be removed in the second region (WCR). The pad trimming process will be described in detail with reference to FIGS. 22a through 22f.
[0126] By the pad trimming process, the third mold structure (MS2) may have a stepped structure formed along the first direction (D1) in the second region (WCR). Accordingly, the length of the second semiconductor films (20) in the second region (WCR) along the first direction (D1) may decrease as it moves away from the substrate (100). The second semiconductor film (20) and the adjacent pad insulation pattern (PLD) may have vertically aligned sidewalls.
[0127] In the embodiments, as the pad trimming process is performed, a step structure may also be formed in the first preliminary line patterns and the second line insulation pattern (106) in the second region (WCR). That is, the thickness (or vertical length) of the first preliminary line patterns and the second line insulation pattern (106) may decrease as it moves away from the first region (BCR).
[0128] Referring to FIG. 8, word lines and bit lines can be formed in the first region (BCR) (S50). This is described in detail with reference to FIG. 18a to FIG. 20c.
[0129] Referring to FIGS. 18a, 18b, and 18c, first trenches (T1) can be formed by removing first preliminary line patterns (103) in a first region (BCR) to expose the sidewalls of a second mold structure (MS2). The first trenches (T1) can expose the sidewalls of channel patterns (SP), the sidewalls of sacrificial patterns (30), and the sidewalls of interlayer insulation patterns (ILD).
[0130] Next, parts of the sacrifice patterns (30) exposed for the first trenches (T1) can be isotropically etched to form fourth horizontal regions (HR4) between the channel patterns (SP) and the interlayer insulation patterns (ILD).
[0131] The fourth horizontal regions (HR4) can be formed by isotropically etching the sacrificial patterns (30) using an etching recipe that has etch selectivity for the channel patterns (SP) and the interlayer insulation patterns (ILD). For example, where the sacrificial patterns (30) are silicon nitride films and the interlayer insulation patterns (ILD) are silicon oxide films, the etching step can form the fourth horizontal regions (HR4) by isotropically etching the sacrificial patterns (30) using an etching solution containing phosphoric acid. The fourth horizontal regions (HR4) can extend in a first direction (D1) between the first and second separation insulation patterns (STI1, STI2).
[0132] As the fourth horizontal regions (HR4) are formed, parts of the sacrificial patterns (30) may remain to form the first sacrificial patterns (31). The first sacrificial patterns (31) may be separated from each other in the first direction (D1) by the second separation insulation patterns (STI2).
[0133] Referring to FIGS. 19a, 19b, and 19c, a gate insulating film (Gox) and word lines (WL) can be formed sequentially within the fourth horizontal regions (HR4).
[0134] Forming the gate insulating film (Gox) and word lines (WL) may include forming a gate insulating film (Gox) that conformally covers the fourth horizontal regions (HR4) where the first sacrificial patterns (31) are formed, forming a gate conductive film that fills the fourth horizontal regions (HR4) on the gate insulating film (Gox), and removing the gate conductive film within the first trenches (T1) to form vertically separated word lines (WL). Here, the sidewalls of the word lines (WL) may be recessed compared to the sidewalls of the channel patterns (SP) and may be filled within parts of the fourth horizontal regions (HR4). The word lines (WL) may be formed on the upper and lower surfaces of the central parts (i.e., channel parts) of the channel patterns (SP) and may extend along the first direction (D1). In other words, each word line (WL) may have a double gate structure provided on the upper and lower surfaces of the channel pattern (SP). Alternatively, the word lines (WL) may have a structure that completely surrounds the central parts (i.e., channel parts) of the channel patterns (SP) (i.e., a gate all around structure).
[0135] The word lines (WL) may have a profile substantially identical to the sidewall profile of the first or second separation insulation patterns (STI1 or STI2) in portions adjacent to the sidewalls of the first or second separation insulation patterns (STI1 or STI2). That is, each of the word lines (WL) may have a non-uniform width in the second direction (D2).
[0136] First spacer insulation patterns (SS1) may be formed within the fourth horizontal regions (HR4) where word lines (WL) are formed. The first spacer insulation patterns (SS1) may expose a portion of the channel patterns (SP).
[0137] Forming the first spacer insulation patterns (SS1) may include forming a capping insulating film on the inner wall of the first trenches (T1) to fill the fourth horizontal regions (HR4), and removing the capping insulating film filled within the first trenches (T1) so that the sidewalls of the interlayer insulation patterns (ILD) are exposed. The capping insulating film may be etched by performing an isotropic etching process having etch selectivity for the interlayer insulation patterns (ILD) and channel patterns (SP). When forming the first spacer insulation patterns (SS1), portions of the gate insulating film (Gox) on the sidewalls of the interlayer insulation patterns (ILD) may be etched.
[0138] Before or after forming the first spacer insulation patterns (SS1), impurities may be doped into parts of the channel patterns (SP) exposed to the first trenches (T1). Accordingly, first dopant regions (see SD1 in FIG. 6) may be formed in the channel patterns (SP).
[0139] After forming the first spacer insulation patterns (SS1), bits within the first trenches (T1) Lines (BL) can be formed.
[0140] Forming bit lines (BL) may include depositing a conductive film on the inner walls of the first trenches (T1) and then removing the conductive film so that the side walls of the first isolation insulation patterns (STI1) are exposed on the inner walls of the first trenches (T1).
[0141] The bit lines (BL) formed in this manner may extend in a third direction (D3) perpendicular to the upper surface of the substrate (100) and may be separated from each other in a first direction (D1) by first isolation insulation patterns (STI1). Each of the bit lines (BL) may come into contact with the first dopant regions of the channel patterns (SP). The bit lines (BL) may include at least one of doped silicon, metal materials, metal nitride films, and metal silicides. For example, the bit lines (BL) may include tantalum nitride or tungsten.
[0142] After forming bit lines (BL), line separation insulation patterns (120) may be formed within the first trenches (T1). The line separation insulation patterns (120) may extend along the first direction (D1) on the substrate (100). The line separation insulation patterns (120) may cover the sidewalls of the bit lines (BL) and the sidewalls of the first separation insulation patterns (STI1). The line separation insulation patterns (120) may be one of insulating materials formed using SOG (Spin On Glass) technology, silicon oxide films, and silicon oxynitride films.
[0143] Referring to FIG. 8 and FIG. 20c, the second semiconductor films (20) of the third mold structure in the second region (WCR) can be replaced with pads (PAD) of word lines (WL) (S60).
[0144] In detail, referring to FIG. 20c, the process of replacing with word line pads (PADs) may include forming a mask pattern (not shown) covering a first region (BCR), forming trenches penetrating a third mold structure (MS3) in a second region (WCR), and performing an isotropic etching process on the second semiconductor films (20) exposed through the trenches. Here, the trenches may be formed by removing a portion of the first preliminary line patterns (103) in the second region (WCR). As the isotropic etching process is performed on the second semiconductor films (20), empty spaces may be defined between the pad insulating films (PLDs) in the second region (WCR). Subsequently, word line pads (PADs) that are vertically separated from each other may be formed by depositing a conductive film to fill the empty spaces and then removing the conductive film from the inner walls of the trenches. After forming word line pads (PAD), second line insulation patterns (113) covering the side walls of the word line pads (PAD) can be formed within the trenches.
[0145] Next, a buried insulating film (110) covering the stepped structure of the stacked structure may be formed in the second region (WCR), and an etch stop film (ESL) conformally covering the stepped structure may be formed before forming the buried insulating film (110).
[0146] Referring to FIG. 8, after forming word line pads (PAD) and a buried insulating film (110), capacitors can be formed in a first region (BCR) (S70).
[0147] In detail, referring to FIGS. 20a, 20b, and 20c, a second trench (T2) can be formed to expose the substrate (100) by removing the second pre-line patterns (105) from the first region (BCR). Here, the sidewalls of the first sacrifice patterns (31), the sidewalls of the channel patterns (SP), and the sidewalls of the interlayer insulation patterns (ILD) can be exposed in the second trenches (T2).
[0148] Afterwards, a fifth horizontal region (HR5) can be formed to expose buffer patterns (40) by removing the first sacrifice patterns (31) exposed in the second trenches (T2).
[0149] Forming the fifth horizontal regions (HR5) may include performing an etching process having etch selectivity for the substrate (100), channel patterns (SP), and interlayer insulation patterns (ILD) to isotropically etch the first sacrificial patterns (31). When isotropically etching the first sacrificial patterns (31), buffer patterns (40) may be used as etch stop films.
[0150] Fifth horizontal regions (HR5) can be formed vertically between the interlayer insulation patterns (ILD) and the channel patterns (SP), and horizontally between the second isolation insulation patterns (STI2), respectively. A first conductivity type dopant (e.g., phosphorus or boron) can be doped into parts of the channel patterns exposed in the fifth horizontal regions (HR5). Accordingly, second dopant regions (see SD2 in FIGS. 3a and 3b) can be formed in the channel patterns (SP).
[0151] Next, referring to FIGS. 4, FIGS. 5a, and FIGS. 5b, storage electrodes (SE) can be locally formed within the fifth horizontal regions (HR5).
[0152] Forming storage electrodes (SE) may include depositing a conductive film conformally covering the inner walls of the fifth horizontal regions (HR5) and the inner walls of the second trenches (T2), and removing portions of the conductive film deposited on the inner walls of the second trenches (T2) to leave locally conductive patterns within the fifth horizontal regions (HR5).
[0153] Storage electrodes (SE) may be spaced apart from each other in a first direction (D1), a second direction (D2), and a third direction (D3). Storage electrodes (SE) may be in contact with channel patterns (SP) exposed in the fifth horizontal regions (HR5). Each of the storage electrodes (SE) may define a void space within the fifth horizontal regions (HR5). In other words, each of the storage electrodes (SE) may have a long axis in the second direction (D2) and may have a hollow cylinder shape. Alternatively, the storage electrode (SE) may have a pillar shape with a long axis in the second direction (D2). The storage electrode (SE) may comprise at least one of a metal material, a metal nitride film, and a metal silicide.
[0154] Subsequently, a capacitor dielectric film (CIL) may be formed conformally covering the fifth horizontal regions (HR5) where the storage electrodes (SE) are formed, and a plate electrode (PE) may be formed to fill the storage electrodes (SE), the fifth horizontal regions (HR5) where the capacitor dielectric film (CIL) is formed, and the second trenches (T2).
[0155] Referring to FIGS. 8, FIGS. 4, FIGS. 5a, and FIGS. 5b, after forming capacitors in the first region (BCR), cell contact plugs (CPLG) connected to word line pads (PAD) in the second region (WCR) can be formed (S70).
[0156] Cell contact plugs (CPLG) connected to each of the pads (PAD) of the word line (WL) may be formed. The cell contact plugs (CPLG) may include metal and / or metal nitride.
[0157] When forming cell contact plugs (CPLG), contact holes can be formed that penetrate the interlayer insulating films (130, 140, 150, 160) and the flat insulating film (120) to expose the pads (PAD) of each word line (WL).
[0158] FIG. 21 is a flowchart illustrating a method for manufacturing a cell array structure of a semiconductor memory device according to embodiments of the present invention.
[0159] Referring to FIG. 21, as described with reference to FIG. 9a, 9b, and 9c, a first mold structure can be formed in the first and second regions (BCR, WCR) (S11).
[0160] Next, as described with reference to FIGS. 10a to 15c, channel patterns and a second mold structure can be formed in the first region (BCR) (S21).
[0161] After forming channel patterns in the first region (BCR), a second mold structure can be formed in the second region (WCR) (S31). That is, in the second region (WCR), the second mold structure (MS2) may include sacrificial patterns (30) and interlayer insulation patterns (ILD) between them, in each of the vertically adjacent pre-channel membranes (21).
[0162] A pad trimming process for the second mold structure can be performed in the second region (WCR) (S41). As described with reference to FIGS. 17a, 17b, and 17c, the pad trimming process can form a stepped structure by repeating the patterning process for the second mold structure in the second region (WCR).
[0163] Next, word lines can be formed in the first region (BCR), and word line pads (PAD) can be formed in the second region (WCR) (S51). Forming the word lines and word line pads (PAD) may include a process of simultaneously replacing the sacrificial patterns (30) of the second mold structure with a conductive material in the first and second regions (BCR, WCR). That is, the word lines and word line pads (PAD) can be formed simultaneously.
[0164] Subsequently, bit lines and capacitors may be formed in the first region (BCR) (S61). Bit lines may be formed perpendicular to the upper surface of the substrate (100) in the first region (BCR), as described with reference to FIGS. 19a, 19b, and 19c. Forming capacitors may include forming storage electrodes (SE) in contact with channel patterns (SP), as described with reference to FIGS. 20a, 20b, and 20c, and forming a capacitor dielectric film (CIL) and a plate electrode (PE) as shields covering the storage electrodes (SE).
[0165] FIGS. 22a to 22f are perspective views illustrating a pad trimming process in a method for manufacturing a cell array structure according to embodiments of the present invention.
[0166] Before performing the pad trimming process, a third mold structure including pad insulation patterns (PLD) and second semiconductor films (20) may be formed in a second region (WCR), as previously described with reference to FIG. 16e. The third mold structure may be placed between the first and second preliminary line patterns (103, 105). For example, the second semiconductor films (20) may be made of a material having etch selectivity with respect to the pad insulation patterns (PLD) and the first and second preliminary line patterns (103, 105).
[0167] Referring to FIG. 22a, a pad mask pattern (TPR) covering the third mold structure and the first and second preliminary line patterns (103, 105) in the first and second regions (BCR, WCR) can be formed.
[0168] The pad mask pattern (TPR) can expose a portion of the third mold structure and a portion of the first and second preliminary line patterns (103, 105) in the second region (WCR). The thickness of the pad mask pattern (TPR) may be greater than the width of the second region (WCR). The pad mask pattern (TPR) may be formed of a material having etch selectivity for the third mold structure and the first and second preliminary line patterns (103, 105). For example, the pad mask pattern (TPR) may be one of organic materials or one of photoresist materials.
[0169] Referring to FIG. 22b, a first etching process can be performed to etch the pad insulation pattern (PLD) and the first and second preliminary line patterns (103, 105) using a pad mask pattern (TPR) as an etching mask. During the first etching process, the second semiconductor film (20) under the pad insulation pattern (PLD) can be used as an etching stop film.
[0170] Referring to FIG. 22c, a second etching process can be performed to etch the second mask film (20) using a pad mask pattern (TPR) as an etching mask. During the second etching process, a pad insulation pattern (PLD) under the second semiconductor film (20) can be used as an etching stop layer. By performing the first and second etching processes, the lengths of the pad insulation pattern and the second semiconductor film are reduced so that the first step can be formed.
[0171] Referring to FIG. 22d, a mask trimming process that reduces the pad mask pattern (TPR) can be performed.
[0172] The mask trimming process can reduce the area of the pad mask pattern (TPRa) by horizontally moving one sidewall of the pad mask pattern (TPR) toward the first region (BCR) by a predetermined distance. Here, in the first direction (D1), the horizontal movement distance of the sidewall of the pad mask pattern (TPR) can correspond to the width of the word line pad (PAD) described above. An isotropic dry or wet etching process for the pad mask pattern (TPR) can be performed through the mask trimming process.
[0173] Meanwhile, before performing the mask trimming process, the previously described first and second etching processes may be repeated two or more times, and in this case, the sidewalls of two or more second semiconductor films (20) may be vertically aligned to form a single stair.
[0174] Referring to FIG. 22e, a first etching process can be performed to etch the pad insulation pattern (PLD) and the first and second preliminary line patterns (103, 105) using the first trimmed pad mask pattern (TPRa) as an etching mask, as previously described with reference to FIG. 22b.
[0175] Referring to FIG. 22f, a second etching process can be performed to etch the second semiconductor film (20) using the first trimmed pad mask pattern (TPRa) as an etching mask. A second step can be formed by performing the first and second etching processes using the first trimmed pad mask pattern (TPRa).
[0176] Subsequently, the mask trimming process, the first etching process, and the second etching process may be repeated in sequence, and accordingly, as described above with reference to FIG. 17a, FIG. 17b, and FIG. 17c, a third mold structure (MS3) having a staircase structure may be formed in the second region (WCR).
[0177] FIGS. 23a and FIGS. 23b are perspective views illustrating a structure formed by a pad trimming process according to embodiments of the present invention.
[0178] Referring to FIG. 23a, after a first etching process in which the pad insulating film and the first and second preliminary line patterns are etched using a pad mask pattern, the levels of the upper surface of the second semiconductor film exposed at each step and the upper surfaces of the first and second preliminary line patterns may differ from each other. That is, as shown in FIG. 23a, the upper surfaces of the first and second preliminary line patterns may be located at a higher level than the upper surface of the second semiconductor film (20). After the first etching process in the pad trimming process, the first and second preliminary line patterns may have an upwardly convex, rounded upper surface.
[0179] Additionally, referring to FIG. 23b, after repeating the mask trimming process, the first etching process, and the second etching process for the first and second preliminary line patterns in sequence, the width of the first and second preliminary line patterns can be reduced as the step width decreases.
[0180] For example, in the first step, the first and second preliminary line patterns may have a first width (W1), and in the second step, the first and second preliminary line patterns may have a second width (W2) that is smaller than the first width (W1).
[0181] FIGS. 24a and FIGS. 24b are perspective views illustrating a structure formed by a pad trimming process according to embodiments of the present invention.
[0182] Referring to FIG. 24a, after a first etching process in which the pad insulating film and the first and second preliminary line patterns are etched using a mask pattern, the upper surfaces of the first and second preliminary line patterns may be located at a lower level than the upper surface of the second semiconductor film (20). After the first etching process in the pad trimming process, the first and second preliminary line patterns may have a rounded upper surface that is convex downward.
[0183] Additionally, as shown in FIG. 24b, that is, in the first step, the width of the second mask film may have a first width (Wa), and in the second step, the width of the second semiconductor film (20) may have a second width (Wb) that is smaller than the first width (Wa). That is, as the step decreases, the width of the second mask films may decrease.
[0184] FIGS. 25a to 25g are drawings for illustrating various arrangement structures of word line pads in a cell array structure according to embodiments of the present invention.
[0185] Referring to FIGS. 25a and 25b, a stacked structure is disposed on a substrate comprising a first region (BCR) and a second region (WCR). The second region (WCR) may include a first connection region (WCR1) located on one side of the first region (BCR) and a second connection region (WCR2) located on the other side of the first region (BCR).
[0186] As previously described with reference to FIGS. 4, 5a, and 5b, the stacked structure may include alternately stacked interlayer insulation patterns (ILD) and word lines (WL1, WL2). Additionally, each word line (WL1, WL2) may include a pad (PAD) connected to a cell contact plug (CPLGa, CPLGb) in a second region (WCR).
[0187] The word lines (WL1, WL2) can be formed to have a length that decreases as the distance from the substrate increases. In addition, from a planar perspective, any one of the word lines (WL1, WL2) may overlap with another word line (WL1, WL2) located below it.
[0188] Word lines (WL1, WL2) can be stacked to form a stepped structure in the first and second connection regions (WCR1, WCR2). In other words, pads (PAD) can form a stepped structure in the first and second connection regions (WCR1, WCR2).
[0189] According to the embodiments, the word lines (WL1, WL2) may include first and second word lines (WL1, WL2) alternately stacked on a substrate. In other words, the first word lines (WL1) may be odd-numbered word lines, and the second word lines (WL2) may be even-numbered word lines.
[0190] A pair of first and second word lines (WL1, WL2) that are vertically adjacent to each other may have vertically aligned side walls in each of the first and second regions (BCR, WCR). Referring to FIG. 25b, pads (PADs) of the first word lines (WL1) may be exposed in the first connecting region (WCR1), and pads (PADs) of the second word lines (WL2) may be exposed in the second connecting region (WCR2).
[0191] The first cell contact plugs (CPLGa) can be connected to the pads (PAD) of the first word lines (WL1) in the first connection area (WCR1), and the second cell contact plugs (CPLGb) can be connected to the pads (PAD) of the second word lines (WL2) in the second connection area (WCR2).
[0192] According to the embodiment illustrated in FIG. 25c, a stacked structure comprising alternately stacked first and second word lines (WL1, WL2) may be provided as described above. In the stacked structure, pads (PADs) of the first and second word lines (WL1, WL2) may all be exposed in a first region (BCR). Here, the pads (PADs) of the first word lines (WL1) may be located at a different level from the pads (PADs) of the second word lines (WL2). Additionally, the pads (PADs) of the first word lines (WL1) may be arranged along a first direction, and the pads (PADs) of the second word lines (WL2) may be arranged adjacent to the pads (PADs) of the first word lines (WL1) in a second direction. Accordingly, the first and second cell contact plugs can be connected to the pads (PAD) of the first and second word lines (WL1, WL2) in the second area (WCR).
[0193] Referring to FIG. 25d, pads (PADs) of the first and second word lines (WL1, WL2) may be distributed and placed in the first connection area (WCR1) and the second connection area (WCR2). For example, some of the pads (PADs) of the first word lines (WL1) may be placed in the first connection area (WCR1), and the remaining pads (PADs) of the first word lines (WL1) may be placed in the second connection area (WCR2).
[0194] Some of the pads (PADs) of the second word lines (WL2) may be placed in the first connection area (WCR1), and the remaining pads (PADs) of the second word lines (WL2) may be placed in the second connection area (WCR2). Furthermore, in each of the first and second connection areas (WCR1, WCR2), the pads (PADs) of the first and second word lines (WL1, WL2) may be placed adjacently in the second direction (D2).
[0195] Referring to FIG. 25e, the laminated structure may include a first portion extending in a first direction (D1) from a first region (BCR) and a second portion extending along a second direction (D2) from first and second connecting regions (WCR1, WCR2) and having a stepped structure.
[0196] In each of the first and second connection areas (WCR1, WCR2), the pads (PAD) of the first and second word lines (WL1, WL2) can be connected to the first and second cell plugs, respectively.
[0197] Referring to FIG. 25f, the laminated structure may have a T-shape in a planar view. Specifically, the laminated structure may include a first part extending in a first direction (D1) from a first connection area (WCR1) and a second part extending along a second direction (D2) from the first and second connection areas (WCR1, WCR2) and having a stepped structure. Here, the second part may have a stepped structure on both sides along the second direction (D2). In the second connection area (WCR2), the pads (PADs) of the first and second word lines (WL1, WL2) may be arranged in both directions.
[0198] Referring to FIG. 25g, the laminated structure may have an I-shape in a planar view. It may include a first part extending in a first direction (D1) from a first connection area (WCR1), a second part extending in a second direction (D2) from the first connection area (WCR1), and a third part extending in a second direction (D2) from a second connection area (WCR2).
[0199] Although embodiments of the present invention have been described above with reference to the attached drawings, those skilled in the art will understand that the present invention may be implemented in other specific forms without changing its technical concept or essential features. Therefore, the embodiments described above should be understood as illustrative in all respects and not restrictive.
Claims
Claim 1 A semiconductor memory device comprising: a lower film including a first region and a second region; and a stacked structure including word lines and interlayer insulating films alternately stacked in a direction perpendicular to the upper surface of the lower film, wherein the stacked structure has a step structure in the second region, and each of the word lines includes sub-gate electrodes extending along a first direction parallel to each other in the first region and a pad commonly connected to the sub-gate electrodes in the second region; channel patterns disposed between the sub-gate electrodes of each word line and spaced apart from each other in the first direction; and dummy insulating patterns disposed between the channel patterns adjacent in the first direction and between the sub-gate electrodes. Claim 2 A semiconductor memory device according to claim 1, wherein in each of the word lines, the thickness of the pad is greater than the thickness of each sub-gate electrode. Claim 3 A semiconductor memory device according to claim 1, further comprising a gate insulating film disposed between the interlayer insulating films and the sub-gate electrodes, wherein the pads of the word lines are in direct contact with the interlayer insulating films. Claim 4 A semiconductor memory device according to claim 1, comprising line insulation patterns disposed on both sides of the stacked structure and extending in a first direction parallel to the stacked structure, wherein each of the line insulation patterns has a step structure in the second region. Claim 5 A semiconductor memory device according to claim 1, wherein each of the line insulation patterns has a width that decreases as it moves away from the first region. Claim 6 A semiconductor memory device according to claim 1, wherein the pads of the word lines have a width that decreases as they move away from the first region. Claim 7 A semiconductor memory device according to claim 1, further comprising: bit lines extending in a direction perpendicular to the upper surface of the lower film across the word lines in the first region and connected to the first ends of the channel patterns; and data storage elements connected to the second ends of the channel patterns. Claim 8 A semiconductor memory device according to claim 7, wherein in each of the word lines, the pad includes a protrusion protruding between the sub-gate electrodes. Claim 9 A semiconductor memory device comprising: a lower film including a first region and a second region; a stacked structure including word lines and interlayer insulating films alternately stacked in a direction perpendicular to the upper surface of the lower film, wherein each of the word lines has sub-gate electrodes extending along a first direction parallel to each other in the first region and a pad in the second region, and wherein the stacked structure has a step structure in the second region; channel patterns stacked in the perpendicular direction across the word lines; bit lines extending in the perpendicular direction across the word lines in the first region and connected to first ends of the channel patterns; data storage elements connected to second ends of the channel patterns in the first region; cell contact plugs each connected to the pads of the word lines in the second region; and dummy insulating patterns disposed between the channel patterns adjacent in the first direction and between the sub-gate electrodes. Claim 10 In claim 9, each of the word lines is a semiconductor memory device having different thicknesses in the first region and the second region. Claim 11 A semiconductor memory device according to claim 9, further comprising a gate insulating film disposed between the interlayer insulating films and the word lines and between the channel patterns and the word lines in the first region. Claim 12 A semiconductor memory device according to claim 11, wherein in the second region, each of the pads of the word lines has an upper surface and a lower surface in contact with the interlayer insulating films. Claim 13 A semiconductor memory device according to claim 9, wherein the word lines include first and second word lines alternately arranged along the vertical direction, and the pads of the first word lines in the second region have side walls aligned with one side wall of the second word lines located below them. Claim 14 A semiconductor memory device according to claim 9, further comprising line insulation patterns disposed on both sides of the stacked structure and extending in a first direction parallel to the stacked structure, wherein the line insulation patterns have a stepped structure substantially identical to the stacked structure in the second region. Claim 15 A cell array structure comprising a memory cell array including memory cells arranged in three dimensions and first bonding pads connected to the memory cell array; and a peripheral circuit structure comprising peripheral circuits and second bonding pads connected to the peripheral circuits and bonded to the first bonding pads, wherein the cell array structure comprises: a lower film including a first region and a second region; a stacked structure comprising word lines and interlayer insulating films alternately stacked in a direction perpendicular to the upper surface of the lower film, wherein each of the word lines has a pad in the second region, the stacked structure has a step structure in the second region, and each of the word lines includes sub-gate electrodes extending along a first direction parallel to each other in the first region; and bit lines extending in the perpendicular direction across the word lines. A semiconductor memory device comprising: cell contact plugs each connected to the pads of the word lines in the second region, wherein the cell contact plugs are connected to the first bonding pads; channel patterns disposed between the sub-gate electrodes of each word line and spaced apart from each other in the first direction; and dummy insulation patterns disposed between the channel patterns adjacent in the first direction and between the sub-gate electrodes. Claim 16 A semiconductor memory device according to claim 15, wherein the word lines extend along a first direction from the first region to the second region, and the sub-gate electrodes are commonly connected to the pads of each word line. Claim 17 A semiconductor memory device according to claim 16, further comprising: channel patterns stacked in a direction perpendicular to the upper surface of the lower film in the first region and crossing the word lines; and data storage elements connected to the first ends of the channel patterns. Claim 18 A semiconductor memory device according to claim 17, further comprising a gate insulating film disposed between the sub-gate electrodes and the channel patterns. Claim 19 A semiconductor memory device according to claim 16, wherein the pad of each of the word lines comprises a protrusion disposed between the sub-gate electrodes. Claim 20 A semiconductor memory device according to claim 15, further comprising line insulation patterns disposed on both sides of the stacked structure and extending in a first direction parallel to the stacked structure, wherein the line insulation patterns have a stepped structure substantially identical to the stacked structure in the second region.
Citation Information
Patent Citations
Semiconductor memory devices
US20130044531A1
Three dimensional semiconductor memory device
KR1020220026654A
Memory device
KR1020220031321A