Method for producing organic-inorganic hybrid membranes and their use for CO2 separation
PL250610B1Active Publication Date: 2026-11-16POLITECHN SLASKA W GLIWICACH
View PDF 0 Cites 0 Cited by
Patent Information
- Application Number
- PL2025451667
- Authority / Receiving Office
- PL · PL
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2025-04-03
- Publication Date
- 2026-11-16
- Estimated Expiration
- 2045-04-03
Smart Images

Figure 00000006_0000
Abstract
The subject of the application is a method for obtaining hybrid organic-inorganic membranes, which consists in adding from 5g to 10g of poly(ether ether ketone) PEEK polymer dried at a temperature of 60°C to 80°C for 12h to 24h to concentrated 95% to 98% sulfuric acid in an amount of 50ml to 100ml, stirring at a speed of 300rpm to 500rpm for 1h to 3h at room temperature, then the process is carried out at a temperature of 40°C to 60°C for 3h to 8h, stirring again at a speed of 300rpm to 500rpm, the obtained polymer solution (55ml to 110ml) is added to 0.5l to 1l of ice-cold deionized water, stirring mechanically at a speed of 100rpm to 300rpm, the SPEEK powder thus obtained is filtered under vacuum, washed with 1 to 2 liters of deionized water until pH 7 is obtained, then dried at room temperature for a maximum of 24 hours, then in a vacuum dryer at a temperature of 60°C to 80°C for 12 to 24 hours,then the degree of sulfonation of PEEK (DS) is determined by back titration, then from 6g to 16g of SPEEK and from 0.03g to 0.70g of zeolite 4A are dried at 60°C to 80°C for 24h to 48h, then from 5g to 15g of SPEEK are dissolved in 100 ml of solvent and stirred at a speed of 300 rpm to 500 rpm at 25°C to 50°C for 12h to 24h, filtered and degassed using ultrasound for 5 min to 10 min, then from 5 ml to 10 ml of the mixture are poured into a Petri dish and the solvent is evaporated, the process is carried out at 60°C to 80°C for 6h to 12h, then heated at a temperature of 80°C to 100°C for another 6h to 12 hours and heated again for 24 hours to 48 hours at 100°C to 120°C in a vacuum dryer, after which 0.025g to 0.60g of zeolite is subjected to priming, activated zeolite particles 0.03g to 0.60g are dispersed in 0.5 ml to 2 ml of solvent, ultrasonically mixed for 1 hour to 2 hours,the homogeneous mixture thus obtained is added from 5% to 10% by weight of the polymer in the SPEEK membrane to the suspension and mixed mechanically at a speed of 100 rpm to 300 rpm for 4 h to 6 h at room temperature, then the solution is evaporated at a temperature of 100°C to 120°C and 0.5 ml to 1 ml of solvent is added, mixed mechanically at a speed of 100 rpm to 300 rpm for 0.5 h to 1 h, then 5 ml to 10 ml of 5% to 15% SPEEK solution in solvent is added in 3 portions and subjected to ultrasound for 1 h to 3 h, the prepared suspension is poured into a Petri dish, the solvent is evaporated at a temperature of 60°C to 80°C for 6 h to 12 h, heated again at a temperature of 80°C to 100°C for another 6 h to 12 hours, heated at 100°C to 120°C for 24 to 48 hours in a vacuum dryer. The application also covers the use of membranes obtained by the above method.