Fuse element, fuse device and protective element

TWI945180BActive Publication Date: 2026-11-11DEXERIALS CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
TW111108523
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-03-09
Filing Date
2022-03-09
Publication Date
2026-11-11
Estimated Expiration
2042-03-08

AI Technical Summary

Technical Problem

Conventional multilayer fuse units face issues with deformation and increased resistance when widened for reduced resistance, leading to potential breaking and delayed fusing during abnormal conditions.

Method used

A fuse unit design with a low-melting-point metal plate and high-melting-point metal layers, featuring a defective portion in the high-melting-point layers, ensures stability during reflow and rapid fusing during abnormalities.

Benefits of technology

The design prevents deformation and ensures quick fusing during overcurrents, maintaining shape stability and reducing fusing delays.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The fuse unit of the present invention comprises: a low-melting-point metal plate having a first main surface and a second main surface facing each other, and a first side surface and a second side surface connecting the first main surface and the second main surface and facing each other; a first high-melting-point metal layer deposited on the first main surface and the second main surface; and a second high-melting-point metal layer deposited on the first side surface and the second side surface; and the second high-melting-point metal layer having at least a partially defective portion.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] This invention relates to a fuse unit, a fuse element using the fuse unit, and a protection element. Priority is claimed based on Japanese Patent Application No. 2021-037365, filed on March 9, 2021, the contents of which are incorporated herein by reference. [Previous Technology]

[0002] As a current blocking element used to block the current path when an overcurrent exceeding the rated current flows through the circuit board, a fuse element is well known. This fuse element blocks the current path by melting the fuse unit itself due to heat. Furthermore, as a current blocking element used to block the current path when an abnormality other than overcurrent occurs in the circuit board, a protective element using a heating element (heater) is well known. This protective element is configured such that, when an abnormality other than overcurrent occurs, current flows through the heating element, causing the heating element to heat up, and the heat is used to melt the fuse unit.

[0003] As a fuse unit used for fuse elements and protective elements, it is well known that a multilayer fuse unit has a low-melting-point metal plate and a high-melting-point metal layer deposited on the surface of the low-melting-point metal plate. As is well known, this multilayer fuse unit has: a pair of first side edges, which are formed to be thicker than the main surface and face each other; and a pair of second side edges, which are formed to be thinner than the first side edges and face each other (Patent Document 1). In the protective element described in Patent Document 1, the second side edges are provided along the energizing direction. Compared to the case where the first side edges are provided along the energizing direction, it can be melted quickly with less heat energy. Previous Art Documents Patent Documents

[0004] Patent Document 1: Japanese Patent No. 6324684 [Summary of the Invention]

[0005] [The problem the invention aims to solve]

[0006] For fuse units, research has been conducted on widening the width relative to the current-carrying direction to reduce resistance. However, when the width of a previous multilayer fuse unit was increased, during reflow soldering to the electrodes or terminals of the fuse element or protective element, the following situation sometimes occurred: the low-melting-point metal plate melted, and the fuse unit deformed into a partially collapsed shape. The resistance value of the partially collapsed fuse unit increases, and it is also easier to apply temperature stress, thus raising concerns about an increased risk of breakage. Furthermore, if the width of the fuse unit is increased, there are concerns that it may be difficult to blow in the event of an abnormality such as overcurrent.

[0007] This invention was made in view of the above circumstances, and its object is to provide a fuse unit, a fuse element using the fuse unit, and a protective element, wherein even if the width of the fuse unit relative to the direction of current flow is widened, it is difficult for low-melting-point metal plates to melt and deform during reflow, and it can quickly melt and break in the event of abnormalities such as overcurrent. [Technical Means for Solving the Problem]

[0008] In order to solve the above-mentioned problems, the present invention provides the following means.

[0009] (1) A fuse unit of one embodiment of the present invention comprises: a low melting point metal plate having a first main surface and a second main surface facing each other, and a first side surface and a second side surface connecting the first main surface and the second main surface and facing each other; a first high melting point metal layer deposited on the first main surface and the second main surface; and a second high melting point metal layer deposited on the first side surface and the second side surface; and the second high melting point metal layer having at least a partially defective portion.

[0010] (2) In the state described in (1) above, the thickness of the second high-melting-point metal layer is thicker than that of the first high-melting-point metal layer. (3) In the state described in (1) or (2) above, the melting point of the material constituting the low-melting-point metal plate is in the range of 138°C or higher and 250°C or lower, and the melting point of the material constituting the first high-melting-point metal layer and the second high-melting-point metal layer is 100°C or higher than the melting point of the material constituting the low-melting-point metal plate. (4) In the state described in (1) to (3) above, the thickness of the second high-melting-point metal layer is in the range of 4 μm or higher and 40 μm or lower, and the thickness of the first high-melting-point metal layer is in the range of 3 μm or higher and 30 μm or lower.

[0011] (5) One embodiment of the present invention includes the fuse unit described in (1) to (4) above, wherein the fuse unit is arranged such that the first side and the second side extend in the direction along the energizing direction.

[0012] (6) One embodiment of the protective element of the present invention includes a fuse unit as described in (1) to (4) above, and a heating element for heating the fuse unit, wherein the fuse unit is arranged such that the first side and the second side extend in the direction along the energizing direction. [Effects of the Invention]

[0013] According to the present invention, a fuse unit, a fuse element using the fuse unit and a protection element can be provided. Even if the width of the fuse unit is widened relative to the direction of current flow, it is not easy for low melting point metal plates to melt and deform during reflow, and it can quickly melt and break when abnormalities such as overcurrent occur.

Implementation Method

[0015] Hereinafter, this embodiment will be described in detail with reference to the drawings as appropriate. In the following description, some features may be enlarged for ease of understanding, and the size ratios of the constituent elements may differ from the actual situation. The materials and dimensions illustrated in the following description are examples only, and the present invention is not limited to these; appropriate modifications can be made within the scope of achieving the effects of the present invention.

[0016] [First Embodiment] FIG1 is a perspective view of the fuse unit according to the first embodiment of the present invention, FIG2 is a top view of the fuse unit shown in FIG1, and FIG3 is a cross-sectional view along line III-III of FIG1.

[0017] As shown in Figures 1 to 3, the fuse unit 10 of this embodiment has a low-melting-point metal plate 11, a first high-melting-point metal layer 12a, 12b and a second high-melting-point metal layer 12c, 12d deposited on the low-melting-point metal plate 11. The second high-melting-point metal layers 12c, 12d have at least a partially damaged defect portion 13.

[0018] The low-melting-point metal plate 11 is a quadrilateral plate as viewed from above, having a first main surface 11a and a second main surface 11b facing each other, and four side surfaces connecting the first main surface 11a and the second main surface 11b. The four side surfaces are a first side surface 11c and a second side surface 11d, a third side surface 11e and a fourth side surface 11f facing each other. The thickness of the low-melting-point metal plate 11 is preferably 30 μm or more. The film thickness of the low-melting-point metal plate 11 can also be 60 μm or more, 100 μm or more, or 500 μm or more. The upper limit of the film thickness of the low-melting-point metal plate 11 can be arbitrarily selected, but for example, it can be 3000 μm or less. Depending on the needs, it can also be 2000 μm or less, 1500 μm or less, etc.

[0019] First high-melting-point metal layers 12a and 12b are respectively deposited on the first main surface 11a and the second main surface 11b of the low-melting-point metal plate 11. Second high-melting-point metal layers 12c and 12d are respectively deposited on the first side surface 11c and the second side surface 11d of the low-melting-point metal plate 11. The thickness Tc of the second high-melting-point metal layer 12c deposited on the first side surface 11c and the thickness Td of the second high-melting-point metal layer 12d deposited on the second side surface 11d are thicker than the thickness Ta of the first high-melting-point metal layer 12a deposited on the first main surface 11a and the thickness Tb of the first high-melting-point metal layer 12b deposited on the second main surface 11b (see Figure 3). The thickness Tc of the second high-melting-point metal layer 12c and the thickness Td of the second high-melting-point metal layer 12d are preferably in the range of 4 μm or more and 40 μm or less, more preferably in the range of 4 μm or more and 30 μm or less. The thickness Ta of the first high-melting-point metal layer 12a and the thickness Tb of the first high-melting-point metal layer 12b are preferably in the range of 3 μm or more and 30 μm or less, more preferably in the range of 3 μm or more and 20 μm or less. Furthermore, when the thicknesses Ta and Tb of the first high-melting-point metal layers 12a and 12b are set to 100, the thicknesses Tc and Td of the second high-melting-point metal layers 12c and 12d are preferably in the range of 110 or more and 150 or less, more preferably in the range of 120 or more and 140 or less.

[0020] The defect 13 is provided in the second high-melting-point metal layers 12c and 12d. In this embodiment, the shape of the defect 13 is a triangle in plan view (see Figure 2), but the shape of the defect 13 is not particularly limited. The shape of the defect 13 may be, for example, a semi-circle in plan view, or a quadrilateral (square, rectangle, trapezoid). In this embodiment, the depth of the defect 13 is set to the depth at which the low-melting-point metal plate 11 is exposed, but the depth of the defect 13 is not particularly limited. The depth of the defect 13 may be, for example, a depth at which the low-melting-point metal plate 11 is not exposed, or a depth at which a portion of the low-melting-point metal plate 11 is damaged. Furthermore, in this embodiment, the number of defects 13 is set to 2 in each of the second high-melting-point metal layers 12c and 12d, but the number of defects 13 is not particularly limited. The number of defects 13 may be, for example, 1, or 3 or more. The ratio of the total area of ​​the defective portion 13 to the area of ​​the second high-melting-point metal layers 12c and 12d is preferably greater than 0% and less than 50%.

[0021] The low-melting-point metal plate 11 preferably has a melting point below the heating temperature during reflow soldering when manufacturing fuse elements or protective elements. When the reflow temperature is between 240°C and 260°C, the melting point TL of the material constituting the low-melting-point metal plate 11 is preferably in the range of 138°C or higher and 250°C or lower. Depending on the need, the melting point TL may also be in the range of 138°C or higher and 218°C or higher and 250°C or lower. Furthermore, the melting point of the material constituting the low-melting-point metal plate 11 may also be the liquidus temperature of the material.

[0022] The material of the low-melting-point metal plate 11 is preferably tin or a tin alloy containing tin as a main component. In the aforementioned tin alloy, "main component" means that the tin content in the tin alloy is preferably 40% by mass or more, more preferably 60% by mass or more. The aforementioned tin content can also be 70% by mass or more, or 80% by mass or more. The upper limit of the aforementioned tin content can be arbitrarily selected, for example, it can be 99% by mass or less, or 97% by mass or less. Examples of tin alloys include Sn-Bi alloys, In-Sn alloys, and Sn-Ag-Cu alloys.

[0023] The high-melting-point metal layer 12 comprises a layer of metallic material melted by the molten material of the low-melting-point metal plate 11. When the material of the low-melting-point metal plate 11 is tin or a tin alloy, the material of the high-melting-point metal layer 12 is preferably at least one metal selected from the group consisting of zinc, antimony, aluminum, silver, gold, copper, nickel, cobalt, and iron, or an alloy with the aforementioned metal as the main component. In the aforementioned alloy, "main component" means that the content of the aforementioned metal in the alloy is preferably 40% by mass or more, more preferably 60% by mass or more. The content of the aforementioned metal can also be 70% by mass or more, or 80% by mass or more. The upper limit of the content of the aforementioned metal can be arbitrarily selected, for example, it can be 99% by mass or less, or 97% by mass or less. Examples of the aforementioned alloys include phosphor bronze, silver-palladium alloy, nickel-iron alloy, and nickel-cobalt alloy. From the viewpoint of improving the electrical conductivity of the fuse unit 10 under normal conditions, the material of the high melting point metal layer 12 is preferably any one of copper, copper alloy, silver and silver alloy.

[0024] Preferably, the melting point TH of the material constituting the high-melting-point metal layer 12 is at least 100°C higher than the melting point TL of the material constituting the low-melting-point metal plate 11. That is, the melting point of the high-melting-point metal layer 12 is preferably at least 100°C higher than that of the low-melting-point metal plate 11. The difference between the melting point TH and the melting point TL (melting point TH - melting point TL) is more preferably at least 500°C, and particularly preferably at least 800°C. The difference between the melting point TH and the melting point TL may also be less than 1500°C. Furthermore, the melting point TH is preferably in the range of 400°C or higher and 1700°C or lower. Depending on the need, the melting point TH may also be in the range of 400°C or higher and 600°C or lower, 600°C or higher and 1000°C or lower, or 1000°C or higher and 1600°C or lower.

[0025] The fuse unit 10 of this embodiment can be manufactured, for example, by coating the surface of a low-melting-point metal plate 11 with a high-melting-point metal that constitutes a high-melting-point metal layer 12. As a method for coating the low-melting-point metal plate 11 with a high-melting-point metal, an electroplating method can be used. Using the electroplating method, a strip-shaped low-melting-point metal plate can be continuously fed into a plating tank along its length to continuously obtain coated low-melting-point metal plates coated with a high-melting-point metal. Furthermore, in the coated low-melting-point metal plates obtained by the electroplating method, the electric field strength is relatively enhanced at the edge portion of the low-melting-point metal plate, that is, on the side portion in the width direction of the strip-shaped low-melting-point metal plate, resulting in a thicker high-melting-point metal layer 12. This allows for the obtaining of a strip-shaped coated low-melting-point metal plate where the thickness of the high-melting-point metal layer on the side portion is thicker than that on the main surface portion. The obtained elongated coated low-melting-point metal plate is cut to a specific length, and a defect 13 is formed on the side surface of the obtained coated low-melting-point metal plate, thereby producing the fuse unit 10 of this embodiment. Furthermore, the cutting of the coated low-melting-point metal plate and the formation of the defect 13 can be performed simultaneously, or the cutting of the coated low-melting-point metal plate can be performed after the formation of the defect 13.

[0026] The fuse unit 10 of this embodiment, configured as described above, has first high-melting-point metal layers 12a and 12b deposited on the first main surface 11a and the second main surface 11b of the low-melting-point metal plate 11, respectively, and second high-melting-point metal layers 12c and 12d deposited on the first side surface 11c and the second side surface 11d, respectively. Therefore, by arranging the fuse unit 10 such that the first side surface 11c and the second side surface 11d extend in the direction of current conduction, even if the width relative to the direction of current conduction is widened, the low-melting-point metal plate 11 is less likely to melt and deform during resoldering, and the shape is stable after resoldering. Furthermore, the second high-melting-point metal layers 12c and 12d have defects 13. In this way, when an abnormality such as overcurrent occurs, the second high-melting-point metal layers 12c and 12d are pre-broken by the defect 13, thus preventing the delay in melting time caused by the melting residue of these layers.

[0027] In the fuse unit 10 of this embodiment, when the thicknesses Tc and Td of the second high melting point metal layers 12c and 12d are thicker than the thicknesses Ta and Tb of the first high melting point metal layers 12a and 12b, the strength of the fuse unit 10 is further improved and the shape after resoldering is more stable.

[0028] In the fuse unit 10 of this embodiment, when the melting point of the material constituting the low-melting-point metal plate 11 is in the range of 138°C or higher and 250°C or lower, when an abnormality such as overcurrent occurs, molten material of the low-melting-point metal plate 11 is easily generated, and the melting speed is faster when an abnormality occurs. Furthermore, when the melting point of the material constituting the first high-melting-point metal layer 12a, 12b and the second high-melting-point metal layer 12c, 12d is 100°C or higher than the melting point of the material constituting the low-melting-point metal plate 11, the first high-melting-point metal layer 12a, 12b and the second high-melting-point metal layer 12c, 12d are less likely to melt during resoldering, and the shape after resoldering is more stable.

[0029] In the fuse unit 10 of this embodiment, when the thicknesses Tc and Td of the second high melting point metal layers 12c and 12d are in the range of 4 μm or more and 40 μm or less, and the thicknesses Ta and Tb of the first high melting point metal layers 12a and 12b are in the range of 3 μm or more and 30 μm or less, the stability of the shape after reflow and the melting speed in case of abnormality will be improved in a better balance.

[0030] In the fuse unit 10 of this embodiment, the third side 11e and the fourth side 11f of the low melting point metal plate 11 are not laminated with a high melting point metal layer, but a high melting point metal layer may be laminated on the third side 11e and the fourth side 11f of the low melting point metal plate 11. In this case, there is no particular limitation on the thickness of the high melting point metal layer laminated on the third side 11e and the fourth side 11f, and it may be thicker than or thinner than the thickness Tc and Td of the second high melting point metal layers 12c and 12d.

[0031] The fuse unit 10 of this embodiment may also be coated with flux. Coating with flux prevents oxidation of the fuse unit 10. Therefore, when using solder or other bonding materials to connect the fuse unit 10 to the electrodes or terminals of the fuse element and protection element, the wettability of the fuse unit 10 relative to the bonding material is improved. Furthermore, by coating with flux, the adhesion of molten metal generated by arc discharge can be suppressed, thereby improving the insulation performance of the fuse unit 10 after it melts.

[0032] [Second Embodiment] FIG4 is a perspective view of the fuse element according to the second embodiment of the present invention, and FIG5 is a cross-sectional view along line VV of FIG4.

[0033] As shown in Figures 4 and 5, the fuse element 20 of this embodiment includes: an insulating substrate 21; a first electrode 22 and a second electrode 23 disposed at opposite ends of the insulating substrate 21; and a fuse unit 10 that electrically connects the first electrode 22 and the second electrode 23. Current flows between the first electrode 22 and the second electrode 23 via the fuse unit 10. The fuse unit 10 is configured such that the first side surface 11c and the second side surface 11d of the low-melting-point metal plate 11 extend in the direction of current flow (current-carrying direction) of the fuse element 20. That is, the second high-melting-point metal layers 12c and 12d of the fuse unit 10 are connected to the first electrode 22 at one end and to the second electrode 23 at the other end.

[0034] The insulating substrate 21 is not particularly limited as long as it has electrical insulation properties. Well-known insulating substrates such as resin substrates, ceramic substrates, and composite substrates of resin and ceramic can be used as circuit boards. Examples of resin substrates include epoxy resin substrates, phenolic resin substrates, and polyimide substrates. Examples of ceramic substrates include alumina substrates, glass-ceramic substrates, aluminum-rich andalusite substrates, and zirconia substrates. Examples of composite substrates include glass epoxy boards.

[0035] The first electrode 22 has an upper surface electrode 22a formed on the upper surface 21a of the insulating substrate 21, a lower surface electrode 22b formed on the lower surface 21b of the insulating substrate 21, and a castle-shaped structure 22c connecting the upper surface electrode 22a and the lower surface electrode 22b. The connection between the upper surface electrode 22a and the lower surface electrode 22b is not limited to the castle-shaped structure; a through-hole can also be used for connection. The second electrode 23 is similar, having an upper surface electrode 23a, a lower surface electrode 23b, and a castle-shaped structure 23c. The first electrode 22 and the second electrode 23 are formed by conductive patterns such as silver wiring and copper wiring, respectively. The surfaces of the first electrode 22 and the second electrode 23 can also be covered with an electrode protective layer to suppress the deterioration of electrode characteristics due to oxidation, etc. As the material of the electrode protective layer, materials such as Sn plating film, Ni / Au plating film, Ni / Pd plating film, and Ni / Pd / Au plating film can be used.

[0036] The fuse unit 10 is electrically connected to the first electrode 22 and the second electrode 23 via a bonding material 24 such as solder. An insulating barrier 25 is provided along the bonding material 24 on the surface electrode 22a of the first electrode 22 and the surface electrode 23a of the second electrode 23. This insulating barrier 25 prevents the bonding material 24 from melting and flowing outwards. Furthermore, the insulating barrier 25 also prevents the solder or other bonding material used when mounting the fuse element 20 onto the circuit board from flowing into the fuse unit.

[0037] The fuse element 20 may also be fitted with a cover. By installing the cover, the interior of the fuse element 20 can be protected, and the molten material generated when the fuse unit 10 blows can be prevented from scattering. Various engineering plastics and ceramics can be used as materials for the cover.

[0038] The fuse element 20 is mounted on the current path of the circuit board across the first electrode 22 and the second electrode 23. During the period when a current below the rated value flows in the current path of the circuit board, the low-melting-point metal plate 11 of the fuse unit 10 of the fuse element 20 does not melt. On the other hand, when an overcurrent exceeding the rated value flows in the current path of the circuit board, the low-melting-point metal plate 11 of the fuse unit 10 heats up and melts. The melt thus generated causes the first high-melting-point metal layers 12a and 12b to melt, and the second high-melting-point metal layers 12c and 12d are broken starting from the defect 13 of the second high-melting-point metal layers 12c and 12d, thereby blowing the fuse unit 10. Moreover, by blowing the fuse unit 10, the connection between the first electrode 22 and the second electrode 23 is broken, thereby blocking the current path of the circuit board.

[0039] The fuse element 20 of this embodiment, configured as described above, uses the aforementioned fuse unit 10 as the fuse unit, and the second high-melting-point metal layers 12c and 12d deposited on the first side 11c and second side 11d of the low-melting-point metal plate 11 of the fuse unit 10 are arranged to extend in the direction of current flow (current-carrying direction) of the fuse element 20. Therefore, during reflow soldering when manufacturing the fuse element 20, the second high-melting-point metal layers 12c and 12d support the low-melting-point metal plate 11, thus preventing the low-melting-point metal plate 11 from melting and deforming, and ensuring the shape of the fuse unit 10 remains stable after reflow. Furthermore, in the event of overcurrent, the second high-melting-point metal layers 12c and 12d are pre-broken by the defective portion 13, thus preventing delays in melting time caused by melting residues.

[0040] [Third Embodiment] FIG6 is an exploded perspective view of the fuse element according to the third embodiment of the present invention, and FIG7 is a cross-sectional view along line VII-VII of FIG6.

[0041] As shown in Figures 6 and 7, the fuse element 30 of this embodiment includes a lower housing 31, an upper housing 32, a first terminal 33, a second terminal 34, and a fuse unit 10a electrically connecting the first terminal 33 and the second terminal 34. Current flows between the first terminal 33 and the second terminal 34 via the fuse unit 10a. The fuse unit 10a is identical to the fuse unit 10, having a low-melting-point metal plate 11, and first high-melting-point metal layers 12a, 12b and second high-melting-point metal layers 12c, 12d deposited on the low-melting-point metal plate 11. Components in the fuse unit 10a that are identical to those in the fuse unit 10 are given the same reference numerals and their descriptions are omitted. The fuse unit 10a is arranged such that the first side surface 11c and the second side surface 11d of the low-melting-point metal plate 11 extend in the direction of current flow (current-carrying direction) of the fuse element 20. Furthermore, a second high-melting-point metal layer 12c is laminated on the first side 11c of the low-melting-point metal plate 11, and a second high-melting-point metal layer 12d is laminated on the first side 11d of the low-melting-point metal plate 11. That is, the second high-melting-point metal layers 12c and 12d of the fuse unit 10a are arranged such that one end is connected to the first terminal 33 and the other end is connected to the second terminal 34.

[0042] The lower housing 31 and the upper housing 32 only need to be electrically insulating, and their materials are not particularly limited. Resin, ceramic, or a composite of resin and ceramic can be used. The resin is preferably a resin with a high glass transition temperature. As for the resin with a high glass transition temperature, nylon-based resin is preferred because it has higher tracking resistance. Among nylon-based resins, nylon 46, nylon 6T, and nylon 9T are particularly preferred.

[0043] The first terminal 33 has an external terminal hole 33a. The second terminal 34 also has an external terminal hole 34a. Materials for the first terminal 33 and the second terminal 34 can include, for example, copper, brass, nickel, etc. From the viewpoint of strengthening rigidity, brass is preferred for the first terminal 33 and the second terminal 34; from the viewpoint of reducing resistance, copper is preferred. The materials for the first terminal 33 and the second terminal 34 can be the same or different.

[0044] The fuse unit 10a has a defect 13a on each of the second high melting point metal layers 12c and 12d. Furthermore, the defect 13a is trapezoidal in shape.

[0045] The fuse element 30 is mounted on the current path of the circuit board via the first terminal 33 and the second terminal 34. During the period when a current below the rated value flows in the current path of the circuit board, the low-melting-point metal plate of the fuse unit 10a of the fuse element 30 does not melt. On the other hand, when an overcurrent exceeding the rated value flows in the current path of the circuit board, the low-melting-point metal plate 11 of the fuse unit 10a heats up and melts. The melt thus generated causes the first high-melting-point metal layers 12a and 12b to melt, and the second high-melting-point metal layers 12c and 12d break from the defect portion 13a of the second high-melting-point metal layers 12c and 12d, thereby blowing the fuse unit 10a. Moreover, the fuse unit 10a blows and the connection between the first terminal 33 and the second terminal 34 is broken, thereby blocking the current path of the circuit board.

[0046] Assuming the fuse element 30 of this embodiment with the above configuration uses the aforementioned fuse unit 10a as the fuse unit, and the second high-melting-point metal layers 12c and 12d of the fuse unit 10a are arranged to extend in the direction of current flow (current-carrying direction) of the fuse element 30. Therefore, during reflow soldering when manufacturing the fuse element 30, the second high-melting-point metal layers 12c and 12d support the low-melting-point metal plate 11, thus making it difficult for the low-melting-point metal plate 11 to melt and deform, and the shape of the fuse unit 10a remains stable after reflow. Furthermore, in the event of overcurrent, the second high-melting-point metal layers 12c and 12d are pre-broken by the defective portion 13a, thus preventing delays in fusing time caused by melting residues.

[0047] [Fourth Embodiment] FIG8 is an exploded perspective view of the protective element according to the fourth embodiment of the present invention, FIG9 is a cross-sectional view along line IX-IX of FIG8, and FIG10 is a cross-sectional view along line XX of FIG8. As shown in FIG8 to FIG10, the protective element 40 of this embodiment includes: an insulating substrate 21; a first electrode 22 and a second electrode 23, which are disposed at a pair of opposite ends of the insulating substrate 21; and a fuse unit 10, which electrically connects the first electrode 22 and the second electrode 23. The insulating substrate 21, the first electrode 22, the second electrode 23, and the fuse unit 10 are the same as those of the fuse element 20 described above, and therefore are given the same reference numerals and detailed descriptions are omitted.

[0048] The protection element 40 further includes a third electrode 41, a heating element 42 connected to the third electrode 41, an insulating member 43 covering the heating element 42, and a fourth electrode 44. The fourth electrode 44 is connected to the heating element 42 at one end and is connected to the first high melting point metal layer 12b deposited on the second main surface 11b of the fuse unit 10 via a bonding material 45.

[0049] The third electrode 41 is supplied with current when an abnormality other than overcurrent occurs on the circuit board. The third electrode 41 has an upper surface electrode 41a formed on the upper surface 21a of the insulating substrate 21, a lower surface electrode 41b formed on the lower surface 21b of the insulating substrate 21, and a castle-shaped structure 41c connecting the upper surface electrode 41a and the lower surface electrode 41b. The connection between the upper surface electrode 41a and the lower surface electrode 41b is not limited to a castle-shaped structure, and can also be made using through holes. The third electrode 41 is formed by conductive patterns such as silver wiring and copper wiring. The surface of the third electrode 41 can also be covered by an electrode protective layer to suppress the deterioration of electrode characteristics caused by oxidation, etc. As the material of the electrode protective layer, materials such as Sn plating film, Ni / Au plating film, Ni / Pd plating film, and Ni / Pd / Au plating film can be used.

[0050] The heating element 42 is formed of a high-resistivity conductive material that generates heat by passing an electric current through it, and has relatively high resistance. As the high-resistivity conductive material, powders containing, for example, nickel-chromium alloys, W, Mo, Ru, or alloys, compositions, or compounds thereof can be used. The heating element 42 can be formed by, for example, by mixing the high-resistivity conductive material with a resin binder to form a paste, using screen printing technology to form a pattern on the surface 21a of the insulating substrate 21, and then calcining it.

[0051] Glass, for example, can be used as the material for the insulating member 43. The fourth electrode 44 is arranged to face the heating element 42 with the insulating member 43 in between. Solder, for example, can be used as the bonding material 45. With this arrangement, the heating element 42 overlaps with the fuse unit 10 with the insulating member 43, the fourth electrode 44, and the bonding material 45 in between. By providing this overlapping structure, the heat generated by the heating element 42 can be efficiently conducted to the fuse unit 10 within a small area.

[0052] The protective element 40 may also be fitted with a cover. By installing the cover, the interior of the protective element 40 can be protected, and the molten material generated when the fuse unit 10 blows can be prevented from scattering. Various engineering plastics and ceramics can be used as materials for the cover.

[0053] The protection element 40 is mounted on the current path of the circuit board via the first electrode 22 and the second electrode 23. During the period when a current below the rated current flows in the current path of the circuit board, the low-melting-point metal plate 11 of the fuse unit 10 of the protection element 40 melts. On the other hand, when an overcurrent exceeding the rated current flows in the current path of the circuit board, the low-melting-point metal plate 11 of the fuse unit 10 heats up and melts. The resulting melt causes the first high-melting-point metal layers 12a and 12b to melt, and the second high-melting-point metal layers 12c and 12d are broken starting from the defect 13 of the second high-melting-point metal layers 12c and 12d, thereby blowing the fuse unit 10. Moreover, the fuse unit 10 blows and the connection between the first electrode 22 and the second electrode 23 is broken, thereby blocking the current path of the circuit board.

[0054] Furthermore, when an abnormality occurs in the circuit board, the protection element 40 energizes the heating element 42 via the third electrode 41 through the current control element provided in the circuit board. The heating element 42 heats up due to this energization. This heat is then conducted to the fuse unit 10 via the insulating member 43, the fourth electrode 44, and the bonding material 45. This heat melts the low-melting-point metal plate 11 of the fuse unit 10, generating a molten material. This molten material causes the first high-melting-point metal layers 12a and 12b to melt, and the second high-melting-point metal layers 12c and 12d break, starting from the defect 13 of the second high-melting-point metal layers 12c and 12d, thereby blowing the fuse unit 10. Moreover, the blowing of the fuse unit 10 breaks the connection between the first electrode 22 and the second electrode 23, thereby blocking the current path of the circuit board.

[0055] Assuming the protection element 40 of the fourth embodiment of the present invention, configured as described above, uses the aforementioned fuse unit 10 as the fuse unit, and the second high-melting-point metal layers 12c and 12d of the fuse unit 10 are arranged to extend in the direction of current flow (current-carrying direction) of the fuse element 20. Therefore, during reflow soldering when manufacturing the protection element 40, the second high-melting-point metal layers 12c and 12d support the low-melting-point metal plate 11, thus preventing the low-melting-point metal plate 11 from melting and deforming, and ensuring the shape of the fuse unit 10 remains stable after reflow. Furthermore, in the event of an overcurrent or other abnormality, the second high-melting-point metal layers 12c and 12d are pre-broken by the defective portion 13, thus preventing delays in melting time caused by melting residues. [Simplified Explanation of the Diagram]

[0014] Figure 1 is a perspective view of the fuse unit according to the first embodiment of the present invention. Figure 2 is a top view of the fuse unit shown in Figure 1. Figure 3 is a cross-sectional view along line III-III of Figure 1. Figure 4 is a perspective view of the fuse element according to the second embodiment of the present invention. Figure 5 is a cross-sectional view along line VV of Figure 4. Figure 6 is an exploded perspective view of the fuse element according to the third embodiment of the present invention. Figure 7 is a cross-sectional view along line VII-VII of Figure 6. Figure 8 is an exploded perspective view of the protection element according to the fourth embodiment of the present invention. Figure 9 is a cross-sectional view along line IX-IX of Figure 8. Figure 10 is a cross-sectional view along line XX of Figure 8.

Claims

1. A fuse unit comprising: a low-melting-point metal plate having a first main surface and a second main surface facing each other, and a first side surface and a second side surface connecting the first main surface and the second main surface and facing each other; a first high-melting-point metal layer deposited on the first main surface and the second main surface; and a second high-melting-point metal layer deposited on the first side surface and the second side surface; wherein the second high-melting-point metal layer has at least a partially defective portion, and the thickness of the second high-melting-point metal layer is thicker than that of the first high-melting-point metal layer.

2. The fuse unit of claim 1, wherein the depth of the defect is the depth of the exposed low-melting-point metal plate, and the number of defects is the number of defects whose area is less than 50% of the area of ​​each of the second high-melting-point metal layers.

3. The fuse unit of claim 1, wherein the melting point of the material constituting the low melting point metal plate is in the range of 138°C or higher and 250°C or lower, and the melting point of the material constituting the first high melting point metal layer and the second high melting point metal layer is 100°C or higher than the melting point of the material constituting the low melting point metal plate.

4. The fuse unit of claim 1, wherein the thickness of the second high melting point metal layer is in the range of 4 μm or more and 40 μm or less, and the thickness of the first high melting point metal layer is in the range of 3 μm or more and 30 μm or less.

5. A fuse element comprising a fuse unit as claimed in any one of claims 1 to 4, wherein the fuse unit is arranged such that the first side and the second side extend in the direction of energization.

6. A protective element having a fuse unit as claimed in any one of claims 1 to 4, and a heating element for heating the fuse unit, wherein the fuse unit is arranged such that the first side and the second side extend in the direction of energization.

Citation Information

Patent Citations

  • Protective element

    TW201517105A

  • Manufacturing method of fusible conductor

    TW201522031A

  • Short element

    TW201526064A

  • Fuse element and fuse device

    US20200176210A1