Fittings and bags with fittings

TWI945408BActive Publication Date: 2026-11-11TAKIRON CORP
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
TW112109920
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-03-31
Filing Date
2023-03-17
Publication Date
2026-11-11
Estimated Expiration
2043-03-16

Smart Images

  • Figure TWG2TB001920153_001
    Figure TWG2TB001920153_001
  • Figure TWG2TB001920153_002
    Figure TWG2TB001920153_002
  • Figure TWG2TB001920153_003
    Figure TWG2TB001920153_003
Patent Text Reader

Abstract

A fitting and a bag body with the fitting are provided to suppress wrinkles during bag making and to meet the requirements of single material. The fitting includes: a convex fitting member having a convex fitting portion provided on the surface of a strip-shaped first substrate along the long side direction; and a concave fitting member having a concave fitting portion provided on the surface of a strip-shaped second substrate along the long side direction; the convex fitting portion and the concave fitting portion are fitted together in a detachable manner; the first substrate and the second substrate each include: a main layer; a sealing layer provided on the side of the main layer opposite to the convex fitting portion and the concave fitting portion; and an intermediate layer provided between the main layer and the sealing layer; both the first substrate and the second substrate are composed of polyethylene resin obtained by polymerization of monomers containing ethylene, and the rigidity is 5~30 N / mm as determined by the required measurement method.
Need to check novelty before this filing date? Find Prior Art

Description

Fittings and bags with fittings This invention relates to a fitting and a bag body with the fitting. Priority is claimed based on Japanese Patent Application No. 2022-060134, filed on March 31, 2022, the contents of which are incorporated herein by reference. In various fields such as food, pharmaceuticals, and groceries, bags with attached fittings are widely used. The aforementioned bag with attached fittings has a fitting that allows the opening to be freely opened and closed on the inner surface near the opening of the bag body. Examples of fittings include: a first fitting part and a second fitting part that can be fitted together to form a mutually detachable state on the opposing surfaces of a pair of strip substrates along the long side direction of their respective substrates (for example, Patent Document 1). In recent years, with the marine plastic problem as a primary concern, there have been calls for the reuse of used plastics. In the packaging industry, efforts are being made to develop "single-material" packaging, using a single material to improve recyclability. However, when inserts made of polyethylene resin are heat-sealed onto a bag body made of polyethylene film, thermal shrinkage occurs, causing the bag to wrinkle easily. To address the issue of wrinkles forming in the bag during heat sealing, one existing type of insert involves providing layers made of high-hardness resin on a portion of a pair of strip-shaped substrates. Specifically, one type of insert uses layers made of polyethylene or polypropylene resin on the surface and inside of the substrate, and uses an intermediate layer made of nylon or polyester resin with a higher hardness than the surface and inner layers between the surface and inner layers (e.g., Patent Document 2). [Prior Art Documents] [Patent Documents] [Patent Document 1] Japanese Patent Publication No. 2003-160147 [Patent Document 2] Japanese Patent Publication No. 06-122460 [Problem to be solved by the invention] However, the existing inserts described in Patent Document 2, although they have the effect of suppressing wrinkles during bag making, cannot meet the requirements of recycling, especially the requirements of single material, since they are not made of a single resin. The present invention was made in view of such circumstances, and its object is to provide an insert that suppresses wrinkles during bag making and can respond to the requirements of a single material. Another object is to provide a bag body with an insert using such an insert. [Means for solving the problem] The present invention includes the following aspects. [1] A fitting member, the fitting member having a convex fitting member and a concave fitting portion, wherein the convex fitting member is provided with a convex fitting portion along the long side direction on the surface of a strip-shaped first substrate, and the concave fitting member is provided with a concave fitting portion along the long side direction on the surface of a strip-shaped second substrate; the convex fitting portion and the concave fitting portion are fitted together in a detachable manner; the first substrate and the second substrate respectively have a main layer, a sealing layer and an intermediate layer, the sealing layer is respectively provided on the side opposite to the convex fitting portion of the main layer and on the side opposite to the concave fitting portion of the main layer, and the intermediate layer is provided between the main layer and the sealing layer; the first substrate and the second substrate are both composed of polyethylene resin obtained by polymerization of monomers containing ethylene, and the rigidity is 5 to 30 N / mm obtained by the following measurement method; rigidity: the convex fitting member is cut into a length of 70 mm to serve as a test piece; The tensile stress at 2% elongation was measured by gripping both ends of the long side of the test piece obtained by a tensile testing machine; the tensile stress was measured for 5 test pieces, and the arithmetic mean of the measured values ​​was used as the tensile stress (rigidity); the peel strength was measured under the conditions of a clamping distance of 50 mm and a test speed of 1 mm / min. [2] As described in [1], the aforementioned rigidity is 7 to 15 N / mm. [3] As described in [1] or [2], the density of the polyethylene resin constituting the aforementioned intermediate layer is 930 kg / m³. 3 The above. [4] The insert as described in [1] to [3], wherein the polyethylene resin constituting the aforementioned intermediate layer has a melting point of 125°C or higher. [5] A bag body with an insert, the bag body with the insert comprising: an insert as described in any one of [1] to [4]; and a bag body for containing contents; the bag body being composed of a polyethylene resin obtained by polymerizing a monomer containing ethylene; the insert being disposed on the inner surface of the bag body. [Effects of the Invention] According to the present invention, an insert that suppresses wrinkling during bag manufacturing and can respond to the requirement of a single material can be provided. Furthermore, a bag body with an attached insert using this type of insert can be provided. Since the insert and the bag body with the attached insert of the present invention are made of polyethylene resin (i.e., a single resin), the insert does not need to be separated from the bag body during reuse, resulting in good recycling efficiency. [Matching Component] Hereinafter, a fitting component of the present invention will be disclosed and described based on the drawings by way of an example. Furthermore, in the following description, the dimensions, etc., of the illustrated drawings are merely examples, and the present invention is not limited thereto, and may be appropriately modified and implemented without changing its spirit. As shown in Figures 1 and 2, one embodiment of the fitting member 1 includes: a convex fitting member 10, which has a convex fitting portion 12 on the surface 11a of the strip-shaped first substrate 11 along the long side direction; and a concave fitting member 20, which has a concave fitting portion 22 on the surface 21a of the strip-shaped second substrate 21 along the long side direction. The convex-side fitting portion 12 shown in Figures 1 and 2 includes: a main body 12a, which rises from the surface 11a of the first substrate 11 facing the second substrate 21; and a head 12b, which is located at the front end of the main body 12a and has a slightly semi-circular cross-section larger than the main body 12a. The concave-side fitting portion 22 includes: a pair of arms 22a and 22b, which rise from the surface 21a of the second substrate 21 facing the first substrate 11 with an arc-shaped cross-section, and a recess 22c is formed on the inner side of these arms 22a and 22b. The convex-side fitting portion 12 and the concave-side fitting portion 22 are fitted together in a detachable manner by the head 12b of the convex-side fitting portion 12 being inserted into the recess 22c of the concave-side fitting portion 22. Furthermore, the convex side fitting portion 12 and the concave side fitting portion 22 can be fitted in a way that allows for easy assembly and disassembly, and are not limited to the forms shown in Figures 1 and 2. As shown in FIG2, the first substrate 11 includes: a main layer 13; a sealing layer 14 disposed on the side of the main layer 13 opposite to the convex fitting portion 12 and the concave fitting portion 22; and an intermediate layer 15 disposed between the main layer 13 and the sealing layer 14. The material forming the main layer 13 is a polyethylene resin obtained by polymerizing monomers containing ethylene. Moreover, the monomers containing ethylene are not particularly limited and can be derived from fossil fuels or biomass. Furthermore, in this specification, "derived from biomass" is used to distinguish it from "derived from fossil fuels," referring to "organic resources derived from living organisms that exclude fossil fuels." Coal, oil, and natural gas are equivalent to fossil fuels. "Polyethylene-based resin" refers to a polymer having polyethylene structures derived from ethylene as its main constituent units. Furthermore, "main constituent unit" refers to a constituent unit that accounts for more than 50% by mass relative to 100% of all constituent units constituting the resin. In the following description, the polyethylene-based resin forming the main layer 13 will also be simply referred to as "polyethylene (A)". [Polyethylene (A)] Polyethylene (A) may contain not only units derived from ethylene, but also units derived from α-olefins. α-olefins may be derived from biomass or fossil fuels. Examples of α-olefins include at least one selected from the group consisting of propylene, 1-butene, 1-pentene, 1-hexene, 1-octene, 1-heptene, 4-methyl-1-pentene, 4-methyl-1-hexene, and 4,4-dimethyl-1-pentene. That is, when polyethylene (A) is a polymer having constituent units from ethylene and constituent units from α-olefins, polyethylene (A) can be a binary copolymer of ethylene and one polyolefin, a terpolymer of ethylene and two polyolefins, or a copolymer of ethylene and three or more polyolefins. Furthermore, without affecting the effects of the present invention, polyethylene (A) may have constituent units derived from monomers other than ethylene and α-olefins. Moreover, it is required that the proportion of other monomers in the total polyethylene (A) does not exceed 10%. Other monomers that can be listed include: vinyl esters, methacrylates, unsaturated carboxylic acids, anhydrous forms of unsaturated dicarboxylic acids, unsaturated dicarboxylic acid esters, (meth)acrylonitrile, styrene, etc. Examples of vinyl esters include: vinyl acetate, etc. Examples of methacrylates include: methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, butyl (meth)acrylate, etc. Examples of unsaturated carboxylic acids include: (meth)acrylic acid, etc. Examples of anhydrous forms of unsaturated dicarboxylic acids include: anhydrous maleic acid, etc. Examples of unsaturated dicarboxylic acid esters include: monomethyl maleate, dimethyl maleate, etc. Examples of other monomers include: (meth)acrylonitrile, styrene, etc. Furthermore, (meth)acrylic acid refers to acrylic acid or methacrylic acid. And (meth)acrylonitrile refers to acrylonitrile or methacrylonitrile. Specific examples of polyethylene (A) include, for example, low-density polyethylene (LDPE), very low-density polyethylene, high-pressure low-density polyethylene, medium-density polyethylene, high-density polyethylene, linear low-density polyethylene (LLDPE) of ethylene-α-olefin copolymers, etc. Among these, low-density polyethylene (LDPE) and linear low-density polyethylene (LLDPE) are preferred as the polyethylene (A) used for the main layer 13. The polyethylene (A) forming the main layer 13 can be one type or two or more types. [Physical properties of polyethylene (A)] Polyethylene (A) is preferably provided with the following physical properties. [Mel Flow Rate] The melt flow rate (MFR) of polyethylene (A) is preferably 0.5 g / 10 min or more, more preferably 1.0 g / 10 min or more, and even more preferably 1.5 g / 10 min or more. Furthermore, the MFR of polyethylene (A) is preferably 15 g / 10 min or less, more preferably 12 g / 10 min or less, and even more preferably 10 g / 10 min or less. The upper and lower limits of the MFR of polyethylene (A) can be combined arbitrarily. For example, the MFR of polyethylene (A) is preferably above 0.5 g / 10 min and below 15 g / 10 min. If the MFR of polyethylene (A) is greater than or equal to the lower limit of the aforementioned range, it is easy to form the insert of this embodiment. If the MFR of polyethylene (A) is less than or equal to the upper limit of the aforementioned range, it becomes easy to operate. Furthermore, in this embodiment, the MFR of the resin was measured according to JIS K 7210-1 under conditions of a temperature of 190°C and a load of 2.16 kg. [Density] The density of polyethylene (A) is preferably 890 kg / m³. 3 The above is preferred to be 905 kg / m³. 3 That's all. Furthermore, the density of polyethylene (A) is preferably 960 kg / m³. 3 The following is preferred: 950 kg / m 3 The optimal value is 940 kg / m³. 3 The following, especially 935kg / m 3 The following is preferred. The upper and lower limits of the density of polyethylene (A) can be combined arbitrarily. For example, the density of polyethylene (A) is preferably 890 kg / m³. 3 Above, 940kg / m 3 the following. If the density of polyethylene (A) is greater than or equal to the lower limit of the aforementioned range, the fitting of this embodiment is easy to form. If the density of polyethylene (A) is less than or equal to the upper limit of the aforementioned range, the fitting of this embodiment becomes soft and has an excellent user experience. Furthermore, in this embodiment, the density of the resin is a value determined according to JIS K7112:1999 (ISO 1183:1987). [Melting Point] The melting point of the polyethylene (A) forming the main layer 13 is preferably 95°C or higher, more preferably 100°C or higher. Furthermore, the melting point of the polyethylene (A) forming the main layer 13 is preferably 140°C or lower, more preferably 135°C or lower. The upper and lower limits of the melting point of polyethylene (A) can be combined arbitrarily. For example, the melting point of polyethylene (A) forming the main layer 13 is preferably above 95°C and below 140°C. If the melting point of the polyethylene (A) forming the main layer 13 is greater than or equal to the lower limit of the aforementioned range, it is easy to form the insert of this embodiment. Furthermore, if the melting point of the polyethylene (A) forming the main layer 13 is less than or equal to the upper limit of the aforementioned range, it exhibits excellent flexibility and is easy to handle. Furthermore, in this embodiment, the melting point of polyethylene (A) is a value determined in accordance with JIS K7121:2012 (ISO 3146). The material forming the sealing layer 14 is a polyethylene-based resin obtained by polymerizing monomers containing ethylene. Furthermore, the monomers containing ethylene are not particularly limited and can be derived from fossil fuels or biomass. The polyethylene (A) described above can be used as the polyethylene-based resin. Among these, low-density polyethylene (LDPE) and linear low-density polyethylene (LLDPE) are preferred as the polyethylene (A) used for the sealing layer 14. One type of polyethylene (A) can be used, or two or more types can be used. The polyethylene (A) forming the sealing layer 14 can be the same resin as the polyethylene (A) forming the main layer 13, or they can be different. In particular, for excellent low-temperature heat sealing performance, a low-melting-point polyethylene-based resin is preferred for the polyethylene (A) forming the sealing layer 14. Specifically, the melting point is preferably below 125°C, and more preferably below 120°C. The material forming the intermediate layer 15 is a polyethylene-based resin obtained by polymerizing monomers containing ethylene. Furthermore, the monomers containing ethylene are not particularly limited and can be derived from fossil fuels or biomass. In the following description, the polyethylene-based resin forming the intermediate layer 15 will also be referred to simply as "polyethylene (B)". [Polyethylene (B)] In addition to the constituent units derived from ethylene, polyethylene (B) may further have constituent units derived from α-olefins. α-olefins may be derived from biomass or fossil fuels. Examples of α-olefins include those listed in polyethylene (A). That is, when polyethylene (B) is a polymer having constituent units from ethylene and constituent units from α-olefins, polyethylene (B) can be a binary copolymer of ethylene and one polyolefin, a terpolymer of ethylene and two polyolefins, or a copolymer of ethylene and three or more polyolefins. Furthermore, without affecting the effects of the present invention, polyethylene (B) may have constituent units derived from monomers other than ethylene and α-olefins. Moreover, it is required that the proportion of other monomers in the total polyethylene (B) does not exceed 10%. Other monomers that can be cited include those listed in polyethylene (A). Specific examples of polyethylene (B) include, for example, medium-density polyethylene (MDPE) and high-density polyethylene (HDPE). Among these, high-density polyethylene (HDPE) is preferred as the polyethylene (B) used for the interlayer 15. The polyethylene (B) forming the interlayer 15 can be one type or two or more types. [Physical properties of polyethylene (B)] Polyethylene (B) is preferably characterized by the following physical properties. [Mel Flow Rate] The melt flow rate (MFR) of polyethylene (B) is preferably 4.0 g / 10 min or more, more preferably 5.0 g / 10 min or more, and even more preferably 6.5 g / 10 min or more. Furthermore, the MFR of polyethylene (B) is preferably 25 g / 10 min or less, more preferably 20 g / 10 min or less, and even more preferably 15 g / 10 min or less. The upper and lower limits of the MFR of polyethylene (B) can be combined arbitrarily. For example, the MFR of polyethylene (B) is preferably above 6.5 g / 10 min and below 15 g / 10 min. If the MFR of polyethylene (B) is greater than or equal to the lower limit of the aforementioned range, curling of the insert in this embodiment can be suppressed. If the MFR of polyethylene (B) is less than or equal to the upper limit of the aforementioned range, it becomes easier to operate. [Density] When polyethylene (B) is polyethylene, the density of polyethylene (B) is preferably 930 kg / m³. 3 The above is preferred to be 950 kg / m². 3 That's all. Furthermore, the density of polyethylene (B) is preferably 1000 kg / m³. 3 The preferred value is 970 kg / m². 3 Therefore, the optimal value is 965 kg / m³. 3 the following. The upper and lower limits of the density of polyethylene (B) can be combined arbitrarily. For example, the density of polyethylene (B) is preferably 950 kg / m³. 3 Above, 970kg / m 3 the following. If the density of polyethylene (B) is greater than or equal to the lower limit of the aforementioned range, the fitting of this embodiment is easily formed. If the density of polyethylene (B) is less than or equal to the upper limit of the aforementioned range, the fitting of this embodiment becomes soft and has an excellent user experience. [Melting Point] The melting point of polyethylene (B) is preferably above 120°C, more preferably above 128°C. Furthermore, the melting point of polyethylene (B) is preferably below 160°C, more preferably below 150°C. The upper and lower limits of the melting point of polyethylene (B) can be combined arbitrarily. For example, the melting point of polyethylene (B) is preferably above 128°C and below 150°C. If the melting point of polyethylene (B) is greater than or equal to the lower limit of the aforementioned range, it has sufficient rigidity and is easy to form into the insert of this embodiment. Furthermore, if the melting point of polyethylene (B) is less than or equal to the upper limit of the aforementioned range, the insert has sufficient flexibility and toughness. [Flexural modulus] The flexural modulus of polyethylene (B) is preferably 950 MPa or more, and more preferably 1000 MPa or more. Furthermore, the flexural modulus of polyethylene (B) is preferably 1500 MPa or less, and more preferably 1300 MPa or less. The upper and lower limits of the flexural modulus of polyethylene (B) can be arbitrarily combined. For example, the flexural modulus of polyethylene (B) is preferably above 1000 MPa and below 1300 MPa. If the flexural modulus of polyethylene (B) is greater than or equal to the lower limit of the aforementioned range, the interlocking component has sufficient rigidity. Furthermore, if the flexural modulus of polyethylene (B) is less than or equal to the upper limit of the aforementioned range, the interlocking component has sufficient flexibility and toughness. Furthermore, in this embodiment, the flexural modulus of polyethylene (B) is a value measured according to JIS K 7171. [Tensive Yield Stress] The tensile yield stress of polyethylene (B) is preferably 20 MPa or more, more preferably 25 MPa or more. Furthermore, the tensile yield stress of polyethylene (B) is preferably 40 MPa or less, more preferably 35 MPa or less. The upper and lower limits of the tensile yield stress of polyethylene (B) can be arbitrarily combined. For example, the tensile yield stress of polyethylene (B) is preferably above 25 MPa and below 35 MPa. If the tensile yield stress of polyethylene (B) is greater than or equal to the lower limit of the aforementioned range, the insert has sufficient rigidity. Furthermore, if the tensile yield stress of polyethylene (B) is less than or equal to the upper limit of the aforementioned range, the insert has sufficient flexibility and toughness. Furthermore, in this embodiment, the tensile yield stress of polyethylene (B) is a value determined in accordance with JIS K 7161:2014 (ISO527-1). The main layer 13, sealing layer 14 and intermediate layer 15 may contain conventional additives such as stabilizers, antioxidants, lubricants, antistatic agents, colorants, and molding aids, as required. For ease of achieving sufficient sealing strength when heat-fused to the bag body, the width W1 of the first substrate 11 is preferably 2 mm or more, and more preferably 3 mm or more. For excellent flexibility and ease of handling, the width W1 of the first substrate 11 is preferably 60 mm or less, and more preferably 40 mm or less. The lower and upper limits of the width W1 of the first substrate 11 can be arbitrarily combined; for example, it is preferably 2 mm or more and 60 mm or less. For a good balance between rigidity and flexibility, the thickness of the first substrate 11 is preferably 0.01 mm or more, and more preferably 0.12 mm or more. For excellent flexibility and user experience, the thickness of the first substrate 11 is preferably 0.4 mm or less, and more preferably 0.3 mm or less. The lower and upper limits of the thickness of the first substrate 11 can be combined arbitrarily; for example, it is preferably 0.01 mm or more and 0.4 mm or less. For sufficient rigidity, the thickness of the main layer 13 is preferably 0.005 mm or more, and more preferably 0.015 mm or more. For excellent flexibility and ease of handling, the thickness of the main layer 13 is preferably 0.3 mm or less, and more preferably 0.2 mm or less. The lower and upper limits of the thickness of the main layer 13 can be combined arbitrarily; for example, it is preferably 0.005 mm or more and 0.3 mm or less. For sufficient sealing strength to be achieved when heat-fused to the bag body, the thickness of the sealing layer 14 is preferably 0.003 mm or more, more preferably 0.008 mm or more, and even more preferably 0.01 mm or more. For the fitting to become soft and have an excellent user experience, the thickness of the sealing layer 14 is preferably 0.2 mm or less, more preferably 0.1 mm or less, and even more preferably 0.08 mm or less. The lower and upper limits of the thickness of the sealing layer 14 can be combined arbitrarily; for example, it is preferably 0.003 mm or more and 0.2 mm or less. The thickness of the intermediate layer 15 is preferably 0.02 mm or more, more preferably 0.03 mm or more, and even more preferably 0.05 mm or more. Furthermore, the thickness of the intermediate layer 15 is preferably 0.4 mm or less, more preferably 0.3 mm or less, and even more preferably 0.25 mm or less. The upper and lower limits of the thickness of the intermediate layer 15 can be combined arbitrarily. If the thickness of the intermediate layer 15 is greater than or equal to the lower limit, sufficient sealing strength can be obtained when the insert is heat-fused to the bag body, thus suppressing wrinkles during bag making. If the thickness of the intermediate layer 15 is less than or equal to the upper limit, the insert becomes soft, providing excellent usability and achieving good point sealing performance. Here, "having point sealing performance" refers to the property of suppressing pinholes in the crushed portion during the point sealing step of the crushed insert when forming the side sealing portion of the package. The second substrate 21 has the same structure as the first substrate 11, and includes: a main layer 23; a sealing layer 24 disposed on the side of the main layer 23 opposite to the convex fitting portion 12 and the concave fitting portion 22; and an intermediate layer 25 disposed between the main layer 23 and the sealing layer 24. The materials used to form the main layer 23, the sealing layer 24 and the intermediate layer 25 are not particularly limited, and can be the same as those used to form the main layer 13, the sealing layer 14 and the intermediate layer 15, and preferably the same as those used to form the main layer 13, the sealing layer 14 and the intermediate layer 15. The main layer 23, sealing layer 24, and intermediate layer 25 may contain conventional additives such as stabilizers, antioxidants, lubricants, antistatic agents, colorants, and molding aids, as required. The materials forming the main layer 13, sealing layer 14, and intermediate layer 15 may be the same as or different from the materials forming the main layer 23, sealing layer 24, and intermediate layer 25, respectively. The width W2 of the second substrate 21 is preferably the same as the width W1 of the first substrate 11. The width W1 of the first substrate 11 may be the same as or different from the width W2 of the second substrate 21. The thickness of the second substrate 21, the main layer 23, the sealing layer 24, and the intermediate layer 25 is preferably the same as the thickness of the first substrate 11, the main layer 13, the sealing layer 14, and the intermediate layer 15. The thickness of the first substrate 11, the main layer 13, the sealing layer 14, and the intermediate layer 15 may be the same as or different from the thickness of the second substrate 21, the main layer 23, the sealing layer 24, and the intermediate layer 25, respectively. The preferred mass ratio of the main layer, sealing layer, and intermediate layer in the overall fitting is: main layer 10% to 90% by mass, sealing layer 5% to 30% by mass, and intermediate layer 5% to 60% by mass; more preferably: main layer 50% to 85% by mass, sealing layer 8% to 20% by mass, and intermediate layer 10% to 45% by mass. Herein, the aforementioned mass ratios of the main layer, sealing layer, and intermediate layer refer to the mass ratio of resin contained in each layer, and the total mass ratio of the main layer, sealing layer, and intermediate layer is 100% by mass. If the mass ratios of the main layer, sealing layer, and intermediate layer are within the aforementioned range, good formability is achieved, and heat shrinkage is easily suppressed. The rigidity of the fitting 1 in this embodiment, as determined by the evaluation method described below, is preferably 5 N / mm or more, more preferably 6 N / mm or more, and even more preferably 7 N / mm or more. Furthermore, the aforementioned rigidity is preferably 30 N / mm or less, more preferably 25 N / mm or less, and even more preferably 15 N / mm or less. The upper and lower limits of the rigidity of the fitting 1 can be arbitrarily combined. The rigidity of the fitting 1 can be 5 N / mm or more and 30 N / mm or less. If the rigidity of the fitting 1 is within the above range, the rigidity of the fitting is sufficient, and when applied to a bag body with the fitting described later, wrinkles during bag making can be suppressed. [Rigidity] The convex-side fitting member was cut into 70mm lengths to serve as test pieces. The test pieces were held at both ends along their long side using a tensile testing machine (Toyo Seiki Co., Ltd., VGS5E), and the tensile stress at 2% elongation was measured. Tensile stress was measured for five test pieces, and the arithmetic mean of the measured values ​​was used as the calculated tensile stress. Peel strength was measured under conditions of a 50mm distance between the clamps and a testing speed of 1mm / min. Furthermore, when the melting point of the entire fitting is 120°C or higher, and its heat of fusion is 100%, the fitting 1 of this embodiment preferably has a melting point heat of less than 20% in the other peaks generated within the temperature range below 120°C. In the fitting 1, if the melting point heat of the aforementioned other peaks is less than 20%, it has sufficient rigidity and excellent formability. Furthermore, in this embodiment, the density of polyethylene (B) in the insert 1 is greater than that of polyethylene (A). Specifically, it is preferable that the density of polyethylene (B) is at least 1.01 times greater than that of polyethylene (A), and more preferably at least 1.05 times greater. If the density of polyethylene (B) is more than 1.01 times greater than the density of polyethylene (A), then sufficient sealing strength can be obtained when the insert 1 of this embodiment is heat-fused to the bag body, thus suppressing wrinkles during bag making. Furthermore, in this embodiment, the insert 1 has a higher melting point than polyethylene (A). Specifically, it is preferable that the melting point of polyethylene (B) is at least 1.01 times higher than that of polyethylene (A), and more preferably at least 1.07 times higher. If the melting point of polyethylene (B) is more than 1.01 times higher than the melting point of polyethylene (A), then, since the insert 1 of this embodiment has sufficient rigidity and low-temperature sealing properties, wrinkles can be suppressed during bag making. [Manufacturing Method] The manufacturing method of the fitting 1 is not particularly limited except for the use of polyethylene (A) and polyethylene (B), and conventional methods can be used. For example, polyethylene (A) can be obtained by mixing one or more polyethylene resins in appropriate proportions and then melt-kneading them at 150-200°C (a temperature with a melting point 40-50°C higher than that of the blended resins) using a single-shaft extruder with a diameter of 50 mm φ and an L / D of 30. Furthermore, polyethylene (B) can be obtained by mixing one or more polyethylene resins in appropriate proportions and then melt-kneading them at 150-200°C (a temperature with a melting point 40-50°C higher than that of the blended resin) using a single-shaft extruder with a diameter of 30 mm φ and an L / D of 30. The obtained polyethylene (A) and polyethylene (B) can be co-extruded into a composite profile mold for convex-side or concave-side interlocking components, and then cooled by water or air cooling to manufacture interlocking parts. The obtained interlocking parts can be wound up in a winding machine. Furthermore, the convex side fitting member 10 can be formed by integrally extruding the main layer 13 and the convex side fitting part 12 using polyethylene (A), and thermally laminating a laminated film made of polyethylene (B) onto another surface 11b of the first substrate 11 of the obtained molded body to provide an intermediate layer 15. Furthermore, the concave side fitting member 20 can also be formed in the following manner: the main layer 23 and the concave side fitting part 22 are integrally extruded using polyethylene (A), and a laminated film made of polyethylene (B) is thermally laminated onto another surface 21b of the second substrate 21 of the obtained molded body to provide an intermediate layer 25. As described above, the insert 1 is formed using polyethylene (A) and polyethylene (B), both composed of polyethylene-based resins. Accordingly, since the insert 1 is made of a single resin (polyethylene-based resin), it can meet the requirement of using a single material during recycling. [Bag with Fitting] Figure 3 is a schematic front view of the bag 100 with fitting according to this embodiment. In the following description, the bag 100 with fitting will be simply referred to as "bag 100". As shown in Figure 3, the bag body 100 of this embodiment includes: a bag body 50; and a fitting 1, which is installed on the upper inner surface of the bag body 50. The bag body 50 is rectangular when viewed from the front. The fitting 1 extends along the shorter side of the bag body 50 on the inner surface of the upper side. However, the shape of the bag body 50 is not limited to a rectangle. The bag body 50 is sealed with contents (not shown) inside. The bag body 50 is obtained by overlapping the first membrane material 52 and the second membrane material 54 and heat-sealing all the peripheral portions 56 around the bag. At the peripheral portions 56, the two ends of the fitting 1 are heat-sealed together with the first membrane material 52 and the second membrane material 54. The first membrane material 52 and the second membrane material 54 can be fused to the insert 1 by heat sealing. They can be single-layer membranes consisting only of a sealing material layer or laminated membranes having at least a sealing material layer and a substrate layer from the inner surface side. As the substrate layer of the laminated film, a polyethylene-based resin can be used, for example, a resin described in polyethylene (A) or polyethylene (B). The polyethylene-based resin used for the substrate layer can be one type or two or more types. As the sealing layer of the laminated film, a polyethylene-based resin can be used, for example, a resin described in polyethylene (A) or polyethylene (B). That is, the first film material 52 and the second film material 54 can also be a laminate of different polyethylene-based resins. Functional layers such as barrier layers can also be set in the laminated film. In this embodiment, the bag body 100 of the attached fitting preferably uses linear low-density polyethylene (LLDPE) as the sealing material layer for the first membrane material 52 and the second membrane material 54. Accordingly, since the bag body 100 of the attached fitting is constructed from a single resin (polyethylene-based resin), it can meet the requirement of using a single material during recycling. Furthermore, the occurrence of wrinkles can be suppressed by using a low-temperature heat-sealing fitting. The bag body 50 is provided with a cutting auxiliary line 58, which is located on the side above the fitting 1 and is set along the fitting 1. The cutting auxiliary line 58 refers to the portion used to assist in cutting the bag body 50 during linear processing. Examples of cutting auxiliary lines 58 include, for instance, weakening lines provided in portions of the cutting auxiliary lines 58 in the first membrane material 52 and the second membrane material 54. Weakening lines can be formed by providing a portion of the membrane material that is thinner than its surroundings. Alternatively, weakening lines can also be formed by perforated lines or by forming rows of small holes. Furthermore, the cutting auxiliary line 58 is not limited to a weakening line, but can also be a line formed by printing or other means to be cut by scissors or a cutter. A notch 60 is formed at the end of the cutting auxiliary line 58 in the peripheral portion 56. The shape of the notch 60 is not particularly limited, and a triangular or semi-circular notch can be used. Furthermore, the notch 60 can also be a notch provided in the peripheral portion 56. Figure 4 is a schematic perspective view showing the opening of the bag body 100. The bag body 100 can be provided with an unheat-sealed end at the top by cutting along the cutting guide line 58 from the notch 60 and removing the upper part of the bag body 50. The bag body 100 can be opened by forming an opening 62 that opens the aforementioned end. The opening 62 formed in the bag body 100 can be repeatedly opened and closed by assembling and disassembling the convex fitting member 10 and the concave fitting member 20 of the fitting member 1. In addition to using the fitting 1, the bag body 100 can be manufactured by conventional methods. Since the bag body 100 of this embodiment uses the fitting 1, the stickiness can be suppressed by the fitting disposed on the inner surface of the bag body 50. Furthermore, since the bag body 100 of this embodiment uses the fitting 1, when the first membrane material 52 and the second membrane material 54 are heat-sealed together with the fitting 1 at the periphery 56, defects such as wrinkles or openings are not easily generated at the sealing position, and good results are easily obtained. The insert 1 constructed as described above can meet the requirement of using a single material during recycling. Furthermore, the bag body 100 with the insert 1 constructed as described above can suppress wrinkles during bag making and meet the requirement of using a single material. While the preferred embodiments of the present invention have been described above with reference to the accompanying drawings, the present invention is not limited to the aforementioned examples. The shapes or combinations of the structural components disclosed in the above examples are merely illustrative, and various modifications can be made based on design requirements, etc., without departing from the spirit of the present invention. Although the present invention will be specifically described below through examples, the present invention is not limited to the following description. In this embodiment, the resin described in Table 1 below is used. [Table 1] Resins LDPE1, LDPE2, and LLDPE1-6 correspond to "polyethylene (A)" in this invention. Furthermore, resins HDPE1-6 correspond to "polyethylene (B)" in this invention. For each resin, MFR, density, melting point, flexural modulus, and tensile yield stress are the manufacturer's nominal values. MFR is the value determined according to JIS K 7210-1 under a load of 2.16 kg. The MFR is measured at 190°C for ethylene-based resins and 230°C for polypropylene-based resins (PP1, PP2). [Examples 1-6, Comparative Examples 1-4] For the main layer, sealing layer and intermediate layer, the resins listed in Table 1 were weighed and mixed in the proportions listed in Table 2 below to prepare polyethylene (A) and polyethylene (B). As the resin material for forming the main layer, polyethylene (A) blended in the main layer is melt-blended at 170°C using a single-shaft extruder with a diameter of 50 mm φ and an L / D ratio of 30. As the resin material for forming the sealing layer, polyethylene (A) blended in the sealing layer is melt-blended at 170°C using a single-shaft extruder with a diameter of 30 mm φ and an L / D ratio of 30. As the resin material for forming the intermediate layer, polyethylene (B) is melt-blended at 190°C using a single-shaft extruder with a diameter of 30 mm φ and an L / D ratio of 30. For Examples 1-6, the molten resin after melt mixing was supplied to composite shaped molds having mold shapes corresponding to the convex and concave side fitting members, and co-extruded. After the obtained molded articles were cooled and solidified in a water bath, they were wound up in a winding machine to obtain the fittings of Examples 1-6. The obtained convex-side fitting member has a resin content (resin content X) of the total structure of the convex-side fitting part and the main layer, the resin content (resin content Y) of the intermediate layer, and the resin content (resin content Z) of the sealing layer, with a ratio of [resin content X]: [resin content Y]: [resin content Z] = 60:30:10. For the concave-side fitting member, the ratio of the resin content of the total structure of the concave-side fitting part and the main layer, the resin content of the intermediate layer, and the resin content of the sealing layer is the same as that of the convex-side fitting member. The obtained fitting is as follows: the convex side fitting member and the concave side fitting member are both: the width of the substrate (the first substrate and the second substrate) is 13 mm, the total thickness of the first substrate and the total thickness of the second substrate (excluding the fitting part) are 0.15 mm, the thickness of the substrate is 55 μm, the thickness of the intermediate layer is 65 μm, and the thickness of the sealing layer is 30 μm. For Comparative Examples 1-3, the main layer was extruded using an extruder with a diameter of 50 mm φ and an L / D of 30, and the sealing layer was extruded using an extruder with a diameter of 30 mm φ and an L / D of 30. The polyester (A) shown in Table 2 was melt-blended at 150-200°C, a temperature 40-50°C higher than the melting point of the blended resin. The mixture was supplied to a composite die having a die shape corresponding to the convex and concave side fitting members, and co-extruded. After the obtained molded article was cooled and cured in a water bath, it was wound up in a winding machine to obtain the fittings of Comparative Examples 1-3. For Comparative Example 4, the main layer was melt-blended at 190°C using an extruder with a diameter of 50 mm φ and an L / D of 30, and the sealing layer was melt-blended at 170°C using the polypropylene resins (PP1, PP2) shown in Table 2 using an extruder with a diameter of 30 mm φ and an L / D of 30. The mixture was supplied to a composite die having mold shapes corresponding to the convex and concave side fitting members, and co-extruded. After the obtained molded body was cooled and cured in a water bath, it was wound up using a winding machine to obtain the fitting of Comparative Example 4. <Evaluation Method> The obtained assemblies are evaluated using the following methods. [1. Melting point of the interlocking component] A 10 mg sample of the interlocking component was collected and placed in an aluminum pot. The melting point was determined by DSC (Shimadzu Corporation, DSC-60 Plus). The determination was carried out in a nitrogen atmosphere at a temperature range of 0-170°C and a heating rate of 10°C / min. [2. Recyclability] Recyclability is assessed using the following criteria. [Judgment Criteria] ○: Can meet the requirements of a single material. ×: Cannot meet the requirements of a single material. [3. Wrinkling Difficulty] The insert is laminated onto a single-layer film composed of linear low-density polyethylene (LLDPE) to form a bag with the insert. The wrinkling difficulty during bag making is evaluated using the following criteria: ○: Wrinkling of the bag with the insert can be visually confirmed. ×: Wrinkling of the bag with the insert cannot be visually confirmed. [4. Rigidity] Rigidity is assessed by measuring tensile stress. The convex-side fitting member was cut into 70mm lengths to serve as test pieces. The test pieces were held at both ends along their long side in a tensile testing machine (Toyo Seiki Co., Ltd., VGS5E) to measure the tensile stress at 2% elongation. Tensile stress was measured for five test pieces, and the arithmetic mean of the measured values ​​was used as the calculated tensile stress. Peel strength was measured under conditions of a 50mm distance between the clamps and a testing speed of 1mm / min. The evaluation results are shown in Table 2. [Table 2] The evaluation results show that the inserts of Examples 1 to 6 can meet the requirements of single materialization and have excellent recyclability. Furthermore, it can be understood that the fittings in Examples 1 to 6 have sufficient rigidity to suppress wrinkles during bag making. In contrast, although the fittings of Comparative Examples 1 to 3 have excellent recyclability, they lack rigidity and cannot suppress wrinkles when manufacturing bags with fittings. Although the insert in Comparative Example 4 has sufficient rigidity and can suppress wrinkles during bag making, it cannot meet the requirements of single materialization and has poor recyclability. Based on the above results, it can be understood that the present invention is useful. 1: Fitting component 10: Convex fitting component 11: First substrate 11a: Surface 12: Convex fitting portion 12a: Main body 12b: Head 13: Main layer 14: Sealing layer 15: Intermediate layer 20: Concave fitting component 21: Second substrate 21a: Surface 22: Concave fitting portion 22a, 22b: Arm portion 22c: Concave portion 23: Main layer 24: Sealing layer 25: Intermediate layer 50: Bag body 52: First membrane material 54: Second membrane material 56: Peripheral portion 58: Cutting auxiliary line 60: Notch 62: Opening portion 100: Bag body with fitting component Figure 1 shows a schematic perspective view of the fitting in this embodiment. Figure 2 shows a cross-sectional view along line II-II in Figure 1. Figure 3 shows a schematic front view of the bag body 100 with the fitting in this embodiment. Figure 4 shows a schematic perspective view of the bag body 100 with its opening open. 1: Fitting parts 10: Convex side fitting component 11: First substrate 11a: Surface 12: Convex side fitting part 12a: Main cadre 12b: Head 20: Concave side fitting component 21: Second substrate 21a: Surface 22: Concave side fitting part 22a, 22b: Arm 22c: concave part

Claims

1. A fitting member comprising a convex fitting member and a concave fitting member, wherein, The aforementioned convex-side fitting member has a convex-side fitting portion on the surface of the strip-shaped first substrate along its long side direction, and the aforementioned concave-side fitting member has a concave-side fitting portion on the surface of the strip-shaped second substrate along its long side direction; the aforementioned convex-side fitting portions and the aforementioned concave-side fitting portions are fitted together in a detachable manner; the aforementioned first substrate and the aforementioned second substrate each have a main layer, a sealing layer, and an intermediate layer, the aforementioned sealing layer is respectively disposed on the side opposite to the aforementioned convex-side fitting portion of the aforementioned main layer and the side opposite to the aforementioned concave-side fitting portion of the aforementioned main layer, and the aforementioned intermediate layer is disposed between the aforementioned main layer and the aforementioned sealing layer; the aforementioned first substrate and the aforementioned second substrate are both composed of polyethylene-based resin obtained by polymerizing monomers containing ethylene, the aforementioned main layer respectively contains low-density polyethylene and linear low-density polyethylene, the aforementioned intermediate layer contains high-density polyethylene, the aforementioned sealing layer contains linear low-density polyethylene, and the density of the polyethylene-based resin in the aforementioned intermediate layer is 930 kg / m3 or more and 1000 kg / m3 or less. The density of the polyethylene resin in the aforementioned intermediate layer is more than 1.01 times greater than the density of the polyethylene resin in the aforementioned main layer. The rigidity obtained by the following measurement method is 5 to 30 N / mm. Rigidity: The convex side fitting member is cut into 70 mm lengths to serve as test pieces. The test pieces are held at both ends of the long side direction using a tensile testing machine, and the tensile stress at 2% elongation is measured. The tensile stress is measured for 5 test pieces, and the arithmetic mean of the measured values ​​is used as the tensile stress (rigidity). The peel strength is measured under the conditions of a 50 mm distance between the clamps and a test speed of 1 mm / min.

2. The fitting as described in claim 1, wherein, The aforementioned rigidity is 7–15 N / mm.

3. The fitting as described in claim 1, wherein, The polyethylene resin constituting the aforementioned intermediate layer has a melting point of 125°C or higher.

4. The fitting as described in claim 1, wherein, The aforementioned intermediate layer polyethylene resin has a melt flow rate of 4.0 g / 10 min or more, a flexural elasticity of 1000 MPa or more, and a tensile yield stress of 20 MPa or more.

5. The fitting as described in claim 1, wherein, The mass ratio of the aforementioned main layer, the aforementioned sealing layer and the aforementioned intermediate layer in the aforementioned fitting assembly is as follows: relative to the total mass of the aforementioned fitting assembly, the aforementioned main layer is more than 50% by mass and less than 85% by mass, the aforementioned sealing layer is more than 8% by mass and less than 20% by mass, and the aforementioned intermediate layer is more than 10% by mass and less than 45% by mass (totaling 100% by mass).

6. A bag body with an attached fitting, wherein, The bag body with the aforementioned fitting includes: a fitting as described in any one of claims 1 to 5, and a bag body for containing contents; the bag body is composed of a polyethylene resin obtained by polymerizing monomers containing ethylene; the aforementioned fitting is installed on the inner surface of the aforementioned bag body.

Citation Information

Patent Citations

  • Zipper tape,packing bag with zipper tape and preparation method of packing bag

    CN102753448B

  • Plastic chuck

    JP1994122460A

  • Easy-to-cut fitting tool and bag body with fitting tool

    JP2003160147A

  • Fastener tape

    JP2011155996A

  • Fitting tool and bag body with fitting tool

    JP2019176996A