Sensing substrate, sensing device and manufacturing method thereof

TWI945481BActive Publication Date: 2026-11-11INNOLUX CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW112142953
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-11-08
Publication Date
2026-11-11
Estimated Expiration
2043-11-07

AI Technical Summary

Technical Problem

The uneven surface of stacked structures in sensing devices leads to poor hermeticity between substrates, affecting packaging vacuum degree and increasing manufacturing costs and complexity.

Method used

A sensing substrate design featuring a planarization layer with openings for sensing units connected to a circuit layer, enhanced by a bonding layer, providing a flat surface for improved adhesion and vacuum tightness when bonded with an optical substrate.

Benefits of technology

Enhances bonding tightness, improves encapsulation vacuum tightness, and increases sensing ability by reducing noise-equivalent temperature difference (NETD) and simplifying the manufacturing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure TWG2TB001920226_001
    Figure TWG2TB001920226_001
  • Figure TWG2TB001920226_002
    Figure TWG2TB001920226_002
  • Figure TWG2TB001920226_003
    Figure TWG2TB001920226_003
Patent Text Reader

Abstract

This disclosure provides a sensing substrate, comprising a first substrate, a circuit layer, a planarization layer, a sensing unit, and a first bonding layer. The circuit layer is disposed on the first substrate. The planarization layer is disposed on the circuit layer and includes openings. The sensing unit is disposed on the planarization layer and is electrically connected to the circuit layer through the openings. The first bonding layer is disposed on the planarization layer. This disclosure also provides a sensing device and a method for manufacturing the same.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a sensing substrate, a sensing device, and a method for manufacturing the same. Prior Art

[0002] Sensing devices are widely used in various electronic products and have become an indispensable necessity in modern society. With the development of automation technology, the usage frequency of sensing devices has grown rapidly, and most modern instruments and equipment use sensing devices.

[0003] Array sensors are a common type of sensing device. The noise-equivalent temperature difference (NETD) is one of the important factors affecting the sensing ability of array sensors, and it is related to the degree of hermeticity of the package. In the general manufacturing process of sensing devices, the uneven surface of the stacked structure easily causes poor hermeticity between the upper and lower substrates, which in turn affects the packaging vacuum degree after bonding. Moreover, the current packaging process is still relatively complex, with problems such as low process yield and high manufacturing costs.

[0004] Therefore, further improving the structural design of sensing devices and their manufacturing methods, such as simplifying the process or increasing the yield, remains one of the topics that the industry is currently committed to researching. Summary of the Invention

[0005] According to some embodiments of the present disclosure, a sensing substrate is provided, including a first substrate, a circuit layer, a planarization layer, a sensing unit, and a first bonding layer. The circuit layer is disposed on the first substrate. The planarization layer is disposed on the circuit layer, and the planarization layer includes an opening. The sensing unit is disposed on the planarization layer, and the sensing unit is electrically connected to the circuit layer through the opening. The first bonding layer is disposed on the planarization layer.

[0006] According to other embodiments of the present disclosure, a sensing device is provided, including a sensing substrate and an optical substrate. The sensing device includes a first substrate, a circuit layer, a planarization layer, a sensing unit, and a first bonding layer. The circuit layer is disposed on the first substrate. The planarization layer is disposed on the circuit layer, and the planarization layer includes an opening. The sensing unit is disposed on the planarization layer, and the sensing unit is electrically connected to the circuit layer through the opening. The first bonding layer is disposed on the planarization layer. The optical substrate includes a second substrate and a second bonding layer disposed on the second substrate. Moreover, the optical substrate and the sensing substrate are bonded to each other through the first bonding layer and the second bonding layer.

[0007] According to some other embodiments of the present disclosure, a method for manufacturing a sensing device is provided, which includes providing a sensing substrate. Providing the sensing substrate includes the following steps: providing a first substrate; forming a circuit layer on the first substrate; forming a planarization layer on the circuit layer, and the planarization layer includes a first opening; forming a sensing unit on the planarization layer, and the sensing unit is electrically connected to the circuit layer through the first opening; and forming a first bonding layer on the planarization layer.

[0008] To make the features or advantages of the present disclosure more obvious and understandable, some embodiments are specifically given below and are described in detail in conjunction with the accompanying drawings as follows. Brief description of the drawings

[0009] Figures 1A to 1E show schematic cross-sectional views of a sensing substrate at different process stages according to some embodiments of the present disclosure; Figures 2A to 2E show schematic cross-sectional views of an optical substrate at different process stages according to some embodiments of the present disclosure; Figure 3 shows a schematic cross-sectional view of a sensing substrate and an optical substrate of a sensing device according to some embodiments of the present disclosure; Figure 4 shows a schematic cross-sectional view of a sensing device according to some embodiments of the present disclosure; Figure 5 shows an equivalent circuit diagram of a sensing device according to some embodiments of the present disclosure. Embodiments

[0010] The following provides a detailed description of the sensing substrate, the sensing device, and the manufacturing method thereof according to the embodiments of the present disclosure. It should be understood that the following description provides many different embodiments for implementing different aspects of some embodiments of the present disclosure. The specific elements and arrangements described below are only for simply and clearly describing some embodiments of the present disclosure. Of course, these are only for illustration and not for limitation of the present disclosure. In addition, similar and / or corresponding reference numerals may be used in different embodiments to label similar and / or corresponding elements to clearly describe the present disclosure. However, the use of these similar and / or corresponding reference numerals is only for simply and clearly describing some embodiments of the present disclosure, and does not represent any correlation between the different embodiments and / or structures discussed.

[0011] It should be understood that in the embodiments, relative terms such as "lower" or "bottom" or "higher" or "top" may be used to describe the relative relationship of one element of the figure to another element. It can be understood that if the device in the figure is turned upside down, the element described on the "lower" side will become the element on the "higher" side. The embodiments of the present disclosure can be understood in conjunction with the figures, and the figures of the present disclosure are also regarded as a part of the disclosure description. It should be understood that the figures of the present disclosure are not drawn to scale. In fact, the sizes of the elements may be arbitrarily enlarged or reduced to clearly show the features of the present disclosure.

[0012] Furthermore, when it is mentioned that a first material layer is located on or above a second material layer, it may include the case where the first material layer is in direct contact with the second material layer or the first material layer and the second material layer may not be in direct contact, that is, there may be one or more other material layers between the first material layer and the second material layer. However, when the first material layer is directly located on the second material layer, it means that the first material layer and the second material layer are in direct contact.

[0013] In addition, it should be understood that the ordinal numbers such as "first", "second", etc. used in the specification and claims are used to modify elements, and they do not themselves imply or represent any previous ordinal numbers of the element (or elements), nor do they represent the order of one element and another element, or the order in the manufacturing method. The use of these ordinal numbers is only used to clearly distinguish an element with a certain name from another element with the same name. The same terms may not be used in the claims and the specification. For example, the first element in the specification may be the second element in the claims.

[0014] In some embodiments of the present disclosure, terms related to joining and connecting such as "connect", "interconnect", etc., unless otherwise defined, may mean that two structures are in direct contact, or may also mean that two structures are not in direct contact, and there are other structures disposed between these two structures. And these terms related to joining and connecting may also include the situation where both structures can move, or both structures are fixed. In addition, the term "electrically connected" or "coupled" includes any direct and indirect electrical connection means.

[0015] In this text, the terms "about", "substantially", and "roughly" generally mean within 10%, or within 5%, or within 3%, or within 2%, or within 1%, or within 0.5% of a given value or range. The term "ranging from a first numerical value to a second numerical value" means that the range includes the first numerical value, the second numerical value, and other numerical values therebetween. Furthermore, there may be a certain error between any two numerical values or directions being compared. If the first numerical value is equal to the second numerical value, it implies that there may be an error of about 10% between the first numerical value and the second numerical value; if the first direction is perpendicular to the second direction, the angle between the first direction and the second direction may range from 80 degrees to 100 degrees; if the first direction is parallel to the second direction, the angle between the first direction and the second direction may range from 0 degrees to 10 degrees.

[0016] It should be understood that, without departing from the spirit of this disclosure, the features in several different embodiments may be replaced, reorganized, and combined to complete other embodiments in the following examples. As long as the features between the embodiments do not violate the spirit of the invention or conflict with each other, they can be arbitrarily combined and used.

[0017] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by those of ordinary skill in the technical field to which this disclosure pertains. It can be understood that these terms, such as those defined in a commonly used dictionary, should be interpreted as having a meaning consistent with the relevant technology and the background or context of this disclosure, and should not be interpreted in an idealized or overly formal manner, unless specifically defined in the embodiments of this disclosure.

[0018] According to an embodiment of this disclosure, a sensing substrate is provided, which includes a sensing unit and a bonding layer disposed on a planarization layer, can provide a relatively flat structural surface, can improve the bonding tightness during bonding, and thus can enhance the encapsulation vacuum tightness of the sensing device, improve the noise-equivalent temperature difference (NETD) of the sensing device, and enhance the sensing ability of the sensing device.

[0019] Please refer to FIGS. 1A to 1E. FIGS. 1A to 1E show schematic cross-sectional views of the sensing substrate 10A at different process stages according to some embodiments of the present disclosure. It should be understood that, according to some embodiments, additional operation steps may be provided before, during, and / or after the manufacturing method of the sensing substrate 10A. According to some embodiments, some of the operation steps may be replaced or omitted. According to some embodiments, the order of some of the operation steps may be interchangeable. Furthermore, for clarity of illustration, some elements of the sensing substrate 10A may be omitted in the figures, and only some elements are schematically shown. According to some embodiments, additional features may be added to the sensing substrate 10A described below. According to other embodiments, some features of the sensing substrate 10A described below may be replaced or omitted.

[0020] First, please refer to FIG. 1A. A first substrate 100 is provided. The first substrate 100 may have regions corresponding to the peripheral area BA, the active area AA, and the fan-out area FA of the sensing device. According to some embodiments, the first substrate 100 may include a flexible substrate, a rigid substrate, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the material of the first substrate 100 may include glass, quartz, sapphire, ceramic, polyimide (PI), polycarbonate (PC), polyethylene terephthalate (PET), polypropylene (PP), other suitable materials, or a combination of the foregoing, but is not limited thereto. Furthermore, according to some embodiments, the first substrate 100 may include a metal-glass fiber composite sheet, or a metal-ceramic composite sheet, but is not limited thereto. In addition, the light transmittance of the first substrate 100 is not limited, that is, the first substrate 100 may be a light-transmitting substrate, a semi-light-transmitting substrate, or an opaque substrate.

[0021] Next, a circuit layer 100C may be formed on the first substrate 100. According to some embodiments, the circuit layer 100C may include a buffer layer (not labeled) and thin-film transistors TR disposed on the buffer layer. The thin-film transistors TR may be located in the active area AA, and the circuit layer 100C may include conductive elements and signal lines electrically connected to the thin-film transistors TR, an insulating layer formed between the conductive elements, and the like. According to some embodiments, the signal lines may include, for example, current signal lines, voltage signal lines, high-frequency signal lines, low-frequency signal lines, and the signal lines may transmit the element operating voltage (VDD), the common ground voltage (VSS), or the driving element terminal voltage. The present disclosure is not limited thereto.

[0022] The thin film transistor TR may include a top gate thin film transistor, a bottom gate thin film transistor, a dual gate or double gate thin film transistor, or a combination thereof. According to some embodiments, the thin film transistor TR may be further electrically connected to a capacitive element, but is not limited thereto. The thin film transistor TR may include at least one semiconductor layer and a gate electrode layer. The semiconductor layer includes a doped region having an appropriate dopant and a channel region located between two doped regions, and the doped region may further have portions with different doping concentrations. Furthermore, the semiconductor layer may include amorphous silicon, low-temp polysilicon (LTPS), metal oxide, other suitable materials, or a combination thereof, but is not limited thereto. The metal oxide may include indium gallium zinc oxide (IGZO), indium zinc oxide (IZO), indium gallium oxide (IGO), indium gallium zinc tin oxide (IGZTO), other suitable materials, or a combination thereof, but is not limited thereto. It should be understood that the number of thin film transistors TR is not limited to that shown in the figure. According to different embodiments, the sensing substrate 10A may have other suitable numbers or types of thin film transistors.

[0023] As shown in FIG. 1A, the circuit layer 100C may include a conductive layer 102. The conductive layer 102 may serve as a contact for the source electrode or drain electrode of the thin film transistor TR, and may electrically connect the source electrode or drain electrode of the thin film transistor TR to the subsequently formed sensing unit 200 (as shown in FIG. 1E).

[0024] Specifically, a part of the gate dielectric layer and the dielectric layer in the circuit layer 100C may be removed by a patterning process to form an opening 100P, and then the conductive layer 102 may be formed in the opening 100P. According to some embodiments, a part of the gate dielectric layer and the dielectric layer may be removed by one or more photolithography processes and / or etching processes to form a via 100P. According to some embodiments, the photolithography process may include photoresist coating (such as spin coating), soft baking, hard baking, mask alignment, exposure, post-exposure baking, photoresist development, cleaning, and drying, etc., but is not limited thereto. The etching process may include a dry etching process or a wet etching process, but is not limited thereto.

[0025] According to some embodiments, the conductive layer 102 may include a metallic material, a transparent conductive material, other suitable conductive materials, or a combination of the foregoing, but is not limited thereto. The metallic material may include, for example, copper (Cu), silver (Ag), gold (Au), tin (Sn), aluminum (Al), molybdenum (Mo), tungsten (W), chromium (Cr), nickel (Ni), platinum (Pt), titanium (Ti), alloys of the foregoing metals, other suitable materials, or a combination of the foregoing, but is not limited thereto. The transparent conductive material may include a transparent conductive oxide (TCO), such as indium tin oxide (ITO), antimony zinc oxide (AZO), tin oxide (SnO), zinc oxide (ZnO), indium zinc oxide (IZO), indium gallium zinc oxide (IGZO), indium tin zinc oxide (ITZO), antimony tin oxide (ATO), other suitable transparent conductive materials, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the conductive layer 102 may be formed by a chemical vapor deposition process, a physical vapor deposition process, an electroplating process, a chemical plating / electroless plating process, other suitable processes, or a combination of the foregoing. The chemical vapor deposition process may include, for example, a low-pressure chemical vapor deposition process (LPCVD), a low-temperature chemical vapor deposition process (LTCVD), a rapid thermal chemical vapor deposition process (RTCVD), a plasma-assisted chemical vapor deposition process (PECVD), or an atomic layer deposition process (ALD), etc., but is not limited thereto. The physical vapor deposition process may include, for example, a sputtering process, an evaporation process, a pulsed laser deposition, etc., but is not limited thereto.

[0026] Referring to FIG. 1A, a planarization layer 110 can be formed on the circuit layer 100C, and the planarization layer 110 can include an opening 110P. The planarization layer 110 can provide a relatively flat structural surface for the subsequent formation of the sensing unit 200 and the first bonding layer BD1. According to some embodiments, the planarization layer 110 can include an insulating material, and the insulating material can include an inorganic material or an organic material. According to some embodiments, the inorganic material can include silicon nitride, silicon oxide, silicon oxynitride, aluminum oxide, other suitable materials, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the insulating material can be formed on the circuit layer 100C by a chemical vapor deposition process, a coating process, a printing process, other suitable processes, or a combination of the foregoing. Moreover, a planarization process can be performed on the foregoing insulating material to form the planarization layer 110 having a substantially flat top surface. According to some embodiments, the planarization process can include a chemical-mechanical polish (CMP) process, a grinding process, other suitable planarization processes, or a combination of the foregoing.

[0027] Furthermore, a portion of the planarization layer 110 can be removed by a patterning process to form the opening 110P, and the opening 110P can expose the conductive layer 102. According to some embodiments, the patterning process can include one or more photolithography processes and / or etching processes.

[0028] Next, a conductive layer 202 can be formed in the opening 110P. The conductive layer 202 can serve as a conductive component of the subsequently formed sensing unit 200, and the sensing unit 200 can be electrically connected to the circuit layer 100C through the opening 110P. According to some embodiments, the material and manufacturing method of the conductive layer 202 can be the same as or similar to those of the foregoing conductive layer 102, and thus will not be repeated herein.

[0029] Referring to FIG. 1B, the sensing unit 200 is formed on the planarization layer 110. As described above, the sensing unit 200 can be electrically connected to the circuit layer 100C through the opening 110P. Specifically, forming the sensing unit 200 on the planarization layer 110 can include the following steps.

[0030] First, a first sacrificial layer SAC1 can be formed on the planarization layer 110, and the first sacrificial layer SAC1 also covers the conductive layer 202. According to some embodiments, the material of the first sacrificial layer SAC1 can include an organic material, such as polyimide (PI), acrylic resin, SU-8 photoresist, parylene C, other suitable materials, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the first sacrificial layer SAC1 can be formed by a chemical vapor deposition process, a coating process, a printing process, other suitable processes, or a combination of the foregoing.

[0031] Furthermore, a portion of the first sacrificial layer SAC1 can be removed by a patterning process to form an opening P1, and the opening P1 can expose the conductive layer 202. According to some embodiments, the patterning process can include one or more photolithography processes and / or etching processes.

[0032] Next, a support element 204a can be formed on the first sacrificial layer SAC, and the support element 204a also fills the opening P1 of the first sacrificial layer SAC1. The support element 204a can support the sensing unit 200 and enhance the structural strength of the sensing unit 200. According to some embodiments, the material of the support element 204a can include titanium nitride (TiN), titanium aluminide (TiAl), titanium aluminum nitride (TiAlN), titanium aluminum oxide (TiAlO), titanium silicon aluminum (TiSiAl), titanium tungsten (TiW), titanium tungsten nitride (TiWN), aluminum nitride (AlNx), other suitable materials, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the support element 204a can have a multi-layer structure. Furthermore, according to some embodiments, the support element 204a can be formed by a chemical vapor deposition process, a physical vapor deposition process, a coating process, a printing process, other suitable processes, or a combination of the foregoing.

[0033] In addition, the support element 204a can be patterned by one or more photolithography processes and / or etching processes. According to some embodiments, the support element 204a can have an annular structure. For example, in a top view, the support element 204a can have a plurality of bent portions or a loop shape, but is not limited thereto. It is worth noting that the support element 204a can reduce heat conduction, reduce the heat dissipation of the sensing unit 200, and thereby improve the sensing ability. A portion of the support element 204a is located in the opening P1 to form an opening 204aP, and the opening 204aP is located within the opening P1.

[0034] Next, a fixing element 204b can be formed in the opening 204aP. According to some embodiments, the fixing element 204b can be partially formed on the support element 204a. The fixing element 204b can further enhance the structural strength of the support element 204a. According to some embodiments, the material of the fixing element 204b can include molybdenum (Mo), molybdenum nitride (MoN), molybdenum tungsten (MoW), tungsten (W), other suitable materials, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the fixing element 204b can be formed by a chemical vapor deposition process, a physical vapor deposition process, an electroplating process, a chemical plating / electroless plating process, other suitable processes, or a combination of the foregoing.

[0035] Next, a second sacrificial layer SAC2 can be formed on the support element 204a, and the second sacrificial layer SAC2 also covers the first sacrificial layer SAC1 and the fixing element 204b. According to some embodiments, the material and manufacturing method of the second sacrificial layer SAC2 can be the same as or similar to those of the first sacrificial layer SAC1 described above, and will not be repeated here.

[0036] Furthermore, a portion of the second sacrificial layer SAC2 can be removed by a patterning process to form an opening P2, and the opening P2 can expose the support element 204a. According to some embodiments, the patterning process can include one or more photolithography processes and / or etching processes.

[0037] Next, an absorption layer 206a can be formed on the second sacrificial layer SAC2, and the absorption layer 206a also fills the opening P2 of the second sacrificial layer SAC2. The absorption layer 206a can absorb light within the wavelength range to be detected. For example, according to some embodiments, the absorption layer 206a can absorb infrared (IR), such as longwave infrared (LWIR), shortwave infrared (SWIR), middle wave infrared (MWIR), or far infrared (FIR). According to some embodiments, the material of the absorption layer 206a can include titanium (Ti), titanium nitride (TiN), platinum (Pt), gold (Au), nickel (Ni), niobium (Nb), other suitable materials, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the absorption layer 206a can be formed by a chemical vapor deposition process, a physical vapor deposition process, an electroplating process, a chemical plating / electroless plating process, other suitable processes, or a combination of the foregoing.

[0038] In addition, according to some embodiments, a portion of the absorption layer 206a is located in the opening P2 to form an opening 206aP, and the opening 206aP is located within the opening P2.

[0039] Next, a fixing element 206b can be formed in the opening 206aP. According to some embodiments, the fixing element 206b can be partially formed on the absorption layer 206a. The fixing element 206b can fix the absorption layer 206a to the support element 204a. According to some embodiments, the material and manufacturing method of the fixing element 206b can be the same as or similar to those of the aforementioned fixing element 204b, and thus will not be repeated here.

[0040] Next, an insulating layer 208 can be formed on the absorption layer 206a, and the insulating layer 208 also covers the second sacrificial layer SAC2 and the fixing element 206b. According to some embodiments, the material of the insulating layer 208 can include silicon nitride (SiNx), silicon oxide (SiOx), silicon oxynitride (SiON), other suitable materials, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the insulating layer 208 can be formed by a chemical vapor deposition process, a physical vapor deposition process, a coating process, a printing process, other suitable processes, or a combination of the foregoing.

[0041] Moreover, a portion of the insulating layer 208 can be removed by a patterning process to expose two end portions EP of the absorption layer 206a. According to some embodiments, the patterning process can include one or more photolithography processes and / or etching processes.

[0042] Next, a sensing layer 210 can be formed on the insulating layer 208, and the sensing layer 210 can be in contact with two ends EP of the absorption layer 206a. The sensing layer 210 can have thermo-sensitive characteristics. The two ends of the sensing layer 210 are connected to the absorption layer 206a, thereby forming a resistance structure. Specifically, one end of the resistance structure can be electrically connected to the conductive layer 202 and the conductive layer 102 through the support structure 204a, and further electrically connected to the thin film transistor TR of the circuit layer 100C, while the other end of the resistance structure can be electrically connected to the conductive layer 202 (labeled as 202-b for convenience of description) connected to the bias signal line. According to some embodiments, the material of the sensing layer 210 can include amorphous silicon (a-Si), vanadium oxide (VOx), yttrium barium copper oxide (YBaCuO), germanium silicon oxide (GeSiO), germanium silicon (SiGe), bismuth lanthanum strontium manganite (BiLaSrMnO), other suitable materials, or combinations of the foregoing, but are not limited thereto. According to some embodiments, the sensing layer 210 can be formed by a chemical vapor deposition process, a physical vapor deposition process, a coating process, a printing process, other suitable processes, or combinations of the foregoing.

[0043] Next, an insulating layer 212 can be formed on the sensing layer 210. According to some embodiments, the material and manufacturing method of the insulating layer 212 can be the same as or similar to those of the foregoing insulating layer 208, and will not be repeated here.

[0044] Please refer to FIGS. 1C, 1D, and 1E. A first bonding layer BD1 is formed on the planarization layer 110. First, a first seed layer 302 can be formed on the planarization layer 110. Specifically, the first seed layer 302 can be formed on the planarization layer 110 located in the peripheral region BA and the fan-out region FA. According to some embodiments, the first seed layer 302 can have a multi-layer structure. For example, it has a sub-layer 302a and a sub-layer 302b disposed on the sub-layer 302a. According to some embodiments, the material of the sub-layer 302a can include molybdenum (Mo), titanium (Ti), or other suitable materials, but is not limited thereto. According to some embodiments, the material of the sub-layer 302b can include copper (Cu) or other suitable materials, but is not limited thereto. It should be understood that although the first seed layer 302 shown in the drawings has two sub-layers, the present disclosure is not limited thereto. According to some embodiments, the first seed layer 302 can have other suitable numbers or types of sub-layers. According to some embodiments, the first seed layer 302 can include a molybdenum / copper composite layer, a titanium / copper composite layer, a molybdenum / aluminum composite layer, or a titanium / aluminum composite layer. The titanium / copper composite layer can serve as an getter in addition to being a seed layer, and can absorb outgassing. According to some embodiments, the first seed layer 302 can be formed by a chemical vapor deposition process, a physical vapor deposition process, an electroplating process, a chemical plating / electroless plating process, other suitable processes, or a combination of the foregoing.

[0045] Next, a first protective layer PR1 can be formed on the first seed layer 302. Specifically, the first protective layer PR1 can be formed on the peripheral region BA, the active region AA, and the fan-out region FA, and the first protective layer PR1 also covers the components of the sensing unit 200 formed above. According to some embodiments, the material of the first protective layer PR1 can include a photoresist material, but is not limited thereto. According to some embodiments, the first protective layer PR1 can be formed by a chemical vapor deposition process, a physical vapor deposition process, a coating process, a printing process, other suitable processes, or a combination of the foregoing.

[0046] Furthermore, a portion of the first protective layer PR1 can be removed by a patterning process to form an opening OP1, and the opening OP1 can expose the first seed layer 302. Specifically, the opening OP1 can expose a partial top surface of the sub-layer 302b located above in the first seed layer 302. According to some embodiments, the patterning process can include one or more photolithography processes and / or etching processes.

[0047] Next, a first metal layer 304 can be formed in the opening OP1, and the first metal layer 304 is located on the first seed layer 302. Herein, the first bonding layer BD1 is substantially completed. According to some embodiments, the first metal layer 304 can have a multi-layer structure, such as having a sub-layer 304a and a sub-layer 304b disposed on the sub-layer 304a. According to some embodiments, the material of the sub-layer 304a can include copper (Cu) or other suitable materials, but is not limited thereto. According to some embodiments, the material of the sub-layer 304b can include tin (Sn) or other suitable materials, but is not limited thereto. It should be understood that although the first metal layer 304 shown in the drawings has two sub-layers, the present disclosure is not limited thereto. According to some embodiments, the first metal layer 304 can have other suitable numbers or types of sub-layers. According to some embodiments, the first metal layer 304 can include a tin / copper composite layer, a tin / gold / nickel / copper composite layer, a tin / gold / nickel composite layer, a gold / nickel composite layer, or a gold / nickel / copper composite layer. According to some embodiments, the first metal layer 304 can be formed by a chemical vapor deposition process, a physical vapor deposition process, an electroplating process, a chemical plating / electroless plating process, other suitable processes, or a combination of the foregoing.

[0048] Next, referring to FIG. 1E, the first protective layer PR1 is removed to expose the first bonding layer BD1. It should be noted that the step of removing the first protective layer PR1 can also remove the first sacrificial layer SAC1 and the second sacrificial layer SAC2 at the same time to expose the sensing unit 200. After removing the first sacrificial layer SAC1 and the second sacrificial layer SAC2, the sensing unit 200 and the sensing substrate 10A are substantially completed. According to some embodiments, the organic material can be removed by a plasma etching process. For example, the first protective layer PR1, the first sacrificial layer SAC1, and the second sacrificial layer SAC2 are removed, but are not limited thereto.

[0049] As described above, the step of removing the first sacrificial layer SAC1 and the second sacrificial layer SAC2 is performed after the step of forming the first bonding layer BD1 on the planarization layer 110, thereby protecting the metal traces in the sensing unit 200 and reducing the damage to the metal traces caused by the etching process.

[0050] As shown in Figure 1E, the formed sensing substrate 10A may include a first substrate 100, a circuit layer 100C, a planarization layer 110, sensing units 200, and a first bonding layer BD1. The circuit layer 100C may be disposed on the first substrate 100. The planarization layer 110 may be disposed on the circuit layer 100C, and the planarization layer 110 includes an opening 110P. The sensing units 200 may be disposed on the planarization layer 110, and the sensing units 200 may be electrically connected to the circuit layer 100C through the opening 110P. The first bonding layer BD1 may be disposed on the planarization layer 110.

[0051] According to some embodiments, the sensing unit 200 may include an absorption layer 206a, an insulating layer 208, an insulating layer 212, and a sensing layer 210. The insulating layer 208 and the insulating layer 212 may be disposed on the absorption layer 206a, and the sensing layer 210 may be disposed between the insulating layer 208 and the insulating layer 212. According to some embodiments, the sensing unit 200 may further include a support element 204a, and the support element 204a may be disposed between the planarization layer 110 and the absorption layer 206a. According to some embodiments, the sensing unit 200 may further include a fixing element 204b, and the fixing element 204b may be disposed in the opening 204aP of the support element. Furthermore, according to some embodiments, the sensing unit 200 may further include a fixing element 206b, and the fixing element 206b may be disposed in the opening 206aP of the absorption layer 206a.

[0052] According to some embodiments, the first bonding layer BD1 may surround the sensing units 200. Continuing from the foregoing, according to some embodiments, the support element 204a may have an annular structure. For example, in a top view, the support element 204a may have a plurality of bent portions or a loop shape, but is not limited thereto. According to some embodiments, the first bonding layer BD1 may include a first seed layer 302 and a first metal layer 304 disposed on the first seed layer 302. According to some embodiments, the first seed layer 302 may include a molybdenum / copper composite layer, a titanium / copper composite layer, a molybdenum / aluminum composite layer, or a titanium / aluminum composite layer. According to some embodiments, the first metal layer 304 may include a tin / copper composite layer, a tin / gold / nickel / copper composite layer, a tin / gold / nickel composite layer, a gold / nickel composite layer, or a gold / nickel / copper composite layer.

[0053] It should be noted that the foregoing sensing units 200 and the first bonding layer BD1 may be located on the same side of the planarization layer 110, which may provide a relatively flat structural surface, improve the adhesion when the sensing substrate 10A is bonded to the opposite optical substrate 10B (as shown in Figure 2E), and thus may improve the vacuum tightness of the packaging of the sensing device.

[0054] Please refer to FIGS. 2A to 2E. FIGS. 2A to 2E show schematic cross-sectional views of the optical substrate 10B at different process stages according to some embodiments of the present disclosure. It should be understood that, according to some embodiments, additional operation steps may be provided before, during, and / or after the manufacturing method of the optical substrate 10B. According to some embodiments, some of the described operation steps may be replaced or omitted. According to some embodiments, the order of some of the described operation steps may be interchangeable. Furthermore, for clarity of illustration, some elements of the optical substrate 10B may be omitted in the figures, and only some elements are schematically shown. According to some embodiments, additional features may be added to the optical substrate 10B described below. According to other embodiments, some of the features of the optical substrate 10B described below may be replaced or omitted.

[0055] First, please refer to FIG. 2A. A second substrate 400 is provided, and the second substrate 400 can serve as a cover plate. According to some embodiments, the second substrate 400 may have the function of filtering a specific wavelength band. For example, the second substrate 400 can filter out light outside the wavelength band to be detected. According to some embodiments, the material of the second substrate 400 may include silicon (Si), germanium (Ge), chalcogenide glass, gallium arsenide (GaAs), other suitable materials, or a combination of the foregoing, but is not limited thereto. According to some embodiments, the second substrate 400 may further include an optical coating (not shown) disposed on its surface. The material of the optical coating may include germanium (Ge), zinc sulfide (ZnS), zinc selenide (ZnSe), magnesium fluoride (MgF2), beryllium fluoride (BeF2), potassium chloride (KCl), arsenic sulfide (As2S3), other suitable materials, or a combination of the foregoing, but is not limited thereto. Next, a second bonding layer BD2 can be formed on the second substrate 400. First, as shown in FIG. 2A, a second seed layer 402 can be formed on the second substrate 400 first. Specifically, a first seed layer 402 can be formed on the second substrate 400 located in the peripheral area BA and the fan-out area FA. According to some embodiments, the second seed layer 402 may have a multi-layer structure. For example, it has a sub-layer 402a and a sub-layer 402b disposed on the sub-layer 402a. According to some embodiments, the material of the sub-layer 402a may include molybdenum (Mo), titanium (Ti), or other suitable materials, but is not limited thereto. According to some embodiments, the material of the sub-layer 402b may include copper (Cu) or other suitable materials, but is not limited thereto. It should be understood that although the second seed layer 402 shown in the figure has two sub-layers, the present disclosure is not limited thereto. According to some embodiments, the second seed layer 402 may have other suitable numbers or types of sub-layers. According to some embodiments, the second seed layer 402 may include a molybdenum / copper composite layer or a titanium / copper composite layer. The titanium / copper composite layer can not only serve as a seed layer but also as a getter, which can absorb outgassing. According to some embodiments, the second seed layer 402 can be formed by a chemical vapor deposition process, a physical vapor deposition process, an electroplating process, a chemical plating / electroless plating process, other suitable processes, or a combination of the foregoing.

[0056] Next, please refer to FIG. 2B. A second protective layer PR2 can be formed on the second seed layer 402. Specifically, the second protective layer PR2 can be formed on the peripheral area BA, the active area AA, and the fan-out area FA. According to some embodiments, the material and manufacturing method of the second protective layer PR2 may be the same as or similar to those of the foregoing first protective layer PR1, and will not be repeated here.

[0057] Furthermore, a portion of the second protective layer PR2 can be removed by a patterning process to form an opening OP2, and the opening OP2 can expose the second seed layer 402. Specifically, the opening OP2 can expose a partial top surface of the upper sub-layer 402b of the second seed layer 402. According to some embodiments, the patterning process can include one or more photolithography processes and / or etching processes.

[0058] Next, referring to FIG. 2C, a second metal layer 404 can be formed in the opening OP2, and the second metal layer 404 is located on the second seed layer 402. According to some embodiments, the second metal layer 404 can have a multi-layer structure, such as having a sub-layer 404a and a sub-layer 404b disposed on the sub-layer 404a. According to some embodiments, the material of the sub-layer 404a can include copper (Cu) or other suitable materials, but is not limited thereto. According to some embodiments, the material of the sub-layer 404b can include tin (Sn) or other suitable materials, but is not limited thereto. It should be understood that although the second metal layer 404 shown in the figure has two sub-layers, the present disclosure is not limited thereto. According to some embodiments, the second metal layer 404 can have other suitable numbers or types of sub-layers. According to some embodiments, the second metal layer 404 can include a tin / copper composite layer, a tin / gold / nickel / copper composite layer, or a gold / nickel / copper composite layer. According to some embodiments, the second metal layer 404 can be formed by a chemical vapor deposition process, a physical vapor deposition process, an electroplating process, a chemical plating / electroless plating process, other suitable processes, or a combination of the foregoing.

[0059] Next, referring to FIG. 2D, the second protective layer PR2 is removed to expose the second bonding layer BD2. It should be noted that the step of removing the second protective layer PR2 can also remove a portion of the second substrate 400 to form a groove RS in the second substrate 400. According to some embodiments, the second protective layer PR2 and a portion of the second substrate 400 can be removed by a plasma etching process, but is not limited thereto.

[0060] Referring to FIG. 2D, after removing the second protective layer PR2, an antireflection layer 410a and an antireflection layer 410b can be formed on both side surfaces of the second substrate 400, and the antireflection layer 410a can be disposed in the groove RS. The antireflection layer 410a and the antireflection layer 410b can reduce the reflectivity and increase the light transmittance. According to some embodiments, the materials of the antireflection layer 410a and the antireflection layer 410b may include germanium (Ge), zinc sulfide (ZnS), zinc selenide (ZnSe), magnesium fluoride (MgF2), beryllium fluoride (BeF2), potassium chloride, arsenic trisulfide (As2S3), other suitable materials, or combinations of the foregoing, but are not limited thereto. Furthermore, the material of the antireflection layer 410a may be the same as or different from the material of the antireflection layer 410b. According to some embodiments, the antireflection layer 410a and the antireflection layer 410b can be formed by a chemical vapor deposition process, a physical vapor deposition process, an electroplating process, a chemical plating / electroless plating process, other suitable processes, or combinations of the foregoing, but are not limited thereto. Here, the optical substrate 10B is substantially completed.

[0061] Referring to FIG. 3, FIG. 3 shows a schematic cross-sectional structure of a sensing substrate 10A and an optical substrate 10B of a sensing device according to some embodiments of the present disclosure. Specifically, FIG. 3 shows a schematic diagram of the sensing substrate 10A and the optical substrate 10B before alignment and bonding. As shown in FIG. 3, the first bonding layer BD1 of the sensing substrate 10A can be aligned with the second bonding layer BD2 of the optical substrate 10B. Further, the first metal layer 304 of the first bonding layer BD1 can be aligned with the second metal layer 404 of the second bonding layer BD2, such that the sensing unit 200 is opposite to the groove RS.

[0062] Referring to FIG. 4, FIG. 4 shows a schematic cross-sectional structure of a sensing device 1 according to some embodiments of the present disclosure. Specifically, FIG. 4 shows a schematic diagram of the sensing substrate 10A and the optical substrate 10B after alignment and bonding. According to some embodiments, the first bonding layer BD1 and the second bonding layer BD2 can be melted by a bonding process to bond the sensing substrate 10A and the optical substrate 10B to each other. The first metal layer 304 of the first bonding layer BD1 and the second metal layer 404 of the second bonding layer BD2 undergo a melting reaction to form a bonding structure 500. According to some embodiments, the bonding structure 500 may include Cu3Sn, Au5Sn, gold (Au), other suitable materials, or combinations of the foregoing, but are not limited thereto. The bonding process includes heating, pressurizing, light irradiation, or combinations of the foregoing. According to some embodiments, the temperature of the bonding process can be between 100°C and 500°C, or between 150°C and 400°C, or between 200°C and 300°C.

[0063] As shown in FIG. 4, the formed sensing device 1 may include a sensing substrate 10A and an optical substrate 10B. The sensing substrate 10A may include a first substrate 100, a circuit layer 100C, a planarization layer 110, sensing units 200, and a first bonding layer BD1. The circuit layer 100C may be disposed on the first substrate 100. The planarization layer 110 may be disposed on the circuit layer 100C, and the planarization layer 110 includes an opening 110P. The sensing units 200 may be disposed on the planarization layer 110, and the sensing units 200 may be electrically connected to the circuit layer 100C through the opening 110P. The first bonding layer BD1 may be disposed on the planarization layer 110.

[0064] The optical substrate 10B may include a second substrate 400 and a second bonding layer BD2 disposed on the second substrate 400. According to some embodiments, the optical substrate 10B may include an antireflection layer 410a and an antireflection layer 410b, and the antireflection layer 410a and the antireflection layer 410b may be disposed on the surface of the second substrate 400. Furthermore, the optical substrate 10B may have a groove RS, and the groove RS may overlap with the sensing units 200. Specifically, the groove RS may overlap with the sensing units 200 in the normal direction of the second substrate 400 (e.g., the Z direction in the drawing).

[0065] Moreover, the optical substrate 10B and the sensing substrate 10A may be joined to each other by the first bonding layer BD1 and the second bonding layer BD2. According to some embodiments, the first bonding layer BD1 and the second bonding layer BD2 may undergo a melting reaction to form a bonding structure 500. The bonding structure 500 may include Cu 3Sn, Au 5Sn, gold (Au), other suitable materials, or a combination of the foregoing, but is not limited thereto. Specifically, the first metal layer 304 of the first bonding layer BD1 and the second metal layer 404 of the second bonding layer BD2 may undergo a melting reaction to form the bonding structure 500. Furthermore, according to some embodiments, the first bonding layer BD1 and the second bonding layer BD2 are joined to each other to form a cavity CV in the sensing device 1. As mentioned above, the configuration of the sensing substrate 10A can improve the tightness during bonding, enhance the packaging vacuum tightness of the sensing device 1, and thereby improve the sensing sensitivity of the sensing device 1 or enhance the overall performance of the sensing device 1.

[0066] Please refer to FIG. 5. FIG. 5 shows an equivalent circuit diagram of the sensing device 1 according to some embodiments of the present disclosure. As shown in FIG. 5, the sensing device 1 may have a sensing array, the sensing array may have a plurality of sensing pixels PX, and the bonding structure 500 may be disposed around the sensing array. According to some embodiments, the sensing pixel PX may include a thin film transistor TR as a driving element and a sensing unit 200. The thin film transistor TR may be electrically connected to the scanning line SL, the data line DL, and the sensing unit 200 respectively. One end of the sensing unit 200 is electrically connected to the thin film transistor TR, and the other end is electrically connected to the bias signal line BL. According to some embodiments, the scanning line SL may be electrically connected to a row driver 11. Furthermore, according to some embodiments, the data line DL may be electrically connected to a readout driver 13. The row driver 11 may be further electrically connected to an integrated circuit (IC) element 15, and the readout driver 13 may be further electrically connected to the integrated circuit (IC) element 15 to read the sensing signal through the integrated circuit element 15.

[0067] In summary, according to the embodiments of the present disclosure, the provided sensing substrate can provide a relatively flat structural surface, which can improve the adhesion when bonding with the optical substrate, thereby improving the encapsulation vacuum tightness of the sensing device, improving the sensing sensitivity of the sensing device, or enhancing the overall performance of the sensing device.

[0068] Although the embodiments of the present disclosure and their advantages have been disclosed above, it should be understood that any person with ordinary skill in the art can make changes, substitutions, and modifications without departing from the spirit and scope of the present disclosure. The features between the embodiments of the present disclosure can be arbitrarily combined and used as long as they do not violate the inventive spirit or conflict with each other. In addition, the protection scope of the present disclosure is not limited to the processes, machines, manufactures, compositions of matter, devices, methods, and steps in the specific embodiments described in the specification. Any person with ordinary skill in the art can understand the processes, machines, manufactures, compositions of matter, devices, methods, and steps developed currently or in the future from the disclosure of the present disclosure. As long as they can perform substantially the same functions or obtain substantially the same results in the embodiments described herein, they can be used according to the present disclosure. Therefore, the protection scope of the present disclosure includes the above-mentioned processes, machines, manufactures, compositions of matter, devices, methods, and steps. The protection scope of the present disclosure shall be determined by the scope of the appended patent application. Any embodiment or claim of the present disclosure does not have to achieve all the purposes, advantages, and features disclosed in the present disclosure.

[0069] 1: Sensing device 10A: Sensing substrate 10B: Optical substrate 11: Scanning line driving element 13: Reading driving element 15: Integrated circuit element 100: First substrate 100P: Opening 100C: Circuit layer 102: Conductive layer 110: Planarization layer 110P: Opening 200: Sensing unit 202: Conductive layer 204a: Support element 204b: Fixing element 206a: Absorbing layer 206aP: Opening 206b: Fixing element 208: Insulating layer 210: Sensing layer 212: Insulating layer 302: First seed layer 302a: Sub-layer 302b: Sub-layer 304: First metal layer 304a: Sub-layer 304b: Sub-layer 400: Second substrate 402: Second seed layer 402a: Sub-layer 402b: Sub-layer 404: Second metal layer 404a: Sub-layer 404b: Sub-layer 410a: Anti-reflection layer 410b: Anti-reflection layer 500: Bonding structure AA: Active area BA: Peripheral area BD1: First bonding layer BD2: Second bonding layer BL: Bias signal line CV: Cavity DL: Data line EP: End FA: Fan-out area OP1: Opening OP2: Opening P1: Opening P2: Opening PR1: First protective layer PR2: Second protective layer PX: Sensing pixel RS: Groove SAC1: First sacrificial layer SAC2: Second sacrificial layer SL: Scanning line TR: Thin film transistor

Claims

1. A sensing substrate, comprising: First substrate; A circuit layer is disposed on the first substrate; A planarization layer is disposed on the circuit layer, and the planarization layer includes an opening; a sensing unit is disposed on the planarization layer, and the sensing unit is electrically connected to the circuit layer through the opening, wherein the sensing unit includes: an absorption layer, a first insulating layer and a second insulating layer disposed on the absorption layer, and a sensing layer disposed between the first insulating layer and the second insulating layer; and a first bonding layer is disposed on the planarization layer.

2. The sensing substrate as claimed in claim 1, wherein the sensing unit and the first bonding layer are located on the same side of the planarization layer.

3. The sensing substrate as claimed in claim 1, wherein the sensing unit further includes a support element disposed between the planarization layer and the absorption layer.

4. The sensing substrate as claimed in claim 3, wherein the sensing unit further includes a fixing element disposed in an opening of the support element.

5. The sensing substrate as claimed in claim 1, wherein the first bonding layer surrounds the sensing unit.

6. The sensing substrate as claimed in claim 1, wherein the first bonding layer includes a first seed layer and a first metal layer disposed on the first seed layer.

7. The sensing substrate as described in claim 6, wherein the first seed layer comprises a molybdenum / copper composite layer, a titanium / copper composite layer, a molybdenum / aluminum composite layer, or a titanium / aluminum composite layer.

8. The sensing substrate as claimed in claim 6, wherein the first metal layer comprises a tin / copper composite layer, a tin / gold / nickel / copper composite layer, a tin / gold / nickel composite layer, a gold / nickel composite layer, or a gold / nickel / copper composite layer.

9. A sensing device, comprising: A sensing substrate includes: a first substrate; a circuit layer disposed on the first substrate; a planarization layer disposed on the circuit layer, the planarization layer including an opening; a sensing unit disposed on the planarization layer, the sensing unit being electrically connected to the circuit layer through the opening, wherein the sensing unit includes: an absorption layer, a first insulating layer disposed on the absorption layer, a second insulating layer, and a sensing layer disposed between the first insulating layer and the second insulating layer; a first bonding layer disposed on the planarization layer; and an optical substrate including a second substrate and a second bonding layer disposed on the second substrate; wherein the optical substrate and the sensing substrate are bonded to each other through the first bonding layer and the second bonding layer.

10. The sensing device as claimed in claim 9, wherein the first bonding layer and the second bonding layer are melt-reacted to form a bonding structure, the bonding structure comprising Cu3Sn, Au5Sn or gold.

11. The sensing device as claimed in claim 9, wherein the optical substrate further includes an anti-reflective layer disposed on the surface of the second substrate.

12. The sensing device as claimed in claim 9, wherein the optical substrate has a groove that overlaps with the sensing unit.

13. The sensing device as claimed in claim 9, wherein the first bonding layer and the second bonding layer are bonded to each other to form a cavity in the sensing device.

14. A method for manufacturing a sensing device, comprising: A sensing substrate is provided, comprising: providing a first substrate; forming a circuit layer on the first substrate; forming a planarization layer on the circuit layer, the planarization layer including a first opening; forming a sensing unit on the planarization layer, the sensing unit being electrically connected to the circuit layer through the first opening, wherein the sensing unit includes: an absorption layer, a first insulating layer disposed on the absorption layer and a second insulating layer, and a sensing layer disposed between the first insulating layer and the second insulating layer; and forming a first bonding layer on the planarization layer.

15. A method of manufacturing a sensing device as claimed in claim 14, wherein the step of forming the sensing unit on the planarization layer includes: A first sacrificial layer is formed on the planarization layer; A support element is formed on the first sacrificial layer; A second sacrificial layer is formed on the support element; The absorption layer is formed on the second sacrificial layer; the first insulating layer is formed on the absorption layer; the sensing layer is formed on the first insulating layer; and the second insulating layer is formed on the sensing layer.

16. The method of manufacturing a sensing device as claimed in claim 15, wherein the step of forming the sensing unit on the planarization layer further includes removing the first sacrificial layer and the second sacrificial layer, and the step of removing the first sacrificial layer and the second sacrificial layer is performed after the step of forming the first bonding layer on the planarization layer.

17. A method of manufacturing a sensing device as claimed in claim 14, wherein the step of forming the first bonding layer on the planarization layer includes: A first seed layer is formed on the planarization layer; A protective layer is formed on the first seed crystal layer; A portion of the protective layer is removed to form a second opening, which exposes the first seed layer; a first metal layer is formed in the second opening; And remove the protective layer.

18. The method of manufacturing the sensing device as described in claim 14 further includes: An optical substrate is provided, comprising: providing a second substrate; and forming a second bonding layer on the second substrate.

19. The method of manufacturing the sensing device as claimed in claim 18 further includes melting the first bonding layer and the second bonding layer by a bonding process to bond the sensing substrate and the optical substrate to each other.

Citation Information

Patent Citations

  • Electronic device

    TW202325645A

  • Electronic device

    TW202341302A