Integrated circuit and method of manufacturing the same

TWI945705BActive Publication Date: 2026-11-11TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW114105898
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Priority Date
2024-12-20
Filing Date
2025-02-18
Publication Date
2026-11-11
Estimated Expiration
2045-02-17

Smart Images

  • Figure TWG2TB001920457_001
    Figure TWG2TB001920457_001
  • Figure TWG2TB001920457_002
    Figure TWG2TB001920457_002
  • Figure TWG2TB001920457_003
    Figure TWG2TB001920457_003
Patent Text Reader

Abstract

An integrated circuit and a method of manufacturing the same are provided. The method includes forming a fin region comprising one or more fin field-effect transistors (finFETs) in a device region of a semiconductor substrate, and forming a high-voltage (HV) plane region adjacent to the fin region. Each finFET in the device region includes one or more fins formed having fin-shaped tops at a first height from the fin substrate region. The HV plane region includes a first HV plane region and a second HV plane region. The first HV plane region is located at a second height from the fin substrate region, greater than the first height. The second HV plane region has an HV isolation structure isolating the first HV plane region from the fin region. The HV isolation structure includes a boundary buffer with an intermediate step at a third height from the fin substrate region, the third height being equal to or greater than the first height and less than the second height.
Need to check novelty before this filing date? Find Prior Art

Description

Prior Technology

[0001] The following content pertains to semiconductor integrated circuits (ICs) using fin field-effect transistors (finFETs) or other three-dimensional (3D) semiconductor structures that include fins and planar boundaries, as well as their fabrication methods. Simple Explanation of the Diagram

[0002] The best understanding of this disclosure will be achieved by reading the following detailed description in conjunction with the accompanying drawings. It should be noted that, according to industry standard practice, the various features are not drawn to scale. In fact, the dimensions of the various features may be arbitrarily increased or decreased for clarity of explanation. Figure 1A is a cross-sectional view of an integrated circuit (IC) structure (Example 1) according to an exemplary embodiment of the present disclosure, which includes a fin field-effect transistor (finFET) region, an internal high voltage (HV) left plane region and an internal low / medium voltage (M / LV) right plane region, wherein the left plane region includes a boundary buffer of the left plane region and the right plane region includes a boundary buffer of the right plane region. Figure 1B is a detailed cross-sectional view of the boundary buffer zone of the left planar region in the IC structure shown in Figure 1A (Example 1) according to an exemplary embodiment of the present disclosure. Figure 1C is a detailed cross-sectional view of the boundary buffer of the right-side planar region in the integrated circuit IC structure (Example 1) shown in Figure 1A according to an exemplary embodiment of the present disclosure, including a depiction of the slope of the boundary buffer relative to the height of the HV planar region and the LV fin field-effect transistor (finFET) region (Example 1). Figure 2A is a top view of a wafer including an IC structure, the IC structure including a planar region of a wafer / IC / device area adjacent to a sealing ring surrounding the wafer, the sealing ring including an outer dummy sealing ring, a finned intermediate sealing ring wall and an inner sealing ring (i.e., a seal ring enhanced zone (SREN)). According to an exemplary embodiment of this disclosure (Example 2), the inner sealing ring includes a planar boundary buffer that reduces the step height from the fins of the sealing ring wall to the planar region of the wafer, the planar boundary buffer being adjacent to the planar region of the wafer. Figure 2B is a detailed top view of the wafer including the integrated circuit (IC) structure shown in Figure 2A, illustrating details of the external dummy sealing ring structure, the intermediate sealing ring wall (fin structure), and the internal sealing ring (planar boundary buffer) structure according to an exemplary embodiment of this disclosure (Example 2). Figure 2C is a cross-sectional view of the planar boundary buffer zone of the sealing ring shown in Figures 2A and 2B according to an exemplary embodiment of the present disclosure, adjacent to the fin-like structure of the sealing ring wall and the planar region of the wafer. Figure 3 is a cross-sectional view of an IC structure (Example 3) according to an exemplary embodiment of the present disclosure, which includes a fin field-effect transistor (finFET) region and an HV left-side plane region of interconnects, wherein the left-side plane region includes a buffer boundary buffer of the left-side plane region. Figure 4 is a semiconductor wafer layout diagram according to an exemplary embodiment of the present disclosure, illustrating an IC layout arrangement, the IC layout including one or more boundary buffers. Figure 5 illustrates a method for forming an IC according to an exemplary embodiment of the present disclosure. The IC includes a fin field-effect transistor (finFET) region, an HV left-side plane region of interconnects, and an M / LV right-side plane region of interconnects. The left-side plane region includes a boundary buffer of the left-side plane region, and the right-side plane region includes a boundary buffer of the right-side plane region. Figures 6A-6E illustrate the various stages of forming an IC (Example 5) according to an exemplary embodiment of the present disclosure, the IC including a fin field-effect transistor (finFET) region, an HV left-side plane region of interconnects and an M / LV right-side plane region of interconnects, the left-side plane region including a boundary buffer of the left-side plane region and the right-side plane region including a boundary buffer of the right-side plane region. Implementation

[0003] The following disclosure provides numerous different embodiments or examples for implementing various features of the provided subject matter. Specific examples of components and arrangements are described below to simplify this disclosure. Of course, these are merely examples and are not intended to be limiting. For example, the dimensions of elements are not limited to the disclosed range or values, but may depend on process conditions and / or desired characteristics of the apparatus. For instance, the following description of a first feature formed above or on a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features may be formed between the first and second features, thereby preventing direct contact between the first and second features. For simplicity and clarity, various features may be drawn at different scales.

[0004] Numerical values ​​in this disclosure and the claims should be understood to include values ​​that remain the same when reduced to the same number of significant figures, as well as values ​​that differ from those determined by experimental errors less than those determined by conventional measurement techniques of the type described in this disclosure. All scopes of this disclosure include the stated endpoints.

[0005] The term "approximately" can be used to include any different numerical value without altering its fundamental function. When used with a range, "approximately" also indicates the range defined by the absolute values ​​of its two endpoints; for example, "approximately 2 to approximately 4" also indicates a range of "from 2 to 4". The term "approximately" can be plus or minus 10% of the indicated numerical value.

[0006] This disclosure relates to structures composed of different layers. When the terms "on" or "on" are used to refer to two different layers (including a substrate), they simply mean that one layer is on or on another layer. These terms do not require that the two layers be in direct contact with each other and allow other layers to be located between them. For example, all layers of a structure can be considered to be "on" the substrate, even if they are not all in direct contact with the substrate. The term "direct" can be used to indicate that two layers are in direct contact with each other, with no layers between them. Furthermore, when referring to performing process steps on a substrate, this should be interpreted as performing such steps on any layers that may be present on the substrate, depending on the context.

[0007] Additionally, for ease of explanation, this document may use spatially relative terms such as "beneath," "below," "lower," "above," "upper," and similar expressions to describe the relationship between one element or feature shown in the figures and another element or feature. These spatially relative terms are intended to encompass different orientations of the device during use or operation, in addition to those shown in the figures. The device may have other orientations (rotated 90 degrees or in other orientations), and the spatially relative descriptions used herein may be interpreted accordingly.

[0008] As used herein, the term "intermediate" or "intermediate step" refers to a step, platform, structure, or surface whose height is higher than the first end of the intermediate step and whose height is lower than or equal to the second end of the intermediate step.

[0009] As used in this article, the term "recess" is related to boundary buffers and refers to a surface or structure that has a height or elevation that is lower than that of one or more adjacent boundary buffers.

[0010] As used herein, the terms "finFET substrate region" or "fin substrate region" or "fin top substrate region" refer to the first end or portion of a fin, wherein the fin extends from an adjacent shallow trench isolation (STI) material or other material to a second end, or from the finFET substrate region to the fin top.

[0011] The term "layer" as used in this article may include a single layer or multiple layers.

[0012] The term "conductive feature" as used in this article may refer to metallized layer contacts, patterned metallized layer contacts, or other electrically conductive metal contacts.

[0013] The term "intermetallic dielectric" (IMD) film or layer, as may be used in this article, refers to a dielectric / insulating material layer between two metal layers.

[0014] The term "interlayer dielectric" (ILD) may be used in this article to refer to an insulating material structure placed between two conductive layers.

[0015] Generally, some embodiments disclosed herein relate to semiconductor devices that use and / or form one or more fin field-effect transistors (FinFETs). FinFETs are so named because the channel between the source and drain regions of a field-effect transistor (FET) typically takes the form of three-dimensional (3D) stacked walls or "fins" built on and / or rising from a semiconductor wafer. Therefore, a FinFET is a 3D transistor. The fins serve as the transistor channel, and the gate typically contacts the top and sides of the fins. Typically, FinFET devices have significantly faster switching times and higher current densities compared to planar transistor devices.

[0016] This disclosure and the exemplary embodiments described herein relate to the optimization of IC structure topology to employ various manufacturing processes used in manufacturing ICs, thereby expanding the process window associated with these semiconductor manufacturing processes and reducing device defects in the manufacturing process. Generally, according to the exemplary embodiments, applicable fields include, but are not limited to, high-voltage / medium-voltage / low-voltage integration processes, such as integration processes and manufacturing processes for low-voltage (LV) (<3.3V), medium-voltage (MV) (3.3V~12V), and high-voltage (HV) (>12V) IC regions for interconnects, integration processes and manufacturing processes for LV (<3.3V) and HV (>20V) IC regions for interconnects, and integration processes and manufacturing processes for planar regions of ICs typically used for interconnects with adjacent fin regions manufactured using FinFET processes.

[0017] According to an example manufacturing process, some conventional static random access memory (SRAM) ICs suffer manufacturing yield losses due to defects in IC manufacturing-related processes, particularly dummy polysilicon (“dummy polysilicon”) gates, especially the 16HV isolation ring / structure. Transmission electron microscopy (TEM) analysis has revealed that the step height between the HV plane region and the FinFET LV region in these SRAM devices results in a relatively narrow process window because the FinFET fins are recessed below the HV plane region, and the height of the LV FinFET substrate region (i.e., the shallow trench isolation (STI) region adjacent to the FinFET fins) is much lower than the height of the HV plane region.

[0018] This disclosure and the exemplary embodiments provided herein offer solutions to improve IC manufacturing-related yields, as previously described, including adjacent HV and LV regions. These solutions are also applicable to other interconnect semiconductor structures, including planar regions interconnected with adjacent fin regions, such as LV regions, or any fin-containing region, whether active or not (e.g., not limited to sealing rings containing fin structures adjacent to IC planar regions, HV, MV, LV regions, or other semiconductor structures where the height of the fin substrate region is lower than the height of adjacent or adjacent planar regions). The exemplary embodiments described herein add planar regions or boundary buffers, including recesses or buffers, between the fins and the planar boundary regions to minimize the step height slope of the relatively high H / MV or other planar regions from the fin substrate region to the interconnects. This disclosure can expand the manufacturing process window relative to IC manufacturing-related process windows without the disclosed boundary buffers. In other words, based on the intermediate step of the boundary buffer located between the HV or higher HV plane region and the LV FinFET region in this example, this disclosure provides a reduced gradient of the step from the FinFET substrate region to the boundary buffer compared to the transition gradient from the FinFET substrate region to the higher interconnect plane region without using the boundary buffer disclosed herein. Therefore, the boundary buffer disclosed here results in a reduction of device defects related to or caused by subsequent IC manufacturing processes such as forming and planarizing dielectric layers, e.g., interlayer dielectric (ILD) layers. In other words, the reduced slope between adjacent and adjacent planes and the fin material-filled region makes the surface relatively smoother to accommodate material filling or formation processes.

[0019] Furthermore, according to some embodiments, the disclosed structure and its formation method utilize existing planar regions and existing processes of currently manufactured devices to manufacture currently manufactured devices. Therefore, according to some embodiments, the disclosed boundary buffer structure and method reduce the slope of the terrain from the planar region to the fin boundary region by using existing IC regions and manufacturing processes, without increasing additional manufacturing costs compared to the manufacturing costs associated with similar devices that do not have the disclosed boundary buffer.

[0020] Another example of current semiconductor structures and related narrow process windows includes finned LV device regions and planar MV device regions covered by planar isolation rings to form isolation wells for each device. Here, the step height from the isolation ring to the fin region is relatively large because the fin region needs to be recessed to form the fin structure.

[0021] Another further example of existing semiconductor structures and associated narrow process windows includes a 16HV sealing ring having a fin region comprising a finned boundary region with a blank planar region or planar isolation ring to an adjacent wafer. Without using the boundary buffer disclosed herein, the sealing ring / wafer topography could result in a narrowing of the process window for subsequent device processing and negatively impact device yield due to a relatively large fin (sealing ring) to planar (wafer) step height.

[0022] According to the exemplary embodiments described below, a wafer, IC, semiconductor device or structure, and a method of manufacturing thereof, includes one or more boundary buffers having intermediate steps and / or recessed planar regions to minimize the step height slope of the transition from fin to planar region and the transition from planar region to fin. According to the following exemplary embodiments, Embodiment 1 1001 includes the use of a boundary buffer formed within an isolation ring structure, the isolation ring structure isolating (a) a boundary buffer of the HV plane region of the interconnect to the logic or LV FinFET region, and (b) a boundary buffer of the M / LV plane region of the interconnect to the logic or LV FinFET region; Embodiment 2 2001 includes the use of a boundary buffer formed within a seal ring reinforcement region (SREZ), the boundary buffer being adjacent to or connected to the HV or M / LV plane region of the wafer; Embodiment 3 3001 includes the use of a boundary buffer formed within an isolation ring structure, the isolation structure including an STI trench deeper than the LV FinFET STI trench to reduce the step height from the FinFET substrate region to the adjacent HV plane region; and Embodiment 4 4001 includes a wafer layout comprising Embodiment 1 1001 (see Figures 1A-1C) and Embodiment 2 One or more boundary buffers from Embodiment 2001 (see Figures 2A-2C) and Embodiment 3 3001 (see Figure 3). Embodiment 4 4001 (see Figure 4) provides an IC wafer layout, which may include one or more of Embodiment 1 1001, Embodiment 2 2001 and Embodiment 3 3001.

[0023] According to some exemplary embodiments, the boundary buffer is formed with intermediate steps or grooves such that the step height from the higher metal-oxide-semiconductor (MOS) silicon HV / MV / LV planar region to the lower MOS LV logic fin region is less than 60 nanometers.

[0024] According to some exemplary embodiments, the boundary buffer is formed with an intermediate step or groove. According to some exemplary embodiments, the boundary buffer with an intermediate step or groove is formed such that the step height from the planar region of the sealing ring (i.e., the boundary buffer) to the higher planar region of the wafer is less than 60 nanometers, and the planar region of the wafer is higher than the planar region of the sealing ring (i.e., the boundary buffer). According to this embodiment, the sealing ring fin region fabrication process is a fin region formation process related to the wafer fin field-effect transistor (FinFET) fabrication process, wherein the sealing ring covers the boundary buffer. Since the original sealing ring is a fin region, and the wafer region contacting the sealing ring is a planar region, the SREZ region of the sealing ring is modified from a fin type to a planar topology, thereby reducing the step height from the sealing ring to the wafer boundary using existing integrated circuit fabrication methods. Because there is no isolation ring between the sealing ring and the boundary buffer of the sealing ring, no electrical operation is required.

[0025] According to some exemplary embodiments, the boundary buffer is formed with an intermediate step or groove, such that the step height does not use an isolation ring or sealing ring, wherein the integrated circuit adds an additional area or zone to accommodate the boundary buffer as disclosed.

[0026] According to some exemplary embodiments, the LV fin region serves as logic circuitry, providing LV voltage operation for high-speed, low-power, or SRAM functions, while the planar region interconnected with the LV logic circuitry includes MV and HV devices. According to some exemplary embodiments, the HV device is used to drive and control the finFET transistors of the LV logic circuitry, thereby controlling the transistors' on / off function. The MV device is used to drive and control the transistor sources to control color and / or brightness via voltage bias, or to drive and control the digital-to-analog converter (DAC) function for signal transmission.

[0027] According to another exemplary embodiment, the existing integrated circuit layout includes a 40 nm step height or height offset from the top of the fin to the fin substrate region (i.e., STI), and a step height of approximately 30 nm from the adjacent and interconnected planar H / MV region to the fin substrate region STI. According to this exemplary embodiment, due to some limitations of the planar process used to manufacture this integrated circuit, a total step height of 70 nm from the H / MV planar region to the LV fin-type substrate region is desired. To accommodate the planar process, the existing structure and available area of ​​this integrated circuit are used to form a boundary buffer to achieve a plane-to-fin substrate region transition height (i.e., step) of less than 70 nm, or less than 60 nm, or less than 50 nm, etc.

[0028] According to some exemplary embodiments, a boundary buffer is used to create a planar boundary region height that is close to or equal to the height of the top of the LV fin region. In this case, the 40 nm step height between the planar boundary buffer and the fin STI, and the approximately 30 nm step height between the planar boundary buffer and the adjacent, interconnected HV planar region, result in a total of approximately 70 nm from the HV planar region to the STI fin substrate region of the LV logic circuit, which is consistent with the structural design constraints of the original integrated circuit before the addition of the boundary buffer. It should be understood that this is only an exemplary embodiment and scenario, and the boundary buffer disclosed herein can be adapted to other structural design constraints or requirements associated with the integrated circuit structure. Specifically, the boundary buffer provides an intermediate step between the planar region and the fin region to accommodate the original integrated circuit structure that requires the total step height from the planar region to the LV fin substrate region to be greater than or less than 70 nm.

[0029] Referring to FIG1A, a cross-sectional view (a cross-sectional view of the plane formed by the x and z directions perpendicular to the y direction) of an integrated circuit (IC) structure (Example 1) 1001 according to an exemplary embodiment of the present disclosure is shown, which includes a finFET region 100, a left plane region 200 for high voltage (HV) interconnects (including a boundary buffer 230 from the left plane region to the fin region) and a right plane region 300 for low / medium voltage (M / LV) interconnects (including a boundary buffer 330 of the right plane region).

[0030] As shown in the figure, this exemplary embodiment is an integrated circuit that includes the following: Semiconductor substrate 2, on which deep N-wells (DNW) 112, 212A, 212B and 312A, and core well 113 are formed; A fin region 100 is formed on the core well 113, the fin region having a first finFET transistor structure 111A, a second finFET transistor structure 111B, a third finFET transistor structure 111C, and a fourth finFET transistor structure 111D, and a shallow trench isolation (STI) region 115 formed next to each finFET transistor fin (see, for example, FIG. 1B: fins 116A1, 116A2, 116B1, and 116B2). Polycrystalline silicon gates 117A, 117B, 117C, and 117D are formed on each fin; The first planar region 200 has an H / MV region 210, on which deep N-wells 212A and 212B are formed, and on which first (MOS) HV transistor devices 211A and HV MOS gates 216A, second (MOS) HV transistor devices 211B and HV MOS gates 216B are formed. Planar HV P-wells 213A, 213B, and 213C, and planar HV N-wells 214A, 214B, and 214C are also formed in the HV planar region 200. STIs 215A, 215B, 215C, 215D, 215E, 215F, 215G, 215H, 215I, 215J, and 215K are formed to provide isolation for the various depicted semiconductor regions for HV planar region operation, and to dummy polysilicon gates 217; and The second planar region 300 has an M / LV region 310, which is formed on the deep N-well 312A, and on which a first M / LV transistor device 311A ​​and an M / LV metal gate 316A, a second M / LV transistor device 311B and an M / LV metal gate 316B, and a third M / LV transistor device 311C and an M / LV metal gate 316C are formed. Planar M / LV P-well 313B, planar M / LV N-wells 314A and 314B, and M / LV region planar well 313A are also formed in the M / LV planar region 300. STI 315A, 315B, 315C, 315D, 315E, 315F, 315G, 315H, 315I, 315J, 315K, 315L, 315L, 315M, and 315N are formed to provide isolation for various depicted semiconductor regions for operation in the M / LV planar region.

[0031] The first planar region 200 further includes an isolation (ring) 220 structure having a boundary buffer 230 from the left planar region to the fin region, and a top surface 231 of the boundary buffer from the left planar region to the fin region.

[0032] The second plane region 300 further includes an isolation (ring) structure 320, which has a boundary buffer 330 from the right plane region to the fin region, and a top surface 331 of the boundary buffer 331 from the right plane region to the fin region, wherein the isolation (ring) structure extends from STI 315N to plane M / LV P well 313B. The complete isolation (ring) structures 220 and 320 surround the LV logic region 100 structure.

[0033] According to an exemplary embodiment, an IC structure 1001 is formed on a wafer made of semiconductor material, wherein the integrated interconnect structure or integrated circuit (IC) structure 1001 is built or formed thereon using conventional semiconductor manufacturing techniques, including but not limited to lithography, such as applying a photoresist layer, patterning a photoresist layer, developing a photoresist layer, then etching, followed by planarization and cleaning, applying a pattern / structure in a given layer. While the specific semiconductor manufacturing process required to form the illustrated IC structure 1001 is not the focus of this disclosure, for completeness, a general description of the semiconductor manufacturing process is provided below.

[0034] The semiconductor substrate 2 material may include silicon, for example, in the form of crystalline silicon or polycrystalline silicon. In alternative embodiments, the substrate may be made of other elemental semiconductors, such as germanium, or may include compound semiconductors such as silicon carbide (SiC), gallium arsenide (GaAs), gallium carbide, gallium phosphide, indium arsenide (InAs), indium phosphide (InP), silicon germanium, silicon germanium carbide, gallium arsenide phosphide, or indium gallium phosphide. In a particular embodiment, the wafer substrate is silicon.

[0035] Typically, photoresist layers can be applied using methods such as spin coating, spray coating, roller coating, dip coating, or extrusion coating. In spin coating, the substrate is typically placed on a rotating platform, which may include a vacuum fixture to hold the substrate in place. The photoresist composition is then coated onto the center of the substrate. The speed of the rotating platform is then increased to allow the photoresist to diffuse uniformly from the center of the substrate to its periphery. The rotational speed of the platform is then fixed, which controls the final thickness of the photoresist layer.

[0036] Next, the photoresist composition is baked or cured to remove the solvent and harden the photoresist layer. In some specific embodiments, baking is performed at a temperature of about 90°C to about 110°C. Baking can be performed using a hot plate or oven, or similar equipment. Thus, a photoresist layer is formed on the substrate.

[0037] The photoresist layer is then patterned by radiation exposure. The radiation can be any wavelength of light carrying the desired mask pattern. In a particular embodiment, extreme ultraviolet light with a wavelength of about 13.5 nanometers is used for patterning because this allows for smaller feature sizes. This results in some portions of the photoresist layer being exposed to radiation, while other portions are not. This exposure makes some portions of the photoresist soluble in the developer, while other portions remain insoluble in the developer.

[0038] An additional photoresist baking step (post-exposure baking, or PEB) may be performed after radiation exposure. For example, this may help release acid leaving groups (ALGs) or other molecules that are important in chemically amplified photoresists.

[0039] The photoresist layer is then developed using a developer. The developer can be an aqueous solution or an organic solvent. The soluble portions of the photoresist layer are dissolved and rinsed away during the development step, leaving the photoresist pattern. A common example of a developer is an aqueous solution of tetramethylammonium hydroxide (TMAH). Other developers may include 2-heptanone, butyl acetate, isoamyl acetate, cyclohexanone, 5-methyl-2-hexanone, methyl-2-hydroxyisobutyrate, ethyl lactate or propylene glycol monomethyl ether acetate, amyl acetate, butyl propionate, hexyl acetate, butyl butyrate, isobutyl butyrate, 2,5-dimethyl-4-hexanone, 2,6-dimethyl-4-heptanone, propyl isobutyrate, or isobutyl propionate. Generally, any suitable developer can be used. Sometimes, a post-development baking or "hard baking" may be performed after development to stabilize the developed photoresist pattern for optimal performance in subsequent steps.

[0040] Next, a portion of the layer beneath the patterned photoresist layer is now exposed. Etching transfers the photoresist pattern to the layer beneath the patterned photoresist layer. After use, the patterned photoresist layer can be removed, for example, using various solvents such as N-methylpyrrolidone (NMP) or alkaline media or other stripping agents at elevated temperatures, or by dry etching using oxygen plasma.

[0041] Generally, any etching step used herein may employ wet etching, dry etching, or plasma etching processes such as reactive ion etching (RIE) or inductively coupled plasma (ICP), or combinations thereof, as appropriate. Etching may be anisotropic. Depending on the material, the etchant may include carbon tetrafluoride (CF4), hexafluoroethane (C2F6), octafluoropropane (C3F8), trifluoromethane (CHF3), difluoromethane (CH2F2), fluoromethane (CH3F), trifluoromethane (CHF3), fluorides, nitrogen (N2), hydrogen (H2), oxygen (O2), argon (Ar), xenon (Xe), xenon difluoride (XeF2), helium (He), carbon monoxide (CO), carbon dioxide (CO2), fluorine (F2), chlorine (Cl2), oxygen (O2), hydrogen bromide (HBr), hydrofluoric acid (HF), nitrogen trifluoride (NF3), sulfur hexafluoride (SF6), boron trichloride (BCl3), ammonia (NH3), bromine (Br2), nitrogen trifluoride (NF3), or similar substances, or combinations thereof, in various proportions. For example, silicon dioxide can be wet-etched using hydrofluoric acid and ammonium fluoride. Alternatively, silicon dioxide can be dry-etched using various mixtures of CHF3, O2, CF4 and / or H2.

[0042] Planarization can be performed to obtain a flat surface. Planarization can be performed, for example, using a chemical mechanical polishing (CMP) process. Typically, CMP is performed using a rotating platform with a polishing pad. The substrate is attached to a rotating carrier. A slurry or solution containing various chemicals and abrasives is dispensed onto the polishing pad or wafer substrate. During polishing, both the polishing pad and the carrier rotate, which creates mechanical and chemical effects on the surface of the wafer substrate and / or its top layers, removing unwanted material and creating a highly flat surface. A post-CMP cleaning step is then performed using a rotating brush and cleaning fluid to clean one or both sides of the wafer substrate.

[0043] Finally, cleaning steps such as wet cleaning can be performed between various process steps. The cleaning solution will depend on the etching formulation and the exposed layers. Examples of cleaning solutions may include deionized water, diluted HF, and other conventional solutions.

[0044] The dielectric structure can be made from any suitable combination of dielectric materials. Examples of dielectric materials may include silicon dioxide (SiO2), silicon nitride (Si3N4), silicon carbide (SiC), hafnium dioxide (HfO2), zirconium dioxide (ZrO2), aluminum oxide (Al2O3), silicon oxynitride (SiOxNy), hafnium oxynitride (HfOxNy), or zirconium oxynitride (ZrOxNy), or hafnium silicate (ZrSixOy), or zirconium silicate (ZrSixOy), or silicon carbonitride (SiCxOyNz), or hexagonal boron nitride (hBN). Other dielectric materials may include tantalum oxide (Ta2O5), nitrides such as silicon nitride, polycrystalline silicon, phosphosilate glass (PSG), fluorosilate glass (FSG), undoped silicate glass (USG), high-stress undoped silicate glass (HSUSG), and borosilicate glass (BSG).

[0045] Any conductive material discussed herein, such as the metal vias 240A and 240B, can generally be any conductive metal or conductive oxide. Examples of suitable metals include copper, aluminum, nickel, chromium, gold, germanium, silver, titanium, tungsten, platinum, tantalum, ruthenium, cobalt, rhenium, palladium, or zirconium; composite materials such as TiN, WN, or TaN; or alloys thereof such as AlCu. Examples of suitable conductive oxides include indium tin oxide (ITO), zinc oxide (ZnO), tin oxide (SnO), zinc aluminum oxide (AlZnO), indium oxide (InO), or cadmium oxide (CdO). Metallic or oxide materials can be deposited, for example, by vapor deposition or sputtering, electroplating, chemical vapor deposition (CVD), physical vapor deposition (PVD), atomic layer deposition (ALD), or other suitable methods.

[0046] As shown in Figures 1A and 1B, the HV plane region 210 is the highest point in the IC wafer / semiconductor structure 1001, while the highest point of the M / LV plane region 310 is at the same vertical height as the fin region 100. Therefore, the boundary buffer 230 implemented in the first or left plane region 200 may have a different intermediate or recessed step height than the boundary buffer 330 implemented in the second or right plane region 300. For example, according to some embodiments, the step height from the HV plane region 210 to the fin substrate region 118 is less than 70 nanometers, while the step height from the M / LV plane region 310 to the fin substrate region 118 is less than 60 nanometers. Although Figures 1A and others show that the M / LV plane region 310 is at the same height as the fin region 100, the M / LV plane region 310 may extend further vertically (in the z-direction), depending on the voltage plateau accommodated by the M / LV plane region 310. However, unless the right-side plane region 300 is the HV plane region, the vertical height of the M / LV plane region 310 will be less than that of the HV plane region 210 and greater than or equal to the vertical height of the fin region 100.

[0047] Furthermore, the HV plane region 200 shown in Figure 1A includes an isolation ring 220 (near the fin region), which is manufactured or modified to include a boundary buffer 230, while the M / LV plane region 300 includes an isolation ring 320, which is manufactured or modified to include a boundary buffer 330. The example structure shown in Figure 1A is a general structure for a display driver IC for mixed LV, MV, and HV devices. The SRAM of the display driver IC (DDIC) is part of the fin field-effect transistor region 100 with isolation rings 220 and 320, while the LV, MV, and HV devices are adjacent to the isolation rings 220 and 320 of the SRAM. Other LV functions associated with the M / LV region 300 may include, but are not limited to, a timing controller (TCON). The SRAM or fin region 100, composed of fin field-effect transistor bit cells, needs to be surrounded by isolation rings (plane regions) 220 and 330 to block MV or HV voltages near the fin region 100 or the SRAM region.

[0048] Referring to Figures 1B and 1A, according to an embodiment of the present disclosure, a detailed cross-sectional view of the boundary buffer zone of the left planar region of the IC structure (Embodiment 1) shown in Figure 1A is presented.

[0049] According to one embodiment, Table 1 below provides various size labels and example size ranges for reference in the figures. [Table 1] Description of size label values Size label The height H1 from the HV plane area to the boundary buffer recess / intermediate step The height H1 is approximately 25 to 35 nanometers. The height H2 from the HV boundary buffer zone (intermediate step) to the fin area (substrate) The height H2 is approximately 35 to 45 nanometers. The height H3 from the HV boundary buffer zone (middle step) to the fin area (top) Height H3 is less than 60 nanometers Height H4 from fin tip to fin substrate (STI) The height H4 is approximately 35 nanometers to 45 nanometers. The length L1 of the HV boundary buffer The length L1 is approximately 2.5 micrometers to 5.5 micrometers. The slope S1 from the HV planar region to the LV fin substrate The slope S1 is less than 1:80 The height H5 from the HV plane region to the fin tip Height H5 less than 60 nanometers The height H6 from the HV planar region to the LV fin substrate The height H6 is equal to or less than approximately 70 nanometers, or Height H6 is the sum of heights H4 and H5, which is equal to or less than approximately 70 nanometers. The height H7 from the ML / LV plane area to the boundary buffer recess (intermediate step) The height H7 is approximately 0 to 35 nanometers. The height H8 from the ML / LV boundary buffer zone (intermediate step) to the fin area (substrate) The height H8 is approximately 35 to 45 nanometers. The height H9 from the ML / LV boundary buffer zone (middle step) to the fin area (top) Height H9 is less than 60 nanometers The slope S2 from the ML / LV planar region to the LV fin substrate The slope S2 is less than 1:80 The length L2 of the M / LV boundary buffer The length L2 is approximately 2.5 micrometers to 5.5 micrometers. The height H10 from the M / LV plane area to the fin tip Height H10 less than 60 nanometers The height H11 from the M / LV planar region to the LV fin substrate Height H11 is less than 70 nanometers; or The height H11 is the sum of heights H4 and H10, which is less than 70 nanometers.

[0050] According to an illustrative example, if the height H5 from the HV plane region to the fin tip is X nanometers, by implementing the disclosed boundary buffer 230, the height H6 from the HV plane region to the LV fin substrate is less than or equal to X+10 nanometers. If the boundary buffer length L1 is Y nanometers, X+10 / Y (e.g., the slope S1) is less than or equal to 1 / 80.

[0051] Referring to FIG1C, a detailed cross-sectional view of the boundary buffer 330 of the right planar region of the integrated circuit IC structure (Embodiment 1) shown in FIG1A is included, depicting the slope of the boundary buffer relative to the height of the M / LV planar region 310 and the LV fin field-effect transistor region 100 (Embodiment 1) according to an embodiment of the present disclosure.

[0052] As previously described, the function of the HV boundary buffer 230 and the M / LV boundary buffer 330 is to reduce or lower the slope of the boundary from the planar region to the fin region. The required length of the boundary buffer depends on the heights H2 and H8. If the length of the boundary buffer is too short, the transition height or slope from the fin substrate 118 to the top surface of the boundary buffer plane may be too steep to accommodate certain subsequent processes, such as planarization, within the required process window. The slope is defined as the height H6 from the LV fin substrate 118 (STI) to the top surface of the HV planar region 210, and the height H11 from the LV fin substrate (STI) to the top surface of the M / LV planar region 310, as shown in Figures 1B and 1C, divided by the lengths L1 and L2 of the boundary buffer, respectively. According to an example IC embodiment, it is desired that the boundary buffer lengths (L1, L2) produce a boundary buffer slope (S1, S2) < 1:80.

[0053] Referring to FIG2A, a top view of a portion of a wafer die is shown, including an IC structure 3, which includes a planar region of a wafer / IC / device area adjacent to a sealing ring 400 surrounding the wafer 3. The sealing ring 400 includes external dummy sealing ring structures 430A and 430B, a fin-type intermediate sealing ring wall 420, and an internal sealing ring buffer 410, i.e., a sealing ring reinforcement region (SREN). The internal sealing ring buffer 410 includes a boundary buffer according to an embodiment (Embodiment 2) of this disclosure, which reduces the step height from the sealing ring wall fin 423 (see FIG2B and 2C) to the planar region of the wafer adjacent to the internal sealing ring boundary buffer. FIG2B shows a detailed top view of the wafer die portion including the integrated circuit (IC) structure as shown in FIG2A, showing details of the external dummy sealing ring structures 430A and 430B, the fin structure of the intermediate sealing ring wall 420, and the structure of the internal sealing ring buffer 410. Figure 2C shows a cross-sectional view of the sealing ring buffer zone 410 adjacent to the fin structure of the sealing ring wall 420 and the planar region of the wafer 3, as shown in Figures 2A and 2B.

[0054] Example 2: The IC structure includes a sealing ring 400 surrounding an IC wafer 3, such as one or both of the previously described Examples 1 1001 and 2 2001, but not limited to these examples. The sealing ring 400 has an inner sealing ring boundary buffer zone 410, including a planar layer 411 and a dummy polysilicon gate 414; an intermediate sealing ring wall (fin structure) 420; and outer dummy sealing rings 430A and 430B. The intermediate sealing ring wall 420 has a plurality of fins 423 formed using a sacrificial element 422 and a dummy polysilicon gate 424, and the outer dummy rings have a plurality of fins 433 formed using a sacrificial element 432 and a dummy polysilicon gate 434. The outer dummy sealing rings 430A and 430B include a metal layer (active layer) 435 formed therein, and the intermediate sealing ring wall 420 includes a metal layer (active layer) 435 formed therein.

[0055] Unlike the boundary buffer integration shown in Figures 1A-1C, the integration of the sealing ring boundary buffer aims to form an intermediate step or transition from the sealing ring fin substrate region 426 to the planar region or surface on the wafer 3 surrounded by the sealing ring 400. The sealing ring intermediate step provides a reduction in the gradient (i.e., slope) from the sealing ring fin substrate region 426 to the adjacent planar surface 3 of the wafer, which can be a high-voltage (HV) planar region, a medium-voltage (MV) planar region, a low-voltage (LV) planar region, and / or a planar region as part of a high-voltage / medium-voltage / low-voltage isolation structure.

[0056] According to exemplary embodiment 2001, embodiment 2001 includes a boundary buffer implemented by modifying an existing sealing ring to have a planar groove, thereby reducing the step height of the surface from the sealing ring to the planar region of the adjacent wafer. The sealing ring structure 400 is modified from being entirely a fin region to include an internal sealing ring buffer 410 comprising a fin + plane (SREZ), which reduces or shortens the boundary step height from the sealing ring to the adjacent wafer. The SREZ is a reserved space between the wafer 3 and the sealing ring wall 420 to prevent dicing stress from damaging the wafer.

[0057] According to an exemplary embodiment, the lengths of the dummy sealing ring structures 430A and 430B are approximately 3.6 to 7.2 micrometers, also referred to as "dicing line dummy strips". More specifically, according to an exemplary embodiment, the lengths of the dummy sealing ring structures 430A and 430B are approximately 7.2 micrometers. In practice, the lengths of the dummy sealing ring structures 430A and 430B depend on the dicing capability. In wafer region 2, according to an exemplary embodiment, the sacrificial width / pitch is approximately 48 nm / 48 nm, however, the sealing ring width / pitch is designed to be approximately 140 nm / 140 nm. The sacrificial used to form the sealing ring fin pattern can also be used during the formation of other fins of the IC, such as fin region transistor fins.

[0058] According to exemplary embodiments, the length of the sealing ring wall is approximately 2.7 micrometers to 5.4 micrometers, depending on the resistance of the sealing ring wall and its resistance to stress and moisture. More specifically, according to some embodiments, the length of the sealing ring wall 420 is approximately 5.4 micrometers.

[0059] The boundary buffer or internal sealing ring buffer 410 (internal sealing ring) has a planar region width of approximately 2.7 micrometers to 6 micrometers. More specifically, according to some embodiments, the boundary buffer width is approximately 2.46 micrometers. According to exemplary embodiments, the sealing ring 400 and the adjacent planar wafer region use the same manufacturing process as wafer 3, which is manufactured / processed concurrently with the sealing ring. Examples of sealing ring materials include, but are not limited to, silicon, oxides, metals, passivation materials, etc.

[0060] Based on exemplary embodiments, Table 2 below provides various size labels and exemplary size ranges. [Table 2] Description of size label values Size label Height H12 of the groove / intermediate step between the sealing ring wall fins / internal sealing fin section STI and the boundary buffer zone (planar STI). The height H12 is approximately 35 to 45 nanometers. The height H13 of the step from the sealing ring boundary buffer zone (plane intermediate step) to the plane area of ​​the device area Height H13 is less than 60 nanometers Height H14 from the fin top of the sealing ring wall to the fin substrate / STI The height H14 is approximately 35 to 45 nanometers. Width W1 of the sealing ring boundary buffer zone The width W1 is approximately 2.7 micrometers to 6 micrometers. The slope S3 of the intermediate sealing ring wall finned substrate to the planar region of the wafer. The slope S3 is less than 1:80 The width W2 of the external dummy sealing ring The width W2 ranges from approximately 3.6 micrometers to approximately 7.2 micrometers. Width W3 of the intermediate sealing ring wall The width W3 is approximately 2.7 to approximately 5.4 micrometers. Width of the inner sealing ring W4 Width W4 ranges from approximately 2.7 micrometers to approximately 6 micrometers.

[0061] Referring to FIG3, a cross-sectional view of an IC structure (Example 3) 3001 is shown, including a finFET region 3100 and an interconnect high voltage left-side planar region 3200, including a planar region to fin region boundary buffer (isolation (ring)) 3220 according to an exemplary embodiment of the present disclosure.

[0062] As shown in the figure, an exemplary embodiment is an IC that includes the following: Semiconductor substrate 3002 has an HV planar region 3211, a low-voltage fin region 3100, and an isolation (ring) structure 3220 (i.e., an isolation ring is formed therein). STI regions 3215A, 3215B, 3215C, and 3215D are further formed in semiconductor substrate 3002. Fin region 3100 has a first finFET transistor structure 3111A, a second finFET transistor structure 3111B, and a third finFET transistor structure 3111C. STI regions 3115A, 3115B, and 3115C are formed adjacent to each finFET transistor fin 3112A, 3112B, and 3112C. A polysilicon gate (not shown) is formed on each fin; and... The HV plane region 3200 has an HV region 3210, on which high-voltage STIs 3215A, 3215B, 3215C, and 3215D are formed, and on which high-voltage MOS transistor devices 3211 and high-voltage MOS gate / GOX (gate oxide) devices 3218 are formed. High-temperature dielectric (HTO) regions 3501A, 3501B, 3501C, and 3501D are also formed in the HV plane region to provide isolation for the various semiconductor regions depicted for operation of the HV plane region.

[0063] ILD0 layers / areas 3502A, 3502B, 3502C, 3502D and 3502F are formed on the high-pressure and low-pressure devices shown for planarization processes.

[0064] Similar to the boundary buffer previously described with reference to FIG1A-C, the IC includes a boundary buffer 3230 having a height H2 of about 35 nanometers to about 45 nanometers and a slope S1 of less than 1:80.

[0065] Unlike the boundary buffer integration shown in Figures 1A-1C, the boundary buffer 3230 integration in Embodiment 3 is designed to form an intermediate step or transition from the HV plane region 3210 to the LV fin substrate region 3118, wherein the IC structure includes an isolation ring 3220 or a structure formed by the mesa of STI 3215B, 3215C and 3215D, and has mesa tops 3216A, 3216B and 3216C respectively, the height of which is lower than the LV fin top.

[0066] Referring to Figure 4, which illustrates a semiconductor wafer layout 4002, the IC layout arrangement according to an exemplary embodiment (Embodiment 4) 4002 disclosed herein includes the previously described HV plane region 200 and M / LV plane region 300. As shown, Embodiment 4 4001 further includes high-density devices 4003A, 4003B, 4003C, 4003D, 4003E, 4003F, and 4003G; medium-voltage devices 4004A, 4004B, and 4004C; and low-voltage devices 4005A, 4005B, and 4005C. A dummy high-voltage isolation ring 4006 surrounds each low-voltage and medium-voltage device to isolate the operation of the low-density and medium-density devices from that of the high-density devices, and a high-voltage isolation ring 4007 is formed to cover areas in the wafer 4002 not used by the low-voltage, medium-voltage, and high-voltage devices. A sealing ring 4008 prevents dicing stress from damaging the wafer 4002.

[0067] According to an exemplary embodiment, and to further aid in understanding the boundary buffer structure disclosed herein, a boundary buffer 230 (not shown) is integrated into the HV plane region 200 of the high-voltage device 4003A. The boundary buffer 230 (not shown) reduces and / or provides an intermediate step from the plane region of the high-voltage device 4003A to the finned substrate region of the low-voltage device 4005A, as previously described with reference to FIG1A-1C and / or FIG3. Furthermore, a boundary buffer 330 (not shown) is integrated into the M / LV plane region 300 of the intermediate-voltage device 4004A. The boundary buffer 330 (not shown) reduces and / or provides an intermediate step from the plane region of the intermediate-voltage device 4004A to the finned substrate region of the low-voltage device 4005A, as previously described with reference to FIG1A-1C and / or FIG3. Furthermore, the sealing ring 4008 may include a sealing ring structure comprising an inner sealing ring having a boundary buffer 410 (not shown), as previously described with reference to FIG2A-2C, the sealing ring boundary buffer providing an intermediate step from the sealing ring 4008 to the planar surface of the wafer 4002 / isolation ring 4007 and / or dummy isolation ring 4006, as previously described.

[0068] Referring to FIG5, the various stages of forming an IC including a finFET region, an interconnect high voltage left plane region (including a buffer zone from the left plane region to the fin region boundary), and an interconnect M / LV right plane region (including a buffer zone from the right plane region boundary) according to an exemplary embodiment of the present disclosure are described.

[0069] In step 501, the method forms a fin region in a device region of a semiconductor substrate, comprising one or more fin field-effect transistors (finFETs), each device region finFET comprising one or more fins, forming a first height of the finFET substrate region such that the fin tops are adjacent to the fins, and forming a gate to cover the one or more fin tops.

[0070] In step 502, the method is formed in the device region of the semiconductor substrate. (1) A high-voltage (HV) planar region adjacent to the fin region, the HV planar region comprising a first HV planar region having one or more planar transistor device structures forming a second height at a distance from the finFET substrate region, the second height being greater than the first height, and a second HV planar region having a high-voltage isolation structure isolating the first HV planar region from the fin region, the high-voltage isolation structure including a boundary buffer with an intermediate step, the intermediate step being a third height at a distance from the finFET substrate region, the third height being equal to or greater than the first height and less than the second height; and (2) (Selective) Medium / Low Voltage (M / LV) Planar Regions Adjacent to and Separated from the HV Plane, the M / LV Planar Regions comprising a first M / LV Planar Region having one or more planar transistor device structures forming a second height at a distance from the finFET substrate region, the second height being greater than the first height, and a second M / LV Planar Region having an M / LV isolation structure that isolates the first M / LV Planar Region from the fin region, the M / LV isolation structure including a boundary buffer having an intermediate step at a third height at a distance from the finFET substrate region, the third height being equal to or greater than the first height and less than the second height.

[0071] Some processes that can be used to form the IC disclosed herein include chemical mechanical polishing (CMP), wet etching, and photolithography to confine the CMP / chemical etched areas. According to some exemplary embodiments, the boundary buffer intermediate step is formed by removing material from the existing isolation ring region surrounding the IC logic low-voltage fin region, or in the case of Embodiment 3, the boundary buffer is integrated with a sealing ring by removing material from the sealing ring inside the sealing ring release zone (SREZ) to form a planar intermediate step between the sealing ring and the adjacent IC wafer planar region.

[0072] In Example 1, where the IC includes an HV planar region and an M / LV planar region, a mid-pressure process mask is used to define the intermediate step / groove region of the boundary buffer in the isolation ring, and the mid-pressure process mask is also used to define the seal ring release zone (SREZ) of the seal ring using a photolithography process. Then, a groove / step formation process is performed using a dry chemical etching process. (Fin groove formation is performed after the planar formation process.) The result is a step height to the fin substrate region similar to the boundary buffer of the mid-pressure planar region, but with high-pressure wells in these regions for isolation purposes.

[0073] Referring to Figures 6A-6E, the various stages of forming an IC (Example 5) 5001, comprising a fin field-effect transistor (finFET) region, an HV left plane region of interconnects (including a boundary buffer of the left plane region), and an M / LV right plane region of interconnects (including a boundary buffer of the right plane region), according to an exemplary embodiment of the present disclosure are described.

[0074] Figure 6A illustrates the initial stage 601 of forming a boundary buffer as previously described with reference to Figures 1A-1C, wherein the IC structure state formed in the initial portion is previously formed using the previously described semiconductor manufacturing photolithography process. The fin region 100, HV plane region 210, and selective M / LV plane region 310, as well as isolation rings 220 and 320, and boundary buffers 230 and 330 are essentially functional equivalents of the same reference characters previously described with reference to Figures 1A-1C, and will not be repeated here.

[0075] As shown in the figure, in the initial stage 601 of the process, the semiconductor IC structure is previously formed to include a recess height R1, which is the initial recess height of the high-voltage gate oxide (HVGOX) gate 216B to the high-voltage STI 215E of the HV plane region 210 before the formation of the boundary buffer 230, for example, about 100 nanometers. Furthermore, the semiconductor IC structure is previously formed to include a recess height R2, which is the initial recess height of the isolation ring plane region 220 relative to the high-voltage STI 215I before the formation of the boundary buffer 230, for example, 100 nanometers.

[0076] The process or manufacturing steps described below focus on forming the planar HV boundary buffer 230 (see Figure 6E). However, it should be understood that a similar process is performed concurrently with the HV boundary buffer manufacturing to form the M / LV boundary buffer 330 (see Figure 6E).

[0077] Figure 6B illustrates stage 602 of the boundary buffer fabrication process, which includes forming an MVGOX (medium-voltage gate oxide) layer 716 on the structure of Figure 6A, thereby covering the entire surface of the HV plane region 210, the isolation ring structure 220, the fin region 100, the isolation ring structure 320, and the M / LV plane region 310. A further etching process is performed to etch the MVGOX layer 716, forming a groove height R3, which is the groove height from the high-voltage gate oxide (HVGOX) gate 216B to the high-voltage STI 215E in the HV plane region 210 after etching, for example, approximately 300 nanometers.

[0078] Figure 6C illustrates the next stage 603, which includes applying a hard mask 717 to the MVGOX layer 716 and performing an etching process to remove a portion of the STI material 115 and form a groove for the fin 116. This also provides a groove height R4, for example, 400 nanometers, from the top surface 231 of the high-voltage isolation ring planar region 210 / boundary buffer.

[0079] Figure 6D illustrates the next stage 604, which includes applying a polycrystalline silicon layer 718 across the entire surface of the structure shown in Figure 6C and performing a CMP process to planarize the surface. For reference, regions 718A, 718B, and 718C outline the polycrystalline silicon gates 718A, 718B, and 718C subsequently formed in the next stage shown in Figure 6E.

[0080] Figure 6E illustrates the next stage 605, which includes performing a lithography process to etch the CMP planarized surface of the polysilicon layer 718 and form polysilicon gates 718A, 718B, and 718C. The resulting semiconductor IC structure 5001 shown includes completed boundary buffers 230 and 330, which are formed and integrated into isolation rings 220 and 320, respectively.

[0081] Based on the foregoing discussion, it is clear that this disclosure provides advantages. However, it should be understood that other embodiments may offer additional advantages, and not all advantages need to be disclosed herein, nor are specific advantages required for all embodiments. One advantage is that the disclosed integrated circuit boundary buffer provides a reduced step height from the fin region to the adjacent planar region, which in turn may improve the process window associated with one or more subsequent semiconductor manufacturing processes.

[0082] Some further embodiments are described below.

[0083] In a non-limiting illustrative embodiment, a method of manufacturing an integrated circuit includes: forming a fin region comprising one or more fin field-effect transistors (finFETs) in a device region of a semiconductor substrate, each of the device regions having one or more fins and a gate, the fins being formed having fin-shaped tops at a first height relative to a fin field-effect transistor substrate region, the fin field-effect transistor substrate region being adjacent to the fin-shaped tops, and the gate being formed to cover one or more of the fin-shaped tops; and forming a high-voltage (HV) plane region adjacent to the fin regions in the device region of the semiconductor substrate, the HV plane region... The surface region includes a first HV plane region and a second HV plane region. The first HV plane region has one or more planar transistor device structures. The planar transistor device structures are formed at a second height from the fin field-effect transistor substrate region. The second height is greater than the first height. The second HV plane region has an HV isolation structure that isolates the first HV plane region from the fin region. The HV isolation structure includes a boundary buffer. The boundary buffer has an intermediate step at a third height from the fin field-effect transistor substrate region. The third height is equal to or greater than the first height and less than the second height.

[0084]

[0085] In another non-limiting illustrative embodiment, an integrated circuit includes: a semiconductor substrate; and a device region including one or more fin field-effect transistors (finFETs), each of the device regions having one or more fins and a gate, the fins being formed with fin-shaped tops at a first height from the fin field-effect transistor substrate region adjacent to the fin-shaped tops, the gates being formed to cover one or more of the one or more fin-shaped tops, wherein the device region includes a high-voltage (HV) plane region adjacent to the fin region, the HV plane region including a first HV plane region and a second HV plane region, the first HV plane region having one or more planar transistor device structures formed at a second height from the fin field-effect transistor substrate region, the second height being greater than the first height, the second HV plane region having an isolation structure that isolates the first HV plane region from the fin region, the isolation structure including a boundary buffer having an intermediate step at a third height from the fin field-effect transistor substrate region, the third height being equal to or greater than the first height and less than the second height.

[0086]

[0087] In another non-limiting illustrative embodiment, a method of manufacturing an integrated circuit includes: forming a fin region comprising one or more fin field-effect transistors (finFETs) and a planar region adjacent to the fin region in a device region of a semiconductor substrate, each fin FET in the device region comprising one or more fins and a gate formed to cover one or more tops of the one or more fins, the planar region comprising one or more planar semiconductor device structures; and forming a sealing ring region surrounding the device region, the sealing ring region comprising an inner sealing ring surrounding the device region and an outer sealing ring surrounding the inner sealing ring and the device region, the outer sealing ring comprising a plurality of fins, each fin having a fin top at a first height from a fin substrate region adjacent to the fin, and the inner sealing ring comprising a planar boundary buffer adjacent to the planar region of the device region, the planar boundary buffer being formed at a second height from the fin substrate region, the second height being less than the first height.

[0088]

[0089] The foregoing outlines features of several embodiments to enable those skilled in the art to better understand the various aspects of this disclosure. Those skilled in the art should understand that they can readily use this disclosure as a basis for designing or modifying other processes and structures to achieve the same purposes and / or advantages as the various embodiments described herein. Those skilled in the art should also recognize that such equivalent constructions do not depart from the spirit and scope of this disclosure, and that various changes, substitutions, and modifications can be made herein without departing from the spirit and scope of this disclosure.

[0090] 2: Base 3: Structure / Chip 100, 200, 300, 210, 310, 3100, 3210, 3211, 3118, 3501A, 3501B, 3501C, 3501D, 3502A, 3502B, 3502C, 3502D, 3502F: Zone 111A, 111B, 111C, 111D, 211A, 211B, 311A, 311B, 311C, 3111A, 3111B, 3111C: Transistor Structure 112, 113, 212A, 212B, 213A, 213B, 213C, 214A, 214B, 214C, 312A, 313A, 313B, 314A, 314B: Well 115: STI Materials / Area 116, 116A1, 116A2, 116B1, 116B2, 423, 433, 3112A, 3112B, 3112C: Fins 117A, 117B, 117C, 117D: Polycrystalline silicon gate 118: Fin-shaped substrate area 119: Fin-shaped top 215A, 215B, 215C, 215D, 215E, 215F, 215G, 215H, 215I, 215J, 215K, 315A, 315B, 315C, 315D, 315 E, 315F, 315G, 315H, 315I, 315J, 315K, 315L, 315L, 315M, 315N, 3215A, 3215B, 3215C, 3215D: STI 216A, 216B, 316A, 316B, 316C: Gate 217, 414, 424, 434: Dummy polycrystalline silicon gates 220, 320, 3220: Isolation rings 230, 330, 410, 3230: Buffer zones 231, 331: Top surface 400, 4008: Sealing rings 411: Planar layer 420: Sealing ring wall 422, 432: Sacrifices 425: Metal layer / Active layer 426: Sealing ring fin-shaped substrate area 430A, 430B: Fictitious sealing ring structure 501, 502: Steps 601, 602, 603, 604, 605: Stages 716: Floor 717: Rigid Screen Cover 718: Polycrystalline silicon layer 718A, 718B, 718C: Zone / Gate 1001: Example 1 / Structure 2001: Example 2 3001: Example 3 3002: Semiconductor substrate 3115A, 3115B, 3115C: STI zone 3200: Planar area 3216A, 3216B, 3216C: Top 3218: High-voltage MOSFET gate / GOX (gate oxide) 4001: Example 4 4002: Chip 4003A, 4003B, 4003C, 4003D, 4003E, 4003F, 4003G, 4004A, 4004B, 4004C, 4005A, 4005B, 4005C: Device 4006, 4007: Isolation ring 5001: Semiconductor IC Structure H1, H2, H3, H4, H5, H6, H7, H8, H9, H10, H11, H12, H13, H14, R1, R2, R3, R4: Height L1, L2: Length S1, S2, S3: Slope W1, W2, W3, W4: Width x, y, z directions

Claims

1. A method for manufacturing an integrated circuit, comprising: In a device region of a semiconductor substrate, a fin region comprising one or more fin field-effect transistors (finFETs) is formed. Each fin in the device region includes one or more fins and a gate. The fins are formed with fin-shaped tops at a first height relative to the fin field-effect transistor substrate region. The fin field-effect transistor substrate region is adjacent to the fin-shaped tops. The gate is formed to cover one or more of the fin-shaped tops. In the device region of the semiconductor substrate, a high-voltage (HV) plane region adjacent to the fin regions is formed. The HV plane region includes a first HV plane region and a second HV plane region. The first HV plane region has one or more planar transistor device structures formed at a second height from the fin field-effect transistor substrate region, the second height being greater than the first height. The second HV plane region has an HV isolation structure that isolates the first HV plane region from the fin region. The HV isolation structure includes a boundary buffer, the boundary buffer having an intermediate step at a third height from the fin field-effect transistor substrate region, the third height being equal to or greater than the first height and less than the second height. The boundary buffer has a slope defined as the second height divided by the length of the boundary buffer, and the slope is less than or equal to 1:

80.

2. The method as described in claim 1, wherein the first height is substantially equal to the third height.

3. The method of claim 2, wherein the boundary buffer is formed by a method comprising the steps of: performing a lithography process to etch at least a portion of the isolation structure to form a groove at the third height, the groove defining the intermediate step of the boundary buffer.

4. The method as described in claim 1, further comprising: In the device region of the semiconductor substrate, a medium / low voltage (M / LV) planar region is formed adjacent to the fin region and separated from the HV plane. The M / LV planar region includes a first M / LV planar region and a second M / LV planar region. The first M / LV planar region has one or more planar transistor device structures formed at a second height from the fin field-effect transistor substrate region, the second height being greater than the first height. The second M / LV planar region has an M / LV isolation structure that isolates the first M / LV planar region from the fin region. The M / LV isolation structure includes a boundary buffer with an intermediate step at a third height from the fin field-effect transistor substrate region, the third height being equal to or greater than the first height and less than the second height.

5. An integrated circuit, comprising: Semiconductor substrate; The device region includes one or more fin field-effect transistors (finFETs). Each finFET in the device region includes one or more fins and a gate. The fins are formed with fin-shaped tops at a first height from the finFET substrate region, adjacent to the fin-shaped tops. The gate is formed to cover one or more of the fin-shaped tops. The device region includes a high-voltage (HV) plane region adjacent to the fin region. The HV plane region includes a first HV plane region and a second HV plane region. The first HV plane region has one or more planar transistor device structures formed at a second height from the finFET substrate region, the second height being greater than the first height. The second HV plane region has an isolation structure that isolates the first HV plane region from the fin region. The isolation structure includes a boundary buffer with an intermediate step at a third height from the finFET substrate region, the third height being equal to or greater than the first height and less than the second height. The boundary buffer has a slope defined as the second height divided by the length of the boundary buffer, and the slope is less than or equal to 1:

80.

6. The integrated circuit as described in claim 5, further comprising: The device region includes a medium / low voltage (M / LV) planar region adjacent to the fin region and separated from the HV plane. The M / LV planar region includes a first M / LV planar region and a second M / LV planar region. The first M / LV planar region has one or more planar transistor device structures formed at a second height from the fin field-effect transistor substrate region. The second height is greater than the first height. The second M / LV planar region has an M / LV isolation structure that isolates the first M / LV planar region from the fin region. The M / LV isolation structure includes a boundary buffer. The boundary buffer has an intermediate step at a third height from the fin field-effect transistor substrate region. The third height is equal to or greater than the first height and less than the second height.

7. A method for manufacturing an integrated circuit, comprising: A fin region comprising one or more fin field-effect transistors (finFETs) and a planar region adjacent to the fin region is formed in a device region of a semiconductor substrate. Each fin field-effect transistor in the device region includes one or more fins and a gate formed to cover one or more tops of the one or more fins. The planar region includes one or more planar semiconductor device structures. A sealing ring region is formed surrounding the device region. The sealing ring region includes an inner sealing ring surrounding the device region and an outer sealing ring surrounding the inner sealing ring and the device region. The outer sealing ring includes a plurality of the fins, each fin having a fin top at a first height from a fin substrate region adjacent to the fin. The inner sealing ring includes a planar boundary buffer adjacent to the planar region of the device region, the planar boundary buffer being formed at a second height from the fin substrate region, the second height being not less than the first height. The slope from the fin substrate region to the planar region of the fins of the outer sealing ring is less than 1:

80.

8. The method of claim 7, wherein the planar region of the device region is adjacent to the inner sealing ring, and the planar region of the device region is at a third height from the finned substrate region of the outer sealing ring, and the third height is greater than the second height, wherein the planar boundary buffer thereby provides an intermediate step from the inner sealing ring to the planar region of the device region.

Citation Information

Patent Citations

  • Semiconductor device and methods of formation