Liner composite material and method for preparing the same

TWI946253BActive Publication Date: 2026-11-11METAL INDS RES & DEV CENT
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
TW114151468
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-12-26
Publication Date
2026-11-11
Estimated Expiration
2045-12-25

Smart Images

  • Figure TWG2TB001921005_001
    Figure TWG2TB001921005_001
  • Figure TWG2TB001921005_002
    Figure TWG2TB001921005_002
  • Figure TWG2TB001921005_003
    Figure TWG2TB001921005_003
Patent Text Reader

Abstract

A method for preparing an inner lining composite material includes (a) subjecting a raw material component comprising an organosilane, water, alkali, and a first solvent to a hydrolysis-condensation reaction to obtain a polyhedral oligomeric silsesquioxane, which is then used as a nanofiller component; and (b) subjecting the nanofiller component to a melt-blending process with high-density polyethylene to obtain an inner lining composite material with a hydrogen permeability coefficient not greater than 4.13 × 10⁻¹⁷ mol·m / (m²·s·Pa), wherein the amount of the nanofiller component is 10 wt% to 30 wt% based on a total amount of 100 wt% of the nanofiller component and high-density polyethylene. The present invention also provides an inner lining composite material prepared by the above method. By using a polyhedral oligomeric silsesquioxane as a nanofiller component and mixing it with high-density polyethylene to prepare an inner lining composite material, the inner lining formed by the inner lining composite material exhibits good hydrogen barrier properties.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A method for preparing an inner lining composite material, comprising the following steps: (a) subjecting a raw material component comprising an organosilane, water, an alkali, and a first solvent to a hydrolysis-condensation reaction to obtain a polyhedral oligomeric silsesquioxane, and using the polyhedral oligomeric silsesquioxane as a nanofiller component; and (b) subjecting the nanofiller component to a melt-blending treatment with high-density polyethylene to obtain an inner lining composite material having a hydrogen permeability coefficient, wherein the hydrogen permeability coefficient is not greater than 4.13 × 10⁻¹⁷ mol·m / (m²·s·Pa); wherein, In step (a), the organosilane is selected from at least one of phenyltrimethoxysilane, vinyltriethoxysilane, isobutyltrimethoxysilane, 3-(methacryloxy)propyltrimethoxysilane, isobutyltriethoxysilane, 3-(methacryloxy)propyltriethoxysilane, isopropyltrimethoxysilane, octadecyltrimethoxysilane, and n-decyltrimethoxysilane, wherein the polyhedral oligomeric silsesquioxane is a T8-polyhedral oligomeric silsesquioxane, and the number-average molecular weight of the T8-polyhedral oligomeric silsesquioxane ranges from 1000 g / mol to 3000 g / mol. In step (b), the amount of the nanofiller component ranges from 10 wt% to 20.4 wt%, with the total amount of the nanofiller component and the high-density polyethylene being 100 wt%.

2. The method for preparing the lining composite material as described in claim 1 further comprises a step (c), wherein the polyhedral oligomeric silsesquioxane and hexagonal boron nitride are subjected to a surface pretreatment to allow the polyhedral oligomeric silsesquioxane and the hexagonal boron nitride to form surface bonds and coat the hexagonal boron nitride, thereby obtaining a composite nanofiller, and the composite nanofiller is used as a component of the nanofiller, wherein, Based on the amount of hexagonal boron nitride being 100 wt%, the amount of polyhedral oligomeric silsesquioxane ranges from 3 wt% to 5 wt%.

3. The method for preparing the lining composite material as described in claim 2, wherein, In step (c), the surface pretreatment is carried out by chemically reacting the polyhedral oligomeric silsesquioxane, the hexagonal boron nitride and the second solvent to obtain a mixture, and then sequentially filtering, drying and sintering the mixture to obtain the composite nanofiller.

4. The method for preparing the lining composite material as claimed in claim 2 further comprises a step (d) of mixing the composite nanofiller with polydimethylsiloxane to disperse the composite nanofiller in the polydimethylsiloxane to obtain a colloidal solution, and using the colloidal solution as the nanofiller component.

5. The method for preparing the lining composite material as claimed in claim 1 further comprises a step (e) of mixing the polyhedral oligomeric silsesquioxane with polydimethylsiloxane to disperse the polyhedral oligomeric silsesquioxane in the polydimethylsiloxane to obtain a colloidal solution, and using the colloidal solution as the nanofiller component.

6. A lining composite material, prepared by any one of claims 1 to 5, wherein the hydrogen permeability coefficient of the lining composite material is not greater than 4.13 × 10⁻¹⁷ mol·m / (m²·s·Pa).

7. The lining composite material as described in claim 6, wherein, The pyrolysis temperature of the lining composite material is 400°C to 450°C.

8. The lining composite material as described in claim 6, wherein, The tensile stress of the lining composite material is 10.4 MPa to 13 MPa, and the tensile strain is 96.8% to 98%.

Citation Information

Patent Citations

  • Polymer nanocomposite

    CN103068927A

  • High-strength alloy composite material and preparation method thereof

    CN115678164A

  • Composite resin and preparation method thereof

    CN118580641A