Regeneration membrance and method for producing the same

TWI946256BActive Publication Date: 2026-11-11NANYA PLASTICS CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW114151825
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-12-30
Publication Date
2026-11-11
Estimated Expiration
2045-12-29

Smart Images

  • Figure TWG2TB001921008_001
    Figure TWG2TB001921008_001
  • Figure TWG2TB001921008_002
    Figure TWG2TB001921008_002
  • Figure TWG2TB001921008_003
    Figure TWG2TB001921008_003
Patent Text Reader

Abstract

This invention discloses a regenerated membrane and a method for manufacturing the same. The regenerated membrane comprises a substrate and a modifying material. The modifying material is formed on the substrate by forming a modifying solution on the substrate and then drying the modifying solution. The modifying solution comprises a modifying agent and a solvent, and the modifying agent is at least one selected from the group consisting of collagen, carboxymethyl cellulose, and hyaluronic acid. Based on a total weight of 100 wt% for the regenerated membrane, the content of the modifying material is between 5 wt% and 50 wt%. The number average molecular weight of the modifying agent is between 10 kDa and 1,000 kDa, and the viscosity of the modifying solution is between 3 cps and 5,000 cps.
Need to check novelty before this filing date? Find Prior Art

Claims

1. A regenerated membrane comprising: a substrate; and a modification material, wherein a modification solution is formed on the substrate and then the modification solution is dried to form the membrane on the substrate; wherein, The modification solution comprises a modifier and a solvent, wherein the modifier is selected from at least one of the materials group consisting of collagen, carboxymethyl cellulose and hyaluronic acid; wherein, based on the total weight of the regenerated membrane being 100 wt%, the content of the modifier is between 5 wt% and 50 wt%; wherein, the number average molecular weight of the modifier is between 10 kDa and 1,000 kDa, and the viscosity of the modification solution is between 3 cps and 5,000 cps.

2. The regenerated membrane as described in claim 1, wherein, The substrate comprises polylactic acid and tricalcium β-phosphate; wherein, based on a total weight of 100 wt% of the substrate, the content of polylactic acid is between 60 wt% and 80 wt%, and the content of tricalcium β-phosphate is between 20 wt% and 40 wt%.

3. The regenerated membrane as claimed in claim 1, wherein, The substrate is an electrospun film, and the substrate has a porosity of between 30% and 95% and an average pore size of between 5 micrometers and 55 micrometers.

4. The regenerated membrane as claimed in claim 1, wherein, The total weight of the regenerated membrane is 100 wt%, and the content of the modifying material is between 10 wt% and 40 wt%.

5. The regenerated membrane as claimed in claim 1, wherein, The modifier is hyaluronic acid, the number average molecular weight of which is between 300 kDa and 1,000 kDa, the viscosity of the modifying solution is between 20 cps and 2,500 cps, and the concentration of the modifying solution is between 0.1 w / v% and 5 w / v%.

6. The regenerated membrane as claimed in claim 1, wherein, The modifier is carboxymethyl cellulose, the number average molecular weight of which is between 90 kDa and 1,000 kDa, the viscosity of the modified solution is between 500 cps and 5,000 cps, and the concentration of the modified solution is between 0.1 w / v% and 5 w / v%.

7. The regenerated membrane as claimed in claim 1, wherein, The modifier is collagen, the number-average molecular weight of which is between 10 kDa and 100 kDa, the viscosity of the modification solution is between 3 cps and 80 cps, and the concentration of the modification solution is between 0.1 w / v% and 10 w / v%.

8. A method for manufacturing a recycled membrane, comprising: a pre-processing step of providing a substrate; and a forming step of forming a modification solution on the substrate and then drying the modification solution to form a modification material on the substrate and form a recycled membrane; wherein, The modification solution comprises a modifier and a solvent, wherein the modifier is selected from at least one of the materials group consisting of collagen, carboxymethyl cellulose and hyaluronic acid; wherein, based on the total weight of the regenerated membrane being 100 wt%, the content of the modifier is between 5 wt% and 50 wt%; wherein, the number average molecular weight of the modifier is between 10 kDa and 1,000 kDa, and the viscosity of the modification solution is between 3 cps and 5,000 cps.

9. A method for manufacturing a recycled membrane as described in claim 8, wherein, The substrate comprises polylactic acid and tricalcium β-phosphate; wherein, based on a total weight of 100 wt% of the substrate, the content of polylactic acid is between 60 wt% and 80 wt%, and the content of tricalcium β-phosphate is between 20 wt% and 40 wt%.

10. A method for manufacturing a recycled membrane as described in claim 8, wherein, In the aforementioned preliminary step, the substrate is formed by electrospinning, and the substrate has a porosity of between 30% and 95% and an average pore size of between 5 micrometers and 55 micrometers.

11. The method for manufacturing the regenerated membrane as described in claim 10, wherein, In the electrospinning method, the substrate is formed in an electric field with a voltage between 30 kV and 40 kV, at a spraying speed between 3,000 mm / s and 5,000 mm / s, and at a spraying spacing between 250 mm and 325 mm.

12. The method for manufacturing the regenerated membrane as described in claim 8, wherein, In the formation step, the modification solution is formed on the substrate and then rolled and dried.

13. The method for manufacturing the regenerated membrane as described in claim 8, wherein, The total weight of the regenerated membrane is 100 wt%, and the content of the modifying material is between 10 wt% and 40 wt%.

14. A method for manufacturing a recycled membrane as described in claim 8, wherein, The modifier is hyaluronic acid, the number average molecular weight of which is between 300 kDa and 1,000 kDa, the viscosity of the modifying solution is between 20 cps and 2,500 cps, and the concentration of the modifying solution is between 0.1 w / v% and 5 w / v%.

15. A method for manufacturing a recycled membrane as described in claim 8, wherein, The modifier is carboxymethyl cellulose, the number average molecular weight of which is between 90 kDa and 1,000 kDa, the viscosity of the modified solution is between 500 cps and 5,000 cps, and the concentration of the modified solution is between 0.1 w / v% and 5 w / v%.

16. A method for manufacturing a recycled membrane as described in claim 8, wherein, The modifier is collagen, the number-average molecular weight of which is between 10 kDa and 100 kDa, the viscosity of the modification solution is between 3 cps and 80 cps, and the concentration of the modification solution is between 0.1 w / v% and 10 w / v%.

Citation Information

Patent Citations

  • Guided tissue regeneration membrane and its preparation method

    CN102716517A

  • Double layer composite collagen base guide tissue regeneration film and its preparing method

    CN1319604C