Method of adjusting polymer dispersions properties for membrane casting
Patent Information
- Application Number
- PCT/US2024/019131
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-10
- Filing Date
- 2024-03-08
- Publication Date
- 2024-10-24
AI Technical Summary
High solid loading in polymer suspensions for anion exchange membrane production leads to increased viscosity, making it challenging to maintain a working range for roll-to-roll casting, which affects membrane quality and cost efficiency.
The method involves mixing a dried anion exchange polymer with solvents and additives, such as nonionic surface-active agents, to achieve a homogeneous polymer dispersion with high solid loading (at least 10 wt.%) and reduced viscosity (not more than 10,000 cp), using an agitator designed for high viscosity liquids, to facilitate low viscosity polymer dispersions for cost-effective membrane manufacturing.
This approach effectively reduces viscosity by 10-40% and improves membrane quality, enabling the use of non-precious metal catalysts and metal bipolar plates, resulting in cost reduction for anion exchange and bipolar membranes, enhancing their commercial viability.
Smart Images

Figure 000001 
Figure 000002 
Figure 000003
Abstract
Description
METHOD OF ADJUSTING POLYMER DISPERSIONS PROPERTIES FOR MEMBRANE CASTINGFIELD OF THE INVENTION
[0001] Methods of producing anion exchange membrane (AEM) with introduction of additives to the polymer suspension are provided. The additives to the anion exchange polymer suspension reduce the viscosity of the suspension of high solid loading and improve final membrane quality.BACKGROUND OF THE INVENTION
[0002] Proton exchange membrane fuel cells (PEMFCs) are considered to be clean and efficient power sources. Steele et al., Nature 2001, 414, 345. However, the high cost and unsatisfactory durability of catalysts are major barriers for large-scale commercialization of PEMFCs. Borup et al., Chem Rev 2007, 107, 3904. By switching the polymer electrolyte from an “acidic” condition to a “basic” one, anion exchange membranes fuel cells are able to work with non-precious metal catalysts and the catalysts are expected to be more durable. Other cheaper fuel cell components are also possible such as metal bipolar plates. Varcoe, et al., Fuel Cells 2005, 5, 187; Gu et al., Angew Chem Int Edit 2009, 48, 6499; Gu et al., Chem Commun 2013, 49, 131.
[0003] Producing AEMs in a roll-to-roll fashion is important in reducing the membrane cost and ensuring the membrane quality from batch to batch. One factor to ensure the AEM quality is the polymer dispersion. The viscosity and solid loading of the dispersion plays an important role in the quality of the dispersion and the final AEM product. Generally, for a given solvent, temperature and pressure, the viscosity of a polymer solution / suspension increases with the solid loading. High solid loading is usually preferred for the roll-to-roll casting if the viscosity of the polymer suspension is within a working range.
[0004] To ensure the viscosity of the polymer suspension is within a pre-set range while having the solid loading of polymer suspension as high as possible, additives are needed.SUMMARY OF THE INVENTION
[0005] A method of making an anion exchange polymer dispersion is provided. The method comprises mixing a dried anion exchange polymer, a solvent(s) and an additive(s) with an agitator designed for high viscosity liquid or gel for a time sufficient to form a homogeneous polymer dispersion having a polymer solids loading of at least 10 wt.%. The addition of an additive(s) can efficiently lower the viscosity of the polymer dispersion by about 10 to about 40%.
[0006] An anion exchange polymer dispersion having a polymer solid loading of at least 10 wt.% is provided, which is prepared by the method as described above.DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] Anion exchange membranes, one of the key components in fuel cells and electrolyzer devices, enable electrochemistry to occur in a basic environment, allowing for the use of less expensive components, such as non-precious metal catalysts and metal bipolar plates, as compared to an acidic environment. The methods of the invention provide an anion exchange polymer dispersion with high solids loading so as to decrease the amount of solvent in the dispersion to reduce the cost of membrane manufacturing. The methods allow for dispersion of the anion exchange polymer in a wide range of solvents with high solids loading while maintaining low viscosity for use of the polymer dispersions, for example, to make bipolar membranes and ionomers at a significantly reduced cost. This cost reduction for the anion exchange and bipolar membranes is important in commercializing the membranes and associated electrochemical devices.
[0008] Herein, a range of nonionic surface-active agents such as alcohols, ethers, esters, fatty alcohol alkoxylates and polyglycols, were determined to adjust the viscosity of the polymer suspension and improve the membrane quality.
[0009] A method of making an anion exchange polymer dispersion is provided. The method comprises mixing an additive and a solvent with an anion exchange polymer to achieve a suspension with polymer solid loading of at least 10 wt.%, preferably from about 15 to about 30 wt.% wherein viscosity of the suspension is not more than 10,000 cp as measured by a Brookfield DV-III Ultra rheometer with spindle # 62 at 25 °C.
[0010] The weight ratio of the additives in the polymer suspension ranges from about 2% to about 20%.
[0011] The viscosity of the polymer suspension was reduced by about 10 to about 40% using the method of the invention.
[0012] The additive comprises an alcohol, a diol, a triol, an ester, a polyglycol, a fatty alcohol alkoxylate, an ether, or any combination thereof.
[0013] The alcohol can comprise n-propanol, 2-propanol, n-butanol, n-pentanol, or any combination thereof.
[0014] The diol can comprise ethylene glycol, propane-1 , 2-diol, 1 ,4-butanediol, 1 ,5- pentanediol, 1 ,6-hexanediol, 1 ,10-decanediol, or any combination thereof.
[0015] The triol can comprise a glycerol.
[0016] The ester can comprise a sorbitan-derived ester such as sorbitan trioleate, sorbitan tristearate or sorbitan monooleate; a glycerol-derived ester such as glycerol monostearate; a polyethylene glyco-derived ester such as POE (20) sorbitan trioleate, PEG-6 octanoic / decanoic glycerides, apricot kernel oil PEG-6 complex, or POE 9 monooleate; a glycerol-derived esters such as a mono- or di-glyceride of octanoic / decanoic acids, or glycerol mono-oleate, or any combination of these esters.
[0017] An anion exchange polymer dispersion having a polymer solid loading of at least 10 wt.% and viscosity of not more than 10,000 cp can be prepared by the method of the invention.
[0018] The time sufficient to form a homogeneous polymer dispersion ranges from about 1 to about 5 hours.
[0019] The mixing speed of the agitator can range from about 200 to about 2,000 rpm to provide a low viscosity polymer dispersion.
[0020] The mixing step of the methods of the invention occurs at a temperature ranging from 10 °C to a boiling point of the solvent(s).
[0021] The homogeneous polymer dispersion of the methods of the invention has a viscosity ranging from about 1000 cp to 10,000 cp as measured by a Brookfield DV-III Ultra rheometer with spindle # 62 at 25 °C.
[0022] The agitator used in the methods is designed for use with high viscosity liquid or gel, and is commercially available as an HV-agitator from various industrial mixing equipment manufacturers.
[0023] The anion exchange polymer in the polymer dispersion can comprise structural units of Formulae 1 A, 2A, 3A, and optionally 4A, wherein the structural units have the formulae:wherein:Ri and R2 are each independently alkyl, alkenyl, alkynyl or aryl, or a quaternary ammonium or a nitrogen-containing heterocyclic group or a salt thereof, the quaternary ammonium group having the formula 5A:and the alkyl, alkenyl, alkynyl or aryl are optionally substituted with halide;R3, R4, R5, R6, R7, R8, Rg, and R10are each independently hydrogen, halide, alkyl, alkenyl, alkynyl or aryl, and the alkyl, alkenyl, alkynyl or aryl are optionally substituted with halide, and wherein R4and R7are optionally linked to form a five membered ring optionally substituted with halide or alkyl; each R11is independently alkyl, alkenyl, alkynyl, orR13, R14, R15, RW, and R17are each independently hydrogen, halide, alkyl, alkenyl, alkynyl or aryl, and the alkyl, alkenyl, alkynyl or aryl are optionally substituted with halide, and wherein R14and R17are optionally linked to form a five membered ring optionally substituted with halide or alkyl;Rwo and R240 are each independently alkylene;R190, R200, R210, R220, and R230 are each independently alkyl, alkenyl, or alkynyl; each m is independently 0, 1 , 2, 3, 4, 5 or 6; n is 0, 1 , 2 or 3;X- is an anion; andZ is N. Such anion exchange polymers are described in U.S. Patent No. 10,290,890, which is incorporated herein by reference in its entirety.
[0024] AEM produced from the polymer dispersion described above showed improved thickness uniformity and enhanced mechanical properties.
[0025] AEMs produced from the polymer dispersion described above have thickness ranges from about 10 to about 200 micrometers.EXAMPLESEXAMPLE 1
[0026] A TP-85 polymer dispersion having solid loading of 20% and viscosity of 4000 pc was prepared. 2 kg of dried TP-85 polymer in bicarbonate form (as shown below) was added to 7.6 kg of solvent and 400 g of ethyl lactate to form a mixture. The mixture was stirred at 700 rpm with a HV-agitator for 1 h to provide a homogenous dispersion having viscosity of 4000 cP at 25 °C. Without adding the ethyl lactate to the mixture the viscosity of the suspension was 5100 cP at 25 °C as measured with the same agitator and stir rate.EXAMPLE 2
[0027] A TP-100 polymer dispersion having solid loading of 20% was prepared. 2 kg of dried TP-100 polymer in bicarbonate form (as shown below) was added to 7.6 kg of solvent and 400 g of ethyl lactate to form a mixture. The mixture was stirred at 700 rpm with a HV-agitator for 1 h to provide a homogenous dispersion having viscosity of 5000 cP at 25 °C. Without adding the 400g of ethyl lactate to the mixture the viscosity of the suspension was 6300 cP at 25 °C as measured with the same agitator and stir rate.EXAMPLE 3
[0028] A BP-100 polymer dispersion having solid loading of 15% was prepared. 2 kg of dried BP-100 polymer in bicarbonate form (as shown below) was added to 10.8 kg of solvent and 500g ethyl lactate to form a mixture. The mixture was stirred at 1000 rpm with a HV-agitator for 1 h to provide a homogenous dispersion having viscosity of 2500 cP at 25 °C. Without adding ethyl lactate to the mixture the viscosity of the suspension was 3100 cP at 25 °C as measured with the same agitator and stir rate.EXAMPLE 4
[0029] A TP-85-MQN polymer dispersion having solid loading of 15% was prepared. 2 kg of dried TP-85-MQN polymer in bicarbonate form (as shown below) was added to 10.8 kg of solvent and 500g ethylene glycol in a cylindrical reactor to form a mixture.The mixture was stirred at 700 rpm with a HV-agitator for 1 h to provide a homogenous dispersion having viscosity of 2800 cP at 25 °C. Without adding ethylene glycol to the mixture the viscosity of the suspension was 4300 cP at 25 °C as measured with the same agitator and stir rate.EXAMPLE 5
[0030] A TP-100-MQN polymer dispersion having solid loading of 15% was prepared. 2 kg of dried TP-100-MQN polymer in bicarbonate form (as shown below) was added to10.8 kg of solvent and 500g ethylene glycol in a cylindrical reactor to form a mixture.The mixture was stirred at 700 rpm with a HV-agitator for 1 h to provide a homogenous dispersion having viscosity of 3300 cP at 25 °C. Without adding ethylene glycol to the mixture the viscosity of the suspension was 4800 cP at 25 °C as measured with the same agitator and stir rate.EXAMPLE 6
[0031] A TP-85-IM polymer dispersion having solid loading of 15% was prepared. 2 kg of dried TP-85-IM polymer in bicarbonate form (as shown below) was added to 10.8 kg of solvent and 500g ethylene glycol in a cylindrical reactor to form a mixture. The mixture was stirred at 700 rpm with a HV-agitator for 1 h to provide a homogenous dispersion having viscosity of 3000 cP at 25 °C. Without adding ethylene glycol to the mixture the viscosity of the suspension was 4100 cP at 25 °C as measured with the same agitator and stir rate.EXAMPLE 7
[0032] A TP-100-IM polymer dispersion having solid loading of 15% was prepared. 2 kg of dried TP-100-IM polymer in bicarbonate form (as shown below) was added to 10.8 kg of solvent and 500g ethylene glycol in a cylindrical reactor to form a mixture. The mixture was stirred at 700 rpm with a HV-agitator for 1 h to provide a homogenous dispersion having viscosity of 3200 cP at 25 °C. Without adding ethylene glycol to the mixture the viscosity of the suspension was 4400 cP at 25 °C as measured with the same agitator and stir rate.DEFINITIONS
[0033] The terms anion exchange membranes / ionomers / polymers are used interchangeably with hydroxide exchange membranes / ionomers / polymers.
[0034] The term “suitable substituent,” as used herein, is intended to mean a chemically acceptable functional group, preferably a moiety that does not negate the activity of the inventive compounds. Such suitable substituents include, but are not limited to halo groups, perfluoroalkyl groups, perfluoroalkoxy groups, alkyl groups, alkenyl groups, alkynyl groups, hydroxy groups, oxo groups, mercapto groups, alkylthio groups, alkoxy groups, aryl or heteroaryl groups, aryloxy or heteroaryloxy groups, aralkyl or heteroaralkyl groups, aralkoxy or heteroaralkoxy groups, HO — (C=O) — groups, heterocylic groups, cycloalkyl groups, amino groups, alkyl - and dialkylamino groups, carbamoyl groups, alkylcarbonyl groups, alkoxycarbonyl groups, alkylaminocarbonyl groups, dialkylamino carbonyl groups, arylcarbonyl groups, aryloxycarbonyl groups,alkylsulfonyl groups, and arylsulfonyl groups. Those skilled in the art will appreciate that many substituents can be substituted by additional substituents.
[0035] The term “alkyl,” as used herein, refers to a linear, branched or cyclic hydrocarbon radical, preferably having 1 to 32 carbon atoms (i.e., 1 , 2, 3, 4, 5, 6, 7, 8, 9, 10, 11 , 12, 13, 14, 15, 16, 17, 18, 19, 20, 21 , 22, 23, 24, 25, 26, 27, 28, 39, 30, 31 , or 32 carbons), and more preferably having 1 to 18 carbon atoms. Alkyl groups include, but are not limited to, methyl, ethyl, n-propyl, isopropyl, n-butyl, iso-butyl, secondary-butyl, and tertiary-butyl. Alkyl groups can be unsubstituted or substituted by one or more suitable substituents.
[0036] The term “alkenyl,” as used herein, refers to a straight, branched or cyclic hydrocarbon radical, preferably having 2, 3, 4, 5, 6, 7, 8, 9, 10, 11 , 12, 13, 14, 15, 16, 17, 18, 19, 20, 21 , 22, 23, 24, 25, 26, 27, 28, 39, 30, 31 , or 32 carbons, more preferably having 1 to 18 carbon atoms, and having one or more carbon-carbon double bonds. Alkenyl groups include, but are not limited to, ethenyl, 1 -propenyl, 2-propenyl (allyl), isopropenyl, 2-methyl-1 -propenyl, 1-butenyl, and 2-butenyl. Alkenyl groups can be unsubstituted or substituted by one or more suitable substituents, as defined above.
[0037] The term “alkynyl,” as used herein, refers to a straight, branched or cyclic hydrocarbon radical, preferably having 2, 3, 4, 5, 6, 7, 8, 9, 10, 11 , 12, 13, 14, 15, 16, 17, 18, 19, 20, 21 , 22, 23, 24, 25, 26, 27, 28, 39, 30, 31 , or 32 carbons, more preferably having 1 to 18 carbon atoms, and having one or more carbon-carbon triple bonds.Alkynyl groups include, but are not limited to, ethynyl, propynyl, and butynyl. Alkynyl groups can be unsubstituted or substituted by one or more suitable substituents, as defined above.
[0038] The term “aryl” or “ar,” as used herein alone or as part of another group (e.g., aralkyl), means monocyclic, bicyclic, or tricyclic aromatic radicals such as phenyl, naphthyl, tetrahydronaphthyl, indanyl and the like; optionally substituted by one or more suitable substituents, preferably 1 to 5 suitable substituents, as defined above. The term "aryl" also includes heteroaryl.
[0039] “Arylalkyl” or “aralkyl” means an aryl group attached to the parent molecule through an alkylene group. The number of carbon atoms in the aryl group and thealkylene group is selected such that there is a total of about 6 to about 18 carbon atoms in the arylalkyl group. A preferred arylalkyl group is benzyl.
[0040] The term “cycloalkyl,” as used herein, refers to a mono, bicyclic or tricyclic carbocyclic radical (e.g., cyclopropyl, cyclobutyl, cyclopentyl, cyclohexyl, cycloheptyl, cyclooctyl, cyclononyl, cyclopentenyl, cyclohexenyl, bicyclo[2.2.1]heptanyl, bicyclo[3.2.1]octanyl and bicyclo[5.2.0]nonanyl, etc.); optionally containing 1 or 2 double bonds. Cycloalkyl groups can be unsubstituted or substituted by one or more suitable substituents, preferably 1 to 5 suitable substituents, as defined above.
[0041] The term “-ene” as used as a suffix as part of another group denotes a bivalent radical in which a hydrogen atom is removed from each of two terminal carbons of the group, or if the group is cyclic, from each of two different carbon atoms in the ring. For example, alkylene denotes a bivalent alkyl group such as ethylene (-CH2CH2-) or isopropylene (-CH2(CH3)CH2-). For clarity, addition of the -ene suffix is not intended to alter the definition of the principal word other than denoting a bivalent radical. Thus, continuing the example above, alkylene denotes an optionally substituted linear saturated bivalent hydrocarbon radical.
[0042] The term “heteroaryl,” as used herein, refers to a monocyclic, bicyclic, or tricyclic aromatic heterocyclic group containing one or more heteroatoms (e.g., 1 to 3 heteroatoms) selected from O, S and N in the ring(s). Heteroaryl groups include, but are not limited to, pyridyl, pyrazinyl, pyrimidinyl, pyridazinyl, thienyl, furyl, imidazolyl, pyrrolyl, oxazolyl (e.g., 1,3-oxazolyl, 1 ,2-oxazolyl), thiazolyl (e.g., 1 ,2-thiazolyl, 1 ,3- thiazolyl), pyrazolyl, tetrazolyl, triazolyl (e.g., 1 ,2,3-triazolyl, 1 ,2,4-triazolyl), oxadiazolyl (e.g., 1 ,2,3-oxadiazolyl), thiadiazolyl (e.g., 1 ,3,4-thiadiazolyl), quinolyl, isoquinolyl, benzothienyl, benzofuryl, and indolyl. Heteroaryl groups can be unsubstituted or substituted by one or more suitable substituents, preferably 1 to 5 suitable substituents, as defined above.
[0043] The term "hydrocarbon" as used herein describes a compound or radical consisting exclusively of the elements carbon and hydrogen.
[0044] The term "substituted" means that in the group in question, at least one hydrogen atom bound to a carbon atom is replaced with one or more substituent groups such as hydroxy (-OH), alkylthio, phosphino, amido (-CON(RA)(RB), wherein RA and RB areindependently hydrogen, alkyl, or aryl), amino(-N(RA)(RB), wherein RA and RB are independently hydrogen, alkyl, or aryl), halo (fluoro, chloro, bromo, or iodo), silyl, nitro (- NO2), an ether (-ORA wherein RA is alkyl or aryl), an ester (-OC(O)RA wherein RA is alkyl or aryl), keto (-C(O)RA wherein RA is alkyl or aryl), heterocyclo, and the like. When the term "substituted" introduces or follows a list of possible substituted groups, it is intended that the term apply to every member of that group. That is, the phrase "optionally substituted alkyl or aryl" is to be interpreted as "optionally substituted alkyl or optionally substituted aryl." Likewise, the phrase "alkyl or aryl optionally substituted with fluoride" is to be interpreted as "alkyl optionally substituted with fluoride or aryl optionally substituted with fluoride."
[0045] The term "tethered" means that the group in question is bound to the specified polymer backbone. For example, an imidazolium-tethered poly (aryl alkylene) polymer is a polymer having imidazolium groups bound to a poly (aryl alkylene) polymer backbone.
[0046] When introducing elements of the present invention or the preferred embodiments(s) thereof, the articles "a", "an", "the" and "said" are intended to mean that there are one or more of the elements. The terms "comprising", "including" and "having" are intended to be inclusive and mean that there may be additional elements other than the listed elements.
[0047] ln view of the above, it will be seen that the several objects of the invention are achieved and other advantageous results attained.
[0048] As various changes could be made in the above products and methods without departing from the scope of the invention, it is intended that all matter contained in the above description and shown in the accompanying drawings shall be interpreted as illustrative and not in a limiting sense.
Claims
WHAT IS CLAIMED IS:1 . A method of making an anion exchange polymer dispersion with low viscosity comprising: mixing a dried anion exchange polymer, a solvent and an additive with an agitator designed for high viscosity liquid or gel for a time sufficient to form a homogeneous polymer dispersion having a polymer solids loading of at least 10 wt.%.
2. The method of claim 1 , wherein the homogeneous polymer dispersion has a viscosity ranging from about 1000 cp to about 10,000 cp as measured by a Brookfield DV-III Ultra rheometer with spindle # 62 at 25 °C.
3. The method of claim 1 or 2, wherein the viscosity of the polymer dispersion is reduced by about 10 to about 40% as compared to the same dispersion without addition of the additive.
4. The method of any one of claims 1-3, wherein the additive comprises an alcohol, a diol, a triol, an ester, a polyglycol, a fatty alcohol alkoxylate, an ether, or any combination thereof.
5. The method of claim 4, wherein the alcohol comprises n-propanol, 2-propanol, n- butanol, n-pentanol, or any combination thereof.
6. The method of claim 4, wherein the diol comprises ethylene glycol, propane-1 ,2-diol, 1 ,4-butanediol, 1 ,5-pentanediol, 1,6-hexanediol, 1 ,10-decanediol, or any combination thereof.
7. The method of claim 4, wherein the triol comprises a glycerol.
8. The method of claim 4, wherein the ester comprises a sorbitan-derived ester, a glycerol-derived ester, a polyethylene glycol-derived ester, or any combination thereof.
9. The method of claim 4, wherein the ester comprises sorbitan trioleate, sorbitan tnstearate, sorbitan monooleate, glycerol monostearate, POE (20) sorbitan trioleate, PEG-6 octanoic / decanoic glyceride, apricot kernel oil PEG-6 complex, POE 9 monooieate, a mono- or di-glyceride of an octanoic or decanoic acid, or any combination thereof.10, The method of any one of claims 1-9, wherein the mixing step occurs at a temperature ranging from 10 °C to a boiling point of the solvent.1 1 .The method of any one of claims 1 -10, wherein the anion exchange polymer in the polymer dispersion comprises structural units of Formulae 1A, 2A, 3A, and optionally 4A, wherein the structural units have the formulae:wherein:Ri and R2 are each independently alkyl, alkenyl alky nyl or aryl, or a quaternary ammonium or a nitrogen-containing heterocyclic group or a salt thereof; the quaternary ammonium group having the formula 5A:and the alkyl, alkenyl, alkynyl or aryl are optionally substituted with halide;R3, R4, R5, R6, R7, R8, R9, and Rw are each independently hydrogen, halide, alkyl, alkenyl alkynyl or aryl and the alkyl alkenyl, alkynyl or aryl are optionally substituted with halide, and wherein R4and R7are optionally linked to form a five membered ring optionally substituted with halide or alkyl; each R11is independently alkyl, alkenyl alkynyl orR13, R14R15, R16, and R17are each independently hydrogen, halide, alkyl, alkenyl alkynyl or aryl, and the alkyl, alkenyl, alkynyl or aryl are optionally substituted with halide, and wherein Ru and Rrr are optionally linked to form a five membered ring optionally substituted with halide or alkyl;R180and R240are each independently alkylene;R190, R200, R210, R220, and R230are each independently alkyl alkenyl, or alkynyl; each m is 0, 1 , 2, 3, 4, 5 or 6; n is 0, 1 , 2 or 3;X- is an anion; andZ is N,12. The method of any one of claims 1-11 , wherein the polymer solid loading ranges from about 10 to about 30 wt.%.
13. The method of any one of claims 1-12, wherein the time sufficient to form a homogeneous polymer dispersion ranges from about 1 to about 5 hours.
14. An anion exchange polymer dispersion having a polymer solid loading of at least 10 wt.% and viscosity of no more than 10,000 cp as prepared by the method of any one of claims 1-13.
15. An anion exchange polymer membrane prepared by the method of any one of claims 1-13, wherein thickness of the membrane ranges from about 10 to about 200 micrometers.
Citation Information
Patent Citations
Ion-conducting membranes
US10774431B2
Liquid compositions of fluorinated anion exchange polymers
WO2012098146A1