Laser annealing energy control method and laser annealing device

By gradually adjusting the laser power during the laser annealing process, the problem of difficult heat dissipation and energy spikes at the edge of the substrate is solved, a more uniform annealing effect is achieved, and the risk of substrate cracking and yield reduction is reduced.

WO2024198367A1PCT designated stage expired Publication Date: 2024-10-03AMIES TECHNOLOGY CO LTD

Patent Information

Application Number
PCT/CN2023/130639
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2023-11-09
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

During the laser annealing process, the lack of a heat dissipation surface at the edge of the substrate makes it difficult to dissipate heat, increases the thermal budget, and can easily lead to substrate cracking or yield reduction after being excited by thermal stress. It is difficult to effectively avoid energy spikes and temperature unevenness with existing technology.

Method used

By gradually adjusting the laser power during the laser annealing process, reducing the power from the outer tangent point of the substrate edge and gradually increasing it to the inner tangent point of the edge, ramp power control is used to avoid energy spikes and thermal stress and ensure annealing uniformity.

Benefits of technology

It effectively reduces the risk of substrate fragmentation and yield reduction, improves annealing uniformity and spot quality, and avoids fragmentation problems caused by energy spikes and thermal stress at the edge of the substrate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023130639_03102024_PF_FP_ABST
    Figure CN2023130639_03102024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention provides a laser annealing energy control method and a laser annealing device. The laser annealing energy control method comprises: moving a laser spot relative to a substrate at a first laser power, and reducing the laser power of the laser spot to a second laser power at a first position relative to the substrate; relative to the substrate, moving the laser spot to a second position relative to the substrate; moving the laser spot relative to the substrate from the second position relative to the substrate to a third position relative to the substrate, and increasing the laser power to a third laser power; and the laser spot performing scanning annealing on the substrate at the third laser power. The laser spot moves to the edge of the substrate relative to the substrate, so that the laser power is reduced, and the problem of energy peak at the edge of the substrate and the problem of fragments caused by thermal stress are avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Laser annealing energy control method and laser annealing equipment Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a laser annealing energy control method and laser annealing equipment. Background Art

[0002] In recent years, as integrated circuit process nodes have progressed toward ever-smaller dimensions (40nm and below), the junction depths of the source / drain and lightly doped drain (LDD) regions have gradually decreased, making shallow junction fabrication an increasingly important process module. To address the short-channel effect caused by reduced gate length, shallow ion implantation is required at the source / drain to form an ultra-shallow junction (USJ). The annealing process determines the junction depth and lateral dimensions of the source / drain PN junction and the lightly doped drain PN junction, requiring a high annealing temperature and a low annealing thermal budget to meet the advanced manufacturing process requirements for low stress, low diffusion, high activation, and high uniformity.

[0003] Laser annealing is a commonly used annealing process in integrated circuit manufacturing. Laser annealing utilizes a laser beam with a certain energy level to rapidly scan across the substrate surface, achieving microsecond-scale annealing of a specific differential region on the substrate. During laser scanning, heat from the center of the substrate can be dissipated to the edge of the substrate. However, the situation at the edge of the substrate is more complex: on the one hand, the edge of the substrate lacks a heat dissipation surface, making heat dissipation difficult, thus extending the annealing time and increasing the thermal budget. On the other hand, the edge of the substrate has potential defects that, when stimulated by thermal stress, can easily cause substrate cracking at these defects.

[0004] One current solution to this problem is to install guard rings at the edge of the substrate. However, annealing from the edge of the substrate can lead to substrate edge cracking due to high power input, edge defects, or thermal stress. This is because during the annealing process, thermal diffusion in the central region of the substrate, edge defects, and energy spikes generated during energy control switching at the edge of the substrate can easily lead to substrate cracking or reduced yield after being stimulated by thermal stress.

[0005] Another solution to the above problem is to perform constant power control through a software interface and suppress the laser power output through a gate signal during the annealing process, that is, high-level light output and low-level light shut-off. However, this method has the problem of excessive power mutation after large energy switching. Energy spikes appear in the energy control at the edge of the substrate, resulting in uneven annealing surface temperature, prone to abnormal traces, thereby reducing yield, or causing fragmentation problems.

[0006] Summary of the Invention

[0007] The object of the present invention is to provide a laser annealing energy control method and a laser annealing device to reduce or avoid the probability of substrate fragmentation or yield reduction during the laser annealing process.

[0008] To solve the above technical problems, the present invention provides a laser annealing energy control method, comprising:

[0009] A laser spot is moved relative to a substrate at a first laser power, and the laser power of the laser spot is reduced to a second laser power at a first position relative to the substrate; the laser spot is moved relative to the substrate to a second position relative to the substrate; the laser spot is moved from the second position relative to the substrate to a third position relative to the substrate and the laser power is increased to a third laser power; the laser spot performs scanning annealing on the substrate at the third laser power.

[0010] Optionally, the laser spot is moved relative to the substrate at the second laser power from a first position relative to the substrate to a second position relative to the substrate.

[0011] Optionally, in the process of moving the laser spot relative to the substrate from the second position relative to the substrate to the third position relative to the substrate, the second laser power is first increased to the fourth laser power and then increased to the third laser power.

[0012] Optionally, a rate of increasing the laser power from the second laser power to the fourth laser power is greater than a rate of increasing the laser power from the fourth laser power to the third laser power.

[0013] Optionally, the fourth laser power is 50% to 150% of the first laser power.

[0014] Optionally, the first position relative to the substrate is at the tangent point of the substrate edge along the movement direction of the laser spot relative to the substrate or in front of the tangent point of the substrate edge; the second position relative to the substrate is at the tangent point of the substrate edge along the movement direction of the laser spot relative to the substrate or behind the tangent point of the substrate edge.

[0015] Optionally, the first laser power is one-third to two-thirds of the third laser power; and the second laser power is less than one-third of the third laser power.

[0016] Based on the same inventive concept, the present invention also provides a laser annealing device for executing any of the above-mentioned laser annealing energy control methods.

[0017] In a laser annealing energy control method and laser annealing equipment provided by the present invention, a laser spot is moved relative to a substrate at a first laser power, and the laser power of the laser spot is reduced to a second laser power at a first position relative to the substrate; the laser spot is moved relative to the substrate to a second position relative to the substrate; the laser spot is moved relative to the substrate from the second position relative to the substrate to a third position relative to the substrate, and the laser power is increased to a third laser power; the laser spot performs scanning annealing on the substrate at the third laser power. The laser spot is moved relative to the substrate to the first position of the substrate, and the first laser power is switched to the second laser power, thereby reducing the laser power and preventing substrate fragmentation.

[0018] Furthermore, the laser spot is moved relative to the substrate to a second position on the substrate. The second laser power is first increased to the fourth laser power. This rapid power increase preheats the lens in the light path, reducing expansion effects, improving spot uniformity, enabling higher-quality spots for scanning, and improving annealing uniformity. The fourth laser power is then increased to the third laser power, avoiding energy spikes at the substrate edge and fragmentation caused by thermal stress. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Those skilled in the art will appreciate that the accompanying drawings are provided for a better understanding of the present invention and do not constitute any limitation on the scope of the present invention.

[0020] FIG1 is a schematic flow chart of a laser annealing energy control method according to an embodiment of the present invention;

[0021] 2 is a schematic structural diagram of a process flow of substrate position and laser power variation in a laser annealing process according to an embodiment of the present invention;

[0022] 3 is a schematic diagram of a process curve showing changes in substrate position and laser power during a laser annealing process according to an embodiment of the present invention;

[0023] 4 is a schematic structural diagram of a substrate scanning field in a laser annealing process according to an embodiment of the present invention;

[0024] In the drawings: 10 - substrate; 10a - first field scan; 10b - second field scan. DETAILED DESCRIPTION

[0025] To make the objects, advantages, and features of the present invention more clearly apparent, the present invention is further described below in conjunction with the accompanying drawings and specific embodiments. It should be noted that the drawings are all in a very simplified form and are not drawn to scale. They are only used to conveniently and clearly assist in illustrating the purposes of the embodiments of the present invention. In addition, the structures shown in the drawings are often part of the actual structure. In particular, different drawings may need to illustrate different focuses and sometimes use different scales.

[0026] As used in the present invention, the singular forms "a", "an", and "the" include plural referents. The term "or" is generally used to include "and / or". The term "several" is generally used to include "at least one". The term "at least two" is generally used to include "two or more". In addition, the terms "first", "second", and "third" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the technical features indicated. Therefore, the features specified as "first", "second", and "third" may explicitly or implicitly include one or at least two of the features. The terms "one end" and "the other end" and "proximal end" and "distal end" generally refer to two corresponding parts, which include not only endpoints. The terms "mounted", "connected", and "connected" should be understood in a broad sense. For example, they can be fixedly connected, detachably connected, or integrated; they can be mechanically connected or electrically connected; they can be directly connected or indirectly connected through an intermediate medium; they can be internal communication between two elements or an interactive relationship between two elements. In addition, as used in the present invention, "one element is disposed on another element" generally only indicates that there is a connection, coupling, cooperation, or transmission relationship between the two elements, and the connection, coupling, cooperation, or transmission between the two elements may be direct or indirect through an intermediate element. It should not be understood as indicating or implying a spatial positional relationship between the two elements. That is, one element can be in any orientation, such as inside, outside, above, below, or to one side of another element, unless the content clearly indicates otherwise. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0027] FIG1 is a flow chart of a laser annealing energy control method according to an embodiment of the present invention. As shown in FIG1 , this embodiment provides a laser annealing energy control method, including:

[0028] Step S10, moving a laser spot relative to a substrate at a first laser power, and reducing the laser power of the laser spot to a second laser power at a first position relative to the substrate;

[0029] The first laser power may be reduced to the second laser power gradually or immediately.

[0030] Step S20: moving the laser spot relative to the substrate to a second position relative to the substrate; moving the laser spot relative to the substrate from the second position relative to the substrate to a third position relative to the substrate and increasing the laser power to a third laser power, wherein the laser spot performs scanning annealing on the substrate with the third laser power.

[0031] The laser spot can be moved relative to the substrate from a first position relative to the substrate to a second position relative to the substrate at the second laser power. During the movement, the power can also be increased or decreased.

[0032] Furthermore, in the process of moving the laser spot relative to the substrate from the second position relative to the substrate to the third position relative to the substrate, the second laser power is first increased to a fourth laser power and then increased to the third laser power. The rate of increasing the laser power from the second laser power to the fourth laser power is greater than the rate of increasing the laser power from the fourth laser power to the third laser power.

[0033] Step S30, moving the laser spot relative to the substrate at a third laser power, and reducing the laser power of the laser spot to a second laser power at a fourth position relative to the substrate;

[0034] Step S40, moving the laser spot relative to the substrate at the second laser power, switching the laser power of the laser spot to the first laser power at a fifth position relative to the substrate, and ending the first field scan;

[0035] Step S50 , looping the above field scanning process until the entire substrate completes the annealing process.

[0036] In this embodiment, the laser annealing process can use analog signals to control the increase or decrease of laser power. Laser modulation uses light as a carrier to load signals onto the light, and realizes signal transmission according to application requirements. Generally, modulation is divided into external modulation and internal modulation. External modulation refers to mechanical modulation or acousto-optic modulation performed outside the laser, and internal modulation refers to power drive modulation. Among them, internal modulation is further divided into TTL (Transister-Transister-Logic) modulation and analog modulation. TTL modulation in the prior art is to input a high or low level (0V or 5V) DC signal of a certain frequency to the laser from the outside. When the low level is low, the light is turned off, and when the high level is high, the full power is output, and the high level amplitude is not adjustable. The laser modulation of this embodiment chooses to use analog modulation, which can freely adjust the waveform and amplitude of the input signal, and the laser output power changes linearly with the input analog voltage signal.

[0037] As shown in FIG2 , before the laser annealing process is performed on the substrate, the laser is located in a safe position. That is, there is no positive film under the laser. A test film or a blocking device that is not burned by the laser is set under the laser. The laser power is increased to the annealing power, the power stability is tested, and then the power is set to the safe power. The laser power is reduced to the safe shutter power and then switched to the travel power. The laser spot is then moved relative to the substrate at the travel power (first laser power) to a first position relative to the substrate. The laser power is reduced from the travel power to the safe power. The laser spot is moved relative to the substrate to a second position relative to the substrate and immediately increased to the travel power. The laser power is then increased to the annealing power using a ramp control function. That is, the laser power is annealing power when the laser spot is moved relative to the substrate to a third position relative to the substrate. The laser spot is moved relative to the substrate to a fourth position relative to the substrate, and the annealing power is switched to the safe power. The laser spot is moved relative to the substrate to a fifth position relative to the substrate, completing the first field scan. The laser power is then switched to the travel power, and the next field scan is performed. Immediately increasing the laser power to the travel power when the laser spot is moved relative to the substrate to the second position relative to the substrate means increasing the safe power to the travel power within the fastest response time of the laser device.

[0038] Specifically, as shown in Figure 2, a substrate 10 is provided. A laser spot is moved relative to the substrate with a first laser power P1 to a first position A relative to the substrate. The first laser power P1 is then reduced to a second laser power P2. This reduction can be immediate or gradual. The first position A of the substrate 10 is located at or before the first circumference point of the substrate 10 along the direction of movement of the laser spot relative to the substrate. The distance between the first position A and the first circumference point of the substrate 10 is, for example, 0-5 mm. In this embodiment, the distance between the first position A and the first circumference point of the substrate 10 is, for example, 0.5 mm. This means that the first laser power P1 is reduced to the second laser power P2 before the laser spot is moved relative to the substrate to the edge of the substrate 10. The first laser power P1 is the travel power between fields. The first laser power P1 (travel power) can be configured as a machine constant according to process requirements. This configuration parameter is used for transition power between fields during scanning. The first laser power P1 is, for example, 1000W-2000W. The first laser power P1 is one-third to two-thirds of the third laser power P3. The second laser power P2 is a safe power. The second laser power P2 (Safe Power) can be configured as a machine constant according to process requirements. This configuration parameter is used for annealing protection power at the edge of the substrate. The second laser power P2 is, for example, 0-1000W. The second laser power P2 is less than one-third of the third laser power P3. The safe laser power is used at the edge of the substrate to move the laser spot relative to the substrate and ensure that the internal power of the laser is in a stable state to avoid a decrease in laser power stability caused by power switching.

[0039] As shown in Figures 2 and 3, the laser spot is moved relative to the substrate 10 from a first position A to a second position B with a second laser power P2. The second laser power P2 is immediately increased to the fourth laser power P4, and then the fourth laser power P4 is increased to the third laser power P3 within a predetermined time. In other words, when the laser spot is moved relative to the substrate from the second position B to the third position C, the second laser power P2 is first increased to the fourth laser power P4, and then to the third laser power P3. The rate of increase in laser power from the second laser power P2 to the fourth laser power P4 is greater than the rate of increase from the fourth laser power P4 to the third laser power P3. The fourth laser power P4 is 50% to 150% of the first laser power P1. In this embodiment, the fourth laser power P4 is 100% of the first laser power P1, meaning that the second laser power P2 is immediately increased to the first laser power P1. The second position B of the substrate 10 is located at or after the first intangent point within the edge of the substrate along the direction of movement of the laser spot relative to the substrate. That is, after the laser spot is moved relative to the substrate to the first intangent point at the substrate edge, the laser power is immediately increased to the first laser power P1. By moving the laser spot relative to the substrate at low power to the first intangent point within the substrate edge, the second laser power P2 is immediately increased to the first laser power P1. This rapid power increase preheats the lens in the light output path, reduces expansion effects, improves spot uniformity, enables higher spot quality during scanning, and improves annealing uniformity. The laser power is increased to a third laser power P3. The substrate is scanned to the annealing starting point, for example, 2 mm from the substrate edge. Annealing is not required for substrates within 2 mm of the substrate edge. The third laser power P3 is the annealing power. For example, the third laser power P3 ranges from 2000 W to 3000 W. The third laser power P3 can be modified based on process requirements. This configuration parameter is used for the annealing process power and is not limited in this embodiment. The ramp power control function is used to increase the first laser power P1 to the third laser power P3. The time for immediately increasing the second laser power P2 to the first laser power P1 is less than the time for increasing the first laser power P1 to the third laser power P3. The predetermined time for increasing the first laser power P1 to the third laser power P3 within the predetermined time is, for example, less than 50ms. In this embodiment, the predetermined time for increasing the first laser power P1 to the third laser power P3 within the predetermined time is 0.01ms-10ms. The ramp power (Ramp Power) control time is within 50ms, which can effectively avoid the laser energy spike problem and the substrate fragmentation problem. The power ramp rate is 500W / ms as the best. Start executing the scanning annealing process of the first field.The ramp power (Ramp Power) control can be used to configure machine constants according to process requirements. This configuration parameter is used to control the power control during the switching process between scanning fields from the first laser power P1 to the third laser power P3. The power ramp time can be adjusted to preheat the scanning starting position to avoid the problem of energy overshoot when switching with high power. By switching the states of the first laser power P1 and the third laser power P3, the abnormal traces or fragments at the starting position of the substrate 10 caused by the excessive power of the first pulse in the large energy switching process can be reduced. The ramp power control function can be used to preheat the laser spot relative to the substrate to the starting position of the substrate 10, while reducing the energy overshoot phenomenon, avoiding the fragmentation problem, and improving the annealing uniformity. The ramp power control function can avoid the problem of energy spikes during energy switching, so that the laser beam energy can be smoothly transitioned and output smoothly, avoiding edge defects or thermal stress causing fragmentation problems.

[0040] Continuing with reference to Figures 2 and 3, the laser spot is moved relative to substrate 10 from third position C to fourth position D at third laser power P3, where it is then switched to second laser power P2. Fourth position D is located at or before the second inscribed point within the substrate edge along the direction of movement of the laser spot relative to the substrate. In other words, the laser power is reduced to the second laser power before the laser spot moves relative to the substrate to the second inscribed point within the substrate edge. In this embodiment, the laser power is switched to second laser power P2 at a point 0.5 mm before the end of the first field scan at the substrate edge inscribed point.

[0041] The laser spot is moved relative to the substrate at the second laser power P2 to the fifth position E of the substrate 10. The second laser power P2 is then switched to the first laser power P1, completing the first field scan. The fifth position E of the substrate 10 is located at or after the second tangent point outside the substrate edge along the direction of motion of the laser spot relative to the substrate, and the distance between the fifth position E and the second tangent point outside the substrate edge is 0-5 mm. In other words, the second laser power P2 is switched to the first laser power P1 only after the laser spot moves relative to the substrate to the second tangent point outside the substrate edge. Specifically, after the scanning synchronization movement reaches the second tangent point outside the substrate edge, upon receiving the scanning synchronization end signal in the first field, the laser power is controlled to decrease to the first laser power P1 via an analog signal. To address the issue of light damage caused by the same point being relatively stationary between the deceleration and acceleration of the workpiece stage during inter-field switching, there is a relative speed stationary section between the deceleration at the end of scanning and the start of acceleration of the moving stage between scanning fields. Laser power control is used to reduce the laser power from the first laser power P1 to the second laser power P2 during the stationary section, reducing static annealing at the same position and the occurrence of abnormal annealing points at the substrate edge. At the beginning of the workpiece stage acceleration phase, the laser is increased to the first laser power P1 to maintain stable laser power, prevent thermal deformation of the lens, and maintain a good spot shape.

[0042] The above field scanning process is looped until the entire substrate completes the annealing process. Specifically, as shown in Figures 1 and 4, there are multiple field scans in the substrate, for example, including a first field scan 10a and a second field scan 10b. After completing the first field scan 10a, the second field scan 10b is continued. Specifically, the second field scan 10b switches the energy to the second laser power P2 (Safe Power) at the first position of the substrate, moves the laser spot relative to the substrate at low power to the inscribed position within the edge of the substrate, and immediately increases the second laser power P2 (Safe Power) to the first laser power P1 (Travel Power). The laser output power is increased to the third laser power P3 through the ramp power control function, and the scanning annealing process of the second field is started. The above scanning process is looped to the last field.

[0043] In Figure 4, the tangent point is where the laser spot contacts the outer edge of the substrate, and the intangent point is where the laser spot contacts the inner edge of the substrate. In this embodiment, the first position A of the substrate 10 is located at the first tangent point outside the edge of the substrate 10 along the movement direction of the laser spot relative to the substrate or before the first tangent point. The distance between the first position A of the substrate and the first tangent point outside the edge of the substrate is, for example, 0-5 mm. The second position B of the substrate 10 is located at the first intangent point inside the edge of the substrate along the movement direction of the laser spot relative to the substrate or after the first intangent point. The third position C of the substrate 10 is where the movement direction of the laser spot relative to the substrate is switched to the third laser power. The fourth position D of the substrate 10 is located at the second intangent point inside the edge of the substrate along the movement direction of the laser spot relative to the substrate or before the second intangent point. The fifth position E of the substrate 10 is located at or behind the second tangent point outside the edge of the substrate along the movement direction of the laser spot relative to the substrate, and the distance between the fifth position E of the substrate and the second tangent point outside the edge of the substrate is 0-5mm.

[0044] This embodiment also provides a laser annealing device for executing the above-mentioned laser annealing energy control method.

[0045] In summary, in a laser annealing energy control method and laser annealing apparatus provided in an embodiment of the present invention, a laser spot is moved relative to a substrate at a first laser power, and at a first position relative to the substrate, the laser power of the laser spot is reduced to a second laser power; the laser spot is moved relative to the substrate to a second position relative to the substrate; the laser spot is moved relative to the substrate from the second position relative to the substrate to a third position relative to the substrate, and the laser power is increased to a third laser power; the laser spot performs scanning annealing on the substrate at the third laser power. The laser spot is moved relative to the substrate to the first and fourth positions relative to the substrate, and the first laser power is switched to the second laser power to reduce the laser power and prevent substrate fragmentation; the laser spot is moved relative to the substrate to the second position relative to the substrate, and the second laser power is increased to the fourth laser power. The rapid power increase can preheat the lenses in the light output path, reduce expansion effects, improve spot uniformity, enable higher spot quality during scanning, and improve annealing uniformity. The laser power is increased to the third laser power using a ramp power control method, avoiding energy spikes at the substrate edge and fragmentation caused by thermal stress. During the switching process between scanning fields, there is a period of near-stationary state between the deceleration or acceleration of the workpiece stage. By switching the laser power to a safe power, abnormal energy trace points or damage can be avoided at the stationary position.

[0046] It should be noted that the various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other. In addition, the different parts between the various embodiments can also be used in combination with each other, and the present invention is not limited to this.

[0047] Furthermore, it should be recognized that although the present invention has been disclosed above with reference to preferred embodiments, the above embodiments are not intended to limit the present invention. Any person skilled in the art can utilize the above disclosed technical content to make many possible changes and modifications to the technical solution of the present invention, or modify it into equivalent embodiments with equivalent variations, without departing from the scope of the technical solution of the present invention. Therefore, any simple modifications, equivalent variations, and modifications made to the above embodiments based on the technical essence of the present invention, without departing from the content of the technical solution of the present invention, shall still fall within the scope of protection of the technical solution of the present invention.

Claims

1. A laser annealing energy control method, It is characterized in that include: Moving a laser spot relative to a substrate at a first laser power, and reducing the laser power of the laser spot to a second laser power at a first position relative to the substrate; The laser spot is moved relative to the substrate to a second position relative to the substrate; the laser spot is moved relative to the substrate from the second position relative to the substrate to a third position relative to the substrate and the laser power is increased to a third laser power; the laser spot performs scanning annealing on the substrate with the third laser power.

2. The laser annealing energy control method according to claim 1, It is characterized in that The laser spot is moved relative to the substrate from the first position relative to the substrate to the second position relative to the substrate at the second laser power.

3. The laser annealing energy control method according to claim 1, It is characterized in that In the process of moving the laser spot relative to the substrate from the second position relative to the substrate to the third position relative to the substrate, the second laser power is first increased to the fourth laser power and then increased to the third laser power.

4. The laser annealing energy control method according to claim 3, It is characterized in that An increasing rate of increasing the laser power from the second laser power to the fourth laser power is greater than an increasing rate of increasing the laser power from the fourth laser power to the third laser power.

5. The laser annealing energy control method according to claim 3, It is characterized in that The fourth laser power is 50% to 150% of the first laser power.

6. The laser annealing energy control method according to claim 1, It is characterized in that The first position relative to the substrate is at the edge tangent point of the substrate along the movement direction of the laser spot relative to the substrate or in front of the edge tangent point of the substrate; the second position relative to the substrate is at the edge tangent point of the substrate along the movement direction of the laser spot relative to the substrate or behind the edge tangent point of the substrate.

7. The laser annealing energy control method according to claim 1, It is characterized in that The first laser power is one third to two thirds of the third laser power; and the second laser power is less than one third of the third laser power.

8. A laser annealing device, It is characterized in that Used to execute the laser annealing energy control method according to any one of claims 1 to 7.

Citation Information

Patent Citations

  • Laser spike annealing using fiber lasers

    CN104882370A

  • Laser annealing method and system

    CN110216370A

  • Laser annealing equipment based on composite laser source and annealing method

    CN113594029A

  • Methodology of improving the manufacturability of laser anneal

    US20080272097A1

  • Apparatus and Methods for Annealing Wafers

    US20130052837A1

Cited By

  • Processing method of edge high-stress hard and brittle semiconductor material

    CN120772693A

  • A method of processing an edge high stress hard brittle semiconductor material

    CN120772693B