Method for producing a monocrystalline body by means of a solid-state recrystallization process

The method of constructing a green body from powders, using fluxes to enhance grain boundary mobility, and applying a temperature gradient with localized laser irradiation addresses the limitations of existing single-crystalline laser crystal production, achieving faster and more efficient recrystallization with improved thermal stability and efficiency.

WO2024200197A1PCT designated stage expired Publication Date: 2024-10-03FRAUNHOFER GESELLSCHAFT ZUR FORDERUNG DER ANGEWANDTEN FORSCHUNG EV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/057579
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-03-21
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Existing methods for producing single-crystalline laser crystals are limited by thermal effects, such as strong thermal lensing and inhomogeneous temperature distributions, which reduce laser efficiency, and are hindered by the inability to achieve optimal three-dimensional doping and the preservation of pores and scattering centers in the recrystallization process.

Method used

A method involving the construction of a green body from powders, sintering to form a ceramic, and subsequent solid-state recrystallization using fluxes like LiF, CaO, and PbF2 to enhance grain boundary mobility, combined with a temperature gradient and localized laser irradiation to minimize pores and scattering centers, allowing for faster and more efficient recrystallization.

Benefits of technology

This method enables the production of single-crystalline laser crystals with reduced pores and scattering centers, improving thermal stability and efficiency, and allowing for optimized three-dimensional doping, thus enhancing laser performance and reducing production time and costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 000001
    Figure 000001
  • Figure 000002
    Figure 000002
  • Figure 000003
    Figure 000003
Patent Text Reader

Abstract

In a method for producing a monocrystalline body, in particular a laser crystal, a green body is constructed from one or more powders of one or more starting materials, the green body is sintered, thereby forming a ceramic, and the ceramic is converted into a monocrystalline structure by means of a solid-state recrystallization process. The method is characterized in that the powder crystals of the powder(s) are mixed or coated with fluxes in order to construct the green body, said fluxes increasing the mobility of grain boundaries during the formation of the ceramic and / or dissolving grain material during the formation of the ceramic and crystallizing the grain material out during the solid-state recrystallization process. The method facilitates a faster recrystallization process and allows a reduction of pores and enclosures in the ceramic starting material and thus a production of a crystal with a higher degree of purity.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Process for producing a single-crystalline body by solid-state recrystallization

[0002] Technical application area

[0003] The present invention relates to a method for producing a single-crystalline body, in which a green body is constructed from one or more powders of one or more starting materials, the green body is sintered to form a ceramic, and the ceramic is converted into a single-crystalline structure by solid-state recrystallization.

[0004] An exemplary technical application area of ​​the proposed method concerns the production of laser crystals. Lasers based on laser crystals are limited in their performance enhancement by thermal effects. These effects cause strong thermal lensing or thermally induced stress and birefringence, which destabilize the laser resonator or worsen the overlap between the laser mode and the pump light or the polarization losses. Pump light absorption can also result in an inhomogeneous temperature distribution, so that parts of the laser crystal become significantly hotter than others, which negatively influences laser efficiency. These negative effects could be reduced or avoided by optimized doping of the laser crystal, ideally varying in the three spatial dimensions.This varying doping could take into account both the geometry of the laser beam and the pump light distribution, thus leading to a more balanced temperature distribution during laser operation. However, this is not possible with most laser crystals that are pulled from a melt. This applies in particular to dopant distributions that are transverse to the pulling direction and generally to crystals where the segregation coefficient of the dopant is almost 1, so that this doping can be doped in any ratio. In this case, no axial gradient in the pulling direction, which could otherwise have been utilized, develops.

[0005] State of the art

[0006] Three-dimensional dopant distributions can be achieved using laser ceramics, where the green body is built up layer by layer from powder, for example, and in this way, similar to 3D printing, the desired areas can be doped differently. Subsequent ceramization or sintering, for example via cold or hot isostatic pressing or by means of spark plasma sintering, produces a transparent ceramic with a high density >99.9% of the maximum crystal density, whereby the 3D doping structure is retained. While the microcrystalline structure means the mechanical strength is superior to that of a single crystal, the ceramic still has pores and scattering centers, which generate increased scattering losses compared to a single crystal.In addition, only ceramics made of isotropic materials can be used in lasers, since otherwise the random orientation of the crystallites in birefringent materials leads to a disruption of the optical propagation. Another known process is in which the sintered ceramics are converted into a single-crystalline structure by means of solid-state recrystallization through contact with a seed single crystal. This technique is described, for example, in I. Milisavl j evic et al., “Current status of solid-state single crystal growth", BMC Mat (2020), pages 1-26. However, pores and scattering centers are also retained and are enclosed by the growing single crystal if the starting ceramic itself was not already highly pure and optimized. A further disadvantage of this technique is the slow growth rate of recrystallization, which makes this process time-consuming and costly.

[0007] The object of the present invention is to provide a method for producing a single-crystal body by solid-state recrystallization of a ceramic, which enables faster recrystallization with a lower proportion of pores and scattering centers in the single crystal. The method is particularly suitable for producing laser crystals.

[0008] Description of the invention

[0009] This object is achieved by the method according to claim 1. Advantageous embodiments of the method are the subject of the dependent claims or can be found in the following description and the exemplary embodiment.

[0010] In the proposed method for producing a single-crystalline body, a green body is first constructed from one or more powders of one or more starting materials. The green body can be shaped using suitable molds and presses, as in comparable prior art processes. Already ground crystallites or mixtures of powders which only form the desired crystallites during sintering can be used as powdered starting materials. Powders obtained by co-precipitation can also be used. In particular, it is possible to build up the green body from powders with different doping levels, so that the subsequent single-crystalline body, for example a laser crystal, has a desired three-dimensional distribution of the doping concentration.A three-dimensional distribution of the doping concentration means that the doping or dopant concentration varies in at least one, preferably in two or three spatial dimensions. The green body is then sintered to form a ceramic and the ceramic is converted into a single-crystalline structure by solid-state recrystallization. This takes place by contact between the ceramic and at least one seed single crystal and can - as in the prior art mentioned at the beginning - take place during the sintering process after formation of the ceramic or by suitable post-treatment of the ceramic in a separate process. The at least one seed single crystal can in this case be integrated into the green body during the construction of the green body.embedded or brought into contact with the green body or with the ceramic formed from the green body from the outside, for example bonded to the green body or the ceramic. The proposed method is characterized in that the powder particles of the powder(s) for constructing the green body are mixed or coated with fluxes which increase the mobility of the grain boundaries during the formation of the ceramic and / or dissolve grain material during the formation of the ceramic and crystallize out during solid-state recrystallization. Examples of such fluxes are LiF, CaO, SiO2, PbO, PbF2, B2O3 or combinations thereof. The fluxes used are preferably two- or three-component.

[0011] By adding the fluxes, the formation of pores and scattering centers during the formation of the ceramic is largely avoided, so that the subsequent solid-state recrystallization process also leads to a single-crystalline structure of higher purity. The rate of recrystallization itself is also increased by the addition of the fluxes. In a particularly advantageous embodiment, the powder particles or powder grains are coated with these fluxes before the base body is built up, in particular as a core-shell structure. This can be done, for example, by co-precipitation in a sol-gel process. In another embodiment, the fluxes are mixed with the powders by joint grinding, e.g. in ball mills.

[0012] In a particularly advantageous embodiment of the proposed method, the solid-state recrystallization process is carried out by post-treatment of the ceramic body obtained by sintering the green body. During this post-treatment, a (local) temperature gradient is generated in the ceramic body, beginning at the seed single crystal, and moved across the ceramic body with the crystallization front. This can be achieved, for example, by arranging suitable heating elements, such as heating coils, around the circumference of the ceramic body, which are then controlled accordingly. The use of a specifically adjusted temperature gradient improves and advances microscopic solid-state recrystallization.

[0013] In a particularly advantageous embodiment, however, the ceramic body is irradiated locally with one or more lasers, for example a CO2 laser, the radiation from which is at least partially absorbed by the ceramic. During the irradiation, which takes place in a vacuum or under a special atmosphere, the ceramic body is heated locally and the hot zone thus created is drawn through the ceramic by moving the laser beam or the ceramic, starting from the seed crystal. By focusing the laser beam, a very limited recrystallization zone is obtained. This means that most of the ceramic which has not yet been recrystallized remains at a lower temperature and the recrystallization process does not start too early. For local heating, a line focus can be created, for example.In the case of a rod-shaped ceramic body in which the single crystal seed is arranged at one end of the rod, a conical laser beam can also be formed, which forms a line focus surrounding the ceramic rod, which is then guided along the rod with the crystallization zone or crystallization front.

[0014] The sintering process for forming the ceramic body can be carried out in different ways, preferably by SPS (SPS: Spark Plasma Sintering), but particularly preferably by hot isostatic pressing, in which case the required temperatures are lower due to the fluxes used, since the solid reactions that occur are then relatively more correlated with the melting point of these fluxes than with the melting and phase transformation temperatures of the pure ceramic.

[0015] The proposed process is particularly advantageous for producing laser crystals, especially rare-earth-doped YAG laser crystals. The process is also suitable for producing other single crystals, particularly for high-power solid-state lasers for military and industrial applications, in the latter case, for example, for laser material processing (cutting, welding).

[0016] The proposed process enables faster recrystallization and allows the elimination of pores and inclusions in the ceramic starting material, as they migrate away from the forming crystal along with the crystallization front. The process also saves time and energy costs.

[0017] In one example for the production of an Nd:YAG laser crystal, for example, already formed Nd:YAG crystallites are provided to build up the rod-shaped green body and mixed with a flux of PbF2 and PbO. This can be achieved by grinding these materials together in a ball mill. The proportion of flux is only a few percent by weight or less. The powder is pressed into a rod-shaped green body in a known manner and sintered by hot isostatic pressing. A seed crystal, for example a YAG crystal, is then bonded to one end of the sintered body. The ceramic rod is then heated locally under vacuum conditions using a CCt laser. The CO2 laser is focused on the ceramic body in such a way that a circumferential line focus is created, which is then guided from the seed crystal together with the crystallization zone to the other end of the rod.The prior addition of fluxes creates a thin layer of flux at the grain boundaries of the final ceramic. These fluxes improve the mobility of the grain boundaries. The fluxes dissolve locally limited material from the grains, from which the single crystal then crystallizes in the temperature gradient. This leads to the avoidance or significant reduction of pores or scattering centers in the ceramic and in the final laser crystal.

Claims

Patent claims 1 . A method for producing a single-crystal body, in which - a green body is constructed from one or more powders of one or more starting materials, - the green body is sintered to form a ceramic and - the ceramic is converted into a single-crystalline structure by solid-state recrystallization, characterized in that powder particles of the powder(s) for building up the green body are mixed or coated with fluxes which increase the mobility of grain boundaries during the formation of the ceramic and / or dissolve grain material during the formation of the ceramic and crystallize out during the solid-state recrystallization.

2. Method according to claim 1, characterized in that the solid-state recrystallization takes place by contact of the ceramic with at least one seed single crystal and is driven by generating a temperature gradient. 3 . Method according to claim 2, characterized in that the temperature gradient is generated locally starting at the seed single crystal and with a Solid-state recrystallization formed Crystallization front is moved over the ceramic.

4. The method according to claim 2 or 3, characterized in that the seed single crystal is embedded in the green body or bonded to the green body or the ceramic.

5. Process according to one of claims 2 to 4, characterized in that the solid-state recrystallization is carried out by a post-treatment after the sintering of the ceramic.

6. Method according to claim 5, characterized in that the temperature gradient is generated by local action of one or more laser beams on the sintered ceramic.

7. Method according to claim 6, characterized in that the laser beam(s) are guided in such a way that they form a line focus on the ceramic, which is guided over the ceramic starting from the seed single crystal.

8. Process according to one of claims 1 to 7, characterized in that the fluxes used are LiF, CaO, SiO2, PbO, PbF2, B2O3, be used.

9. A process according to any one of claims 1 to 7, characterized in that combinations of at least two of the following compounds are used as fluxes: LiF, CaO, SiO2, PbO, PbF2 and B2O3.

10. Process according to one of claims 1 to 9, characterized in that the sintering is carried out by hot isostatic pressing.

11. Method according to one of claims 1 to 10, characterized in that the green body is constructed from powders of different doping.

12. The method according to claim 11, characterized in that the green body is constructed from powders of different doping in such a way that a predeterminable three-dimensional distribution of a doping concentration is obtained in the single-crystalline body.

13. Method according to one of claims 1 to 12 for producing a laser crystal, in particular a rare earth-doped YAG laser crystal.

Citation Information

Patent Citations

  • Production of barium titanate single crystal

    JP1997263496A

  • Rare earth-iron garnet single crystal material and method for preparation thereof and device using rare earth-iron garnet single crystal material

    US20030177975A1

  • Process for producing single-crystal ceramics

    US4900393A

  • Method for tailoring the dopant profile in a laser crystal using zone processing

    WO2013025926A1