Self-luminous display device and method for manufacturing self-luminous display device

By adjusting gate length and oxide semiconductor reduction in self-emissive display devices through specific manufacturing processes, the solution addresses the issue of uneven brightness and aging-related quality deterioration, achieving improved display quality and stability.

WO2024201685A1PCT designated stage expired Publication Date: 2024-10-03SHARP DISPLAY TECHNOLOGY CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/012359
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

The variation in transistor threshold values due to differences in gate length and oxide semiconductor reduction leads to uneven brightness and deteriorated display quality in self-emissive display devices, which is difficult to adjust and worsens with aging.

Method used

The design includes a first and second pixel circuit with transistors having channel layers made of oxide semiconductors, where the gate length and oxide semiconductor reduction are adjusted to cancel out threshold differences, using a manufacturing process involving plasma treatment and annealing to form insulating layers with varying hole diameters and oxygen distribution, resulting in improved uniformity and stability of brightness.

Benefits of technology

This approach reduces the difference in threshold values between transistors, enhancing display quality by minimizing raw brightness unevenness and maintaining improved performance after aging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023012359_03102024_PF_FP_ABST
    Figure JP2023012359_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A self-luminous display device according to the present disclosure comprises: a first pixel circuit that includes a first transistor (T1) having a first channel layer (C1) containing an oxide semiconductor; and a second pixel circuit that has the same circuit configuration as that of the first pixel circuit, and that includes a second transistor (T2) corresponding to the first transistor (T1) and having a second channel layer (C2) containing an oxide semiconductor. The gate length (L2) of the second transistor (T2) is greater than the gate length (L1) of the first transistor (T1). The oxide semiconductor contained in the second transistor (T2) is reduced more than the oxide semiconductor contained in the first transistor (T1).
Need to check novelty before this filing date? Find Prior Art

Description

Self-luminous display device and method for manufacturing the same

[0001] The present disclosure relates to a self-emissive display device and a method for manufacturing a self-emissive display device.

[0002] Patent Document 1 discloses that the thickness of the gate insulating film affects the threshold value of a transistor.

[0003] JP 2015-060996 A (March 30, 2015)

[0004] The threshold voltage of a transistor is affected by the gate length and the carrier concentration in the channel layer, which can lead to variations in the actual threshold voltage of the transistor and a decrease in display quality.

[0005] A self-luminous display device according to one aspect of the present disclosure includes a first pixel circuit including a first transistor having a first channel layer including an oxide semiconductor, and a second pixel circuit having the same circuit configuration as the first pixel circuit, including a second transistor corresponding to the first transistor and having a second channel layer including an oxide semiconductor, wherein the gate length of the second transistor is longer than the gate length of the first transistor, and the oxide semiconductor included in the second channel layer is more reduced than the oxide semiconductor included in the first channel layer.

[0006] A method for manufacturing a self-luminous display device according to one embodiment of the present disclosure includes the steps of forming a channel layer including an oxide semiconductor for a transistor, forming a first insulating layer in contact with the channel layer, etching the first insulating layer using a first plasma to form a hole penetrating the first insulating layer or introducing oxygen into the first insulating layer, annealing the channel layer and the first insulating layer after the step using the first plasma, forming a conductor layer that will be the material for the gate electrode of the transistor, and etching the conductor layer using a second plasma to form the gate electrode of the transistor from the conductor layer.

[0007] According to one aspect of the present disclosure, the display quality of a display device can be improved.

[0008] 5 is a plan view showing an example of the configuration of a self-luminous display device according to an embodiment of the present disclosure. FIG. 6 is a plan perspective view showing an example of the configuration of a first transistor and a second transistor shown in FIG. 1. FIG. 7 is a cross-sectional view showing an example of the configuration of the first transistor and the second transistor shown in FIG. 1. FIG. 8 is a cross-sectional view showing an example of the configuration of the first transistor and the second transistor shown in FIG. 1. FIG. 9 is a cross-sectional view showing an example of the manufacturing method of a self-luminous display device according to an embodiment of the present disclosure. FIG. 10 is a cross-sectional view showing an example of the manufacturing method of a self-luminous display device according to an embodiment of the present disclosure.

[0009] [Embodiment 1] (Configuration) Fig. 1 is a plan view showing an example configuration of a self-emissive display device according to an embodiment of the present disclosure. As shown in Fig. 1, the self-emissive display device 1 according to the present disclosure includes a display unit DA including a plurality of pixels PX, and a drive circuit 10 that drives the display unit DA. Each of the plurality of pixels PX includes a light-emitting element 2 and a pixel circuit 3 that controls the current or voltage applied to the light-emitting element 2. Each of the pixel circuits 3 includes a transistor TX, and each of the transistors TX has a channel layer including an oxide semiconductor.

[0010] The self-luminous display device 1 includes a first pixel circuit 31 including a first transistor T1 having a first channel layer including an oxide semiconductor, and a second pixel circuit 32 having the same circuit configuration as the first pixel circuit 31, corresponding to the first transistor T1, and including a second transistor T2 having a second channel layer including an oxide semiconductor. More specifically, the second pixel circuit 32 has the same circuit element layout and connection relationship as the first pixel circuit 31, and the same characteristics as the corresponding circuit elements. The characteristics of the circuit elements include, for example, the threshold value of the transistor and the capacitance value of the capacitor. As is well known, the threshold value of the gate voltage of a transistor using an oxide semiconductor depends on the gate length of the transistor and the degree of reduction of the oxide semiconductor in the transistor. Therefore, the first transistor T1 and the second transistor T2 have the same threshold value, gate length, and degree of reduction by design. The first transistor T1 and the second transistor T2 may be drive transistors. Hereinafter, attention will be focused on the first transistor T1 and the second transistor T2.

[0011] 2, 3, and 4 are plan perspective views, cross-sectional views, and cross-sectional views showing configuration examples of the first transistor and the second transistor shown in FIG. 1. FIG. 3 shows the ABCD cross section of FIG. 2, and FIG. 4 shows the EFGHIJ cross section of FIG. 2. As shown in FIGS. 2 to 4, the first transistor T1 has a gate electrode G1, a source electrode S1, a drain electrode D1, and a first channel layer C1 including an oxide semiconductor. The second transistor T2 has a gate electrode G2, a source electrode S2, a drain electrode D2, and a second channel layer C2 including an oxide semiconductor.

[0012] The actual gate length L2 of the second transistor T2 is longer than the actual gate length L1 of the first transistor T1, and the oxide semiconductor contained in the actual second channel layer C2 is more reduced than the oxide semiconductor contained in the actual first channel layer C1. These actual differences are due to the manufacturing process. Hereinafter, actual values ​​and differences will be described unless otherwise specified as "design" or "ideal."

[0013] According to the above configuration, the difference between the gate lengths L1 and L2 acts to make the threshold value of the second transistor T2 larger than that of the first transistor T1. On the other hand, the difference in the degree of reduction of the oxide semiconductor acts to make the threshold value of the second transistor T2 smaller than that of the first transistor T1. As a result of these effects (at least partially) canceling each other out, the difference in threshold value between the first transistor T1 and the second transistor T2 can be reduced.

[0014] As a comparative example, consider transistors with different gate lengths but the same degree of oxide semiconductor reduction. In this case, differences in gate lengths directly lead to differences in threshold values, resulting in large threshold differences. In multiple pixel circuits of a self-luminous display device, such large threshold differences cause brightness unevenness and degrade display quality. Commercially, adjustments (known as "de-unevenness processing") are typically performed before shipping to make brightness unevenness invisible, but brightness unevenness that is difficult to adjust may remain. Furthermore, differences in threshold values ​​lead to differences in aging, which causes brightness unevenness after aging and degrades display quality.

[0015] According to the configuration of the present disclosure, the difference in threshold value is small, and therefore the original luminance unevenness before the demurration process is small, which improves the display quality of the self-luminous display device 1, and in particular improves the display quality after aging.

[0016] The first transistor T1 and the second transistor T2 may each be a thin-film transistor. The oxide semiconductor included in the first channel layer C1 and the oxide semiconductor included in the second channel layer C2 may be the same material. The oxide semiconductor may be, for example, copper oxide, silver oxide, zinc oxide, gallium oxide, tin oxide, indium oxide, indium gallium zinc oxide, indium tin oxide, indium zinc oxide, titanium oxide, indium titanium oxide, or indium titanium zinc oxide. The gate electrode G1 and the gate electrode G2 are formed from the same layer, and the first channel layer C1 and the second channel layer C2 are formed from the same layer. The source electrodes S1, S2 and the drain electrodes D1, D2 may be formed from the same layer.

[0017] The self-luminous display device 1 includes a first insulating layer I1 having a first portion P1 in contact with the top surface of the first channel layer C1 and a second portion P2 in contact with the top surface of the second channel layer C2. The density of hydrogen contained in the second portion P2 is greater than the density of hydrogen contained in the first portion P1. Furthermore, the diameter of the second hole H2 penetrating the vicinity of the second portion P2 is smaller than the diameter of the first hole H1 penetrating the vicinity of the first portion P1. The first hole H1 is a through hole for dehydrogenating the first portion P1, and the second hole H2 is a through hole for dehydrogenating the second portion P2. The diameter of the second hole H2 may be zero; in other words, there may be no dehydrogenation hole in the vicinity of the second portion P2. The first insulating layer I1 may be an inorganic insulating layer and may include, for example, silicon nitride (SiN), silicon oxide (SiO), or silicon oxynitride (SiNO).

[0018] (Manufacturing Method) Figure 5 is a cross-sectional view showing an example of a manufacturing method of a self-luminous display device according to an embodiment of the present disclosure. As shown in Figure 5, first, a first channel layer CX including an oxide semiconductor of a transistor is formed (step S10), and then a first insulating layer I1 in contact with the channel layer CX is formed (step S20). The channel layer CX includes a first channel layer C1 and a second channel layer C2. The first insulating layer I1 is formed on the channel layer CX. The first insulating layer I1 contains hydrogen when formed.

[0019] Next, a photoresist layer 21 having an opening OX is formed on the first insulating layer I1 (step S22). The opening OX includes a first opening O1 overlapping the planned position of the first hole H1 and a second opening O2 overlapping the planned position of the second hole H2. Ideally, the depth and diameter of the second opening O2 are the same as the depth and diameter of the first opening O1. It is beneficial that the opening OX does not penetrate through the substrate. The photoresist layer 21 having the non-penetrating opening OX can be realized using a half-tone mask or a gray-tone mask.

[0020] Then, the photoresist layer 21 and the first insulating layer I1 are etched using the first plasma 41 to form holes HX penetrating the first insulating layer I1 (step S24), and the photoresist layer 21 is removed (step S26). The openings OX overlap the holes HX in a plan view. The holes HX penetrating the first insulating layer I1 include a first hole H1 and a second hole H2. In step S24, the stronger the first plasma 41, the larger the diameters of the openings OX and the holes HX. Specifically, the diameter of the first holes H1 formed in areas where the intensity of the first plasma 41 is strong is larger than the diameter of the second holes H2 formed in areas where the intensity of the first plasma 41 is weak.

[0021] If the opening OX does not penetrate the photoresist layer 21 in step S22, the photoresist layer 21 is etched with the first plasma 41 in step S24 so that the opening OX penetrates the photoresist layer 21, and the first insulating layer I1 is further etched to form the hole HX. This makes it easy to differentiate the diameters of the first hole H1 and the second hole H2. In particular, the diameter of the second hole H2 can be set to zero, in other words, dehydrogenation holes can be prevented from being formed in areas where the first plasma 41 is weak.

[0022] After the step using the first plasma 41, the channel layer CX and the first insulating layer I1 are annealed (step S30). The annealing liberates hydrogen from the first insulating layer I1, and some of the liberated hydrogen reduces the oxide semiconductor contained in the channel layer CX, while another portion escapes without reducing it. The larger the diameter of the hole HX, the more easily hydrogen escapes through the hole HX, and therefore, the oxide semiconductor near the hole HX is not reduced as much. Specifically, due to the difference in diameter between the first hole H1 and the second hole H2, hydrogen liberated from the first portion P1 toward the first channel layer C1 escapes more easily than hydrogen liberated from the second portion P2 toward the second channel layer C2. Therefore, the oxide semiconductor contained in the second channel layer C2 is reduced more than the oxide semiconductor contained in the first channel layer C1.

[0023] Next, a conductor layer 13, which will be the material for the transistor gate electrode GX, is formed (step S40), and a patterned template layer 51 is formed on the conductor layer 13 (step S42). Then, the conductor layer 13 is etched using a second plasma 42 according to the template layer 51 to form the transistor gate electrode GX from the conductor layer 13 (step S44), and the template layer 51 is removed. The gate electrode GX includes a gate electrode G1 and a gate electrode G2. In step S44, the stronger the second plasma 42, the shorter the gate length. Specifically, the gate length L1 of the first transistor T1 formed in a region where the second plasma 42 is strong is shorter than the gate length L2 of the second transistor T2 formed in a region where the second plasma 42 is weak.

[0024] According to this manufacturing method, the effects of the gate length and the degree of reduction of the oxide semiconductor on the transistor threshold value are (at least partially) canceled out, thereby reducing the difference between the design threshold value of the transistor and the actual threshold value of the transistor, and also reducing the difference in threshold value between the first transistor T1 formed in the region where the plasma intensity is strong and the second transistor T2 formed in the region where the plasma intensity is weak.

[0025] FIG. 6 is a plan view showing an example of the intensity distribution of the plasma shown in FIG. 5 . As shown in FIG. 6 , the first and second plasmas 41 and 42 may each have a spatially non-uniform intensity distribution. Typically, within the chamber 40 where the plasma is generated, the plasma is weak in the central region F1 and the peripheral region F2, and strong in the intermediate region F3 between them. The shape of the intermediate region F3 corresponds to the shape of the plasma generating electrode and is usually annular. It is beneficial that the intensity distributions of the first and second plasmas 41 and 42 are substantially identical to each other. Specifically, it is beneficial that the first and second plasmas 41 and 42 are strong in the region where the first transistor T1 is formed and weak in the region where the second transistor T2 is formed. The intensity distribution may be measured or estimated from the configuration of the plasma generating device. If the shape and arrangement of the plasma generating electrodes are identical, it can be determined that the intensity distributions of the first and second plasmas 41 and 42 are identical. The first and second plasmas 41 and 42 may also be generated by the same device.

[0026] [Embodiment 2] Another embodiment of the present disclosure will be described below. For ease of explanation, the same reference numerals will be used to designate components having the same functions as those described in the above embodiment, and the description thereof will not be repeated.

[0027] 7 is a cross-sectional view showing an example of the configuration of a self-luminous display device according to an embodiment of the present disclosure. As shown in FIG. 7 , the self-luminous display device 1 according to the present disclosure includes a second insulating layer I2 having a third portion P3 in contact with the lower surface of the first channel layer C1 and a fourth portion P4 in contact with the lower surface of the second channel layer C2. The density of hydrogen contained in the fourth portion P4 is greater than the density of hydrogen contained in the third portion P3. Furthermore, the diameter of the fourth hole H4 penetrating the vicinity of the fourth portion P4 is smaller than the diameter of the third hole H3 penetrating the vicinity of the third portion P3. The third hole H3 is a through hole for dehydrogenating hydrogen from the third portion P3, and the fourth hole H4 is a through hole for dehydrogenating hydrogen from the fourth portion P4. The diameter of the fourth hole H4 may be zero; in other words, there may be no dehydrogenation hole near the fourth portion P4. The second insulating layer I2 may be an inorganic insulating layer and may contain, for example, silicon nitride (SiN), silicon oxide (SiO), or silicon oxynitride (SiNO). The third hole H3 may or may not overlap the first hole H1 in a planar view. The fourth hole H4 may or may not overlap the second hole H2 in a planar view.

[0028] FIG. 8 is a cross-sectional view showing an example of a method for manufacturing a self-luminous display device according to an embodiment of the present disclosure. As shown in FIG. 8 , a second insulating layer I2 is formed on the side opposite the first insulating layer I1, contacting the channel layer CX (step S50). In the example shown in FIG. 8 , the channel layer CX is to be formed on the second insulating layer, and the first insulating layer I1 is to be formed on the channel layer CX. The second insulating layer I2 also contains hydrogen when formed. Next, a photoresist layer 22 having an opening OY is formed on the second insulating layer I2 (step S52). The opening OY includes a third opening O3 overlapping the planned position for forming the third hole H3 and a fourth opening O4 overlapping the planned position for forming the fourth hole H4. Ideally, the depth and diameter of the fourth opening O4 are the same as those of the third opening O3. It is also beneficial that the opening OY does not penetrate through the substrate.

[0029] Then, the photoresist layer 22 and the second insulating layer I2 are etched with the third plasma 43 to form holes HY penetrating the second insulating layer I2 (step S54), and the photoresist layer 22 is removed (step S56). In other words, the photoresist layer 22 is etched with the third plasma 43 to form openings OY penetrating the photoresist layer 22, and the second insulating layer I2 is further etched to form holes HY. The openings OY overlap the holes HY in a plan view. The holes HY penetrating the second insulating layer I2 include a third hole H3 and a fourth hole H4. The diameter of the third hole H3 formed in the region where the intensity of the third plasma 43 is strong is larger than the diameter of the fourth hole H4 formed in the region where the intensity of the third plasma 43 is weak. The diameter of the fourth hole H4 may be zero.

[0030] The third plasma 43 may have a spatially non-uniform intensity distribution. It is advantageous that the intensity distribution of the third plasma 43 is the same as the intensity distributions of the first and second plasmas 41 and 42. The first to third plasmas 41 to 43 may be generated by the same device.

[0031] After the step using the third plasma 43, the channel layer CX and the second insulating layer I2 are annealed (step S60). The annealing liberates hydrogen from the second insulating layer I2, and some of the liberated hydrogen reduces the oxide semiconductor contained in the channel layer CX. Then, step S10 and subsequent steps are performed in order. The annealing in step S60 and step S30 may be performed in the same step. In other words, the channel layer CX, the first insulating layer I1, and the second insulating layer I2 may be annealed after the step using the first plasma 41 and after the step using the third plasma 43.

[0032] [Embodiment 3] Figure 9 is a perspective plan view showing an example of the configuration of a self-luminous display device according to an embodiment of the present disclosure. The ABCD cross section of Figure 9 is the same as Figure 3. As shown in Figure 9, in a self-luminous display device 1 according to the present disclosure, dehydrogenation holes are not provided near the first channel layer C1 and the second channel layer C2, and the first insulating layer I1 is doped with oxygen. As shown in Figure 3, the self-luminous display device 1 includes a first insulating layer I1 having a first portion P1 in contact with the top surface of the first channel layer C1 and a second portion P2 in contact with the top surface of the second channel layer C2, and the density of oxygen contained in the second portion P2 is lower than the density of oxygen contained in the first portion P1.

[0033] 10 is a cross-sectional view showing an example of a method for manufacturing a self-luminous display device according to an embodiment of the present disclosure. As shown in FIG. 10 , steps S10 and S20 are performed in order. Then, with the entire upper surface of the first insulating layer I1 exposed, oxygen is introduced into the first insulating layer I1 using a first plasma 41 (step S28). This can be achieved by using oxygen as the first plasma 41, and is a so-called "oxygen plasma treatment." In step S28, the stronger the first plasma 41, the greater the amount of oxygen introduced. Specifically, more oxygen is introduced into the first portion P1 located in a region where the first plasma 41 is strong than into the second portion P2 located in a region where the first plasma 41 is weak.

[0034] Then, step S30 is performed. The annealing process liberates oxygen from the first insulating layer I1, oxidizing the oxide semiconductor contained in the channel layer CX. The more oxygen contained in the first insulating layer I1, the more oxygen is liberated, and therefore the more the oxide semiconductor is oxidized. Specifically, due to the difference in the amount of oxygen between the first portion P1 and the second portion P2, the oxide semiconductor contained in the first channel layer C1 is more oxidized than the oxide semiconductor contained in the second channel layer C2. Additionally or alternatively, oxygen reacts with hydrogen, and the more oxygen there is, the less the oxide semiconductor is reduced by hydrogen.

[0035] Subsequently, steps S40, S42, and S44 are performed to remove the template layer 51.

[0036] This manufacturing method also (at least partially) cancels out the effects of the gate length and the degree of reduction of the oxide semiconductor on the transistor threshold, thereby reducing the difference between the designed threshold and the actual threshold of the transistor. Furthermore, it is possible to reduce the difference in threshold between the first transistor T1 formed in a region with a strong plasma intensity and the second transistor T2 formed in a region with a weak plasma intensity.

[0037] 9 and 3 , the self-luminous display device 1 according to the present disclosure may have the second insulating layer 12 doped with oxygen. The self-luminous display device 1 includes the second insulating layer 12 having a third portion P3 in contact with the top surface of the first channel layer C1 and a fourth portion P4 in contact with the top surface of the second channel layer C2, and the density of oxygen contained in the fourth portion P4 is lower than the density of oxygen contained in the third portion P3.

[0038] 11 is a cross-sectional view showing an example of a method for manufacturing a self-luminous display device according to an embodiment of the present disclosure. As shown in FIG. 11 , a second insulating layer I2 is formed on the side opposite the first insulating layer I1, contacting the channel layer CX (step S50). In the example shown in FIG. 11 , the channel layer CX is to be formed on the second insulating layer, and the first insulating layer I1 is to be formed on the channel layer CX. Next, with the entire top surface of the second insulating layer I2 exposed, oxygen is introduced into the second insulating layer I2 using a third plasma 43 (step S58). This can be achieved by using oxygen for the third plasma 43. More oxygen is introduced into the third portion P3, which is located in an area where the intensity of the third plasma 43 is strong, than into the fourth portion P4, which is located in an area where the intensity of the third plasma 43 is weak.

[0039] After the step using the third plasma 43, the channel layer CX and the second insulating layer I2 are annealed (step S60). The annealing liberates oxygen from the second insulating layer I2, oxidizing the oxide semiconductor contained in the channel layer CX. Due to the difference in the amount of oxygen between the third portion P3 and the fourth portion P4, the oxide semiconductor contained in the first channel layer C1 is more oxidized than the oxide semiconductor contained in the second channel layer C2. Additionally or alternatively, oxygen reacts with hydrogen, and the more oxygen there is, the less the oxide semiconductor is reduced by hydrogen. Then, step S10 and subsequent steps are performed in sequence. The annealing steps S60 and S30 may be performed in the same process.

[0040] The present disclosure is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present disclosure. Furthermore, new technical features can be formed by combining the technical means disclosed in each embodiment.

[0041] For example, dehydrogenation holes may be formed only in the insulating layer in contact with the lower surface of the channel layer. For example, oxygen may be doped only in the insulating layer in contact with the lower surface of the channel layer. For example, dehydrogenation holes may be formed in the insulating layer in contact with one surface of the channel layer, and oxygen may be doped in the insulating layer in contact with the other surface.

[0042] REFERENCE SIGNS LIST 1 Self-luminous display device 13 Conductor layer 21, 22 Photoresist layer 31 First pixel circuit 32 Second pixel circuit 41 First plasma 42 Second plasma 43 Third plasma C1 First channel layer C2 Second channel layer CX Channel layer G1, G2, GX Gate electrode H1 First hole H2 Second hole H3 Third hole H4 Fourth hole HX Hole I1 First insulating layer I2 Second insulating layer L1, L2 Gate length OX, OY Opening T1 First transistor T2 Second transistor P1 First portion P2 Second portion P3 Third portion P4 Fourth portion

Claims

1. A self-luminous display device comprising: a first pixel circuit including a first transistor having a first channel layer including an oxide semiconductor; and a second pixel circuit having the same circuit configuration as the first pixel circuit, including a second transistor corresponding to the first transistor and having a second channel layer including an oxide semiconductor, wherein the gate length of the second transistor is longer than the gate length of the first transistor, and the oxide semiconductor included in the second channel layer is more reduced than the oxide semiconductor included in the first channel layer.

2. The self-luminous display device according to claim 1, wherein the first transistor and the second transistor are each a thin film transistor.

3. The self-luminous display device according to claim 1 or 2, wherein the oxide semiconductor contained in the first channel layer and the oxide semiconductor contained in the second channel layer are made of the same material.

4. A self-luminous display device according to any one of claims 1 to 3, wherein a gate electrode of the first transistor and a gate electrode of the second transistor are formed from the same layer, and the first channel layer and the second channel layer are formed from the same layer.

5. A self-luminous display device as described in any one of claims 1 to 4, comprising a first insulating layer having a first portion in contact with an upper surface of the first channel layer and a second portion in contact with an upper surface of the second channel layer, wherein the density of hydrogen contained in the second portion is greater than the density of hydrogen contained in the first portion.

6. A self-luminous display device as claimed in any one of claims 1 to 5, comprising a first insulating layer having a first portion in contact with an upper surface of the first channel layer and a second portion in contact with an upper surface of the second channel layer, wherein the diameter of the second hole penetrating the vicinity of the second portion is smaller than the diameter of the first hole penetrating the vicinity of the first portion.

7. A self-luminous display device as claimed in any one of claims 1 to 4, comprising a first insulating layer having a first portion in contact with an upper surface of the first channel layer and a second portion in contact with an upper surface of the second channel layer, wherein the density of oxygen contained in the second portion is lower than the density of oxygen contained in the first portion.

8. A self-luminous display device as claimed in any one of claims 1 to 7, comprising a second insulating layer having a third portion in contact with the lower surface of the first channel layer and a fourth portion in contact with the lower surface of the second channel layer, wherein the density of hydrogen contained in the fourth portion is greater than the density of hydrogen contained in the third portion.

9. A self-luminous display device as claimed in any one of claims 1 to 8, comprising a second insulating layer having a third portion in contact with the underside of the first channel layer and a fourth portion in contact with the underside of the second channel layer, wherein the diameter of a fourth hole penetrating the vicinity of the fourth portion is smaller than the diameter of a third hole penetrating the vicinity of the third portion.

10. A self-luminous display device as claimed in any one of claims 1 to 7, comprising a second insulating layer having a third portion in contact with the lower surface of the first channel layer and a fourth portion in contact with the lower surface of the second channel layer, wherein the density of oxygen contained in the third portion is lower than the density of oxygen contained in the fourth portion.

11. A method for manufacturing a self-luminous display device, comprising: a step of forming a channel layer including an oxide semiconductor of a transistor; a step of forming a first insulating layer in contact with the channel layer; a step of etching the first insulating layer using a first plasma so as to form a hole penetrating the first insulating layer or a step of introducing oxygen into the first insulating layer; a step of annealing the channel layer and the first insulating layer after the step using the first plasma; a step of forming a conductor layer that will be a material for a gate electrode of the transistor; and a step of etching the conductor layer using a second plasma so as to form the gate electrode of the transistor from the conductor layer.

12. The method of manufacturing a self-luminous display device according to claim 11, wherein the first and second plasmas each have a spatially non-uniform intensity distribution.

13. The method for manufacturing a spontaneous light-emitting display device according to claim 11 or 12, wherein the intensity distributions of the first and second plasmas are identical to each other.

14. The method for producing a self-luminous display device according to any one of claims 11 to 13, wherein the first and second plasmas are generated by a same device.

15. A method for manufacturing a self-luminous display device according to any one of claims 11 to 14, further comprising the step of forming a photoresist layer having a non-penetrating opening on the first insulating layer, and etching the photoresist layer and the first insulating layer with the first plasma.

16. The method for manufacturing a self-luminous display device according to claim 15, wherein the photoresist layer is etched by the first plasma so that the opening penetrates the photoresist layer, and the opening overlaps with the hole in a plan view.

17. A method for manufacturing a self-luminous display device according to any one of claims 11 to 16, wherein oxygen is introduced into the first insulating layer by the first plasma while the entire top surface of the first insulating layer is exposed.

18. The method for manufacturing a self-luminous display device according to any one of claims 17, wherein oxygen is used for the first plasma.

19. The method for manufacturing a self-luminous display device according to any one of claims 11 to 18, further comprising forming the first insulating layer on the channel layer.

20. A method for manufacturing a self-luminous display device as claimed in any one of claims 11 to 19, further comprising the steps of: forming a second insulating layer in contact with the channel layer on the side opposite to the first insulating layer; etching the second insulating layer by a third plasma so as to form a hole penetrating the second insulating layer, or introducing oxygen into the second insulating layer; and annealing the channel layer and the second insulating layer after the step using the third plasma.

Citation Information

Patent Citations

  • Manufacturing method of array substrate

    CN111081551A

  • Method of manufacturing semiconductor device

    JP2011096958A

  • Method of manufacturing semiconductor device

    JP2020010058A

  • Method of transistor matching

    US20120117519A1

  • Method for manufacturing self-aligned thin film transistor

    US20140011329A1