Resource-saving mould for producing continuously cast steel blanks
The use of a nickel-made cylindrical sleeve with protrusions and a two-circuit cooling system employing a nanofluid with AlO3 nanoparticles addresses the limitations of existing crystallizers by enhancing heat transfer and reducing resource consumption, resulting in high-quality, crack-free continuous casting of high-alloy steel billets.
Patent Information
- Application Number
- PCT/RU2023/000096
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-27
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-03
AI Technical Summary
Existing crystallizers for continuous casting of high-alloy steels and alloys face limitations in heat transfer intensity, are prone to crust cracking due to overcooling, and inefficiently use cooling water, leading to reduced productivity and increased resource consumption.
A nickel-made cylindrical sleeve with protrusions and a two-circuit cooling system using a nanofluid with AlO3 nanoparticles, where the first circuit maintains a temperature of 130-150 °C and the second circuit outputs cooling water at 60-70 °C, enhancing heat transfer and reducing cooling medium consumption.
The solution achieves high-quality, crack-free continuous casting with intensified heat transfer, increased crystallizer reliability, extended liner service life, and reduced cooling medium consumption, effectively utilizing high-potential heat for technological purposes.
Smart Images

Figure RU2023000096_03102024_PF_FP_ABST
Abstract
Description
[0001] RESOURCE-SAVING CRYSTALLIZER FOR PRODUCING CONTINUOUS CASTING
[0002] STEEL BLANKS
[0003] Field of technology to which the invention relates
[0004] The invention relates to metallurgy, in particular to continuous casting of metals and alloys.
[0005] State of the art
[0006] A method for controlling the cooling of a crystallizer is known [1. Patent No. 2601713 of the Russian Federation. Stulov V. V. Published 10.11.2016. Bulletin No. 31], which includes heating the walls of the crystallizer before pouring liquid metal, supplying cooling water, cooling the hot water circulating in a closed circuit, which is carried out simultaneously with pouring liquid metal into the crystallizer and after the heating of the walls of the crystallizer has ceased, monitoring the temperature and flow rate of water at the inlet and outlet of the crystallizer, wherein the walls of the crystallizer and the water circulating in a closed circuit and in the channels of the walls of the crystallizer are preheated to a temperature of 150 - 170 °C. The known invention [1] is aimed only at controlling the cooling of the crystallizer.
[0007] A crystallizer for producing continuously cast cylindrical blanks from high-alloy alloys is known [2. Patent No. 2739358 of the Russian Federation. Stulov V. V. Published. 23.12.2020. Bulletin No. 36], comprising a housing with a heat pipe located therein, formed by pipes coaxially installed one inside the other to form a closed space between them for the coolant, a steam condenser connected by steam pipes and condensate pipes to the heat pipe to form a closed evaporation-condensation circuit, electric heating elements, thermocouples connected to the automatic crystallizer cooling control system.
[0008] The disadvantage of the known crystallizer [2] is the limitation of the transferred heat flux density of 3 - 4 MW L 2 during high-speed casting, caused by the boiling crisis of the coolant and the transition from the bubble boiling regime to the film boiling regime with an increase in the temperature of the cooled wall.
[0009] A crystallizer for producing slab blanks is known [3. Patent No. 2748425 RF. Stulov V.V. Published. 05.25. 2021. Bulletin No. 15], containing four longitudinal walls arranged in pairs, vertical channels for cooling water, thermocouples installed in the vertical channels of the longitudinal walls and connected to the automatic cooling control system of the crystallizer, and the working part of the walls is made in the form of a nickel sheet, the thickness of which "b" and thermal conductivity "A" are related by the ratio b / L = (0.83 - 1) 10 4 m 2 °C / W. The known crystallizer [3] is intended only for obtaining slab blanks.
[0010] A sleeve crystallizer for high-speed casting is known [4. Patent No. 2152843 RF. Pankin VB et al. Published 20.07.2000. Bulletin No. 20], containing a square or rectangular sleeve with an internal cavity open at both ends, a gap for the passage of cooling water and cooling elements on the outer surface of the sleeve, the upper funnel-shaped part of which on the side of metal pouring is made in cross-section in the form of bulges on four walls and in the form of rectilinear side sections near the rounded corners of the walls.
[0011] The disadvantage of the known crystallizer [4] is that it is not intended for high-speed casting of blanks from highly alloyed steels and alloys, as well as for resource conservation due to the possible cracking of the forming crust of the blank due to overcooling of the metal in the crystallizer. In addition, the direction of the low-potential cooling water leaving the crystallizer into a cooling tower or refrigerator generally reduces the efficiency of using the crystallizer.
[0012] Disclosure of the essence of the invention
[0013] The technical task is to create a reliable and efficient crystallizer aimed at implementing high-speed continuous casting and obtaining high-quality cylindrical blanks, including those with a diameter of more than 150 mm, from high-alloy steels and alloys, ensuring high intensity of the heat transfer process from the surface of the liner, a long service life of the liner, a reduction in the overall consumption of the cooling medium by 2-2.5 times, as well as the use of high-potential heat of cooling water with a temperature of 60-70 °C for technological needs.
[0014] The technical result consists in obtaining high-quality, crack-free continuously cast blanks from steels and alloys, intensifying the process of heat transfer from the surface of the liner, increasing the reliability and efficiency of using the crystallizer, increasing the service life of the liner, reducing the consumption of the cooling medium, and using the high-potential heat of the cooling water for technological needs.
[0015] The technical result is achieved due to the fact that the crystallizer for producing continuously cast steel blanks contains a cylindrical sleeve with an internal cavity open at both ends, a slit gap for the passage of a cooling medium, thermocouples connected to the automatic control system of the crystallizer operation, while the sleeve is made of nickel with a wall thickness of 5 - 7 mm, on the outer surface of which protrusions are made with a depth of 0.6 - 0.7 mm, a width of 0.3 - 0.5 mm and a distance between the protrusions of 0.4 - 0.6 mm, and a nanofluid with AlO3 nanoparticles in an amount of 1 - 3% is used as a cooling medium for the crystallizer sleeve.
[0016] In addition, the crystallizer contains two cooling circuits, wherein the temperature of the cooling medium in the first cooling circuit of the crystallizer sleeve is 130 - 150 °C, and the temperature of the outgoing cooling water in the second cooling circuit is 60 - 70 °C.
[0017] Brief description of the drawings
[0018] Fig.1 - Cylindrical sleeve;
[0019] Fig.2 - Cylindrical sleeve, section A - A;
[0020] Fig.3 - Diagram of connection of the crystallizer to the closed circuit of circulation of the cooling medium.
[0021] Implementation of the invention
[0022] The resource-saving crystallizer in Fig. 1-3 consists of a cylindrical sleeve 1 with an internal cavity, walls 2 with projections 3, a housing 4 of the sleeve with pipes 5 and 6 for supplying and removing a cooling medium, a slot gap 7 for the passage of a cooling medium, a pump 8 for pumping the medium, an electric heater 9, connecting pipelines 10, a heat exchanger 11 with pipes 12 and 13 for cold water, slot channels 14 and 15 for a cooling medium and cold water, respectively, thermocouples 16-20 connected to the automatic control system of the crystallizer operation.
[0023] The cylindrical sleeve is made of nickel with a wall thickness of 5 - 7 mm, on the outer surface of which there are projections with a depth of 0.6 - 0.7 mm, a width of 0.3 - 0.5 mm and a distance between projections of 0.4 - 0.6 mm with an internal cavity.
[0024] The crystallizer contains two crystallizer cooling circuits, the temperature of the cooling medium in the first cooling circuit of the sleeve is t B = 130 -150 °C; temperature of the outgoing cooling water in the second cooling circuit t B = 60 - 70 °C.
[0025] A nanofluid with AlO3 nanoparticles is used as a cooling medium for cooling the sleeve in the first cooling circuit of the crystallizer; the amount of AlO3 nanoparticles in the nanofluid is n = 1 - 3%.
[0026] The crystallizer works as follows.
[0027] The crystallizer, connecting pipelines, and heat exchanger included in the first circulation circuit are preliminarily filled with a cooling medium. Electric heater 9 and pump 8 for circulation of the cooling medium are switched on. After reaching the specified heating temperature of the cooling medium and the crystallizer sleeve, recorded by the readings of thermocouples 19 and 16, the electric heater 9 is switched off by the automatic control system of the crystallizer operation. At the same time, the melt is poured into the internal cavity of the cylindrical sleeve 1 and the supply of cold water through the branch pipe 12 to the heat exchanger 11 is switched on. The cooling medium passing in the slit gap 7 of the crystallizer removes heat from the projections 3, transferred from the melt to the wall 2 of the cylindrical sleeve 1 with a temperature recorded by the reading of the thermocouple 16.
[0028] The temperature of the circulating cooling medium is controlled by the readings of thermocouples 19 and 20, and the temperature of the cooling cold water is controlled by the readings of thermocouples 17 and 18. The cooling medium from the pipeline through the branch pipe 5 enters the body 4 of the crystallizer and is removed from it through the branch pipe 6 into the heat exchanger 11 for cooling with cold water. In the heat exchanger 11, when the cooling medium moves in the slot channel 14, heat is transferred to the cold water moving in the slot channel 15. By regulating the flow rate of cold water entering the heat exchanger 11 through the branch pipe 12, its heating to a temperature of 60 - 70 °C is achieved, which is recorded at the outlet from the branch pipe 13 according to the reading of the thermocouple 18. The cold water heated in this way passes into high-potential water and is further used for technological needs.
[0029] The cause-and-effect relationship between the set of essential features of the claimed crystallizer and the achieved technical result is as follows.
[0030] Manufacturing of a cylindrical sleeve made of nickel with a wall thickness of b г = 5 - 7 mm increases its service life several times compared to a sleeve made of copper. Additionally, a nickel sleeve is designed for operation at higher temperatures of the working surface (more than 300 - 350 °C), compared to the temperature of a sleeve (no more than 200 °C) made of copper. Due to this, it is possible to achieve a significant reduction (by hundreds of °C) in the temperature gradient At between the temperature of the poured melt and the temperature of the sleeve, eliminating the occurrence of stresses that lead to cracking of the workpiece crust.
[0031] Reducing the wall thickness of a cartridge case made of nickel, 5 Г < 5 mm leads to the possibility of its deformation during high-speed steel casting, as well as to a limitation of its service life before repair due to wear of the working surface.
[0032] Increasing the wall thickness of a sleeve made of nickel, 5 Г > 7 mm leads to an unreasonable increase in its mass and cost, as well as to an unreasonable increase in its thermal resistance b г A (where L is the thermal conductivity of nickel), causing a significant increase in temperature on its working surface.
[0033] The implementation of protrusions on the outer surface of the sleeve in contact with the cooling medium with a height of h = 0.6 - 0.7 mm, a width of b = 0.3 - 0.5 mm and a distance between the protrusions of I = 0.4 - 0.6 mm allows to increase (more than 2 times) the cooling surface area of the sleeve and the amount of heat removed by the cooling medium, and also allows to intensify the process of heat transfer from the surface of the sleeve. Reducing the height of the protrusions on the outer surface of the sleeve h < 0.6 mm does not allow to intensify the process of heat exchange from the surface of the sleeve with the cooling medium to the required extent.
[0034] Increasing the height of the protrusions h > 0.7 mm leads to an inappropriate reduction in the wall thickness of the sleeve b г and reducing its service life.
[0035] Reducing the width of the protrusions b < 0.3 mm makes their manufacture difficult and reduces strength.
[0036] Increasing the width of the protrusions b > 0.5 mm leads to an inappropriate reduction in the heat exchange surface area of the sleeve and a reduction in the amount of heat removed from it.
[0037] Reducing the distance between the protrusions I < 0.4 mm complicates their manufacture and does not lead to a significant increase in the intensity of heat exchange of the cooling medium with the sleeve.
[0038] Increasing the distance between the protrusions I > 0.6 mm leads to a decrease in the intensity of heat exchange between the sleeve and the cooling medium and an inappropriate decrease in the heat exchange surface area.
[0039] The use of a nanofluid with Al2O3 nanoparticles as a cooling medium for the sleeve at a concentration of 1-3% of the total volume of the cooling medium allows for a significant (by 30-50%) increase in the intensity of heat transfer from the sleeve and the amount of heat removed from its surface by the cooling medium.
[0040] A decrease in the amount of nanoparticles in the nanofluid n < 1% leads to a slight increase in the intensity of heat transfer of the sleeve and the amount of heat removed from its surface.
[0041] An increase in the amount of nanoparticles in a nanofluid n > 3% leads to an unreasonable increase in the costs of preparing the nanofluid, an increase in its density and energy costs for pumping the nanofluid.
[0042] The implementation of a crystallizer with two cooling circuits allows for the heating of the shell walls to a temperature of over 100 °C in the first cooling circuit before pouring the melt and reduces the temperature difference between the crust temperature of the formed blank and the melt, which reduces the likelihood of crust cracking. The use of a second cooling circuit allows for heat to be removed from the cooling medium heated in the crystallizer during melt pouring.
[0043] The use of a superheated cooling medium circulating in the first cooling circuit of the crystallizer sleeve allows for an additional increase in the intensity of sleeve cooling and improvement of the surface quality of the resulting blanks.
[0044] Reduction of the cooling medium temperature t c< 130 °C, circulating in the first cooling circuit of the crystallizer sleeve, does not allow a significant increase in the intensity of heat transfer on the surface of the sleeve without increasing the speed of the cooling medium, compared with the heat transfer coefficient of cold water (t B = 15 - 35 °C) at the same speed. Higher thermophysical properties of the heated cooling medium (t c = 130 - 150 °C) compared to cold water determines a higher value of the heat transfer coefficient of the cooling medium on the surface of the crystallizer sleeve. An increase in the temperature of the cooling medium t c> 150 °C, circulating in the first cooling circuit of the crystallizer sleeve, leads to an inappropriate increase in pressure in the first circuit and the need to increase the thickness of the pipeline walls, increase the requirements for the design of the pumping pump, increase the power of the electric heater for heating the cooling medium before pouring the melt. A decrease in the temperature of the outgoing cooling water in the second cooling circuit t B < 60 °C leads to an increase in the water flow to the heat exchanger in order to remove the required amount of heat supplied by the cooling medium, as well as to the likelihood of the water reaching low-potential heat in the second cooling circuit and to a decrease in the thermal work of the crystallizer. An increase in the temperature of the outgoing cooling water in the second cooling circuit t B > 70 °C leads to increased requirements for the purity of cooling water in order to prevent intensive formation of salt deposits on the walls of pipelines.
Claims
CLAUSES OF THE INVENTION 1. A crystallizer for producing continuously cast steel blanks, comprising a cylindrical sleeve with an internal cavity open at both ends, a slit gap for the passage of a cooling medium, thermocouples connected to an automatic control system for the operation of the crystallizer, characterized in that the sleeve is made of nickel with a wall thickness of 5 - 7 mm, on the outer surface of which projections are made with a depth of 0.6 - 0.7 mm, a width of 0.3 - 0.5 mm and a distance between projections of 0.4 - 0.6 mm, wherein a nanofluid with AlO3 nanoparticles in an amount of 1 - 3% is used as a cooling medium for the crystallizer sleeve.
2. The crystallizer according to claim 1, characterized in that it contains two cooling circuits, wherein the temperature of the cooling medium in the first cooling circuit of the crystallizer sleeve is 130 - 150 °C, and the temperature of the outgoing cooling water in the second cooling circuit is 60 - 70 °C. 7
Citation Information
Patent Citations
Crystallizer for casting copper pipe
CN202667574U
Ingot-forming equipment
RU2374032C2
Method of injection steam-evaporation cooling of tube-type mould
RU2411105C1
Mould for production of continuously cast cylindrical billets
RU2556167C2
Method of crystallizer cooling
RU2601713C2