Biodegradable composite structure for use as artificial leather
A biodegradable composite structure for artificial leather, composed of a water-dispersible polymer cover layer, biodegradable polymer lining, and textile carrier, addresses the non-biodegradability of conventional artificial leather by achieving high abrasion resistance and compostability, enabling environmentally friendly disposal.
Patent Information
- Application Number
- PCT/EP2024/059044
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-14
- Filing Date
- 2024-04-03
- Publication Date
- 2024-10-17
AI Technical Summary
Conventional artificial leather composite structures are non-biodegradable, leading to disposal challenges, with materials often requiring thermal recycling due to inseparable layers, whereas there is a growing need for biodegradable materials that maintain mechanical properties and abrasion resistance.
A completely biodegradable composite structure comprising a cover layer of water-dispersible biodegradable polymer, a lining layer of biodegradable polymer composition, and a fabric layer of biodegradable textile carrier material, achieving at least 50% degradation within 6 months, with suitable polymers like polybutylene adipate terephthalate and polybutylene succinate providing stability and abrasion resistance.
The composite structure achieves high mechanical and usage properties while being fully biodegradable, suitable for composting, and maintains abrasion resistance comparable to conventional artificial leather, ensuring environmentally friendly disposal and industrial compostability.
Smart Images

Figure IMGF000008_0001 
Figure IMGF000021_0001 
Figure IMGF000022_0001
Abstract
Description
[0001] Description
[0002] Biodegradable composite for use as artificial leather
[0003] The present invention relates to fully biodegradable composite structures which are in particular flat and can be made up as artificial leather, wherein the composite structures have a cover layer formed from a biodegradable polymer as a polymeric component, a lamination layer made from a biodegradable polymer composition and a fabric layer formed from a biodegradable textile carrier material, and wherein the cover layer is made from a water-dispersible or emulsifiable, biodegradable polymer.The present invention further relates to methods for producing such composite structures, wherein the composite structures can be provided with a desired surface structure, methods for composting such composite structures and methods for separating layers of such a composite structure, wherein the composite structure is treated with an organic solvent which selectively dissolves one or more of the layers of the composite structure.
[0004] State of the art
[0005] Composite structures are structures made of composite materials that are obtained by combining different materials and whose chemical, physical, and other properties exceed those of the individual components. Composite materials include textile composites, nonwovens, laminates (i.e., materials bonded together in a sandwich arrangement by bonding or lamination, such as plywood, composite films, and laminates), and artificial leather.
[0006] Artificial leather is a multi-layer, flexible composite structure comprising a polymer surface layer and a carrier material, particularly made of textile, nonwoven, or a foamed material, e.g., PVC, polyolefin (especially in the form of TPO), or polyurethane. The polymeric top layer is responsible for abrasion and fabric resistance and determines the appearance, while the carrier provides the desired strength and elasticity. Polyurethanes, among others, are used as coating polymers, although a basic distinction is made between one-component and two-component coating systems.
[0007] EP 1 059 379 B1 describes, by way of example, the production of a composite structure with a polyurethane cover layer, wherein the polyurethane is obtained by reacting diisocyanates and / or a diisocyanate prepolymer with bifunctional and trifunctional polyols. The use of the trifunctional polyol in EP 1 059 379 B1 ensures that a composite structure with sufficient resistance is obtained, but in individual cases, it can result in the composite structure lacking the desired flexibility and also exhibiting undesirable brittleness.
[0008] Another patent application dealing with the production of conventional synthetic leather is EP 1 927 466 B1, which uses a coating composition consisting of an aliphatic polyol and a polyisocyanate as the top layer. The polyol used in EP 1 927 466 B1 has at least two CH2 groups terminal to the OH group and is sufficiently reactive to be processed together with the polyisocyanate as a reactive coating composition.
[0009] The resulting conventional synthetic leathers are characterized by high durability and longevity. While these properties are desirable for the synthetic leather's intended use, they pose a significant problem for its disposal, as the individual materials can usually no longer be separated from one another, and thermal recycling through incineration or gasification is often the only option for disposing of the materials after their intended use.
[0010] In recent years, the need and demand for materials derived from renewable resources and materials that can be reused more quickly and efficiently after use have increased significantly. Therefore, increased efforts have been made to at least partially replace the generally non-biodegradable raw materials in synthetic leather with biodegradable raw materials, with the aim of using renewable raw materials for the production of synthetic leather wherever possible. However, since there is no willingness to accept compromises in the performance properties of synthetic leathers constructed in this way, the production of such synthetic leather presents a major challenge.
[0011] Examples of bio-based synthetic leathers that are not derived from animal skin include pineapple leather (e.g., known under the brand "Pinatex®"), cork-based leather, apple leather, wine leather, cactus leather, and mushroom leather. Another new, bio-based synthetic leather based on hemp, called "LOVR™," has been proposed by a small start-up (Revoltech), but is not yet available on the market.
[0012] DE 42 28 779 describes a composite material consisting of a foam in the form of a hardened starch foam and another material, which may be, among other things, artificial leather. However, in this composite material, only the starch foam is biodegradable, and it is also said to be designed as a solid foam, thus preventing the tactile impression of artificial leather.
[0013] DE 102020210811 A1 describes an artificial leather comprising a plastic layer and / or a textile carrier made of a biodegradable biopolymer, which degrades to a powder of at least 50% within a maximum of 28 days when stored above 70°C and at a humidity of at least 80%. According to DE 102020210811 A1, both layers of such an artificial leather can also be formed from such a biodegradable biopolymer. DE 102020210811 A1 proposes, in particular, PLA (polylactic acid) as the cover layer material, which can be processed into a layer by calendering or extrusion. Against this background, there is a need for flat composite structures, particularly for use as artificial leather, which are characterized by good mechanical properties and high abrasion resistance, but which can be treated in such a way that they can be biodegraded as extensively as possible within an acceptable period of time.Preferably, these composite structures should be compostable at least in industrial composting facilities.
[0014] The present invention addresses this need.
[0015] Description of the invention
[0016] In the investigations underlying this application, it was surprisingly discovered that such biodegradable composite structures can be obtained by combining a cover layer formed from a biodegradable polymer as the polymer component, a lamination layer made of a biodegradable polymer composition, and a fabric layer formed from a biodegradable textile carrier material, while simultaneously ensuring that the composite structure has favorable mechanical and performance properties. Water-dispersible or water-emulsifiable biodegradable polymers are used for the cover layer, which can be easily processed and dried as a polymer dispersion.
[0017] According to a first aspect, the present invention accordingly relates to an at least three-layer, fully biodegradable composite structure, in particular in the form of an artificial leather, which comprises a cover layer formed from a biodegradable polymer as the polymeric component, a lamination layer formed from a biodegradable polymer composition, and a fabric layer formed from a biodegradable textile carrier material, wherein the cover layer is made from a water-dispersible, biodegradable polymer. In the context of the invention described here, the term "biodegradable" refers to the fact that the organic material can be biologically degraded, so that CO2, H2O, biomass, and mineral salts are released under aerobic conditions, or CO2, methane, biomass, and mineral salts under anaerobic conditions.According to the invention, using the standardized measurement method according to DIN EN 14046:2016 (also published under the designation DIN EN ISO 14855:2013 "Determination of ultimate aerobic biodegradability of plastic materials under controlled composting conditions"), a degradation rate of at least 50% within 6 months, preferably at least 70%, and more preferably at least 90% within 6 months, is to be achieved. The degradation rate is determined gravimetrically according to DIN EN ISO 14855-2.
[0018] "Biodegradable" in the context of the composite structure according to the invention means that only either biodegradable or biocompatible components are included. "Biocompatible" in the context of the invention described here refers to substances that are not degraded, but also do not exhibit any adverse effects on microorganisms that degrade biodegradable components in the composite structures, and do not negatively affect the quality of the resulting compost (determination of ecotoxicity according to OECD Guideline 208). "Fully biodegradable" refers to the fact that all layers of the composite structure are biodegradable within the meaning of the above definition, i.e., that the layers are made of biodegradable and / or biocompatible components, and that the biodegradable components achieve a degree of degradation of at least 50% within 6 months under the conditions specified in DIN EN ISO 14855:2013.
[0019] "Water-dispersible" means that a stable aqueous dispersion of the polymer can be formed in water. The dispersion can be stabilized by ionic functional groups in the polymer or by the addition of dispersion-stabilizing additives. If such additives have been used, they are detectable in the top layer even after drying and solidification. Particle sizes can typically range from a few nanometers (2 nm) to a few micrometers (10 pm). In emulsions, particles from polymeric raw materials are converted, for example, by grinding, to the desired fineness, which can be in the range from 100 nm to several hundred micrometers (500 pm), preferably in the range from 250 nm to 100 pm, and more preferably in the range from 250 nm to 80 pm. These particles can be kept suspended in the aqueous medium by emulsifiers, but are not necessarily contained in the medium.
[0020] Biodegradable polymers that can be used to produce the cover layer are known to those skilled in the art, and in principle, any biodegradable polymer that can provide the necessary stability properties, such as high abrasion resistance, can be used to produce the cover layer. Particularly suitable biodegradable polymers for producing the cover layer are those selected from the following group: polyester polyurethanes, polybutylene adipate terephthalate (PBAT),
[0021] Polybutylene succinate, polybutylene succinate adipate, cellulose, cellulose acetate, polycaprolactone, polyhydroxyalkanoates, especially in the form of poly-3-hydroxybutyrate (P3HB), poly-4-hydroxybutyrate (P4HB), polyhydroxyvalerate (PHV), polyhydroxyhexanoate (PHH), or polyhydroxyoctanoate (PHO), and polyhydroxyalkanoate copolymers, especially in the form of P3HB4HB, P3HB3HV, P3HB3HV4HV, P3HB3Hx, P3HB3HO, or P3HB3HD, polylactic acid, polyvinyl alcohol, starch, and other natural polymers and mixtures thereof. Suitable polyester polyurethanes include, in particular, anionic aliphatic polyester polyurethanes, such as the products commercially marketed by Covestro as Impranil DLN.
[0022] Preferred top layer polymers are polybutylene adipate terephthalate, polybutylene succinate, polybutylene succinate adipate, and mixtures thereof. A particularly suitable polymer for the top layer is polybutylene adipate terephthalate, as this material is stable to isopropanol and can provide a disinfectable surface. Polybutylene adipate terephthalate also exhibits properties comparable to polyethylene terephthalate (PET), and colorants such as pigments or carbon black can be easily and homogeneously incorporated into the polymer.
[0023] The polymers mentioned are used as an aqueous dispersion, which can be applied to a suitable substrate and forms the top layer after the water has evaporated.
[0024] The polymer in the top layer can be uncrosslinked or crosslinked by adding a suitable additive. For crosslinking, the polymer can, for example, contain functional OH groups, which can be crosslinked by adding polyepoxides, which should also be biodegradable. Such polyepoxides include, for example, epoxidized vegetable oils such as soybean oil, linseed oil, rapeseed oil, castor oil, or karanja oil. Other biodegradable polyepoxides that can be used are based on vanillyl alcohol or phloroglucinol. These polyepoxides contain aromatic components.
[0025] It is also possible to achieve crosslinking indirectly through ionic interactions and the inclusion of alginates and polyvalent cations. Alginates are salts of polyalginic acid, i.e., anionic polysaccharides that contain one carboxyl group per sugar unit. They consist of the monomer subunits D-mannuronic acid and L-guluronic acid in varying ratios, as shown schematically below.
[0026] Depending on the polymer chain length and pH value, these polymers are soluble in water and sometimes significantly increase the viscosity.
[0027] Alginates here include not only non-functionalized alginates but also functionalized alginates, especially those functionalized with ethylene glycol. Ethylene glycol-functionalized alginates can be functionalized with an ethylene glycol monomer or polymer, preferably an ethylene glycol oligomer, which are attached to the alginate, particularly as side groups.
[0028] To provide the desired crosslinking, the alginate is formulated as a salt with a metal or ammonium cation. This mixture is then mixed, for example, with an aqueous polyurethane dispersion and then processed into a layer and dried. The metal cation can preferably be a multivalent, particularly divalent, metal cation or a mixture thereof. Suitable multivalent, particularly divalent, metal cations are calcium and magnesium. When using combinations of alginates and multivalent cations, in contrast to conventional crosslinking, the polymer itself is not crosslinked; rather, a network of alginate and the multivalent cations is created, in which the polymer is present in the free spaces of the network.
[0029] The polymer is generally the essential component of the cover layer and advantageously makes up at least 60% by weight, preferably at least 70% by weight and more preferably about 75 to 98% by weight of the total weight of the cover layer, based on the dry weight.
[0030] In addition, as already mentioned, the top layer can in particular contain colorants in order to impart a color to the top layer that is different from transparent. Pigments and other colorants that can be used by the person skilled in the art for such coloring are readily familiar to the person skilled in the art, with carbon black, which is biodegradable, e.g. Xfast® Black 0066 from BASF or Algae Black Pigment™ Grade J1 from Living Ink Technologies, being an example here as a colorant for imparting a black color impression, and calcium carbonate, which can be mentioned as a colorant for imparting a white color impression. Other colorants that can be incorporated into the top layer to color it include phycocyanins or effect pigments, such as those in the form of glitter (e.g. SiLiglam NATURE, SiLiglam PURE NATURE or SiLiglam PURE Bio Sparkle from Sigmund Lindner), which are biodegradable, or iron oxides, which are biocompatible.
[0031] The colorant is advantageously incorporated into the topcoat in an amount suitable for imparting the desired color impression, with an amount in the range of 0.5 to 20 wt.%, in particular 4 to 10 wt.%, and particularly preferably 5 to 8 wt.% being particularly suitable. The weight specifications also refer to the dry weight of the topcoat.
[0032] Other additives that can be incorporated into the top layer of the biodegradable composite structure according to the invention include, for example, biodegradable defoamers such as BYK-1740 or biodegradable dispersing additives such as Schwego® wett 6267 and 8319 (Schwegmann), TEGO® Dispers 658 (Evonik), or Emulan® TO 2080 (BASF). Another class of additives that can be incorporated into the top layer are plasticizers, e.g., cardanol (CD, renewable natural cashew nutshell), triethyl citrate (TEC), acetyl tributyl citrate (ATBC), epoxidized soybean oil (ESO), L-lactide, polyethylene glycols (PEGs), glycerin, triacetin, sorbitol, or Polysorb® ID46 (Roquette). By selecting the plasticizers, the glass transition temperature can be reduced to a range of approximately -40 to +30 °C, and the formation of crystal structures can be prevented, thus preventing stress whitening, which can occur when bending crystalline materials.Carbonates based on calcium, magnesium, or other metals, as well as oxides, can be incorporated into the top layer as fillers. Thickeners can also be incorporated into the top layer of the biodegradable composite structure according to the invention, particularly in the form of alginate thickeners in combination with monovalent metal cations such as sodium or potassium, or ammonium ions.
[0033] The cover layer in the composite structures according to the invention is formed with a thickness that provides sufficient mechanical strength against external influences. On the other hand, the skilled person will strive to limit the thickness of the cover layer to a necessary level, because, for example, a soft impression comparable to leather cannot be conveyed by a compact cover layer. It is therefore preferred if the cover layer has a basis weight in the range of 10 to 200 g / m 2 and preferably 30 to 100 g / m 2is formed. With the compact surface layer and a density of the dry surface layer material of about 1-1.3 g / cm 3 This results in preferred cover layer thicknesses in the range of approximately 10 to 260 pm and more preferably 30 to 130 pm.
[0034] As already mentioned, the cover layer is preferably formed as a compact layer (i.e. without relevant gas inclusions).
[0035] The "laminating layer" in the composite structure according to the invention has the task of connecting the cover layer, or a further layer applied thereon, to the biodegradable textile carrier material. The connection to the biodegradable textile carrier material can be achieved by applying a laminating compound in liquid form to this layer, and then at least partially embedding the textile carrier material in the laminating layer. By solidifying the laminating compound, e.g. by evaporating a solvent or dispersant (water), the textile is subsequently anchored by the laminating layer to the cover layer or to a further layer applied thereon. The laminating compound therefore does not necessarily have to be a pressure-sensitive adhesive, since adhesion can also be achieved mechanically through partial embedding.Adhesive webs or nonwovens can also be used, which melt at a defined temperature and bond the polymer layers to the textile carrier under pressure. These are also used as hot-melt adhesives. Depending on the polymer chain length, the degradable polymers listed above can also be used.
[0036] In the context of the invention described here, the lamination layer is preferably formed by a biodegradable polymer, which can also be used in the cover layer. Since the lamination layer generally has no visible function in the composite structure according to the invention, it is also preferred if it is formulated without coloring agents. Thus, in one embodiment, the lamination layer can be formed solely by a biodegradable polymer or a mixture of several biodegradable polymers.
[0037] In another embodiment, the lamination layer contains a biodegradable polymer and a biocompatible flame retardant. Examples of such biocompatible flame retardants include calcium alginate or metal hydroxides such as aluminum hydroxide or magnesium hydroxide, zeolites, clays, or silicas.
[0038] Additives that promote the growth of bacteria and microorganisms can be used in the top film, foam, or intermediate layer, as well as in the lamination layer. These can include, for example, sugar, proteins, compost accelerators (nitrogen compounds, potassium, but also lime, various trace elements, and horn or bone meal), as well as cellulose components.
[0039] In principle, all of the biodegradable polymers listed above as suitable for the cover layer can be used for the lamination layer. In a particularly preferred embodiment, polybutylene adipate terephthalate is used as the biodegradable polymer in the lamination layer, which is processed in particular as an aqueous dispersion.
[0040] The third component of the composite structure according to the invention is the biodegradable textile carrier material. Biodegradable textile carrier materials are readily known and familiar to those skilled in the art, and in principle any known biodegradable textile carrier material can be used to produce the composite structures according to the invention. Preferred biodegradable textile carrier materials in the context of the invention described here are textile carrier materials made of PBAT, polyvinyl alcohol, polylactide (PLA), cotton, cellulose, or other renewable raw materials, in particular selected from flax fibers, hemp fibers, pineapple fibers, or wool. It is also possible for the biodegradable textile carrier material to be a biodegradable spacer fabric in which the fibers are not regularly arranged.
[0041] In one embodiment, the biodegradable composite structure according to the invention is formed with a transparent cover layer and lamination layer, through which the underlying biodegradable textile carrier material is visible. In this case, the lamination layer and the cover layer are formulated without transparency-limiting additives or gas bubbles. To impart the desired resistance to external mechanical stresses, the cover layer in such a composite structure can also be thicker than stated above, e.g., with a basis weight in the range of 100 to 300 g / m². 2 or 150 to 280 g / m 2 .
[0042] In another preferred embodiment, the composite structure according to the invention comprises a foam layer between the cover layer and the lamination layer, which imparts a softer tactile impression to the composite structure. This foam is preferably a foam based on a biodegradable polymer that is mixed with a gas and applied as a foam, with the foam layer forming upon solidification.
[0043] The polymers mentioned above for the cover layer can be used as the biodegradable polymer in the foam layer. The content of the biodegradable polymer in the foam layer is usually lower than in the cover layer, especially if the foam layer contains flame-retardant components, and is preferably in the range of 30 to 70 wt.% and particularly preferably in the range of 45 to 65 wt.%, based on the dry weight of the foam layer. Furthermore, the additives mentioned above as optional for producing the cover layer can also be used in the foam layer. Preferred fillers for the foam layer are polymer powders, such as PBAT powder, calcium carbonate, clays, or zeolites. Furthermore, it is preferred to include a thickener, especially an alginate thickener, and most preferably sodium alginate, in the foam layer.Furthermore, a biodegradable soap or foaming agent can be added to the foam layer. Examples include stearates, which may contain sodium, potassium, or nitrogen compounds such as ammonia as counterions. Ammonium stearates, in particular, exhibit good degradability.
[0044] The foam typically has a density that differs significantly from that of a compact layer such as the top layer, ensuring that the foam can be easily compressed when a force is applied. The lower density also ensures that the composite structure is comparatively lightweight. To provide favorable haptic properties, the density of the foam layer can therefore be advantageously between 200 and 900 g / m². 3 and is preferably between 300 and 800 g / m 3In a particularly preferred embodiment, the foam is designed as an open-pore foam, which creates a softer feel and has the additional advantage of increased biodegradability of the composite structure. This results from the fact that degrading bacteria can easily penetrate the foam through the open pores and decompose it from within.
[0045] The foam layer can also be constructed compactly and is thus described as an intermediate coat. Density differences can be the same or greater than those in the top coat, depending on the filler content.
[0046] For the production of the foam layer, suitable additives can be added to the foam composition, in particular biodegradable foam stabilizers such as Ortegol P1 (Evonik), sodium cocoyl isethionate (Pureact I-78C from Innospec) or ammonium stearate, which is commercially available, for example, under the name Stokal STA (Bozzetto). If the composite structure according to the invention has a foam layer, it is preferred if this is thicker than the cover layer and the lamination layer. Thus, it is advantageous if the foam layer has a basis weight in the finished composite structure that is 1.5 to 5 times the basis weight of the cover layer and / or the adhesive layer. It is particularly preferred if the basis weight of the foam layer is 2.5 to 4 times the basis weight of the cover layer and / or the lamination layer. In particular, the foam layer in the composite structures according to the invention can have a basis weight in the range of 20 to 500 g / m3 The biodegradable textile carrier can have an even higher weight in the composite structure than the foam layer and, in one embodiment, can make up 5 to 80% by weight, preferably 30-70%, of the total weight of the composite structure according to the invention.
[0047] Due to the potentially higher basis weight, additives can be advantageously incorporated into the foam layer to improve flame behavior. In particular, the substances already mentioned in connection with the lamination layer can be used. Furthermore, other additives that are typically used to optimize and control the properties of such foams can be incorporated into the foam layer. Examples of suitable crosslinkers include the ionic crosslinking systems already described in connection with the top layer, or crosslinking through a combination of epoxides and OH groups contained in the polymer of the foam layer.
[0048] The thickness of an existing foam layer is adjusted within a suitable range, whereby this thickness usually lies in the range of 0.1 to 1 mm, preferably 0.15 to 0.6 mm and more preferably 0.2 to 0.4 mm.
[0049] To convey an advantageous aesthetic visual impression, it is further preferred if the cover layer has a textured or grained surface structure. The structure can be a regular structure, such as a pattern. In the context of the invention described here, a grain refers to a surface structure that the user associates with the appearance of the top surface of animal leather, or a surface structure that the user connects with the appearance of split leather. Such structuring lends the composite structure the advantageous impression of leather.
[0050] In addition to the components specifically explained above in connection with the description of the layers, all of the aforementioned layers may also contain additives that support the biological degradation of the layers by bacteria. Such substances include, in particular, starch, modified starches, yeasts or yeast extracts, or salts, particularly in the form of ammonium, phosphate, magnesium, calcium, and iron salts, as well as nitrate or sulfate salts.
[0051] The composite structures described above are biodegradable and already exhibit high abrasion resistance even without an additional coating layer. Furthermore, these composite structures are relatively easy to manufacture, as each layer can be created through a simple painting / coating process followed by drying.
[0052] To improve and optimize the final properties, it may still be advisable to modify the composite structures with one or more coating layers. Suitable materials for forming such coating layers (it should be noted that the coating layers should also be biodegradable) include inorganic-organic hybrid polymers such as those available under the name bioORMOCER®, as well as coatings based on biopolymers, particularly hemicellulose, and / or polyvinyl alcohol.
[0053] If the composite structure according to the invention contains lacquer layers, it is preferred if the number of lacquer layers is not greater than four; particularly preferably, the composite structure according to the invention comprises one or two lacquer layers.
[0054] For the composite structure according to the invention, it is further preferred if it is not only biodegradable but also compostable according to DIN EN 14995:2003. This ensures that the composite structure can be decomposed in industrial composting facilities within a reasonable time. With regard to performance properties, it is further preferred, particularly if the composite structure is synthetic leather, that the composite structure has an abrasion resistance according to DIN EN 5470-2 of at least 50,000 cycles and more preferably at least 100,000 cycles of Martindale abrasion. Furthermore, it is preferred if the composite structure according to the invention is non-flammable according to FMVSS 302 through the use of suitable flame retardants and textiles.
[0055] The biodegradable composite structure according to the invention can also be combined with a hook-and-loop fastener, which can also be made of a biodegradable material. Such a construction makes it possible for layers attached to the composite structure to be selectively replaced via the hook-and-loop connection, or for the composite structure itself to form the replaceable layer and be attached to a substrate via the hook-and-loop fastener.
[0056] To further improve biodegradability, it is also possible to specifically weaken the composite structure according to the invention by using structuring systems such as mechanical perforation, laser ablation or water jet cutting in order to introduce a defined local degradability or predetermined breaking points.
[0057] The composite structure according to the invention can be used for all applications and uses in which synthetic leather or structured surface coverings that are not biodegradable are currently used. The composite structures according to the invention are particularly useful in applications such as coverings in automotive passenger compartments, e.g., for car seats or as door or front panel trim, as well as in furniture construction.
[0058] In a further aspect, the present invention relates to a process for producing a biodegradable composite structure as described above, the process comprising the following steps:
[0059] (i) applying an aqueous polymer dispersion and any additives contained therein to a support and drying the mixture to obtain a covering layer;
[0060] (ii) optionally applying a polymer foam to the cover layer obtained in (i) and drying or solidifying the polymer foam to form a foam layer;
[0061] (iii) applying a lamination layer to the cover layer of (i) or the foam layer of (ii), inserting a biodegradable textile carrier material into the lamination layer and drying or solidifying the lamination layer;
[0062] (iv) removing the carrier while maintaining the biodegradable composite structure.
[0063] In the specified process, all layers of the biodegradable composite structure are preferably made from aqueous dispersions, as this avoids adverse evaporation of volatile organic compounds (VOCs).
[0064] Drying in steps (i) to (iii) can be carried out in an oven designed for this purpose. Because the composite structure is produced via a sequence of application and drying processes, the process is particularly material-, time-, and energy-efficient, making the composite structure cost-effective to manufacture. The temperature under typical drying conditions usually ranges between 70 and 210 °C. The time to which the layers are exposed to the elevated temperature can expediently be set in the range of 20 to 120 seconds. The support to which the polymer dispersion is applied in step (i) is preferably a paper or a film, which can have a surface structure corresponding to the negative of a surface structure desired on the cover layer.In a particularly preferred embodiment, the carrier therefore has a regularly structured surface or a surface structure that corresponds to the negative of a leather grain.
[0065] Alternatively, a desired surface structuring can be carried out in a process downstream of step (iv) in the manufacturing process, wherein a substrate with a flat surface is used in step (i), and the composite structure, after step (iv), is subjected to a step of embossing a structured surface or a surface structure corresponding to the negative of a leather grain. This can be done, for example, by embossing using steel or silicone rollers or via a die in a vacuum process, for example, by introducing attractive leather grains into the cover layer by heating to temperatures between 100 and 280 °C. It is also possible to form such structures using a press.
[0066] In the specified process, a lacquer layer can be applied either before step (i) or after step (iv). In particular, the composite structure can be provided with at least one lacquer layer by either applying the at least one lacquer layer to the carrier before step (i) and applying the polymer dispersion over the at least one lacquer layer, or by applying the at least one lacquer layer to the cover layer of the composite structure after step (iv).
[0067] After its intended use, the composite structure can be degraded by composting; composting is also possible for remnants of the composite structure, such as edge trimmings or those arising during the production of, for example, covers that can no longer be used. Accordingly, in a further aspect, the present invention relates to methods for composting a biodegradable composite structure as described above, wherein the composting is carried out in an industrial composting facility. Alternatively, the composite structure according to the invention can also be used in a biogas plant (anaerobic degradation) or degraded in other environments, such as landfills, home composting, in the soil, and in fresh and salt water.
[0068] If the different layers of the composite structure are formed from polymer materials with different solubility properties, it is also possible to selectively dissolve one or more of the layers of the composite structure and thus separate them from the other layers and, if necessary, reuse or recycle them separately. Accordingly, a further aspect of the present invention relates to a method for processing composite structures according to the invention, in which the composite structure is treated with an organic solvent that selectively dissolves one or more of the layers of the composite structure.An example of a composite structure that can be prepared using such a process is a composite structure comprising layers of polyester-polyurethane (PU) and polybutylene adipate terephthalate, wherein the polybutylene adipate terephthalate is soluble in ethyl acetate but not in isopropyl alcohol, and the polyester-polyurethane is soluble in isopropyl alcohol but not in ethyl acetate. A cellulose textile would not be soluble in any of these solvents and could thus also be selectively separated from the other layers of the composite structure. In a particularly preferred embodiment, the composite structure according to the invention therefore comprises a cover and lamination layer with polybutylene adipate terephthalate as the polymeric component (preferably without other additional polymer components) and a foam layer formed from a polyurethane-based foam, in particular polyester-polyurethane.
[0069] In the following, the present invention is illustrated in more detail using an embodiment, which, however, should not be considered in any way as limiting the scope of the application:
[0070] Example 1: A composite structure comprising a cover layer, an intermediate coat formulated as a foam layer, a laminating coat (as the “laminating layer”) and a textile carrier was produced according to the process described below. The cover coat mixture was applied to a carrier paper and the mixture was then placed in an oven for drying. The mixture was dried at a temperature of 120 °C and 200 °C for 1 minute in each case. The intermediate coat was then applied and dried at 80 °C and 150 °C for 1.5 minutes in each case. The laminating coat was then applied. Before drying, the textile was placed in the laminating coat and the resulting composite structure was dried at 100 °C and 150 °C for 2 minutes in each case.
[0071] The compositions of the individual strokes are given in the following Table 1:
[0072] The resulting composite materials were tested for their abrasion resistance according to DIN EN ISO 5470-2 (Martindale). The abrasion fabrics MD100 and Cotton Duck 10 achieved a rating of 1 after 100,000 cycles.
Claims
Patent claims 1. At least three-layered, fully biodegradable composite structure, in particular for use as artificial leather, comprising a cover layer formed from a biodegradable polymer as the polymeric component, a lamination layer formed from a biodegradable polymer composition, and a fabric layer formed from a biodegradable textile carrier material, wherein the cover layer is made from a water-dispersible biodegradable polymer.
2. Biodegradable composite structure according to claim 1, characterized in that it additionally comprises a foam layer with a density in the range of 200 to 900 kg / m 3 and preferably 300 to 800 kg / m 3 wherein the foam in the foam layer is preferably formed as an open-pore foam.
3. Biodegradable composite structure according to claim 2, characterized in that the foam layer is formed between the cover layer and the lamination layer and / or on the side of the textile carrier material opposite the lamination layer.
4. Biodegradable composite structure according to at least one of claims 1 to 3, characterized in that the biodegradable polymer in the cover layer is selected from the group comprising polyester polyurethanes, polybutylene adipate terephthalate, polybutylene succinate, polybutylene succinate adipate, cellulose, cellulose acetate, polycaprolactone, polyhydroxyalkanoates, in particular in the form of poly-3-hydroxybutyrate (P3HB), poly-4-hydroxybutyrate (P4HB), polyhydroxyvalerate (PHV), polyhydroxyhexanoate (PHH), or polyhydroxyoctanoate (PHO), and polyhydroxyalkanoate copolymers, in particular in the form of P3HB4HB, P3HB3HV, P3HB3HV4HV, P3HB3Hx, P3HB3HO or P3HB3HD, polylactic acid, polyvinyl alcohol, starch and other natural polymers and mixtures thereof, and preferably in the form of polybutylene adipate terephthalate.
5. Biodegradable composite structure according to at least one of the preceding claims, characterized in that the cover layer is cross-linked, preferably by ionic interactions of an alginate incorporated into the cover layer or by the reaction of a biodegradable epoxide with OH groups contained in the biodegradable polymer.
6. Biodegradable composite structure according to at least one of the preceding claims, characterized in that the cover layer further comprises biodegradable or biocompatible pigments, preferably selected from the group comprising carbon black, phycocyanins, iron oxide, or effect pigments, preferably in the form of glitter pigments, and / or the foam layer contains a foam stabilizer, preferably in the form of ammonium stearate and / or flame retardant, preferably selected from the group comprising calcium alginate, aluminum hydroxide or magnesium hydroxide.
7. Biodegradable composite structure according to at least one of the preceding claims, characterized in that it has a structured or grained surface structure, which preferably corresponds to a leather grain.
8. Biodegradable composite structure according to at least one of the preceding claims, characterized in that the textile carrier is formed from polylactide (PLA), cotton, cellulose or other renewable raw materials, in particular selected from flax fibers, hemp fibers, pineapple fibers or wool.
9. Biodegradable composite structure according to at least one of the preceding claims, characterized in that it further comprises one or more lacquer layers, preferably based on inorganic-organic hybrid polymers (bioORMOCER®) and biopolymers, in particular based on hemicellulose, and / or based on polyvinyl alcohol.
10. Biodegradable composite structure according to at least one of the preceding claims, characterized in that it is compostable according to DIN EN 14995:2003 and / or has an abrasion resistance according to DIN EN 5470-2 of at least 100,000 Martindale abrasion cycles.
11. A process for producing a biodegradable composite structure according to any one of claims 1 to 10, comprising the steps (i) applying an aqueous polymer dispersion and any additives contained therein to a support and drying the mixture to obtain a covering layer; (ii) optionally applying a polymer foam to the cover layer obtained in (i) and drying or solidifying the polymer foam to form a foam layer; (iii) applying a lamination layer to the cover layer of (i) or the foam layer of (ii), inserting a biodegradable textile carrier material into the lamination layer and drying or solidifying the lamination layer; (iv) removing the carrier to obtain the biodegradable composite structure, wherein preferably in step (i) a carrier with a flat surface is used, and the composite structure after step (iv) is subjected to a step of embossing a structured surface or a surface structure which corresponds to the negative of a leather grain, or a surface structure is produced by application to a carrier in step (i) which has the negative of the desired surface structure, in particular corresponding to the negative of a leather grain.
12. The method according to claim 11, characterized in that the composite structure is provided with at least one lacquer layer by either applying the at least one lacquer layer to the carrier before step (i) and applying the polymer dispersion over the at least one lacquer layer, or applying the at least one lacquer layer to the cover layer of the artificial leather after step (iv).
13. Use of a composite structure according to any one of claims 1 to 10 for use as a covering material in the passenger compartment of an automobile or as a covering for furniture.
14. A process for composting a biodegradable composite structure according to any one of claims 1 to 10, characterized in that the composting is carried out in an industrial composting facility.
15. A method for separating layers of a biodegradable composite structure according to any one of claims 1 to 10, wherein the composite structure is treated with an organic solvent which selectively dissolves one or more of the layers of the composite structure.
Citation Information
Patent Citations
Easily recyclable films and synthetic leather materials based on biopolymers for short-term use and controlled decomposition into monomers
DE102020210811A1
Biologically degradable cpd. material - is based on hardened starch foam during prodn., and is simultaneously mixed with further material
DE4228779A1
Laminates with one or more polyurethane layers, method of manufacture and their use
EP1059379B1
Composite structure with a polyurethane coating, method for its manufacture and application
EP1927466B1