Light-emitting device and manufacturing method therefor
The integration of a carboxyl group-containing functional layer between electron auxiliary layers in light-emitting devices addresses inefficiencies in electron injection and trap site reduction, enhancing efficiency and lifespan through improved electron injection and corrosion prevention in the manufacturing process.
Patent Information
- Application Number
- PCT/KR2024/004939
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-14
- Filing Date
- 2024-04-12
- Publication Date
- 2024-10-17
AI Technical Summary
Current light-emitting devices face inefficiencies in electron injection and trap site reduction, leading to suboptimal performance in terms of efficiency and lifespan.
Incorporating a functional layer with a compound containing a carboxyl group between electron auxiliary layers to reduce trap sites and improve electron injection efficiency, along with a method of manufacturing that includes heat-treating a preliminary functional layer to prevent inkjet device corrosion.
Enhances electron injection efficiency, resulting in improved light-emitting device characteristics and extended lifespan by reducing trap sites and preventing inkjet device corrosion.
Smart Images

Figure KR2024004939_17102024_PF_FP_ABST
Abstract
Description
Light-emitting device and method for manufacturing the same
[0001] The present invention relates to a display device. More specifically, it relates to a light-emitting element included in a display device and a method for manufacturing the same.
[0002] A light-emitting element is a device in which, when voltage is applied to two opposing electrodes, a light-emitting layer disposed between the electrodes emits light. Specifically, when voltage is applied to the two electrodes, electrons and holes injected from the electrodes meet within the light-emitting layer to form excitons. When the excitons transition from an excited energy state to a relatively low energy state, they emit light of a certain wavelength.
[0003] Since a light-emitting device requires that as many electrons and holes as possible meet in the light-emitting layer to form excitons, it is desirable to adjust the movement characteristics of holes and electrons so that the holes and electrons injected from the anode and cathode meet well in the light-emitting layer. Accordingly, a light-emitting device may include organic layers that improve the movement characteristics of electrons or holes on the upper and / or lower portions of the light-emitting layer.
[0004] In particular, an electron transport layer can be provided that enhances electron mobility. Electron transport layers are composed of various materials, and numerous electron transport materials are being researched to supply electrons with appropriate mobility characteristics even at relatively low operating voltages.
[0005] One object of the present invention is to provide a light-emitting device with improved efficiency and lifespan.
[0006] Another object of the present invention is to provide a method for manufacturing the light-emitting device.
[0007] However, the purpose of the present invention is not limited to the above-described purposes, and may be expanded in various ways without departing from the spirit and scope of the present invention.
[0008] In order to achieve one object of the present invention, a light-emitting device according to embodiments may include a first electrode, a second electrode facing the first electrode, a light-emitting layer disposed between the first electrode and the second electrode, a first electron-assistant layer disposed between the first electrode and the light-emitting layer, and a functional layer disposed between the light-emitting layer and the first electron-assistant layer and including a compound containing a carboxyl group.
[0009] In one embodiment, the compound comprising the carboxyl group may comprise any one of the following compounds:
[0010] [Compound 1]
[0011]
[0012] [Compound 2]
[0013]
[0014] In each of the above compounds 1 and 2, R1 is independently , , or can be expressed as
[0015] In one embodiment, the first electron-assisted layer may comprise metal-inorganic nanoparticles.
[0016] In one embodiment, the first electron-assisted layer may include at least one of TiO2, ZnO, ZnMgO, ZnAlO, and SnO2.
[0017] In one embodiment, the light emitting element may further include a second electron auxiliary layer disposed on the first electron auxiliary layer.
[0018] In one embodiment, the first electron auxiliary layer may be an electron injection layer, and the second electron auxiliary layer may be an electron transport layer.
[0019] In one embodiment, the first electron-assisted layer may include ZnO, and the second electron-assisted layer may include ZnMgO.
[0020] In one embodiment, the functional layer may be disposed between the first electronic auxiliary layer and the second electronic auxiliary layer.
[0021] In one embodiment, the functional layer may be in direct contact with the first electronic auxiliary layer.
[0022] In one embodiment, the functional layer may be disposed between the second electronic auxiliary layer and the light-emitting layer.
[0023] In one embodiment, the functional layer may be in direct contact with the second electronic auxiliary layer.
[0024] In one embodiment, the light-emitting layer may include quantum dots.
[0025] In one embodiment, the light-emitting layer may comprise an organic material.
[0026] In one embodiment, the light-emitting element may further include a hole auxiliary layer disposed between the second electrode and the light-emitting layer.
[0027] In order to achieve another object of the present invention, a method for manufacturing a light-emitting device according to embodiments may include a step of forming a first electrode, a step of forming a first electron-assisting layer on the first electrode, a step of forming a functional layer including a compound including a carboxyl group on the first electron-assisting layer, a step of forming a light-emitting layer on the functional layer, and a step of forming a second electrode on the light-emitting layer.
[0028] In one embodiment, the step of forming the functional layer may include the step of forming a preparatory functional layer including a compound including an ester group on the first electron auxiliary layer and the step of heat-treating the preparatory functional layer.
[0029] In one embodiment, the compound comprising the ester group may comprise any one of the following compounds:
[0030] [Compound 3]
[0031]
[0032] [Compound 4]
[0033]
[0034] In each of the above compounds 3 and 4, R1 is independently , , or , and R2 represents , , or can be expressed as
[0035] In one embodiment, the method for manufacturing the light-emitting device may further include, before the step of forming the light-emitting layer, a step of forming a second electron auxiliary layer on the first electron auxiliary layer.
[0036] In one embodiment, the functional layer may be formed on the first electronic auxiliary layer, and the second electronic auxiliary layer may be formed on the functional layer.
[0037] In one embodiment, the functional layer may be formed on the second electronic auxiliary layer.
[0038] In a display device according to embodiments of the present invention, a light-emitting element is disposed between a first electron-auxiliary layer and a second electron-auxiliary layer, and further includes a functional layer including a compound including a carboxyl group, so that the number of trap sites on an upper surface of the first electron-auxiliary layer can be reduced. That is, by forming a film of the functional layer on the upper surface of the first electron-auxiliary layer, the number of trap sites on the upper surface of the first electron-auxiliary layer can be reduced. By reducing the number of trap sites on the upper surface of the first electron-auxiliary layer, the efficiency of electron injection into the light-emitting layer can be increased. As a result, the characteristics of the light-emitting element can be improved.
[0039] By heat-treating a pre-functional layer comprising a compound containing an ester group to form a functional layer, corrosion of the inkjet device forming the functional layer can be prevented. Specifically, compounds containing carboxylic acids may cause corrosion of the inkjet device when they come into contact with the inkjet device. Therefore, by forming a pre-functional layer using a compound containing a relatively stable ester group, corrosion of the inkjet device can be prevented, and by subsequently heat-treating the pre-functional layer to form a functional layer, the efficiency of the light-emitting element can be improved.
[0040] However, the effects of the present invention are not limited to the effects described above, and may be expanded in various ways without departing from the spirit and scope of the present invention.
[0041] Figure 1 is a cross-sectional view of a light-emitting device according to one embodiment of the present invention.
[0042] Figure 2 is a cross-sectional view of a display device according to one embodiment of the present invention.
[0043] Figure 3 is a cross-sectional view of a light emitting element according to another embodiment of the present invention.
[0044] Figures 4 to 7 are drawings showing a method for manufacturing a light-emitting element according to one embodiment of the present invention.
[0045] FIGS. 8 to 10 are drawings showing a method for manufacturing a light-emitting element according to another embodiment of the present invention.
[0046] Figure 11 is a graph showing current density according to voltage.
[0047] Figure 12 is a graph showing luminance over time.
[0048] Hereinafter, embodiments of the present invention will be described in more detail with reference to the attached drawings. Identical components in the drawings will be designated by the same reference numerals, and redundant descriptions of identical components will be omitted.
[0049] Figure 1 is a cross-sectional view of a light-emitting device according to one embodiment of the present invention.
[0050] Referring to FIG. 1, the light emitting element (10) may include a first electrode (100), an intermediate layer (200), and a second electrode (300).
[0051] In one embodiment, the first electrode (100) may be a cathode. The first electrode (100) may have light-transmitting or reflective properties. For example, the first electrode (100) may include a metal and / or a conductive material having reflective properties.
[0052] In one embodiment, the second electrode (300) may face the first electrode (100). For example, the second electrode (300) may be disposed on the first electrode (100). The second electrode (300) may be an anode. The second electrode (300) may have light-transmitting or reflecting properties. For example, the second electrode (300) may include a metal and / or a conductive material having light-transmitting properties.
[0053] The intermediate layer (200) may be disposed between the first electrode (100) and the second electrode (300). That is, the intermediate layer (200) may be disposed on the first electrode (100) and under the second electrode (300). The intermediate layer (200) may include a light-emitting layer (230), an electron auxiliary layer, a hole auxiliary layer, and a functional layer (220).
[0054] A light-emitting layer (230) may be disposed between the first electrode (100) and the second electrode (300). That is, the light-emitting layer (230) may be disposed on the first electrode (100) and under the second electrode (300). The light-emitting layer (230) may include an organic and / or inorganic light-emitting material. In one embodiment, the light-emitting layer (230) may include quantum dots. However, the present invention is not limited thereto, and in another embodiment, the light-emitting layer (230) may include an organic material.
[0055] The above-described electron-assisting layer may be disposed between the first electrode (100) and the light-emitting layer (230). The above-described electron-assisting layer may include metal inorganic nanoparticles. For example, examples of the metal inorganic nanoparticles include TiO2, ZnO, ZnMgO, ZnAlO, SnO2, etc. These may be used alone or in combination with each other.
[0056] The above-described electronic auxiliary layer may include a first electronic auxiliary layer (211) and a second electronic auxiliary layer (213). The first electronic auxiliary layer (211) may be disposed between the first electrode (100) and the light-emitting layer (230). The second electronic auxiliary layer (213) may be disposed on the first electronic auxiliary layer (211) and below the light-emitting layer (230).
[0057] For example, the first electron auxiliary layer (211) may be an electron injection layer, and the second electron auxiliary layer (213) may be an electron transport layer. In addition, the first electron auxiliary layer (211) may include ZnO, and the second electron auxiliary layer (213) may include ZnMgO. However, the present invention is not limited thereto.
[0058] The above hole auxiliary layer may be disposed between the second electrode (300) and the light-emitting layer (230). The hole auxiliary layer may include a first hole auxiliary layer (240) and a second hole auxiliary layer (250). The second hole auxiliary layer (250) may be disposed on the first hole auxiliary layer (240). For example, the first hole auxiliary layer (240) may be a hole transport layer, and the second hole auxiliary layer (250) may be a hole injection layer.
[0059] In one embodiment, the functional layer (220) may be disposed between the light-emitting layer (230) and the first electron-auxiliary layer (211). For example, the functional layer (220) may be disposed between the first electron-auxiliary layer (211) and the second electron-auxiliary layer (213). At this time, the functional layer (220) may be in direct contact with the first electron-auxiliary layer (211). That is, the functional layer (220) may be in direct contact with the upper surface of the first electron-auxiliary layer (211).
[0060] In one embodiment, the functional layer (220) may include a compound containing a carboxyl group. The compound containing a carboxyl group may include any one of the following compounds.
[0061] [Compound 1]
[0062]
[0063] [Compound 2]
[0064]
[0065] In each of the above compounds 1 and 2, R1 is independently , , or can be expressed as
[0066] In one embodiment, the light-emitting device (10) further includes the functional layer (220) disposed between the first electron-auxiliary layer (211) and the second electron-auxiliary layer (213) and including a compound including a carboxyl group, so that the number of trap sites on the upper surface of the first electron-auxiliary layer (211) can be reduced. That is, by forming the functional layer (220) on the upper surface of the first electron-auxiliary layer (211), the number of trap sites on the upper surface of the first electron-auxiliary layer (211) can be reduced. By reducing the number of trap sites on the upper surface of the first electron-auxiliary layer (211), the efficiency of electron injection into the light-emitting layer (230) can be increased. As a result, the characteristics of the light-emitting device (10) can be improved.
[0067] Figure 2 is a cross-sectional view of a display device according to one embodiment of the present invention.
[0068] For example, FIG. 2 may be a cross-sectional view showing a display device including the light emitting element (10) of FIG. 1.
[0069] Referring to FIGS. 1 and 2, the display device (1) may include a substrate (SUB), a circuit element layer (20), a light emitting element layer (30), and an encapsulation layer (40).
[0070] The circuit element layer (20) may be disposed on the substrate (SUB) and may include a buffer layer (BFR), at least one transistor (TR), a first insulating layer (IL1), a second insulating layer (IL2), and a third insulating layer (IL3). The transistor (TR) may include an active layer (ACT), a gate electrode (GE), a source electrode (SE), and a drain electrode (DE). The light-emitting element layer (30) may be disposed on the circuit element layer (20) and may include a fourth insulating layer (IL4) and light-emitting elements (10).
[0071] The substrate (SUB) may include a transparent or opaque material. For example, the substrate (SUB) may be a flexible substrate including polyimide or the like. The flexible substrate may have a structure in which a polyimide layer and a barrier layer are alternately laminated. As another example, the substrate (SUB) may be a rigid substrate including quartz, glass, or the like.
[0072] The above buffer layer (BFR) may be disposed on the substrate (SUB). The buffer layer (BFR) may prevent metal atoms or impurities from diffusing from the substrate (SUB) to the active layer (ACT).
[0073] The above active layer (ACT) may be disposed on the above buffer layer (BFR). The above active layer (ACT) may be divided into a source region and a drain region doped with impurities and a channel region between the source region and the drain region.
[0074] The first insulating layer (IL1) may be disposed on the buffer layer (BFR). The first insulating layer (IL1) covers the active layer (ACT) and may be formed with a substantially constant thickness along the profile of the active layer (ACT). However, the present invention is not limited thereto. For example, the first insulating layer (IL1) may include an inorganic material.
[0075] The gate electrode (GE) may be disposed on the first insulating layer (IL1). In one embodiment, the gate electrode (GE) may overlap the channel region of the active layer (ACT).
[0076] The second insulating layer (IL2) may be disposed on the first insulating layer (IL1). In addition, the second insulating layer (IL2) may cover the gate electrode (GE) and may be disposed with a substantially constant thickness along the profile of the gate electrode (GE). However, the present invention is not limited thereto.
[0077] The source electrode (SE) and the drain electrode (DE) may be disposed on the second insulating layer (IL2). The source electrode (SE) may be in contact with the source region of the active layer (ACT) through a first contact hole defined in the first and second insulating layers (IL1, IL2). The drain electrode (DE) may be in contact with the drain region of the active layer (ACT) through a second contact hole defined in the first and second insulating layers (IL1, IL2).
[0078] The third insulating layer (IL3) may be disposed on the second insulating layer (IL2). In addition, the third insulating layer (IL3) may cover the source and drain electrodes (SE, DE) and may have a substantially flat upper surface without creating a step around the source and drain electrodes (SE, DE). For example, the third insulating layer (IL3) may include an organic material.
[0079] The light-emitting element (10) may be placed on the third insulating layer (IL3). The light-emitting element (10) may include the first electrode (100), the intermediate layer (200), and the second electrode (300).
[0080] The first electrode (100) may be disposed on the third insulating layer (IL3). The first electrode (100) may be in contact with the source electrode (SE) or the drain electrode (DE) through a third contact hole defined in the third insulating layer (IL3). Through this, the first electrode (100) may be connected to the transistor (TR).
[0081] The fourth insulating layer (IL4) may be disposed on the third insulating layer (IL3), and an opening exposing the upper surface of the first electrode (100) may be defined in the fourth insulating layer (IL4). For example, the fourth insulating layer (IL4) may include an organic material or an inorganic material.
[0082] A spacer may be further disposed on the fourth insulating layer (IL4). For example, the spacer may include an organic or inorganic material. The spacer may maintain a gap between the sealing layer (40) and the substrate (SUB).
[0083] The intermediate layer (200) may be disposed on the first electrode (100). The intermediate layer (200) may be disposed in the opening defined in the fourth insulating layer (IL4).
[0084] The second electrode (300) covers the intermediate layer (200) and can be placed on the fourth insulating layer (IL4) and the spacer.
[0085] The encapsulating layer (40) covers the light-emitting element layer (30) and can be disposed on the light-emitting element layer (30). The encapsulating layer (40) can prevent moisture and oxygen from penetrating from the outside into the light-emitting elements (10). For example, the encapsulating layer (40) can include a first inorganic encapsulating layer (IEL1), an organic encapsulating layer (OEL), and a second inorganic encapsulating layer (IEL2).
[0086] The first inorganic encapsulating layer (IEL1) may be disposed on the second electrode (300) with a substantially constant thickness along the profile of the second electrode (300). The organic encapsulating layer (OEL) may be disposed on the first inorganic encapsulating layer (IEL1) and may have a substantially flat upper surface without creating a step around the first inorganic encapsulating layer (IEL1). The second inorganic encapsulating layer (IEL2) may be disposed on the organic encapsulating layer (OEL).
[0087] Figure 3 is a cross-sectional view of a light emitting element according to another embodiment of the present invention.
[0088] For example, the light emitting element (11) of FIG. 3 may be identical to the light emitting element (10) described with reference to FIGS. 1 and 2 except for the stacking order of the functional layer (220) and the second electronic auxiliary layer (213). Therefore, overlapping descriptions may be omitted or simplified.
[0089] Referring to FIG. 3, the light-emitting element (11) may include a first electrode (100), an intermediate layer (200), and a second electrode (300). The intermediate layer (200) may include a light-emitting layer (230), an electron auxiliary layer, a hole auxiliary layer, and a functional layer (220).
[0090] In one embodiment, the functional layer (220) may be disposed between the light-emitting layer (230) and the first electron-auxiliary layer (211). For example, the functional layer (220) may be disposed between the second electron-auxiliary layer (213) and the light-emitting layer (230). At this time, the functional layer (220) may be in direct contact with the second electron-auxiliary layer (213). That is, the functional layer (220) may be in direct contact with the upper surface of the second electron-auxiliary layer (213).
[0091] In one embodiment, the functional layer (220) may include a compound containing a carboxyl group. The compound containing a carboxyl group may include any one of the following compounds.
[0092] [Compound 1]
[0093]
[0094] [Compound 2]
[0095]
[0096] In each of the above compounds 1 and 2, R1 is independently , , or can be expressed as
[0097] In one embodiment, the light-emitting element (11) is disposed between the second electron-auxiliary layer (213) and the light-emitting layer (230), and further includes the functional layer (220) including a compound including a carboxyl group, so that the number of trap sites on the upper surface of the second electron-auxiliary layer (213) can be reduced. That is, by forming the functional layer (220) as a film on the upper surface of the second electron-auxiliary layer (213), the number of trap sites on the upper surface of the second electron-auxiliary layer (213) can be reduced. By reducing the number of trap sites on the upper surface of the second electron-auxiliary layer (213), the electron injection efficiency into the light-emitting layer (230) can be increased. As a result, the characteristics of the light-emitting element (11) can be improved.
[0098] Figures 4 to 7 are drawings showing a method for manufacturing a light-emitting element according to one embodiment of the present invention.
[0099] For example, the method for manufacturing a light-emitting element described with reference to FIGS. 4 to 7 may be a method for manufacturing a light-emitting element (10) described with reference to FIG. 1. Therefore, redundant descriptions may be omitted or simplified.
[0100] Referring to FIG. 4, a first electrode (100) may be formed. The first electrode (100) may be a cathode. For example, the first electrode (100) may include a metal and / or a conductive material having reflective properties.
[0101] A first electron auxiliary layer (211) may be formed on the first electrode (100). The first electron auxiliary layer (211) may include metal inorganic nanoparticles. Examples of the metal inorganic nanoparticles include TiO2, ZnO, ZnMgO, ZnAlO, SnO2, etc. These may be used alone or in combination with each other. For example, the first electron auxiliary layer (211) may include ZnO. However, the present invention is not limited thereto.
[0102] Referring further to FIG. 5, a functional layer (220) including a compound containing a carboxyl group may be formed on the first electronic auxiliary layer (211). The functional layer (220) may be formed using an inkjet process.
[0103] Specifically, a pre-functional layer may be formed on the first electronic auxiliary layer (211). The pre-functional layer may include a compound containing an ester group. The compound containing an ester group may include any one of the following compounds.
[0104] [Compound 3]
[0105]
[0106] [Compound 4]
[0107]
[0108] In each of the above compounds 3 and 4, R1 is independently , , or , and R2 represents , , or It represents.
[0109] Thereafter, the pre-functional layer may be heat-treated. As the pre-functional layer is heat-treated, the ester group may be hydrolyzed. The ester group may be hydrolyzed to form a carboxylic acid and an alcohol. The alcohol may be removed by heat, and only the carboxylic acid may remain, thereby forming the functional layer (220) comprising a compound including a carboxyl group. The compound including a carboxyl group may include any one of the following compounds.
[0110] [Compound 1]
[0111]
[0112] [Compound 2]
[0113]
[0114] In each of the above compounds 1 and 2, R1 is independently , , or can be expressed as
[0115] Referring further to FIG. 6, a second electron auxiliary layer (213) may be formed on the functional layer (220). The second electron auxiliary layer (213) may include metal inorganic nanoparticles. Examples of the metal inorganic nanoparticles include TiO2, ZnO, ZnMgO, ZnAlO, SnO2, etc. These may be used alone or in combination with each other. For example, the second electron auxiliary layer (213) may include ZnMgO. However, the present invention is not limited thereto.
[0116] Referring further to FIG. 7, a light-emitting layer (230) may be formed on the second electronic auxiliary layer (213). The light-emitting layer (230) may include an organic and / or inorganic light-emitting material. In one embodiment, the light-emitting layer (230) may include quantum dots. However, the present invention is not limited thereto, and in another embodiment, the light-emitting layer (230) may include an organic material.
[0117] A first hole auxiliary layer (240) may be formed on the light-emitting layer (230). A second hole auxiliary layer (250) may be formed on the first hole auxiliary layer (240). A second electrode (300) may be formed on the second hole auxiliary layer (250). The second electrode (300) may be an anode. For example, the second electrode (300) may include a metal and / or a conductive material having light-transmitting properties. Accordingly, a light-emitting element (10) may be formed.
[0118] In one embodiment, the pre-functional layer including the compound including the ester group is heat-treated to form the functional layer (220), thereby preventing corrosion of the inkjet device forming the functional layer (220). Specifically, in the case of the compound including the carboxylic acid, if it comes into contact with the inkjet device, corrosion of the inkjet device may be induced. Therefore, by forming the pre-functional layer using the relatively stable compound including the ester group, corrosion of the inkjet device can be prevented, and thereafter, by heat-treating the pre-functional layer to form the functional layer (220), the efficiency of the light-emitting element can be improved.
[0119] FIGS. 8 to 10 are drawings showing a method for manufacturing a light-emitting element according to another embodiment of the present invention.
[0120] For example, the method for manufacturing a light-emitting element described with reference to FIGS. 8 to 10 may be the same as the method for manufacturing a light-emitting element described with reference to FIGS. 4 to 7 except for the order of forming the functional layer (220) and the second electron auxiliary layer (213). In addition, the method for manufacturing a light-emitting element described with reference to FIGS. 8 to 10 may be a method for manufacturing a light-emitting element (11) described with reference to FIG. 3. Therefore, overlapping descriptions may be omitted or simplified.
[0121] Referring to Fig. 8, a first electrode (100) may be formed. A first electron auxiliary layer (211) may be formed on the first electrode (100). A second electron auxiliary layer (213) may be formed on the first electron auxiliary layer (211).
[0122] Referring further to Fig. 9, a functional layer (220) including a compound containing a carboxyl group may be formed on the second electronic auxiliary layer (213). The functional layer (220) may be formed using an inkjet process.
[0123] Specifically, a pre-functional layer may be formed on the second electronic auxiliary layer (213). The pre-functional layer may include a compound containing an ester group. The compound containing an ester group may include any one of the following compounds.
[0124] [Compound 3]
[0125]
[0126] [Compound 4]
[0127]
[0128] In each of the above compounds 3 and 4, R1 is independently , , or , and R2 represents , , or It represents.
[0129] Thereafter, as the preparatory functional layer is heat-treated, the ester group may be hydrolyzed. The ester group may be hydrolyzed to form a carboxylic acid and an alcohol. The alcohol may be removed by heat, and only the carboxylic acid may remain, thereby forming the functional layer (220) comprising a compound including a carboxyl group. The compound including a carboxyl group may include any one of the following compounds.
[0130] [Compound 1]
[0131]
[0132] [Compound 2]
[0133]
[0134] In the above compounds 1 and 2, R1 is , , or can be expressed as
[0135] Referring further to Fig. 10, a light-emitting layer (230) may be formed on the functional layer (220). A first hole auxiliary layer (240) may be formed on the light-emitting layer (230). A second hole auxiliary layer (250) may be formed on the first hole auxiliary layer (240). A second electrode (300) may be formed on the second hole auxiliary layer (250). Accordingly, a light-emitting element (11) may be formed.
[0136] Hereinafter, the effects of the present invention will be further described with reference to Table 1, FIG. 11, and FIG. 12.
[0137] Light-emitting device manufacturing
[0138] [Comparative Example 1]
[0139] A 15Ω / cm2 ITO glass substrate (50 mm × 50 mm × 0.7 mm) was ultrasonically cleaned in isopropyl alcohol and pure water for 30 minutes each to manufacture a first electrode. 1 mL of an electron auxiliary layer composition, 1 mL of a light-emitting layer composition, 1 mL of a first hole auxiliary layer composition, and 1 mL of a second hole auxiliary layer composition were deposited on the first electrode using a solution process using spin coating.
[0140] Specifically, a ZnO composition was spin-coated on the first electrode after cleaning to form a film with a thickness of 30 nm, and then baked at 200°C for 10 minutes to form a first electron-assisting layer. A ZnMgO composition was spin-coated on the first electron-assisting layer to form a film with a thickness of 20 nm, and then baked at 200°C for 10 minutes to form a second electron-assisting layer. An emission layer was spin-coated on the second electron-assisting layer to form a film with a thickness of 20 nm, and then baked at 100°C for 10 minutes to form a emission layer. A first hole-assisting layer composition was spin-coated on the layer formed up to the emission layer to form a film with a thickness of 20 nm, and then baked at 100°C for 10 minutes to form a first hole-assisting layer. A second hole-assisting layer composition was spin-coated on the first hole-assisting layer to form a film with a thickness of 10 nm, and then baked at 100°C for 10 minutes to form a second hole-assisting layer. Next, on the second hole-assist layer, AgMg was vacuum-deposited to form a second electrode with a thickness of 10 nm, thereby fabricating a light-emitting device. A Suicel plus 200 deposition device from Sunik Systems was used as the deposition device. The driving voltage, luminous efficiency, and color coordinates of the light-emitting device fabricated in the comparative example were measured using a Keithley SMU 236 and a PR650 luminance meter.
[0141] [Example 1]
[0142] A 15Ω / cm2 ITO glass substrate (50 mm × 50 mm × 0.7 mm) was ultrasonically cleaned in isopropyl alcohol and pure water for 30 minutes each to manufacture a first electrode. 1 mL of an electron auxiliary layer composition, 1 mL of a functional layer composition, 1 mL of a light-emitting layer composition, 1 mL of a first hole auxiliary layer composition, and 1 mL of a second hole auxiliary layer composition were deposited on the first electrode using a solution process using spin coating.
[0143] Specifically, a ZnO composition was spin-coated on the first electrode after cleaning to form a film with a thickness of 30 nm, and then baked at 200°C for 10 minutes to form a first electron-assisted layer. A functional layer composition was spin-coated on the first electron-assisted layer to form a film with a thickness of 10 nm, and then baked at 150°C for 10 minutes to form a functional layer. A ZnMgO composition was spin-coated on the functional layer to form a film with a thickness of 20 nm, and then baked at 200°C for 10 minutes to form a second electron-assisted layer. An emission layer was spin-coated on the second electron-assisted layer to form a film with a thickness of 20 nm, and then baked at 100°C for 10 minutes to form a emission layer. A first hole-assisted layer composition was spin-coated on the layer formed up to the emission layer to form a film with a thickness of 20 nm, and then baked at 100°C for 10 minutes to form a first hole-assisted layer. A second hole auxiliary layer composition was spin-coated on the first hole auxiliary layer to form a 10 nm thick film, and then baked at 100°C for 10 minutes to form a second hole auxiliary layer. Subsequently, AgMg was vacuum-deposited on the second hole auxiliary layer to form a 10 nm thick second electrode, thereby manufacturing a light-emitting device. A Suicel plus 200 deposition device from Sunik Systems was used as the deposition device. The driving voltage, luminous efficiency, and color coordinates of the light-emitting device manufactured in Example 1 were measured using a Keithley SMU 236 and a luminance meter PR650.
[0144] The functional layer composition included any one of the following compounds, and the electronic auxiliary layer composition included at least one of TiO2, ZnO, ZnMgO, ZnAlO, and SnO2.
[0145] [Compound 3]
[0146]
[0147] [Compound 4]
[0148]
[0149] In each of the above compounds 3 and 4, R1 is independently , , or , and R2 represents , , or It represents.
[0150] [Example 2]
[0151] A light-emitting device was manufactured in the same manner as in Example 1, except that the order of formation of the functional layer and the second electronic auxiliary layer was changed.
[0152] That is, the light-emitting device of Example 2 was manufactured by forming a first electrode, a first electron auxiliary layer on the first electrode, a second electron auxiliary layer on the first electron auxiliary layer, a functional layer on the second electron auxiliary layer, a light-emitting layer on the functional layer, a first hole auxiliary layer on the light-emitting layer, a second hole auxiliary layer on the first hole auxiliary layer, and a second electrode on the second hole auxiliary layer.
[0153] [Comparative Example 2]
[0154] A 15Ω / cm2 ITO glass substrate (50 mm × 50 mm × 0.7 mm) was ultrasonically cleaned in isopropyl alcohol and pure water for 30 minutes each to manufacture a first electrode. 1 mL of an inorganic ETL composition, 1 mL of a light-emitting layer composition, 1 mL of a hole transport layer composition, and 1 mL of a hole injection layer composition were deposited on the first electrode using a solution process using spin coating.
[0155] Specifically, a composition mixing ZnO and a functional layer material was spin-coated on the first electrode after cleaning to form a film with a thickness of 30 nm, and then baked at 200°C for 10 minutes to form a first electron-assistant layer. A composition mixing ZnMgO and a functional layer material was spin-coated on the first electron-assistant layer to form a film with a thickness of 20 nm, and then baked at 200°C for 10 minutes to form a second electron-assistant layer. An emission layer was spin-coated on the second electron-assistant layer to form a film with a thickness of 20 nm, and then baked at 100°C for 10 minutes to form a emission layer. A first hole-assistant layer composition was spin-coated on the layer formed up to the emission layer to form a film with a thickness of 20 nm, and then baked at 100°C for 10 minutes to form a first hole-assistant layer. A second hole auxiliary layer composition was spin-coated on the first hole auxiliary layer to form a 10 nm thick film, and then baked at 100°C for 10 minutes to form a second hole auxiliary layer. Subsequently, AgMg was vacuum-deposited on the second hole auxiliary layer to form a 10 nm thick second electrode, thereby manufacturing a light-emitting device. A Suicel plus 200 deposition device from Sunik Systems was used as the deposition device. The driving voltage, luminous efficiency, and color coordinates of the light-emitting device manufactured in Example 1 were measured using a Keithley SMU 236 and a luminance meter PR650.
[0156] [Comparative Example 3]
[0157] A light-emitting device was manufactured in the same manner as in Example 1, except that the formation order of the first electronic auxiliary layer and the functional layer was changed.
[0158] That is, the light-emitting element of Comparative Example 3 was manufactured by forming a first electrode, a functional layer on the first electrode, a first electron auxiliary layer on the functional layer, a second electron auxiliary layer on the first electron auxiliary layer, a light-emitting layer on the second electron auxiliary layer, a first hole auxiliary layer on the light-emitting layer, a second hole auxiliary layer on the first hole auxiliary layer, and a second electrode on the second hole auxiliary layer.
[0159] The voltage (Op. V), current efficiency (LE), and external quantum efficiency (EQE) that can produce the required luminance (1850 nit) of the light-emitting devices manufactured in Comparative Examples 1 to 3 and Examples 1 and 2 were measured, and the results are shown in Table 1. At this time, Comparative Examples 1 to 3 and Examples 1 and 2 all compare the device results for the green light-emitting layer.
[0160] Op. V (V)LE (cd / A)CIExCIEyEQE (%)Comparative Example 14.865.70.2440.72517.5Example 14.774.00.2580.71519.5Example 25.072.50.2570.71519.1Comparative Example 26.441.00.2490.72510.5Comparative Example 34.862.30.2830.69917.1
[0161] Fig. 11 is a graph showing current density according to voltage. Fig. 12 is a graph showing luminance according to time.
[0162] Referring to Table 1, Figures 11 and 12 above, it can be confirmed that Examples 1 and 2 show superior results in both efficiency and lifespan compared to Comparative Examples 1 to 3.
[0163] Specifically, referring to Table 1, it can be confirmed that Examples 1 and 2 have lower voltages (Op. V) capable of producing the required luminance (approximately 1850 nit) than Comparative Examples 1 to 3. In addition, it can be confirmed that Examples 1 and 2 have higher current efficiency (LE) and external quantum efficiency (EQE) than Comparative Examples 1 to 3.
[0164] Referring to FIG. 11, it can be confirmed that Examples 1 and 2 have lower resistance compared to Comparative Example 2, and have similar resistance characteristics compared to Comparative Examples 1 and 3.
[0165] Referring to Fig. 12, it can be confirmed that the luminance values of Examples 1 and 2 decrease relatively less over time compared to Comparative Examples 1 to 3. Therefore, it can be confirmed that Examples 1 and 2 have a superior lifespan compared to Comparative Examples 1 to 3.
[0166] Although the present invention has been described with reference to exemplary embodiments thereof, it will be understood by those skilled in the art that various modifications and changes may be made to the present invention without departing from the spirit and scope of the present invention as set forth in the claims below.
[0167] The light-emitting element according to exemplary embodiments of the present invention can be applied to display devices included in computers, laptops, mobile phones, smart phones, smart pads, automobiles, PMPs, PDAs, MP3 players, etc.
[0168] Although the present invention has been described above with reference to exemplary embodiments thereof, it will be understood by those skilled in the art that various modifications and changes may be made to the present invention without departing from the spirit and scope of the present invention as set forth in the claims below.
[0169] <Explanation of symbols>
[0170] 10, 11: Light-emitting element 100: First electrode
[0171] 200: Middle layer 300: Second electrode
[0172] 211: First electron transport layer 213: Second electron transport layer
[0173] 220: Functional layer 230: Emissive layer
[0174] 240: First hole transport layer 250: Second hole transport layer
[0175] 20: Circuit element layer 30: Light-emitting element layer
[0176] 40: Encapsulation layer 1: Display device
Claims
1. First electrode; A second electrode opposite to the first electrode; A light-emitting layer disposed between the first electrode and the second electrode; A first electron auxiliary layer disposed between the first electrode and the light-emitting layer; and A light-emitting device comprising a functional layer disposed between the light-emitting layer and the first electron-assisting layer, the functional layer comprising a compound containing a carboxyl group.
2. A light-emitting device according to claim 1, characterized in that the compound containing a carboxyl group contains any one of the following compounds. [Compound 1] [Compound 2] (In each of the above compounds 1 and 2, R1 is independently , , or ) 3. A light-emitting device according to claim 1, characterized in that the first electron auxiliary layer comprises metal inorganic nanoparticles.
4. In the third paragraph, the first electron auxiliary layer is TiO 2 , ZnO, ZnMgO, ZnAlO, SnO 2 A light emitting device characterized by comprising at least one of:
5. In paragraph 1, A light-emitting device further comprising a second electron auxiliary layer disposed on the first electron auxiliary layer.
6. In paragraph 5, the first electron auxiliary layer is an electron injection layer, A light-emitting device, characterized in that the second electron auxiliary layer is an electron transport layer.
7. A light-emitting device according to claim 5, wherein the first electron auxiliary layer comprises ZnO and the second electron auxiliary layer comprises ZnMgO.
8. A light-emitting device according to claim 5, characterized in that the functional layer is disposed between the first electron auxiliary layer and the second electron auxiliary layer.
9. A light-emitting device according to claim 8, characterized in that the functional layer is in direct contact with the first electronic auxiliary layer.
10. A light-emitting device according to claim 5, characterized in that the functional layer is disposed between the second electron auxiliary layer and the light-emitting layer.
11. A light-emitting device according to claim 10, characterized in that the functional layer is in direct contact with the second electronic auxiliary layer.
12. A light-emitting device according to claim 1, characterized in that the light-emitting layer includes quantum dots.
13. A light-emitting device according to claim 1, characterized in that the light-emitting layer comprises an organic material.
14. In paragraph 1, A light-emitting device further comprising a hole auxiliary layer disposed between the second electrode and the light-emitting layer.
15. Step of forming the first electrode; A step of forming a first electron auxiliary layer on the first electrode; A step of forming a functional layer including a compound containing a carboxyl group on the first electron auxiliary layer; A step of forming a light-emitting layer on the above functional layer; and A method for manufacturing a light-emitting element, comprising the step of forming a second electrode on the light-emitting layer.
16. In the 15th paragraph, the step of forming the functional layer is: A step of forming a pre-functional layer comprising a compound containing an ester group on the first electronic auxiliary layer; and A method for manufacturing a light-emitting device, characterized by including a step of heat-treating the above-mentioned preliminary functional layer.
17. A method for manufacturing a light-emitting device, characterized in that in claim 16, the compound containing the ester group contains any one of the following compounds. [Compound 3] [Compound 4] (In each of the above compounds 3 and 4, R1 is independently , , or , and R2 represents , , or ) 18. In paragraph 16, Before the step of forming the above-mentioned light-emitting layer, A method for manufacturing a light-emitting device, characterized in that it further comprises the step of forming a second electron auxiliary layer on the first electron auxiliary layer.
19. In the 18th paragraph, the functional layer is formed on the first electronic auxiliary layer, A method for manufacturing a light-emitting device, characterized in that the second electronic auxiliary layer is formed on the functional layer.
20. A method for manufacturing a light-emitting device, characterized in that in claim 18, the functional layer is formed on the second electronic auxiliary layer.
Citation Information
Patent Citations
Organic electroluminescent element
JP2005285663A
Manufacturing method of organic electroluminescent element
JP2020135985A
Neutralized anode buffer layers to improve processing and performances of organic electronic devices
KR101366655B1
Manufacturing method for pottery decorated with pearl mark
KR1020230030199A
KR20220150499A