Barrier coating for paper and paperboard

The aqueous barrier coating composition of carboxymethyl cellulose, cyclic monosaccharide, and kaolin particles provides a cost-effective and biodegradable oxygen barrier for packaging, enhancing recyclability and reducing carbon footprint while maintaining high performance.

WO2024218669A1PCT designated stage expired Publication Date: 2024-10-24STORA ENSO OYJ
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/IB2024/053733
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-21
Filing Date
2024-04-17
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Existing packaging materials for oxygen-sensitive products, such as food and pharmaceuticals, rely on costly and non-biodegradable polymer and aluminum layers to achieve oxygen barrier properties, which increase carbon dioxide load and hinder recyclability.

Method used

An aqueous barrier coating composition comprising 30-60% carboxymethyl cellulose, 20-40% cyclic monosaccharide or its derivative, and 25-35% platy-type kaolin particles, allowing for efficient application and providing excellent oxygen barrier properties while maintaining high total solids content and low viscosity.

Benefits of technology

The coating composition effectively reduces oxygen transmission rates and supports biodegradability and recyclability by offering a cost-effective, high-performance oxygen barrier that can be applied using conventional methods, thereby addressing the limitations of prior art materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 000001
    Figure 000001
  • Figure 000002
    Figure 000002
  • Figure 000003
    Figure 000003
Patent Text Reader

Abstract

The present invention relates to an aqueous barrier coating composition comprising: 30-60 % by weight of carboxymethyl cellulose, 20-40 % by weight of a cyclic monosaccharide or a derivative thereof and 25-35% by weight of platy-type kaolin particles, based on the total dry weight of the aqueous barrier coating composition. The cyclic monosaccharide or derivative thereof is in particular xylose.
Need to check novelty before this filing date? Find Prior Art

Description

[0001]BARRIER COATING FOR PAPER AND PAPERBOARD Technical field 5 The present disclosure relates to coating compositions for coating of fiber-based substrates, such as paper or paperboard to improve their barrier properties, particularly oxygen barrier properties. The disclosure further relates to fiber-based substrates coated with such coating compositions. 10 Background Effective gas, aroma, and / or moisture barriers are required in packaging industry for shielding sensitive products. Particularly, oxygen-sensitive products require an oxygen barrier to extend their shelf-life. Oxygen-sensitive products include many 15 food products, but also pharmaceutical products and electronic industry products. Known packaging materials with oxygen barrier properties may be comprised of one or several polymer films or of a fiber-based substrate, e.g. paper or board, coated with one or several layers of an oxygen barrier polymer, usually as part of a multilayer coating structure. 20 Barriers are normally created by coating the fiber-based substrate with a composition which gives the substrate barrier properties. Different coatings can be applied depending on the required barrier properties. The most commonly used materials when forming a barrier on a fiber-based substrate, are polyethylene 25 (PE), polypropylene (PP), polyethylene terephthalate (PET), ethylene vinyl alcohol (EVOH) or ethylene vinyl acetate (EVA). EVOH is normally used in order to create oxygen barriers and PE or PET is normally used in order to create a liquid and / or vapor barrier. The polymers are normally either laminated or extrusion coated to the fiber-based substrate. However, a polymer layer that gives a product barrier 30 properties normally needs to be relatively thick and it is thus quite costly to produce such barrier. The most common way to approach reduction of oxygen transmission (OTR) through a paper or paperboard is to use multiple polymer layers. In this way, one layer can provide low OTR, whereas layers can provide water repellency and / or low water vapor transmission rates. Another commonly used barrier material is aluminum. Aluminum layers are 5 typically used in order to improve the oxygen and light barrier of paper or paperboard products. The aluminum layers are thin, typically around 7-9 μm. Aluminum provides excellent barrier properties, but it significantly increases the carbon dioxide load of the product. 10 A problem with both polymer and aluminum layers is also that they decrease the biodegradability and the possibility to efficiently recycle the packaging materials. There is a demand from producers, converters and end users to avoid the use of synthetic polymer and aluminum layers in paper or paperboard products in order 15 to decrease the carbon dioxide load and improve the biodegradability and recyclability of the products. Therefore, there exists a need for improved processes for providing fiber-based substrates, such as paper or paperboard, with improved barrier properties. 20 Description of the invention of the present disclosure to provide a barrier film or coating for fiber- based substrates that alleviates at least some of the problems of prior art barrier 25 films and coatings. It is a further object of the present disclosure to provide a barrier film or coating for fiber-based substrates that provides good resistance to oxygen. 30 It is a further object of the present disclosure to provide a barrier film or coating, which can be efficiently applied to fiber-based substrates using conventional coating methods. According to a first aspect illustrated there is provided an aqueous barrier coating composition comprising: 30-60 % by weight of carboxymethyl cellulose; 5 20-40 % by weight of a cyclic monosaccharide or a derivative thereof; and 25-35% by weight of platy-type kaolin particles; 10 based on the total dry weight of the aqueous barrier coating composition. The present invention is based on the surprising realization that addition of the cyclic monosaccharide or a derivative thereof, in particular the cyclic monosaccharide xylose, to the coating system significantly improved the oxygen 15 barrier properties compared to a coating comprising only CMC and kaolin particles. The inventors have found that in addition to providing barrier films and coatings having excellent oxygen barrier properties, the combination of a relatively high 20 amount of carboxymethylcellulose, a cyclic monosaccharide or a derivative thereof and platy-type kaolin particles makes it possible to prepare aqueous barrier coating compositions with a high total solids content, such as at least 15-35 % by weight, while still maintaining a reasonably low viscosity. This allows for the aqueous barrier coating composition to be efficiently applied to a substrate using 25 conventional coating methods. The aqueous barrier coating composition comprises the carboxymethyl cellulose, and cyclic monosaccharide or a derivative thereof dissolved or dispersed in an aqueous medium. The platy-type kaolin particles are dispersed in an aqueous 30 medium. The aqueous medium may be water or an aqueous solution, or it may comprise a mixture of water or an aqueous solution with an organic solvent. In a preferred embodiment, the aqueous medium is water based, i.e., it is comprised of more than 50 % by weight of water. In a more preferred embodiment, the aqueous medium is water. The aqueous barrier coating can be a dilute or a high solids composition. However, a high solids composition is typically preferred. 5 An advantage of the inventive coating composition is that it allows high total solids content, such as 30 % by weight or even higher, while still maintaining a reasonably low viscosity. The terms “total solids content” or “solids content” as used herein refer to the total fraction of dissolved solids plus suspended and settleable solids in an aqueous solution or suspension. 10 The high solids content combined with low viscosity reduces transportation costs of the coating composition and makes it possible prepare coatings with high basis weight in a single coating step. A high solids content also reduces the amount of water to be removed when the film or coating is dried, which can reduce the drying 15 energy requirement of the coating process. Preferably, the total solids content of the coating composition is at least 10 % by weight, more preferably at least 20 %, or at least 30 % by weight based on the total weight of the coating composition. The total solids content of the coating composition is typically 90 % by weight or 20 less, preferably 80 % by weight or less, more preferably 70 % by weight or less, based on the total weight of the coating composition. In some embodiments the aqueous barrier coating composition has a total solids content in the range 10-90 % by weight, preferably in the range of 20-80 % by 25 weight, more preferably in the range of 30-70 % by weight, based on the total weight of the coating composition. The total solids content of the aqueous barrier coating composition comprises the carboxymethyl cellulose as its main component. The total solids content of the 30 aqueous barrier coating composition comprises 30-60 % by weight of carboxymethyl cellulose. In some embodiments, the aqueous coating composition comprises 40-50 % by weight of carboxymethyl on the total dry weight of the aqueous barrier coating composition. 5 The cyclic monosaccharide can be natural or prepared synthetically, e.g. by chemical or synthetic hydrolysis of a longer polysaccharide. Examples of cyclic monosaccharides useful in the present invention include xylose. The aqueous barrier coating composition comprises 20-40 % by weight of cyclic monosaccharide based on the total dry weight of the aqueous barrier coating 10 composition. A derivative of a cyclic monosaccharide means a compound obtained by modifying cyclic monosacchride to add, remove, or modify a functional group on the molecule. This can be done by, for example, replacing a hydroxyl group in a cyclic monosaccharide with an amino group, an acid group, a phosphate group or an acetate group or reacting the hydroxyl group with a long or short chain 15 chemical reagent or a compound obtained by oxidation of a carbon of a cyclic monosaccharide to a carboxyl group or undergoing the chemical processes like hydrogenation, ring opening reactions, oxidation and reduction of any kind. Examples of such derivatives are sorbitol and xylitol. 20 The total solids content of the aqueous barrier coating composition further comprises 25-35 % by weight of platy-type kaolin particles. As used herein, the term platy-type kaolin particles means particles having a shape factor in the range of from 5 to 30. "Shape factor" as used herein is a measure of an average value (on a weight average basis) of the ratio of mean particle diameter to particle 25 thickness for a population of particles of varying size and shape as measured using the electrical conductivity method and apparatus described in GB-A- 2240398 / U.S. Patent No.5,128,606 / EP-A-0528078. In the measurement method described in EP-A-0528078 the electrical conductivity of a fully dispersed aqueous suspension of the particles under test is caused to flow through an elongated tube. 30 Measurements of the electrical conductivity are taken between (a) a pair of electrodes separated from one another along the longitudinal axis of the tube, and (b) a pair of electrodes separated from one another across the transverse width of the tube, and using the difference between the two conductivity measurements, the shape factor of the particulate material under test is determined. More preferably, the platy-type kaolin used according to the present invention have a shape factor of at least 40, or at 50. In another aspect, the platy-type kaolin particles have a shape factor ranging from 30 to 60, such as a shape factor ranging from 30 to 40, a shape factor ranging from 40 to 50, or a shape factor 5 ranging from 45 to 50. In one embodiment, the platy-type kaolin particles have a shape factor ranging from 45 to 50 and at least 96% by weight of the kaolin particles have an equivalent spherical diameter of less than 2 μm, at least 80% by weight of the kaolin particles have an equivalent spherical diameter of less than 1 μm, and the amount of the kaolin particles having an equivalent spherical diameter 10 of less than about 0.25 μm ranges from 35% to 45% by weight. The D50 of the platy-type kaolin particles, determined using a Malvern Mastersizer 3000 using light scattering principle according to ISO13320:2009, is preferably in a range of from 0.4 μm to 3 μm. 15 The formulation of the aqueous barrier coating composition may vary greatly depending on the intended use of the coating and the coated substrate. In some embodiments, the total solids content of the aqueous barrier coating composition consists solely of the carboxymethyl cellulose, cyclic monosaccharide or a derivative thereof and platy-type kaolin particles. In other embodiments, the 20 coating composition may further include a wide range of ingredients in varying quantities to improve the end performance of the product or processing of the coating. In some embodiments, a plasticizer is added to the aqueous barrier coating 25 composition to increase the elasticity of the resulting films or coatings and make them less brittle. This allows the formed films or coatings to better withstand bending without losing their barrier properties. In some embodiments, the aqueous barrier coating composition comprises 1-10 % 30 by weight of a plasticizer based on the total dry weight of the aqueous barrier coating composition. In some embodiments, the plasticizer selected from the group consisting of glycerol, maltitol, ethylene glycol, glycol, butanediol, and combinations thereof. 5 In some embodiments a filler is added to the aqueous barrier coating composition to improve the barrier properties and the mechanical properties of the resulting films or coatings. In some embodiments, the aqueous barrier coating composition further comprises 10 1-30 % by weight of a filler based on the total dry weight of the aqueous barrier coating composition. In some embodiments, the filler is selected from the group consisting of TiO2, carbon black, lignin or carbonized lignin or a mixture thereof. 15 The coating composition is preferably provided in a formulation suitable for application to paper or paperboard using conventional paper coating equipment and techniques, such blade coaters and bar coaters. Accordingly, the coating composition may include 0.1-10% by weight of various additives to impart suitable 20 coating characteristics. Such coating additives may include, but are not limited to, a dispersing agent (e.g. a surfactant), a lubricant (e.g. a stearate), a rheology modifier, an insolubilizer, a humectant, a barrier chemical, and a pH adjusting agent (e.g. NaOH). 25 The aqueous barrier coating composition can be applied to a substrate and dried to form a barrier film or coating. Thus, according to a second aspect illustrated herein, there is provided a barrier film or coating comprising: 30-60 % by weight of carboxymethyl cellulose; 30 20-40 % by weight of a cyclic monosaccharide or a derivative thereof; and 25-35% by weight of platy-type kaolin particles; based on the total dry weight of the film or coating. The barrier film or coating is preferably dry or substantially dry. The barrier film or coating preferably has a total solids content above 90 % by weight, preferably 5 above 95 % by weight. It is understood that the composition of the barrier film or coating according to the second aspect will correspond to the composition of the total solids content of the aqueous barrier coating composition according to the first aspect. For example a 10 dry content of 30-60 % by weight of carboxymethyl cellulose in the aqueous barrier coating composition results in a content of 30-60 % by weight of carboxymethyl cellulose in the dry barrier film or coating. The film or coating according to the invention may generally have a basis weight of 15 30 g / m2or less. Typically, a basis weight of at least 10 g / m2is required to obtain acceptable barrier properties. In some embodiments, the basis weight of the film or coating is in the range of 10-55 g / m2, preferably in the range of 10-20 g / m2. In one embodiment, the film or coating according to the present invention is provided in one layer. In one embodiment, the film or coating according to the present 20 invention is provided in more than one layer, such as one two layers or three layers. For example, two layers may be provided, wherein each layer has a basis weight of 5-10 g / m2, such as 7-8 g / m2. The film or coating according to the invention may generally have a thickness of 25 100 µm or less. In particular, the film or coating may have a thickness of 50 µm or less, or more specifically the film or coating may have a thickness of 15 µm or less or 10 µm or less. In some embodiments, the thickness of the film or coating is in the range of 1-15 µm, preferably in the range of 5-10 µm. 30 The barrier film or coating is preferably prepared from an aqueous barrier coating composition as described above with reference to the first aspect. The inventive barrier film or coating has good oxygen barrier properties. In some embodiments, the film or has an oxygen transmission rate (OTR), measured according to the standard D-3985 at 50% relative humidity and 23 °C, of less than 20 cc / m2 / 24h / atm, preferably less than 10 cc / m2 / 24h / atm, and more preferably less than 5 cc / m2 / 24h / atm and most preferably less than 2 5 cc / m2 / 24h / atm. In some embodiments, the film or coating has a KIT value above 8, preferably above 10 or above 11, as measured according to standard TAPPI T559. 10 According to a third aspect illustrated herein, there is provided a coated substrate comprising a substrate coated with an aqueous barrier coating composition according to the first aspect. The aqueous barrier coating composition according to the first aspect is of 15 particular interest for coating of fiber-based substrates. Thus, in some embodiments, the coated substrate is a fiber-based substrate. The fiber-based substrate is preferably a paper or paperboard or a moulded fiber product, which may also be referred to as a formed fiber product. 20 Paper generally refers to a material manufactured in sheets or rolls from the pulp of wood or other fibrous substances comprising cellulose fibers, used for e.g. writing, drawing, or printing on, or as packaging material. Paper can either be bleached or unbleached, coated or uncoated, and produced in a variety of thicknesses, depending on the end-use requirements. 25 Paperboard generally refers to strong, thick paper or cardboard comprising cellulose fibers used for example as flat substrates, trays, boxes and / or other types of packaging. Paperboard can either be bleached or unbleached, coated or uncoated, and produced in a variety of thicknesses, depending on the end-use 30 requirements. The aqueous barrier coating composition can either be added on the papermaking machine (on-machine coating) or on a separate machine (off-machine coating). A variety of paper coating equipment and techniques may be used for applying the coating composition, for example air knife coaters, and cast coaters. The coating composition can applied to one side or both sides of the paper or paperboard. 5 The surface of the paper or paperboard on which the aqueous barrier coating is to be applied may preferably be pre-treated, e.g. by dispersion coating mineral coating, to decrease the porosity of the surface. This way the amount of the aqueous barrier coating can be reduced. Thus, in some embodiments, coated substrate is a dispersion coated, preferably mineral coated, paper or paperboard. 10 The coated substrate is preferably suitable for being repulped. In some embodiments, the coated substrate has a repulpability characterized by a reject rate (as determined according to the PTS RH 021 / 97 test method) below 20%, preferably below 10%, more preferably below 5%, and most preferably below 1%. 15 According to a fourth aspect illustrated herein, there is provided a method for the manufacture of a barrier film or coating, comprising: a) preparing an aqueous barrier coating composition according to the first 20 aspect; b) forming a wet film or coating of the aqueous barrier coating composition; and c) drying the wet film or coating to obtain the barrier film or coating. 25 In some embodiments the aqueous barrier coating composition has a total solids content in the range 10-90 % by weight, preferably in the range of 20-80 % by weight, more preferably in the range of 30-70 % by weight, based on the total weight of the coating composition. 30 In the drying step c), the total solids content of the wet film or coating is increased by evaporation of water. The resulting barrier film or coating preferably has a total solids content above 90 % by weight. In some embodiments, the basis the dried barrier film or coating is in the range of 5-15 g / m2, preferably in the range of 5-10 g / m2. In some embodiments, the thickness of the dried barrier film or coating is in the 5 range of 5-15 µm, preferably in the range of 5-10 µm. The term coating as used herein refers generally to a finishing operation in which the surface of a substrate, e.g. a fiber-based substrate such as a paper or paperboard, is covered with a composition to impart a desired finish or texture to 10 the substrate or to improve its printability or other properties, such as optical or barrier properties. The term barrier coating as used herein refers generally to a coating designed to impart improved barrier properties to the substrate. The term film as used herein refers generally to a thin continuous sheet formed 15 material. The term barrier film as used herein refers generally to a film designed to provide good barrier properties. Generally, while the products, polymers, materials, layers and processes are described in terms of “comprising” various components or steps, the products, 20 polymers, materials, layers and processes can also “consist essentially of” or “consist of” the various components and steps. While the invention has been described with reference to various exemplary embodiments, it will be understood by those skilled in the art that various changes 25 may be made and equivalents may be substituted for elements thereof without departing from the scope of the invention. In addition, many modifications may be made to adapt a particular situation or material to the teachings of the invention without departing from the essential scope thereof. Therefore, it is intended that the invention not be limited to the particular embodiment disclosed as the best 30 mode contemplated for carrying out this invention, but that the invention will include all embodiments falling within the scope of the appended claims. EXAMPLES Materials: - CMC powder, moisture content <10% (Nouryon) - Xylose powder, purity 99%, moisture content 1% (Sigma-Aldrich) 5 - Platy-type kaolin dispersion, 70wt% (Kamin) - Platy type kaolin powder “Supreme” grade (Imerys) - Dried Xylan powder, DP 2-7, 95wt% purity (Coreychem) Preparation of CMC / water dispersion: 10 A 8,5 wt% CMC mixture was prepared by adding gradually 8,5 g of CMC into a stirred and heated vessel at 40°C containing 91,5 g of water. The rotational speed was slowly increased up to 1000 RPM as the CMC dissolves and the viscosity increases. The mixture had a final viscosity of 2200 mPas (Brookfield, spindle 2 at 23°C, 20 RPM). 15 Preparation of xylose / water mixture: A 60 wt% xylose mixture was prepared by adding gradually 60 g of xylose powder into a stirred and heated vessel at 40°C containing 40 g of water. 20 Preparation of xylan / water mixture: A 45,7 wt% xylan mixture was prepared by adding gradually 45,7 g of xylan powder into a stirred and heated vessel at 40°C containing 54,3 g of water. Preparation of sorbitol / water mixture: 25 A 70 wt% sorbitol mixture was prepared by adding gradually 70 g of sorbitol powder into a stirred and heated vessel at 40°C containing 30 g of water. Preparation of Supreme / water mixture: A 36 wt% xylose mixture was prepared by adding gradually 60 g of Supreme 30 powder into a stirred vessel containing 64 g of water. The mixture was left under stirring using a high shear disc at 1400 RPM (Dispermill device). Preparation of the different coating CMC based formulations containing components were mixed in various composition (see Table 1) were prepared at room temperature. All chemical components were mixed using a Dispermill device at room temperature in the 5 following order: platy like minerals first gradually added to CMC under stirring. Then xylose, xylans or sorbitol was added last. Once all chemical elements were added, the formulation was left under stirring for 30min at 1300-1600 RPM. Then air bubbles were removed using high centrifugal forces under low vacuum. 10 Coating of paperboard: The coating formulations were applied on the fiber side (Natura RFA) paperboard with a TQC Sheen laboratory coater using a grooved rod. In total 2 layers of a same formulation were applied on each paperboard. After each layer, the coated paperboard was oven-dried at 105°C for 2-5 min. The samples were then 15 conditioned at 23 °C and 50 % relative humidity for 48 hours before being analyzed. Analysis: The coated samples were tested for total coat weight and oxygen transmission 20 rate (OTR) as follows: - The coat weight was measured using the oven drying method by comparing the dry weight of the base board and the coated sample. - The oxygen transfer rate (OTR) was measured in accordance to ASTM 25 D3985 at a temperature of 23°C and at 50 % relative humidity (RH) using a Mocon Ox-Tran device 2 / 22. 30 Table 1. Sample 1 2 3 4 5 Ref** CMC 70% 70% 45% 45% 45% - Xylan - - 25% - - - Xylose - - - 25% - - Sorbitol - - - - 25% - (Plastilys) Platy type 30% - 30% 30% 30% - minerals (Kamin) Platy type - 30% - - - - minerals (Imerys) Coat 2 weight 12.25 11.48 15 20.73 19.35 0 (g / m ) OTR 321.3 3.8 1.1 0.6 0.4 OR* (cm / day*m ) Coating 7.4% 10.3% 15.9% 16.3% 16.5% - color dry content Normalized 0.106 0.331 0.073 0.029 0.021 - OTR (OTR / coat weight) *Over range >2000 cm3 / (day·m2) **Reference base board without coating

Claims

CLAIMS 1. An aqueous barrier coating composition comprising: 5 30-60 % by weight of carboxymethyl cellulose; 20-40 % by weight of a cyclic monosaccharide or a derivative thereof; and 25-35% by weight of platy-type kaolin particles; 10 based on the total dry weight of the aqueous barrier coating composition.

2. An aqueous barrier coating composition according to claim 1, comprising 40-60 % by weight of carboxymethyl cellulose based on the total dry weight of the 15 aqueous barrier coating composition.

3. An aqueous barrier coating composition according to any one of the preceding claims, wherein the cyclic monosaccharide or derivative thereof is selected from the group consisting of xylose, xylan, sorbitol, or combinations 20 thereof.

4. An aqueous barrier coating composition according to claim 3, wherein the cyclic monosaccharide or derivative thereof is selected from the group consisting of xylose, sorbitol, or combinations thereof. 25 5. An aqueous barrier coating composition according to claim 4, wherein the cyclic monosaccharide is xylose.

6. An aqueous barrier coating composition according to any one of the 30 preceding claims, further comprising 1-10 % by weight of a plasticizer based on the total dry weight of the aqueous barrier coating composition.

7. An aqueous barrier coating according to claim 6, wherein the plasticizer is selected from the group of glycerol, maltitol, ethylene glycol, propylene glycol, butanediol, and combinations thereof. 5 8. An aqueous barrier coating composition according to any one of the preceding claims, further comprising 5-40 % by weight of a filler based on the total dry weight of the aqueous barrier coating composition.

9. An aqueous barrier coating composition according to claim 8, wherein the 10 filler is selected from the group consisting of clay, talcum, CaCO3, and fibers, or combinations thereof.

10. A barrier film or coating comprising: 15 30-60 % by weight of carboxymethyl cellulose; 20-40 % by weight of a cyclic monosaccharide or a derivative thereof; and 25-35% by weight of platy-type kaolin particles; 20 based on the total dry weight of the barrier film or coating.

11. A barrier film or coating according to claim 10, wherein the basis weight of the film or coating is in the range of 5-15 g / m2, preferably in the range of 5-10 25 g / m2.

12. A coated substrate comprising a substrate coated with an aqueous barrier coating composition according to any one of claims 1-11. 30 13. A coated substrate according to claim 12, wherein the coated substrate is a fiber-based substrate, preferably a paper or paperboard or a moulded fiber product, preferably a mineral coated paper or paperboard.

14. A coated substrate according one of claims 12-13, wherein said coated substrate has a repulpability by a reject rate (as determined according to the PTS RH 021 / 97 test method) below 20%, preferably below 10%, more preferably below 5%, and most preferably below 1%. 5 15. A method for the manufacture of a barrier film or coating, comprising: a) preparing an aqueous barrier coating composition according to any one of claims 1-9; 10 b) forming a wet film or coating of the aqueous barrier coating composition; and c) drying the wet film or coating to obtain the barrier film or coating. 15

Citation Information

Patent Citations

  • Paperboard and laminate comprising a BIO-barrier

    WO2021005451A1

  • Coated paper and paperboard structures

    WO2021126477A1

  • Coating structure, sheet-like product and its use

    WO2021255334A1

  • Barrier coating for paper and paperboard

    WO2022259134A1