Electrode assembly and method of manufacturing electrode assembly

The electrode assembly addresses stability and productivity issues by folding the cathode around the anode with a separator, allowing for separate manufacturing and storage of units, which enhances stability and assembly efficiency.

WO2024219867A1PCT designated stage expired Publication Date: 2024-10-24LG ENERGY SOLUTION LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2024/005271
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2024-04-18
Filing Date
2024-04-19
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Conventional electrode assemblies face challenges in manufacturing stability and productivity due to exposure to external impacts, risk of short circuits, difficulty in disassembling and reassembling, inconsistent folding structures, and reduced battery capacity, particularly in zigzag and jelly-roll types.

Method used

The electrode assembly features a cathode folded to surround the anode with a separator in between, allowing for improved stability and productivity through separate manufacturing and storage of electrode units and anodes, enabling easier assembly and reduced risk of damage during manufacturing.

Benefits of technology

This design enhances manufacturing stability and productivity by preventing external damage, simplifying the assembly process, and maintaining consistent folding structures, thereby improving the overall efficiency and capacity of the electrode assembly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2024005271_24102024_PF_FP_ABST
    Figure KR2024005271_24102024_PF_FP_ABST
Patent Text Reader

Abstract

An electrode assembly according to one embodiment of the present invention is formed from sequentially stacking an electrode unit and an assembly cathode, wherein the electrode unit includes: an anode of which first surfaces are folded in the direction of facing each other; a unit cathode positioned between the folded first surfaces; and a first separator positioned between the first surfaces and the unit cathode, the first surfaces cover the top and bottom surfaces of the unit cathode and one side surface of the unit cathode, and two end portions of the first surfaces extend along the top and bottom surfaces of the unit cathode.
Need to check novelty before this filing date? Find Prior Art

Description

Electrode assembly and method for manufacturing electrode assembly

[0001] Cross-citation with related application(s)

[0002] This application claims the benefit of priority to Korean Patent Application No. 10-2023-0051864, filed April 20, 2023, and Korean Patent Application No. 10-2024-0052125, filed April 18, 2024, the entire contents of which are incorporated herein by reference.

[0003] The present invention relates to an electrode assembly and a method for manufacturing an electrode assembly, and more particularly, to an electrode assembly and a method for manufacturing an electrode assembly having improved manufacturing stability and productivity.

[0004] As technological developments and demand for mobile devices increase, the demand for secondary batteries as an energy source is rapidly increasing. In particular, secondary batteries are attracting significant attention as an energy source not only for mobile devices such as cell phones, digital cameras, laptops, and wearable devices, but also for powertrains such as electric bicycles, electric cars, and hybrid electric vehicles.

[0005] These secondary batteries are classified into cylindrical batteries and prismatic batteries in which the electrode assembly is built into a cylindrical or prismatic metal can, depending on the shape of the battery case, and pouch-type batteries in which the electrode assembly is built into a pouch-type case made of aluminum laminate sheet. Here, the electrode assembly built into the battery case is a power plant capable of charging and discharging, consisting of a positive electrode, a negative electrode, and a separator structure interposed between the positive electrode and the negative electrode, and is classified into a jelly-roll type in which a separator is interposed between long sheets of an active material-coated positive electrode and negative electrode and rolled up, a stack type in which a plurality of positive electrodes and negative electrodes are sequentially stacked while interposing the separator, and a zigzag type in which the negative electrode is wrapped with a separator and then the positive electrodes are cross-stacked on both sides of the separator and folded in a zigzag shape.

[0006] Figures 1 and 2 are drawings showing cross-sections of a conventional electrode assembly.

[0007] As shown in Fig. 1, the stacked electrode assembly (10) has a structure in which a negative electrode (11) having a negative active material layer (11a) positioned on the upper and lower surfaces of a negative electrode current collector (11b), a positive electrode (15) having a positive active material layer (15b) positioned on the upper and lower surfaces of a positive electrode current collector (15a), and a separator interposed between the negative electrode (11) and the positive electrode (15) are sequentially stacked. In particular, since the side surface of the electrode assembly of the stacked electrode assembly (10) is exposed to the outside, each component can be easily damaged by external impact, and stability can be reduced due to the risk of short circuit.

[0008] In addition, as shown in FIG. 2, the zigzag-shaped electrode assembly (20) has a structure in which a negative electrode (21) is wrapped with a separator (29a, 29b) and a positive electrode (25) is cross-laminated on both sides of the separator (29a, 29b), and the negative electrode (21) is folded in a zigzag shape. Here, the negative electrode (21) includes a negative electrode active material layer (21a), a negative electrode current collector (not shown), and a negative electrode tab (21b), and the positive electrode (25) includes a positive electrode active material layer (25a), a negative electrode current collector (not shown), and a positive electrode tab (25b). Here, the negative electrode current collector (not shown) is positioned inside the negative electrode active material layer (21a), and a negative electrode tab (21b) extending from the negative electrode current collector (not shown) extends to the outside of the negative electrode (21). This can be explained in the same way for the positive electrode (25).

[0009] However, in the case of a zigzag-shaped electrode assembly (20), since one cathode (21) has a structure in which it is folded in a zigzag shape, it is difficult to disassemble and reassemble the electrode assembly (20) in the event of a manufacturing defect. In other words, it is impossible to reuse the cathode (21), which causes a problem in that productivity is reduced.

[0010] In addition, in the case of the zigzag-shaped electrode assembly (20), since the negative electrode (21) has a relatively long length, it may not be easy to fold it at a constant interval when folding it in a zigzag shape. In particular, when manufacturing the zigzag-shaped electrode assembly (20), it may be difficult to manufacture the folding structure of the negative electrode (21) consistently due to an error in the position where the positive electrode (25) is laminated on the negative electrode (21). In addition, if floating occurs during the manufacturing process of the zigzag-shaped electrode assembly (20), there is a problem of reduced productivity because the entire manufacturing process is stopped.

[0011] In addition, although not shown in FIGS. 1 and 2, similar to the zigzag-shaped electrode assembly (20), in the case of a jelly-roll-shaped electrode assembly in which a separator is interposed between long sheet-shaped positive and negative electrodes coated with active materials and rolled up, it may not be easy to roll up at a constant interval during rolling, and if floating occurs during the manufacturing process, the entire manufacturing process is stopped, which causes a problem of reduced productivity. In particular, in the case of a jelly-roll-shaped electrode assembly, the thickness of the active material layer may differ depending on the upper and lower positions to facilitate rolling, which causes problems such as a decrease in battery capacity.

[0012] Accordingly, there is a need to develop an electrode assembly having a structure with improved manufacturing stability and productivity, unlike conventional electrode assemblies.

[0013] The problem to be solved by the present invention is to provide an electrode assembly and a method for manufacturing an electrode assembly with improved manufacturing stability and productivity.

[0014] The problems to be solved by the present invention are not limited to the problems described above, and problems not mentioned can be clearly understood by a person having ordinary skill in the art to which the present invention pertains from this specification and the attached drawings.

[0015] An electrode assembly according to one embodiment of the present invention is an electrode assembly in which an electrode unit and an assembly anode are sequentially stacked, wherein the electrode unit includes a cathode folded in a direction in which first surfaces face each other; a unit anode positioned between the folded first surfaces; and a first separator positioned between the first surface and the unit anode, wherein the first surface surrounds upper and lower surfaces of the unit anode and one side of the unit anode, and both ends of the first surface extend along upper and lower surfaces of the unit anode.

[0016] The first separator is attached to the first surface, and both ends of the first separator may extend to both ends of the first surface.

[0017] The two ends of the first separator extend across the upper and lower surfaces of the unit anode to the other side of the unit anode, and the two ends of the first separator may be joined to each other on the other side of the unit anode.

[0018] The two ends of the cathode extend across the upper and lower surfaces of the unit anode to the other side of the unit anode, and the two ends of the cathode may be joined to each other on the other side of the unit anode.

[0019] The above first separator may be attached to the upper and lower surfaces of the unit anode and to both sides of the unit anode.

[0020] The first separator is attached to the upper and lower surfaces of the unit anode and one side of the unit anode, and both ends of the first separator may extend along the upper and lower surfaces of the unit anode, respectively.

[0021] The two ends of the first separator extend across the upper and lower surfaces of the unit anode to the other side of the unit anode, and the two ends of the first separator may be joined to each other on the other side of the unit anode.

[0022] The assembly anode is positioned on a second surface opposite the first surface, and further includes a second separator positioned between the assembly anode and the second surface and attached to the second surface, and both ends of the second separator may extend to both ends of the second surface, respectively.

[0023] The two ends of the second separator may extend across the sides of the two ends of the cathode to the sides of the unit anode, and the two ends of the second separator may be joined to each other on the other side of the unit anode.

[0024] The two ends of the cathode extend across the upper and lower surfaces of the unit anode to the other side of the unit anode, and the two ends of the cathode may be joined to each other on the other side of the unit anode.

[0025] The assembly anode may further include an external separator positioned on a second surface opposite the first surface, positioned between the assembly anode and the second surface, and attached to at least a portion of the surface of the assembly anode.

[0026] The above outer separator may include a first outer separator attached to the upper surface of the assembly anode and a second outer separator attached to the lower surface of the assembly anode.

[0027] The above outer separator may be attached to the upper and lower surfaces of the assembly anode and both sides of the assembly anode.

[0028] The above outer separator is attached to the upper and lower surfaces of the assembly anode and one side of the assembly anode, and both ends of the outer separator may extend along the upper and lower surfaces of the assembly anode, respectively.

[0029] Both ends of the outer separator extend across the upper and lower surfaces of the assembly anode to the other side of the assembly anode, and on the other side of the assembly anode, both ends of the outer separator may be joined to each other.

[0030] At least one negative electrode tab included in the negative electrode and the unit positive electrode tab included in the unit positive electrode extend in the same direction, and the at least one negative electrode tab is positioned on the same vertical line, and the at least one negative electrode tab and the unit positive electrode tab can be positioned on different vertical lines.

[0031] At least one cathode tab included in the cathode and one unit anode tab included in the unit anode may extend in different directions.

[0032] The at least one cathode tab may be a cathode tab extending along one side of the cathode.

[0033] According to another embodiment of the present invention, a method for manufacturing an electrode assembly comprises the steps of: marking a folding line indicated at the center of a first surface of the cathode; folding the first surface of the cathode based on the folding line; positioning the unit anode on a portion of the folded first surface; and folding the remaining portion of the first surface toward the upper surface of the unit anode based on the folding line, wherein the first separator may be attached to the first surface or may be attached to at least a portion of an outer surface of the unit anode.

[0034] The method further includes a step of positioning an assembly anode on a second surface opposite to the first surface positioned on the upper surface of the unit anode, and includes a second separator or an outer separator positioned between the second surface and the assembly anode, wherein the second separator is attached to the second surface, and the outer separator may be attached to at least a portion of an outer surface of the assembly anode.

[0035] According to embodiments, the present invention provides an electrode assembly in which an electrode unit and an assembly anode are sequentially laminated, and a method for manufacturing the same, wherein a cathode included in the electrode unit has a structure in which the cathode is folded to surround the upper and lower surfaces and one side of the anode, so that manufacturing stability and productivity can be improved.

[0036] The effects of the present invention are not limited to the effects described above, and effects not mentioned can be clearly understood by a person having ordinary skill in the art to which the present invention pertains from this specification and the attached drawings.

[0037] Figures 1 and 2 are drawings showing cross-sections of a conventional electrode assembly.

[0038] Figure 3 is a perspective view of an electrode assembly according to one embodiment of the present invention.

[0039] Fig. 4 is a drawing showing a cross-section of the electrode assembly of Fig. 3.

[0040] FIGS. 5 to 10 are perspective views of electrode units included in an electrode assembly according to another embodiment of the present invention.

[0041] FIG. 11 is a perspective view of an assembly anode included in an electrode assembly according to another embodiment of the present invention.

[0042] FIG. 12 and FIG. 13 are drawings showing a method for manufacturing an electrode unit included in an electrode assembly according to one embodiment of the present invention.

[0043] FIGS. 14 to 16 are perspective views showing various arrangement forms of positive and negative tabs in an electrode unit included in an electrode assembly according to another embodiment of the present invention.

[0044] FIG. 17 is a drawing showing a form in which an electrode unit and an assembly anode included in an electrode assembly according to one embodiment of the present invention are stored.

[0045] Hereinafter, various embodiments of the present invention will be described in detail with reference to the attached drawings so that those skilled in the art can easily implement the invention. The present invention may be implemented in various different forms and is not limited to the embodiments described herein.

[0046] In order to clearly explain the present invention, parts that are not related to the description are omitted, and the same reference numerals are used for identical or similar components throughout the specification.

[0047] Furthermore, the sizes and thicknesses of each component shown in the drawings are arbitrarily indicated for convenience of explanation, and thus the present invention is not necessarily limited to the illustrated components. In the drawings, the thicknesses are enlarged to clearly represent various layers and regions. Furthermore, in the drawings, the thicknesses of some layers and regions are exaggerated for convenience of explanation.

[0048] Additionally, throughout the specification, whenever a part is said to “include” a component, this does not mean that it excludes other components, but rather that it may include other components, unless otherwise specifically stated.

[0049] Additionally, throughout the specification, when we say "in plan", we mean when the target portion is viewed from above, and when we say "in cross section", we mean when the target portion is viewed from the side in a cross-section cut vertically.

[0050] Hereinafter, an electrode assembly according to one embodiment of the present invention will be described in detail.

[0051] Fig. 3 is a perspective view of an electrode assembly according to one embodiment of the present invention. Fig. 4 is a drawing showing a cross-section of the electrode assembly of Fig. 3.

[0052] Referring to FIGS. 3 and 4, an electrode assembly (100) according to one embodiment of the present invention may be an electrode assembly in which an electrode unit (200) and an assembly anode (300) are sequentially stacked. More specifically, the electrode assembly (100) may have an assembly anode (300) stacked on an electrode unit (200) with the electrode unit (200) positioned at the bottommost surface, and this structure may be repeated multiple times.

[0053] Here, the assembly anode (300) is a component distinct from the electrode unit (200), and the assembly anode (300) is sequentially stacked with the electrode unit (200) to form the electrode assembly (100), and the assembly anode (300) can be located on the outside of the electrode unit (200). In other words, the assembly anode (300) can mean an anode located on the upper surface and / or lower surface of the electrode unit (200).

[0054] In addition, in the electrode assembly (100) according to one embodiment of the present invention, as shown in FIGS. 3 and 4, the electrode units (200) and the assembly anodes (300) are sequentially stacked, and the cathodes (210) included in one electrode unit (200) and the cathodes (210) included in another electrode unit (200) may be separated, and the assembly anodes (300) may also be separated from one another. In other words, the assembly anodes (300) are arranged between the electrode units (200) that are positioned adjacent to each other, so that the cathodes (210) included in each of the electrode units (200) that are positioned adjacent to each other may be spaced apart from each other. In addition, the electrode units (200) are arranged between the assembly anodes (300) that are positioned adjacent to each other, so that the assembly anodes (300) that are positioned adjacent to each other may be spaced apart from each other.

[0055] Accordingly, the electrode assembly (100) according to the present embodiment can be manufactured by sequentially stacking electrode units (200) and assembly anodes (300) that have been manufactured and / or stored in advance in a semi-finished state, thereby simplifying the manufacturing process of the electrode assembly (100) and increasing the production speed. In addition, the electrode assembly (100) according to the present embodiment has the advantage that the electrode units (200) and assembly anodes (300) can be manufactured and / or stored individually, so that the manufacturing and storage processes of the electrode units (200) and assembly anodes (300) are separated, and the productivity and manufacturing stability of the electrode assembly (100) are improved. Referring to FIGS. 3 and 4, the electrode unit (200) includes: a cathode (210) folded in a direction in which first surfaces face each other; a unit anode (250) positioned between the folded first surfaces; And it includes a first separator (410) positioned between the first surface and the unit anode (250).

[0056] Here, the unit anode (250) is a component included in the electrode unit (200), and the unit anode (250) constitutes the electrode unit (250) by being positioned between the first faces where the cathode (210) is folded, and the unit anode (250) can be positioned inside the electrode unit (200). In other words, the unit anode (300) can mean an anode positioned between the first faces where the cathode (210) of the electrode unit (200) is folded.

[0057] More specifically, the negative electrode (210) may include a negative electrode active material layer (211) and a negative electrode tab (215). In addition, although not shown in FIGS. 3 and 4, the negative electrode active material layer (211) may be positioned on at least one of the upper and lower surfaces of a negative electrode current collector (not shown). For example, the negative electrode (210) may have the negative electrode active material layer (211) formed on the upper and lower surfaces with a negative electrode current collector (not shown) interposed therebetween, as shown in FIGS. 3 and 4. Here, since the negative electrode current collector (not shown) is positioned inside the negative electrode active material layer (211), the negative electrode current collector (not shown) is omitted in the drawings for convenience of explanation. In addition, the negative electrode tab (215) may be a portion extending from the negative electrode current collector (not shown), and may be a portion on the upper and lower surfaces of the negative electrode current collector (not shown) where the negative electrode active material layer (211) is not positioned. For example, the negative electrode tab (215) may protrude outward from one of the side surfaces of the negative electrode current collector (not shown) positioned inside the negative electrode active material layer (211).

[0058] The negative electrode current collector (not shown) is not particularly limited as long as it has high conductivity without causing chemical changes in the battery, and for example, copper, stainless steel, aluminum, nickel, titanium, calcined carbon, copper or stainless steel surface-treated with carbon, nickel, titanium, silver, etc., aluminum-cadmium alloy, etc. can be used.

[0059] The negative electrode active material layer (211) can be manufactured in a form in which a negative electrode slurry containing a negative electrode active material is attached or applied on the negative electrode current collector (not shown), and the negative electrode slurry can further include a conductive material and a polymer material in addition to the negative electrode active material.

[0060] More preferably, the negative electrode active material may be lithium metal. That is, in this case, the negative electrode active material layer (211) may refer to a lithium metal layer. In particular, lithium metal is softer than graphite used in conventional negative electrodes, and lithium metal has the characteristic of being foldable. In addition, lithium metal has the advantage of being easily bonded to other components even with relatively light compression compared to materials used in conventional negative electrodes.

[0061] Accordingly, in the electrode assembly (100) according to the present embodiment, the negative electrode active material layer (211) included in the negative electrode (210) may include lithium metal (metal), so that the negative electrode (210) may have a folding structure with the unit positive electrode (250) therebetween, as shown in FIGS. 3 and 4. In addition, as described below, since the negative electrode (210) included in the electrode unit (200) has relatively high bonding properties, there is an advantage in that the electrode unit (200) and the positive electrode (300) can be assembled in a P&P (Pick and Place) manner when manufacturing the electrode assembly (100).

[0062] In addition, the unit positive electrode (250) may include a unit positive electrode active material layer (251), a unit positive electrode current collector (not shown), and a unit positive electrode tab (255). In addition, although not shown in FIGS. 3 and 4, the unit positive electrode active material layer (251) may be positioned on at least one of the upper and lower surfaces of the unit positive electrode current collector (not shown). For example, the unit positive electrode (250) may have the unit positive electrode active material layer (251) formed on the upper and lower surfaces with the unit positive electrode current collector (not shown) interposed therebetween, as shown in FIGS. 3 and 4. Here, the unit positive electrode current collector (not shown) is omitted from the drawings for convenience of explanation since it is positioned inside the unit positive electrode active material layer (211). In addition, the unit positive electrode tab (255) may be a portion of the upper and lower surfaces of the unit positive electrode current collector (not shown) where the unit positive electrode active material layer (251) is not positioned. For example, the unit positive electrode tab (255) may protrude outward from one side of the unit positive electrode current collector (not shown) located inside the unit positive electrode active material layer (251).

[0063] The above unit cathode current collector (not shown) is not particularly limited as long as it has high conductivity without causing chemical changes in the battery, and for example, stainless steel, aluminum, nickel, titanium, calcined carbon, or aluminum or stainless steel surface-treated with carbon, nickel, titanium, silver, etc. can be used.

[0064] The unit cathode active material layer (251) can be manufactured in a form in which a cathode slurry containing a cathode active material is attached or applied on the unit cathode current collector (not shown), and the cathode slurry may further include a conductive material and a polymer material in addition to the cathode active material. The cathode active material may include, for example, lithium cobalt oxide (LiCoO2), lithium nickel oxide (LiNiO2); lithium manganese oxide; lithium copper oxide (Li2CuO2); vanadium oxide; Ni-site type lithium nickel oxide; lithium manganese composite oxide; spinel structured lithium manganese composite oxide; LiMn2O4 in which a portion of the chemical formula Li is substituted with an alkaline earth metal ion; disulfide compounds; Fe2(MoO4)3, etc. However, the present invention is not limited thereto, and a material generally used in a lithium secondary battery may be applied as the cathode active material.

[0065] More specifically, based on the state before the cathode (210) is folded as shown in FIGS. 3 and 4, the first surface may be one of the upper surface and the lower surface of the cathode (210). For example, when the first surface is the upper surface of the cathode (210), the cathode (210) may be folded in a direction in which the upper surfaces of the cathodes (210) face each other. Conversely, when the first surface is the lower surface of the cathode (210), the cathode (210) may be folded in a direction in which the lower surfaces of the cathodes (210) face each other. In addition, the unit anode (250) may be positioned between the folded first surfaces. More specifically, the distance between the folded first surfaces of the cathode (210) may be equal to or greater than the thickness of the unit anode (250).

[0066] In addition, in the electrode unit (200), the first surface of the cathode (210) surrounds the upper and lower surfaces of the unit anode (250) and one side of the unit anode (250), and both ends of the first surface extend along the upper and lower surfaces of the unit anode (250). For example, the cathode (210) may have a structure that is folded once and may surround the upper and lower surfaces of the unit anode (250) and one side of the unit anode (250). As another example, the cathode (210) may have a bent shape like the letter C and may surround the upper and lower surfaces of the unit anode (250) and one side of the unit anode (250). That is, the other side of the unit anode (250) may not be covered by the cathode (210).

[0067] Additionally, in the electrode unit (200), the first separator (410) may be positioned between the first surface of the cathode (210) and the unit anode (250). As described below, the first separator (410) may be attached to the first surface of the cathode (210) or the unit anode (250).

[0068] Here, the first separator (410) separates the negative electrode (210) and the unit positive electrode (250) and provides a passage for lithium ions to move. If it is a separator commonly used in lithium secondary batteries, it can be used without any special restrictions. In particular, it is preferable that it has low resistance to ion movement of the electrolyte and excellent electrolyte moisture retention capacity.

[0069] Accordingly, in the electrode assembly (100) according to the present embodiment, the cathode (210) included in the electrode unit (200) has a structure in which the unit anode (250) is folded to surround the unit anode (250), thereby preventing the unit anode (250) from being exposed to the outside, thereby preventing it from being easily damaged by external impact, and improving stability against the risk of short circuit. In addition, the electrode unit (200) can be stored in a semi-finished product state having the above-described structure, so that it can be stored separately even if floating occurs during the manufacturing process, and there is an advantage in that productivity and manufacturing stability are improved.

[0070]

[0071] FIGS. 5 to 10 are perspective views of electrode units included in an electrode assembly according to another embodiment of the present invention.

[0072] Referring to FIGS. 4 to 7, in an electrode unit (200, 200a, 200b) included in an electrode assembly (100) according to one embodiment of the present invention, a first separator (410, 410a, 410b) may be attached to the first surface of the cathode (210, 210a, 210b). More specifically, in the electrode unit (200, 200a, 200b), both ends of the first separator (410) may extend to both ends of the first surface of the cathode (210, 210a, 210b).

[0073] Referring to FIGS. 8 to 10, in the electrode unit (200c, 200d, 200e) included in the electrode assembly (100) according to the present embodiment, the first separator (410c, 410d, 410e) is attached to the first surface of the cathode (210c, 210d, 210e), and both ends of the first separator (410c, 410d, 410e) may extend across the upper and lower surfaces of the unit anode (250c, 250d, 250e) to the other side of the unit anode (250c, 250d, 250e). In particular, on the other side of the unit anode (250c, 250d, 250e), both ends of the first separator (410c, 410d, 410e) may be joined to each other.

[0074] For example, the two ends of the first separators (410c, 410d, 410e) may be joined to each other by ultrasonic or heat sealing. As another example, the two ends of the first separators (410c, 410d, 410e) may be joined to each other by an adhesive or pressure-sensitive adhesive. However, the present invention is not limited thereto, and any method that can join the two ends of the first separators (410c, 410d, 410e) may be applied to the present embodiment.

[0075] In addition, as shown in FIGS. 8 to 10, in the electrode units (200c, 200d, 200e), both ends of the cathodes (210c, 210d, 210e) may extend across the upper and lower surfaces of the unit anodes (250c, 250d, 250e) to the other side surfaces of the unit anodes (250c, 250d, 250e), respectively. More specifically, the cathodes (210c, 210d, 210e) may extend outward from the other side surfaces of the unit anodes (250c, 250d, 250e), and both ends of the cathodes (210c, 210d, 210e) may be folded along the other side surfaces of the unit anodes (250c, 250d, 250e), respectively.

[0076] In particular, on the other side of the unit anode (250c, 250d, 250e), both ends of the cathodes (210c, 210d, 210e) may be joined to each other. That is, as shown in FIGS. 8 to 10, in the electrode unit (200c, 200d, 200e), a cathode junction (219c, 219d, 219e) may be formed in which both ends of the cathodes (210c, 210d, 210e) are joined to each other.

[0077] For example, the two ends of the cathodes (210c, 210d, 210e) may be joined to each other by ultrasonic or heat sealing. As another example, the two ends of the cathodes (210c, 210d, 210e) may be joined to each other by an adhesive or pressure-sensitive adhesive. However, the present invention is not limited thereto, and any method that can join the two ends of the cathodes (210c, 210d, 210e) may be applied to the present embodiment.

[0078] Accordingly, in the electrode assembly (100) according to the present embodiment, as shown in FIGS. 5 to 10, the electrode units (200, 200a, 200b, 200c, 200d, 200e) may have a first separator (410, 410a, 410b, 410c, 410d, 410e) attached to the first surface of the cathode (210, 210a, 210b, 210c, 210d, 210e) in various forms.

[0079] At this time, the unit positive electrode (250, 250a, 250b, 250c, 250d, 250e) can be inserted between the folded first surfaces of the negative electrodes (210, 210a, 210b, 210c, 210d, 210e) without a separate separator bonded thereto. In addition, the unit positive electrode (250, 250a, 250b, 250c, 250d, 250e) can be used as an assembly positive electrode (300) or in other manufacturing processes because a separate separator is not bonded thereto.

[0080] In particular, in the electrode units (200, 200a, 200b, 200c, 200d, 200e) such as those in FIGS. 5 to 10, in the process of folding the cathode (210, 210a, 210b, 210c, 210d, 210e), the first side of the cathode can be protected by the first separator (410, 410a, 410b, 410c, 410d, 410e), thereby preventing the cathode (210, 210a, 210b, 210c, 210d, 210e) from being damaged during the manufacturing process.

[0081] In addition, in the electrode assembly (100) according to the present embodiment, as shown in FIGS. 8 to 10, the electrode units (200c, 200d, 200e) may have the upper and lower surfaces and both sides of the unit anodes (250c, 250d, 250e) covered with the first separator (410c, 410d, 410e), so that there is an advantage in that stability is improved in the risk of short circuit.

[0082] In addition, as shown in FIGS. 9 and 10, the electrode units (200d, 200e) have both ends of the cathodes (210d, 210e) joined to each other, so that even if the electrode units (200d, 200e) are lifted upward, the shape of the electrode units (200d, 200e) can be maintained, and there is an advantage in that the electrode units (200d, 200e) can be assembled in a P&P (Pick and Place) manner when manufacturing the electrode assembly (100).

[0083]

[0084] Referring to FIGS. 4 to 7, unlike the above, in an electrode unit (200, 200a, 200b) included in an electrode assembly (100) according to another embodiment of the present invention, the first separator (410, 410a, 410b) may be attached to the upper and lower surfaces of the unit anode (250, 250a, 250b) and one side of the unit anode (250, 250a, 250b). More specifically, in the electrode unit (200, 200a, 200b), both ends of the first separator (410) may extend along the upper and lower surfaces of the unit anode (250, 250a, 250b), respectively. For example, as shown in FIGS. 4 to 7, in an electrode unit (200, 200a, 200b), one side of the unit anode (250, 250a, 250b) may not be covered by the first separator (410, 410a, 410b).

[0085] Referring to FIGS. 8 to 10, in the electrode units (200c, 200d, 200e) included in the electrode assembly (100) according to the present embodiment, the first separator (410c, 410d, 410e) may be attached to the upper and lower surfaces of the unit anodes (250c, 250d, 250e) and to both sides of the unit anodes (250, 250a, 250b). More specifically, both ends of the first separator (410c, 410d, 410e) may extend across the upper and lower surfaces of the unit anodes (250c, 250d, 250e) to the other side surfaces of the unit anodes (250c, 250d, 250e), respectively. In particular, on the other side of the unit anode (250c, 250d, 250e), both ends of the first separator (410c, 410d, 410e) may be joined to each other, or both ends of the first separator (410c, 410d, 410e) may be integrated with each other.

[0086] For example, the first separator (410, 410a, 410b, 410c, 410d, 410e) may be bonded to at least one surface of the unit anode (250, 250a, 250b, 250c, 250d, 250e) by ultrasonic or heat sealing. As another example, the first separator (410, 410a, 410b, 410c, 410d, 410e) may be bonded to at least one surface of the unit anode (250, 250a, 250b, 250c, 250d, 250e) by an adhesive or a pressure-sensitive adhesive. As another example, the first separator (410, 410a, 410b, 410c, 410d, 410e) may be bonded to at least one surface of the unit anode (250, 250a, 250b, 250c, 250d, 250e) by a lamination method. However, the present invention is not limited thereto, and any method that can bond the first separator (410, 410a, 410b, 410c, 410d, 410e) to the unit anode (250, 250a, 250b, 250c, 250d, 250e) may be applied to the present embodiment.

[0087] Accordingly, in the electrode assembly (100) according to the present embodiment, as shown in FIGS. 5 to 10, the electrode units (200, 200a, 200b, 200c, 200d, 200e) may have a first separator (410, 410a, 410b, 410c, 410d, 410e) attached to the unit anodes (250, 250a, 250b, 250c, 250d, 250e) in various forms. At this time, a unit positive electrode (250, 250a, 250b, 250c, 250d, 250e) can be inserted between the folded first surfaces of the negative electrodes (210, 210a, 210b, 210c, 210d, 210e) without a separate separator bonded to the first surface of the negative electrodes (210, 210a, 210b, 210c, 210d, 210e).

[0088] In addition, as described above, in the electrode assembly (100) according to the present embodiment, as shown in FIGS. 8 to 10, the electrode units (200c, 200d, 200e) have the upper and lower surfaces and both sides of the unit anodes (250c, 250d, 250e) attached with first separators (410c, 410d, 410e), so that there is an advantage in that stability is further improved in the risk of short circuit.

[0089]

[0090] Referring to FIGS. 3 and 4, in an electrode unit (200) included in an electrode assembly (100) according to another embodiment of the present invention, the assembly anode (300) may be positioned on a second surface opposite the first surface of the cathode (210). In addition, the electrode unit (200) may further include a second separator (450) positioned between the second surface of the cathode (210) and the assembly anode (300). More specifically, at least a portion of the second separator (450) may be positioned between the second surface of the cathode (210) and the assembly anode (300).

[0091] Here, the second separator (450) separates the negative electrode (210) and the positive electrode (300) of the assembly and provides a passage for lithium ions to move. If it is a separator commonly used in lithium secondary batteries, it can be used without any special restrictions. In particular, it is preferable that it has low resistance to ion movement of the electrolyte and excellent electrolyte moisture retention capacity.

[0092] Referring to FIGS. 3 to 6, 8, and 9, in an electrode unit (200, 200a, 200c, 200d) included in an electrode assembly (100) according to another embodiment of the present invention, a second separator (450, 450a, 450c, 450d) may be attached to the second surface of the cathode (210, 210a, 210c, 210d).

[0093] As shown in FIGS. 3 and 4, in the electrode unit (200) according to one embodiment of the present invention, the second separator (450) extends along the second surface of the cathode (210), and both ends of the second separator (450) may extend to both ends of the second surface of the cathode (210).

[0094] As shown in FIGS. 5 and 6, in the electrode unit (200a) according to another embodiment of the present invention, both ends (451a, 455a) of the second separator (450a) may extend across the side surfaces of both ends of the cathode (210a) to the side surfaces of the unit anode (250a), respectively. More specifically, both ends (451a, 455a) of the second separator (450a) may extend outward from both ends of the second surface of the cathode (210a), and both ends (451a, 455a) of the second separator (450a) may be folded along the side surfaces of both ends of the cathode (210a) and the side surfaces of the unit anode (250a), respectively. In particular, on the other side of the unit anode (250a), the two ends (451a, 455a) of the second separator (450a) may be joined to each other. That is, as shown in FIG. 5, in the electrode unit (200a), a second separator joint (459a) may be formed in which the two ends (451a, 455a) of the second separator (450a) are joined to each other.

[0095] For example, the two ends (451a, 455a) of the second separator (450a) may be joined to each other by ultrasonic or heat sealing. As another example, the two ends (451a, 455a) of the second separator (450a) may be joined to each other by an adhesive or a pressure-sensitive adhesive. However, the present invention is not limited thereto, and any method that can join the two ends (451a, 455a) of the second separator (450a) may be applied to the present embodiment.

[0096] In addition, as shown in FIGS. 8 and 9, in the electrode unit (200c, 200d), both ends of the cathodes (210c, 210d) may extend across the upper and lower surfaces of the unit anodes (250c, 250d) to the other side of the unit anodes (250c, 250d), respectively. In particular, on the other side of the unit anodes (250c, 250d), both ends of the cathodes (210c, 210d) may be joined to each other. That is, as shown in FIGS. 8 and 9, in the electrode unit (200c, 200d), a cathode joint (219c, 219d) may be formed in which both ends of the cathodes (210c, 210d) are joined to each other.

[0097] Here, as shown in FIG. 8, the second separator (450c) is attached to the second surface of the cathode (210c), but the second separator (450c) may not be attached to the side where the cathode junction (219c) of the cathode (210c) is formed.

[0098] In contrast, as shown in FIG. 9, the second separator (450d) is attached to the second surface of the cathode (210d), and the second separator (450d) may be attached up to the side where the cathode junction (219d) of the cathode (210d) is formed. At this time, both ends of the second separator (450d) may be joined in the manner described above, so that the second separator junction (459d) may be formed on one surface of the cathode (210d). For example, both ends of the second separator (450d) may be formed on the side where the cathode junctions (219c, 219d) of the cathode (210d) are formed.

[0099] Accordingly, in the electrode assembly (100) according to the present embodiment, as shown in FIGS. 3 to 6, 8, and 9, the electrode units (200, 200a, 200c, 200d) may have a second separator (450, 450a, 450c, 450d) attached in various forms to the second surface of the cathode (210, 210a, 210c, 210d).

[0100] At this time, the assembly positive electrode (300) can be laminated on the second surface of the negative electrode (210) without a separate separator being bonded thereto. In addition, since the assembly positive electrode (300) is not bonded with a separate separator, it can be used as a unit positive electrode (250, 250a, 250b, 250c, 250d, 250e) or in other manufacturing processes.

[0101] In particular, in the process of stacking electrode units (200, 200a, 200c, 200d) and assembly anodes (300) as shown in FIGS. 3 to 6, 8, and 9, the second surface of the cathode (210, 210a, 210c, 210d) included in the electrode units (200, 200a, 200c, 200d) can be protected by the second separator (450, 450a, 450c, 450d), thereby preventing the cathode (210, 210a, 210c, 210d) from being damaged during the manufacturing process.

[0102] In addition, in the electrode assembly (100) according to the present embodiment, as shown in FIGS. 5 and 6, the other side of the unit anode (250a) of the electrode unit (200a) may be covered with a second separator (450a), thereby providing an advantage in that stability against the risk of a short circuit is improved. In addition, as shown in FIG. 9, the other side of the unit anode (250d) of the electrode unit (200d) may be covered with both ends of the cathode (210d) and a second separator (450d), thereby providing an advantage in that stability against the risk of a short circuit is further improved.

[0103] In addition, as shown in FIGS. 5, 6, and 9, the electrode unit (200a, 200d) has the other side of the unit anode (250a, 250d) covered with a second separator (450a, 450d) or both ends of the cathode (210d) are joined to each other, so that even if the electrode unit (200a, 200d) is lifted upward, the shape of the electrode unit (200a, 200d) can be maintained. That is, there is an advantage in that the electrode unit (200a, 200d) can be assembled in a P&P (Pick and Place) manner when manufacturing the electrode assembly (100).

[0104]

[0105] FIG. 11 is a perspective view of an assembly anode included in an electrode assembly according to another embodiment of the present invention.

[0106] Referring to FIGS. 4 and 11, the assembly anode (300) may be positioned on the second surface of the cathode (210) included in the electrode unit (200). Here, unlike FIG. 4, the second separator (450) of the electrode unit (200) may be omitted, and an external separator (390a, 390b, 390c, 390d) may be attached to at least a portion of the surface of the assembly anode (300a, 300b, 300c, 300d). More specifically, at least a portion of the external separator (390a, 390b, 390c, 390d) may be positioned between the assembly anode (300a) and the second surface of the cathode (210).

[0107] The assembly anode (300, 300a, 300b, 300c, 300d) may include an assembly anode active material layer (310, 310a, 310b, 310c, 310d) and an assembly anode tab (350, 350a, 350b, 350c, 350d) similar to the unit anode (250), and the remaining description may be the same as that of the unit anode (250) described above.

[0108] The external separator (390) separates the negative electrode (210) and the positive electrode (300) of the assembly and provides a passage for lithium ions to move. If it is a separator commonly used in lithium secondary batteries, it can be used without any special restrictions. In particular, it is preferable that it has low resistance to ion movement of the electrolyte and excellent electrolyte moisture retention capacity.

[0109] More specifically, referring to FIG. 11 (a), the outer separators (390a, 390b, 390c, 390d) may include a first outer separator (391a) attached to the upper surface of the assembly positive electrode (300a) and a second outer separator (395a) attached to the lower surface of the assembly positive electrode (300a). For example, the first outer separator (391a) and the second outer separator (395a) may have a size that is larger than or equal to the upper and lower surfaces of the assembly positive electrode (300a), and the first outer separator (391a) and the second outer separator (395a) may have the same size.

[0110] Referring to FIGS. 11 (b) and (c), the external separators (390b, 390c) are attached to the upper and lower surfaces of the assembly anodes (300b, 300c) and one side of the assembly anodes (300b, 300c), and both ends of the external separators (390b, 390c) may extend along the upper and lower surfaces of the assembly anodes (300b, 300c), respectively.

[0111] Also, referring to Fig. 11 (b), both ends of the outer separator (390b) may extend across the upper and lower surfaces of the assembly anode (300b) to the other side of the assembly anode (300b). In particular, on the other side of the assembly anode (300b), both ends of the outer separator (390b) may be joined to each other. That is, as shown in Fig. 11 (b), an outer separator joint (399b) may be formed in which both ends of the outer separator (390b) are joined to each other. For example, both ends of the outer separator (390b) may be joined to each other by an ultrasonic or heat sealing method. As another example, both ends of the outer separator (390b) may be joined to each other with an adhesive or a pressure-sensitive adhesive. However, the present invention is not limited thereto, and any method that can join both ends of the outer separator (390b) may be applied to the present embodiment.

[0112] Referring to Fig. 11 (d), the external separator (390d) may be attached to the upper and lower surfaces of the assembly anode (300d) and to both sides of the assembly anode (300d). For example, the external separators (390d) may be attached to the upper and lower surfaces of the assembly anode (300d) and to both sides of the assembly anode (300d) in an integrated form. In another example, the external separators (390d) may be attached to the upper and lower surfaces of the assembly anode (300d) and to both sides of the assembly anode (300d) in a separate form for each surface of the assembly anode (300d).

[0113] Accordingly, in the electrode assembly (100) according to the present embodiment, as shown in FIG. 11, an external separator (390a, 390b, 390c, 390d) may be attached in various forms to at least one surface of the assembly positive electrode (300a, 300b, 300c, 300d). At this time, as shown in FIGS. 7 and 10, the assembly positive electrode (300a, 300b, 300c, 300d) to which the above-described external separator (390a, 390b, 390c, 390d) is attached may be laminated on an electrode unit (200b, 200e) to which the second separator (450) is not attached to the second surface of the negative electrode (210b, 210e).

[0114]

[0115] FIG. 12 and FIG. 13 are drawings showing a method for manufacturing an electrode unit included in an electrode assembly according to one embodiment of the present invention.

[0116] Referring to FIGS. 12 and 13, a method for manufacturing an electrode assembly according to another embodiment of the present invention may be a method for manufacturing an electrode assembly for manufacturing the electrode assembly (100) described above.

[0117] More specifically, referring to FIG. 3, FIG. 12(a), and FIG. 13(a), the method for manufacturing an electrode assembly according to the present embodiment may include a step of displaying a folding line indicated at the center of the first surface of the negative electrode (210). Here, the folding line display portion (1000) may be positioned on the same vertical line as the position corresponding to the center of the first surface of the negative electrode (210).

[0118] In addition, referring to FIG. 3, FIG. 12(b) and FIG. 13(b), the method for manufacturing an electrode assembly according to the present embodiment may include a step of folding a first surface of a cathode (210) based on the folding line and a step of positioning a unit cathode (250) on a portion of the folded first surface. Here, the first surface of the cathode (210) may be primarily folded at a predetermined angle. For example, the first surface of the cathode (210) may be folded at an angle greater than 90 degrees.

[0119] As described above, for example, as shown in FIG. 12, the first separator (410) may be attached to the first surface of the cathode (210), and at this time, a separate separator may not be attached to the outer surface of the unit anode (250). As another example, as shown in FIG. 13, the first separator (410) may be attached to at least a portion of the outer surface of the unit anode (250), and at this time, a separate separator may not be attached to the first surface of the cathode (210).

[0120] In addition, referring to FIG. 3, FIG. 12(c) and FIG. 13(c), the method for manufacturing an electrode assembly according to the present embodiment may include a step of folding the remaining side of the first side of the cathode (210) toward the upper surface of the unit anode (250) based on the folding line.

[0121] In addition, although not shown in FIGS. 12 and 13, referring to FIG. 3, the step of positioning the assembly anode (300) on the second surface opposite the first surface positioned on the upper surface of the unit anode (250) is further included.

[0122] As described above, as an example, as shown in FIG. 3, the second separator (450) positioned between the second surface of the negative electrode (210) and the assembly positive electrode (300) may be included, and the second separator (450) may be attached to the second surface of the negative electrode (210), and at this time, a separate separator may not be attached to the outer surface of the assembly positive electrode (300). As another example, as shown in FIG. 11, the external separator (390) positioned between the second surface of the negative electrode (210) and the assembly positive electrode (300) may be included, and the external separator (390) may be attached to at least a portion of the outer surface of the assembly positive electrode (300), and at this time, a separate separator may not be attached to the second surface of the negative electrode (210).

[0123] Accordingly, the electrode assembly manufacturing method according to the present embodiment can easily manufacture the electrode unit (200) and the assembly anode (300) by repeating the above-described steps, and can also easily manufacture the electrode assembly (100) in which the electrode unit (200) and the assembly anode (300) are laminated. In addition, the electrode unit (200) and the assembly anode (300) manufactured through the above-described manufacturing method can be stored in a semi-finished product state, so that even if floating occurs during the manufacturing process, they can be stored separately, and there is an advantage in that productivity and manufacturing stability are improved.

[0124]

[0125] FIGS. 14 to 16 are perspective views showing various arrangement forms of positive and negative tabs in an electrode unit included in an electrode assembly according to another embodiment of the present invention.

[0126] In FIGS. 14 to 16, the arrangement of the electrode tabs included in the electrode unit (200) will be described in detail. However, for convenience of explanation, the structure in which the unit anode (250) is arranged on the first surface of the cathode (210) while the first surface is folded at a predetermined angle, as shown in FIGS. 14 to 16, is described based on this structure, and the first separator (410) located between the cathode (210) and the unit anode (250) is described as a structure that is omitted.

[0127] Referring to FIG. 14, in the electrode unit (200) according to the present embodiment, when the first side of the cathode (210) is completely folded toward the unit anode (250) while the first side of the cathode (210) is folded at a predetermined angle, at least one cathode tab (215) included in the cathode (210) and the unit anode tab (255) included in the unit anode (250) may extend in the same direction, respectively. More specifically, when the first side of the cathode (210) is completely folded toward the unit anode (250) while the first side of the cathode (210) is folded at a predetermined angle, at least one cathode tab (215) may be positioned on the same vertical line, and at least one cathode tab (215) and the unit anode tab (255) may be positioned on different vertical lines.

[0128] Accordingly, as shown in FIG. 14, when the first side of the cathode (210) is completely folded toward the unit anode (250) while the first side of the cathode (210) is folded at a predetermined angle, the electrode unit (200) has the cathode tab (215) and the unit anode tab (255) positioned in one direction, so that the space that must be secured to arrange the electrical connection structure of the cathode tab (215) and the unit anode tab (255) between other electrode units (200) can be minimized.

[0129] Referring to FIGS. 15 and 16, in the electrode unit (200) according to the present embodiment, when the first side of the cathode (210) is completely folded toward the unit anode (250) while the first side of the cathode (210) is folded at a predetermined angle, at least one cathode tab (215) included in the cathode (210) and one unit anode tab (255) included in the unit anode (250) may extend in different directions.

[0130] For example, referring to FIG. 15 (b), FIG. 16 (b), and FIG. 16 (c), in the electrode unit (200) according to the present embodiment, at least one negative electrode tab (215) may be one negative electrode tab (215) extending along one side of the negative electrode (210).

[0131] Accordingly, as shown in FIGS. 15 and 16, when the first side of the cathode (210) is completely folded toward the unit anode (250) while the first side of the cathode (210) is folded at a predetermined angle, the electrode unit (200) has the cathode tab (215) and the unit anode tab (255) positioned in both directions, so that the cathode tab (215) and the unit anode tab (255) may not interfere with each other. That is, in the case of the present embodiment, there is an advantage in that the notching process of the cathode tab (215) and the unit anode tab (255) can be omitted. More specifically, the manufacturing time due to the notching process of the cathode tab (215) and the unit anode tab (255) can be shortened, and the defect problem occurring in the notching process can be minimized.

[0132]

[0133] FIG. 17 is a drawing showing a form in which an electrode unit and an assembly anode included in an electrode assembly according to one embodiment of the present invention are stored.

[0134] Referring to FIG. 17, in the electrode assembly (100) according to the present embodiment, the electrode unit (200) can be stored in a stacked state on an electrode unit tray (2000), and the assembly anode (300) can be stored in a stacked state on an assembly anode tray (3000). However, although not shown in FIG. 17, the electrode unit (200) can be replaced with an electrode unit (200a, 200b, 200c, 200d, 200e) as in FIGS. 5 to 10, and the assembly anode (300) can be replaced with an assembly anode (300a, 300b, 300c, 300d) as in FIG. 11.

[0135] Accordingly, unlike the conventional stacked electrode assembly (10) and zigzag electrode assembly (20), the electrode assembly (100) according to the present embodiment can be manufactured separately from the electrode unit (200) and the assembly anode (300) and then stored in a semi-finished state in the electrode unit tray (2000) or the anode tray (3000). That is, in the case of the electrode assembly (100) according to the present embodiment, even if some process fluctuations occur during the manufacturing process, the electrode unit (200) and the assembly anode (300) can be manufactured and stored separately, which has the advantage of improving productivity and manufacturing stability.

[0136] Although the preferred embodiments of the present invention have been described in detail above, the scope of the present invention is not limited thereto, and various modifications and improvements made by those skilled in the art using the basic concept of the present invention defined in the following claims also fall within the scope of the present invention.

[0137] [Explanation of symbols]

[0138] 100: Electrode assembly

[0139] 200: Electrode Unit

[0140] 210: Cathode

[0141] 211: Negative active material layer

[0142] 215: Negative tab

[0143] 251: Unit positive electrode active material layer

[0144] 255: Unit positive tap

[0145] 250: Unit Anode

[0146] 300: Assembly anode

[0147] 310: Assembly positive electrode active material layer

[0148] 350: Assembly positive tab

[0149] 390a, 390b, 390c, 390d: Outer membrane

[0150] 410: First membrane

[0151] 450: Second membrane

[0152] 2000: Electrode unit tray

[0153] 3000: Assembly anode tray

Claims

1. An electrode assembly in which electrode units and assembly anodes are sequentially stacked, The above electrode unit, A cathode folded in such a way that the first faces face each other; a unit anode positioned between the first surfaces that are folded; and Including a first separator positioned between the first surface and the unit anode, An electrode assembly in which the first surface surrounds the upper and lower surfaces of the unit anode and one side of the unit anode, and both ends of the first surface extend along the upper and lower surfaces of the unit anode.

2. In paragraph 1, The above first separator is attached to the first surface, An electrode assembly in which both ends of the first separator extend to both ends of the first surface.

3. In paragraph 2, The two ends of the first separator extend across the upper and lower surfaces of the unit anode to the other side of the unit anode, respectively. An electrode assembly in which both ends of the first separator are joined to each other on the other side of the above unit anode.

4. In paragraph 2, The two ends of the cathode extend across the upper and lower surfaces of the unit anode to the other side of the unit anode, respectively. An electrode assembly in which both ends of the cathode are joined to each other on the other side of the positive electrode of the above unit.

5. In paragraph 1, The above first separator is an electrode assembly attached to the upper and lower surfaces of the unit anode and both sides of the unit anode.

6. In paragraph 1, The above first separator is attached to the upper and lower surfaces of the unit anode and one side of the unit anode, An electrode assembly in which both ends of the first separator extend along the upper and lower surfaces of the unit anode.

7. In paragraph 6, The two ends of the first separator extend across the upper and lower surfaces of the unit anode to the other side of the unit anode, respectively. An electrode assembly in which both ends of the first separator are joined to each other on the other side of the above unit anode.

8. In paragraph 1, The above assembly anode is located on the second surface opposite to the first surface, Further comprising a second separator positioned between the assembly anode and the second surface and attached to the second surface, An electrode assembly in which both ends of the second separator extend to both ends of the second surface.

9. In paragraph 8, The two ends of the second separator each extend across the side surfaces of the two ends of the cathode to the side surfaces of the unit anode, An electrode assembly in which both ends of the second separator are joined to each other on the other side of the above unit anode.

10. In paragraph 9, The two ends of the cathode extend across the upper and lower surfaces of the unit anode to the other side of the unit anode, respectively. An electrode assembly in which both ends of the cathode are joined to each other on the other side of the positive electrode of the above unit.

11. In paragraph 1, The above assembly anode is located on the second surface opposite to the first surface, An electrode assembly further comprising an external separator positioned between the positive electrode of the assembly and the second surface, the external separator being attached to at least a portion of the surface of the positive electrode of the assembly.

12. In paragraph 11, An electrode assembly comprising a first outer separator attached to the upper surface of the positive electrode of the assembly and a second outer separator attached to the lower surface of the positive electrode of the assembly.

13. In paragraph 11, The above outer separator is an electrode assembly attached to the upper and lower surfaces of the assembly anode and both sides of the assembly anode.

14. In paragraph 11, The above outer separator is attached to the upper and lower surfaces of the assembly anode and one side of the assembly anode, An electrode assembly in which both ends of the above outer separator extend along the upper and lower surfaces of the above assembly anode.

15. In paragraph 14, Both ends of the above outer separator extend across the upper and lower surfaces of the above assembly anode to the other side of the above assembly anode, An electrode assembly in which both ends of the outer separator are joined to each other on the other side of the above assembly.

16. In paragraph 1, At least one cathode tab included in the cathode and a unit anode tab included in the unit anode are each extended in the same direction, wherein at least one of the cathode tabs is positioned on the same vertical line, An electrode assembly wherein at least one of the cathode tabs and the unit anode tab are positioned on different vertical lines.

17. In paragraph 1, An electrode assembly in which at least one negative electrode tab included in the cathode and a unit positive electrode tab included in the unit positive electrode extend in different directions.

18. In paragraph 17, An electrode assembly wherein at least one cathode tab is a cathode tab extending along one side of the cathode.

19. A method for manufacturing an electrode assembly for manufacturing an electrode assembly of the first clause, A step of displaying a folding line indicated at the center of the first side of the above cathode; A step of folding the first side of the cathode based on the folding line; A step of positioning the unit anode on some of the folded first surfaces; A step of folding the remaining side of the first side toward the upper surface of the unit anode based on the folding line, A method for manufacturing an electrode assembly, wherein the first separator is attached to the first surface or to at least a portion of the outer surface of the unit anode.

20. In paragraph 19, Further comprising the step of positioning the assembly anode on the second surface opposite to the first surface positioned on the upper surface of the unit anode, A second separator or an outer separator positioned between the second surface and the assembly anode, A method for manufacturing an electrode assembly, wherein the second separator is attached to the second surface, and the outer separator is attached to at least a portion of the outer surface of the positive electrode of the assembly.

Citation Information

Patent Citations

  • Electrode assembly and method of manufacturing electrode assembly

    KR1020240155802A

  • Sheet-like lithium secondary battery

    JP1998172607A

  • Cell stacking method for Secondary Battery and cell stack for using the same

    KR1020140035646A

  • Rechargeable battery

    KR1020170130855A

  • Display device

    KR1020200145899A