Purifying spray for preventing nuclear radiation, and preparation method therefor and use thereof

By using a purification spray for preventing nuclear radiation prepared by a compound containing bismuth and boron elements, the problem of difficulty in removing low-concentration radionuclides and the decay and release of radionuclides in the existing technology has been solved, and the effective purification and purification of the nuclear-contaminated environment has been achieved. Personnel health protection.

WO2024221623A1PCT designated stage expired Publication Date: 2024-10-31SHANDONG HENGYI HIGH TECHNOLOGY IND CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/108213
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2023-07-19
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

It is difficult to effectively remove radionuclides such as low-concentration small molecule elements iodine, hydrogen iodide and organic iodine with existing technology, and radionuclides decay in the filter material to release radiation and neutrons, causing environmental pollution, and the lead element used has Toxic and unable to continuously block nuclear radiation hazards.

Method used

Compounds containing bismuth and boron elements are used to prepare purification sprays for preventing nuclear radiation. The efficient absorption of X-rays and gamma rays by bismuth and the strong neutron absorption ability of boron are combined with non-toxic or low-toxicity and high-abundance natural boron elements. A water-soluble compound is formed to prepare a purifying spray that absorbs and shields nuclear radiation and neutrons.

Benefits of technology

This purification spray can efficiently absorb and shield radioactive elements and neutrons in a nuclear-contaminated environment, prevent the continued release of radionuclides, and reduce harm to the environment and personnel. The process is simple and controllable, and is suitable for large-scale production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PCTCN2023108213-FTAPPB-I100001
    Figure PCTCN2023108213-FTAPPB-I100001
  • Figure PCTCN2023108213-FTAPPB-I100002
    Figure PCTCN2023108213-FTAPPB-I100002
Patent Text Reader

Abstract

A purifying spray for preventing nuclear radiation, and a preparation method therefor and the use thereof in the absorption of radioactive elements, radioactive rays or neutrons in a nuclear radiation pollution environment. The preparation method comprises: dispersing a bismuth source in deionized water, and adding glycerol thereto; and adding Arabic gum and glycerol thereto, performing ultrasonic dissolution, then adding absolute ethyl alcohol and gelatin thereto, performing ultrasonic stirring and dissolution, adding a boron source after dilution, adding an antibacterial agent and an antioxidant after the boron source is dissolved, optionally adding a stabilizer, and uniformly stirring same to obtain a purifying spray for preventing nuclear radiation. The purifying spray for preventing nuclear radiation can absorb both rays and neutrons in a nuclear pollution environment, and eliminate nuclear radioactive ray and neutron radiation hazards in the nuclear pollution environment. After the purifying spray for preventing nuclear radiation is solidified, radionuclides in the nuclear pollution environment can be wrapped, thereby preventing the radionuclides from continuing to release rays and neutrons into the environment, and facilitating the subsequent treatment of nuclear pollution waste.
Need to check novelty before this filing date? Find Prior Art

Description

Purification spray for preventing nuclear radiation, and its production method and application

[0001] The present invention claims priority to the Chinese patent application filed with the Patent Office of China on April 28, 2023, with application number 202310476984.X and invention name “A purification spray for nuclear radiation protection, its preparation method and application”, the entire contents of which are incorporated by reference into the present invention and constitute a part of the present invention. Technical Field

[0002] The invention relates to a purification spray for preventing nuclear radiation, a preparation method and an application thereof, and belongs to the field of nuclear radiation protection. Background Art

[0003] In recent years, nuclear medicine isotope imaging and therapy technologies have developed rapidly, and the use of radioactive diagnostic and therapeutic drugs has increased rapidly year by year. The resulting radioactive waste gases, wastewater, and solid waste have become key and challenging areas for radiation safety and protection regulation. Commonly used radionuclides in nuclear medicine include iodine-131 (I-131), technetium-99 (Tc-99), and fluorine-18 (F-18). Among these, radionuclides used to treat thyroid diseases account for over 90% of all radionuclide therapy, and I-131 is virtually the only radionuclide used. Therefore, I-131 is the largest source of radioactive waste gases in nuclear medicine activities. I-131 has 78 neutrons in its nucleus, four more than the number of neutrons in the nucleus of stable iodine nuclides. I-131 is a beta-decaying nuclide, emitting beta rays (99%) and gamma rays (1%). I-131 has a long biological half-life. After taking the drug, patients become living radioactive sources, emitting beta and gamma rays that can cause external exposure to nearby personnel. I-131 radioactive waste gases primarily originate from waste gases generated during the packaging and oral administration of radioactive drugs, volatilization from patient excrement, bedding, and other solid waste, and exhaled gases containing radioactive elements during hospitalization. I-131 nuclides in the atmosphere typically exist in two forms: aerosols and gaseous products. Aerosols are suspensions of solid particles or liquid droplets of I-131 dispersed in the air, primarily consisting of non-volatile iodides and iodates. Gaseous products primarily include elemental iodine, hydrogen iodide, and organic iodine (such as radioactive methyl iodide, CH3131I). Currently used waste gas disposal methods primarily involve aerosol filtration and gaseous product adsorption. However, filtration and gaseous product adsorption methods are only effective for micron-sized aerosol particles and higher concentrations of radioactive nuclear waste gases, respectively. They are ineffective at removing low concentrations of small-molecule elemental iodine, hydrogen iodide, and organic iodine dispersed in the air. Furthermore, studies have shown that the gaseous product adsorption efficiency of radioactive methyl iodide decreases rapidly when the concentration of organic pollutants in the environment exceeds 10%. Furthermore, currently used aerosol filtration and gaseous product adsorption technologies can only adsorb I-131 within filter materials such as filter paper and activated carbon. The radionuclides continue to decay within the filter material, releasing harmful substances such as radiation and neutrons into the environment. Promptly preventing radionuclide contamination of the surrounding environment has become a pressing issue for current nuclear radiation protection products. Currently, lead is commonly used to block absorption of persistent nuclear radiation hazards. However, lead and its compounds are toxic and, upon entry into the body, can harm multiple systems, including the nervous system, hematopoietic system, digestive system, kidneys, cardiovascular system, and endocrine system.

[0004] In addition to nuclear contamination from the use of radiopharmaceuticals, neutrons produced during the production of radioisotopes using cyclotrons in hospitals are another major source of radiation contamination. Neutrons have strong penetrating power when passing through matter, posing a greater risk to the human body than the same dose of X-rays or gamma rays. Furthermore, the interaction of neutrons with the air in the equipment room can produce induced radioactive gases such as nitrogen-13 (N-13), carbon-11 (C-11), oxygen-15 (O-15), and argon-41 (Ar-41), further exacerbating nuclear contamination.

[0005] The research and development of new and efficient purification materials and products for nuclear radiation protection is the key to current nuclear radiation protection technology, and is also the inevitable trend and development direction for the further practical application of nuclear medicine technology and other nuclear energy technologies.

[0006] Summary of the Invention

[0007] The technical problem to be solved by the present invention is to provide a purification spray for protecting against nuclear radiation, a preparation method thereof and an application thereof, wherein the purification spray for protecting against nuclear radiation contains boron and bismuth.

[0008] Bismuth's X-ray absorption performance is similar to that of lead, and it strongly absorbs gamma rays. Bismuth has one more outer electron than lead and a larger attenuation coefficient, making it more suitable for use in radiation protection. Compared to other neutron-absorbing shielding materials, boron-10 has advantages such as a large neutron absorption cross-section, no gamma particle release, water solubility, non-toxicity or low toxicity, low reactivity in air, and low acidity and alkalinity. Furthermore, the abundances of boron-10 and boron-11 in natural boron are 19.78% and 80.22%, respectively, making it possible to use high-dose natural boron in place of boron-10 as a neutron shielding material. Furthermore, natural boron exists in the form of compounds in minerals, making it abundant and cost-effective. Therefore, the present invention utilizes compounds containing bismuth and boron to prepare a nuclear radiation protection spray product that can simultaneously protect against nuclear radiation and neutrons, eliminating the hazards of radiation and neutrons in nuclear-contaminated environments. This product has both high scientific research value and practical significance for managing nuclear-contaminated environments and protecting the health of personnel in nuclear-exposed areas. How to configure the nuclear radiation protection purification spray product is a technical problem that needs to be solved at present. The present invention also provides a method for preparing the nuclear radiation protection purification spray.

[0009] In order to solve the above technical problems, the present invention provides a purification spray for nuclear radiation protection, which contains boron and bismuth elements.

[0010] Preferably, the boron element is derived from at least one of boric acid, boric acid-10 and soluble boron-containing drugs (such as bortezomib, ixazomib, tavaborole, crisaborole, and vaborbactam-meropenem).

[0011] More preferably, the mass concentration of the boric acid is 0.1-10%.

[0012] Preferably, the bismuth element is derived from at least one of non-toxic or low-toxic inorganic bismuth compounds such as bismuth citrate, potassium bismuth citrate, ammonium bismuth citrate, bismuth aluminate, colloidal pectin bismuth, bismuth subcarbonate, bismuth oxide, bismuth tungstate, and bismuth oxychloride.

[0013] Preferably, the purification spray for nuclear radiation protection comprises, by weight, the following components:

[0014] 1-5 parts of bismuth source, 4-15 parts of boron source, 2-15 parts of glycerol, 5-10 parts of gum arabic, 10-100 parts of anhydrous ethanol, 5-10 parts of gelatin, and 50-100 parts of deionized water.

[0015] Preferably, the purification spray for nuclear radiation protection comprises, by weight, the following components:

[0016] 1-5 parts of bismuth source, 4-15 parts of boron source, 2-15 parts of glycerol, 5-10 parts of gum arabic, 10-100 parts of anhydrous ethanol, 5-10 parts of gelatin, 50-100 parts of deionized water, 0.05-0.5 parts of antioxidant, and 0.1-1 parts of antibacterial agent.

[0017] Preferably, the purification spray for nuclear radiation protection comprises, by weight, the following components:

[0018] 1-5 parts of bismuth source, 4-15 parts of boron source, 2-15 parts of glycerol, 5-10 parts of gum arabic, 10-100 parts of anhydrous ethanol, 5-10 parts of gelatin, 50-100 parts of deionized water, 0.05-0.5 parts of antioxidant, 0.1-1 parts of antibacterial agent, 0.05-0.5 parts of defoaming agent, 0.1-1 parts of stabilizer, and 0.05-0.5 parts of essential oil.

[0019] The present invention also provides a method for preparing the above-mentioned purification spray for nuclear radiation protection: dispersing a bismuth source in deionized water, adding glycerol, and stirring to prepare liquid A; adding gum arabic and glycerol to liquid A, ultrasonically dissolving, then adding anhydrous ethanol and gelatin, and ultrasonically stirring to dissolve to obtain liquid B; after diluting liquid B, adding a boron source, and after the boron source is dissolved, adding an antibacterial agent and an antioxidant and optionally a stabilizer, and stirring evenly to obtain the purification spray for nuclear radiation protection.

[0020] Preferably, the method comprises: dispersing a bismuth source in deionized water, adding glycerol, and stirring to prepare liquid A; adding gum arabic and glycerol to liquid A, ultrasonically dissolving, then adding anhydrous ethanol and gelatin, ultrasonically stirring to dissolve, to obtain liquid B; after diluting liquid B, adding a boron source, and after the boron source is dissolved, adding a stabilizer, an antibacterial agent, and an antioxidant, stirring evenly, to obtain the purification spray for protecting against nuclear radiation.

[0021] Preferably, in the liquid A, the mass ratio of the bismuth source to water is 1:(5-5000), and the volume ratio of glycerol to water is 1:(1-1000).

[0022] Preferably, the bismuth source is selected from at least one of non-toxic or low-toxic inorganic bismuth compounds such as bismuth citrate, potassium bismuth citrate, ammonium bismuth citrate, bismuth aluminate, colloidal pectin bismuth, bismuth subcarbonate, bismuth oxide, bismuth tungstate, and bismuth oxychloride.

[0023] Preferably, in the liquid B, the mass ratio of gum arabic to water is 1:(1-2000), the volume ratio of glycerol to water is 1:(1-1000), the volume ratio of anhydrous ethanol to water is 1:(1-2000), and the mass ratio of gum arabic to gelatin is 1:(0.1-10).

[0024] Preferably, an appropriate amount of defoaming agent can be added during the ultrasonic stirring and dissolving process, and the amount added is 0.01-1% by mass, preferably 0.1%. The defoaming agent can be, for example, an organosilicon defoaming agent, such as silicone oil.

[0025] Preferably, after the gelatin is completely dissolved, the pH is adjusted to acidic (for example, to pH 4.5). For example, hydrochloric acid can be used to adjust the pH.

[0026] Preferably, after the gelatin is completely dissolved, an appropriate amount of essential oil can be added, wherein the amount of essential oil added is 0.01-1% by volume, preferably 0.1%. The essential oil is a plant essential oil, such as tea tree essential oil, eucalyptus essential oil, etc.

[0027] Preferably, the dilution ratio of the solution B is 1 to 1000, for example, deionized water is used for dilution.

[0028] Preferably, the boron source is selected from at least one of boric acid, boric acid-10, and soluble boron-containing drugs (such as bortezomib, ixazomib, tavaborole, crisaborole, and vaborbactam-meropenem).

[0029] Preferably, the amount of the boron source added is 0.1 wt% to 10 wt%. Preferably, the mass ratio of the added bismuth source to the boron source is 1:4-10.

[0030] Preferably, the antioxidant is added in an amount of 0.01 to 1% by weight. The antioxidant is, for example, tea polyphenols, preferably added in an amount of 0.1 wt%.

[0031] Preferably, the stabilizer is added in an amount of 0.01 to 1% by weight. The stabilizer is, for example, hydroxycellulose, preferably added in an amount of 0.3 wt%.

[0032] Preferably, the amount of the antibacterial agent added is 0.01-1% by weight. For example, the antibacterial agent is potassium sorbate, and the amount of the antibacterial agent added is preferably 0.3 wt%.

[0033] The present invention also provides the use of the purification spray for nuclear radiation protection in absorbing radioactive elements, radiation or neutrons in a nuclear radiation contaminated environment.

[0034] The invention provides a simple, quick and highly controllable method for preparing a purification spray for nuclear radiation protection.

[0035] Compared with the prior art, the present invention has the following beneficial effects:

[0036] 1) The nuclear radiation protection purification spray obtained by the method of the present invention can simultaneously absorb radiation and neutrons in a nuclear contaminated environment, thereby eliminating the hazards of nuclear radiation and neutron radiation in the nuclear contaminated environment.

[0037] 2) The anti-nuclear radiation purification spray obtained by the method of the present invention can be solidified to encapsulate radioactive nuclides in the nuclear contaminated environment, thereby preventing the radioactive nuclides from continuing to release radiation and neutrons into the environment, thereby facilitating subsequent treatment of nuclear contaminated waste.

[0038] 3) The preparation method of the present invention does not require special equipment and harsh conditions, has a simple process, is highly controllable, is easy to implement large-scale production, and is practical. DETAILED DESCRIPTION

[0039] In order to make the present invention more clearly understood, preferred embodiments are described in detail below.

[0040] The following embodiments of the present invention provide several examples of preparing a decontamination spray for radiation protection. Defoamers, stabilizers, and essential oils are optional components that can be added or omitted without affecting the removal and / or shielding effects of radioactive substances. The defoamer prevents excessive foaming during the atomization process, which can affect the atomization effect. It reduces the surface tension of the drug solution, making it easier for high-frequency vibration or high-speed airflow to break it into fine particles. It also prevents bubbles from forming during storage and use due to temperature fluctuations or vibrations, which can lead to uneven mixing. Silicone oil was used in the following examples. Essential oils primarily enhance odor and freshness during spraying. Tea tree oil was used in the following examples. Stabilizers primarily maintain dispersibility. For example, hydroxycellulose is used in one or more of the following examples. It increases the distance and charge between particles, preventing particle aggregation or sedimentation, maintaining a uniform dispersion of the mixed liquid, and preventing stratification or precipitation. Unless otherwise specified, potassium sorbate was used in the following examples as an antibacterial agent.

[0041] Example 1

[0042] 1 g of bismuth citrate is dispersed in 20 mL of deionized water and stirred for a certain period of time to obtain a suspension of bismuth citrate. 5 mL of glycerol and 6 g of gum arabic are added to the suspension and dissolved by ultrasonic stirring. 5 mL of glycerol and 10 mL of anhydrous ethanol are added and stirred uniformly. 6 g of gelatin is added and dissolved by ultrasonic stirring. After the gelatin is completely dissolved, the pH is adjusted to 4.5 with hydrochloric acid. The obtained solution is diluted 10-fold with deionized water, 10 g of boric acid is added and stirred to dissolve, 0.1 wt % of tea polyphenols and 0.3 wt % of an antibacterial agent are added and stirred uniformly to prepare the purification spray for nuclear radiation protection.

[0043] Example 2

[0044] 1 g of potassium bismuth citrate is dispersed in 10 mL of deionized water and stirred for a certain period of time to obtain a potassium bismuth citrate solution. 5 mL of glycerol and 6 g of gum arabic are added to the solution and dissolved by ultrasonic stirring. 5 mL of glycerol and 10 mL of anhydrous ethanol are added and stirred uniformly. 6 g of gelatin is added and dissolved by ultrasonic stirring. After the gelatin is completely dissolved, the pH is adjusted to 4.5 with hydrochloric acid. The obtained solution is diluted 10-fold with deionized water, 10 g of boric acid is added and stirred to dissolve, 0.1 wt % of tea polyphenols, 0.3 wt % of hydroxycellulose, and 0.3 wt % of an antibacterial agent are added and stirred uniformly to prepare the purification spray for nuclear radiation protection.

[0045] Example 3

[0046] 1 g of potassium bismuth citrate is dispersed in 10 mL of deionized water and stirred for a certain period of time to obtain a potassium bismuth citrate solution. 2 mL of glycerol is added to the solution, 5 g of gum arabic is added, and ultrasonic stirring is added to dissolve the solution. 10 mL of anhydrous ethanol is added and stirred evenly. 5 g of gelatin is added and ultrasonic stirring is added to dissolve the gelatin. After the gelatin is completely dissolved, the pH is adjusted to 4.5 with hydrochloric acid. The obtained solution is diluted 10-fold with deionized water, 6 g of boric acid is added and stirred to dissolve the solution, 0.1 wt % of tea polyphenols, 0.3 wt % of hydroxycellulose, and 0.3 wt % of an antibacterial agent are added and stirred evenly to obtain the nuclear radiation protection purification spray.

[0047] Example 4

[0048] 1 g of colloidal bismuth pectin is dispersed in 100 mL of deionized water and stirred for a certain period of time to obtain a suspension of colloidal bismuth pectin. 2 mL of glycerol and 5 g of gum arabic are added to the suspension and dissolved by ultrasonic stirring. 100 mL of anhydrous ethanol is added and stirred uniformly. 5 g of gelatin is added and dissolved by ultrasonic stirring. After the gelatin is completely dissolved, the pH is adjusted to 4.5 with hydrochloric acid. The obtained solution is diluted 10-fold with deionized water, 4 g of boric acid is added and stirred to dissolve, 0.1 wt% of tea polyphenols, 0.3 wt% of hydroxycellulose, and 0.3 wt% of an antibacterial agent are added and stirred uniformly to prepare the purification spray for nuclear radiation protection.

[0049] Example 5

[0050] 1g of bismuth citrate was dispersed in 20mL of deionized water and stirred for a certain period of time to obtain a suspension of bismuth citrate. 5mL of glycerol was added to the suspension, 6g of gum arabic was added, and after ultrasonic stirring to dissolve, 5mL of glycerol was added, 10mL of anhydrous ethanol was added, and after stirring, 6g of gelatin was added and dissolved with ultrasonic stirring. 0.1% of a defoamer was added during the dissolution process. After the gelatin was completely dissolved, 0.1% of essential oil by volume was added, and the pH was adjusted to 4.5 with hydrochloric acid. The obtained solution was diluted 10 times with deionized water, 10g of boric acid was added and stirred to dissolve, 0.1wt% of tea polyphenols was added, 0.3wt% of hydroxycellulose was added, and 0.3wt% of an antibacterial agent was added and stirred to obtain the anti-nuclear radiation purification spray, which was labeled as sample 1.

[0051] Example 6

[0052] 1g of potassium bismuth citrate was dispersed in 10mL of deionized water and stirred for a certain period of time to obtain a solution of potassium bismuth citrate. 5mL of glycerol was added to the solution, 6g of gum arabic was added, and after ultrasonic stirring to dissolve, 5mL of glycerol was added, 10mL of anhydrous ethanol was added, and after stirring evenly, 6g of gelatin was added and dissolved under ultrasonic stirring. 0.1% of a defoamer was added during the dissolution process. After the gelatin was completely dissolved, 0.1% by volume of essential oil was added, and the pH was adjusted to 4.5 with hydrochloric acid. The obtained solution was diluted 10 times with deionized water, 10g of boric acid was added and stirred to dissolve, 0.1wt% of tea polyphenols was added, 0.3wt% of hydroxycellulose was added, and 0.3wt% of an antibacterial agent was added and stirred evenly to obtain the nuclear radiation protection purification spray, which was marked as sample 2.

[0053] Example 7

[0054] 1 g of potassium bismuth citrate was dispersed in 10 mL of deionized water and stirred for a period of time to obtain a solution of potassium bismuth citrate. 2 mL of glycerol was added to the solution, 5 g of gum arabic was added, and after ultrasonic stirring to dissolve, 10 mL of anhydrous ethanol was added and stirred evenly. 5 g of gelatin was added and dissolved under ultrasonic stirring. 0.1% of a defoamer was added during the dissolution process. After the gelatin was completely dissolved, 0.1% by volume of essential oil was added. The pH was adjusted to 4.5 with hydrochloric acid. The obtained solution was diluted 10-fold with deionized water, 6 g of boric acid was added and stirred to dissolve, 0.1 wt % of tea polyphenols was added, 0.3 wt % of hydroxycellulose was added, and 0.3 wt % of an antibacterial agent was added and stirred evenly to obtain the nuclear radiation protection purification spray, which was labeled as Sample 3.

[0055] Example 8

[0056] 1 g of colloidal bismuth pectin was dispersed in 100 mL of deionized water and stirred for a period of time to obtain a suspension of colloidal bismuth pectin. 2 mL of glycerol was added to the suspension, followed by 5 g of gum arabic and ultrasonic stirring to dissolve the mixture. 100 mL of anhydrous ethanol was then added and stirred to dissolve the mixture. 5 g of gelatin was then added and ultrasonic stirring to dissolve the mixture. 0.1% of a defoamer was added during the dissolution process. After the gelatin was completely dissolved, 0.1% by volume of an essential oil was added. The pH was adjusted to 4.5 with hydrochloric acid. The resulting solution was diluted 10-fold with deionized water, 4 g of boric acid was added and stirred to dissolve the mixture, 0.1 wt % of tea polyphenols, 0.3 wt % of hydroxycellulose, and 0.3 wt % of an antibacterial agent were added and stirred to obtain the radiation protection purification spray, which was labeled as Sample 4.

[0057] The method of using the nuclear radiation protection purification spray of the present invention is as follows: the sample prepared by the present invention is divided into a spray bottle, and the switch is pressed to spray the spray to the target to be implemented, and the spraying amount is 50mL / m 3 .

[0058] Taking the removal of radioactive methyl iodide from the air as an example, the test was conducted in a sealed glass container. The test results for some samples are shown in Table 1.

[0059] Table 1: Performance of the purification spray for nuclear radiation protection obtained in the examples for removing radioactive methyl iodide

[0060] Taking shielding radioactive neutrons in air as an example, the test was conducted in a sealed lead box. The relevant performance test results of some samples are shown in Table 2.

[0061] Table 2: Neutron radiation shielding performance of the purification spray for nuclear radiation protection obtained in the examples

Claims

1. A purification spray for nuclear radiation protection, characterized in that: Contains boron and bismuth.

2. The purification spray for nuclear radiation protection according to claim 1, characterized in that: The boron element is derived from at least one of boric acid, boric acid-10 and soluble boron-containing medicines.

3. The purification spray for nuclear radiation protection according to claim 2, characterized in that: The mass concentration of the boric acid is 0.1-10%.

4. The purification spray for nuclear radiation protection according to claim 1, characterized in that: The bismuth element is derived from at least one of bismuth citrate, potassium bismuth citrate, ammonium bismuth citrate, bismuth aluminate, colloidal pectin bismuth, bismuth subcarbonate, bismuth oxide, bismuth tungstate, and bismuth oxychloride.

5. The method for producing the purification spray for nuclear radiation protection according to any one of claims 1 to 4, characterized in that: The bismuth source is dispersed in deionized water, glycerol is added, and the mixture is stirred to prepare liquid A; gum arabic and glycerol are added to liquid A, and the mixture is ultrasonically dissolved; anhydrous ethanol and gelatin are then added, and the mixture is ultrasonically stirred to dissolve, so as to obtain liquid B; after liquid B is diluted, a boron source is added, and after the boron source is dissolved, a stabilizer, an antibacterial agent and an antioxidant are added, and the mixture is stirred evenly, so as to obtain the purification spray for protecting against nuclear radiation.

6. The method according to claim 5, characterized in that: In the liquid A, the mass ratio of bismuth element in the bismuth source to water is 1:(5-5000), and the volume ratio of glycerol to water is 1:(1-1000).

7. The method according to claim 5, characterized in that: In the liquid B, the mass ratio of gum arabic to water is 1:(1-2000), the volume ratio of glycerol to water is 1:(1-1000), the volume ratio of anhydrous ethanol to water is 1:(1-2000), and the mass ratio of gum arabic to gelatin is 1:(0.1-10).

8. The method according to claim 5, characterized in that: The dilution multiple of the B solution is 1 to 1000.

9. The method according to claim 5, characterized in that: The added amount of the antioxidant is 0.01-1% by mass.

10. Use of the purification spray for nuclear radiation protection according to any one of claims 1 to 4 in absorbing radioactive elements, radiation or neutrons in a nuclear radiation contaminated environment.

Citation Information

Patent Citations

  • Light-fragrance electronic cigarette atomized smoke solution and preparation method thereof

    CN102960852A

  • Sterilization gel, preparation thereof, ultrasonic coupling agent based on sterilization gel, and preparation and application of ultrasonic coupling agent

    CN115252830A

  • Radiation shield material composition

    JP2003255081A

  • Composition for adsorbing radioactive material, coating peeling type radioactive decontamination material, decontamination technique, and decontamination and shielding technique

    JP2013234918A

  • Amorphous composition for high level radiation and environmental protection

    US20040124374A1