Die-casting system

By using spiral channels and cooling pieces for temperature control in the die-casting system, and improving the ejection mechanism and forming device, the problem of poor temperature control in semi-solid aluminum material molding is solved, and the molding quality and product density are improved.

WO2024221894A1PCT designated stage expired Publication Date: 2024-10-31CHONGQING SHUNDUOLI LOCOMOTIVE CO LTD

Patent Information

Application Number
PCT/CN2023/134242
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2023-11-27
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

In existing semi-solid die-casting technology, poor temperature control affects the molding quality of aluminum materials, making it difficult to maintain a semi-solid state and affecting product quality.

Method used

A die-casting system is designed, including a pulping device and a liquid die forging machine. By setting up a spiral channel and cooling parts in the pulping device, the temperature of the aluminum liquid is controlled by using insulation oil and cooling parts to ensure that the aluminum material remains stable during the forming process. Uniform temperature and reduce product deformation through improved ejection mechanism and forming device.

Benefits of technology

Effectively control the temperature of the aluminum material, improve the molding quality, reduce product deformation, and improve the density and molding accuracy of the aluminum material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023134242_31102024_PF_FP_ABST
    Figure CN2023134242_31102024_PF_FP_ABST
Patent Text Reader

Abstract

A die-casting system, comprising a slurry preparation device (b0) and a liquid die forging machine (c0), wherein the slurry preparation device (b0) can implement preparation of semi-solid aluminum from molten aluminum, and the liquid die forging machine (c0) can implement forming of the aluminum. The slurry preparation device (b0) comprises a first accommodating cup (b2) and a first ejection mechanism at the bottom of the first accommodating cup (b2), wherein a helical channel (b211) is provided in a side wall of the first accommodating cup (b2), thermal insulation oil being provided in the helical channel (b211); and a cooling member (b8) is provided at the bottom of the first accommodating cup (b2).
Need to check novelty before this filing date? Find Prior Art

Description

A die casting system Technical Field

[0001] The present invention relates to the field of die casting, and in particular to a die casting system. Background Art

[0002] Semi-solid die casting involves using a stirring rod to transform the dendrites formed during solidification into a non-dendritic structure in a slurry-making vessel within a slurry-making machine. This creates a semi-solid slurry (hereinafter referred to as aluminum material) of liquid-solid mixture. This slurry is then clamped into a die forging machine using a clamping mechanism and die-cast to produce a high-density alloy. Semi-solid metal has a higher viscosity than liquid metal, making it easier to control the forming process. Its lower flow stress than solid metal allows for faster forming of parts, even for complex parts. This results in shorter processing cycles, no waste, and high material utilization.

[0003] However, in order to maintain the semi-solid state of aluminum, the temperature needs to be strictly controlled. The semi-solid state cannot be maintained if the temperature is too high or too low. In the existing technology, from the production of semi-solid aluminum to the die-casting of aluminum, the product quality is often easily affected by poor temperature control. Temperature has become a key control factor for the molding quality of semi-solid aluminum. Summary of the Invention

[0004] The present invention aims to provide a die-casting system to improve the molding quality of semi-solid aluminum material.

[0005] To achieve the above objectives, the present invention adopts the following technical solution: a die-casting system including a slurrying device and a liquid die forging machine. The slurrying device can form molten aluminum into semi-solid aluminum material, and the liquid die forging machine can shape the aluminum material. The slurrying device includes a first receiving cup and a first ejection mechanism at the bottom of the first receiving cup. A spiral channel is provided in the side wall of the first receiving cup, and insulation oil is contained in the spiral channel. A cooling member is provided at the bottom of the first receiving cup.

[0006] In order to improve the molding quality of semi-solid aluminum material, the inventors need to make improvements from the perspective of temperature control. First, they need to analyze the heat dissipation process of the aluminum material.

[0007] During the process of converting molten aluminum into aluminum material, it needs to be cooled and continuously stirred. During this process, the temperature changes most rapidly and is most difficult to control. The inventors discovered that with continuous stirring, the upper end of the first holding cup is open, and the upper part of the molten aluminum cools down faster. After the molten aluminum is converted into aluminum material, a first ejection mechanism is provided at the bottom of the molten aluminum to facilitate ejection of the molten aluminum upward. In addition, the bottom of the first holding cup is closed, which makes it difficult to dissipate heat from the bottom of the first holding cup, resulting in slow heat dissipation from the lower part of the molten aluminum.

[0008] In order to facilitate temperature control, it is necessary to control the temperature dissipation rate to a similar degree. The inventors set up a spiral channel and a cooling element, which has the following beneficial effects:

[0009] The good thermal insulation effect of the thermal insulation oil is utilized to improve the thermal insulation performance of the side wall of the first holding cup, thereby slowing down the cooling speed of the upper part of the aluminum liquid.

[0010] The bottom of the first holding cup is cooled by a cooling member to ensure that after the aluminum liquid is made into aluminum material, the temperatures of the upper and lower parts of the aluminum material are similar, so as to facilitate temperature control and keep the aluminum material in a semi-solid state.

[0011] Preferably, as an improvement, the first holding cup is cylindrical with upper and lower openings, the first ejection mechanism includes a first injection rod, a connecting piece and a punch are provided on the top of the first injection rod, the top of the punch and the side wall of the first holding cup form a first material trough, the punch is a hollow structure, the punch can close the lower opening of the first holding cup and slide with the inner wall of the first holding cup, and the top of the punch is perpendicular to the side wall of the first holding cup.

[0012] The aluminum liquid temperature is above 900°C, and the first ejection mechanism of this solution is set below the slurrying part. At the same time, in order to prevent the first ejection mechanism from failing under continuous high temperature, a heat dissipation mechanism is also set, which has the following beneficial effects:

[0013] 1. The first shot rod drives the punch upward, inserts into and closes the lower opening of the first holding cup. The top of the punch and the side wall of the first holding cup form the first material trough. The aluminum liquid is introduced into the first material trough and stirred with a stirring rod for dozens of seconds to form a semi-solid aluminum material; the first shot rod continues to drive the punch upward to push the aluminum material in the first holding cup upward so that the clamping mechanism can clamp the aluminum material away; after removing the aluminum material, the first shot rod drives the punch downward out of the vertical channel for cooling, thereby realizing the three-in-one functions of slurrying, ejection, and heat dissipation.

[0014] 2. Before slurrying begins, in order to facilitate the reinsertion of the punch and close the lower opening of the first containing cup, the punch and the lower opening of the first containing cup are matched with each other, and the aluminum liquid will not flow out from the gap between the punch and the side wall of the first containing cup in a short time; and during slurrying, in order to prevent the aluminum liquid from slowly seeping out from the gap between the punch and the side wall of the first containing cup, the punch is set to a hollow structure, which has a more obvious thermal expansion effect than a solid structure. After the high-temperature aluminum liquid comes into contact with the punch, the punch contacts the side wall of the first containing cup more closely under the action of thermal expansion, thereby preventing the aluminum liquid from seeping out from the gap between the punch and the side wall of the first containing cup.

[0015] 3. When ejecting the aluminum material, the bottom of the first trough is completely formed by the punch, maximizing the contact area between the punch and the aluminum material, thereby reducing the pressure of the punch on the aluminum material; since the top of the punch is perpendicular to the side wall of the vertical channel, no eccentric force is generated, and the thrust generated by the punch at the bottom of the first trough on the aluminum material is uniform and stable, and after the punch expands, it is pressed against the side wall of the pulping part, thereby avoiding the situation of material hanging on the side wall of the pulping part.

[0016] 4. After the aluminum material is ejected, the punch moves downward out of the first holding cup, and a ventilated state is formed at the upper and lower ends of the first holding cup. Wind is generated due to the temperature difference between the inside and outside of the first holding cup. The wind takes away the heat in the vertical channel and passes through the punch, taking away the heat of the punch. The punch cools down and shrinks, and the volume of the punch becomes smaller, making it easier to insert it into the lower end of the vertical channel next time.

[0017] Preferably, as an improvement, the connecting member and the first injection rod are both hollow structures, an external liquid inlet and an external liquid outlet are provided on the side wall of the injection tube, the cooling member is vertically arranged in the injection tube, and the cooling member includes a fixed portion, a liquid inlet portion and a liquid outlet portion from bottom to top, the fixed portion is connected to the injection tube, an internal liquid inlet is provided on the side of the liquid inlet portion, and an internal liquid outlet is provided on the top of the liquid outlet portion, and the external liquid inlet, internal liquid inlet, liquid inlet, liquid outlet, internal liquid outlet and external liquid outlet are connected in sequence. In this way,

[0018] 1. Both the external liquid inlet and the external liquid outlet can be set far away from the punch to prevent the coolant delivery pipe from being affected by high temperature, thereby improving durability.

[0019] 2. Completely wrap the cooling element in coolant to avoid direct contact between the cooling element and the connecting element, the connecting element and the first injection rod, thereby improving the durability of the cooling element.

[0020] 3. The coolant is first transported to the top of the liquid outlet through the cooling element, directly contacting the punch with the highest temperature. At this time, the coolant temperature is the lowest and the cooling effect is the best; then it flows back from the outside of the cooling element, cooling the connecting piece and the first injection rod in turn.

[0021] Preferably, as an improvement, the liquid forging machine includes a forming device and a pressurizing device, the forming device includes a lower die mechanism and an upper die mechanism, the lower die mechanism includes a lower die, a first ejection hole is opened in the middle of the lower die, the upper die mechanism includes an upper die and an ejection unit, the lower surface of the upper die and the upper surface of the lower die are combined to form a die cavity, the pressurizing device includes a second ejection mechanism, the second ejection mechanism pushes the aluminum material into the die cavity from the first ejection hole and applies pressure to the aluminum material, the ejection unit includes a plurality of tie rods, the plurality of tie rods pass through the upper die and contact with the lower surface of the upper die, and the plurality of tie rods can eject the peripheral positions of the product in the upper die.

[0022] For thinner products, when the mold is first opened, the product fits tightly against the upper surface of the lower mold. This thinness can cause deformation when the product is ejected. While this deformation is minor, it can still affect quality for high-performance products. To improve product quality, the inventors have investigated various causes of product deformation in the hope of finding a solution.

[0023] Initially, the inventors increased the contact area between the second ejector mechanism and the product to reduce pressure and thus avoid product deformation. However, this not only increased the size and cost of the second ejector mechanism, but also led to a decline in molding quality. Specifically, because the second ejector mechanism is movable and its position is not fixed, the molding quality of the part of the product that contacts the second ejector mechanism is far inferior to that of the part that contacts the lower mold cavity. Therefore, the smaller the contact area with the second ejector mechanism, the better the molding quality.

[0024] Subsequently, the inventors discovered that the second ejector usually ejects the product from the middle of the lower mold while the edge of the product is still attached to the lower mold. Even after the middle of the product has been ejected a distance by the ejector, the edge of the product is still attached to the lower mold, causing product deformation. The greater the displacement difference between the middle and edge of the product, the greater the product deformation. Therefore, the inventors solved this problem from two aspects:

[0025] First, the inventors designed an ejector unit. After the mold is closed, a second ejector mechanism pushes the aluminum material into the mold cavity. This ejector unit is located on the upper mold. When the mold is opened, the second ejector mechanism pushes the product upward, and the product moves upward with the upper mold. Because the upper side of the product is tightly attached to the upper mold, it is less likely to deform and moves upward with the upper mold.

[0026] In the existing technology, the product tends to move closer to the lower mold under the action of gravity. However, after the mold is opened in this solution, the product moves upward with the upper mold, and the product tends to move away from the upper mold under the action of gravity. The ejection unit only needs a smaller thrust to demold the product.

[0027] Second, since the second ejection mechanism is used to push the aluminum material into the mold cavity and apply pressure to the aluminum material in the mold cavity, after the product is formed, the middle of the product fits most closely with the upper mold. If the product is ejected directly from the middle of the product, a large thrust is required to eject the product. The inventors dispersedly set the positions where the ejection units contact the product around the product. The ejection units first push open the edge of the product, which not only reduces the displacement difference at each position when the product is ejected, thereby reducing product deformation, but also allows the surrounding air to enter from the edge of the product and gradually fill the space between the upper mold and the product, reducing the air pressure difference between the upper and lower sides of the product, and then driving the middle of the product away from the upper mold through the edge of the product, thereby achieving the purpose of reducing deformation.

[0028] The beneficial effects of this program are:

[0029] 1. The product is ejected from the upper mold through multiple tie rods. The contact surfaces between the tie rods and the product are dispersed, and the average displacement difference generated on each contact surface is small. The displacement difference is controlled within the elastic range of the product, thereby avoiding product deformation and improving product quality.

[0030] 2. The ejector unit first pushes open the edge of the product, allowing the surrounding air to gradually fill in between the upper mold and the product, reducing the pressure difference between the upper and lower sides of the product, and then drives the middle of the product out of the upper mold through the edge of the product to achieve the purpose of reducing deformation.

[0031] Preferably, as an improvement, the upper mold mechanism further includes a center beam plate and an upper mold driver, the lower end of the upper mold driver output shaft is connected to the center beam plate, and the lower side of the center beam plate is connected to the upper mold, and the ejection unit further includes an ejection driver and a connecting plate, the ejection driver is arranged in the center beam plate, the upper end of the ejection driver output shaft passes through the center beam plate and is connected to the connecting plate, the upper ends of the pull rods are connected to the lower side of the connecting plate, and the lower ends of the pull rods pass through the center beam plate and the upper mold in sequence. Such an arrangement can produce the following effects:

[0032] 1. The upper mold drive component drives the center beam plate downward, thereby driving the upper mold downward and providing support for the upper mold when the aluminum material is formed; after the aluminum material is formed, the upper mold drive component drives the center beam plate and the upper mold upward, and the ejector drive component drives the connecting plate downward, thereby driving the pull rod downward, and then ejecting the product downward.

[0033] 2. If the output shaft of the ejector drive is directly set downward, due to the thickness of the center beam plate, the ejector drive may have insufficient stroke to drive the pull rod to eject the product. Therefore, this solution sets the ejector drive in the opposite direction, setting the output shaft of the ejector drive upward and connecting it to the pull rod through a connecting plate, thereby meeting the stroke requirements for ejecting the product.

[0034] 3. If the tie rod only passes through the upper mold, it will be difficult to detect even if the upper mold is skewed relative to the center beam plate, which will cause the upper mold to shift when the lower mold is closed, thereby reducing the product molding quality; in this solution, the tie rod passes through the center beam plate and the upper mold in turn, and plays a positioning role for the center beam plate and the upper mold, thereby preventing the upper mold from skewing relative to the center beam plate, thereby ensuring the product molding quality.

[0035] Preferably, as an improvement, the pressure device has the same structure as the pulping device. In this way, before the aluminum material is pushed into the mold cavity, the temperature of the aluminum material is maintained to ensure that the aluminum material is always maintained in a semi-solid state before being formed.

[0036] Preferably, as an improvement, a scraping device is further included, comprising a crucible and a scraping mechanism next to the crucible, the scraping mechanism comprising a frame, a horizontal moving unit provided on the frame, a vertical moving unit provided on the horizontal moving unit, a cantilever provided horizontally on the vertical moving unit, a scraping rod provided vertically at one end of the cantilever away from the vertical moving unit, and a scraping plate provided at the lower end of the scraping rod. This arrangement can produce the following beneficial effects:

[0037] After the raw materials in the crucible are melted into molten aluminum, the horizontal moving unit drives the vertical moving unit to move horizontally close to the crucible, so that the scraper plate is as close as possible to the side wall of the crucible away from the frame. The cantilever is driven downward by the vertical moving unit, thereby driving the scraper rod close to the surface of the molten aluminum, partially inserting the scraper plate into the molten aluminum, and driving the scraper plate to move toward the side close to the frame, thereby pushing the aluminum slag to the side wall of the crucible close to the frame. At this time, the aluminum liquid is scooped up with a spoon to minimize the amount of aluminum slag scooped up by the spoon, thereby improving the molding quality of the aluminum product.

[0038] Although the frame is set on the side of the crucible, the scraping rod is lifted by the cantilever part, and then the scraping plate is lifted. When scraping is needed, the scraping plate is sent into the crucible, and when scraping is not needed, the scraping plate is retracted, thereby avoiding compressing the operating space of other processes and reducing the interference of the scraping equipment with other equipment.

[0039] Since the scraper plate needs to overcome the resistance of the aluminum liquid and move horizontally when scraping the slag in the crucible, the horizontal movement of the scraper plate requires more power than the vertical movement. Therefore, the horizontal movement unit is directly fixed to the frame instead of the vertical movement unit, so as to provide more direct power for the horizontal movement.

[0040] 4. Compared with rotational motion, the horizontal moving unit and the vertical moving unit in this solution are both linear motion, with simple structure, low cost, simple trajectory, and not easy to interfere with other equipment.

[0041] Preferably, as an improvement, the inner wall of the crucible has a circular cross-section, a rotating motor is provided on the cantilever, the output shaft of the rotating motor is fixedly connected to the scraping rod, the scraping rod is rotatably connected to the cantilever, the scraping plate includes a rotating plate and a fixed plate, the fixed plate can cover the rotating plate, a limiting groove is provided on the fixed plate, the limiting groove matches the shape of the upper edge of the crucible, the fixed plate is rotatably connected to the scraping rod, and the rotating plate is fixedly connected to the scraping rod.

[0042] This configuration results in a round crucible with uniform thickness and heat transfer, without the corners of a rectangular crucible. This design is relatively common on the market, and when upgrading scraping equipment, the original crucible can be reused, saving costs and procurement time. Therefore, this solution continues to use a round crucible. However, using only a scraping blade for scraping slag creates a straight line, preventing the aluminum slag at both ends from being scraped away. To adapt the crucible shape to the desired shape, the inventors have tried various methods:

[0043] First, an elastic member is set in the scraper plate so that the length of the scraper plate can be changed according to the shape of the crucible, so that the two ends of the scraper plate are pressed against the side wall of the crucible. However, the elastic member usually cannot withstand high temperatures and is easily ineffective in molten aluminum.

[0044] Then, with the scraper rod as the axis, the scraper plate rotates around the scraper rod. Since the radius of the crucible is constant, the length of the scraper plate does not need to be changed to scrape away all the aluminum slag. However, the scraper plate drives the aluminum liquid to rotate. Even if the scraper plate scrapes the aluminum liquid to the side away from the spoon, the aluminum liquid continues to drive the aluminum slag to rotate due to inertia and returns to the side close to the spoon. Some of the aluminum slag will still be scooped away by the spoon, thereby reducing the molding quality of the aluminum product.

[0045] Next, the inventor set up a fixed plate to prevent the aluminum liquid from driving the aluminum slag to rotate back to the side close to the soup spoon. However, in order to achieve the purpose of blocking, the fixed plate needs to be connected to at least one of the scraping rod and the side wall of the crucible. But in order to facilitate the movement of the scraping rod after scraping, the inventor fixed the fixed plate on the side wall of the crucible. After the rotating plate rotates one circle, the aluminum slag sticks to the fixed plate. In order to facilitate the cleaning of the aluminum slag on the fixed plate, the fixed plate and the crucible are set to be detachable.

[0046] Later, the inventors discovered that due to precision issues, it was impossible to ensure that the scraper rod was in the same position every time it scraped the slag, which sometimes resulted in a large gap between the rotating plate and the fixed plate, allowing aluminum slag to leak through the gap, thereby reducing the molding quality of the aluminum product. Therefore, the inventors rotatably connected one end of the fixed plate to the scraper rod and provided a limit groove on the other end. On the one hand, during the downward movement of the vertical moving unit, the side wall of the limit groove was driven to apply downward pressure to the upper edge of the crucible, thereby fixing the other end of the fixed plate to the crucible; on the other hand, when the vertical moving unit drove the scraper rod upward, the aluminum slag attached to the fixed plate fell back into the crucible due to its own gravity and the tension of the aluminum liquid surface, reducing the efficiency of cleaning the aluminum slag. Compared with the use of other clamps, since the fixed plate is fixed to the crucible through the limit groove, there is no clamp obstructing the side of the fixed plate and it can be tightly attached to the rotating plate, so that the aluminum slag is sandwiched between the rotating plate and the fixed plate, thereby preventing the aluminum slag from falling when the scraper rod moves upward. After the scraper rod brings the aluminum slag to the position for processing the aluminum slag, the scraper rod drives the rotating plate to rotate, and the rotating plate pushes the fixed plate to rotate together, then the speed of the scraper rod drops rapidly, and the fixed plate separates from the rotating plate under the action of inertia, and the aluminum slag originally clamped between the two falls off; after the two are separated, the rotating plate rotates in the opposite direction, and the fixed plate collides with the rotating plate again, and the remaining aluminum slag attached to the fixed plate and the rotating plate falls off due to the collision between the two, thereby automatically cleaning the aluminum slag on the fixed plate and the rotating plate to prepare for the next scraping.

[0047] Therefore, this setting has the following effects:

[0048] Under the premise of the same capacity, the round crucible has a larger volume than the rectangular crucible and is more efficient in melting raw materials.

[0049] Through the horizontal moving unit and the vertical moving unit, the scraping rod moves to the center of the crucible, the limiting groove aligns with the upper edge of the crucible and applies downward pressure, and the scraping rod drives the rotating plate to rotate under the drive of the rotating motor, thereby scraping off the slag on the surface of the aluminum liquid.

[0050] Preferably, as an improvement, a slag trough is provided on the side wall of the crucible. Without the slag trough, after the scraper scrapes away a large amount of aluminum slag, some of the aluminum slag cannot stick to the side wall of the crucible, and some of the aluminum slag rebounds back to the side near the spoon, thereby reducing the molding quality of the aluminum product; however, the scraper scrapes the aluminum slag into the slag trough, and the aluminum slag will no longer rebound back to the side near the spoon.

[0051] Preferably, as an improvement, the slag trough includes a disassembly portion, which can accommodate aluminum slag, a filter hole is provided at the bottom of the disassembly portion, and a sealing plate is horizontally provided on the side wall of the crucible, and a plurality of sealing protrusions are provided on the sealing plate. The sealing protrusions are hemispherical, and the filter holes and the sealing protrusions cooperate with each other. With this arrangement, before the aluminum liquid melts, the disassembly portion is placed on the sealing plate. The weight and density of the disassembly portion, under the action of gravity, ensure that the sealing protrusions and the filter holes are tightly combined, so that the aluminum liquid will not enter the disassembly portion after melting, thereby preventing the aluminum slag from floating after entering the disassembly portion. If the height of the floating height is close to the height of the aluminum liquid, the aluminum slag in the disassembly portion will prevent the aluminum slag outside the disassembly portion from entering, thereby causing the aluminum slag to rebound back to the side close to the soup spoon, thereby reducing the molding quality of the aluminum product. When the aluminum slag in the disassembly portion accumulates to a certain level, the disassembly portion is removed, and the aluminum liquid that enters the disassembly portion along with the aluminum slag flows back into the crucible through the filter holes, avoiding waste of aluminum liquid. BRIEF DESCRIPTION OF THE DRAWINGS

[0052] FIG1 is a plan view of the layout of Example 1;

[0053] FIG2 is a top view of the scraping device of Example 1;

[0054] FIG3 is a three-dimensional axonometric view of the scraping mechanism of the scraping device according to Example 1;

[0055] FIG4 is a cross-sectional view of the pulping device of Example 1;

[0056] FIG5 is a cross-sectional exploded view of the first ejection mechanism of the pulping device of Example 1 (the oil cylinder is omitted).

[0057] FIG6 is a cross-sectional view of a cooling element of the pulping device of Example 1;

[0058] FIG7 is a front view of the liquid die forging machine according to Example 1;

[0059] FIG8 is a side view of the liquid die forging machine of Example 1;

[0060] FIG9 is a bottom view of the center beam plate of the liquid die forging machine of Example 1;

[0061] FIG10 is a top view of the crucible of the scraping device of Example 2;

[0062] FIG11 is a cross-sectional view taken along line AA in FIG10 ;

[0063] FIG12 is a top view of the crucible of the scraping device of Example 3;

[0064] FIG13 is a cross-sectional view taken along line BB in FIG12 . Implementation Method

[0065] The following is further described in detail through specific implementation methods:

[0066] The reference numerals in the drawings of the specification include:

[0067] Slag scraping device a0, operating table a1, turntable a2, crucible a3, slag trough a300, disassembly part a310, lifting rod a311, filter hole a312, sealing plate a320, sealing protrusion a321, slag scraping mechanism a4, frame a410, support frame a411, cantilever part a420, scraping rod a430, scraping plate a440, rotating plate a441, fixing plate a442, limiting groove a443, circular ring a444, horizontal threaded rod a451, horizontal sliding rod a452, horizontal driving member a453, sliding plate a461, sliding block a462, ridge a463, upper horizontal plate a464, lower horizontal plate a465, vertical threaded rod a466, vertical driving member a467;

[0068] Pulping device b0, upper connecting plate b101, lower connecting plate b102, positioning screw b103, first holding cup b2, upper heat-insulating portion b210, spiral channel b211, lower positioning portion b220, vertical channel b230, oil cylinder b3, first injection rod b4, external liquid port b401, external liquid inlet b402, connecting member b5, external thread b501, bearing portion b502, internal thread b503, punch b6, internal convex portion b601, sealing ring b7, cooling member b8, fixing portion b810, liquid inlet portion b820, internal liquid inlet b821, liquid outlet portion b830, internal liquid outlet b831;

[0069] Liquid forging machine c0, base c110, support legs c111, bottom plate c112, drive box c120, guide column c130, second accommodating cup c2, ejection drive c3, second injection rod c4, upper die drive c510, upper die drive output shaft c511, center beam plate c520, guide hole c521, bolt groove c522, ejection hole c523, ejection drive c531, connecting plate c532, pull rod c533, baffle c610, frame c611, cardboard c612, guide ring c613, fixing bar c614, enclosure drive c620, guide rod c630, electrical box c7. Example

[0070] Example 1 is basically as shown in Figure 1: a die-casting system, including a scraping device a0, a slurrying device b0 and a liquid die forging machine c0. The scraping device a0 heats the raw material to melt it into molten aluminum and scrapes away the aluminum slag (aluminum oxide) on the surface of the molten aluminum. The slurrying device b0 can make the molten aluminum into a semi-solid aluminum material. The liquid die forging machine c0 can shape the aluminum material. The planar layout of the scraping device a0, the slurrying device b0 and the liquid die forging machine c0 is shown in Figure 1. Figures 2 to 13 only show the core components in the corresponding positions.

[0071] As shown in Figure 2, the scraping device a0 includes an operating table a1, on which a turntable a2 and a scraping mechanism a4 are provided next to the turntable a2. Two crucibles a3 are placed on the turntable a2, and the scraping mechanism a4 includes a frame a410. As shown in Figure 3, the frame a410 includes a rectangular support frame a411, on which a horizontal moving unit is provided, on which a vertical moving unit is provided, and on which a cantilever a420 is horizontally provided. A scraping rod a430 is vertically welded at one end of the cantilever a420 away from the vertical moving unit, and a scraping plate a440 is integrally formed at the lower end of the scraping rod a430. The scraping plate a440 is a rectangular plate.

[0072] The horizontal unit includes a horizontal threaded rod a451, a horizontal sliding rod a452 and a horizontal driving member a453. The horizontal driving member a453 is arranged on the side of the support frame a411. The horizontal threaded rod a451 and the horizontal sliding rod a452 are arranged in parallel. One end of the horizontal threaded rod a451 is connected to the output shaft of the horizontal driving member a453, and the other end is rotatably connected to the frame a410. Both ends of the horizontal sliding rod a452 are welded to the support frame a411.

[0073] The vertical moving unit includes a skateboard a461, and a slider a462 is integrally formed on the rear side of the skateboard a461. The slider a462 is threadedly connected to the horizontal threaded rod a451, and the slider a462 is slidably connected to the horizontal slide rod a452. A rectangular convex strip a463 is vertically integrally formed on the left and right sides of the front side of the skateboard a461. An upper horizontal plate a464 and a lower horizontal plate a465 are respectively provided at the upper and lower ends of the front side of the skateboard a461. A vertical driving member a;467 is provided on the upper horizontal plate a464, and a vertical threaded rod a466 parallel to the two convex strips a463 is rotatably connected to the lower horizontal plate a465. The lower end of the output shaft of the vertical driving member a;467 passes through the upper horizontal plate a464 and is welded to the upper end of the vertical threaded rod a466. The right end of the cantilever a420 is threadedly connected to the vertical threaded rod a466 and is slidably connected to the vertical convex strip a463.

[0074] The horizontal driving component a453 and the vertical driving component a467 are both motors. In this embodiment, the motors are fixed by bolt connection and are both servo motors of model MR-J2S-100A.

[0075] As shown in Figure 4, the semi-solid pulping machine includes a frame, which includes an upper connecting plate b101 and a lower connecting plate b102. Four vertical positioning screws b103 are bolted between the upper connecting plate b101 and the lower connecting plate b102 (for ease of display, the positioning screws b103 are indicated by bold straight lines, and only two of them are indicated in the figure; the section lines of the upper connecting plate b101 and the lower connecting plate b102 are omitted), and a positioning hole is opened on the upper connecting plate b101.

[0076] A first accommodating cup b2 is provided on the upper connecting plate b101. The first accommodating cup b2 is a cylinder with upper and lower openings. The upper part of the first accommodating cup b2 is an upper insulation part b210, and the lower part is a lower positioning part b220. An insulation unit is provided in the side wall of the upper insulation part b210. The insulation unit includes an oil inlet, a spiral channel b211 and an oil outlet which are connected in sequence. There is insulation oil in the spiral channel b211. The inner diameter of the lower positioning part b220 is equal to that of the upper insulation part b210, and the outer diameter is smaller than that of the upper insulation part b210; the bottom of the upper insulation part b210 is bolted to the upper connecting plate b101, and the lower positioning part b220 is gap-matched with the positioning hole of the upper connecting plate b101 and passes through the positioning hole.

[0077] The lower connecting plate b102 is provided with a first ejection mechanism, which includes, from bottom to top, an oil cylinder b3, a first pressure injection rod b4, a connecting piece b5 and a punch b6. The lower connecting plate b102 is bolted to the oil cylinder b3, and the upper end of the output shaft of the oil cylinder b3 is threadedly connected to the bottom of the first pressure injection rod b4. As shown in FIG5 , the first pressure injection rod b4, the connecting piece b5 and the punch b6 are all hollow structures with circular cross-sections and are internally connected. The hollow section in the connecting piece b5 is smaller than the hollow section in the first pressure injection rod b4 and the punch b6. External threads b501 are provided at the upper and lower ends of the connecting piece b5. The middle part of the connecting piece b5 protrudes circumferentially to form a bearing portion b502, which bears Part b502 can transmit the impact force of the first pressing rod b4 to the punch b6. The lower end of the punch b6 and the upper end of the first pressing rod b4 are provided with internal threads b503, and are respectively threadedly connected to the upper and lower ends of the connecting member b5. A sealing ring b7 is provided between the connecting member b5, the punch b6 and the first pressing rod b4; the punch b6 is clearance-matched with the vertical channel b230, the punch b6 and the vertical channel b230 are slidingly connected and can close the lower end of the vertical channel b230, the top of the punch b6 is perpendicular to the side wall of the vertical channel b230, the punch b6 is an inverted "U" shape, the hollow structure of the punch b6 forms a top inner cavity, and the middle part of the top inner cavity bulges inward to form an inner convex part b601.

[0078] An external liquid inlet b402 and an external liquid outlet b401 are provided on the side wall of the first injection rod b4. As shown in FIG6 , a vertical cooling member b8 is also provided inside the first injection rod b4 (for ease of display, the cooling member b8 is omitted in FIG4 and FIG5 ). The cooling member b8 includes, from bottom to top, a fixed portion b810, a liquid inlet portion b820, and a liquid outlet portion b830. The fixed portion b810 and the liquid inlet portion b820 are integrally formed. The liquid inlet portion b820 and the liquid outlet portion b830 are welded. The bottom of the fixed portion b810 is bolted to the first injection rod b4. Two sealing rings b7 are also provided between the fixed portion b810 and the side wall of the first injection rod b4. The two sealing rings b 7 are all located below the external liquid port b401. The side of the liquid inlet b820 has an internal liquid inlet b821. The liquid outlet b830 is a copper tube that passes through the connector b5 and is inserted into the punch b6. The top of the liquid outlet b830 is the internal liquid outlet b831. The space between the cooling element b8, the punch b6, the connector b5, and the first injection rod b4 forms a reflux channel that connects the internal liquid outlet b831 and the external liquid port b401. The external liquid inlet b402, the internal liquid inlet b821, the liquid inlet b820, the liquid outlet b830, the internal liquid outlet b831, the reflux channel, and the external liquid port b401 are connected in sequence. An annular cutout is provided on the liquid inlet b820. It is located below the internal liquid inlet b821 and above the two sealing rings b7. Some coolant is contained between the annular cutout and the inner wall of the first injection rod b4.

[0079] As shown in Figure 7, the liquid forging machine c0 includes a frame a, a forming device, a pressurizing device and an electrical box c7. The bracket includes a rectangular base c110 and a drive box c120. A second top entry hole is opened on the base c110. Four legs c111 are integrally formed under the base c110. A bottom plate c112 is integrally formed at the lower ends of the four legs c111. A guide column c130 is interference fit at each of the four corners on the upper side of the base c110. The upper ends of the four guide columns c130 are interference fit with the lower side of the drive box c120.

[0080] The forming device is arranged on the frame a. The forming device includes an upper mold mechanism, a lower mold mechanism and a blocking mechanism. The upper mold mechanism includes an upper mold driving component c510, a middle beam plate c520, an upper mold (not shown in the figure) and an ejection unit. The oil tank of the upper mold driving component c510 is bolted to the side of the driving box c120. The upper mold driving component c510 is bolted inside the driving box c120. In this embodiment, there are two upper mold driving components c510.

[0081] The lower ends of the output shafts of the two upper mold driving members c510 are bolted to the upper side of the middle beam plate c520. As shown in Figure 9, the middle beam plate c520 is rectangular, and a guide hole c521 is opened at each of the four corners of the middle beam plate c520. The guide column c130 passes through the guide hole c521 and is slidably connected to the guide hole c521. At the position between the upper mold driving member output shafts c511 of the two upper mold driving members c510, a number of vertical ejection holes c523 are opened on the middle beam plate c520, and a number of bolt grooves c522 are opened on the lower side of the middle beam plate c520.

[0082] Depending on the type of upper mold, the upper mold can be directly connected to the bolt groove c522 bolt, or the clamp can be first connected to the bolt groove c522 bolt, and then the clamp is used to fix the upper mold.

[0083] The ejection unit includes an ejection drive member c531, a connecting plate c532 and a plurality of tie rods c533, as shown in Figure 8. For ease of display, the figure only shows a cross-sectional view of the output shaft portion of the ejection drive member c531. The upper end of the output shaft of the ejection drive member c531 passes through the middle beam plate c520 and is threadedly connected to the left end of the connecting plate c532. The plurality of tie rods c533 are welded to the lower right end of the connecting plate c532. The plurality of tie rods c533 pass through the ejection hole c523 of the middle beam plate c520 and the upper mold (not shown in the figure) in turn as shown in Figure 9, and then contact the lower surface of the mold cavity of the upper mold. The plurality of tie rods c533 can eject the peripheral position of the product in the upper mold downward.

[0084] As shown in FIG7 , the lower mold mechanism includes a lower mold (not shown), the lower surface of the upper mold and the upper surface of the lower mold enclose a closed mold cavity, the lower mold is bolted to the base c110, and an entry hole is opened in the middle of the lower mold.

[0085] The pressurizing device includes a second receiving cup c2 and a second ejection mechanism. The second ejection mechanism includes a second pressing rod c4 and an ejection drive member c. The ejection drive member c is bolted on the base plate c112. The upper end of the output shaft of the ejection drive member c is welded to the lower end of the second pressing rod c4. The top of the second pressing rod c4 is slidably connected to the second receiving cup c2. The second receiving cup c2 is bolted to the second ejection hole of the base c110. The top of the second pressing rod c4 and the side wall of the second receiving cup c2 form a second material trough that can accommodate aluminum material. The second material trough is aligned with the first ejection hole. The second ejection mechanism structure pushes the aluminum material into the mold cavity from the first ejection hole and applies pressure to the aluminum material.

[0086] As shown in Figures 7 and 8, the enclosure mechanism includes four enclosure units, which are respectively arranged in four directions of the frame a. When the second pressing rod c4 presses the aluminum material into the mold cavity, it can prevent the aluminum material from splashing out under the action of pressure and injuring people, thereby improving safety. The four enclosure units all include a baffle c610, an enclosure drive c620 and two vertically arranged guide rods c630. The upper ends of the two guide rods c630 are welded to the bottom side of the drive box c120, and the lower ends are welded to the upper side of the base c110. The baffle c610 includes a frame c611 and a cardboard c612. The cardboard c612 is glued to the frame c611 for easy replacement. Three guide rings c613 are welded on both sides of the frame c611. A guide rod c630 passes through the three guide rings c613 and is slidably connected to the three guide rings c613. An L-shaped fixing strip c614 is provided above the cardboard c612. One side of the fixing strip c614 is welded to the frame c611, and the other side of the fixing strip c614 is bolted to the upper end of the output shaft of the enclosure drive c620. The lower end of the enclosure drive c620 is bolted to the base plate c112.

[0087] The upper mold driving component c510, the ejection driving component c531, the ejection driving component c and the enclosure driving component c620 are all hydraulic cylinders and are powered by the electrical box c7.

[0088] The specific implementation steps are as follows:

[0089] 1. After the raw materials in the crucible a3 are melted into molten aluminum, the crucible a3 is rotated to the side close to the scraping mechanism a by the turntable a2, and the vertical moving unit is driven by the horizontal moving unit to horizontally approach the crucible a3, so that the scraping plate a440 is as close as possible to the side wall of the crucible a3 away from the side of the frame a410. The cantilever part a420 is driven downward by the vertical moving unit, thereby driving the scraping rod a430 close to the liquid surface of the aluminum liquid, and partially inserting the scraping plate a440 into the aluminum liquid.

[0090] 2. Drive the scraper plate a440 to move toward the side close to the frame a410, and then push the aluminum slag to the side wall of the crucible a3 close to the frame a410; rotate the turntable a2, rotate the crucible a3 to the side close to the soup spoon, use the soup spoon to scoop the aluminum liquid out of the crucible a3, and rotate the other crucible a3 with molten aluminum liquid to the side close to the scraper mechanism a; at the same time, drive the oil cylinder b3 of the slurry making device b0 to drive the first injection rod b4 to move upward, and then drive the punch b6 to move upward, blocking the lower end of the first receiving cup b2. The top of the punch b6 and the side wall of the first receiving cup b2 form a first material trough, and the scooped aluminum liquid is placed in the first material trough.

[0091] 3. After the high-temperature aluminum liquid comes into contact with the punch b6, the punch b6 is pressed against the side wall of the first holding cup b2 due to thermal expansion. The aluminum liquid is stirred for tens of seconds using a stirring rod to form a semi-solid aluminum material. At the same time, the insulation oil enters from the oil inlet and flows out from the oil outlet to form a circulation, which has an insulating effect on the aluminum liquid in the spiral channel b211. The coolant enters from the external liquid inlet b402 of the cooling part b8, first flows upward through the liquid outlet b830 into the punch b6, and cools the punch b6. The inner convex part b601 of the punch b6 blocks the coolant from flowing downward, thereby increasing the time the coolant stays in the punch b to improve the cooling effect. The coolant then flows out from the outside of the cooling part b8, that is, from the reflux channel and the external liquid outlet b401 in sequence. When the coolant flow rate is too slow to reduce the temperature to a reasonable range, the coolant contained between the annular cutout and the inner wall of the first injection rod b4 begins to expand due to the high temperature. The coolant generates a reaction force on both sides, thereby widening the gap between the fixed part b810 and the inner wall of the first injection rod b4. The fixed part b810 and the inner wall of the first injection rod b4 cannot clamp the sealing ring b7, causing the coolant to overflow out of the first injection rod b4. The operator observes the coolant overflow and finds that the cooling effect is insufficient, and then speeds up the flow rate of the coolant to improve the cooling effect.

[0092] 4. Drive the oil cylinder b3 to drive the first injection rod b4 to continue to move upward, and then drive the punch b6 to move upward, ejecting the aluminum material in the first receiving cup b2 upward so that the clamping mechanism can take away the aluminum material; at the same time, bolt the upper die of the liquid forging machine c0 to the lower side of the center beam plate c520, so that the lower end of the tie rod c passes through the upper die and contacts the lower surface of the upper die, bolt the lower die to the upper side of the base c110, align the first ejection hole of the lower die with the second trough, and place the aluminum material taken away by the clamping mechanism into the second trough.

[0093] 5. Drive the upper mold driver c510 to move the center beam c520 downward, thereby driving the upper mold downward and closing the upper and lower molds; drive the enclosure driver c620 to move the baffle c610 upward to surround the upper and lower molds; drive the ejection driver c, which drives the second injection rod c4 upward. The second injection rod c4 pushes the aluminum material into the mold cavity. The second injection rod c4 continuously applies pressure to the aluminum material in the mold cavity, thereby forming the aluminum material.

[0094] 6. Drive the enclosure drive c620, which drives the baffle c610 to move downward, exposing the upper and lower molds, and drives the upper mold drive c510, thereby driving the center beam c520 and the upper mold to move upward. At the same time, the ejection drive c drives the second injection rod c4 to move upward, and the second injection rod c4 pushes the product upward, so that the product moves upward with the upper mold; the ejection drive c531 drives the connecting plate c532 to move downward, thereby driving the pull rod c533 to move downward, and then ejecting the product downward, so that the product is separated from the upper mold. Example

[0095] The difference between the scraping device a0 in Example 2 and Example 1 is that the inner wall of the crucible a3 is a circular cross-section, a rotating motor is provided at the left end of the cantilever a420, the lower end of the output shaft of the rotating motor passes through the cantilever a420 and is welded to the upper end of the scraping rod a430, and a horizontally arranged annular groove is opened on the scraping rod a430. As shown in Figure 10, the scraper plate a440 includes a rotating plate a441 and a fixed plate a442. The side of the rotating plate a441 and the fixed plate a442 close to the scraper rod a430 is the inner side. As shown in Figure 11, the fixed plate a442 can cover the rotating plate a441. A limiting groove a443 is opened on the lower side of the fixed plate a442. The limiting groove a443 matches the shape of the upper edge of the crucible a3. The fixed plate a442 is rotatably connected to the scraper rod a430. Specifically, a circular ring a444 is integrally formed on the upper end of the inner side of the fixed plate a442, and the circular ring a444 is rotatably matched with the annular groove on the scraper rod a430; the inner side of the rotating plate a441 is integrally formed with the scraper rod a430.

[0096] The specific implementation steps differ from those in Example 1 in that:

[0097] In step 1: the scraper rod a430 is moved to the center of the crucible a3 through the horizontal moving unit and the vertical moving unit, the limiting groove a443 is aligned with the upper edge of the crucible a3 and exerts downward pressure, and the fixing plate a442 is clamped on the edge of the crucible a3.

[0098] In step 2: the scraper rod a430 drives the rotating plate a441 to rotate under the drive of the rotating motor, thereby scraping off the filter residue on the surface of the aluminum liquid; the rotating plate a441 and the fixed plate a442 clamp the aluminum slag, and the horizontal moving unit and the vertical moving unit drive the scraper rod a430 to move upward, thereby taking out the aluminum slag. Example

[0099] The slag scraping device a0 in Example 3 differs from that in Example 1 in that, as shown in Figures 12 and 13, a slag trough a300 is integrally formed on the sidewall of the crucible a3. The side of the slag trough a300, facing away from the sidewall, is flat and has the same width as the scraping plate a440. The slag trough a300 includes a disassembly portion a310 and a sealing plate a320. For ease of illustration, the cross-hatching of these two components has been omitted. The disassembly portion a310 is cup-shaped and can hold aluminum slag. A lifting lever a311 is provided at its upper end to facilitate manual lifting of the disassembly portion a310. A sealing plate a320 is integrally formed on the sidewall of the crucible a3. Several hemispherical sealing protrusions a321 are integrally formed on the sealing plate a320. The bottom of the disassembly portion a310 is provided with several filter holes a312. The bottom thickness of the disassembly portion a310 is 3-10 cm, with 5 cm being preferred in this embodiment. The filter holes a312 cooperate with the sealing protrusions a321. The sealing performance of the sealing protrusions a321 against the filter holes a312 is sufficient to ensure that the volume of the molten aluminum entering the disassembly portion a310 is negligible relative to the volume of the aluminum slag. The thickness of the upper end of the sidewall of the disassembly portion a310, away from the sidewall of the crucible a3, gradually decreases from bottom to top.

[0100] The specific implementation steps differ from those in Example 3 in that:

[0101] In step 1: before the aluminum liquid melts, the disassembly part a310 is placed on the sealing plate a320. Due to the weight and density of the disassembly part a310, under the action of gravity, the sealing protrusion a321 and the filter hole a312 are tightly combined, so that the aluminum liquid will not enter the disassembly part a310 after melting.

[0102] In step 2: when there is a lot of aluminum slag in the disassembly part a310, lift the lifting rod a311, the filter hole a312 is separated from the sealing protrusion a321, and the aluminum liquid that enters the disassembly part a310 together with the aluminum slag flows back to the crucible a3 from the filter hole a312. Example

[0103] Example 4 is based on Example 1: the pressurizing device and the pulping device b0 have the same structure.

[0104] The above is only an embodiment of the present invention, and the common knowledge such as the specific technical solutions and / or characteristics in the solution are not described in detail here. It should be pointed out that for those skilled in the art, without departing from the technical solution of the present invention, several variations and improvements can be made, which should also be regarded as the scope of protection of the present invention, and these will not affect the effect of the implementation of the present invention and the practicality of the patent. The scope of protection required by this application shall be based on the content of its claims, and the specific implementation methods and other records in the description can be used to interpret the content of the claims.

Claims

1. A die casting system, characterized in that: It includes a pulping device and a liquid die forging machine. The pulping device can make aluminum liquid into semi-solid aluminum material, and the liquid die forging machine can shape the aluminum material. The pulping device includes a first receiving cup and a first ejection mechanism at the bottom of the first receiving cup. A spiral channel is arranged in the side wall of the first receiving cup, and there is insulation oil in the spiral channel. A cooling piece is arranged at the bottom of the first receiving cup.

2. A die casting system according to claim 1, characterized in that: The first receiving cup is in the shape of a cylinder with upper and lower openings. The first ejection mechanism includes a first ejection rod. A connecting piece and a punch are provided on the top of the first ejection rod. The top of the punch and the side wall of the first receiving cup form a first material trough. The punch is a hollow structure. The punch can close the lower opening of the first receiving cup and slide with the inner wall of the first receiving cup. The top of the punch is perpendicular to the side wall of the first receiving cup.

3. A die casting system according to claim 2, characterized in that: The connecting piece and the first injection rod are both hollow structures, an external liquid inlet and an external liquid outlet are provided on the side wall of the injection tube, the cooling piece is vertically arranged in the injection tube, and the cooling piece includes a fixed part, a liquid inlet part and a liquid outlet part from bottom to top, the fixed part is connected to the injection tube, an internal liquid inlet is provided on the side of the liquid inlet part, and an internal liquid outlet is provided on the top of the liquid outlet part, and the external liquid inlet, the internal liquid inlet, the liquid inlet part, the liquid outlet part, the internal liquid outlet and the external liquid outlet are connected in sequence.

4. A die casting system according to claim 3, characterized in that: The liquid die forging machine includes a forming device and a pressurizing device. The forming device includes a lower die mechanism and an upper die mechanism. The lower die mechanism includes a lower die with a first ejection hole in the middle. The upper die mechanism includes an upper die and an ejection unit. The lower surface of the upper die and the upper surface of the lower die are combined to form a die cavity. The pressurizing device includes a second ejection mechanism. The second ejection mechanism ejects aluminum material into the die cavity from the first ejection hole and applies pressure to the aluminum material. The ejection unit includes a plurality of tie rods. The plurality of tie rods pass through the upper die and contact the lower surface of the upper die. The plurality of tie rods can eject the peripheral position of the product in the upper die.

5. A die casting system according to claim 4, characterized in that: The upper mold mechanism also includes a center beam plate and an upper mold driving component. The lower end of the output shaft of the upper mold driving component is connected to the center beam plate, and the lower side of the center beam plate is connected to the upper mold. The ejection unit also includes an ejection driving component and a connecting plate. The ejection driving component is arranged in the center beam plate, and the upper end of the output shaft of the ejection driving component passes through the center beam plate and is connected to the connecting plate. The upper ends of the pull rods are connected to the lower side of the connecting plate, and the lower ends of the pull rods pass through the center beam plate and the upper mold in sequence.

6. A die casting system according to claim 5, characterized in that: The pressurizing device has the same structure as the pulping device.

7. A die casting system according to claim 6, characterized in that: It also includes a scraping device, which includes a crucible and a scraping mechanism next to the crucible. The scraping mechanism includes a frame, a horizontal moving unit is provided on the frame, a vertical moving unit is provided on the horizontal moving unit, a cantilever is horizontally provided on the vertical moving unit, a scraping rod is vertically provided at one end of the cantilever away from the vertical moving unit, and a scraping plate is provided at the lower end of the scraping rod.

8. The die casting scraping equipment according to claim 7, characterized in that: The inner wall of the crucible has a circular cross-section, and a rotating motor is provided on the cantilevered part. The output shaft of the rotating motor is fixedly connected to the scraping rod, and the scraping rod is rotatably connected to the cantilevered part. The scraping plate includes a rotating plate and a fixed plate, and the fixed plate can cover the rotating plate. A limiting groove is provided on the fixed plate, and the limiting groove matches the shape of the upper edge of the crucible. The fixed plate is rotatably connected to the scraping rod, and the rotating plate is fixedly connected to the scraping rod.

9. The die casting scraping equipment according to claim 7, characterized in that: A slag groove is provided on the side wall of the crucible.

10. The die casting scraping equipment according to claim 9, characterized in that: The slag trough comprises a disassembly part which can hold aluminum slag, a filtering hole is arranged at the bottom of the disassembly part, a sealing plate is arranged horizontally on the side wall of the crucible, a plurality of sealing protrusions are arranged on the sealing plate, the sealing protrusions are hemispherical, and the filtering hole and the sealing protrusions cooperate with each other.

Citation Information

Patent Citations

  • Aluminium alloy frying pan liquid die-forging die and technique for producing aluminium alloy frying pan

    CN101468378A

  • Liquid forging and molding die for aluminum alloy wheel

    CN105397066A

  • Heating equipment for semisolid die-casting slurry

    CN106216630A

  • Punch assembly and die casting machine including punch assembly

    CN109382496A

  • Special aluminum alloy semi-solid material preparation and automatic forming device

    CN109732054A

Cited By

  • Automobile part die-casting die capable of automatically taking materials