Method for recycling a glazing unit

The glass recycling process addresses the challenge of recycling flat glass with non-glass components by using non-breakable adhesive films to separate glass pieces, ensuring efficient recycling and maintaining chemical integrity, thus overcoming the inefficiencies of existing methods.

WO2024223761A1PCT designated stage expired Publication Date: 2024-10-31SAINT GOBAIN SEKURIT FRANCE
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/061435
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2024-04-25
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

The recycling of flat glass glazing with non-glass components, such as defrosting resistors in vehicle rear windows, is challenging due to the risk of metallic materials melting and altering the glass composition, and existing separation processes are inefficient and costly.

Method used

A glass recycling process that involves bonding non-breakable components to the glazing surface before breaking, allowing for the separation of glass pieces with and without significant non-glass material, using flexible adhesive films to isolate areas with non-glass components, facilitating easy separation and recycling.

Benefits of technology

This process enables efficient separation and recycling of glass substrates with minimal chemical alteration, allowing for the production of recycled glass with desired chemical characteristics, reducing energy consumption and costs associated with sorting and processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024061435_31102024_PF_FP_ABST
    Figure EP2024061435_31102024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention relates to a method for recycling a glazing unit (1) comprising components made of non-glass material, the method comprising a step of breaking up the glazing unit followed by a step of sorting the pieces (100) of the glazing unit (1) in order to separate the pieces (100) of the glazing unit (1) that are associated with a substantial amount of the non-glass material from the pieces of the glazing unit that are not associated with a substantial amount of the non-glass material. According to the invention, the method comprises a preliminary step, before the step of breaking up the glazing unit (1), of bonding at least one non-breakable component (31, 32) to a portion of the surface of the glazing unit (1) in the regions of the glazing unit that are associated with the components made of non-glass material and the sorting step is carried out by removing, from among the pieces (100) of the glazing unit (1), the one or more non-breakable components (31, 32) with the pieces (100) of the glazing unit (1) that are adhered thereto.
Need to check novelty before this filing date? Find Prior Art

Description

Glass recycling process Field of invention

[0001] The present invention relates to the recycling of flat glass glazing.

[0002] In particular, the invention relates to the recycling of glazing composed of a glass substrate on which a component made of non-glass material is assembled. Prior art

[0003] Glass is generally made by melting raw materials that include silica. It is also possible to make it by melting pieces of recycled glass. This process using recycled glass requires less energy to produce the same quantity of glass than the process requiring the melting of raw materials and their transformation to form the desired glass composition. Manufacturing glass from recycled glass is therefore particularly advantageous and has a lower CO2 impact.

[0004] To make glass from recycled glass, recycled glass must have the desired chemical composition for the glass to be made. A particular challenge arises when recycling objects composed of both glass and components made of a non-glass material. If these components are infusible, they may float on the molten glass and must be removed. If, on the other hand, these components are fusible at the melting temperature of the glass, they may melt along with the recycled glass and mix with it, changing its chemical composition, or even interact chemically with the molten glass or tin bath. It is therefore generally not desirable to recycle such objects composed of both glass and fusible non-glass components.

[0005] Such a difficulty can arise in particular for the recycling of automotive glazing, and in particular vehicle rear windows. Vehicle rear windows most often include a defrosting resistor formed of electrically conductive tracks, deposited on one side of a glass substrate of the rear window. These tracks are often formed by an electrically conductive silver paste, which is deposited by screen printing on the glass substrate and solidified by high-temperature baking. When the vehicle is in use, these tracks can be crossed by an electric current in order to heat up to allow the rear window to be demisted or defrosted.Typically, on a rear window, the defrosting resistor is made up of thin tracks offering high electrical resistance, allowing the rear window to be defrosted or demisted, and thick tracks, offering lower electrical resistance, which ensure the electrical connection of the thin tracks.

[0006] Such defrosting resistors can also be provided on vehicle windscreens or, in certain cases, on vehicle side windows.

[0007] Recycling such vehicle glazing is problematic, as the metallic material contained in the defrosting resistor is likely to melt with the recycled glass, changing its composition in an unacceptable way or altering the properties of the tin bath.

[0008] To enable, however, the recycling of glass substrates from vehicle rear windows, documents US20200165697A1, WO2009087908A1, US2022228235 and WO2020240126 are known, for example, describing chemical processes for dissociating a metal component from the glass with which it is associated. However, it is not very efficient to subject the entire rear window glazing to such a separation process.

[0009] It is also known to sort glass pieces according to whether or not they are associated with non-glass components. However, such sorting is complicated and expensive.

[0010] The present invention aims to overcome these drawbacks of the prior art.

[0011] In particular, the invention aims to provide a glass recycling method allowing optimized recycling of flat glass glazing composed of a glass substrate on which a component made of non-glass material is assembled.

[0012] A particular objective of the invention is to enable the optimized recycling of automotive glazing, and in particular of motor vehicle rear windows equipped with defrosting resistors comprising metallic materials.

[0013] Yet another objective of the invention is to propose such a recycling process which allows the production of recycled glass, which has chemical characteristics as close as possible to those desired.

[0014] Yet another object of the invention is to provide such a recycling method which is easy to implement.

[0015] These objectives, as well as others which will become more clearly apparent later, are achieved using a method for recycling a glazing unit comprising a glass substrate and at least one component made of non-glass material secured to the glass substrate, this method comprising a step of breaking the glazing unit, followed by a step of separating the pieces of glazing unit, to separate the pieces of glazing secured to a substantial quantity of the non-glass material, from the pieces of glazing unit which are not secured to a substantial quantity of the non-glass material.According to the invention, this method comprises a preliminary step, before the step of breaking the glazing, of bonding at least one non-breakable component to a portion of the surface of the glazing, at least one area of ​​the glazing to which at least one of the components made of non-glass material is secured, and the separation step comprises separating the non-breakable components, with the pieces of glazing bonded thereto, from the other pieces of glazing which are not bonded to the non-breakable component.

[0016] Advantageously, the glazing is automotive glazing.

[0017] Advantageously, the glazing is a rear window of a motor vehicle, comprising a defrosting resistor constituting one of the components made of non-glass material.

[0018] According to an advantageous embodiment, the component made of non-glass material is a component screen-printed on the glass substrate, to form said glazing.

[0019] Preferably, the non-glass component comprises a metal alloy screen-printed onto the glass substrate.

[0020] According to an advantageous embodiment, the non-breakable component is a flexible adhesive film.

[0021] Preferably, this flexible adhesive film is made of plastic material.

[0022] According to a preferred embodiment, the non-breakable component is bonded to one face of said glass substrate on which the component made of non-glass material is secured.

[0023] According to another possible embodiment, one of the non-breakable components is bonded to each of the two opposite faces of the glass substrate, at least one of the areas of the glazing on which at least one of the components made of non-glass material is secured. Description of figures

[0024] The invention will be better understood upon reading the following description of preferred embodiments, given as a simple figurative and non-limiting example, and accompanied by the figures among which: La represents a glazing constituting a rear window of a motor vehicle. La represents the glazing of the, after it has been broken. La represents the glazing of the on which non-breakable adhesive components have been glued, according to an embodiment of the method of the invention. La represents the glazing of the, on which the non-breakable adhesive components have been glued, after it has been broken. La represents the non-breakable adhesive components as well as the fragments of the glazing of the which adhere thereto. La is a graph showing the steps of a recycling method according to an embodiment of the invention.

[0025] It represents, in front view, a glazing 1 constituting a rear window of a motor vehicle.

[0026] Motor vehicle glazings, such as windshields or rear windows of a motor vehicle, may consist of several glass substrates superimposed on each other, between which layers of non-glass materials, such as plastic materials, may be interposed. The term "glazing" used in the present description preferably applies to a single glass substrate. However, it may also apply to a composite assembly comprising several superimposed glass substrates.

[0027] The glazing 1 is formed from a glass substrate 10, onto which components made of non-glass material are secured.

[0028] A glass substrate, within the meaning of the present description, is a flat glass plate, made of a glass material, that is to say a non-crystalline solid material exhibiting the glass transition phenomenon. Preferably, this glass substrate is transparent, that is to say it allows specular transmission of radiation at least in the wavelength ranges useful for the intended application of the element. In this case, the glass substrates used as glazing for motor vehicles are normally transparent at least in the visible wavelength range. The glass substrate may also be covered by components such as enamels, which may themselves be made of a glass material that does not prevent the recycling of the glass substrate.

[0029] Non-glass material components, within the meaning of this description, are components which are not formed mainly or essentially of a glass material, which can be secured to a glass substrate.

[0030] The glass substrate may, in a known manner, be covered on one or both of its faces with a thin coating layer. Such a coating, which may be made of a non-glass material, generally has a very thin thickness, and its mass therefore forms only a tiny proportion of the total mass of the glazing. The small proportion of non-glass material that such a coating brings into a glazing is generally not considered to constitute an obstacle to the recycling of this glazing.

[0031] In the embodiment shown, components made of non-glass material constitute a defrosting resistor 2, formed of electrically conductive tracks, deposited on one face of the glass substrate. These tracks are formed by an electrically conductive material, which is deposited for example by screen printing on the glass substrate and solidified and secured to the glass substrate by high-temperature firing.

[0032] The mass of such a non-glass component remains low, compared to the total mass of the glazing. However, it is significant enough to affect the recycling conditions of this glazing. For example, a glazing comprising a glass substrate and a non-glass component may be considered to comprise a significant quantity of non-glass material when the mass of this non-glass component represents more than 200 ppm (parts per million) of the total mass of the glazing. However, such a definition is only indicative, and may vary, for example, depending on the recycling process implemented.

[0033] The electrically conductive material implemented in the defrosting resistor 2 may be an at least partially metallic alloy which, in the embodiment shown, comprises a mixture of at least 80% silver and a glass frit, which facilitates its adhesion to the glass substrate. This coating thus has a high hardness and cannot be easily removed from the glass substrate.

[0034] Conventionally, the defrosting resistor 2 of the glazing 1 is composed of thin tracks offering a high electrical resistance, and thick tracks, offering a lower electrical resistance. The thick tracks form the lateral collectors 21, 22 and 23, placed along two lateral edges of the glass substrate. The lateral collector 21 being located along one of the edges, is connected to the lateral collectors 22 and 23, located along the other edge, by a plurality of thin tracks forming the heating wires 24.

[0035] The lateral collectors 21, 22 and 23 are intended to ensure efficient conduction of the electric current, without opposing any significant resistance. These collectors therefore have large dimensions, using a relatively large quantity of non-glass material.

[0036] On the contrary, the heating wires 24 are intended to heat up when an electric current passes through them. They must therefore offer a high resistance and consequently have a very small cross-section. These heating wires 24 are therefore formed by a very small quantity of non-glass material.

[0037] A large part of the non-glass material used to form the defrosting resistor 2 is therefore placed in the collectors 21, 22 and 23. Although the heating wires 24 cover a larger surface area of ​​the glazing 1, the mass of non-glass material that they use is, on the contrary, relatively low.

[0038] To recycle the glazing 1, it is necessary to break it to melt the pieces. This represents the glazing 1 broken into pieces 100. Among these pieces 100, the vast majority consists solely of glass material, or has only a very small proportion of non-glass material associated with the glass material. On the contrary, the pieces 100 corresponding to the parts of the glazing 1 comprising the collectors 21, 22 and 23 have a more significant proportion of non-glass material.

[0039] Processing all of the glass pieces 100 to separate the non-glass material from the glass material would be inefficient. Efficient recycling of the glass would require separating the pieces 100 comprising exclusively or almost exclusively glass material, which can be recycled directly, from the pieces 100 comprising a significant portion of non-glass material, which can undergo processing to separate the glass material from the non-glass material. Such sorting of the pieces 100 is, however, very complicated and expensive.

[0040] To facilitate the separation of pieces of glass 100 composed exclusively or almost exclusively of glass material from pieces 100 comprising a significant portion of non-glass materials, the invention proposes a particular method for recycling glass.

[0041] According to the invention, the method for recycling glass comprises, before a step 92 of breaking the glazing, a preliminary step 91 of bonding non-breakable components to a portion of the surface of this glazing. A non-breakable component, within the meaning of the present description, is a component that can be secured to a glazing and does not break when the glazing is broken. Such a non-breakable component may be a rigid component, for example metallic, having mechanical characteristics that prevent it from breaking under the effect of an impact breaking the glazing. It may also be made of a flexible material, such as a plastic film, capable of deforming without breaking under the effect of an impact breaking the glazing.

[0042] According to still other possible embodiments of the invention, the bonding of non-breakable component on a part of the surface of the glazing can be done by depositing, on a part of the surface of this glazing, a liquid component solidifying after its deposition, such as for example an organic resin or a plastic coating. This liquid component constitutes a non-breakable component within the meaning of the present invention if, after its solidification and after the breaking of the glazing, it is capable of retaining the shards of the glazing to which it is secured.

[0043] According to the invention, the non-breakable component is only bonded to a portion of the surface of the glazing, in order to allow separate recycling of the portions of the glazing bonded to a non-breakable component and the portions of the glazing which are not bonded to a non-breakable component. It is particularly advantageous for the non-breakable component(s) to be bonded only to a portion of the surface of a face of the glazing less than 50% of the total surface area of ​​the face of this glazing, and even preferably less than 10% of the total surface area of ​​the face of this glazing.

[0044] The represents the glazing 1 on which such components made of non-breakable material have been applied. In this case, these components made of non-breakable material consist of portions of adhesive film 31 and 32, such as adhesive tape, which are glued to one face of the glazing 1, at the collectors 21, 22 and 23.

[0045] More precisely, a portion of adhesive film 31 is glued to one face of the glazing 1, to an area of ​​this glazing 1 on which the collector 21 is secured, and a portion of adhesive film 32 is placed on one face of the glazing 1, to an area of ​​this glazing 1 on which the collectors 22 and 23 are secured. These portions of adhesive film 31 and 32, constituting non-breakable components, therefore cover the areas of the glazing 1 on which significant quantities of non-glass material are secured.

[0046] In the embodiment shown, it has in fact been chosen to only bond the components made of non-breakable material to the areas of the glazing 1 to which the collectors 21, 22 and 23 are secured, which concentrate a large part of the non-glass materials of the glazing 1, and not to bond them to the heating wires 24. It would also be possible, in a variant of this embodiment, to bond components made of non-breakable material to all the areas of the glazing 1 at which the non-glass components are secured, that is to say to the areas of this glazing 1 to which the collectors 21, 22 and 23 are secured as well as to the areas of this glazing 1 to which the heating wires 24 are secured.

[0047] The non-breakable components may, according to the invention, be bonded to one or other of the faces of the glazing 1, or to both faces, on the portions of this glazing which comprise non-glass components in significant quantity. In the preferred embodiment shown, however, the portions of adhesive film 31 and 32 constituting the non-breakable components are bonded to the face of the glazing 1 which comprises the deposits of non-glass material. The choice of bonding the non-breakable components to this face in fact makes it possible to delimit as precisely as possible the outline of the areas of the glazing which comprise non-glass components in significant quantity, on which to bond the non-breakable component.

[0048] Following the step 91 of bonding non-breakable components to the glazing 1, the recycling method according to the invention comprises a step 92 of breaking the glazing. The glazing 1 can thus be reduced to pieces 100, as shown in 1a. This breaking of the glazing does not result in breakage or separation of the non-breakable components formed by the portions of adhesive film 31 and 32, which remain associated with the pieces of glazing to which they were bonded.

[0049] After this step 92 of breaking the glazing 1, the method according to the invention implements a step 93 of separating the pieces 100 of the glazing 1 associated with the non-breakable components, on the one hand, and the pieces 100 of the glazing 1 which are not associated with the non-breakable components, on the other hand.

[0050] Such a separation can be done very easily. It can, for example, be done by removing the non-breakable materials, taking with it the pieces of glass 100 associated with them. It is thus possible, on the broken glazing 1 shown in the, to remove the portions of adhesive film 31 and 32, taking with it the pieces of glass 100 which are stuck to it.

[0051] According to another possible embodiment, this separation step 93 can also be implemented by sieving the pieces of glass 100. The pieces 100 which are not associated with non-breakable components then pass through the meshes of the sieve, while the non-breakable components, as well as the pieces which are stuck thereto, do not pass through these meshes.

[0052] Lamontre thus shows the portions of adhesive film 31 and 32, constituting non-breakable components, glued to the pieces 100 of the portion of the glazing 1 on which they were glued. These pieces 100 are advantageously those which carry the portions of the collectors 21, 22 and 23, comprising a significant portion of non-glass material.

[0053] These pieces 100 bonded to the non-breakable components may undergo specific recycling, during a reuse step 94. They may, for example, be melted to form a glass material whose composition may include the non-glass material. Alternatively, they may undergo recycling steps aimed at separating the glass material from the non-glass material, to recycle them separately.

[0054] On the contrary, the pieces of the glazing 1 which are not stuck to these portions of adhesive film 31 and 32 do not comprise any non-glass material, or only comprise a small part thereof, corresponding in particular to portions of the heating wires 24. These materials can advantageously be recycled like glass not comprising any non-glass material, during a reuse step 95.

[0055] The separation of the pieces 100 of the glazing, within the meaning of the present invention, does not necessarily allow all of the pieces of the glazing which are bonded to the non-breakable material to be associated with non-glass materials, nor that all of the pieces of the glazing which are not bonded to the non-breakable material are free of non-glass materials. However, it allows, in a very easy manner, to concentrate the pieces of the glazing which are associated with the largest quantities of non-glass material.

[0056] Thus, by way of example, the inventors applied a recycling method according to one embodiment of the invention to a rear window of a motor vehicle which is composed of a glass substrate on which is secured a defrosting resistor composed of a silver alloy. The glass substrate has a mass of approximately 5 kg. The defrosting resistor is formed of a silver alloy weighing approximately 1.3 g distributed between the lateral collectors and the heating wires. The silver alloy therefore represents approximately 0.0265% of the mass of the glazing, or 265 ppm (parts per million).

[0057] The application to this rear window of the recycling process described by the figures, according to which components made of non-breakable material are glued only to the areas of the glazing on which the collectors are secured, makes it possible to easily separate the pieces of this glazing between a first part, weighing approximately 4,750 g, which contains only approximately 170 ppm of silver alloy, and a second part, weighing approximately 250 g, which contains 2,000 ppm of silver alloy. These two parts can advantageously be recycled separately.

[0058] The application to this rear window of a variant of the recycling process described by the figures, according to which components made of non-breakable material are glued to all the areas of the glazing on which the collectors and the conductive wires are secured, makes it possible to easily separate the pieces of this glazing between a first part, weighing approximately 3,950 g, which does not contain any silver alloy, and a second part, weighing approximately 1,050 g, which contains 1,260 ppm of silver alloy. These two parts can advantageously be recycled separately.

Claims

A method of recycling a glazing unit (1) comprising a glass substrate (10) and at least one component made of non-glass material (2) secured to said glass substrate (10), said method comprising a step (92) of breaking said glazing unit (1), followed by a step (93) of separating the pieces of said glazing unit, to separate the pieces (100) of said glazing unit (1) secured to a substantial quantity of said non-glass material, from the pieces (100) of said glazing unit (1) which are not secured to a substantial quantity of said non-glass material, characterized in that it comprises a preliminary step (91), before the step (92) of breaking said glazing unit (1), of bonding to a portion of the surface of said glazing unit (1) at least one non-breakable component (31, 32), at least in one area of ​​said glazing unit (1) on which at least one of said components made of non-glass material (2) is secured, and in that said step (93) separation comprises separating said non-breakable components (31, 32),with the pieces (100) of said glazing (1) which are glued thereto, other pieces (100) of said glazing (1) which are not glued to said non-breakable components (31, 32)., Recycling method according to the preceding claim, characterized in that said glazing (1) is automotive glazing. Recycling method according to the preceding claim, characterized in that said glazing (1) is a rear window of a motor vehicle, comprising a defrosting resistor (2) constituting one of said components made of non-glass material. Recycling method according to any one of the preceding claims, characterized in that said non-glass material component (2) is a component screen-printed on said glass substrate (10), to form said glazing (1). Recycling method according to any one of the preceding claims, characterized in that said non-glass component (2) comprises a metal alloy screen-printed on said glass substrate (10). Recycling method according to any one of the preceding claims, characterized in that said non-breakable component (31, 32) is a flexible adhesive film. Recycling method according to claim 6, characterized in that said flexible adhesive film (31, 32) is made of plastic material. Recycling method according to any one of claims 1 to 6, characterized in that said non-breakable component (31, 32) is bonded to a face of said glass substrate (10) on which said component made of non-glass material (2) is secured. Recycling method according to any one of claims 1 to 6, characterized in that one of said non-breakable components (31, 32) is bonded to each of the two opposite faces of said glass substrate (10), at least in one area of ​​said glazing (1) on which at least one of said components made of non-glass material (2) is secured.

Citation Information

Patent Citations

  • Integrated recovery of metals from complex substrates

    US20200165697A1

  • Method for recycling silver present on a photovoltaic cell

    US20220228235A1

  • Method of recycling useful metal

    WO2009087908A1

  • Method for recycling silver present on a photovoltaic cell

    WO2020240126A1

  • Recycling insulating and / or laminated glass panels

    DE4418573C1