Method for making an adhesive-free tufted rug and a tufted rug

The method of soaking and washing yarns and base materials in a tufted rug manufacturing process creates an adhesive-free, strong, and washable tufted rug by using mechanical friction to form an inherent fixation, addressing the limitations of adhesive-backed rugs in washability and storage.

WO2024224152A1PCT designated stage expired Publication Date: 2024-10-31KVADRAT
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/IB2023/054456
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-28
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Tufted rugs with adhesive backings face issues such as increased weight, chemical emissions, limited washability, and storage constraints due to the use of adhesives like latex, which can lead to damage and irreversible creases, making them difficult to wash and store without compromising quality.

Method used

A method involving soaking yarns and base materials in water for an extended period before washing, using mechanical friction in a washing machine to create an inherent fixation between the yarns and the base material, eliminating the need for adhesive or latex backing, thereby forming a strong and rigid tufted rug construction.

Benefits of technology

This method results in a strong, rigid, and washable tufted rug that can be folded for storage and transported easily, maintaining its original appearance, with structural properties similar to adhesive-backed rugs but without the drawbacks of adhesives, ensuring durability and ease of handling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure IB2023054456_31102024_PF_FP_ABST
    Figure IB2023054456_31102024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention relates to a method for making an adhesive-free tufted rug (10) and a tufted rug having an adhesive free fixation. The tufted rug (10) comprises a base material (12) and a number of yarns (14), where the base material (12) and the yarns (14) are arranged in an amount of water for a predetermined period of time and exposed to mechanical friction, causing a rubbing between the yarns, such that fibres (14') of the individual yarns (14) felt and connect, hereby forming a tufted rug (10) having an inherent fixation between the yarns (14) and the base material (12), formed from the felted yarns on said first side and said second side of the base material.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Method for making an adhesive-free tufted rug and a tufted rug

[0002] TECHNICAL FIELD

[0003] The present invention relates to a method for making an adhesive-free tufted rug and a tufted rug having an adhesive free fixation.

[0004] BACKGROUND OF THE INVENTION

[0005] The present invention relates to a method for making a tufted rug, and a tufted rug.

[0006] More specifically, the present invention relates to a method for manufacturing a tufted rug and a tufted rug that is free from any layer of adhesive for strengthening the bond between the yarns and the base material.

[0007] The known process of manufacturing a tufted rug comprises the steps of providing a primary base layer, such as a fabric, and tufting in the primary base layer with yarns to obtain the tufted rug. The rug has a face side, which shows the cut pile and / or loop pile, and a back side where backstitches are shown. The cut pile and the loop pile are the visual parts of the rug on the face side, and are typically made from natural materials such as wool, cotton and silk or man-made fibers such as viscose, polyamides, polyester, polypropylene and acrylics. The yarns on the face side are usually cut to length by a suitable cutting tool, and a backing layer of adhesive is applied to the opposite side to create the bond between the base layer and the yarns to obtain a strong and rigid rug construction. The backing layer may also be made of e.g., latex.

[0008] After locking the tufts in place, another layer can be applied onto the backside of the tufted rug to obtain a tufted carpet, for example in the form of broadloom carpets, carpet tiles or mats.

[0009] It is known, however, that the adhesives or latex, such as hot melt adhesives, used must be cured prior to use, is adding to the weight if the total product and that the latex and binding adhesives emit chemicals and odors.

[0010] Further, tufted rugs with adhesive backings cannot be washed in an industrial washing machine, and strong hand washing may damage their original appearance, e,g, the backing might break or irreversible creases might occur, and the surface of rugs made from wool might felt. Also, tufted rugs with adhesive backing should not be folded for shipping or stocking as it can result in irreversible creases. The rugs should be shipped or stocked on rolls to avoid any damage to their quality which requires large storage space.

[0011] Consequently, elimination of adhesives or latex is required, and at the same time a strong and rigid rug construction must be obtained where the cut pile and or loop pile are fixated and cannot be pulled out of the base material.

[0012] It is therefore an object of the present invention to provide a method for manufacturing a rug, where no backing layer of adhesive or latex is used in order to maintain a strong and rigid rug construction, where the cut pile and / or loop pile are fixated and cannot be pulled out of the base material. It is further an object of the invention to provide a rug having no backing layer containing adhesive or latex. In the further description of the invention, the term adhesive is to be understood as covering both adhesive and latex and the like. It is an even further object to arrange a light rug that can easily be transported or stored by folding without damaging the rug, and to arrange a rug that can be washed in a standard industrial washing machine without altering the original appearance of the rug.

[0013] The above object and advantages, together with numerous other objects and advantages, which will be evident from the description of the present invention, are according to a first aspect of the present invention obtained by:

[0014] A method for making an adhesive free tufted rug, having the following steps:

[0015] • arranging a base material, such as a woven fabric, having a first side forming an upper surface of the base material and a second side forming a lower surface of the base material,

[0016] • arranging a yarn of wool or a mix of wool, the yarn having fibers,

[0017] • inserting the yarn through the base material, hereby forming a number of loop yarns, on the first and second sides,

[0018] • arranging the base material and pile yarns in a washing machine,

[0019] • adding an amount of water to the base material and the yarns,

[0020] • allowing said base material and the yarns to soak for a predetermined first period of time not below 10 minutes, before a following washing step, and • washing the base material and pile yarn in said water, for a predetermined second period of time not below 15 minutes, hereby causing a friction motion between the yarns on the first side and the second side, whereby the fibers of individual yarns felt and connect, hereby forming a tufted rug having an inherent fixation between the yarns and the base material, formed from the felted yarns on the first side and the second side.

[0021] The tufted rug is made from a base material and yarns, which via a tufting machine, tufting gun or tufting tool are shot through the base material from the back side and which leaves a number of pile yarns on the front side for each shot. The base material is preferably arranged as a type of fabric, such as polyester or cotton, and the yarns are preferably manufactured from wool, but may alternatively be manufactured from a woolen blend. The yarns are inserted by the tufting machine, the tufting gun or the tufting tool through the base material forming a number of pile yarns, which is the part of the yarn that extends from the front side.

[0022] The base material may be any suitable material for tufting and is in a preferred embodiment made from polyester.

[0023] The base material and the yarns are arranged in a predefined amount of water in a suitable equipment, such as an industrial washing machine or other type of washing machine suitable for washing the base material and yarns.

[0024] Before the step of washing, which causes a mechanical impact on the materials, as the drum of the washing machine rotates, the materials are soaked in an amount of water, either in the washing machine or an amount of water outside the washing machine. When the soaking step is arranged outside the washing machine, the soaked materials are introduced into the washing machine before the washing step. It is however preferred that the soaking step takes place in the washing machine for easy operation.

[0025] The yarns inserted through the base material are not mechanically locked to the base material and may thus be considered as loosely inserted through the base material. At this point, the rug is rather fragile, in the sense that care must be taken in order to prevent the yarns from disengaging the base material and the rug, before completion, will be destroyed. If the base material and yarns are arranged in a washing machine and exerted to the washing step immediately and without a soaking step, the yarns will, due to the mechanical impact from the washing machine during the washing step, loose the connection with the base material, and the rug will be destroyed.

[0026] It is therefore of crucial importance that a fixation between the yarns and the base material is established before the actual washing process starts and the material is exposed to the mechanical impact therefrom.

[0027] Due to the soaking before the washing step, the yarns and fibers soak water and as a result thereof swell on both sides of the base material.

[0028] Due to the swelling, the fixation between the yarns and the base layer is increased, and the yarns will not lose fixation with the base material during the washing process.

[0029] Several soaking steps may take place during the soaking process. During a first soaking step, a first amount of water is added to the rug, wherefrom it’s woolen fibers absorb an amount of, or all of the water. Then after the first soaking step, a second soaking step or even third soaking step may take place, where further amounts of water are added to the washing machine / rug.

[0030] Hereby the total weight and volume of the materials inside the washing machine is increased. Increased weight and volume inside the washing machine increases the mechanical friction between the yarns during the washing process, which increases the felting between the yarns and creates a felting early in the washing step.

[0031] Tests performed by the applicant have surprisingly shown that the above-defined method arranges a tufted rug where no backing layer of adhesive or latex is used in order to maintain a strong and rigid rug construction. During the washing step having a duration of not under 15 minutes, the fibers of the yarns felt and connect to each other at the front side and the backside due to the mechanical friction (rubbing of the yarns against each other) caused by the washing machine, such that the felted and connected backstitches form an inherent fixation with similar structural properties as a backing layer made from e.g., latex or adhesive.

[0032] Hereby, a method for manufacturing a rug having the earlier described advantages, is achieved.

[0033] A further advantage achieved by the soaking step is that the fibers in the yarns, besides swelling, open up with the effect that the fibers and yarns easier interconnect during the washing process. According to a further embodiment of the first aspect of the invention, during the step of soaking, the base material and the yarns receives no substantial mechanical impact from the washing machine.

[0034] In a preferred embodiment, the drum of the washing machine does not turn so as to impact as little as possible on the materials before the washing step. However, the drum may alternatively slowly rotate a few times, such as 1 or 2 times, in order to distribute the water on the materials.

[0035] According to a further embodiment of the first aspect of the invention, the soaking step has a duration of above 10 minutes, such as between 20 and 60 minutes.

[0036] As disclosed above, the soaking step does not have a duration below 10 minutes.

[0037] However, though time consuming, the best results and optimal swelling and fixation of the yarns and the base material are achieved with a soaking step having a duration of above 10 minutes and preferably between 20-60 minutes, depending on the yarn size. Thinner yarns may need more time to sufficiently swell compared to thicker yarns.

[0038] According to a further embodiment of the first aspect of the invention, during the soaking step, the dry weight in kg of the base material and the yarns, compared to the amount of water in liter, has a ratio of between 1 / 10 and 1 / 20, preferably approximately 1 / 15.

[0039] Tests by the applicant have shown that yarns of wool or a mix of wool need a certain amount of water in order to sufficiently swell and open up. In order to have a sufficient ratio between yarns and water, the dry weight in kg of the base material and the yarns, compared to the amount of water in liter, has a ratio of between 1 / 10 and 1-20, preferably approximately 1 / 15.

[0040] The pile yarn is a loop (loop pile) of yarn, which may be cut at the end, hereby arranging a number of cut piles. Some tufting machines automatically cut the loops, but when using a tufting gun, the loop piles may be cut manually, e.g., by a pair of scissors. The loop piles may be cut at the end, the outer most point of the loop, or the loops may be cut closer to the base material if shorter cut piles are requested, which arranges a rug with shorter yarns. The loops may be left uncut. According to a further embodiment of the first aspect of the invention, the water, during the soaking step has a temperature of between 15-50 degrees, preferably between 35- 45 degrees most preferably approximate 40 degrees and / or during the washing step, a temperature of above 20 degrees, preferably 35-50 degrees, most preferably approximately 45 degrees.

[0041] Tests performed by the applicant have shown that the best result of the felting and connection of the yarn fibers is made when the water has a temperature of above 20 degrees, preferably 35-50 degrees, and most preferably approximately 45 degrees. Using water temperatures below 20 significantly reduces the felting and connection between yarn fibers. In the preferred embodiment, the water is approximately 35-50 degrees, such as approximately 45 degrees, which provides the best result.

[0042] The temperature of the water during the soaking step may be lower in order to save energy. However, a temperature below 15 degrees slows down the swelling and opening of the fibers and yarns. The best result achieved during the soaking process is when the water has a temperature of 35-45 degrees preferably approximate 40 degrees.

[0043] According to a further embodiment of the first aspect of the invention, the predetermined second period is above 15 minutes, preferably 20-40 minutes, most preferably approximately 30 minutes.

[0044] During the washing step of the base material and the yarns, the mechanical friction interconnects and forms the inherent fixation, which washing and mechanical friction are performed during a predefined second period of time, such as above 15 minutes. In a preferred embodiment, the washing is performed during a period of 20-40 minutes, such as e.g., approximately 30 minutes, which provides the most optimal result compared to processing costs.

[0045] According to a further embodiment of the first aspect of the invention, the water during said washing step comprises an amount of soap, preferably between 5-20 ml / kg dry wool, and most preferably between, 7-10 ml / kg dry wool.

[0046] The water used for washing the base material and the yarns may comprise an amount of soap, such as green soap. The soap changes the pH value of the water / yarns and modifies and opens up the fibers' structure, such that the fibers felt and connect more easily. In order to ensure an optimal pH value, preferably, the amount of soap used is between 5-20 ml / kg dry wool, and most preferably between, 7-10 ml / kg dry wool.

[0047] According to a further embodiment of the first aspect of the invention, the method comprises a rinsing step for a predetermined third period, such as above 1 minute, preferably between 1-30 minutes, such as between 5-20 minutes, most preferably between 5-10- 15 minutes.

[0048] When using an amount of soap in the water, the soap needs to be rinsed out of the material during the rinsing process, so that no soap is left in the tufted rug. The soap needs to be rinsed out of the water in order to “neutralize” the pH value of the yarns. If soap is still present, there is a chance that the alkaline pH value destroys the fibers with the time. Therefore, the method comprises a rinsing step, where tufted rug is rinsed for a predetermined third period of time, as defined above.

[0049] After the washing and rinsing steps, and before removing the rug from the washing machine and an afterwards drying process, water needs to be extracted from the rug. The washing machine performs at least one spinning cycle. Preferably the drum spins between 20-50 rpm, most preferred between 30-36 rpm. A normal washing machine may spin approximate up to 900 rpm, which in this case could destroy the structure and deform the rug. Thus, in order to spin water out of the rug and maintain the structure of the rug, the most optimal settings are as defined above.

[0050] According to a further embodiment of the first aspect of the invention, the washing is performed with a washing equipment having a predetermined maximum load, wherein said washing equipment is loaded between 20-80% of said maximum load, preferably between 70-80%.

[0051] The most optimal washing result is achieved when the washing equipment is not fully loaded. As described above, the washing causes a mechanical friction, which is necessary for the yarn fibers to felt, and a fully loaded washing machine will not create the necessary mechanical friction. On the other hand, if the washing machine is only loaded with a very small amount, the necessary mechanical friction is also not created. Tests have shown that the most optimal result is achieved when the washing machine is loaded between 20-80%. In a most preferred embodiment, the washing machine is loaded with between 70-80% which gives the optimal felting result. According to a further embodiment of the first aspect of the invention, during the washing step, the water is provided in a quantity of between 5-40 liters water / kg of said base material and yarn, preferably in a quantity of between 10-20 liters water / kg of said base material and yarn, such as approximately 8 liters water / kg of said base material and yarn.

[0052] As described above, the amount of material in the washing machine is crucial, but also the amount of water / kg material (base material and yarns) during the washing step is of most importance when a strong inherent fixation is needed. The best result of the inherent fixation is achieved when the water used amounts to between 10-40 5-40 liters of water / kg, preferably between 20-30 10-20 liters of water / kg, such as approximately-24 8 liters of water / kg of said base material and yarn. The above-defined amounts result in sufficient soaking of the material and optimal conditions for the mechanical friction.

[0053] According to a further embodiment of the first aspect of the invention, the soap has a pH value of min 7 and max 14, such as preferably approximate between 8-9 pH.

[0054] Using oil-based soap has proven to provide the best result of changing the pH value of the water / yarns, which modifies / opens up the yarn structure such that the yarn fibers will easily felt. The above-defined pH values have during tests shown the best results.

[0055] When using soap in the water during the washing step, it is important to use the abovedefined specific amounts. Too much soap (more than the predefined amounts) prolongs the rinsing step and contributes to no further technical result compared to the defined amounts.

[0056] According to a further embodiment of the first aspect of the invention, the method further comprises a drying step, where said base material with said yarn is being dried.

[0057] After the tufted rug has been washed, the tufted rug needs to be dried, whereby the felted fibers stiffen up and get more structural stability, which results in an increased strength of the inherent fixation. The equipment used for drying may be any type of suitable drying machine which is capable of handling the size of the rug and at temperatures of up to approximately 90 degrees. Preferably an industrial drying machine is being used, which machine is capable of both handling larger sized rugs and drying at a high drying temperature. According to a further embodiment of the first aspect of the invention, the material base has a tensile strength of >1100N / 5cm.

[0058] The tensile strength of the fabric is the amount of stretching force (load) at which the fabric begins to break when it comes under stretching conditions. The tensile strength depends on the thread count per square inch of the fabric, which increases the tensile strength as the thread count increases, which also provides a more dense base material, which to some degree fixates the yarns to the base material during the washing process. The best result has been achieved when the tensile strength of the base material is above 1100N / 5cm.

[0059] According to a further embodiment of the first aspect of the invention, the water comprises an amount of dyestuff for dying the fibers.

[0060] For manufacturing rugs often coloured yarns are used. The yarns are coloured by an independent dyeing process. Afterwards the coloured yarns will be used for creating the rug for a specific need. This dying process is energy and water consuming and often processed by another company. With adding an amount of dye to the water, it is possible to both construct the rug and at the same time arrange the rug with a desired colour. The combined washing and dying step eliminates an extra process step for dying, whereby both water and energy and additional transportation have been saved.

[0061] According to a second aspect of the present invention, the above objects and advantages are obtained by:

[0062] A tufted rug manufactured by a process according to any of the steps of the first aspect of the invention.

[0063] According to a third aspect of the present invention, the above objects and advantages are obtained by:

[0064] A tufted rug without an adhesive backing layer comprising a base layer of a woven fabric having a first side and a second side, and an amount of yarns arranged through the base layer and forming a number of pile yarns on the first side, the tufted rug further comprising on the second side an inherent fixation arranged from felted fibers of the yarns. With the above-defined tufted rug, a backing layer containing adhesive or latex is completely avoided, as the yarn fibers on the first side and the second side are felted and create an inherent fixation with similar structural properties as a common type of backing layer made from adhesive or latex.

[0065] Fig. 1A-1C show a method for arranging a known prior art tufted rug.

[0066] Fig. 2A-2C show a method for arranging an adhesive free tufted rug.

[0067] Fig. 3A-3B show friction movement between the yarn and the fibers.

[0068] Fig. 4 shows the individual elements in the method according to the invention.

[0069] The present invention will now be described more fully hereinafter with reference to the accompanying drawings, in which exemplary embodiments of the invention are shown. The invention may, however, be embodied in different forms and should not be construed as limited to the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the invention to those skilled in the art. Like reference numerals refer to like elements throughout. Like elements will thus not be described in detail with respect to the description of each figure.

[0070] Fig. 1A-1C show a method for arranging a known prior art tufted rug 10’.

[0071] The known process of manufacturing a tufted rug 10’ comprises the steps of providing a primary base material 12, such as a fabric, and tufting the primary base material 12 with tufting yarns 14 to obtain the tufted rug 10’. The tufting is made by a tufting machine or a tufting gun, where a needle 16 inserts the yarn 14 through the base material 12, hereby arranging a number of loop yarns as illustrated in figure 1A. The loop yarns are located on the face side (the visual side of the rug) of the rug 10’, and as shown in the figure, the backside comprises the backstitches.

[0072] As shown in figure 1 B, the pile yarns (loop pile) have been cut by a suitable tool, e.g., a pair of scissors to a desired length and cut at the end of the loop, hereby forming a number of cut piles 18. The step of cutting the loop piles is optional, and the shown embodiment also corresponds to a tufted rug having loop piles. Some tufting machines automatically cut the loops, but when using a tufting gun, the loop piles may be cut manually, e.g., by a pair of scissors. The loop piles may be cut at the end, the outer most point of the loop, or the loops may be cut closer to the base material 12 if shorter cut piles are requested, which arranges a rug with shorter yarns. As shown in figure 1 C, a backing layer 20 of adhesive or latex is applied to the backside, covering the backstitches, hereby forming a structural stable backing layer keeping the rug 10’ together.

[0073] Fig. 2A-2C shows a method for arranging an adhesive free tufted rug 10 according to a possible embodiment of the invention. The steps shown in figure 2A and 2B correspond to the steps shown in figure 1 A and 1 B.

[0074] In figure 2C, the base material 12 and the yarns have been arranged in a predefined amount of water in a suitable equipment, such as an industrial washing machine or other type of washing machine suitable for washing the base material 12 and the yarns 14. Optionally, an amount of soap is included in the water or an amount of soap and dyestuff.

[0075] Before the washing step where the yarns felt and intertangle, the unwashed rug is left in the water, preferably inside the washing machine, for a period of not less than 10 minutes, and preferably above 10 minutes, and most preferred in a period of between 20-60 minutes.

[0076] Due to the soaking before the washing step, the yarns soak water and as a result thereof swell on both sides of the base material. Due to the swelling, the fixation between the yarns and the base layer is increased, and the yarns will not lose fixation with the base material during the washing process. A further advantage achieved by the soaking step is that the yarns, besides swelling, open up with the effect that the fibers and yarns easier interconnect during the washing process.

[0077] During the washing step, the fibers 14’ of the yarns 14 at the front side and the backside felt and connect to each other, due to the mechanical friction caused by the washing machine. The felted and connected back stiches, and the felted pile forms an inherent fixation 22 with the similar structural properties as a backing layer made from e.g., latex or adhesive.

[0078] Fig. 3A-3B shows friction movement between yarn 14 and fibers 14’. The figures are illustrative drawings, where figure 3A shows the non-connected yarn 14 and fibers 14’ being exposed to mechanical friction, where the base material 12 and the yarns 14 are being processed, such that the yarns 14 and the yarn 14 and fibers 14’ rub against each other. Figure 3B shows an illustration where the base material 12 and the yarns 14 have been processed by a suitable washing machine for a predetermined sufficient amount of time, such that the yarn 14 and fibers 14’ have been felted and connected and hereby forming the inherent fixation 22.

[0079] Fig. 4 shows the individual elements of a method according to the invention.

[0080] The main elements in the method are the base material 12 and the yarns 14 being arranged in water and soaking for a predetermined period of time and afterwards exposed to mechanical friction during the washing step, whereby the inherent fixation is formed.

[0081] In the following is given a list of reference signs that are used in the detailed description of the invention and the drawings referred to in the detailed description of the invention.

[0082] 10 Adhesive free tufted rug

[0083] 10’ Tufted rug with adhesive backing

[0084] 12 Base material

[0085] 14 Yarns

[0086] 14’ Yarn fibers

[0087] 16 Needle

[0088] 18 Cut piles

[0089] 20 Adhesive / latex backing layer

[0090] 22 Inherent fixation

Claims

CLAIMS1. A method for making an adhesive free tufted rug, having the following steps:• arranging a base material, such as a woven fabric, having a first side forming an upper surface of said base material and a second side forming a lower surface of said base material,• arranging a yarn of wool or a mix of wool, said yarn having fibers,• inserting the yarn through the base material, hereby forming a number of loop yarns, on said first and second sides,• arranging said base material and pile yarns in a washing machine,• adding an amount of water to said base material and said yarns,• allowing said base material and said yarns to soak for a predetermined first period of time not below 10 minutes, before a following washing step, and• washing said base material and pile yarn in said water, for a predetermined second period of time not below 15 minutes, hereby causing a friction motion between the yarns on said first side and said second side, whereby said fibers of individual yarns felt and connect, hereby forming a tufted rug having an inherent fixation between the yarns and the base material, formed from said felted yarns on said first side and said second side.

2. A method according to claim 1 , wherein during said step of soaking, said base material and said yarns receives no substantial mechanical impact from said washing machine.

3. A method according to claim 1 or 2, wherein said soaking step has a duration of above 10 minutes, such as between 20 and 60 minutes.

4. A method according to any of the previous claims, wherein during the soaking step, the dry weight in kg of said base material and said yarns, compared to the amount of water in liter, has a ratio of between 1 / 10 and 1 / 20, preferably approximate 1 / 15.

5. A method according to any of claims 1-4, wherein said water, during said soaking step has a temperature of between 15-50 degrees, preferably between 35-45 degrees most preferably approximate 40 degrees and / or during said washing step, a temperature of above 20 degrees, preferably 35-50 degrees, most preferably approximately 45 degrees.

6. A method according to any of claims 1-5, wherein said predetermined second period is above 15 minutes, preferably 20-40 minutes, most preferably approximately 30 minutes.

7. A method according to any of the previous claims, wherein said water during said washing step comprises an amount of soap preferably between 5-20 ml / kg dry wool, and most preferably between, 7-10 ml / kg dry wool.

8. A method according to claim 7, wherein said method comprises a rinsing step for a predetermined third period, such as above 1 minute, preferably between 1-30 minutes, such as between 5-20 minutes, most preferably between 10-15 minutes.

9. A method according to any of the previous claims, wherein said washing is performed with a washing equipment having a predetermined maximum load, wherein said washing equipment is loaded between 20-80% of said maximum load, preferably between 70-80%.

10. A method according to any of the previous claims, wherein said water, during said washing step, is provided in a quantity of between 5-40 liters of water / kg of said base material and yarn, preferably in a quantity of 10-20 liters of water / kg, of said base material and yarn, such as approximately 8 liters of water / kg of said base material and yarn.

11. A method according to any of claims 7-10, wherein said soap has a pH value of min 7 and max 14, such as preferably approximately between 8-9.

12. A method according to any of the previous claims, wherein said method further comprises a drying step, where said base material with said yarn is being dried.

13. A method according to any of claims 1-12, wherein said base material has a tensile strength of >1100N / 5 cm.

14. A method according to any of claims 1-13, wherein said water comprises an amount of dyestuff for dying said fibers.

15. A tufted rug manufactured by a process according to any of claims 1-14.

Citation Information

Patent Citations

  • Convenient-dedusting carpet and finishing technology thereof

    CN107354754A

  • Preparation method of wear-resistant and antibacterial tufted carpet

    CN113622109A

  • Wool carpet and wool carpet manufacturing method

    ES2799832A1

  • JP1976107954U

  • Reversible cotton bathroom rug and method of manufacture

    US6468621B1