Gum base for bubble gum

The gum base for bubble gum, featuring vinyl acetate resin with a degree of polymerization of 750 or more and natural rubber, addresses the manufacturing and stability issues of conventional compositions, achieving enhanced expansion volume and comfort.

WO2024225137A1PCT designated stage expired Publication Date: 2024-10-31LOTTE CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/015280
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2024-04-17
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Conventional bubble gum compositions using vinyl acetate resin with high polymerization degree struggle with manufacturing suitability and film stability, leading to reduced maximum inflation volume and compromised chewing comfort.

Method used

A gum base for bubble gum that excludes vinyl acetate resin with a degree of polymerization less than 500 and incorporates vinyl acetate resin with a degree of polymerization of 750 or more, combined with natural rubber, to enhance manufacturing suitability and film stability.

Benefits of technology

The solution results in improved manufacturing ease, increased film stability, and a maximum expansion volume more than twice that of conventional bubble gum, while maintaining chewing comfort and inflation ease.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JPOXMLDOC01-APPB-T000001
    Figure JPOXMLDOC01-APPB-T000001
  • Figure JPOXMLDOC01-APPB-T000002
    Figure JPOXMLDOC01-APPB-T000002
Patent Text Reader

Abstract

The present invention is for providing a bubble gum excellent in production aptitude and stability of a film compared to the prior art. The present invention provides a gum base for a bubble gum characterized by not containing a vinyl acetate resin having a polymerization degree of less than 500 and containing a natural rubber and a vinyl acetate resin having a polymerization degree of 750 or more.
Need to check novelty before this filing date? Find Prior Art

Description

bubble gum base

[0001] The present invention relates to a gum base for bubble gum.

[0002] Among chewing gums, so-called "bubble gum" is intended to be played with by blowing up the gum, so it is required to have physical properties that make it easy to inflate when blowing into the gum base, which is the residue left after chewing, and that make it difficult for the balloon membrane to break when inflated.

[0003] Conventionally, bubble gum bases have been made of compositions primarily composed of vinyl acetate resin, which has excellent elasticity and film strength. However, although vinyl acetate resins with a high degree of polymerization (1000 or higher) have favorable properties in terms of increasing film strength when inflated into balloons, they have drawbacks in terms of manufacturability (e.g., miscibility of raw materials and fluidity) and quality (e.g., film uniformity and stability). Therefore, vinyl acetate resins with a low to medium degree of polymerization (approximately 400 to 600) have generally been used alone, or vinyl acetate resins with a low degree of polymerization (approximately 100 to 200) and a medium degree of polymerization (approximately 500 to 800) have often been used in combination.

[0004] In response to this, a bubble gum (Patent Document 1) has been proposed in which a mixture of vinyl acetate resins with a high degree of polymerization (1,000-7,000) and a low degree of polymerization (100-250) is used to increase the maximum expansion volume of the bubble gum when inflated into a balloon by two to three times that of conventional bubble gums. Also proposed is a gum base composition (Patent Document 2) that is non-adhesive by containing a homogeneous premix of a vinyl acetate polymer having a molecular weight of about 38,000 to about 94,000 (corresponding to a degree of polymerization of 440-1,100) and an emulsifier. Another chewing gum composition (Patent Document 3) has been proposed that combines cohesiveness (quality) and flowability (manufacturability) by using a gum base made of vinyl acetate resin with a molecular weight of about 20,000 or more (corresponding to a degree of polymerization of 290 or more) to which a non-hygroscopic plasticizer has been added, in combination with a cohesive sweetening-bulking component.

[0005] Furthermore, bubble gum base compositions have been proposed that have improved texture and shelf life by using a mixture of vinyl acetate resins with low molecular weights of about 12,000 to about 16,000 (corresponding to a degree of polymerization of 140 to 190) and medium molecular weights of about 35,000 to about 55,000 (corresponding to a degree of polymerization of 410 to 640), together with an elastomer such as synthetic rubber or natural rubber and an acetylated monoglyceride (Patent Documents 4 and 5).

[0006] JP 63-66497, JP 3-51382, JP 62-195251, JP 3-71098, JP 3-172143

[0007] As described above, bubble gums have been produced by avoiding the use of vinyl acetate resins with a high degree of polymerization (a degree of polymerization of 1000 or more) or by compensating for their drawbacks, but the bubble gums produced to date have not been fully satisfactory in terms of manufacturability and shell stability. In view of this, an object of the present invention is to provide a bubble gum that is more manufacturable and has a more stable shell than conventional bubble gums.

[0008] The present invention solves the above-mentioned problems by providing a gum base for bubble gum that does not contain a vinyl acetate resin with a degree of polymerization of less than 500, and that contains a vinyl acetate resin with a degree of polymerization of 750 or more and natural rubber.

[0009] The bubble gum gum base of the present invention has favorable physical properties in terms of suitability for manufacturing, and when bubble gum is manufactured using it, the stability of the balloon shell is improved compared to conventional ones.

[0010] The bubble gum gum base of the present invention is characterized in that it does not contain a vinyl acetate resin having a degree of polymerization of less than 500, and contains a vinyl acetate resin and natural rubber having a degree of polymerization of at least 750. However, there is no problem if the gum base contains a vinyl acetate resin having a degree of polymerization of at least 500 but less than 750, which is intermediate between the above two types of vinyl acetate resins, and in fact, it can be said that such inclusion is preferable in terms of improving chewing comfort.

[0011] Since polymers such as vinyl acetate resin (polyvinyl acetate) are generally polydisperse systems with molecular weight distribution, their degree of polymerization is usually expressed as an average degree of polymerization. The average degree of polymerization can be measured by number-average degree of polymerization, weight-average degree of polymerization, viscosity-average degree of polymerization, z-average degree of polymerization, etc. In the present invention, the weight-average degree of polymerization, which can be measured by gel permeation chromatography (GPC), is used.

[0012] Generally, gum bases are produced by blending one or more raw material resins. "Not containing vinyl acetate resins with a degree of polymerization less than 500" means that vinyl acetate resins with a weight-average degree of polymerization less than 500 are not used as raw materials for the gum base. "Containing vinyl acetate resins with a degree of polymerization of 750 or more" means that vinyl acetate resins with a weight-average degree of polymerization of 750 or more are used as raw materials for the gum base. Therefore, the weight-average degree of polymerization (hereinafter simply referred to as "degree of polymerization") of the entire vinyl acetate resin in the gum base of the present invention will be 750 or more when only vinyl acetate resins with a degree of polymerization of 750 or more are used as raw materials. However, this does not necessarily mean that the degree of polymerization of the entire vinyl acetate resin in the gum base of the present invention will be 750 or more when vinyl acetate resins with a degree of polymerization of 500 or more but less than 750 are also used. However, the degree of polymerization of the entire vinyl acetate resin in the gum base of the present invention will not be less than 500.

[0013] Conventional bubble gum gum bases do not contain high-polymerization vinyl acetate resins with a degree of polymerization of 1000 or more, or, if they contain high-polymerization vinyl acetate resins with a degree of polymerization of 1000 or more, they have been used in combination with low-polymerization vinyl acetate resins with a degree of polymerization of less than 500 to compensate for the difficulties associated with using high-polymerization vinyl acetate resins in terms of manufacturability and balloon shell stability. However, although the inclusion of low-polymerization vinyl acetate resins improves chewing comfort and ease of inflation, it reduces the proportion of high-polymerization vinyl acetate resins, which relatively increase shell strength, making it disadvantageous in increasing the maximum inflation volume (the upper limit of the size that can be inflated into a balloon).

[0014] The bubble gum gum base of the present invention does not contain a low-polymerization vinyl acetate resin with a degree of polymerization of less than 500, but instead contains natural rubber, which is a high molecular weight material but has smoother physical properties than synthetic rubber. This eliminates the problems with manufacturing suitability and film stability that arise when using a medium to high-polymerization vinyl acetate resin with a degree of polymerization of 750 or more, and also avoids the problem of reduced film strength that arises when using a low-polymerization vinyl acetate resin.

[0015] As mentioned above, generally, a high-polymerization vinyl acetate resin refers to one with a degree of polymerization of 1,000 or more, a medium-polymerization vinyl acetate resin refers to one with a degree of polymerization of 500 or more but less than 1,000, and a low-polymerization vinyl acetate resin refers to one with a degree of polymerization of less than 500. However, the bubble gum gum base of the present invention does not contain a low-polymerization vinyl acetate resin with a degree of polymerization of less than 500, but contains a vinyl acetate resin with a degree of polymerization of 750 or more and natural rubber. Therefore, in the following description of this specification, a vinyl acetate resin with a degree of polymerization of 750 or more will be referred to as a "high-polymerization resin," a vinyl acetate resin with a degree of polymerization of 500 or more but less than 750 will be referred to as a "medium-polymerization resin," and a vinyl acetate resin with a degree of polymerization of less than 500 will be referred to as a "low-polymerization resin."

[0016] The bubble gum base of the present invention preferably contains about 4 to 20% by weight, and more preferably about 12 to 15% by weight, of a high-polymerization resin. As mentioned above, the bubble gum base of the present invention preferably contains a medium-polymerization resin in addition to the high-polymerization resin. In this case, the medium-polymerization resin is preferably contained in the gum base at about 0 to 35% by weight, and more preferably at about 10 to 20% by weight. The combined high-polymerization resin and medium-polymerization resin content of the gum base is preferably about 15 to 40% by weight.

[0017] The bubble gum base of the present invention contains natural rubber in addition to the high-polymerization resin (and medium-polymerization resin). Natural rubber is a refined product of rubber tree sap (latex) that has been coagulated, washed, dehydrated, and dried, and is chemically a high-cis polyisoprene (a polyisoprene composed mostly of cis-isoprene monomers).

[0018] The bubble gum gum base of the present invention preferably contains about 2 to 9% by weight of natural rubber, and more preferably about 4 to 9% by weight. If the natural rubber content is less than 2% by weight, the effect of adding natural rubber is not exerted, so improvement in manufacturing suitability cannot be expected, and even if a bubble gum is formed using it, it becomes difficult to inflate a balloon. If the natural rubber content is 4% by weight or more, more preferable manufacturing suitability is obtained, and if a bubble gum is made using it, it becomes easier to inflate a balloon. On the other hand, if the natural rubber content exceeds 9% by weight, the physical properties of the gum become too hard, and the flexible extensibility of the balloon is lost, making it difficult to inflate a balloon to a large size.

[0019] The bubble gum base of the present invention can contain, in addition to vinyl acetate resin and natural rubber, synthetic rubbers such as polyisobutylene and polybutene, waxes such as microcrystalline wax and candelilla wax, emulsifiers such as glycerin fatty acid esters and lecithin, fillers such as talc and calcium carbonate, ester gum, etc. The blending amounts of these additives are typically about 3 to 25% by weight of synthetic rubber, 10 to 25% by weight of waxes, 5 to 25% by weight of emulsifiers, 5 to 30% by weight of fillers, and 0 to 25% by weight of ester gum.

[0020] The bubble gum base of the present invention is used to add usual bubble gum additives such as sugars (sugar, glucose, corn syrup, etc.), sweeteners (xylitol, etc.), flavorings, colorings, etc., and the mixture is kneaded, passed through an extruder, and then cut and molded into plates, blocks, spheres, etc. to obtain bubble gum products.

[0021] The ease of bubble gum expansion is typically evaluated by a sensory test conducted by a panel of multiple panelists. Alternatively, it can be evaluated by chewing the gum until the sweetness disappears (usually about 10 to 15 minutes) and then measuring the moisture content (wt %) and compression load (kgf) of the gum residue. Generally, the higher the moisture content of the gum residue, the smoother the balloon will expand. For bubble gums using the gum base of the present invention, the moisture content suitable for expanding a balloon is preferably 18.0% or more, more preferably 20.0% or more, and even more preferably 22.0% or more. Furthermore, a higher compression load of the gum residue increases the film strength and allows for larger balloon expansion, but too high a compression load requires excessive breath pressure to inflate the balloon. The maximum compression load is preferably 2.0 kgf or more, more preferably 2.1 kgf or more. It is particularly preferable that the moisture content is 18.0% or more and the maximum compressive load is 2.0 kgf or more.

[0022] The maximum expansion volume, or the limit to which a balloon can be inflated when a particular bubble gum is used, can be determined by an inflation test conducted by an experienced panel, but a more objective evaluation can be made by measuring using equipment that can optimally adjust the gas pressure and inflow rate. The bubble gum using the gum base of the present invention exhibited a maximum expansion volume that was more than twice as large as that of conventional bubble gum under the same conditions, indicating high film stability.

[0023] Example 1 A vinyl acetate resin having a molecular weight of 55,000 to 75,000 (average degree of polymerization: approximately 750) was prepared as a high-polymerization resin, a vinyl acetate resin having a molecular weight of 47,000 to 57,000 (average degree of polymerization: approximately 580) as a medium-polymerization resin, and a vinyl acetate resin having a molecular weight of 12,000 to 18,000 (average degree of polymerization: approximately 180) as a low-polymerization resin. A gum base was produced by combining the components in the following ratios (unit: weight %) shown in Table 1 using a 3-liter heater-equipped kneader and heating and melt-mixing them at 135°C for 50 minutes. Resin mixture 29.2 (of which low polymerization degree resin 0.0) (of which medium polymerization degree resin 15.3) (of which high polymerization degree resin 13.9) Rubber content 9.0 (of which natural rubber 2.3) Other ingredients Ester gum 24.4 Wax 20.8 Emulsifier 10.0 Filler 6.6 Total 100.0

[0024] Examples 2 to 4, Comparative Examples 1 to 3 Gum bases were produced in the same manner as in Example 1, except that the blending ratio of each component was changed as shown in Table 1.

[0025] (Evaluation of Examples 1-4 and Comparative Examples 1-3) <Evaluation of Manufacturability> The ease of manufacturability when producing the gum bases in Examples 1-4 and Comparative Examples 1-3 was evaluated according to the following criteria. A The raw materials were well compatible, and the manufacturability was good. B The raw materials were not sufficiently compatible, and there was roughness, and the manufacturability was not very good. C The raw materials were not compatible, and the gum base could not be produced. The evaluation results are shown in Table 2.

[0026] <Evaluation of Gums Using Gum Bases> The gum bases produced in Examples 1-4 and Comparative Examples 1-3 were kneaded in the following ratios: gum base 42%, sugar 36%, starch syrup 13%, softener 4%, acidulant 2.5%, flavoring 1.3%, gelatin 1%, antioxidant 0.1%, and coloring 0.1%. The kneaded gums were then molded into balls, and a sensory evaluation test and objective evaluations, including evaluation of maximum expansion volume, moisture content, and compressive load, were conducted. <Sensory Evaluation Test> Three panelists were asked to chew gums using the gum bases produced in Examples 1-4 and Comparative Examples 1-3 for three minutes, and then to inflate the chewed gums into balloons. They were then asked to rate the extent of expansion using the following five-point scale. The arithmetic mean of the panelists' evaluation results was calculated to determine the evaluation result. 1: No expansion at all. 2: Very little expansion. 3: Fairly good expansion. 4. Expands well. 5. Expands very well. The results are shown in Table 2.

[0027] <Evaluation of Maximum Expansion Volume (Coating Stability)> Using a testing device equipped with a sample mounting section simulating the inside of a human mouth, a gas supply section for supplying gas to the sample mounting section, and a flow control section for controlling the flow rate of the supplied gas, the gums using the gum bases produced in Examples 1-4 and Comparative Examples 1-3 were evaluated for their coating stability by measuring their maximum expansion volumes. Specifically, each sample was masticated for 10 to 15 minutes and then attached to the sample mounting section of the testing device. Nitrogen gas was then passed through at the optimal flow rate (L / min) determined in advance through preliminary testing, and the total flow rate (mL) was measured until the sample no longer expanded. Ten measurements were performed for each sample, and the arithmetic mean was calculated. The results are shown in Table 2.

[0028] <Measurement of Moisture Content> The moisture content of the gums using the gum bases produced in Examples 1-4 and Comparative Examples 1-3 was measured using the following procedure. Specifically, 3 g of each sample was chewed at a rate of 80 times per minute for 15 minutes, and the weight of the chewed product was immediately weighed. Next, the chewed product was dried under reduced pressure at 105°C for 1 hour, and the weight of the dried chewed product was weighed, and the moisture content was calculated using the following formula: Moisture content (%) = 100 - (weight of dried chewed product / weight of chewed product x 100) The measurement was performed three times for each sample, and the arithmetic average was taken. The results are shown in Table 2.

[0029] <Measurement of Compression Load> The compression load of the gums using the gum bases prepared in Examples 1-4 and Comparative Examples 1-3 was measured using the following procedure. Specifically, 3 g of each sample was chewed for 15 minutes at a rate of 80 times / min, and the chewed material was then sandwiched between wax paper and molded to a thickness of 3.2 mm. Then, 20 seconds after the chewed material was removed from the mouth, the compression load was measured under the following conditions. Specifically, using an Instron 68SC-05 universal testing machine, the sample was compressed with a 20 mm diameter hemispherical plunger at a rate of 2 mm / sec with a clearance of 0.3 mm. After a 0.1 second hold, the plunger was raised at a rate of 2 mm / sec to measure the maximum compression load (kgf). The measurement environment was 30°C using a precision air conditioner and a temperature-controlled stage. Each sample was measured three times, and the arithmetic mean was calculated. The results are shown in Table 2.

[0030]

[0031] (-: Unmeasurable) Industrial Applicability

[0032] By using the bubble gum base of the present invention, it is possible to produce bubble gum that expands to a larger size than conventional bubble gums.

[0033] [Aspects of the Invention] Various aspects of the present invention include the following. 1. A bubble gum gum base that does not contain any vinyl acetate resin having a degree of polymerization of less than 500, and that contains a vinyl acetate resin having a degree of polymerization of 750 or more and natural rubber. 2. The bubble gum gum base of above 1, containing 12 to 15% by weight of a vinyl acetate resin having a degree of polymerization of 750 or more. 3. The bubble gum gum base of above 1 or 2, containing 2 to 9% by weight of natural rubber. 4. The bubble gum gum base of above 1 or 2, containing 4 to 9% by weight of natural rubber. 5. The bubble gum gum base of any of above 1 to 4, further containing a vinyl acetate resin having a degree of polymerization of 500 to 750. 6. The bubble gum gum base of above 5, containing 10 to 20% by weight of a vinyl acetate resin having a degree of polymerization of 500 to 750. 7. 7. A bubble gum base according to any one of 1 to 6 above, further comprising at least one component selected from the group consisting of synthetic rubber, waxes, emulsifiers, fillers, and ester gum. 8. A bubble gum comprising a bubble gum base according to any one of 1 to 7 above and ordinary bubble gum components. 9. The bubble gum according to 8 above, which has a moisture content after mastication of 18% or more and a maximum compressive load of 2.0 kgf or more.

[0034] This application claims priority from Japanese Patent Application No. 2023-075074, filed on April 28, 2023, the contents of which are incorporated herein by reference.

Claims

1. A gum base for bubble gum, which does not contain vinyl acetate resin having a degree of polymerization of less than 500, and contains vinyl acetate resin having a degree of polymerization of 750 or more and natural rubber.

2. The gum base for bubble gum according to claim 1, wherein the vinyl acetate resin having a degree of polymerization of 750 or more is contained in an amount of 12 to 15% by weight.

3. The gum base for bubble gum according to claim 1, wherein the natural rubber is contained in an amount of 2 to 9% by weight.

4. The gum base for bubble gum according to claim 1, wherein the natural rubber is contained in an amount of 4 to 9% by weight.

5. The gum base for bubble gum according to claim 1, further comprising a vinyl acetate resin having a degree of polymerization of 500 to 750.

6. The gum base for bubble gum according to claim 5, wherein the vinyl acetate resin having a degree of polymerization of 500 to 750 is contained in an amount of 10 to 20% by weight.

7. The gum base for bubble gum according to claim 1, further comprising at least one component selected from the group consisting of synthetic rubbers, waxes, emulsifiers, fillers and ester gums.

8. A bubble gum comprising the bubble gum base according to any one of claims 1 to 7 and conventional bubble gum ingredients.

9. The bubble gum according to claim 8, which has a moisture content after chewing of 18% or more and a maximum compressive load of 2.0 kgf or more.

Citation Information

Patent Citations

  • Chewing gum composition having flow property

    JP1985186249A

  • Decorative bubble gum and its preparation

    JP1986028349A

  • Decorative bubble gum

    JP1986158751A

  • Decorative bubble gum