Polymerizable composition, resin obtained by polymerizing and curing same, and optical material comprising said resin
The use of a bismuth compound in a polymerizable composition addresses the challenge of creating transparent, lightweight, and processable radiation shielding materials, enabling effective radiation protection and visual confirmation in medical and nuclear applications.
Patent Information
- Application Number
- PCT/JP2024/015663
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-01
- Filing Date
- 2024-04-22
- Publication Date
- 2024-11-07
AI Technical Summary
Current radiation shielding materials for medical and nuclear applications are either opaque, lack workability, or are heavy, making it difficult to achieve both radiation shielding and transparency for visual confirmation in complex shapes and lightweight applications.
A polymerizable composition containing a bismuth compound with specific structures, which forms transparent and thermoplastic resins that can be easily processed and cured, providing radiation shielding while allowing visible light transmission.
The bismuth-based polymerizable composition enables the creation of transparent, lightweight, and easily processable radiation shielding materials suitable for complex shapes, allowing for both radiation protection and visual confirmation, enhancing their applicability in medical and nuclear environments.
Smart Images

Figure JP2024015663_07112024_PF_FP_ABST
Abstract
Description
Polymerizable composition, resin obtained by polymerizing and curing the same, and optical material containing the resin
[0001] The present invention relates to a polymerizable composition, a resin obtained by polymerizing and curing the polymerizable composition, and an optical material containing the resin.The present invention particularly relates to a polymerizable composition suitable for use in optical materials, particularly filters and plastic lenses, as transparent members that require radiation shielding, such as filters, plastic lenses, prisms, and optical fibers, and to a resin obtained by polymerizing and curing the polymerizable composition.
[0002] Generally, radiation shielding materials can easily shield against alpha rays by using thin materials such as paper, and against beta rays by using thin metal plates such as aluminum, but they can weaken gamma rays and X-rays by using thick plates such as lead or iron as shielding materials.However, these materials are not transparent, so it is not possible to visualize the other side of the shielding material.
[0003] In such circumstances, at advanced medical facilities where CT (computed tomography) and PET (positron emission tomography) devices are used for diagnosis and treatment, and at nuclear power plants, it is necessary to transmit images visually or via camera to check the situation at the site where radiation is being used while also providing sufficient shielding from radiation. This requires materials that are transparent to visible light while providing sufficient shielding from radiation.
[0004] In response to such demands, lead-containing glass is generally known as a material that is transparent to visible light and capable of shielding radiation (Patent Documents 1 and 2). However, unlike plastics, lead-containing glass is poor in processability and moldability, and therefore is not suitable for complex shapes, and its high specific gravity makes it disadvantageous for applications requiring light weight.
[0005] On the other hand, rubber sheets filled with heavy metals such as barium sulfate, cerium oxide, and barium oxide are commonly known as radiation-shielding plastics (Patent Document 3). However, these rubber sheets are opaque to visible light, making it impossible to visually or camera-visually confirm the location where radiation is being used.
[0006] For these reasons, there is a demand for plastic materials that are lightweight, easy to process, and have radiation shielding capabilities.
[0007] JP 2016-008146 JP 2014-062863 JP 2015-224967
[0008] An object of the present invention is to solve at least one of the problems in the prior art described above. Another object of the present invention is to provide a polymerizable composition that is solvent-soluble and thermoplastic, can be easily processed, and can be cured by heat or light, and can provide a transparent resin or optical material having radiation-shielding ability.
[0009] In view of the above circumstances, the present inventors have conducted extensive research and found that the above problems can be solved by using a bismuth-containing compound having a specific structure. Specifically, the present invention includes the following aspects.
[0010] <1> A polymerizable composition containing a compound (a) represented by the following formula (1): (In formula (1), X 1 ~X 3 are the same or different and represent a structure represented by the following formula (2) or a phenyl group; X 1 ~X 3 At least one of the above represents a structure represented by formula (2). When the bismuth atom of formula (1) is bonded to the structure represented by formula (2), it is bonded to an oxygen atom of formula (2). The oxygen atom of formula (2) is bonded to the same bismuth atom to form a cyclic structure, or to another bismuth atom to form a chain structure. (In formula (2), Z represents a hydrocarbon group.) <2> The polymerizable composition according to <1> above, wherein the structure represented by formula (2) represents a structure represented by formula (3): (In formula (3), n represents an integer of 0 to 10. R 1 represents a hydrogen atom or a hydrocarbon group. 1 represents a substituent represented by the following formula (4): (In formula (4), m represents an integer of 0 to 3. R 2represents a hydrocarbon group having 1 to 10 carbon atoms.) <4> The polymerizable composition according to any one of <1> to <3> above, further comprising (b) a compound having at least one group selected from the group consisting of an acryloyl group, a methacryloyl group, an allyl group, and a vinyl group. <5> The polymerizable composition according to any one of <1> to <4> above, further comprising (c) a compound having two or more thiol groups in one molecule. <6> The polymerizable composition according to <2> above, wherein the structure represented by formula (3) is at least one of structures represented by formula (5) or formula (6) below: (In formula (5), R 2 represents a hydrocarbon group having 1 to 10 carbon atoms. <7> The compound (b) having at least one group selected from the group consisting of an acryloyl group, a methacryloyl group, an allyl group, and a vinyl group is selected from the group consisting of methyl (meth)acrylate, butyl (meth)acrylate, isobutyl (meth)acrylate, 2-hydroxyethyl (meth)acrylate, benzyl (meth)acrylate, glycidyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, cyclohexyl (meth)acrylate, ethylene glycol di(meth)acrylate, diethylene glycol di(meth)acrylate, triethylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate, butanediol di(meth)acrylate, neopentyl glycol di(meth)acrylate, hexanediol di(meth)acrylate, nonanediol di(meth)acrylate, methyl acrylate, butyl acrylate, isobutyl ... acrylate, glycidyl (meth) The polymerizable composition according to <4> above, wherein the compound is one or more compounds selected from the group consisting of diol di(meth)acrylate, glycerin di(meth)acrylate, trimethylolpropane tri(meth)acrylate, pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, dipentaerythritol hexa(meth)acrylate, an ethylene oxide adduct of bisphenol A di(meth)acrylate, isobornyl (meth)acrylate, tetrahydrofurfuryl (meth)acrylate, allyl (meth)acrylate, 2-carboxyethyl (meth)acrylate, dimethyl (meth)acrylamide, phenyl vinyl sulfide, phenyl vinyl sulfoxide, 4-methyl-5-vinylimidazole, and 1-vinylimidazole. <8> A resin obtained by polymerizing and curing the polymerizable composition according to any one of <1> to <7> above. <9> An optical material comprising the resin according to <8> above. <10> A color tone changing material containing the resin according to <8> above.
[0011] According to the present invention, it is possible to provide a polymerizable composition that is solvent-soluble and thermoplastic, can be easily processed, and can be cured by heat or light, and can provide a transparent resin or optical material having radiation-shielding ability.
[0012] FIG. 1 shows the polycondensate obtained in Example 1. 1H-NMR (400MHz, CDCl 3 1 is a diagram showing the results of measuring the spectrum of the polycondensate obtained in Example 1. The structure bonded to the bismuth element in FIG. 1 is a phenyl group or a carboxylic acid group represented by formula (2). 13 C-NMR (100MHz, CDCl 3 2 shows the results of measuring the IR spectrum (KBr, cm) of the polycondensate obtained in Example 1. Note that the structure bonded to the bismuth element in FIG. 2 is a phenyl group or a carboxylic acid group represented by formula (2). FIG. 3 shows the results of measuring the IR spectrum (KBr, cm) of the polycondensate obtained in Example 1. -1 4 is a graph showing the measurement results of the polycondensation product obtained in Example 5. 1 H-NMR (400MHz, CDCl 3 4 shows the results of measuring the IR spectrum (KBr, cm) of the polycondensate obtained in Example 5. Note that the structure bonded to the bismuth element in FIG. 4 is a phenyl group or a carboxylic acid group represented by formula (2). FIG. 5 shows the results of measuring the IR spectrum (KBr, cm) of the polycondensate obtained in Example 5. -1 6 is a diagram showing the measurement results of the IR spectrum (KBr, cm -1 7 is a diagram showing the measurement results of the IR spectrum (KBr, cm -1 8 is a graph showing the measurement results of the polycondensation product obtained in Example 9. 1 H-NMR (400MHz, CDCl 3 8 is a diagram showing the measurement results of the spectrum. Note that the structure bonded to the bismuth element in FIG. 8 is a phenyl group or a carboxylic acid group represented by formula (2).
[0013] Hereinafter, the present invention will be described in detail by illustrating production examples and examples, but the present invention is not limited to the exemplified production examples and examples, and can be modified in any manner as long as it does not significantly deviate from the content of the present invention. In one embodiment of the present invention, a polymerizable composition is provided that contains a compound (a) represented by the following formula (1). Note that the polymerizable composition of the present invention encompasses both an embodiment that contains only the compound (a) represented by the following formula (1) and an embodiment that contains the compound (a) represented by the following formula (1) and other components. (In formula (1), X 1 ~X 3 are the same or different and represent a structure represented by the following formula (2) or a phenyl group; X 1 ~X 3 At least one of the above represents a structure represented by formula (2). When the bismuth atom of formula (1) is bonded to the structure represented by formula (2), it is bonded to an oxygen atom of formula (2). The oxygen atom of formula (2) is bonded to the same bismuth atom to form a cyclic structure, or to another bismuth atom to form a chain structure. (In formula (2), Z represents a hydrocarbon group).
[0014] Each component will be described below. Compound (a) represented by the above formula (1) (hereinafter also referred to as "(a) compound") includes all compounds that satisfy the above conditions. These may be used alone or in combination of two or more. The (a) compound used in the present invention has the advantage of not having the odor of sulfur compounds.
[0015] A preferred embodiment of the present invention preferably includes a structure represented by the following formula (3): (In formula (3), n represents an integer of 0 to 10. R 1 represents a hydrogen atom or a hydrocarbon group. 1 preferably represents a substituent represented by the following formula (4). (In formula (4), m represents an integer of 0 to 3. R 2 represents a hydrocarbon group having 1 to 10 carbon atoms.
[0016] In another preferred embodiment of the present invention, the structure represented by formula (3) is at least one of the structures represented by the following formula (5) or formula (6). (In formula (5), R 2 represents a hydrocarbon group having 1 to 10 carbon atoms.
[0017] The compound (a) can be obtained by reacting a triphenylbismuthine compound with a precursor dicarboxylic acid compound, as shown below. The precursor dicarboxylic acid compound used in the present invention is not particularly limited, but preferred examples include 2-octenylsuccinic acid, itaconic acid, phenylsuccinic acid, suberic acid, malonic acid, succinic acid, glutaric acid, adipic acid, azelaic acid, sebacic acid, allylsuccinic acid, 4-cyclohexene-1,2-dicarboxylic acid, cyclohexane-1,2-dicarboxylic acid, cyclohexane-1,3-dicarboxylic acid, cyclohexane-1,4-dicarboxylic acid, 4-methylcyclohexane-1,2-dicarboxylic acid, norbornane-2,3-dicarboxylic acid, 5-norbornene-2,3-dicarboxylic acid, and oxa-5-norbornene-2,3-dicarboxylic acid.
[0018] (wherein n represents 0 or 1. R 1 represents a substituent having at least an ene structure.
[0019] The molar ratio of the triphenylbismuthine compound to the precursor dicarboxylic acid compound when charged is preferably triphenylbismuthine compound / precursor dicarboxylic acid compound=1 / 3 to 3 / 3, more preferably triphenylbismuthine compound / precursor dicarboxylic acid compound=1.5 / 3 to 2.5 / 3, and even more preferably 1.8 / 3 to 2.2 / 3. The closer the ratio is to triphenylbismuthine compound / precursor dicarboxylic acid compound=2 / 3, where the numbers of phenyl groups and carboxylic acid groups are the same, the fewer unreacted phenyl groups and carboxylic acid groups there will be, which is expected to stabilize the network structure of the resin and improve heat resistance, etc.
[0020] As the solvent for the reaction, aliphatic hydrocarbon compounds such as hexane, heptane, and octane; aromatic hydrocarbon compounds such as benzene, toluene, and xylene; ketone compounds such as acetone, methyl ethyl ketone, and methyl isobutyl ketone; ether compounds such as diethyl ether, tetrahydrofuran, and methyl cyclopentyl ether; ester compounds such as ethyl acetate and butyl acetate; and halogen compounds such as dichloromethane, chloroform, and dichloroethane. Among these, tetrahydrofuran and methyl ethyl ketone are preferred.
[0021] After the reaction, the reaction solution is mixed with a solvent in which the resin has low solubility to cause reprecipitation, and the solvent is separated by a common technique such as filtration or centrifugation to obtain the target compound (a) represented by formula (1). Examples of solvents for reprecipitation include aliphatic hydrocarbon compounds such as hexane, heptane, and octane, and alcohol compounds such as methanol. Among these, aliphatic hydrocarbon compounds such as hexane, heptane, and octane are preferred. The reprecipitation solvent may be mixed in advance during the reaction, and after the reaction, the solvent that dissolves compound (a) represented by formula (1) may be distilled off first to allow reprecipitation.
[0022] The compound (a) represented by formula (1) can have multiple structures, rather than a single structure. For example, since the bismuth atom has three substitution sites, two of the substitution sites may form an intramolecular cyclic structure with the precursor dicarboxylic acid compound, and the remaining substitution site may bond to another bismuth atom via the precursor dicarboxylic acid compound. Therefore, the compound (a) can have structures such as those exemplified by the following formulas (7) to (10). However, the compound (a) represented by formula (1) is not limited to these.
[0023] The polymerizable composition containing the compound (a) may further contain (b) a compound having at least one group selected from the group consisting of an acryloyl group, a methacryloyl group, an allyl group, and a vinyl group, and / or (c) a compound having two or more thiol groups in one molecule.
[0024] (b) Compounds having at least one group selected from the group consisting of an acryloyl group, a methacryloyl group, an allyl group, and a vinyl group (hereinafter also referred to as "(b) compounds") include all compounds that satisfy this condition.
[0025] Examples of the (b) compound include methyl (meth)acrylate, butyl (meth)acrylate, isobutyl (meth)acrylate, 2-hydroxyethyl (meth)acrylate, benzyl (meth)acrylate, glycidyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, cyclohexyl (meth)acrylate, ethylene glycol di(meth)acrylate, diethylene glycol di(meth)acrylate, triethylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate, butanediol di(meth)acrylate, neopentyl glycol di(meth)acrylate, hexanediol di(meth)acrylate, and nonanediol di(meth)acrylate. Examples of suitable acrylates include, but are not limited to, glycerin di(meth)acrylate, trimethylolpropane tri(meth)acrylate, pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, dipentaerythritol hexa(meth)acrylate, ethylene oxide adduct di(meth)acrylate of bisphenol A, isobornyl (meth)acrylate, tetrahydrofurfuryl (meth)acrylate, allyl (meth)acrylate, 2-carboxyethyl (meth)acrylate, dimethyl (meth)acrylamide, phenyl vinyl sulfide, phenyl vinyl sulfoxide, 4-methyl-5-vinylimidazole, and 1-vinylimidazole. These may be used alone or in combination of two or more.
[0026] The ratio of the (a) compound to the (b) compound can be arbitrarily determined. This allows the viscosity of the polymerizable composition to be adjusted to a range that is easy to handle, improves the uniformity of the solution, and produces a homogeneous cured product after curing. Furthermore, mixing allows the mechanical strength of the cured resin and optical properties such as refractive index to be adjusted. The (b) compound can also be used as a solvent.
[0027] (c) Compounds having two or more thiol groups in one molecule (hereinafter also referred to as "(c) compounds") include all compounds that satisfy this condition.
[0028] (c) Compounds include o-dimercaptobenzene, m-dimercaptobenzene, p-dimercaptobenzene, 1,3,5-trimercaptobenzene, methanedithiol, 1,2-dimercaptoethane, 2,2-dimercaptopropane, 1,3-dimercaptopropane, 1,2,3-trimercaptopropane, 1,4-dimercaptobutane, 1,6-dimercaptohexane, bis(2-mercaptoethyl)sulfide, 1,2-bis(2-mercaptoethylthio)ethane, 1,5-dimercapto-3-oxapentane, 1,8-dimercapto-3,6-dioxaoctane, 2,2-dimethylpropane-1,3-dithiol, 3,4-dimethoxybutane-1,2- Dithiol, 2-mercaptomethyl-1,3-dimercaptopropane, 2-mercaptomethyl-1,4-dimercaptopropane, 2-(2-mercaptoethylthio)-1,3-dimercaptopropane, 1,2-bis(2-mercaptoethylthio)-3-mercaptopropane, 1,1,1-tris(mercaptomethyl)propane, tetrakis(mercaptomethyl)methane, 4,8-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, 4,7-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, 5,7-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, 1,1,3,3-Tetrakis(mercaptomethylthio)propane, 1,2,6,7-tetramercapto-4-thiapentane, ethylene glycol bis(2-mercaptoacetate), ethylene glycol bis(3-mercaptopropionate), 1,4-butanediol bis(2-mercaptoacetate), 1,4-butanediol bis(3-mercaptopropionate), trimethylolpropane tris(2-mercaptoacetate), trimethylolpropane tris(3-mercaptopropionate), pentaerythritol tetrakis(2-mercaptoacetate), pentaerythritol tetrakis(3-mercaptopropionate), 1,1-dimercaptocyclohexane, 1,2-dimercaptocyclohexane, 1,3-dimercaptocyclohexane Examples of the mercaptocyclohexane include, but are not limited to, hexane, 1,4-dimercaptocyclohexane, 1,3-bis(mercaptomethyl)cyclohexane, 1,4-bis(mercaptomethyl)cyclohexane, 2,5-bis(mercaptomethyl)-1,4-dithiane, 2,5-bis(mercaptoethyl)-1,4-dithiane, 1,2-bis(mercaptomethyl)benzene, 1,3-bis(mercaptomethyl)benzene, 1,4-bis(mercaptomethyl)benzene, bis(4-mercaptophenyl)sulfide, bis(4-mercaptophenyl)ether, 2,2-bis(4-mercaptophenyl)propane, bis(4-mercaptomethylphenyl)sulfide, bis(4-mercaptomethylphenyl)ether, and 2,2-bis(4-mercaptomethylphenyl)propane. These mercaptocyclohexanes may be used alone or in combination of two or more.
[0029] Preferred compounds as the compound (c) include bis(2-mercaptoethyl)sulfide, pentaerythritol tetrakis(2-mercaptoacetate), pentaerythritol tetrakis(3-mercaptopropionate), 2,5-bis(mercaptomethyl)-1,4-dithiane, 1,2-bis(2-mercaptoethylthio)-3-mercaptopropane, 1,2,6,7-tetramercapto-4-thiapentane, 4,8-dimercapto Examples of preferred compounds include methyl-1,11-dimercapto-3,6,9-trithiaundecane, 4,7-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, 5,7-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, 1,1,3,3-tetrakis(mercaptomethylthio)propane, 1,3-bis(mercaptomethyl)benzene, and 1,4-bis(mercaptomethyl)benzene. Specific examples of more preferred compounds include bis(2-mercaptoethyl)sulfide, pentaerythritol tetrakis(3-mercaptopropionate), 1,2-bis(2-mercaptoethylthio)-3-mercaptopropane, and 1,3-bis(mercaptomethyl)benzene.
[0030] The ratio of the (a) compound, the (b) compound, and the (c) compound may be any ratio. A preferred range of the composition is a ratio of (the number of SH groups in the (c) compound) / (the number of double bonds in the (a) compound + the number of double bonds in the (b) compound) of 10.0 or less, more preferably 5.0 or less, and most preferably 1.2 or less. If the ratio exceeds 10.0, polymerization may not be sufficient, resulting in a decrease in heat resistance.
[0031] In another embodiment of the present invention, the polymerizable composition containing the compound (a) is provided as a thermoplastic resin as it is, or a resin obtained by polymerizing and curing the polymerizable composition containing the compound (a).
[0032] The polymerizable composition containing the compound (a) of the present invention has a polymerizable group containing an unsaturated double bond, and therefore is cured by a polymerization reaction to obtain a resin. Examples of the polymerization reaction include a photopolymerization curing reaction and a heat polymerization curing reaction. In a preferred embodiment of the present invention, a photopolymerization curing reaction, which allows polymerization in a short time, is preferred. In another embodiment of the present invention, a thermal polymerization curing reaction may be selected. In an embodiment of the present invention, a thermal curing reaction and a photocuring reaction may be combined.
[0033] The polymerization and curing reaction of the polymerizable composition containing the compound (a) of the present invention can be carried out in the presence or absence of a polymerization catalyst. When polymerizing the polymerizable composition containing the compound (a) of the present invention to obtain a resin, it is preferable to polymerize and curing in the presence of a polymerization catalyst to promote the polymerization reaction. Therefore, in one embodiment of the present invention, a resin obtained by polymerizing and curing the polymerizable composition of the present invention in the presence of a polymerization catalyst, as well as an optical material obtained from the resin, are provided. The resin and optical material thus obtained are preferably transparent. In another embodiment of the present invention, a method for producing a cured product, preferably an optical material, is provided, characterized by curing the polymerizable composition of the present invention by irradiation with ultraviolet or visible light in the presence of a polymerization catalyst.
[0034] In the case of a photopolymerization reaction, a polymerizable composition containing the compound (a) of the present invention is cured by irradiation with light rays (active energy rays), to produce a resin as a cured product. The light rays are not particularly limited as long as they can cure the polymerizable composition, but typically include ultraviolet light, visible light, radiation, and electron beams. Preferred are ultraviolet light or visible light, and more preferred is ultraviolet light because of its fast polymerization rate. The irradiation intensity of the light rays is not particularly limited, but is typically 10 to 100,000 mW / cm. 2 The irradiation time is not particularly limited, but is usually from 1 minute to several hours, preferably from 1 to 60 minutes. The irradiation temperature is not particularly limited, and polymerization is possible at around room temperature. When the polymerizable composition containing the compound (a) of the present invention is solid at room temperature, photocuring may be carried out while heating it to a temperature equal to or higher than the melting point.
[0035] The polymerization catalyst is not particularly limited and may be appropriately selected depending on the type of reactant, polymerization conditions, etc. In the case of photopolymerization, a compound that generates radicals upon irradiation with light (preferably active energy rays) (photodecomposition-type radical polymerization initiator) is preferred, and specific examples include, but are not limited to, benzoin derivatives, benzyl derivatives, benzophenone derivatives, and acetophenone derivatives. Among these, commercially available products such as hydroxycyclohexyl-phenyl ketone (trade name Irgacure (registered trademark) 184, manufactured by Ciba Specialty Chemicals), 2,2-dimethoxy-2-phenylacetophenone (Irgacure (registered trademark) 651), 1-[4-(2-hydroxyethoxy)-phenyl]-2-hydroxy-2-methyl-1-propan-1-one (Irgacure (registered trademark) 2959), and 2,4,6-trimethylbenzoyl-diphenylphosphine oxide (Irgacure (registered trademark) TPO) are preferably used.
[0036] Alternatively, it is also preferable to use a compound (redox polymerization initiator) that generates radicals in the coexistence of an oxidizing agent and a reducing agent as a polymerization catalyst for the photopolymerization reaction. Specific examples include a system that combines an oxide selected from persulfates such as sodium persulfate, potassium persulfate, and ammonium persulfate, and peroxides such as hydrogen peroxide, t-butyl peroxide, and methyl ethyl ketone peroxide with a reducing compound selected from L-ascorbic acid, sodium hydrogen sulfite, and the like.
[0037] Alternatively, a photoredox catalyst that generates radicals upon irradiation with light such as visible light is also preferably used as a polymerization catalyst for the photopolymerization reaction. Specific examples include ruthenium (II) polypyridyl complexes (e.g., Ru(bpz) 3 - (PF 6 ) 2 catalysts), and transition metal complexes such as iridium(III) phenylpyridyl complexes.
[0038] In the case of a thermal polymerization reaction, a polymerizable composition containing the compound (a) of the present invention is polymerized (cured) by heating to produce a resin as a cured product.
[0039] The polymerization catalyst used in the thermal polymerization reaction is preferably a compound that generates radicals upon heating (thermal decomposition type radical polymerization initiator). Specific examples include persulfates such as sodium persulfate, ammonium persulfate, and potassium persulfate; hydrogen peroxide; organic peroxides such as t-butyl hydroperoxide; and azo compounds such as 2,2'-azobis(2-amidinopropane) dihydrochloride, 2,2'-azobis[2-2(-imidazolin-2-yl)propane] dihydrochloride, 2,2'-azobis(2-methylpropionitrile), and 2,2'-azobis(isobutyronitrile) (AIBN).
[0040] The polymerization catalyst may be one or more compounds selected from the group consisting of peroxides, azo compounds, redox polymerization initiators, and transition metal complexes. The polymerization catalysts may be used alone or in combination.
[0041] The amount of polymerization catalyst added cannot be determined in general terms because it varies depending on the components, mixing ratio, and polymerization / curing method of the polymerizable composition containing the compound (a) of the present invention. However, it is typically 0.0001% by mass to 10% by mass, preferably 0.001% by mass to 5% by mass, more preferably 0.01% by mass to 1% by mass, and most preferably 0.01% by mass to 0.5% by mass, relative to 100% by mass of the total polymerizable composition. If the amount added is more than 10% by mass, rapid polymerization may occur. If the amount added is less than 0.0001% by mass, the resulting composition may not be sufficiently cured, resulting in poor heat resistance. Therefore, in a preferred embodiment of the present invention, the resin production method includes the steps of adding a polymerization catalyst in an amount of 0.0001 to 10% by mass, relative to the total amount of the polymerizable composition, and polymerizing and curing the composition.
[0042] Polymerization (curing) of the polymerizable composition containing the compound (a) of the present invention by heating is usually carried out as follows. That is, the curing time is usually 1 to 100 hours, and the curing temperature is usually -10°C to 140°C. The polymerization is carried out by a step of maintaining the polymerizable composition at a predetermined polymerization temperature for a predetermined time, a step of increasing the temperature at a rate of 0.1°C to 100°C / h, and a step of decreasing the temperature at a rate of 0.1°C to 100°C / h, or a combination of these steps. The curing time refers to the polymerization and curing time including the temperature increase process, and includes the step of maintaining the polymerizable composition at the predetermined polymerization (curing) temperature as well as the step of increasing the temperature and cooling the temperature to the predetermined polymerization (curing) temperature.
[0043] The polymerization and curing process (photopolymerization and thermal polymerization) is not particularly limited, but is preferably a curing process using a metal, ceramic, glass, resin, or other mold. Specifically, the components of the polymerizable composition containing the compound (a) of the present invention and a polymerization catalyst are mixed together. These may be mixed simultaneously in the same container under stirring, or the raw materials may be added and mixed stepwise, or several components may be mixed separately and then remixed in the same container. Furthermore, the raw materials and auxiliary materials may be mixed in any order. The set temperature and time required for mixing are essentially any conditions that ensure sufficient mixing of the components. The polymerizable composition thus obtained is poured into a mold or other form, and the polymerization and curing reaction is carried out by heating or irradiation with ultraviolet light or other light, and then the mixture is removed from the mold. In this way, a resin is obtained by curing the polymerizable composition containing the compound (a) of the present invention. The polymerization reaction (curing process) can be carried out in air, in an inert gas atmosphere such as nitrogen, or under reduced pressure or pressure.
[0044] After curing, the resulting resin is preferably annealed for about 10 minutes to 5 hours at a temperature of 50 to 150° C. to remove distortion. Furthermore, the resulting resin may be subjected to surface treatment such as hard coating or anti-reflection, as needed.
[0045] When producing the resin of the present invention, additives such as ultraviolet absorbers, antioxidants, adhesion improvers, and mold release agents may be added to the polymerizable composition to further improve the practical utility of the resulting resin.
[0046] As described above, the polymerizable composition containing the compound (a) of the present invention can provide a resin excellent in at least one property such as a high refractive index, photopolymerization curability, thermal polymerization curability, etc. Thus, a resin (cured product) obtained by curing the polymerizable composition also represents one embodiment of the present invention.
[0047] One embodiment of the present invention is a molded article produced using a resin obtained by polymerizing and curing a polymerizable composition containing the compound (a) of the present invention. The molded article is useful, for example, in advanced medical settings where diagnostics are performed using CT (computed tomography) or PET (positron emission tomography) devices, and in nuclear power plants. It can be used as a radiation shielding plate or shielding filter, or it can be used directly as an optical material (component). For example, its use in a camera lens can protect the camera sensor from radiation damage and transmit images with radiation noise removed. These applications include optical materials (components), machine component materials, electrical and electronic component materials, automotive component materials, civil engineering and construction materials, molding materials, and various other applications, including paints and adhesives. Among these, preferred are optical materials for optical applications such as spectacle lenses, (digital) camera imaging lenses, light beam focusing lenses, light diffusing lenses, and other lenses, LED sealants, optical adhesives, optical transmission bonding materials, prisms, filters, diffraction gratings, watch glasses, and transparent glass and cover glass for display devices; display device applications such as substrates for display elements such as LCDs, organic ELs, and PDPs, color filter substrates, touch panel substrates, display backlights, light guide plates, display protective films, anti-reflection films, and anti-fogging films; optical memories, recording media such as electronic paper, sensor materials for UV checkers, light-adjusting materials for window glass, sunglasses, and automotive window glass; textiles, cosmetic materials, photochromic materials, and other color-changing materials for printing materials. Optical adhesives, prisms, and coating agents are particularly preferred as optical materials.
[0048] The present invention will be described in detail with reference to the following examples, but the present invention is not limited to these. The obtained monomers and cured products were evaluated by the following methods. NMR: Measurement was performed using an ECX-400 manufactured by JEOL Ltd. IR: Measurement was performed using a Jasco FT-IR460Plus manufactured by JASCO Corporation.
[0049] (Example 1) Triphenylbismuthine (BiPh 3 Polycondensation of bis(2-octenylsuccinic acid) (cis, trans mixture) (Bi-OSA:1-1) with 2-octenylsuccinic acid (cis, trans mixture) (Bi-OSA:1-1) (Typical Example) Triphenylbismuthine (220 mg, 0.500 mmol) represented by the structural formula below and 2-octenylsuccinic acid (cis, trans mixture) (OSA) (114 mg, 0.500 mmol) represented by the structural formula below were placed in a two-necked test tube, and dehydrated THF (1.00 mL) was added under a nitrogen atmosphere, followed by a reaction under reflux conditions for 24 hours. After completion of the reaction, the solution was purified by precipitation with approximately 30 to 50 times the amount of hexane, and centrifuged to obtain a white solid in a yield of 84.2% (390 mg). An example of the structure of the white solid obtained in Example 1 is shown in the following formula (11). 1 H-NMR (400MHz, CDCl 3 The results of the spectrum measurement are shown in Figure 1. 13 C-NMR (100MHz, CDCl 3 The IR spectrum (KBr, cm) of the polycondensate obtained in Example 1 is shown in FIG. -1 The measurement results are shown in Figure 3.
[0050] Examples 2 to 4 Polymerization was carried out in the same manner as in Example 1, except that the compounding ratio of triphenylbismuthine and 2-octenylsuccinic acid and the solvent were changed as shown in Table 1 below. The obtained results are shown in Table 1 below.
[0051]
[0052] (Example 5) Triphenylbismuthine (BiPh 3Polycondensation of bismuth triphenylbismuthine (220 mg, 0.500 mmol), 2-octenylsuccinic acid (cis, trans-mixture) (103 mg, 0.450 mmol), and itaconic acid (6.50 mg, 0.0500 mmol) represented by the following structural formula were added to a two-necked test tube, and dehydrated THF (1.00 mL) was added under a nitrogen atmosphere, followed by a reaction under reflux for 24 hours. After completion of the reaction, the solution was purified by precipitation with approximately 30 to 50 times the amount of hexane, and centrifuged to obtain a white solid in a yield of 78.0% (193 mg). An example of the structure of the white solid obtained in Example 5 is shown in the following formula (12). 1 H-NMR (400MHz, CDCl 3 The IR spectrum (KBr, cm) of the polycondensate obtained in Example 5 is shown in FIG. -1 The measurement results are shown in Figure 5.
[0053] (Example 6) Triphenylbismuthine (BiPh 3 Polycondensation of bismuth triphenylbismuthine (220 mg, 0.500 mmol), 2-octenylsuccinic acid (cis, trans mixture), and phenylsuccinic acid [Bi(OSA-PSA:5-5)]. Triphenylbismuthine (220 mg, 0.500 mmol), 2-octenylsuccinic acid (cis, trans mixture) (57.1 mg, 0.250 mmol), and phenylsuccinic acid (48.5 mg, 0.250 mmol) represented by the following structural formula were added to a two-necked test tube, and dehydrated THF (1 mL) was added under a nitrogen atmosphere. The reaction was carried out under reflux conditions for 24 hours. After completion of the reaction, isolation and purification were carried out to obtain a white solid in a yield of 77.6% (230 mg). An example of the structure of the white solid obtained in Example 6 is shown in formula (13) below. The IR spectrum (KBr, cm) of the polycondensate obtained in Example 6 was -1 The measurement results are shown in FIG.
[0054] (Example 7) Triphenylbismuthine (BiPh 3Polycondensation of bismuth triphenylbismuthine (220 mg, 0.500 mmol), 2-octenylsuccinic acid (cis, trans mixture), and methacrylic acid [Bi(OSA-MA:5-5)]. Triphenylbismuthine (220 mg, 0.500 mmol), 2-octenylsuccinic acid (cis, trans mixture) (114 mg, 0.500 mmol), and methacrylic acid (43.0 mg, 0.500 mmol) were placed in a two-necked test tube, and dehydrated THF (1.5 mL) was added under a nitrogen atmosphere. The reaction was carried out under reflux for 24 hours. After completion of the reaction, 251 mg of a white solid was obtained. An example of the structure of the white solid obtained in Example 7 is shown in formula (14) below. The IR spectrum (KBr, cm) of the polycondensate obtained in Example 7 was -1 The measurement results are shown in FIG.
[0055] (Example 8) Triphenylbismuthine (BiPh 3 Polycondensation of bismuth triphenylbismuthine (220 mg, 0.500 mmol), 2-octenylsuccinic acid (cis, trans mixture), and methacrylic acid [Bi(OSA-MA:5-5)]. Triphenylbismuthine (220 mg, 0.500 mmol), 2-octenylsuccinic acid (cis, trans mixture) (114 mg, 0.500 mmol), and methacrylic acid (43.0 mg, 0.500 mmol) were placed in a two-necked test tube, and anhydrous THF (1.5 mL) was added under a nitrogen atmosphere. The reaction was carried out under reflux for 24 hours. After completion of the reaction, 251 mg of a white solid was obtained.
[0056] (Example 9) BiPh 3 Polycondensation of 2-octenylsuccinic acid (cis, trans mixture) and suberic acid [Bi(OSA-SA:7-3)] Triphenylbismuthine (220 mg, 0.500 mmol), 2-octenylsuccinic acid (cis, trans mixture) (79.9 mg, 0.350 mmol), and suberic acid (26.1 mg, 0.15 mmol) represented by the following structural formula were added to a two-necked test tube, and dehydrated THF (1 mL) was added under a nitrogen atmosphere, followed by a reaction under reflux for 24 hours. After completion of the reaction, the solution was precipitated and purified with approximately 30 to 50 times the amount of hexane, and centrifuged to obtain a white solid in a yield of 72.4% (144 mg). An example of the structure of the white solid obtained in Example 9 is shown in the following formula (15). 1H-NMR (400MHz, CDCl 3 The results of the spectrum measurement are shown in FIG.
[0057] (Example 10) Hot-press molding of Bi-OSA:1-1 Bi-OSA:1-1 (250 mg) obtained in Example 1 was sandwiched between two polyimide films and pressed in an Imoto Manufacturing press (IMC-1A45) at 150°C for 1 minute under a pressure of 15 kN. After that, the mixture was slowly cooled to room temperature to obtain a film with a transmittance of 50%.
[0058] The X-ray shielding properties of the bismuth-containing film were evaluated using a small-angle X-ray scattering device (SAXS: NANO-Viewer, manufactured by Rigaku Corporation) as the X-ray source (detector). X-ray transmittance was calculated using the following formula: X-ray source: CuKα 1.54 angstroms (8.048 keV) Tube voltage (accelerating voltage): 40 kV X-ray transmittance (Tr) = Σ transmitted light intensity of sample [counts] / Σ direct intensity (transmitted light intensity without sample) [counts] The X-ray transmittance of the Bi-OSA:1-1 film obtained above was 0.012% at a thickness of 449 μm (0.0449 cm) and less than 0.001% at a thickness of 947 μm (0.0947 cm). The results are shown in Table 2.
[0059] Comparative Example 1: X-ray shielding property of Poly(BiMA-co-DMAA) film (BiMA content: 40 wt%) Poly(BiMA-co-DMAA) was prepared with the maximum BiMA content of 40 wt%, as described in JP 2022-128911 A. The X-ray shielding property of a 450 μm-thick Poly(BiMA-co-DMAA) film measured under the same conditions was 5%. This result was inferior to that of Example 10.
[0060]
Claims
1. A polymerizable composition comprising a compound (a) represented by the following formula (1): (In formula (1), X 1 ~X 3 are the same or different and each represents a structure represented by the following formula (2) or a phenyl group; X 1 ~X 3 At least one of the above represents a structure represented by formula (2). When the bismuth atom of formula (1) is bonded to the structure represented by formula (2), it is bonded to an oxygen atom of formula (2). The oxygen atom of formula (2) is bonded to the same bismuth atom to form a ring structure, or to another bismuth atom to form a chain structure. (In formula (2), Z represents a hydrocarbon group).
2. The polymerizable composition according to claim 1, wherein the structure represented by formula (2) is a structure represented by formula (3): (In formula (3), n represents an integer of 0 to 10. R 1 represents a hydrogen atom or a hydrocarbon group.
3. R in formula (3) 1 The polymerizable composition according to claim 1 or 2, wherein: represents a substituent represented by the following formula (4): (In formula (4), m represents an integer of 0 to 3. 2 represents a hydrocarbon group having 1 to 10 carbon atoms.
4. The polymerizable composition according to any one of claims 1 to 3, further comprising (b) a compound having at least one group selected from the group consisting of an acryloyl group, a methacryloyl group, an allyl group, and a vinyl group.
5. The polymerizable composition according to any one of claims 1 to 4, further comprising (c) a compound having two or more thiol groups in one molecule.
6. The polymerizable composition according to claim 2, wherein the structure represented by formula (3) is at least one of structures represented by the following formula (5) or formula (6): (In formula (5), R 2 represents a hydrocarbon group having 1 to 10 carbon atoms.
7. The compound (b) having at least one group selected from the group consisting of an acryloyl group, a methacryloyl group, an allyl group, and a vinyl group is selected from the group consisting of methyl (meth)acrylate, butyl (meth)acrylate, isobutyl (meth)acrylate, 2-hydroxyethyl (meth)acrylate, benzyl (meth)acrylate, glycidyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, cyclohexyl (meth)acrylate, ethylene glycol di(meth)acrylate, diethylene glycol di(meth)acrylate, triethylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate, butanediol di(meth)acrylate, neopentyl glycol di(meth)acrylate, hexanediol di(meth)acrylate, The polymerizable composition according to claim 4, which is one or more compounds selected from the group consisting of nandiol di(meth)acrylate, glycerin di(meth)acrylate, trimethylolpropane tri(meth)acrylate, pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, dipentaerythritol hexa(meth)acrylate, ethylene oxide adduct di(meth)acrylate of bisphenol A, isobornyl (meth)acrylate, tetrahydrofurfuryl (meth)acrylate, allyl (meth)acrylate, 2-carboxyethyl (meth)acrylate, dimethyl (meth)acrylamide, phenyl vinyl sulfide, phenyl vinyl sulfoxide, 4-methyl-5-vinylimidazole, and 1-vinylimidazole.
8. A resin obtained by polymerizing and curing the polymerizable composition according to any one of claims 1 to 7.
9. An optical material comprising the resin according to claim 8.
10. A color-changing material comprising the resin according to claim 8.
Citation Information
Patent Citations
A colloidal bismuth tartrate compound, its drug formulation, preparation method, and applications
CN102276445A
Bismuth bitartrate-beta-cyclic lactone compound, preparation method thereof, medicine composition thereof and application thereof
CN108250244A
Polymerizable composition, and optical material and color-changing material that are obtained therefrom
JP2021172797A
Polymerizable composition and resin made by polymerizing and curing the same
JP2022128911A
Polymerizable composition and resin made by polymerizing and curing the same
JP2022128912A
Cited By
Bismuth-containing polymer compound and method for producing same
WO2026094884A1