A method for the production of monograms on vehicles

WO2024232846A1PCT designated stage expired Publication Date: 2024-11-14DURDEN PLASTIK URUNLER & YAPISKAN FILM TICARET & SANAYI ANONIM SIRKETI
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/TR2024/050117
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-02-15
Publication Date
2024-11-14

Smart Images

  • Figure 000001
    Figure 000001
  • Figure 000002
    Figure 000002
  • Figure 000003
    Figure 000003
Patent Text Reader

Abstract

The invention relates to an eco-friendly method for the production of monograms, without the use of dyes or chemicals, particularly on the top, bottom, or side adjacent to the headlights, for use on all vehicles, particularly but not limited to large or small land vehicles.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] A METHOD FOR THE PRODUCTION OF MONOGRAMS ON VEHICLES

[0002] TECHNICAL FIELD

[0003] The invention relates to an eco-friendly method for the production of monograms, without the use of dyes or chemicals, particularly positioned on the top, bottom, or side adjacent to the headlights, for use on all vehicles, particularly but not limited to large or small land vehicles.

[0004] BACKGROUND

[0005] A monogram is a type of design in which one or more letters or other type units are arranged side by side or on top of one another to form a single symbol. Monograms are typically created by combining the initials of a person or company, the object being to create a distinguishable symbol or logo.

[0006] Monograms are produced by making the necessary arrangements for placement on land vehicles, which are then mounted on the vehicles. Monograms are placed in a variety of places on vehicles. Monograms, in particular, can be positioned above, below, or adjacent to vehicle headlight elements.

[0007] In order to make vehicles more visually appealing, monograms are used in prominent and striking designs or coatings such as dyeing or chroming.

[0008] Dyes are obtained by combining a pigment or pigment mixture with a binder part; the remainder of the binder is filtered and packaged after color and viscosity adjustments with additives and solvents. Dyes frequently comprise chemicals and / or heavy metals that harm human and environmental health. Obtaining these dyes, or processes involving dyes, generates wastewater that is harmful to the environment, climate, and human health. Since dyes and dye wastewater contain toxic chemicals such as Pb, Cr, and Cd; the direct discharge of the wastewater into receiving environments harms the ecological balance. Inorganic acids, heavy metals, and toxic organic compounds all disrupt the biochemical balance in surface waters. Several studies have shown that organic substances and dyestuff have a toxic impact on fish.

[0009] Chromium plating refers to the process of coating metal surfaces with chromium using heat treatment. In the relevant technical field, these processes are also called chroming. Chroming processes are used to increase the surface hardness of steel materials like iron alloys and to provide resistance to prevent oxidation and corrosion at high temperatures. However, the chromium-based compounds used in chroming processes are carcinogenic and dangerous for the environment and human health.

[0010] In particular, since land vehicles are inextricably linked to humans and the environment, it is expected that the components or elements used in their production are also made from materials that do not harm the environment or human health. Therefore, it is aimed to disclose production methods that are not harmful to the environment or human health for the production of apparatus to be used in vehicles such as monograms, which are expected to have interesting designs.

[0011] BRIEF DESCRIPTION OF THE INVENTION

[0012] In the present art, interesting and distinctive designs are frequently used to obtain monograms on vehicles, particularly land vehicles, but not exclusively. For obtaining monograms, dyeing and / or coating processes such as chroming are often performed. These coating and / or dyeing processes frequently involve the use of chemicals or heavy metals that are dangerous to the environment and human health, so their use should be reduced. The present inventors describe a method for producing monograms suitable for use on vehicles, particularly but not limited to land vehicles, that is not harmful to human or environmental health, for the relevant technical field.

[0013] In this regard, the present invention discloses a method for producing monograms with an attractive and distinctive design, and without using coating or dyeing processes such as chroming.

[0014] In another aspect, the invention discloses a method for obtaining monograms with an extended lifetime. DETAILED DESCRIPTION OF THE INVENTION

[0015] In this detailed description, the subject matter of the invention is a method of producing monograms particularly positioned above, below, or adjacent to the top, bottom, or side of headlights, for use on all vehicles, particularly but not limited to large or small land vehicles and is described only by way of non-limiting examples for a better understanding of the subject matter.

[0016] The inventive method relates to the production of monograms. The main object of the invention is to produce monograms without performing dyeing and coating processes such as chroming.

[0017] In the inventive method, the monogram for the vehicles is obtained in two parts and combined in the final processing step. The monogram obtained by the said method comprises a main part comprising the monogram and an upper part comprising a lens to extend the lifetime of said main part and to provide protection against impacts.

[0018] In the production method described in the present invention, the main part and the upper part are produced separately and then joined together using the joining method.

[0019] - Obtaining the main part

[0020] In a preferred application, the monogram is created on a polymer-based material. The monogram can be created based on the desired design to be created. The shape, design, and color of the monogram do not limit the scope of protection for this invention.

[0021] In the present invention, the main part of the monogram is made of a material that is intrinsically interesting and distinct and does not require any dyeing or coating process. In the present invention, the production main part containing the monogram comprises at least one of acrylonitrile butadiene styrene (abbreviated as ABS), polycarbonate (abbreviated as PC), polyacrylate (abbreviated as PA), polypropylene (abbreviated as PP), polymethylmethacrylate (abbreviated as PMMA), and / or acrylonitrile styrene acrylate (abbreviated as ASA) compounds as a raw material.

[0022] In a preferred embodiment of the invention, at least one of the ASA and / or PMMA compounds is used as a raw material in the production of the main part with the monogram. In a preferred application, the main part with the monogram comprises a mixture of ASA-PMMA compound as raw material.

[0023] In this invention, the raw material is subjected to plastic injection processes during the production of the main part comprising the monogram.

[0024] Before conducting the injection processes with the desired properties, the raw material is dried at temperatures ranging from 80 and 100°C. The drying process is conducted for 200 to 300 minutes. Furthermore, the molds that will provide the desired shape configurations are heated to temperatures ranging from 60 and 80°C before injection operations.

[0025] In order to carry out the injection processes, the raw material is subjected to a melting process at temperatures between 200 to 300 °C before being injected into molds that have been previously heated to specific temperatures. The melting process and the subsequent placement in the molds are preferably carried out for 30 seconds to 75 seconds.

[0026] Through plastic injection, it is ensured that the raw material is formed into monograms in the desired designs. Hot stamping is used to provide the resulting monogram design with an appearance similar to chrome plating, making it more interesting and distinct. As is known in the art, the hot stamping process is performed on a surface using a hot stamping machine. The pressure rollers in the hot-pressing machine place the foil to be hot pressed on the surface of the raw material used in the invention. Wherein preferably chrome or silver foils can be used to give a chrome or silver appearance. The temperature values of the pressure rollers used for the adhesion processes preferred in the invention are designed to be applied on the film roll at temperatures between 240-275 °C. The temperature values determined here are the result of research and development activities to ensure full interaction between the raw material and the foil to be used in hot stamping processes.

[0027] - Obtaining the upper part

[0028] The region to be used as the upper part of the invention consists of two parts. The lens part is the transparent and light-transmitting part. The lens part corresponds to the monogram in the main part. In this way, the monogram's design, color, and shape are clearly visible through the lens. While the lens part allows for a clear view of the monogram, it also protects it from corrosive and mechanical effects in the external environment. In this way, it allows monograms to be better protected.

[0029] Another part in the upper part is the other integral auxiliary part, which will be formed by injection processes alongside the lens. Again, the said part supports the main part's design while also being capable of providing additional strength for the lens.

[0030] As previously stated, the upper part is obtained by combining two materials using the 2K injection method. Wherein the lens is preferably transparent and particularly allows the monogram to be seen from the outside. The other auxiliary component in the upper part is obtained from raw materials with a shiny appearance similar to the main part.

[0031] As is known, the 2K injection method is the process of making multiple joints in two stages. Although the materials vary, this method usually involves a hard plastic and a different material on top of it. Here, there are two molding operations are these molding operations are completed one after another. It is a method that allows both hard and softer materials to be combined in a single piece.

[0032] The lens material is at least one of the polycarbonate and / or PMMA polymer-based materials, preferably in a transparent color. As the auxiliary component, it comprises at least one of the compounds among acrylonitrile butadiene styrene, polycarbonate, polyacrylate, polypropylene, polymethylmethacrylate, and / or acrylonitrile styrene acrylate.

[0033] In a preferred embodiment of the invention, at least one of the ASA and / or PMMA compounds is used as a raw material in the production of the auxiliary component. In a preferred application, the main part with the monogram comprises a mixture of ASA-PMMA compound as raw material.

[0034] When performing a 2K injection in this invention, the lens part is pressed into the injection mold first. The next process step is to rotate the mold containing the lens part 180° in the machine and inject the other auxiliary part into the injection mold. As a result of all the processes, with 2K injection, the upper part's lens part and the auxiliary part can be combined into one material.

[0035] - Combining the Main Part and the Upper Part

[0036] As the final process step, the inventive method assembles the main part and the upper part obtained through separate process steps. The said combining process is performed using vibration welding or laser welding methods.

[0037] In the present invention, the vibration welding method is performed to combine the main part and the upper part.

[0038] In the art, Vibration Welding refers to the process of combining materials with the same molecular structure, usually thermoplastics. In this method, the parts are joined by applying pressure with vibration frequencies, then the vibration is stopped to allow for cooling of the parts that were joined under pressure. Combining is performed by locally applying high-frequency vibration energy to the surfaces held together. Although the temperature increases slightly on the contact surfaces, it can never reach a value that can cause melting.

[0039] The said merging process is carried out as follows, - the main part is placed in the lower mold of the vibration machine,

[0040] - the upper part is attached to the upper mold via vacuum,

[0041] - with the operation of the vibration machine, the lower mold moves upwards towards the upper mold, and the combining processes are performed using the predetermined values.

[0042] The said vibration welding process is carried out with frequency values between 200 and 275 Hz. The welding process is preferably carried out under a pressure between 15 and 20 bar.

[0043] Through the method described in the present invention, it is possible to obtain an interesting and distinctive monogram without the need for dyeing and coating processes, which cause problems in the state of the art. In this way, the need for coating and dyeing processes that use chemicals or heavy metals that are dangerous to the environment and human health is eliminated. Both the use of chemicals or heavy metals in the application of said methods and the disposal of the wastes generated were costly for businesses. With the inventive method, these costs and labor force, as well as storage operations, are eliminated and the secondary objects of cost and time savings are achieved.

[0044] The monogram product produced by the method of the invention is made by combining several materials, and these materials also provide strength and resistance to corrosive environments for monograms.

[0045] The protection scope of the invention is set out in the appended claims and cannot be strictly limited to what is described in this detailed description for illustrative purposes. It is clear that a person skilled in art can come up with similar embodiments in light of the foregoing without deviating from the main theme of the invention.

Claims

CLAIMS1 . The invention is a method for the production of monograms suitable for use on vehicles, characterized in that, without the need of dyeing and chroming and similar coating processes, it comprises the following steps;- obtaining said main part by applying the plastic injection method in molds of suitable design to at least one component forming the main part in which the monogram is located in suitable designs,- performing the hot stamping process on the upper adjacency of the main part obtained by the plastic injection method, corresponding to the monogram zone,- obtaining the upper part by applying a 2K injection method of at least one component forming the lens portion and at least one component forming the auxiliary component,- combining the main part and the upper part, which are obtained separately, by laser or vibration welding method.

2. The method according to Claim 1 , characterized in that at least one of acrylonitrile butadiene styrene, polycarbonate, polyacrylate, polypropylene, polymethylmethacrylate and / or acrylonitrile styrene acrylate compounds is used as raw material in obtaining said main part.

3. The method according to any one of the preceding claims, characterized in that it comprises at least one of ASA and / or PMMA compounds as raw material in obtaining the main part.

4. The method according to any one of the preceding claims, characterized in that the raw material is subjected to a drying process at a temperature between 80 and 100°C before plastic injection process.

5. The method according to Claim 4, characterized in that said drying process is carried out for a period of 200 to 300 minutes.

6. The method according to any one of the preceding claims, characterized in that the molds to be used in the plastic injection process are heated to a temperature between 60 and 80°C, before process.

7. The method according to any one of the preceding claims, characterized in that the plastic injection process are subjected to a melting process between 200 and 300°C.

8. The method according to any one of the preceding claims, characterized in that chrome or silver foils are used for hot stamping process.

9. The method according to any one of the preceding claims, characterized in that the temperature of the pressure rollers used in the hot stamping process is between 240-275°C.

10. The method according to any one of the preceding claims, characterized in that at least one of the polycarbonate and / or PMMA polymer-based materials is used as the lens part in obtaining the said upper part.1 1 .The method according to any one of the preceding claims, characterized in that at least one of acrylonitrile butadiene styrene, polycarbonate, polyacrylate, polypropylene, polymethylmethacrylate and / or acrylonitrile styrene acrylate compounds is used as an auxiliary component in obtaining said upper part.

12. The method according to any one of the preceding claims, characterized in that the upper part and the main part are combined by the vibration welding method.

13. The method according to Claim 12, characterized in that the vibration welding method is performed at a value ranging from 200 to 275 Hz.

14. The method according to Claim 12, characterized in that the vibration welding method is performed at a value ranging from 15 to 20 bar.

Citation Information

Patent Citations

  • Laminated plastic and metal component and process for producing same

    US20010053431A1

  • Emblem for motor vehicle

    US20060237995A1

  • Method for producing a dimensionally stable inscription

    US20100123265A1

  • Emblem for automobile and method of manufacturing the same

    US20190299541A1