Method for optimizing catalytic performance of hydrogen peroxide electrocatalyst
Patent Information
- Application Number
- PCT/CN2023/094650
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-17
- Publication Date
- 2024-11-21
Smart Images

Figure 000009 
Figure 000010 
Figure 000011
Abstract
Description
Method For Optimizing Catalytic Performance Of Hydrogen Peroxide ElectrocatalystField
[0001] The present invention belongs to the field of chemical engineering.Background
[0002] As an environment-friendly strong oxidant and potential energy carrier, Hydrogen peroxide (H2O2) is widely used in various industrial processes. Producing H2O2 in concentrated form by anthraquinone process is the most widely used method at present. However, the anthraquinone process is complicated in operation and tends to cause environmental damage, how to synthesize H2O2 in a green and economic way is an urgent problem to be solved at present.
[0003] Hydrogen peroxide (H2O2) production via electrocatalytic oxygen reduction reaction (ORR) has aroused great attention due to the mild reaction conditions and environment-friendly properties. Theoretically, the selectivity of ORR is highly dependent on the adsorption model of oxygen molecules (O2) on the surface of catalysts. The side-on adsorption with a “*O–O*” configuration (*presents the active site) is conducive to weakening the O–O bond for reduction of O2 into H2O via a four-electron (4e) ORR pathway, while the end-on configuration formed by a solo oxygen atom coordinated on a single active site ( “*OOH” intermediate) facilitates to selectively catalyzing oxygen to generate H2O2 via a two-electron (2e) ORR pathway.
[0004] To realize 2e oxygen electroreduction, various strategies including alloying, chemical functionalization, downsizing, and single-atom engineering have been developed to regulate the physicochemical properties of the catalysts. Though substantial progress has been made, the activity and durability of reported works still cannot compete with the demand of the practical application.
[0005] In view of prior art have been shortcomings, embodiments herein relate to an alternative and highly efficient concept that introducing cationic vacancies on nickel phosphide by cation vacancy engineering, as a proof-of-concept to regulate the catalyst’s physico-chemical properties, are introduced for efficient H2O2 electrosynthesis.Summary of The Invention
[0006] A method for optimizing the catalytic performance of hydrogen peroxide (H2O2) electrocatalyst wherein the optimization method comprises: introducing cationic vacancies into the active metal matrix by cationic vacancy engineering to regulate the distance between active sites, and optimize the structure of the metal matrix, thereby improve the catalytic activity and stability of the active metal matrix as an electrocatalyst.
[0007] The optimization method according to preceding claim 1, wherein the feature comprises that as-fabricated Ni cationic vacancies (VNi) -enriched Ni2-xP-VNi electrocatalyst as a proof-of-concept, and Ni cationic vacancies induced the formation of *OOH adsorption favorable, thereby promoting charge transfer rate and redox kinetics during electrocatalysis.
[0008] The Ni cationic vacancies (VNi) -enriched Ni2-xP-VNi according to preceding claim 2, wherein the preparation method comprises in-situ phosphating the carbonized Ni-MOF using pH3 released by NaH2PO2 (puriss, 98-100%) .
[0009] The preparation method according to preceding claim 3, wherein the detailed procedure comprises as follows:
[0010] 32 mL N, N-dimethylformamide (DMF) , 2 mL ethanol, and 2 mL DI water were mixed in a 50 mL poly (tetrafluoroethylene) tube, then 0.75 mmol benzenedicarboxylic acid (BDC, 98%) was dissolved into the mixed solution with bath sonication assistance for 15 min, 0.75 mmol NiCl2·6H2O (99.9%) was added and homogenized via bath sonication for another 15 min;
[0011] the mixed solution was transferred into a 40 mL Teflon-lined stainless-steel autoclave and was subjected to hydrothermal reaction at 160 ℃ for 12 h, the as-obtained solid product (denoted as Ni-MOF) was collected via centrifugal separation at 6000 rpm and was washed with 70%ethanol under bath sonication for 10 min;
[0012] the centrifugal separation and ultrasonic washing were repeated three times to remove the unreacted BDC ligand;
[0013] the as-collected Ni-MOF was carbonized via thermal annealing at 800 ℃ at a ramping rate of 5 ℃ min–1 under the argon protection (200 sccm) ;
[0014] the carbonized solid (denoted as NiO / Ni) was placed downstream of the tube furnace and was in situ phosphatized by pH3 released from NaH2PO2 (puriss, 98-100%) at 300 ℃ (2.5 ℃ min–1) for 2h under argon protection, the as-synthesized final product was denoted as Ni2-xP-VNi.
[0015] The formation of *OOH adsorption favorable of claim 2, wherein the unique configuration comprises the end-on configuration favoring 2e ORR, which is verified by Operando X-ray absorption near-edge spectroscopy (XANES) and synchrotron Fourier transform infrared (SR-FTIR) combining theoretical calculations.Brief Description of The Drawings
[0016] FIGS. 1a-1g show a [Fig. 1a] Schematic illustration of the synthetic procedure of Ni2-xP-VNi. [Fig. 1b] HAADF-STEM image of the Ni2-xP-VNi’s local structure. [Fig. 1c] EDS-STEM element mapping image. [Fig. 1d] The atomic-scale view of the red frame region in Figure 1b. [Fig. 1e, f] The HRTEM images of the red frame region in Figure 1b. [Fig 1g] Intensity profile recorded of corresponding areas in Figure 1f.
[0017] FIGS. 2a-2f show a [Fig. 2a] The EPR spectra of Ni2-xP-VNi and pristine Ni2P. [Fig. 2b] Fourier-transform EXAFS spectra of Ni2-xP-VNi and reference samples. [Fig. 2c] Ni K-edge EXAFS fitting curves of Ni2-xP-VNi nanosheets in R-space. [Fig. 2d] Ni K-edge XANES. [Fig. 2e] Ni L-edge XANES spectra. [Fig. 2f] P L-edge XANES spectra for Ni2-xP-VNi and reference samples.
[0018] FIGS. 3a-3f show a [Fig. 3a] LSV curves of Ni2-xP-VNi, NiO / Ni, and pristine Ni2P on RRDE collected at a rotation speed of 1600 rpm and a scan rate of 5 mV s–1 in 0.1 M KOH. The H2O2 current was recorded on the ring electrode at a constant potential of 1.2 V. [Fig. 3b] H2O2 selectivity and electron transfer number calculated from the LSV curves. [Fig. 3c] LSV curves of Ni2-xP-VNi in an Ar-saturated 0.1 M KOH with 10 × 10-3 M H2O2. [Fig. 3d] Stability measurement of Ni2-xP-VNi at the constant disk and ring potentials of 0.45 and 1.2 V, respectively. [Fig. 3e] Schematical configuration of a homemade cell for bulk H2O production. [Fig. 3f] The Faradaic efficiency selectivity of Ni2-xP-VNi in various electrolytes under alkaline (0.1 M KOH, pH 12.9) , neutral (0.1 M PBS, pH 8.76) , and acidic conditions (0.5 M H2SO4, pH 0.46) .
[0019] FIGS. 4a-4d show a [Fig. 4a] Operando Ni K-edge XANES spectra of Ni2-xP-VNi at the potentials of 0.8–0.2 V. [Fig. 4b] Corresponding Fourier transform (FT) curves of Ni K-edge EXAFS k3χ (k) functions. [Fig. 4c] Operando SR-FTIR measure-ments of Ni2-xP-VNi at the potentials of 0.8-0.2 V. [Fig. 4d] Operando SR-FTIR measurements of Ni2-xP-VNi and pristine Ni2P at the potentials of 0.2 V.
[0020] FIGS. 5a-5e show a [Fig. 5a] *OOH adsorption model on three atomic configurations: i) VNi-free Ni2P, ii) Ni2-xP-VNi, and iii) NiO / Ni. [Fig. 5b] Density of states (DOS) . [Fig. 5c] d-band center of as-proposed models. [Fig. 5d] Free energy diagram of 2e ORR on all models at 0.70 V . [Fig. 5e] 2e ORR activity volcano plot, where the horizontal dashed line is the standard redox potential for 2e ORR at 0.70 V.
[0021] Specific Embodiments
[0022] Specific embodiments will now be described in detail with reference to the accompanying figures. Like elements in the various figures are denoted by like reference numerals for consistency.
[0023] In the following detailed description of embodiments, numerous specific details are set forth in order to provide a more thorough understanding.
[0024] However, it will be apparent to one of ordinary skill in the art that embodiments may be practiced without these specific details. In other instances, well-known features have not been described in detail to avoid unnecessarily complicating the description.
[0025] In the following description, any component described with regard to a figure, in various embodiments of the present disclosure, may be equivalent to one or more like-named components described with regard to any other figure.
[0026] Throughout the application, ordinal numbers (e.g., first, second, third, etc. ) may be used as an adjective for an element (i.e., any noun in the application) . The use of ordinal numbers is not to imply or create any particular ordering of the elements nor to limit any element to being only a single element unless expressly disclosed, such as by the use of the terms “before” , “after” , “single” , and other such terminology. Rather, the use of ordinal numbers is to distinguish between the elements. By way of an example, a first element is distinct from a second element, and the first element may encompass more than one element and succeed (or precede) the second element in an ordering of elements, if an ordering exists.
[0027] One or more embodiments of the present disclosure relate to methods and systems for the efficient electrosynthesis of hydrogen peroxides.
[0028] One or more embodiments of the present disclosure relate to the method for optimizing the catalytic performance of hydrogen peroxide (H2O2) electrocatalyst.
[0029] In accordance with one or more embodiments of the present disclosure, the optimized H2O2 electrocatalyst exhibits remarkable 2e ORR performance with H2O2 molar fraction of >95%and Faradaic efficiencies of >90%in all pH conditions under a wide range of applied potentials, the as-created VNi possesses superb long-term durability for over 50 h impressively, suppassing all the recently reported catalysts for H2O2 electrosynthesis.
[0030] One or more embodiments of the present disclosure may be directed towards processes for the highly efficient and large-scale synthesis of commercial-level concentrated H2O2 via a cost-effective electrocatalytic oxygen reduction route (ORR) .
[0031] One or more embodiments of the present disclosure employ the cation vacancy engineering to design the catalytic materials for H2O2 electrosynthesis, cationic vacancies on nickel phosphide, as a proof-of-concept to regulate the catalyst’s physico-chemical properties.
[0032] One or more embodiments of the present disclosure may relate to the preparation method of Ni cationic vacancies (VNi) -enriched Ni2-xP-VNi, that includes several specific steps:
[0033] 32 mL N, N-dimethylformamide (DMF) , 2 mL ethanol, and 2 mL DI water were mixed in a 50 mL poly (tetrafluoroethylene) tube, then 0.75 mmol benzenedicarboxylic acid (BDC, 98%) was dissolved into the mixed solution with bath sonication assistance for 15 min, 0.75 mmol NiCl2·6H2O (99.9%) was added and homogenized via bath sonication for another 15 min;
[0034] the mixed solution was transferred into a 40 mL Teflon-lined stainless-steel autoclave and was subjected to hydrothermal reaction at 160 ℃ for 12 h, the as-obtained solid product (denoted as Ni-MOF) was collected via centrifugal separation at 6000 rpm and was washed with 70%ethanol under bath sonication for 10 min;
[0035] the centrifugal separation and ultrasonic washing were repeated three times to remove the unreacted BDC ligand;
[0036] the as-collected Ni-MOF was carbonized via thermal annealing at 800 ℃ at a ramping rate of 5 ℃ min–1 under the argon protection (200 sccm) ;
[0037] the carbonized solid (denoted as NiO / Ni) was placed downstream of the tube furnace and was in situ phosphatized by pH3 released from NaH2PO2 (puriss, 98-100%) at 300 ℃ (2.5 ℃ min–1) for 2h under argon protection, the as-synthesized final product herein was denoted as Ni2-xP-VNi.
[0038] One or more embodiments of the present disclosure may contains a verification of the end-on configuration favoring 2e ORR, which is verified by Operando X-ray absorption near-edge spectroscopy (XANES) and synchrotron Fourier transform infrared (SR-FTIR) combining theoretical calculations.
[0039] The optimization method of electrocatalyst in the electro-synthesis of H2O2 can be determined according to the actual situation. That is to say, in the electrocatalytic synthesis of H2O2, there are many kinds of active metal electrocatalysts. No matter what kind of active metal electrocatalyst is used, as long as it introduces cationic vacancies to regulate the distance between active sites, better catalytic properties can be achieved.
Claims
1.A method for optimizing the catalytic performance of hydrogen peroxide (H2O2) electrocatalyst wherein the optimization method comprises: introducing cationic vacancies into the active metal matrix by cationic vacancy engineering to regulate the distance between active sites, and optimize the structure of the metal matrix, thereby improve the catalytic activity and stability of the active metal matrix as an electrocatalyst.2.The optimization method according to preceding claim 1, wherein the feature comprises that as-fabricated Ni cationic vacancies (VNi) -enriched Ni2-xP-VNi electrocatalyst as a proof-of-concept, and Ni cationic vacancies induced the formation of *OOH adsorption favorable, thereby promoting charge transfer rate and redox kinetics during electrocatalysis.3.The Ni cationic vacancies (VNi) -enriched Ni2-xP-VNi according to preceding claim 2, wherein the preparation method comprises in-situ phosphating the carbonized Ni-MOF using pH3 released by NaH2PO2 (puriss, 98-100%) .4.The preparation method according to preceding claim 3, wherein the detailed procedure comprises as follows:(1) 32 mL N, N-dimethylformamide (DMF) , 2 mL ethanol, and 2 mL DI water were mixed in a 50 mL poly (tetrafluoroethylene) tube, then 0.75 mmol benzenedicarboxylic acid (BDC, 98%) was dissolved into the mixed solution with bath sonication assistance for 15 min, 0.75 mmol NiCl2·6H2O (99.9%) was added and homogenized via bath sonication for another 15 min;(2) the mixed solution was transferred into a 40 mL Teflon-lined stainless-steel autoclave and was subjected to hydrothermal reaction at 160 ℃ for 12 h, the as-obtained solid product (denoted as Ni-MOF) was collected via centrifugal separation at 6000 rpm and was washed with 70%ethanol under bath sonication for 10 min;(3) the centrifugal separation and ultrasonic washing were repeated three times to remove the unreacted BDC ligand;(4) the as-collected Ni-MOF was carbonized via thermal annealing at 800 ℃ at a ramping rate of 5 ℃ min–1 under the argon protection (200 sccm) ;(5) the carbonized solid (denoted as NiO / Ni) was placed downstream of the tube furnace and was in situ phosphatized by pH3 released from NaH2PO2 (puriss, 98-100%) at 300 ℃ (2.5 ℃ min–1) for 2h under argon protection, the as-synthesized final product was denoted as Ni2-xP-VNi.5.The formation of *OOH adsorption favorable of claim 2, wherein the unique configuration comprises the end-on configuration favoring 2e ORR, which is verified by Operando X-ray absorption near-edge spectroscopy (XANES) and synchrotron Fourier transform infrared (SR-FTIR) combining theoretical calculations.
Citation Information
Patent Citations
Method for preparing porous Ni2P / C electrode based on two-dimensional metal organic framework template
CN109055975A
Preparation and application of MOF-guided nickel-cobalt bimetallic phosphide
CN111111716A
Oxidation catalyst based on MOF-derived non-noble metal phosphide / carbon composite hydrazine as well as preparation method and application of oxidation catalyst
CN113948727A
Catalyst for generating hydrogen peroxide and preparation method thereof
CN114144258A
Preparation method of phosphide with bimetal organic framework structure
CN114807965A