Preparation system and preparation process for producing flexible circuit board by laser cutting
By using laser cutting technology and protective layer treatment in the production of flexible circuit boards, the chemical reaction problem between copper foil and etching liquid is solved, processing convenience and environmental protection performance are improved, and product performance and service life are improved.
Patent Information
- Application Number
- PCT/CN2023/100364
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-18
- Filing Date
- 2023-06-15
- Publication Date
- 2024-11-21
AI Technical Summary
In the existing flexible circuit board production process, the chemical reaction between copper foil and etching liquid leads to chemical waste pollution and metal waste, increasing production costs and environmental pollution.
The flexible circuit board is produced using laser cutting technology. By applying protective layer to the copper foil base layer and using protective film and thermal adhesive film layers during laser etching and hot pressing, it reduces chemical reactions and pollution, improves processing convenience and Environmentally friendly performance.
The processing convenience and environmental protection performance of flexible circuit boards are optimized, the performance and service life of products are improved, and the production and treatment costs of chemical waste are reduced.
Smart Images

Figure CN2023100364_21112024_PF_FP_ABST
Abstract
Description
Preparation system and process for producing flexible circuit boards using laser cutting Technical Field
[0001] The present invention relates to the field of new energy semiconductor technology, and in particular to a preparation system and preparation process for producing flexible circuit boards using laser cutting, and is targeted at flexible laser direct circuit board (LDC) direct forming products. Background Art
[0002] Flexible Laser Direct Circular (LDC), also known as soft printed circuits or flexible printed circuits, is highly sought after for its lightweight, thin, and flexible properties. Flexible printed circuits offer high reliability and exceptional flexibility. By embedding circuit designs onto thin, flexible plastic sheets, they enable the integration of numerous precision components within confined spaces, creating a flexible, flexible circuit. Flexible printed circuits can be bent and folded freely, are lightweight, compact, offer excellent heat dissipation, and are easy to install, revolutionizing traditional interconnect technologies. The materials used in flexible circuit construction are insulating films, conductors, and adhesives.
[0003] One of the main processes in the existing flexible circuit board production is development-etching-stripping. Development is to remove the covering film of the non-circuit area on the copper foil flexible circuit board to expose the covering film of the circuit area. The copper foil in the non-circuit area is then etched with an etching solution to react and remove the unnecessary copper. The predetermined track is then processed on the flexible circuit board. Finally, the covering film is stripped off and the etched flexible circuit board is cleaned and dried. For example, the existing patent: CN201711203417.8, discloses a FPC flexible wireless charging transmission coil module manufacturing process; a FPC flexible wireless charging transmission coil module manufacturing process, including the following steps, S1: preparing pure copper foil for processing and cleaning the copper foil processing surface; S2: using laser etching to etch a groove on the copper foil surface prepared in step S1; S3: etching a channel; after the groove processing is completed in step S2, a channel is engraved on the copper foil processing surface; S4: pre-treating the copper foil after the processing in step S3; S5: pressing a substrate on the surface of the copper foil; S6: further etching the other end face of the pressed copper foil relative to the substrate.
[0004] However, this processing method causes the copper foil in the FPC to react chemically with the etching solution during etching, thereby generating chemical waste. If directly discharged, it will cause heavy metal pollution and the metal in the chemical waste will be wasted. However, if the metal in the chemical waste is recovered, it will cost a high cost to recycle and treat the pollution emissions, thereby increasing production costs.
[0005] Summary of the Invention
[0006] The present invention overcomes the shortcomings of the existing technology and provides a preparation system and preparation process for producing flexible circuit boards using laser cutting. Flexible circuit boards can be produced by laser processing, thereby optimizing the processing convenience and environmental performance of flexible circuit boards and improving the product performance and service life of flexible circuit boards.
[0007] To achieve the above object, the technical solution adopted by the present invention is: a preparation process for producing a flexible circuit board by laser cutting, comprising the following steps:
[0008] S1. Loading and attaching a protective layer; importing a copper foil base layer and attaching a protective layer to the upper and lower surfaces of the copper foil base layer;
[0009] S2. Laser cutting the semi-finished product after step S1 into the circuit structure;
[0010] S3. The semi-finished product after step S2 is subjected to waste treatment, active cleaning and hot pressing of false stickers;
[0011] S4. The semi-finished product after step S3 is subjected to combined hot pressing;
[0012] S5. Perform a window opening operation on the semi-finished product processed in step S4 to expose the solder joints of the copper foil base layer.
[0013] In a preferred embodiment of the present invention, in step S1, the protective layer includes a matte film, a double-layer protective film, or a single-layer protective film;
[0014] The double-layer protective film is used as the substrate, the copper foil base layer is laminated to the upper surface of the double-layer protective film, the matte film is laminated on the copper foil base layer, and the single-layer protective film is laminated on the lower side of the double-layer protective film.
[0015] In a preferred embodiment of the present invention, in step S3, the matte film, copper foil waste, and single-layer protective film of the semi-finished product after processing in step S2 are removed; then, the outer surface of the copper foil base layer in the semi-finished product is actively cleaned and the upper covering film and the upper protective film are sequentially attached to the upper surface of the copper foil base layer from the inside to the outside; then, the lower layer of the semi-finished product is false hot pressed; the false hot pressing temperature is 60-130°C.
[0016] In a preferred embodiment of the present invention, in step S3, the double-layer protective film on the lower layer of the semi-finished product after the lower layer is falsely hot-pressed is removed; then, the lower surface of the copper foil base layer in the semi-finished product is actively cleaned and the lower covering film and the lower protective film are sequentially attached to the lower surface of the copper foil base layer from the inside to the outside; then, the upper layer of the semi-finished product is falsely hot-pressed; the false hot-pressing temperature is 60-130°C.
[0017] In a preferred embodiment of the present invention, in step S3, the upper and lower sides of the semi-finished product with the upper covering film and the upper protective film and the lower covering film and the lower protective film respectively attached to both sides are hot pressed; the hot pressing temperature is 60-130°C.
[0018] In a preferred embodiment of the present invention, in step S4, the upper protective film and the lower protective film of the semi-finished product processed in step S3 are removed; then the upper auxiliary hot pressing film and the lower auxiliary hot pressing film are respectively attached to the upper and lower sides, and then the finished product hot pressing operation is performed, and the upper auxiliary hot pressing film and the lower auxiliary hot pressing film on the semi-finished product after the finished product hot pressing operation are removed; wherein, the finished product hot pressing temperature is 120-200°C, the pressure range is 70-150kg, and the time is 120-180 seconds.
[0019] In a preferred embodiment of the present invention, the system for producing flexible circuit boards using laser cutting according to claim 4 is characterized in that: after step S5, it also includes S6, in which the semi-finished product processed in step S5 is photographed and transmitted to an imaging mechanism for inspection, and then the inspected finished product is coded and discharged.
[0020] In a preferred embodiment of the present invention, a method for preparing a flexible laser circuit board is adopted. The flexible laser circuit board preparation system includes a loading and pre-lamination module, a laser etching module, a waste discharge active cleaning and false lamination hot pressing module, a combined hot pressing module, a laser window opening module, and a waste discharge marking and inspection discharge module, which are arranged in sequence according to the process.
[0021] After the copper foil base layer is introduced into the loading and pre-lamination module, the operation of step S1 is performed;
[0022] The semi-finished product processed in step S1 is led out from the loading and pre-lamination module and transferred to the laser etching module to perform the operation of step S2;
[0023] Then the semi-finished product processed in step S1 is led out from the laser etching module and transferred to the waste discharge active cleaning false sticker hot pressing module to perform the operation of step S3;
[0024] Then, the semi-finished product processed in step S3 is led out from the waste discharge and false pasting hot pressing module and transferred to the combined hot pressing module to perform the operation of step S4;
[0025] Then, the semi-finished product processed in step S4 is led out from the combined hot pressing module and transferred to the laser window opening module to perform the operation of step S5;
[0026] Then, the semi-finished product processed in step S5 is led out from the laser window opening module and transferred to the waste discharge, marking, inspection and discharging module to perform the operation of step S6.
[0027] In a preferred embodiment of the present invention, the loading and pre-laminating module includes a conveying passage 1 and a plurality of unloading rollers 1 and film tearing rollers 1 corresponding to the conveying passage 1, and the conveying passage 1 is further provided with a suction mechanism 1;
[0028] Or / and, the laser etching module includes a second conveying passage, a first suction conveying platform is provided on the second conveying passage, and a laser etching machine corresponding to the first suction conveying platform is provided on the first suction conveying platform;
[0029] Or / and, the waste discharge fake sticker hot pressing module includes a transmission path three, and several discharge rollers three and film tearing rollers three corresponding to the transmission path three, as well as a lower layer hot pressing roller group for realizing false hot pressing of the lower layer, an upper layer hot pressing roller group for realizing false hot pressing of the upper layer, and a double-sided hot pressing roller group for realizing hot pressing on both the upper and lower sides.
[0030] Or / and, the combined hot pressing module includes a conveying passage four, and a plurality of material discharge rollers four and film tearing rollers four corresponding to the conveying passage four, and a split finished product hot pressing mechanism for achieving finished product hot pressing;
[0031] Or / and, the laser window opening module includes a transmission path five, and a laser window opening machine corresponding to the transmission path five;
[0032] Or / and, the waste discharge marking verification and discharging module includes a transmission path six, and an image verification mechanism, a coding mechanism, and a plurality of waste discharge rollers six corresponding to the transmission path six;
[0033] 10. The system for producing flexible printed circuit boards using laser cutting according to claim 6, characterized in that:
[0034] The matte film comprises a polyester film, a heat-resistant base film is provided on the polyester film, and a high-temperature resistant adhesive layer is provided between the polyester film and the heat-resistant base film;
[0035] Or / and, the double-layer protective film comprises a base film and a polyester film, and a high-temperature resistant adhesive layer is provided between the base film and the bottom film;
[0036] Or / and, the lower covering film and the upper covering film are made of a heat-sensitive adhesive film layer;
[0037] or / and, a lower protective film and an upper protective film, wherein the lower protective film, the upper protective film and the single-layer protective film use a polyester film as a base material and are coated with an acrylic adhesive layer on one side;
[0038] Or / and, the upper auxiliary hot pressing film and the lower auxiliary hot pressing film use polyester film as a base material and are coated with a release agent layer on both sides.
[0039] The present invention solves the defects existing in the background technology:
[0040] The present invention discloses a preparation system and preparation process for producing flexible circuit boards using laser cutting. The target product is a flexible laser direct circuit board (LDC). The present invention can produce flexible circuit boards by laser cutting, optimizes the processing convenience and environmental performance of flexible circuit boards, and improves the product performance and service life of flexible circuit boards. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] The present invention will be further described below with reference to the accompanying drawings and examples.
[0042] FIG1 is a process flow chart 1 of a preferred embodiment of the present invention;
[0043] FIG2 is a process flow chart 2 of a preferred embodiment of the present invention;
[0044] FIG3 is a schematic structural diagram of a loading and pre-lamination module and a laser etching module according to a preferred embodiment of the present invention;
[0045] FIG4 is a schematic structural diagram of a waste discharge and false pasting hot pressing module according to a preferred embodiment of the present invention;
[0046] FIG5 is a schematic structural diagram of a combined hot pressing module according to a preferred embodiment of the present invention;
[0047] FIG6 is a schematic structural diagram of a laser window opening module according to a preferred embodiment of the present invention;
[0048] FIG7 is a waste discharge marking and verification discharge module of a preferred embodiment of the present invention;
[0049] FIG8 is a comparison of the appearance of a preferred embodiment of the present invention and the prior art;
[0050] 9 is a peeling performance test table of a preferred embodiment of the present invention;
[0051] FIG10 is a graph showing the peeling performance of a preferred embodiment of the present invention;
[0052] FIG11 is a conductivity performance test table of a preferred embodiment of the present invention;
[0053] 12 is a preferred embodiment of the present invention, the circuit fuse (FUSE) overcurrent and fuse test;
[0054] 13 is a state diagram of a product produced by a preferred embodiment of the present invention undergoing a tin-bleaching test;
[0055] FIG14 is a schematic cross-sectional view of the layer structure of the product produced according to the present invention;
[0056] In the figure: feeding pre-lamination module, 11-double-layer protective film discharge roller, 13-copper foil base discharge roller, 14-matt film discharge roller, 16-single-layer protective film discharge roller, 2-laser etching module, 3-waste discharge false lamination hot pressing module, 31-waste tape discharge roller, 32-product waste film tearing roller, 33-upper cover film discharge roller, 35-upper protective film discharge roller, 37-lower protective film discharge roller, 38-lower cover film discharge roller, 39-double-layer protective film waste tearing roller Film roller, 310-single-layer protective film waste tearing roller, 311-matt film waste tearing roller, 4-combined hot pressing module, 41-upper protective film waste tearing roller, 42-lower protective film waste tearing roller, 43-lower auxiliary hot pressing film discharge roller, 44-upper auxiliary hot pressing film discharge roller, 45-upper auxiliary hot pressing film tearing roller, 46-lower auxiliary hot pressing film tearing roller, 5-laser window opening module, 6-waste discharge, marking and calibration discharge module, a-copper foil base layer, b-CVL layer. DETAILED DESCRIPTION
[0057] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments. These drawings are simplified schematic diagrams that only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.
[0058] Example 1
[0059] As shown in Figures 1 to 7, a process for producing a flexible circuit board using laser printing includes the following steps:
[0060] S1. Loading and attaching a protective layer: A copper foil base layer is introduced, and protective layers are laminated to the upper and lower surfaces of the copper foil base layer. In step S1, the protective layer comprises a matte film, a double-layer protective film, or a single-layer protective film. Specifically, the double-layer protective film is used as the substrate, the copper foil base layer is laminated to the upper surface of the double-layer protective film, the matte film is laminated above the copper foil base layer, and the single-layer protective film is laminated to the lower side of the double-layer protective film.
[0061] S2. Laser printing and cutting the semi-finished product processed in step S1 to obtain a circuit structure.
[0062] S3. The semi-finished product after step S2 is subjected to waste treatment, active cleaning and hot pressing.
[0063] Specifically, after step S2, the semi-finished product is subjected to the removal of the matte film, the copper foil waste, and the single-layer protective film; then, the outer surface of the copper foil base layer in the semi-finished product is actively cleaned, and the upper covering film and the upper protective film are sequentially attached to the upper surface of the copper foil base layer from the inside to the outside; then, the semi-finished product is subjected to false hot pressing of the lower layer; the false hot pressing temperature of the lower layer is 60-130°C, and the other side is pressed at room temperature. The double-layer protective film of the lower layer of the semi-finished product after the false hot pressing of the lower layer is removed; then, the lower surface of the copper foil base layer in the semi-finished product is actively cleaned, and the lower covering film and the lower protective film are sequentially attached to the lower surface of the copper foil base layer from the inside to the outside; then, the semi-finished product is subjected to false hot pressing of the upper layer; the false hot pressing temperature of the upper layer is 60-130°C, and the other side is pressed at room temperature. The upper and lower sides of the semi-finished product with the upper covering film and the upper protective film and the lower covering film and the lower protective film attached on both sides are hot pressed; the hot pressing temperature of the upper and lower sides is 60-130°C. Furthermore, the active cleaning adopts plasma cleaning. The operation in step S2 is convenient for removing bubbles in the semi-finished product.
[0064] S4. Hot-press the semi-finished product after step S3. In step S4, remove the upper and lower protective films of the semi-finished product after step S3. Then, apply the upper and lower auxiliary hot-pressing films to the upper and lower sides of the semi-finished product, respectively, and then perform the hot-pressing operation on the finished product. The upper and lower auxiliary hot-pressing films on the semi-finished product after the hot-pressing operation are removed. The hot-pressing temperature of the finished product is 120-200°C, and the pressure range is 70-150kg.
[0065] S5. Perform a window opening operation on the semi-finished product processed in step S4 to expose the solder joints of the copper foil base layer.
[0066] After step S5, the process further includes step S6, in which the semi-finished product processed in step S5 is photographed and transmitted to an imaging device for inspection, and then the inspected finished product is coded and discharged. The inspection by the imaging device includes inspecting the product appearance through image comparison or observation.
[0067] Example 2
[0068] On the basis of the first embodiment, the matte film includes a polyester film, a heat-resistant base film is provided on the polyester film, and a high-temperature resistant adhesive layer is provided between the polyester film and the heat-resistant base film.
[0069] Alternatively, the double-layer protective film comprises a base film and a polyester film, with a high-temperature-resistant adhesive layer disposed between the base film and the bottom film. This serves as a carrier for conveying the copper foil substrate, facilitates lamination force during lamination, removes air bubbles, strengthens the copper foil substrate during production, and protects the product surface from scratches and contamination.
[0070] Alternatively, the lower and upper cover films may be thermally sensitive adhesive films. Alternatively, the thermally sensitive adhesive films may be conventional thermally sensitive adhesive films. The lower and upper cover films are combined and hot-pressed to form a CVL layer that wraps around the copper foil base layer.
[0071] or / and, a lower protective film and an upper protective film, wherein the lower protective film, the upper protective film, and the single-layer protective film are based on a polyester film and coated on one side with an acrylic adhesive layer. The lower protective film and the upper protective film serve to enhance the hardness of the product during production and protect the product surface from scratches and dirt.
[0072] Alternatively, the upper and lower auxiliary hot pressing films may be formed from polyester film and coated with a release agent on both sides. The upper and lower auxiliary hot pressing films may have anti-stick properties to prevent the product from adhering to the laminating plate of the laminating equipment after hot pressing.
[0073] Example 3
[0074] As shown in Figures 1 to 7, based on Example 1 or Example 2, a flexible laser circuit board preparation system is used, and the flexible laser circuit board preparation system includes a loading and pre-lamination module 1, a laser etching module 2, a waste discharge and false lamination hot pressing module 3, a combined hot pressing module 4, a laser window opening module 5, and a waste discharge, marking, and verification discharge module 6, which are arranged in sequence according to the process.
[0075] The loading and pre-laminating module 1 includes a conveyor path 1 and several corresponding unloading rollers 1 and film tearing rollers 1. The conveyor path 1 is also provided with a suction mechanism 1. After the copper foil substrate is introduced into the loading and pre-laminating module 1, step S1 is performed.
[0076] Specifically, the first unloading rollers include a copper foil base unloading roller 13 and a matte film unloading roller 14, located above the conveyor path in the order of conveyance, as well as a double-layer protective film unloading roller 11 located on the loading side of the conveyor path, and a single-layer protective film unloading roller 16 located below the conveyor path. The first unloading rollers are used to remove waste from the double-layer protective film raw material and the matte film raw material, respectively. This arrangement ensures that the copper foil base is always carried on the protective layer and transported to the next process, improving processing fluidity and convenience.
[0077] Laser etching module 2 includes a second conveyor path, on which is disposed a first suction conveyor platform. A laser etching machine corresponding to the first suction conveyor platform is disposed on the first suction conveyor platform. The semi-finished product processed in step S1 is drawn from loading and pre-laminating module 1 and conveyed to laser etching module 2 for step S2.
[0078] The waste removal and dummy labeling hot pressing module 3 includes a conveyor path 3, a number of corresponding discharge rollers 3 and film tearing rollers, as well as a lower hot pressing roller group for performing dummy hot pressing on the lower layer, an upper hot pressing roller group for performing dummy hot pressing on the upper layer, and a double-sided hot pressing roller group for performing hot pressing on both the upper and lower sides. The semi-finished product processed in step S1 is transferred from the laser etching module 2 to the waste removal and dummy labeling hot pressing module 3 for step S3.
[0079] Specifically, the plurality of discharge rollers (3) and the plurality of film tearing rollers (3) include a dummy film waste tearing roller 311, a waste tape discharge roller 31, a product waste tearing roller 32, an upper cover film discharge roller 33, and an upper protective film discharge roller 35, located above the conveyor path 4; and a single-layer protective film waste tearing roller 310, a double-layer protective film waste tearing roller 39, a lower cover film discharge roller 38, and a lower protective film discharge roller 37, located below the conveyor path 4. The upper hot-pressing roller group comprises upper and lower rollers arranged side by side, capable of opposing pressure, and the upper rollers are heated. The lower hot-pressing roller group comprises upper and lower rollers arranged side by side, capable of opposing pressure, and the lower rollers are heated.
[0080] The combined hot pressing module 4 includes a conveyor path 4, a plurality of discharge rollers 4 and film tearing rollers 4 corresponding to the conveyor path 4, and a split-type hot pressing mechanism for hot pressing the finished product. The semi-finished product after step S3 is drawn from the waste discharge hot pressing module 3 and transferred to the combined hot pressing module 4 for step S4.
[0081] Specifically, the plurality of film tearing rollers four and the discharge rollers four respectively include an upper protective film waste tearing roller 41, an upper auxiliary hot pressing film discharge roller 44, and an upper auxiliary hot pressing film tearing roller 45 arranged above the conveying path four; and a lower protective film waste tearing roller 42, a lower auxiliary hot pressing film discharge roller 43, and a lower auxiliary hot pressing film tearing roller 46 arranged below the conveying path four.
[0082] The laser window opening module 5 includes a conveyor channel 5 and a laser window opening machine corresponding to the conveyor channel 5. The semi-finished product after step S4 is drawn out from the combined hot pressing module 4 and conveyed to the laser window opening module 5 for step S5. During the window opening operation, the solder joints of the copper foil base layer are exposed by laser etching.
[0083] The waste discharge, marking, verification, and discharging module 6 includes a conveyor path 6, an image verification mechanism, a coding mechanism, and several waste discharge rollers 6 corresponding to the conveyor path 6. The semi-finished product processed in step S5 is guided out of the laser window opening module 5 and transferred to the waste discharge, marking, verification, and discharging module 6 for step S6.
[0084] Working principle:
[0085] As shown in Figures 1 to 7, a preparation system and preparation process for producing flexible circuit boards using laser cutting are targeted at flexible laser direct circuit boards (LDC). The present invention can produce flexible circuit boards by laser cutting, optimizes the processing convenience and environmental performance of flexible circuit boards, and improves the product performance and service life of flexible circuit boards. In the production process of the present invention, the copper foil base layer carried between the double-layer protective film and the matt film is conveyed to the workstations of step S2 and step S3 together by using a matt film, a double-layer protective film, and a single-layer protective film as carriers during the conveying process from step S1 to step S2. In step S3, the matt film and the single-layer protective film are removed, and then the covering film and the upper protective film are affixed. The double-layer protective film is then removed and the lower covering film and the lower protective film are affixed. On the one hand, this facilitates the conveying of processing, and on the other hand, the lower protective film and the upper protective film can enhance the hardness of the product during the production process and protect the surface of the product from risks such as scratches and dirt. During subsequent hot pressing, auxiliary hot pressing films and lower auxiliary hot pressing films are affixed to the outer sides of the upper and lower cover films to provide anti-stick properties, preventing the product from adhering to the pressing plate after hot pressing. Simultaneously, the upper and lower cover films on the outer sides of the copper foil base layer after hot pressing are heated to form a CVL layer attached to the outer side of the copper foil base layer, wherein the CVL (coverlay, abbreviated as "CVL"). The product produced by the technical solution of the present invention includes a copper foil base layer and a CVL layer attached to the outer side of the copper foil base layer, and the corresponding solder joints of the copper foil base layer in the product are exposed to the CVL layer.
[0086] As shown in Figure 8, the preferred embodiment of the present invention exhibits a clear and smooth appearance compared to conventional flexible circuit boards, with no notches or blackened circuit edges, and no metal particles on the surface. However, conventional circular die-cutting methods can result in fuses being unable to be die-cut, resulting in indentations and collapsed edges on the circuit edges, and puncture risk through skin analysis.
[0087] The peel performance of the product produced by the technical solution of the present invention is shown in Figure 9. A 180-degree peel strength test was conducted on the CVL layer and the copper foil base layer of the product produced by the technical solution of this application using a tensile tester. This test involves the CVL layer peeling in a U-shaped direction relative to the copper foil base layer. The test chart shown in Figure 9 and the corresponding peel performance curve shown in Figure 10 indicate that the test standard is >1000gf / cm, and the actual average value is 1514gf / cm, which meets the test standard for flexible circuit board peel resistance.
[0088] The conductivity performance of products produced using the technical solution of the present invention was tested using a constant current source, as shown in the conductivity performance test table in Figure 11. The test parameters used 1A and 7A constant current sources. The fuse status of the copper foil substrate in the product was determined by determining the maximum fuse duration at 7A, with a maximum duration of 0.72 seconds. At 1A, the overcurrent duration was consistently over 300 seconds.
[0089] Figure 12 shows photographs of each stage of the solder float test for a product produced using the technical solution of the present invention. The product was placed in a lead-free solder bath at 260±5°C and immersed for 10±1 seconds. The product was then tested, and the copper foil substrate circuit bonded well to the CVL layer, showing no peeling or bubbles. The solder pad coverage was ≥95%.
[0090] The product produced by the technical solution of the present invention was subjected to a bending test with 5000 bending times and an angle of ±135°. The circuit of the copper foil substrate of the product produced by the present invention was well bonded to the CVL without separation, cracking or open circuit; and the change in normal resistance after bending was less than 20%.
[0091] Products produced using the technical solution of the present invention were subjected to thermal shock testing. The products were placed in a thermal shock test chamber. The test conditions were: -40°C for 45 minutes, 125°C for 45 minutes, and 100 cycles. The copper foil substrates of the products produced by the present invention exhibited good bonding between the circuit and the CVL, with no separation, cracking, or open circuits. The copper foil substrates also exhibited normal conduction after bending, with a resistance change of less than 20%.
[0092] Products produced using the technical solution of the present invention were subjected to constant temperature and humidity testing in a constant temperature and humidity test chamber. The test conditions were 85±2°C, 85±2% RH, and 1008 hours. The copper foil substrate of the product exhibited good bonding between the circuit and the CVL, with no separation, cracking, or open circuits. The copper foil substrate also exhibited normal conduction after bending, with a resistance change of less than 20%.
[0093] The salt spray test of the product produced by the technical solution of the present invention was carried out by placing the product produced by the present invention into a salt spray tester (model: AOS-108); the test conditions were: temperature 35±2°C, saturated barrel temperature 47±2°C; solution solubility 50g / L±5g / L NaCl, solution pH value: 6.5-7.2; salt spray deposition: 1-2ml / 80CM per hour 2 The test time is 48 hours. After the test, the product is tested and the circuit conduction of the product is normal.
[0094] Based on the ideal embodiments of the present invention, and with reference to the above description, relevant personnel can make various changes and modifications without departing from the technical scope of the present invention. The technical scope of the present invention is not limited to the contents of the specification, but must be determined according to the scope of the claims.
Claims
1. A process for producing a flexible circuit board by laser cutting, characterized in that: The following steps are involved: S1. Loading and attaching a protective layer; importing a copper foil base layer, and attaching a protective layer to the upper and lower surfaces of the copper foil base layer; S2. Laser cutting the circuit structure of the semi-finished product after step S1; S3. The semi-finished product after step S2 is subjected to waste treatment, active cleaning and hot pressing; S4. Combination hot pressing of the semi-finished product after step S3; S5. Perform window opening operation on the semi-finished product processed in step S4 to expose the solder joints of the copper foil base layer.
2. The process for producing a flexible printed circuit board by laser cutting according to claim 4, characterized in that: In step S1, the protective layer includes a dumb film or a double-layer protective film or a single-layer protective film; The double-layer protective film is used as the substrate, the copper foil base layer is laminated to the upper surface of the double-layer protective film, the matte film is laminated on the copper foil base layer, and the single-layer protective film is laminated on the lower side of the double-layer protective film.
3. The process for producing a flexible printed circuit board by laser cutting according to claim 2, characterized in that: In step S3, the semi-finished product after the processing in step S2 is subjected to the removal of the matte film, the copper foil waste, and the single-layer protective film; then, the outer surface of the copper foil base layer in the semi-finished product is actively cleaned and the upper covering film and the upper protective film are sequentially attached to the upper surface of the copper foil base layer from the inside to the outside; then, the lower layer of the semi-finished product is subjected to false hot pressing; the false hot pressing temperature is 60-130°C.
4. The process for producing a flexible printed circuit board by laser cutting according to claim 2, characterized in that: In step S3, the double-layer protective film of the lower layer of the semi-finished product after the lower layer false hot pressing is peeled off; then the lower surface of the copper foil base layer in the semi-finished product is actively cleaned and the lower covering film and the lower protective film are sequentially attached to the lower surface of the copper foil base layer from the inside to the outside; then the upper layer of the semi-finished product is false hot pressed; the false hot pressing temperature is 60-130°C.
5. The process for producing a flexible printed circuit board by laser cutting according to claim 2, characterized in that: In step S3, the upper and lower sides of the semi-finished product with the upper covering film and the upper protective film and the lower covering film and the lower protective film respectively attached to both sides are hot pressed; the hot pressing temperature is 60-130°C.
6. The process for producing a flexible printed circuit board by laser cutting according to claim 2, characterized in that: In step S4, the upper protective film and the lower protective film of the semi-finished product processed in step S3 are peeled off; then the upper auxiliary hot pressing film and the lower auxiliary hot pressing film are respectively attached to the upper and lower sides, and then the finished product hot pressing operation is performed, and the upper auxiliary hot pressing film and the lower auxiliary hot pressing film on the semi-finished product after the finished product hot pressing operation are peeled off; wherein, the finished product hot pressing temperature is 120-200°C, the pressure range is 70-150kg, and the time is 120-180 seconds.
7. The process for producing a flexible printed circuit board by laser cutting according to claim 4, characterized in that: The process further includes S6 after step S5. In step S6, the semi-finished product processed in step S5 is photographed and transmitted to an image mechanism for inspection, and then the inspected finished product is coded and discharged.
8. The process for producing a flexible circuit board by laser cutting according to claim 4, characterized in that: A flexible laser circuit board preparation system is used, and the flexible laser circuit board preparation system includes a feeding pre-lamination module, a laser etching module, a waste discharge active cleaning false lamination hot pressing module, a combined hot pressing module, a laser window opening module, and a waste discharge marking inspection and discharging module which are arranged in sequence according to the process; After the copper foil base layer is introduced into the loading and pre-lamination module, the operation of step S1 is performed; The semi-finished product processed in step S1 is led out from the feeding and pre-laminating module and transferred to the laser etching module to perform the operation of step S2; Then the semi-finished product processed in step S1 is led out from the laser etching module and transferred to the waste discharge active cleaning dummy sticker hot pressing module to perform the operation of step S3; Then the semi-finished product processed in step S3 is led out from the waste discharge and false sticker hot pressing module and transferred to the combined hot pressing module to perform the operation of step S4; Then the semi-finished product processed in step S4 is led out from the combined hot pressing module and transferred to the laser window opening module to perform the operation of step S5; Then, the semi-finished product processed in step S5 is led out from the laser window opening module and transferred to the waste discharge marking inspection and discharging module to perform the operation of step S6.
9. The process for producing a flexible printed circuit board by laser cutting according to claim 9, characterized in that: The feeding and pre-film laminating module comprises a conveying passage 1 and a plurality of unloading rollers 1 and film tearing rollers 1 corresponding to the conveying passage 1, and a suction mechanism 1 is also arranged on the conveying passage 1; Or / and, the laser etching module comprises a second conveying passage, a first suction conveying platform is arranged on the second conveying passage, and a laser etching machine corresponding to the first suction conveying platform is arranged on the first suction conveying platform; Or / and, the waste discharge fake sticker hot pressing module includes a conveying passage three, and a plurality of material discharge rollers three and film tearing rollers three corresponding to the conveying passage three, as well as a lower layer hot pressing roller group for realizing fake hot pressing of the lower layer, an upper layer hot pressing roller group for realizing fake hot pressing of the upper layer, and a double-sided hot pressing roller group for realizing hot pressing on both the upper and lower sides. Or / and, the combined hot pressing module includes a conveying passage four, and a plurality of material discharge rollers four and film tearing rollers four corresponding to the conveying passage four, and a split finished product hot pressing mechanism for realizing hot pressing of finished products; Or / and, the laser window opening module includes a transmission path five, and a laser window opening machine corresponding to the transmission path five; Or / and, the waste discharge marking verification and discharging module includes a conveying passage six, and an image mechanism verification mechanism, a coding mechanism, and a plurality of waste discharge rollers six corresponding to the conveying passage six; 10. The process for producing a flexible printed circuit board by laser cutting according to claim 6, characterized in that: The matte film comprises a polyester film, a heat-resistant base film is arranged on the polyester film, and a high-temperature resistant adhesive layer is arranged between the polyester film and the heat-resistant base film; Or / and, the double-layer protective film comprises a base film and a polyester film, and a high-temperature resistant adhesive layer is provided between the base film and the bottom film; Or / and, the lower covering film and the upper covering film are made of a heat-sensitive adhesive film layer; or / and, a lower protective film and an upper protective film, wherein the lower protective film and the upper protective film are The protective film is made of polyester film as the base material, and is coated with an acrylic adhesive layer on one side; Or / and, the upper auxiliary hot pressing film and the lower auxiliary hot pressing film use a polyester film as a base material, and are coated with a release agent layer on both sides.
Citation Information
Patent Citations
Processing method for rigid-flex board by using pure glue semi-pressing
CN110446371A
Wireless charging coil plate surface cover film laminating method
CN112074087A
FPC die cutting production method
CN114900965A
Production method of aluminum-based film-coated plate for LED (light-emitting diode)
CN115413134A
Rapid FPC production process of full dry process
CN115580990A
Cited By
Lens module base processing technology
CN119388668A