Absorption product and preparation method therefor
Through the reaction of modified acrylate and acrylic monomer and the porous structure design, the problem of slow absorption and re-seepage of traditional sanitary napkin absorber core is solved, faster liquid transmission and prevent blood accumulation, and improved the absorption of sanitary napkin Performance and comfort.
Patent Information
- Application Number
- PCT/CN2024/091435
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-18
- Filing Date
- 2024-05-07
- Publication Date
- 2024-11-21
AI Technical Summary
The absorbent core of traditional liquid sanitary napkins is prone to accumulate blood clots when menstrual blood penetrates, resulting in slow absorption, lateral leakage and re-seepage, which cannot meet the comfort needs of women during menstruation.
The modified acrylic acid ester with hyperbranched structure reacts with acrylic monomer to form an absorbent core with stronger absorption performance, and enhances the capillary function by adjusting the pore size of the upper and lower layers, and designs a porous structure of the upper and lower permeability layer. Combining the structure of the hydrophilic surface layer and the water-repellent bottom layer, a liquid reservoir is formed to prevent blood accumulation and re-seepage.
It effectively improves the liquid transmission ability, prevents blood from agglomerating on the surface of the absorbent core, reduces slow absorption and lateral leakage, ensures faster absorption and prevents re-seepage, and improves the comfort of using sanitary napkins.
Smart Images

Figure CN2024091435_21112024_PF_FP_ABST
Abstract
Description
Absorbent product and preparation method thereof Technical Field
[0001] The present invention belongs to the technical field of sanitary products, and in particular relates to an absorbent product and a preparation method thereof. Background Art
[0002] Sanitary napkins are sanitary products invented to help women have a better quality of life during menstruation. After years of development, the designs of sanitary napkins have become more and more diverse, thereby improving comfort at different levels.
[0003] However, in the absorbent core structure used in traditional liquid sanitary napkins, when female users use them, blood clots are easily accumulated on the surface of the absorbent core when menstrual blood penetrates downward on the surface of the absorbent core, which causes the absorbent core to absorb slowly, resulting in side leakage and easy back seepage of the sanitary napkin.
[0004] In summary, there is an urgent need to develop a new technical solution to solve the problems existing in the existing technology and meet the development needs of the current market.
[0005] Summary of the Invention
[0006] In order to overcome the defects of the existing technology, the present invention introduces a large number of active functional groups by adding modified acrylates with a hyperbranched structure. After reacting with acrylic acid monomers, an absorbent core with stronger absorption performance can be obtained. At the same time, the present invention adjusts the pore size of the upper and lower layers of the absorbent core so that the product can produce good capillary action, further improving the liquid transfer capacity, and solving the problems of slow liquid absorption, side leakage and easy back seepage caused by the easy accumulation of menstrual blood on the surface of the absorbent core. Therefore, it has good application prospects.
[0007] An object of the present invention is to provide an absorbent article comprising an absorbent core (1), wherein the absorbent core (1) comprises:
[0008] An upper permeable layer and a lower permeable layer, wherein the upper permeable layer and the lower permeable layer are an integrated polymer microporous foam structure, the upper permeable layer is provided with a plurality of first permeable holes, and the lower permeable layer is provided with a plurality of second permeable holes, wherein the pore diameter of the first permeable holes is larger than that of the second permeable holes;
[0009] The upper surface of the absorbent core (1) is provided with a hydrophilic surface layer (2), and the lower surface is provided with a water-repellent bottom layer (3); a non-adhesive area is provided between the absorbent core (1) and the water-repellent bottom layer (3) and a liquid storage cavity (6) is formed;
[0010] The water-repellent bottom layer (3) is provided with a viscose portion on a side away from the absorbent core (1), and the viscose portion is located on both sides of the liquid storage cavity (6);
[0011] The edges of the hydrophilic surface layer (2) and the water-repellent bottom layer (3) are connected by a peripheral sealing embossed layer (5), and the hydrophilic surface layer (2) and the water-repellent bottom layer (3) are bonded to each other by a glue layer, so as to seal the absorbent core (1) between the hydrophilic surface layer (2) and the water-repellent bottom layer (3). A vertical hole area is provided on the absorbent core (1), and a non-glue area is provided between the water-repellent bottom layer (3) and the vertical hole area, so that the vertical hole area and the water-repellent bottom layer (3) are not bonded, thereby forming the liquid storage cavity (6);
[0012] in,
[0013] The absorbent core (1) is obtained by reacting acrylate monomer, modified acrylate, crosslinking agent, photoinitiator, emulsifier and initiator;
[0014] The modified acrylate is obtained by reacting the reaction product of isosorbide and glycidyl ether with acrylic acid.
[0015] Furthermore, the preparation method of the modified acrylate comprises the following steps:
[0016] S1. isosorbide, glycidyl ether, and a catalyst are added to a solvent, the reaction is heated under an inert gas atmosphere, and after cooling, the reaction is allowed to settle, washed, and dried to obtain an intermediate product;
[0017] S2. adding the intermediate product and polymerization inhibitor to a solvent, heating and stirring, and adding a mixed solution of a catalyst and acrylic acid. After the reaction, sedimentation, washing, and drying are performed to obtain the modified acrylate.
[0018] Furthermore, in step S1, the temperature of the heating reaction is 60-70°C; and in step S2, the temperature of the heating and stirring is 80-100°C.
[0019] Furthermore, the glycidyl ether is selected from one or more of triglycidyl ether and pentaerythritol glycidyl ether.
[0020] Furthermore, the preparation method of the absorbent core (1) comprises the following steps:
[0021] L1. The acrylate monomer, modified acrylate, crosslinker, photoinitiator and emulsifier are mixed to obtain an oil phase 1, and then an aqueous phase A comprising an inorganic salt and an aqueous phase B comprising an initiator are added to obtain a high internal phase emulsion 1;
[0022] L2. The acrylate monomer, modified acrylate, crosslinker, photoinitiator and emulsifier are mixed to obtain an oil phase 2, and then an aqueous phase C comprising an inorganic salt and an aqueous phase D comprising an initiator is added to obtain a high internal phase emulsion 2;
[0023] L3. The high internal phase emulsion 1 and the high internal phase emulsion 2 are respectively applied to the upper and lower surfaces of the fabric, and the absorbent core is obtained by light exposure, steam treatment, dehydration and drying.
[0024] Furthermore, the high internal phase emulsion 1 and the high internal phase emulsion 2 are prepared using a continuous emulsification device.
[0025] Furthermore, the pore size of the first permeable pore is 60-130 μm, and the pore size of the second permeable pore is 5-40 μm.
[0026] Furthermore, a plurality of through holes (10) penetrating the absorbent core (1) are provided in the vertical hole region, a guide region located on the absorbent core (1) is provided on one side of the vertical hole region, and a plurality of arc-shaped guide grooves (11) arranged along the length direction of the absorbent core (1) are provided in the guide region, and the lengths of the plurality of arc-shaped guide grooves (11) decrease toward the vertical hole region.
[0027] Furthermore, both the hydrophilic surface layer (2) and the water-repellent bottom layer (3) have wing portions (4), and the adhesive portion comprises a first adhesive strip (12) and a second adhesive strip (13) arranged on the water-repellent bottom layer (3), wherein the first adhesive strip (12) is located on the wing portion (4), and the second adhesive strip (13) is symmetrically arranged on both sides of the liquid storage cavity (6).
[0028] Furthermore, the connection between the wing portion (4) and the hydrophilic surface layer (2) and the water-repellent bottom layer (3) is provided with an arc-shaped corner (8), and the edge of the arc-shaped corner (8) is provided with an embossed separation area, so that the hydrophilic surface layer (2) and the water-repellent bottom layer (3) are completely separated from the peripheral embossed layer (5) at the edge of the wing portion (4);
[0029] The circumferential sealing embossed layer (5) is provided with at least two layers, and each layer of the circumferential sealing embossed layer (5) is composed of a plurality of evenly arranged embossed holes (7). The embossed holes (7) on the two adjacent layers of the circumferential sealing embossed layers (5) are on the same straight line. The number of embossed holes (7) on the embossed separation area of at least two layers of the circumferential sealing embossed layers (5) decreases toward the absorbent core (1), so that at least two layers of the circumferential sealing embossed layers (5) form an inclined line (9) at the end near the embossed separation area; so that the end of the circumferential sealing embossed layer at the arc angle (8) is arranged obliquely, so as to further reduce the development of fracture and prevent the wing portion from being torn off.
[0030] Furthermore, the inorganic salt is selected from one or more of chlorides or sulfates of alkaline earth metals, chlorides or sulfates of alkali metals;
[0031] The fabric is selected from woven fabric or non-woven fabric.
[0032] Furthermore, the acrylate monomer 1 and the acrylate monomer 2 are alkyl acrylate or alkyl methacrylate, and the alkyl group in the alkyl acrylate or alkyl methacrylate is selected from a C4-C20 alkyl group.
[0033] Furthermore, the cross-linking agent is ethylene glycol dimethacrylate.
[0034] Furthermore, the wavelength of the light is 205-450nm and the intensity is 40-1000mW / cm 2 , time is 5-180s.
[0035] Furthermore, the initiator is selected from one or more of ammonium persulfate, sodium persulfate, potassium persulfate, and azo initiators.
[0036] Furthermore, the photoinitiator is preferably one or more of benzophenone, benzil, thioxanthone, benzyl ketal, α-hydroxyalkyl phenone, α-aminoalkyl phenone and acylphosphine oxide.
[0037] The emulsifier added in the present invention has a dispersing and emulsifying effect on the monomers, providing the necessary conditions for the formation and stability of the emulsion. The emulsifier includes two types: primary emulsifier and auxiliary emulsifier. The primary emulsifier is a hydrophobic emulsifier, which is conducive to dispersing the polymerized monomers and reducing their solubility in water; the primary emulsifier is selected from monoglycerol, diglycerol, 3-10 polyglycerol mono- or polystearate, isostearate and oleate, more preferably diglycerol monoisostearate or oleate and poly-3-glycerol monoisostearate or oleate. The auxiliary emulsifier is selected from C2-C4 short carbon and C12-C22 long carbon chain aliphatic betaine or quaternary ammonium salt, more preferably propyl dimethyl ammonium bromide and dioctadecyl dimethyl ammonium bromide.
[0038] Specifically, the present invention relates to the following embodiments:
[0039] 1. An absorbent article, comprising:
[0040] A hydrophilic surface layer, a water-repellent bottom layer, and an absorbent core disposed therebetween;
[0041] wherein the absorbent core comprises a high internal phase emulsion foam, and the high internal phase emulsion foam comprises an acrylate monomer, a modified acrylate, a crosslinking agent, a photoinitiator and an emulsifier;
[0042] wherein the modified acrylate is obtained by reacting the reaction product of isosorbide and glycidyl ether with acrylic acid;
[0043] The absorbent core includes an upper permeable layer and a lower permeable layer, wherein the upper permeable layer includes a plurality of first permeable holes having a first pore size, and the lower permeable layer includes a plurality of second permeable holes having a second pore size, wherein the first pore size is larger than the second pore size.
[0044] 2. The absorbent article according to embodiment 1, wherein the glycidyl ether is selected from one or more of triglycidyl ether and pentaerythritol glycidyl ether.
[0045] 3. The absorbent article according to any one of the preceding embodiments, wherein the emulsifier comprises a primary emulsifier and a secondary emulsifier.
[0046] 4. An absorbent article according to embodiment 3, wherein the primary emulsifier is selected from monoglycerol, diglycerol, 3-10 polyglycerol mono- or polystearate, isostearate and oleate, preferably diglycerol monoisostearate or oleate and poly-3-glycerol monoisostearate or oleate.
[0047] 5. The absorbent article according to embodiment 4, wherein the auxiliary emulsifier is selected from C2-C4 short carbon and C12-C22 long carbon chain fatty betaines or quaternary ammonium salts, preferably propyldimethylammonium bromide and dioctadecyldimethylammonium bromide.
[0048] 6. The absorbent article according to any one of the preceding embodiments, wherein the first pore size is from 60 to 130 μm.
[0049] 7. The absorbent article according to any one of the preceding embodiments, wherein the second pore size is from 5 to 40 μm.
[0050] 8. The absorbent article according to any one of the preceding embodiments, wherein the method for preparing the modified acrylate comprises the following steps:
[0051] a. adding isosorbide, glycidyl ether and a catalyst to a solvent, heating the mixture under an inert gas atmosphere to carry out a reaction, cooling the mixture, and then settling the cooled mixture, washing and drying to obtain an intermediate product; and
[0052] b. adding the intermediate product and the polymerization inhibitor to a solvent, heating and stirring, adding a mixed solution of a catalyst and acrylic acid, reacting, settling, washing and drying to obtain the modified acrylate.
[0053] 9. The absorbent article according to embodiment 8, wherein in step (a), the temperature of the heating reaction is 60 to 70°C, and wherein in step (b), the temperature of the heating and stirring is 80-100°C.
[0054] 10. The absorbent article according to any one of the preceding embodiments, wherein the aqueous phase comprises an initiator; wherein the initiator is selected from one or more of ammonium persulfate, sodium persulfate, potassium persulfate, and azo initiators.
[0055] 11. The absorbent article according to any one of the preceding embodiments, wherein the photoinitiator is one or more of benzophenone, benzil, thioxanthone, benzyl ketal, α-hydroxyalkyl phenone, α-aminoalkyl phenone, and acylphosphine oxide.
[0056] 12. A method for preparing an absorbent core, the method comprising the following steps:
[0057] a. mixing an acrylate monomer, a modified acrylate, a crosslinker, a photoinitiator, and an emulsifier to form an oil phase;
[0058] b. adding the aqueous phase to the oil phase to form a first high internal phase emulsion;
[0059] c. depositing the first high internal phase emulsion on the surface;
[0060] d. exposing the first high internal phase emulsion to light treatment;
[0061] e. The first high internal phase emulsion is placed in a steam tunnel oven;
[0062] f. Dehydrating and drying the high internal phase emulsion to obtain the absorbent core;
[0063] The modified acrylate is obtained by reacting the reaction product of isosorbide and glycidyl ether with acrylic acid.
[0064] 13. The method according to embodiment 12, wherein the glycidyl ether is selected from one or more of triglycidyl ether and pentaerythritol glycidyl ether.
[0065] 14. The method of embodiment 12 or 13, wherein the aqueous phase comprises an initiator; wherein the initiator is selected from one or more of ammonium persulfate, sodium persulfate, potassium persulfate, and an azo initiator.
[0066] 15. The method according to any one of embodiments 12 to 14, wherein the oil phase comprises 60 parts by weight of isooctyl acrylate, 15 parts by weight of modified acrylate, 20 parts by weight of the crosslinker, 1 part by weight of the photoinitiator, and 5 parts by weight of an emulsifier.
[0067] 16. The method according to any one of embodiments 12 to 15, wherein the preparation method of the modified acrylate comprises the following steps:
[0068] a. adding isosorbide, glycidyl ether and a catalyst to a solvent, heating the mixture under an inert gas atmosphere to carry out a reaction, cooling the mixture, and then settling the cooled mixture, washing and drying to obtain an intermediate product; and
[0069] b. adding the intermediate product and the polymerization inhibitor to a solvent, heating and stirring, adding a mixed solution of a catalyst and acrylic acid, reacting, settling, washing and drying to obtain the modified acrylate.
[0070] 17. The method according to any one of embodiments 12 to 16, further comprising mixing a second acrylate monomer, a second modified acrylate, a second crosslinker, a second photoinitiator, and a second emulsifier to form a second oil phase; and adding a second aqueous phase to the second oil phase to form a second high internal phase emulsion.
[0071] 18. The method of embodiment 17, wherein the second high internal phase emulsion is deposited on the first high internal phase emulsion.
[0072] The beneficial effects of the present invention are:
[0073] 1. The present invention uses modified acrylate to compound with acrylic monomer and cross-linking agent to prepare an absorbent core with stronger adsorption performance. On the one hand, the modified acrylate has a hyperbranched structure, so it can form a more three-dimensional cross-linked structure during the polymerization reaction; on the other hand, the present invention introduces a large number of organic functional groups, including hydroxyl groups, ester groups, epoxy groups, etc., which can produce strong intermolecular forces and are more likely to form a synergistic effect with ingredients such as emulsifiers, which is conducive to building a more stable and uniform structure, so that the product has a higher porosity and a dense microporous structure, and realizes a stronger 3D three-dimensional fluid storage function.
[0074] 2. The absorbent core of the present invention is composed of an upper permeable layer and a lower permeable layer, wherein the plurality of first permeable holes in the upper permeable layer and the plurality of second permeable holes in the lower permeable layer cooperate with each other, and the permeable holes are cross-linked with each other. When the pore size of the first permeable hole is larger than that of the second permeable hole, menstrual blood enters the upper permeable layer having the first permeable holes with large pore size on the surface of the absorbent core, and then quickly disperses into the lower permeable layer, so that the menstrual blood is quickly and evenly dispersed and stored in the lower permeable layer, ensuring that the blood does not accumulate on the surface of the sanitary napkin, and preventing the menstrual blood from easily accumulating on the surface of the absorbent core and causing slow liquid absorption; and the liquid storage cavity provided between the absorbent core and the water-repellent bottom layer enables the menstrual blood to quickly penetrate downward into the liquid storage cavity when the amount of menstrual blood is large, store liquid through the liquid storage cavity, and then be reabsorbed by the absorbent core again, effectively preventing the menstrual blood from seeping back; in addition, the absorbent product can be conveniently attached to underwear through the viscose portion. Since the viscose portion is located on both sides of the liquid storage cavity, the liquid storage cavity is prevented from being torn and leaking during the process of tearing off the absorbent product. BRIEF DESCRIPTION OF THE DRAWINGS
[0075] FIG1 is a schematic front view of the absorbent article of the present invention.
[0076] FIG2 is a schematic diagram of the rear structure of the absorbent article of the present invention.
[0077] FIG3 is a schematic cross-sectional view of the absorbent article of the present invention.
[0078] FIG4 is an enlarged structural diagram of point A in FIG1 .
[0079] Figure markings: 1-absorbent core, 2-hydrophilic surface layer, 3-water-repellent bottom layer, 4-wing portion, 5-circumferential sealing embossed layer, 6-liquid storage chamber, 7-pressed hole, 8-arc corner, 9-inclined line, 10-through hole, 11-arc guide groove, 12-first adhesive strip, 13-second adhesive strip.
[0080] FIG5 is an electron microscope image of the upper permeation layer and the lower permeation layer in Example 1.
[0081] FIG6 is a graph showing the surface results of the blood absorption rate test in the test example;
[0082] The left side is the test result diagram of comparative example 1, and the right side is the test result diagram of embodiment 1.
[0083] FIG7 is a diagram showing the back side of the blood absorption rate test result in the test example;
[0084] The left side is the test result diagram of comparative example 1, and the right side is the test result diagram of embodiment 1. DETAILED DESCRIPTION
[0085] In order to more clearly illustrate the technical solutions of the present invention, the following examples are given. Unless otherwise stated, the raw materials, reactions and post-processing methods mentioned in the examples are common raw materials on the market and technical methods well known to those skilled in the art.
[0086] The cross-linking agent in the embodiment of the present invention is ethylene glycol dimethacrylate.
[0087] The initiator in the embodiment of the present invention is ammonium persulfate.
[0088] The photoinitiator in the embodiment of the present invention is 1-hydroxycyclohexyl phenyl ketone (photoinitiator 184).
[0089] The emulsifier in the embodiment of the present invention is diglycerol monoisostearate and dioctadecyl dimethyl ammonium bromide in a mass ratio of 1:1.
[0090] The “parts” in the embodiments of the present invention refer to parts by mass.
[0091] Example 1
[0092] An absorbent article comprising an absorbent core (1), wherein the absorbent core (1) comprises:
[0093] An upper permeable layer and a lower permeable layer, wherein the upper permeable layer and the lower permeable layer are an integrated polymer microporous foam structure, the upper permeable layer is provided with a plurality of first permeable holes, and the lower permeable layer is provided with a plurality of second permeable holes, wherein the pore diameter of the first permeable holes is larger than that of the second permeable holes;
[0094] The upper surface of the absorbent core (1) is provided with a hydrophilic surface layer (2), and the lower surface is provided with a water-repellent bottom layer (3); a non-adhesive area is provided between the absorbent core (1) and the water-repellent bottom layer (3) and a liquid storage cavity (6) is formed;
[0095] The water-repellent bottom layer (3) is provided with a viscose portion on a side away from the absorbent core (1), and the viscose portion is located on both sides of the liquid storage cavity (6);
[0096] The edges of the hydrophilic surface layer (2) and the water-repellent bottom layer (3) are connected by a peripheral sealing embossed layer (5), and the hydrophilic surface layer (2) and the water-repellent bottom layer (3) are bonded to each other by a glue layer, so that the absorbent core (1) is sealed between the hydrophilic surface layer (2) and the water-repellent bottom layer (3). A vertical hole area is provided on the absorbent core (1), and a non-glue area is provided between the water-repellent bottom layer (3) and the vertical hole area, so that the vertical hole area and the water-repellent bottom layer (3) are not bonded, thereby forming the liquid storage cavity (6);
[0097] A plurality of through holes (10) penetrating the absorbent core (1) are provided in the vertical hole region, a flow guide region located on the absorbent core (1) is provided on one side of the vertical hole region, a plurality of arc-shaped flow guide grooves (11) arranged along the length direction of the absorbent core (1) are provided in the flow guide region, and the lengths of the plurality of arc-shaped flow guide grooves (11) decrease toward the vertical hole region;
[0098] The hydrophilic surface layer (2) and the water-repellent bottom layer (3) both have wing portions (4), and the adhesive portion comprises a first adhesive strip (12) and a second adhesive strip (13) arranged on the water-repellent bottom layer (3), wherein the first adhesive strip (12) is located on the wing portion (4), and the second adhesive strip (13) is symmetrically arranged on both sides of the liquid storage cavity (6);
[0099] The connection between the wing portion (4) and the hydrophilic surface layer (2) and the water-repellent bottom layer (3) is provided with an arc-shaped corner (8), and the edge of the arc-shaped corner (8) is provided with an embossed separation area, so that the hydrophilic surface layer (2) and the water-repellent bottom layer (3) are completely separated from the peripheral embossed layer (5) at the edge of the wing portion (4);
[0100] The circumferential sealing embossed layer (5) is provided with at least two layers, each layer of the circumferential sealing embossed layer (5) is composed of a plurality of evenly arranged embossed holes (7), the embossed holes (7) on two adjacent layers of the circumferential sealing embossed layer (5) are on the same straight line, and the number of embossed holes (7) on the embossed separation area of at least two layers of the circumferential sealing embossed layer (5) decreases toward the absorbent core (1), so that at least two layers of the circumferential sealing embossed layer (5) form an inclined line (9) at the end near the embossed separation area;
[0101] in,
[0102] The absorbent core (1) is obtained by reacting acrylate monomer, modified acrylate, crosslinking agent, photoinitiator, emulsifier and initiator.
[0103] The preparation method of the modified acrylate comprises the following steps:
[0104] S1. Isosorbide, glycidyl ether (isosorbide: glycidyl ether = 1:1, n / n), and a catalytic amount of tetrabutylammonium bromide were added to tetrahydrofuran, and the mixture was heated at 65°C under a nitrogen atmosphere for 50 h. After cooling, cyclohexane was added for precipitation, and the mixture was washed with deionized water and diethyl ether, and then dried in vacuo to obtain an intermediate product.
[0105] S2. The intermediate product and polymerization inhibitor (1% by mass of hydroquinone) are added to a solvent (1,4-dioxane), heated and stirred at 100°C, and a mixture of catalyst DMA and acrylic acid (epoxy groups in the intermediate product: acrylic acid = 2:1, n / n) is added dropwise. The acid value is then checked at intervals of 30 minutes. The reaction is terminated when the acid value no longer changes. After cooling, the mixture is precipitated and washed with deionized water, and vacuum dried to obtain the modified acrylate.
[0106] The preparation method of the absorbent core (1) comprises the following steps:
[0107] L1. 60 parts of isooctyl acrylate, 15 parts of modified acrylate, 20 parts of crosslinker, 1 part of photoinitiator, and 5 parts of emulsifier were mixed to obtain oil phase 1. Then, aqueous phase A containing 2% by mass of calcium chloride and aqueous phase B containing 7% by mass of initiator were added. The volume ratio of the oil phase 1, aqueous phase A, and aqueous phase B was 1:25:1 to obtain a high internal phase emulsion 1.
[0108] Specifically, in the continuous emulsification device, the oil phase is prepared in the oil phase material storage tank, the inorganic salt phase is prepared in the water phase material storage tank, and the initiator water phase is prepared in the initiator storage tank. When the emulsification device is stably running, the emulsion part of the primary mixing and emulsification in the first static mixer module is controlled to be transported back to the first emulsification kettle by the first reflux constant flow pump, and the emulsion part of the secondary mixing and emulsification in the second static mixer module is controlled to be transported back to the second emulsification kettle by the second reflux constant flow pump; the reflux flow rate is precisely controlled by the first reflux constant flow pump, and at the same time, the oil phase in the oil phase material storage tank and the water phase in the water phase material storage tank are continuously transported to the first emulsification kettle by the oil phase feeding constant flow pump and the water phase feeding constant flow pump respectively, and are premixed with the emulsion being mixed and emulsified in the kettle to obtain a premixed material, and the premixed material is transported to the first static mixer module for mixing and emulsification to obtain a premixed emulsion 1 with a water-oil ratio of 14:1;
[0109] The premixed emulsion 1 is partially controlled to be transported to the first emulsification kettle through the first reflux constant flow pump and is controlled to be transported to the second emulsification kettle through the premixed emulsion 1 feeding constant flow pump. The premixed emulsion 1 in the premixed emulsion 1 feeding constant flow pump is premixed with the aqueous phase continuously transported to the second emulsification kettle through the aqueous phase feeding constant flow pump to obtain a premixed material. The premixed material is transported to the second static mixer module for mixing and emulsification to obtain premixed emulsion 2; the premixed emulsion 2 is partially controlled to be transported to the second emulsification kettle through the second reflux constant flow pump and is controlled to be transported to the third static mixer module through the constant flow pump and is finally mixed and emulsified with the initiator aqueous phase continuously transported by the initiator feeding constant flow pump. After mixing and emulsification, a high internal phase emulsion 1 is obtained, which is continuously transported to the next process through the emulsified product output interface;
[0110] L2. 45 parts of isooctyl acrylate, 5 parts of modified acrylate, 10 parts of crosslinker, 1 part of photoinitiator, and 2 parts of emulsifier were mixed to obtain oil phase 2, followed by the addition of aqueous phase C containing 1% by mass of calcium chloride and aqueous phase D containing 8% by mass of initiator. The volume ratio of the oil phase 2, aqueous phase C, and aqueous phase D was 1:32:1 to obtain a high internal phase emulsion 2.
[0111] The treatment process of high internal phase emulsion 2 in the continuous emulsification device is the same as that described in L1;
[0112] L3. The high internal phase emulsion 1 is applied to the lower surface of the non-woven fabric to a thickness of 1.5 mm; the high internal phase emulsion 2 is applied to the upper surface of the non-woven fabric to a thickness of 0.5 mm; then a wavelength of 450 nm and an intensity of 50 mW / cm 2 The absorbent core is irradiated with light for 120 seconds, then placed in a steam tunnel oven for curing for 5 minutes, and dehydrated, dried, and cut to obtain the absorbent core.
[0113] FIG1 is a schematic front view of the absorbent article of the present invention.
[0114] FIG2 is a schematic rear structural view of the absorbent article of the present invention.
[0115] FIG3 is a schematic cross-sectional view of the absorbent article of the present invention.
[0116] FIG4 is an enlarged structural diagram of point A in FIG1 .
[0117] Figure markings: 1-absorbent core, 2-hydrophilic surface layer, 3-water-repellent bottom layer, 4-wing portion, 5-circumferential sealing embossed layer, 6-liquid storage chamber, 7-pressed hole, 8-arc corner, 9-inclined line, 10-through hole, 11-arc guide groove, 12-first adhesive strip, 13-second adhesive strip.
[0118] FIG5 is an electron microscope image of the upper permeation layer and the lower permeation layer in Example 1. It can be seen that the pore size of the first permeation pore is 60-130 μm, and the pore size of the second permeation pore is 5-40 μm.
[0119] Comparative Example 1
[0120] An absorbent product. The difference between this comparative example and Example 1 is that in steps L1 and L2, the modified acrylate is replaced with acrylate of equal mass, and other materials and preparation methods are the same as those in Example 1.
[0121] Comparative Example 2
[0122] An absorbent product. The difference between this comparative example and Example 1 is that no emulsifier is added in steps L1 and L2, and other materials and preparation methods are the same as those in Example 1.
[0123] Test Case
[0124] A performance comparison test was performed on Example 1 and Comparative Examples 1-2.
[0125] Test method: GB / T14207-2008 was used to test water absorption and blood absorption.
[0126] The test results are shown in Table 1.
[0127] Table 1 Absorption performance test results
[0128] FIG6 is a graph showing the surface results of the blood absorption rate test in the test example;
[0129] The left side is the test result diagram of comparative example 1, and the right side is the test result diagram of embodiment 1.
[0130] FIG7 is a diagram showing the back side of the blood absorption rate test result in the test example;
[0131] The left side is the test result diagram of comparative example 1, and the right side is the test result diagram of embodiment 1.
[0132] According to Table 1, Example 1 of the present invention uses a modified acrylic ester compounded with acrylic monomer and other ingredients to produce a good synergistic effect. The absorbent product prepared has excellent liquid absorption capacity, and its penetration time, back-infiltration amount, water absorption amount and other data are significantly better than those of Comparative Examples 1-2. However, due to the replacement of the modified acrylic ester component in Comparative Example 1, the absorbent core obtained by the reaction is difficult to form a more three-dimensional and dense microporous structure, which significantly reduces the absorption capacity of the core and fails to produce an ideal capillary action. Comparative Example 2 deletes the emulsifier component and cannot obtain a suitable emulsion for polymerization. The product performance is greatly reduced, resulting in poor liquid conductivity and absorption efficiency. In addition, Comparative Example 1 showed obvious leakage and exudation in the blood absorption rate test, while the absorbent sample prepared in the example was able to keep the liquid in the liquid storage cavity, effectively preventing the phenomenon of menstrual blood back-infiltration.
[0133] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above and that the invention can be embodied in other specific forms without departing from the spirit or essential characteristics of the invention. Therefore, the embodiments should be considered in all respects as illustrative and non-restrictive, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations that come within the meaning and range of equivalents of the claims be embraced therein.
[0134] In addition, it should be understood that although this specification is described in terms of implementation methods, not every implementation method contains only one independent technical solution. This description is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment can also be appropriately combined to form other implementation methods that can be understood by those skilled in the art.
Claims
1. An absorbent article, comprising: A hydrophilic surface layer, a water-repellent bottom layer, and an absorbent core disposed therebetween; wherein the absorbent core comprises a high internal phase emulsion foam, and the high internal phase emulsion foam comprises an acrylate monomer, a modified acrylate, a crosslinking agent, a photoinitiator and an emulsifier; wherein the modified acrylate is obtained by reacting the reaction product of isosorbide and glycidyl ether with acrylic acid; The absorbent core comprises an upper permeable layer and a lower permeable layer, wherein the upper permeable layer comprises a plurality of first permeable holes having a first pore size, and the lower permeable layer comprises a plurality of second permeable holes having a second pore size, wherein the first pore size is larger than the second pore size.
2. The absorbent article according to claim 1, wherein the glycidyl ether is selected from one or more of triglycidyl ether and pentaerythritol glycidyl ether.
3. The absorbent article according to any one of the preceding claims, wherein the emulsifier comprises a primary emulsifier and a secondary emulsifier.
4. An absorbent article according to claim 3, wherein the primary emulsifier is selected from monoglycerol, diglycerol, 3-10 polyglycerol mono- or polystearate, isostearate and oleate, preferably diglycerol monoisostearate or oleate and poly-3-glycerol monoisostearate or oleate.
5. The absorbent article according to claim 4, wherein the auxiliary emulsifier is selected from C2-C4 short carbon and C12-C22 long carbon chain aliphatic betaines or quaternary ammonium salts, preferably propyl dimethyl ammonium bromide and dioctadecyl dimethyl ammonium bromide.
6. The absorbent article according to any one of the preceding claims, wherein the first pore size is from 60 to 130 μm.
7. The absorbent article according to any one of the preceding claims, wherein the second pore size is from 5 to 40 μm.
8. The absorbent article according to any one of the preceding claims, wherein the process for preparing the modified acrylate comprises the following steps: a. adding isosorbide, glycidyl ether and a catalyst to a solvent, heating the mixture under an inert gas atmosphere to react, cooling the mixture, and then settling the cooled mixture, washing and drying to obtain an intermediate product; as well as b. adding the intermediate product and the polymerization inhibitor into a solvent, heating and stirring, adding a mixed solution of a catalyst and acrylic acid, reacting, settling, washing and drying to obtain the modified acrylate.
9. The absorbent article according to claim 8, wherein in step (a), the temperature of the heating reaction is 60°C to 70°C, and wherein in step (b), the temperature of the heating and stirring is 80-100°C.
10. The absorbent article according to any one of the preceding claims, wherein the aqueous phase comprises an initiator; wherein the initiator is selected from one or more of ammonium persulfate, sodium persulfate, potassium persulfate and azo initiators.
11. The absorbent article according to any one of the preceding claims, wherein the photoinitiator is one or more of benzophenone, benzil, thioxanthone, benzyl ketal, α-hydroxyalkyl phenone, α-aminoalkyl phenone and acylphosphine oxide.
12. A method for preparing an absorbent core, the method comprising the following steps: a. mixing an acrylate monomer, a modified acrylate, a crosslinker, a photoinitiator and an emulsifier to form an oil phase; b. adding an aqueous phase to the oil phase to form a first high internal phase emulsion; c. depositing the first high internal phase emulsion on a surface; d. exposing the first high internal phase emulsion to light treatment; e. placing the first high internal phase emulsion into a steam tunnel oven; f. Dehydrating and drying the high internal phase emulsion to obtain the absorbent core; The modified acrylate is obtained by reacting a reaction product of isosorbide and glycidyl ether with acrylic acid.
13. The method according to claim 12, wherein the glycidyl ether is selected from one or more of triglycidyl ether and pentaerythritol glycidyl ether.
14. The method according to claim 12 or 13, wherein the aqueous phase comprises an initiator; wherein the initiator is selected from one or more of ammonium persulfate, sodium persulfate, potassium persulfate and an azo initiator.
15. The method according to any one of claims 12 to 14, wherein the oil phase comprises 60 parts by weight of isooctyl acrylate, 15 parts by weight of modified acrylate, 20 parts by weight of the crosslinking agent, 1 part by weight of the photoinitiator and 5 parts by weight of an emulsifier.
16. The method according to any one of claims 12 to 15, wherein the preparation method of the modified acrylate comprises the following steps: a. adding isosorbide, glycidyl ether and a catalyst to a solvent, heating the mixture under an inert gas atmosphere to react, cooling the mixture, and then settling the cooled mixture, washing and drying to obtain an intermediate product; as well as b. adding the intermediate product and the polymerization inhibitor into a solvent, heating and stirring, adding a mixed solution of a catalyst and acrylic acid, reacting, settling, washing and drying to obtain the modified acrylate.
17. The method according to any one of claims 12 to 16, further comprising mixing a second acrylate monomer, a second modified acrylate, a second crosslinker, a second photoinitiator, and a second emulsifier to form a second oil phase; and adding a second water phase to the second oil phase to form a second high internal phase emulsion.
18. The method of claim 17, wherein the second high internal phase emulsion is deposited on the first high internal phase emulsion.
Citation Information
Patent Citations
Acrylic ester porous polymer and manufacturing method thereof
CN108084330A
Menstrual blood absorbing material
CN108524998A
Preparation method of acrylic ester foam material absorption core body
CN113289049A
Method for preparing open-cell foam material from ultrahigh-internal-phase Pickering emulsion, foam absorbing material and application of foam absorbing material
CN113980344A
Water-absorbing foam based on double emulsifiers and preparation method of water-absorbing foam
CN115215961A