Wet etching method for improving critical dimension uniformity

By controlling the replacement and spraying time of the etching liquid in the wet etching device, the problem of inconsistency in characteristic size caused by the evaporation of the etching liquid during wet etching is solved, the consistency of product characteristic size is achieved, and the yield and performance of the product are improved .

WO2024239195A1PCT designated stage expired Publication Date: 2024-11-28BEIJING ADVANCED MEMORY TECH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/095495
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-22
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

The evaporation of moisture of the etching liquid during wet etching leads to an increase in the etching rate, resulting in inconsistent feature sizes, affecting the yield and performance of the product.

Method used

By setting an acid tank, spray head and conduit in the wet etching device, the replacement and spraying time of the etching liquid are controlled, and the uniform etching of the semiconductor component is achieved by using platform rotation, and the etching time is adjusted to maintain the consistency of the characteristic size.

Benefits of technology

Improve the consistency of the characteristic size of the etched products at different times, and improve the yield and performance of the products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023095495_28112024_PF_FP_ABST
    Figure CN2023095495_28112024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention belongs to the field of integrated-circuit manufacturing. Provided is a wet etching method for improving critical dimension uniformity. The wet etching method in the present invention comprises: a step of forming a semiconductor assembly, which involves forming a semiconductor assembly on a semiconductor substrate of a wafer; a step of replacing an etching solution, which involves replacing an etching solution in an acid tank; and a step of performing etching, which involves: guiding the etching solution from the acid tank to a sprayer by means of a guide tube, spraying the etching solution onto the surface of the wafer by means of the sprayer while a platform drives the wafer to rotate, so as to etch the semiconductor assembly, and controlling an etching time t according to the interval L between the step of replacing the etching solution and the step of performing etching. By means of the wet etching method in the present invention, critical dimension uniformity can be improved, thereby improving the yield and performance of products.
Need to check novelty before this filing date? Find Prior Art

Description

Wet etching method to improve feature size uniformity Technical Field

[0001] The present invention relates to the field of integrated circuit manufacturing, and in particular to a wet etching method for improving feature size consistency. Background Art

[0002] Wet etching requires the use of an etchant, which typically has a shelf life and cannot be used beyond that point. Therefore, the etchant must be replaced periodically before etching can resume. However, over time, the water in the etchant evaporates, causing the etchant concentration to increase, leading to a continuous increase in the etch rate. This can cause the CD (characteristic dimension) of the etched key hole to increase when etching structures such as key holes. After a period of time, when the etchant is replaced with a new one, the CD of the etched key hole will decrease again. This results in inconsistent CDs for products etched at different times, reducing product yield and affecting product performance. Technical issues

[0003] The present invention aims to provide a wet etching method capable of improving CD consistency. Technical Solutions

[0004] The wet etching device used in the wet etching method for improving CD consistency provided by the present invention includes: a chamber, a platform arranged at the bottom of the chamber for placing a wafer, a nozzle arranged at the top of the chamber for spraying etching liquid onto the wafer, an acid tank arranged outside the chamber for storing the etching liquid, a conduit connecting the nozzle and the acid tank, and a waste liquid collection component arranged around the platform. The wet etching method includes: a semiconductor component forming step of forming a semiconductor component on a semiconductor substrate of the wafer; an etching liquid replacing step of replacing the etching liquid in the acid tank; and an etching step of guiding the etching liquid in the acid tank to the nozzle through the conduit, and spraying the etching liquid onto the surface of the wafer through the nozzle, while the platform drives the wafer to rotate, thereby etching the semiconductor component, and controlling the etching time t according to the interval L between the etching liquid replacing step and the etching step. Beneficial effects

[0005] The wet etching method of the present invention can improve the CD consistency of products etched at different times, thereby improving the yield and performance of the products. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] FIG1 is a schematic diagram of a wet etching apparatus according to the present invention;

[0007] FIG2 is a flow chart of a wet etching method of the present invention;

[0008] FIG3 is a schematic diagram of a semiconductor device before wet etching according to the present invention; and

[0009] FIG. 4 is a schematic diagram of a semiconductor device after wet etching according to the present invention.

[0010] Explanation of symbols

[0011] 100 Wet etching equipment

[0012] 1 chamber

[0013] 2 wafers

[0014] 3 Platform

[0015] 4 nozzles

[0016] 5 Acid Tanks

[0017] 6 Catheter

[0018] 7 Waste liquid collection parts

[0019] 10. Semiconductor substrate

[0020] 11. First silicon nitride layer

[0021] 12 Silicon oxide layer

[0022] 13. Second silicon nitride layer

[0023] 14 First Hole

[0024] 15 Second Hole

[0025] 16 The third hole

[0026] 20 semiconductor components Best Mode for Carrying Out the Invention

[0027] The wet etching method for improving CD uniformity of the present invention will be described below with reference to FIG. 1 to FIG. 4 .

[0028] As shown in Figure 1, the wet etching device 100 used in the wet etching method of the present invention includes: a chamber 1, a platform 3 arranged at the bottom of the chamber 1 for placing a wafer 2, a nozzle 4 arranged at the top of the chamber 1 for spraying etching liquid onto the wafer 2, an acid tank 5 arranged outside the chamber 1 for storing the etching liquid, a conduit 6 connecting the nozzle 4 and the acid tank 5, and a waste liquid collection component 7 arranged around the platform 3.

[0029] In this embodiment, the wet etching apparatus 100 is a DV-PRIME wet etching apparatus from LAM Corporation in the United States. However, the present invention is not limited thereto; other wet etching apparatuses may also be used. The etching solution comprises HF (hydrofluoric acid), NH₄F (ammonium fluoride), and water. This etching solution is primarily used for etching silicon oxide. However, the present invention is not limited thereto; etching solutions with other components may also be used.

[0030] As shown in FIG2 and FIG3, the wet etching method of the present invention includes:

[0031] Semiconductor device forming step S100 : forming a semiconductor device 20 on a semiconductor substrate 10 of a wafer 2 .

[0032] In this embodiment, semiconductor component 20 includes a first silicon nitride layer 11, a silicon oxide layer 12, and a second silicon nitride layer 13. However, the present invention is not limited thereto. Semiconductor component 20 may also have other structures, as long as they can be etched using a wet etching process. Semiconductor substrate 10 may be a silicon substrate or a substrate made of other materials, such as ceramic, organic, or glass. Semiconductor component 20 may be formed directly on semiconductor substrate 10, or other layers may be present between semiconductor component 20 and semiconductor substrate 10.

[0033] Preferably, the semiconductor component forming step S100 includes: forming a first silicon nitride layer 11, a silicon oxide layer 12 and a second silicon nitride layer 13 on the semiconductor substrate 10 of the wafer 2, and forming a first hole 14 in the silicon oxide layer 12, and forming a second hole 15 in the second silicon nitride layer 13, and the diameter D1 of the first hole 14 is equal to the diameter D2 of the second hole 15.

[0034] The first silicon nitride layer 11, the silicon oxide layer 12, and the second silicon nitride layer 13 can be formed using methods commonly used in the art, such as PVD (physical vapor deposition) and CVD (chemical vapor deposition) processes. The first holes 14 can be formed in the silicon oxide layer 12, and the second holes 15 can be formed in the second silicon nitride layer 13 using methods commonly used in the art, such as photolithography and etching processes.

[0035] As shown in FIG1 and FIG2, the wet etching method of the present invention further includes:

[0036] Etching solution replacement step S200: Replace the etching solution in the acid tank 5. The etching solution in this embodiment has a life cycle (life time) of approximately three days, so the etching solution in the acid tank 5 is replaced every three days. However, the present invention is not limited to this, and other number of days may also be used.

[0037] As shown in FIG1-3, the wet etching method of the present invention further includes:

[0038] Etching step S300: The etching liquid in the acid tank 5 is guided to the nozzle 4 through the conduit 6, and the etching liquid is sprayed onto the surface of the wafer 2 through the nozzle 4. At the same time, the platform 3 drives the wafer 2 to rotate, thereby etching the semiconductor component 20, and the etching time t is controlled according to the interval time L between the etching liquid replacement step S200 and the etching step S300.

[0039] Specifically, etching time t refers to the time it takes for the nozzle 4 to spray the etching solution and the time it takes for the platform 3 to rotate the wafer 2. In this embodiment, the waste liquid collection component 7 is cylindrical and positioned around the platform 3. As the wafer 2 rotates at high speed, the etching solution is thrown onto the waste liquid collection component 7 and then discharged from the chamber 1 through a drainage device (not shown) on the waste liquid collection component 7.

[0040] Preferably, as shown in Figures 1 and 4, etching step S300 includes: using an etching solution to perform pull-back etching on the silicon oxide layer 12, thereby forming a third hole 16 in the silicon oxide layer 12. The diameter D3 of the third hole 16 is larger than the diameter D2 of the second hole 15. In this embodiment, the etching solution performs pull-back etching on the silicon oxide layer 12, but the present invention is not limited to this embodiment, and other etching methods may also be used.

[0041] Preferably, the longer the interval L, the shorter the etching time t. Because the longer the interval L, the more water evaporates from the etching solution, the higher the concentration of the etching solution, and the higher the etching rate (Etch Rate). Therefore, in order to maintain a consistent diameter D3 (i.e., CD) of the third hole 16 after etching, the etching time t needs to be appropriately reduced. In this embodiment, on the day the etching solution is changed, that is, when the interval L is 0 days, the etching time is t0. When the interval L is 1 day, the etching time is t1. When the interval L is 2 days, the etching time is t2. Here, t0>t1>t2. This ensures that the CD of key holes etched on different days remains consistent, thereby improving product yield and performance.

[0042] Although the present invention has been disclosed in the form of embodiments as described above, they are not intended to limit the present invention. Any professional and technical personnel in this field may make various necessary changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be based on the scope defined by the attached claims. Industrial Applicability

[0043] The wet etching method of the present invention can improve the CD consistency of products etched at different times, thereby improving the yield and performance of the products.

Claims

1. A wet etching method for improving feature size consistency, characterized in that: The wet etching device (100) used in the wet etching method comprises: a chamber (1), a platform (3) arranged at the bottom of the chamber (1) for placing a wafer (2), a nozzle (4) arranged at the top of the chamber (1) for spraying etching liquid onto the wafer (2), an acid tank (5) arranged outside the chamber (1) for storing the etching liquid, a conduit (6) connecting the nozzle (4) and the acid tank (5), and a waste liquid collection component (7) arranged around the platform (3). The wet etching method comprises: Semiconductor component forming step: forming a semiconductor component (20) on the semiconductor substrate (10) of the wafer (2); Etching liquid replacement step: replacing the etching liquid in the acid tank (5); and Etching step: the etching liquid in the acid tank (5) is guided to the nozzle (4) through the conduit (6), and the etching liquid is sprayed onto the surface of the wafer (2) through the nozzle (4), while the platform (3) drives the wafer (2) to rotate, thereby etching the semiconductor component (20), and the etching time t is controlled according to the interval time L between the etching liquid replacement step and the etching step.

2. The wet etching method for improving feature size consistency according to claim 1, characterized in that: The semiconductor component forming step comprises: forming a first silicon nitride layer (11), a silicon oxide layer (12) and a second silicon nitride layer (13) on the semiconductor substrate (10), forming a first hole (14) in the silicon oxide layer (12), and forming a second hole (15) in the second silicon nitride layer (13), wherein a diameter D1 of the first hole (14) is equal to a diameter D2 of the second hole (15).

3. The wet etching method for improving feature size consistency according to claim 2, characterized in that: The etching step comprises: the etching solution performs side etching on the silicon oxide layer (12), thereby forming a third hole (16) in the silicon oxide layer (12), wherein a diameter D3 of the third hole (16) is greater than a diameter D2 of the second hole (15).

4. The wet etching method for improving feature size consistency according to claim 1, characterized in that: The larger the interval time L is, the shorter the etching time t is.

Citation Information

Patent Citations

  • Semiconductor device and method for accurate wet etching and wafer edge cleaning

    CN113436995A

  • Silicon wafer etching method and etching apparatus

    CN113614890A

  • Wet etching method and wet etching device for metal silicification layer

    CN113921393A

  • Silicon nitride mask layer etching solution, preparation method, application and etching method

    CN116023946A

  • Etching method, etching device and storage medium

    JP2015088603A