Fluidic self-assembly method applicable to micro-nano device

By performing surface treatment and two-step alignment process on micro-nano devices and assembled substrates, the problems of poor assembly accuracy and complex substrate preparation in fluid self-assembly technology are solved, and efficient and accurate assembly of micro-nano devices is achieved.

WO2024240235A1PCT designated stage expired Publication Date: 2024-11-28BEIJING UNIV OF CHEM TECH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/095019
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-25
Filing Date
2024-05-23
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

The existing fluid self-assembly technology has problems such as poor assembly accuracy of micro-nano devices, complex assembly substrate preparation, and difficult to take into account both assembly efficiency and accuracy.

Method used

By surface treatment of micro-nano devices and assembled substrates, the surface energy has similar differences. A liquid bridge is formed in the fluid using a two-step alignment process to achieve fine alignment and stable combination of micro-nano devices and assembled substrates, simplifying The structure and preparation process of assembling the substrate.

Benefits of technology

It improves the self-assembly accuracy of fluids, simplifies the preparation process of assembling substrates and micro-nano devices, solves the contradiction between assembly accuracy and efficiency, and achieves efficient and accurate assembly of micro-nano devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024095019_28112024_PF_FP_ABST
    Figure CN2024095019_28112024_PF_FP_ABST
Patent Text Reader

Abstract

A fluidic self-assembly method applicable to a micro-nano device. The method comprises: S1, separately subjecting a micro-nano device and an assembly substrate (2) to a surface treatment; S2, in a first assembly container (31), assembling the modified micro-nano device and the modified assembly substrate (2) in a solution B (362) or at an interface to complete primary alignment and form a primary assembly of the micro-nano device and the assembly substrate (2); S3, transferring the primary assembly into a second assembly container (32), and enabling a liquid bridge consisting of a solution A (361) between the micro-nano device and the assembly substrate (2) in the primary assembly to be controllably dissolved in or volatilized into a fluid C (363), so as to complete secondary alignment and form a final assembly; and S4, taking out the final assembly from the second assembly container (32), and subjecting same to a post-treatment to make the micro-nano device and the assembly substrate be stably bonded, thereby achieving the conduction of various physical and chemical properties and completing a packaging process. By means of a two-step alignment process, the disappearing speed of the liquid bridge is regulated and controlled, thereby solving the problems of relatively low assembly efficiency and relatively poor assembly precision during fluidic self-assembly of a microelectronic device.
Need to check novelty before this filing date? Find Prior Art

Description

Fluid self-assembly method for micro-nano devices

[0001] Cross-references

[0002] This application claims priority to the Chinese patent application filed with the China Patent Office, application number 2023106051152, application date May 25, 2023, and application name “A fluid self-assembly method for micro-nano devices”. The entire contents of the application are incorporated by reference into this application. Technical Field

[0003] The present application relates to the field of semiconductor technology, and in particular to a fluid self-assembly method applied to micro-nano devices. Background Art

[0004] With the advancement of science and technology, microelectronic systems have gradually developed. These systems achieve functions such as display, sensing, and photoelectric conversion by integrating large numbers of tiny components at high density onto driver circuit boards. For example, micro-LED display technology, which integrates tens of millions of micro-LED chips, offers advantages over traditional display technologies, such as high energy conversion efficiency, fast response time, long lifespan, and high contrast. The fabrication of these microelectronic systems often requires the high-density and high-precision integration of numerous microelectronic devices onto driver circuit boards to achieve the desired functions. These demands necessitate a high-efficiency, high-precision, high-density, and low-cost microelectronic integration technology. Mass transfer technology has emerged as a result.

[0005] Mass transfer technology refers to the process of arranging millions, or even tens of millions, of small-scale micro-nano devices onto a driver panel in a rational and orderly manner. The development and advancement of micro-nano manufacturing technology has placed higher demands on transfer accuracy, efficiency, yield, and cost.

[0006] Among the existing mass transfer technology routes, fluid self-assembly technology has attracted the attention of researchers with its advantages of low cost and high efficiency. Fluid self-assembly technology uses mechanical principles such as fluid force and shape matching to allow micro-nano devices to fall into pre-made special structures to achieve the effect of self-assembly. After the micro-nano devices are dispersed in the fluid, they achieve random movement with the help of fluid movement, and are filled and arranged by matching the shape of the groove structure on the receiving panel. Because fluid self-assembly technology does not rely on precision instruments to achieve the capture, positioning, and assembly of micro-nano devices, and the filling process is fast, efficient, and low-cost, it is considered to be the most promising mass transfer technology.

[0007] However, existing fluid self-assembly technologies have the following main disadvantages:

[0008] 1) Poor assembly precision in fluid self-assembly. In existing fluid self-assembly methods based on the principle of surface free energy minimization, the disappearance of the liquid bridge between the micro-nano device and the assembly substrate is uncontrollable, making it difficult to regulate the process of the micro-nano device falling and assembling onto the assembly substrate. The rapid removal of the liquid bridge prevents the micro-nano device from having sufficient time to make fine adjustments, which may lead to horizontal displacement and assembly deviation. Although the absolute error generated by this process is not large, the relative error is large compared to the smaller size of the micro-nano device, affecting the subsequent bonding process.

[0009] 2) It's difficult to balance assembly accuracy and efficiency during fluidic self-assembly. Existing fluidic self-assembly methods often utilize grooves to capture micro-nano devices. In this process, for devices of the same size, larger grooves increase their capture efficiency. However, once a micro-nano device is trapped in a groove, it can still move within the structure, resulting in poor assembly accuracy. Reducing the groove size can effectively improve assembly accuracy, but it also reduces assembly efficiency. Therefore, existing strategies struggle to reconcile the trade-off between assembly accuracy and efficiency.

[0010] 3) The assembly substrate requires a complex three-dimensional structure. In existing fluidic self-assembly methods, in order for the assembly substrate to effectively capture the randomly moving micro-nano devices in the fluid, a three-dimensional structure with grooves or protrusions is often provided on the assembly substrate to facilitate the assembly of the micro-devices and the assembly substrate. The preparation of this three-dimensional structure is complex, significantly increasing the number of steps and difficulty in preparing the assembly substrate.

[0011] 4) Micro-nano devices require complex structures to achieve surface selectivity during assembly. During fluidic self-assembly, micro-nano devices must be assembled onto the assembly substrate with specific surfaces to achieve specific functions. There are two main methods currently used to achieve surface selectivity in micro-nano devices: first, constructing a specific three-dimensional structure on the surface; second, adjusting the center of gravity of the micro-nano device. However, these strategies require additional processing steps, thereby increasing the complexity of the preparation process.

[0012] In view of this, existing fluidic self-assembly technologies still suffer from poor assembly precision, complex preparation of micro-nano devices and assembly substrates, and difficulty balancing assembly efficiency and assembly precision. It is urgent for those skilled in the art to provide a new strategy to address these issues.

[0013] Application Contents

[0014] Purpose of application

[0015] To this end, the present application provides a fluid self-assembly method for microelectronic devices to solve the problems existing in the prior art.

[0016] Solution

[0017] In order to achieve the above objectives, this application provides the following technical solutions:

[0018] A fluid self-assembly method for micro-nano devices, comprising the following steps:

[0019] S1. Surface treatments are performed on the micro-nano device and the assembly substrate. Different surfaces of the micro-nano device have different surface energies. The assembly position and non-assembly position of the assembly substrate also have different surface energies. The surface of the micro-nano device to be assembled and the predetermined assembly position of the assembly substrate have similar surface energies.

[0020] S2. Within a first assembly container, the modified micro-nano device and assembly substrate are dropped through Solution A into Solution B. Under external disturbance, the assembly surface of the micro-nano device and the droplets of Solution A attached to the assembly position of the assembly substrate contact and fuse to form a liquid bridge, completing a primary alignment and forming a primary assembly of the micro-nano device and assembly substrate.

[0021] S3. The primary assembly is transferred to a second assembly container, and the liquid bridge composed of solution A between the micro-nano device and the assembly substrate in the primary assembly is controllably dissolved or evaporated into fluid C to complete the secondary alignment and form the final assembly;

[0022] S4. The final assembly is removed from the second assembly container, and the final assembly consisting of the micro-nano device and the assembly substrate is post-processed to form a stable bond between the two, achieve the conduction of various physical and chemical properties, and complete the packaging process.

[0023] In some embodiments, the micro-nano device has a size ranging from nanometers to centimeters, has a columnar structure, and has a bottom surface of the columnar structure as a first surface. The material of the micro-nano device is at least one of gallium nitride, silicon dioxide, metal, or polymer, and the density of the micro-nano device is greater than the density of solution B.

[0024] In some embodiments, the first surface of the micro-nano device has a different surface energy from other surfaces. The surface energy of the first surface enables it to be wetted by solution A but not by solution B, and the surface energy of other surfaces enables it to be wetted by solution B but not by solution A.

[0025] In some embodiments, the assembly substrate is flat or curved, made of metal, silicon dioxide, or polydimethylsiloxane, and the assembly positions on the surface of the assembly substrate are patterned protrusions, patterned grooves, or planar structures.

[0026] In some embodiments, the surface of the assembly substrate is patterned specifically modified so that different positions on the surface have different surface energies, the size and shape of the assembly position are consistent with the size and shape of the first surface of the micro-nano device, the surface energy of the assembly position on the assembly substrate allows it to be wetted with solution A but not with solution B, and the surface energy of the non-assembly position on the assembly substrate allows it to be wetted with solution B but not with solution A.

[0027] In some embodiments, the fluid disturbance method is a plunger pump, a circulation pump, a peristaltic pump, a brush, a shaker, an oscillation or a centrifugal method.

[0028] In some embodiments, step S2 is replaced by the following steps:

[0029] S201. The modified micro-nano devices are uniformly dispersed at the interface between solution A and solution B, and the assembly substrate is slowly inserted into the solution at any angle of 30-90°. The micro-nano devices are assembled to the assembly position on the assembly substrate based on the interface interaction, completing one alignment and forming a primary assembly of the micro-nano devices and the assembly substrate.

[0030] In some embodiments, in step S2, the upper layer of the first assembly container is solution A, and the lower layer is solution B, and a conveying mechanism leading to the second assembly container is installed at the bottom of the first assembly container, and a disturbing component is installed in the first assembly container for disturbing the solution B;

[0031] The modified micro-nano device and the assembly substrate are transferred to solution B through solution A. During this process, droplets of solution A are attached to the assembly position on the surface of the assembly substrate and the first surface of the micro-nano device.

[0032] The assembly substrate is fixed to a conveyor mechanism at the bottom of the first assembly container, and the patterned, specifically modified surface contacts the solution. Under the action of the flow-disrupting component, the micro-nano device moves irregularly in the solution B. During this process, droplets at the assembly position on the assembly substrate collide and merge with droplets on the first surface of the micro-nano device to form a liquid bridge. Based on interfacial tension, the micro-nano device is assembled at the assembly position on the assembly substrate, completing a primary alignment.

[0033] The assembly status of the assembly substrate and the micro-nano device is monitored in real time by an image monitoring device. After all assembly positions of the assembly substrate are assembled with micro-nano devices, the disturbance of solution B is stopped to form a primary assembly of the assembly substrate and the micro-nano device.

[0034] In some embodiments, in step S3, after the primary assembly is completed, the primary assembly is transferred to a second assembly container via an automatic conveying mechanism;

[0035] The primary assembly enters the second assembly container, where the liquid bridge formed by solution A between the first surface of the micro-nano device and the assembly position of the assembly substrate slowly dissolves or evaporates into fluid C. As the liquid bridge gradually shrinks, the relative position between the assembly position of the micro-nano device and the assembly substrate is finely adjusted due to changes in interfacial tension, completing secondary alignment and forming the final assembly.

[0036] In some embodiments, in step S4, the final assembly is taken out from the second assembly container, and the bonding between the micro-nano device and the assembly substrate is achieved by welding. The welded assembly continues to complete the subsequent packaging process.

[0037] In some embodiments, in step S201, the upper layer of the first assembly container is solution A, the lower layer is solution B, and an automatic conveying mechanism leading to the second assembly container is installed at the bottom of the first assembly container;

[0038] Due to the combined effect of density and surface energy, the modified micro-nano device is evenly dispersed at the interface between solution A and solution B with the first surface facing solution A.

[0039] The assembly substrate is patterned with one side facing the solution and the other side facing the sidewall of the first assembly container, and is slowly inserted into the solution at any angle between 30 and 90 degrees. During the insertion process, due to the difference in surface energy, the assembly position of the assembly substrate is at the interface between solution A and solution B, causing interface deformation, so that the first surface of the micro-nano device is assembled with the assembly position of the assembly substrate, completing a single alignment and forming a primary assembly consisting of the assembly substrate and multiple micro-nano devices. After the assembly substrate with the assembled micro-nano devices is completely immersed in solution B, the angle of the assembly substrate is adjusted, and the side of the assembly substrate with the assembly position faces the solution, and it is fixed to the automatic conveying mechanism at the bottom of the first assembly container.

[0040] In some embodiments, solution A and solution B are immiscible with each other, solution A and fluid C are slightly soluble, solution A is deionized water, saline solution or alkaline solution; solution B is toluene, n-hexane, cyclohexane or xylene; fluid C is ethyl acetate, chloroform, ether or nitrogen. Beneficial effects

[0041] Compared with existing fluid self-assembly technologies, the fluid self-assembly method for micro-nano devices provided in this application has the following technical advantages:

[0042] 1) Improved fluid self-assembly precision. Through a two-step alignment assembly process, the dissolution or evaporation rate of the liquid bridge between the micro-nano device and the assembly substrate is regulated. This effectively solves the problem of poor assembly precision caused by the relative displacement of the micro-nano chip and the assembly substrate during the rapid removal of the liquid bridge, which is difficult to finely adjust due to rapid fixation.

[0043] 2) Simplified assembly substrate preparation. The assembly substrate's assembly positions utilize similar surface energies on a flat surface to capture micro-nano devices, eliminating the need for complex three-dimensional assembly substrates and simplifying the fabrication process. This also fundamentally resolves the conflict between assembly accuracy and efficiency in shape-matching fluid self-assembly.

[0044] 3) Simplifies the fabrication process of micro-nano devices. The surface energies of different surfaces in micro-nano devices vary significantly, enabling surface selectivity during assembly without requiring additional structures or fabrication processes. This simplifies the fabrication process of micro-nano devices. BRIEF DESCRIPTION OF THE DRAWINGS

[0045] To more clearly illustrate the embodiments of this application or the technical solutions in the prior art, the following briefly introduces the drawings required for the embodiments or the description of the prior art. Obviously, the drawings described below are merely illustrative, and those skilled in the art can derive other implementation drawings based on the provided drawings without inventive effort.

[0046] The structures, proportions, sizes, etc. illustrated in this specification are only used to match the contents disclosed in the specification so as to facilitate understanding and reading by persons familiar with this technology. They are not intended to limit the conditions under which this application can be implemented, and therefore have no substantive technical significance. Any structural modifications, changes in proportions, or adjustments in sizes should still fall within the scope of the technical contents disclosed in this application without affecting the efficacy and objectives that can be achieved by this application.

[0047] FIG1 is a schematic flow chart of a fluid self-assembly method for microelectronic devices provided in this application;

[0048] FIG2 is a schematic structural diagram of a specific embodiment of the chip provided in this application;

[0049] FIG3 is a cross-sectional view taken along the AA direction in FIG2 ;

[0050] FIG4 is a schematic structural diagram of a specific embodiment of an assembly substrate provided in this application;

[0051] FIG5 is a cross-sectional view taken along the BB direction in FIG4 ;

[0052] FIG6 is a schematic structural diagram of a specific embodiment of the device used in the fluid self-assembly method provided in this application;

[0053] FIG7 is a schematic diagram of a chip and an assembly substrate in a correctly aligned manner in the fluid self-assembly method provided by the present application;

[0054] FIG8 is a schematic diagram of a chip and an assembly substrate in a misaligned state in the fluid self-assembly method provided by the present application;

[0055] FIG9 is a schematic structural diagram of the hot pressing process in the fluid self-assembly method provided in the present application;

[0056] FIG10 is a schematic structural diagram of another specific embodiment of the device used in the fluid self-assembly method provided in this application;

[0057] FIG11 is a schematic structural diagram of another specific embodiment of the device used in the fluid self-assembly method provided in this application.

[0058] Explanation of the accompanying drawings: 1-chip; 12-first electrode, 13-second electrode, 14-insulating layer; 2-assembly substrate; 22-third electrode, 23-fourth electrode; 31-first assembly container, 32-second assembly container, 33-isolation plate A, 34-isolation plate B, 35-conveyor belt, 361-solution A, 362-solution B, 363-fluid C, 37-image monitoring system, 38-plunger pump, 391-discharge valve, 392-temperature and pressure regulating device; 41-hot pressing welding plate. DETAILED DESCRIPTION

[0059] The following specific embodiments illustrate the implementation of this application. People familiar with this technology can easily understand other advantages and functions of this application from the content disclosed in this specification. Obviously, the described embodiments are part of the embodiments of this application, but not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of this application.

[0060] The fluid self-assembly method for micro-nano devices provided in the present application performs surface treatment on the micro-nano devices and the assembly substrate 2 so that the assembly surface of the micro-nano devices and the assembly position of the assembly substrate 2 have similar surface energies. The modified micro-nano devices and the assembly substrate 2 are placed in a pre-built first assembly container 31. In the disturbed fluid, the assembly surface of the micro-nano devices and the droplets attached to the assembly position of the assembly substrate 2 contact and fuse with each other to form a liquid bridge, completing a primary alignment to form a primary assembly of the micro-nano devices and the assembly substrate 2; the primary assembly is transferred to a second assembly container 32, and then the liquid bridge between the micro-nano devices and the assembly substrate 2 in the primary assembly slowly dissolves or evaporates to complete a secondary alignment to form a final assembly. The fluid self-assembly method for micro-nano devices provided in the present application has the advantages of high assembly precision and a simple structure of the micro-nano devices and the assembly substrate 2. The method can be used in the fields of Micro-LED display, flexible solar cells, microelectronics integration, flexible electronics, micro robots, automotive lighting, etc.

[0061] In a specific embodiment, as shown in FIG1 , the fluid self-assembly method for micro-nano devices provided in the present application includes the following steps:

[0062] S1. Surface treatment is performed on the micro-nano device and the assembly substrate 2. Different surfaces of the micro-nano device have different surface energies, and the assembly position and non-assembly position of the assembly substrate 2 also have different surface energies. The surface of the micro-nano device to be assembled and the predetermined assembly position of the assembly substrate 2 have similar surface energies.

[0063] The micro-nano device can be sized from nanometers to centimeters and can be shaped like any columnar structure, such as a cube, cuboid, or cylinder. A bottom surface of the columnar structure serves as the first surface. The material can be single or composite, such as gallium nitride, silicon dioxide, metal, or polymer. The overall density of the micro-nano device should be slightly greater than the density of solution B 362. The first surface of the micro-nano device has a different surface energy than the other surfaces. The surface energy of the first surface allows it to be wetted by solution A 361 but not by solution B 362, while the surface energy of the other surfaces allows it to be wetted by solution B 362 but not by solution A 361.

[0064] In some embodiments, the shape of the assembly substrate 2 can be any shape such as a plane or a curved surface, and the material can be a hard material such as metal, silicon dioxide, or a soft material such as polydimethylsiloxane. The assembly position on the surface of the assembly substrate 2 can be a patterned protrusion / patterned groove / planar structure. The surface of the assembly substrate 2 is pattern-specifically modified so that different positions on the surface have different surface energies. The size and shape of the assembly position are consistent with the size and shape of the first surface of the micro-nano device. The surface energy of the assembly position on the assembly substrate 2 allows it to be wetted by solution A361 but not by solution B362, and the surface energy of the non-assembly position on the assembly substrate 2 allows it to be wetted by solution B362 but not by solution A361.

[0065] S2. Within the first assembly container 31, the modified micro-nano device and assembly substrate 2 are dropped into solution B 362 via solution A 361. Under external disturbance, the assembly surface of the micro-nano device and the droplets of solution A 361 attached to the assembly position of the assembly substrate 2 contact and fuse to form a liquid bridge, completing the primary alignment and forming a primary assembly of the micro-nano device and assembly substrate 2. The fluid disturbance can be achieved by various means, such as a plunger pump, a circulation pump, a peristaltic pump, a brush, a shaker, oscillation, or a centrifuge.

[0066] Furthermore, in step S2, the upper layer of the first assembly container 31 contains solution A 361, and the lower layer contains solution B 362. A conveying mechanism leading to the second assembly container 32 is installed at the bottom of the first assembly container 31. A flow disturbance component is installed within the first assembly container 31 to disturb the solution B 362. The modified micro-nano device and the assembly substrate 2 are transported through solution A 361 into solution B 362. During this process, droplets of solution A 361 adhere to the assembly position on the surface of the assembly substrate 2 and the first surface of the micro-nano device. The assembly substrate 2 is fixed to the conveying mechanism at the bottom of the first assembly container 31, with the patterned, specifically modified surface in contact with the solution. Under the action of the flow disturbance component, the micro-nano device moves irregularly in the solution B 362. During this process, the droplets at the assembly position on the surface of the assembly substrate 2 collide and merge with the droplets on the first surface of the micro-nano device to form a liquid bridge. Based on the interfacial tension, the micro-nano device is assembled at the assembly position of the assembly substrate 2, completing one alignment. The assembly status of the assembly substrate 2 and the micro-nano device is monitored in real time by an image monitoring device. After all assembly positions of the assembly substrate 2 are assembled with micro-nano devices, the disturbance of solution B362 is stopped to form a primary assembly of the assembly substrate 2 and the micro-nano device.

[0067] S3. The primary assembly is transferred to the second assembly container 32. The liquid bridge composed of solution A361 between the micro-nano device and the assembly substrate 2 in the primary assembly is controllably dissolved or evaporated into the fluid C363 to complete the secondary alignment and form the final assembly. In step S3, after the primary assembly is completed, the primary assembly is transferred to the second assembly container 32 via the automatic conveying mechanism; the primary assembly enters the second assembly container 32, and the liquid bridge composed of solution A361 between the first surface of the micro-nano device and the assembly position of the assembly substrate 2 slowly dissolves or evaporates into the fluid C363. As the liquid bridge gradually becomes smaller, the relative position between the assembly position of the micro-nano device and the assembly substrate 2 is finely adjusted due to changes in interfacial tension, completing the secondary alignment and forming the final assembly.

[0068] S4. The final assembly is removed from the second assembly container 32. Post-processing is performed on the final assembly consisting of the micro-nano device and assembly substrate 2 to ensure a stable bond between the two, achieve the transfer of various physical and chemical properties, and complete the packaging process. In step S4, the final assembly is removed from the second assembly container 32 and bonded to the micro-nano device and assembly substrate 2 using welding or other connection methods to achieve electrical and thermal conductivity. The welded assembly then proceeds to complete the subsequent packaging process.

[0069] In some other embodiments, step S2 is replaced by the following steps. It should be understood that the other steps are the same as those in the above embodiment:

[0070] S201. The modified micro-nano device is evenly dispersed at the interface between solution A 361 and solution B 362. Assembly substrate 2 is slowly inserted into the solution at an angle ranging from 30° to 90°. The micro-nano device is assembled into the assembly position on assembly substrate 2 based on interfacial interactions, completing a primary alignment and forming a primary assembly of the micro-nano device and assembly substrate 2.

[0071] In step S201, the upper layer of the first assembly container 31 is solution A361, and the lower layer is solution B362, and the bottom of the first assembly container 31 is equipped with an automatic conveying mechanism leading to the second assembly container 32; due to the combined effect of density and surface energy, the modified micro-nano device is uniformly dispersed at the interface between solution A361 and solution B362 with the first surface contacting solution A361; the patterned modified assembly substrate 2 is slowly inserted into the solution at an arbitrary angle of 30-90° with one side facing the solution and the other side facing the side wall of the first assembly container 31. During the insertion process, due to the difference in surface energy, the assembly position of the assembly substrate 2 is at the interface between solution A361 and solution B362, causing interface deformation, so that the first surface of the micro-nano device is assembled with the assembly position of the assembly substrate 2, completing one alignment and forming a primary assembly consisting of the assembly substrate 2 and multiple micro-nano devices. After the assembly substrate 2 with the micro-nano device assembled thereon is completely immersed in the solution B362, the angle of the assembly substrate 2 is adjusted and it is fixed on the automatic conveying mechanism at the bottom of the first assembly container 31 so that the patterned specific modified surface contacts the solution.

[0072] Specifically, solution A 361 and solution B 362 are mutually immiscible, while solution A 361 and fluid C 363 are slightly soluble. Solution A 361 is a low-viscosity aqueous solution such as deionized water, a saline solution, or an alkaline solution; solution B 362 is a low-viscosity organic solvent that is insoluble in water, such as toluene, n-hexane, cyclohexane, or xylene; and fluid C 363 can be a low-viscosity organic solvent that is slightly soluble in water, such as ethyl acetate, chloroform, or diethyl ether, or a gas such as nitrogen or air.

[0073] For ease of understanding, the implementation process of the method provided in this application is briefly described below using several specific embodiments as examples.

[0074] In Example 1, the fluid self-assembly process of the Micro-LED chip includes the following steps:

[0075] S110: Preparation of chip 1. The structure of Micro-LED chip 1 is shown in Figures 2 and 3. First, a multi-layer gallium nitride structure is prepared on the surface of the growth wafer, and then the light-emitting micro-LED chip 1 is prepared by etching. Its shape can be circular, quadrilateral, hexagonal and other shapes. Here, the preparation process is described using a circular chip 1 as an example. Electrodes are prepared on the surface of the prepared chip 1 using magnetron metal sputtering coating technology, silver paste coating, screen printing technology, chemical deposition technology and other technologies to construct a complete circuit structure. The two electrodes are concentric structures and can be rotationally symmetrical shapes such as circular, quadrilateral, hexagonal, etc. The electrode material is composed of gold, silver, aluminum and other materials. An insulating layer 14 is prepared between the prepared first electrode 12 and the second electrode 13. The insulating layer 14 is composed of insulators such as silicon dioxide, resin, and polymer. The electrodes and the insulating layer 14 are modified to have high surface energy and hydrophilicity by using surface modification methods such as plasma bombardment, dip coating, reactive ion beam etching, and femtosecond laser, while the other parts of the light-emitting device still maintain hydrophobicity.

[0076] S120: Design of assembly substrate 2. The structure of assembly substrate 2 is shown in Figures 4 and 5. First, the entire surface of assembly substrate 2 is modified using surface modification methods such as dip coating, vapor deposition, spray coating, and femtosecond laser lithography to give it a hydrophobic structure. Electrodes are also prepared on the surface of assembly substrate 2 using magnetron metal sputtering, silver paste application, screen printing, and chemical deposition techniques to construct a complete circuit structure. These are the third electrode 22 and the fourth electrode 23, respectively, and their shapes are consistent with those of the electrodes in micro-LED chip 1. The electrode materials are composed of gold, silver, aluminum, and other materials. An insulating layer 14 is formed between the prepared first electrode 12 and the second electrode 13. Insulating layer 14 is composed of an insulator such as silicon dioxide, resin, or polymer. Subsequently, using a high-precision metal template combined with vapor deposition, chemical etching, femtosecond laser lithography, and two-photon lithography, the electrodes and insulating layer 14 are modified to have a high surface energy, resulting in hydrophilic properties. The assembled substrate 2 is hydrophobic as a whole, and the electrodes and the insulating layer 14 are hydrophilic.

[0077] S130: Fluid self-assembly process. The fluid self-assembly process is shown in Figure 6. The entire container is divided into two left and right tanks. The upper layer of the left tank contains solution A361, and the lower layer contains solution B362. As the assembly substrate 2 and micro-LED chip 1 are immersed in solution B362 through the layer of solution A361, the high-surface-energy metal electrodes and the insulating layer 14 adhere to liquid A361, forming droplets. By disturbing the fluid, the micro-LED chip 1 moves randomly within liquid B362. In the immiscible liquid, different liquids adhere to different surfaces of the micro-LED chip 1 and different areas of the assembly substrate 2. During the fluid disturbance, since the electrodes of the micro-LED chip 1 and the assembly substrate 2 adhere to the same liquid A361, self-assembly occurs. Due to the principle of minimizing interfacial energy, initial alignment is achieved, forming the primary assembly shown in Figure 7(a). However, due to the large amount of solution A361 between the electrode surfaces of the micro-LED chip 1 and the electrode locations of the assembly substrate 2, alignment accuracy is insufficient. Solution A361 is a low-viscosity aqueous solution such as pure water, saline solution, or alkaline solution. Liquid B361 is a low-viscosity organic solvent incompatible with solution A361, such as toluene, n-hexane, cyclohexane, or xylene. The fluid is disturbed by various methods, including a plunger pump, brush drive, circulating pump, vertical oscillation, and centrifugation.

[0078] As the micro-LED chips 1 self-assemble in liquid B, the image monitoring system 37 above monitors the assembly process in real time. Once the image monitoring system 37 detects that a micro-LED chip 1 is assembled at each electrode position on the assembly substrate 2, the perturbation ceases. After solution B 362 in the first assembly container 31 stops moving, the isolation plate A 33 opens, and the bottom conveyor mechanism transports the primary assembly consisting of the micro-LED chip 1 and the assembly substrate 2 to the right trough. The isolation plate A 33 then closes. The second assembly container 32 contains fluid C 363. Solution A 361 between the electrode surface of the micro-LED chip 1 and the electrode position of the assembly substrate 2 gradually diffuses and dissolves into fluid C 362, gradually reducing the amount of solution A 361 between the two, and the liquid bridge gradually decreases. Because the surface energies of the electrode surfaces of the micro-LED chip 1 and the electrode surfaces of the assembly substrate 2 are similar, as the liquid bridge gradually decreases, the relative position between the electrode surfaces of the micro-LED chip 1 and the electrode positions of the assembly substrate 2 is finely adjusted due to changes in interfacial tension, completing the secondary alignment and forming the final assembly as shown in Figure 7(b). Compared to existing fluid self-assembly based on the principle of minimizing interfacial free energy, this two-step alignment strategy significantly improves assembly accuracy and can reduce assembly errors to one-tenth of the original. After the final assembly is completed, the rightmost isolation plate B34 is opened to remove the final assembly consisting of the micro-LED chip 1 and the assembly substrate 2 for the next step. Here, the fluid C363 is a low-viscosity organic solvent that is slightly soluble in the solution A361, such as ethyl acetate, chloroform, ether, etc. Figure 8 shows the incorrect contact between the micro-LED chip 1 and the assembly substrate 2. Under fluid disturbance, the assembly interface interaction force of the incorrect structure is weak and easy to remove. Then, through repeated trial and error, it is adjusted to the correct assembly structure and stabilized by strong interfacial forces.

[0079] S140: Bonding and packaging of micro-LED chip 1 and assembly substrate 2. After the micro-LED chip 1 and assembly substrate 2 are properly assembled in the fluid (the bonded structure is shown in Figure 9), the entire assembly is removed from solution C363. Bonding between the micro-LED chip 1 and assembly substrate 2 is completed using various methods such as thermocompression welding, eutectic welding, or soldering to achieve electrical and thermal conductivity. The bonded assembly then proceeds to the subsequent packaging process.

[0080] In Example 2, the fluid self-assembly process of the micro-LED chip 1 includes the following steps.

[0081] S210: The design and preparation process of the micro-LED chip 1 are consistent with those in Example 1.

[0082] S220: The design and preparation process of the assembly substrate 2 is consistent with that of Example 1.

[0083] S230: Fluid Self-Assembly Process. The fluid self-assembly process is shown in Figure 10. The entire container is divided into two left and right chambers. The upper layer of the left chamber contains solution A361, and the lower layer contains solution B362. The overall density of the prepared micro-LED chips 1 is slightly greater than that of solution B362. Due to the combined effects of density and interfacial tension, all micro-LED chips 1 are dispersed at the interface between solution A361 and solution B362, with electrodes contacting solution A361 and light-emitting devices contacting solution B362. Assembly substrate 2, with one side decorated with electrode sites facing the solution and the other facing the left sidewall of the chamber, is slowly inserted into the solution at a certain angle. The angle between assembly substrate 2 and the liquid surface is 30° to 90°, and the speed is 0.1-10 cm / s. Because the electrodes on the surface of assembly substrate 2 are hydrophilic, as assembly substrate 2 passes through the liquid-liquid interface between solution A361 and solution B362, it pulls on the liquid surface to deform, causing the electrodes of the micro-LED chips 1, which are also hydrophilic, to assemble with the electrodes on assembly substrate 2. The two achieve the first stage of alignment based on the principle of minimizing interfacial free energy. The electrode surface of micro-LED chip 1 is aligned with the electrode position of assembly substrate 2. Assembly substrate 2 continues to descend until the entire assembly substrate 2 is completely immersed in solution B362. At this point, all electrode positions on assembly substrate 2 are assembled with micro-LED chips 1, forming a primary assembly. Assembly substrate 2 lands on conveyor belt 35, and the assembly configuration at this point resembles that shown in Figure 7(a). Due to the large amount of solution A361 between micro-LED chip 1 and assembly substrate 2 at this point, the droplets are large, resulting in insufficient alignment accuracy. Isolator A33 opens, and the bottom conveyor belt 35 moves rightward, transporting assembly substrate 2 with micro-LED chip 1 to the right trough. Isolator A33 then closes. The right trough contains fluid C363. Solution A361 between the electrode surface of micro-LED chip 1 and the electrode position of assembly substrate 2 gradually diffuses and dissolves into fluid C363, gradually reducing the amount of solution A361 between the two, and the liquid bridge gradually decreases. Because the surface energy of the electrode surface of the micro-LED chip 1 is similar to that of the electrode position of the assembly substrate 2, as the liquid bridge gradually becomes smaller, the relative position between the electrode surface of the micro-LED chip 1 and the electrode position of the assembly substrate 2 is finely adjusted due to the change in interfacial tension, completing the secondary alignment and forming the final assembly shown in Figure 7 (b). Compared with the existing fluid self-assembly based on the principle of minimizing interfacial free energy, this two-step alignment strategy significantly improves the assembly accuracy and can reduce the assembly error to one-tenth of the original. After the assembly is completed, open the rightmost isolation plate B34 to remove the final assembly and proceed to the next step. Here, solution A361 is a low-viscosity aqueous solution such as pure water, salt solution, alkaline solution, etc., and liquid B362 is a low-viscosity organic solvent incompatible with solution A361, such as toluene, n-hexane, cyclohexane, xylene, etc.Fluid C363 is a low-viscosity organic solvent that is slightly soluble in solution A361, such as ethyl acetate, chloroform, or ether.

[0084] S240: The bonding process of the micro-LED chip 1 and the assembly substrate 2 is consistent with that in Example 1.

[0085] In Example 3, the fluid self-assembly process of the micro-LED chip 1 includes the following steps:

[0086] S310: The design and preparation process of the micro-LED chip 1 are consistent with those in Example 1.

[0087] S320: The design and preparation process of the assembly substrate 2 is consistent with that of Example 1.

[0088] S330: Fluid self-assembly process. The assembly process for the primary assembly is consistent with that of Example 1. As shown in Figure 11, after the primary assembly is formed, the transport mechanism transports the primary assembly consisting of the micro-LED chip 1 and the assembly substrate 2 to the second assembly container 32 containing fluid C363. The bottom drain valve 391 is opened to drain excess liquid from the second assembly container 32. Due to surface tension, a liquid bridge composed of solution A361 still exists between the electrodes of the micro-LED chip 1 and the electrodes of the assembly substrate 2. The temperature and pressure regulating device 392 regulates the temperature and pressure of fluid C363 in the second assembly container 32 to maintain the saturated vapor pressure of solution A362 in the right tank at an appropriate level, thereby facilitating the gradual evaporation of solution A361 between the electrode surface of the micro-LED chip 1 and the electrode of the assembly substrate 2 into fluid C363. The amount of solution A361 between the two electrodes gradually decreases, and the liquid bridge gradually decreases. Because the surface energy of the electrode surface of micro-LED chip 1 is similar to that of the electrode position of assembly substrate 2, as the liquid bridge gradually decreases, the relative position between the electrode surface of micro-LED chip 1 and the electrode position of assembly substrate 2 is finely adjusted due to changes in interfacial tension, completing the secondary alignment and forming the final assembly. Compared with the existing fluid self-assembly based on the principle of minimizing interfacial free energy, this two-step alignment strategy significantly improves assembly accuracy and can reduce the assembly error to one-tenth of the original. After assembly is completed, the rightmost isolation plate B34 is opened to remove the assembled assembly substrate 2 and proceed to the next step. Here, solution A361 is a low-viscosity aqueous solution such as pure water, salt solution, alkaline solution, etc., and liquid B362 is a low-viscosity organic solvent incompatible with solution A, such as toluene, n-hexane, cyclohexane, xylene, etc. Fluid C363 is a gas such as air and nitrogen.

[0089] S340: The bonding process between the chip and the assembly substrate is consistent with that in Example 1.

[0090] Compared with existing fluid self-assembly technologies, the fluid self-assembly method for micro-nano devices provided in this application has the following technical advantages:

[0091] 1) Improved fluid self-assembly precision. Through a two-step alignment assembly process, the dissolution or evaporation rate of the liquid bridge between the micro-nano device and the assembly substrate is regulated. This effectively solves the problem of poor assembly precision caused by the relative displacement of the micro-nano chip and the assembly substrate during the rapid removal of the liquid bridge, which is difficult to finely adjust due to rapid fixation.

[0092] 2) Simplified assembly substrate preparation. The assembly substrate's assembly positions utilize similar surface energies on a flat surface to capture micro-nano devices, eliminating the need for complex three-dimensional assembly substrates and simplifying the fabrication process. This also fundamentally resolves the conflict between assembly accuracy and efficiency in shape-matching fluid self-assembly.

[0093] 3) Simplifies the fabrication process of micro-nano devices. The surface energies of different surfaces in micro-nano devices vary significantly, enabling surface selectivity during assembly without requiring additional structures or fabrication processes. This simplifies the fabrication process of micro-nano devices.

[0094] The above specific implementation methods further illustrate the purpose, technical solutions and beneficial effects of this application in detail. It should be understood that the above are only specific implementation methods of this application and are not intended to limit the scope of protection of this application. Any modifications, equivalent replacements, improvements, etc. made on the basis of the technical solutions of this application should be included in the scope of protection of this application.

Claims

1. A fluid self-assembly method for micro-nano devices, It is characterized in that The following steps are involved: S1. The micro-nano device and the assembly substrate are subjected to surface treatment respectively, different surfaces of the micro-nano device have different surface energies, the assembly position and the non-assembly position of the assembly substrate also have different surface energies, and the surface of the micro-nano device to be assembled and the preset assembly position of the assembly substrate have similar surface energies; S2. In the first assembly container, the modified micro-nano device and the assembly substrate are dropped into solution B through solution A. Under external disturbance, the assembly surface of the micro-nano device and the droplets composed of solution A attached to the assembly position of the assembly substrate contact and fuse with each other to form a liquid bridge, completing one alignment and forming a primary assembly of the micro-nano device and the assembly substrate; S3. The primary assembly is transferred to a second assembly container, and the liquid bridge composed of solution A between the micro-nano device in the primary assembly and the assembly substrate is controllably dissolved or volatilized into fluid C to complete the secondary alignment and form a final assembly; S4. The final assembly is taken out from the second assembly container, and the final assembly consisting of the micro-nano device and the assembly substrate is post-processed to form a stable bond between the two, achieve the conduction of various physical and chemical properties, and complete the packaging process.

2. The fluid self-assembly method for micro-nano devices according to claim 1, It is characterized in that The micro-nano device has a size of nanometer to centimeter level, has a columnar structure, and has a bottom surface of the columnar structure as a first surface. The material of the micro-nano device is at least one of gallium nitride, silicon dioxide, metal or polymer, and the density of the micro-nano device is greater than the density of solution B.

3. The fluid self-assembly method for micro-nano devices according to claim 1, It is characterized in that The first surface of the micro-nano device has a different surface energy from other surfaces. The surface energy of the first surface enables it to be wetted by solution A but not by solution B, and the surface energy of other surfaces enables it to be wetted by solution B but not by solution A.

4. The fluid self-assembly method for micro-nano devices according to claim 1, It is characterized in that The shape of the assembly substrate is a plane or a curved surface, the material of the assembly substrate is metal, silicon dioxide or polydimethylsiloxane, and the assembly position on the surface of the assembly substrate is a patterned protrusion, a patterned groove or a plane structure.

5. The fluid self-assembly method for micro-nano devices according to claim 1, It is characterized in that The surface of the assembly substrate is patterned and specifically modified so that different positions on the surface have different surface energies. The size and shape of the assembly position are consistent with the size and shape of the first surface of the micro-nano device. The surface energy of the assembly position on the assembly substrate allows it to be wetted with solution A but not with solution B. The surface energy of the non-assembly position on the assembly substrate allows it to be wetted with solution B but not with solution A.

6. The fluid self-assembly method for micro-nano devices according to claim 1, It is characterized in that The fluid disturbance method is a plunger pump, a circulation pump, a peristaltic pump, a brush, a shaker, an oscillation or a centrifugal method.

7. The fluid self-assembly method for micro-nano devices according to any one of claims 1 to 6, It is characterized in that Step S2 is replaced by the following steps: S201. The modified micro-nano devices are uniformly dispersed at the interface between solution A and solution B, and the assembly substrate is slowly inserted into the solution at any angle of 30-90°. The micro-nano devices are assembled to the assembly positions on the assembly substrate based on the interface interaction, completing one alignment and forming a primary assembly of the micro-nano devices and the assembly substrate.

8. The fluid self-assembly method for micro-nano devices according to claim 7, It is characterized in that In step S2, the upper layer of the first assembly container is solution A, the lower layer is solution B, and a conveying mechanism leading to the second assembly container is installed at the bottom of the first assembly container, and a flow disturbance component is installed in the first assembly container for disturbing the solution B; The modified micro-nano device and the assembly substrate are sent to solution B through solution A. During this process, droplets composed of solution A are attached to the assembly position on the surface of the assembly substrate and the first surface of the micro-nano device; The assembly substrate is fixed on the conveying mechanism at the bottom of the first assembly container, and the patterned specific modified surface is in contact with the solution. Under the action of the spoiler, the micro-nano device moves irregularly in the solution B. In this process, the surface of the assembly substrate The liquid droplets at the assembly position of the assembly substrate collide and merge with the liquid droplets on the first surface of the micro-nano device to form a liquid bridge, and based on the interfacial tension, the micro-nano device is assembled at the assembly position of the assembly substrate, completing an alignment; The assembly status of the assembly substrate and the micro-nano device is monitored in real time by an image monitoring device. After all assembly positions of the assembly substrate are assembled with the micro-nano device, the disturbance of solution B is stopped to form a primary assembly of the assembly substrate and the micro-nano device.

9. The fluid self-assembly method for micro-nano devices according to any one of claims 1 to 6, It is characterized in that In step S3, after the primary assembly is completed, the primary assembly is transferred to the second assembly container via the automatic conveying mechanism; The primary assembly enters the second assembly container, and the liquid bridge formed by solution A between the first surface of the micro-nano device and the assembly position of the assembly substrate slowly dissolves or evaporates into fluid C. In the process of the liquid bridge gradually becoming smaller, the relative position between the assembly position of the micro-nano device and the assembly substrate is finely adjusted due to the action of interfacial tension, completing the secondary alignment and forming the final assembly.

10. The fluid self-assembly method for micro-nano devices according to any one of claims 1 to 6, It is characterized in that In step S4, the final assembly is taken out from the second assembly container, and the micro-nano device is bonded to the assembly substrate by welding. The welded assembly continues to complete the subsequent packaging process.

11. The fluid self-assembly method for micro-nano devices according to claim 7, It is characterized in that In step S201, the upper layer of the first assembly container is solution A, the lower layer is solution B, and an automatic conveying mechanism leading to the second assembly container is installed at the bottom of the first assembly container; Due to the combined effect of density and surface energy, the modified micro-nano device is evenly dispersed at the interface between solution A and solution B with the first surface facing solution A; The assembly substrate is patterned and modified with one side facing the solution and the other side facing the side wall of the first assembly container, and is slowly inserted into the solution at any angle of 30-90°. During the insertion process, due to the difference in surface energy, the assembly position of the assembly substrate is at the interface between solution A and solution B, causing interface deformation, so that the first surface of the micro-nano device is assembled with the assembly position of the assembly substrate, completing one alignment, and forming a primary assembly consisting of the assembly substrate and multiple micro-nano devices; After the assembly substrate with the micro-nano device assembled thereon is completely immersed in solution B, the angle of the assembly substrate is adjusted so that the side of the assembly substrate with the assembly position faces the solution and is fixed on the automatic conveying mechanism at the bottom of the first assembly container.

12. The fluid self-assembly method for micro-nano devices according to claim 7, It is characterized in that Solution A and solution B are immiscible with each other, solution A and fluid C are slightly soluble, solution A is deionized water, saline solution or alkaline solution; solution B is toluene, n-hexane, cyclohexane or xylene; fluid C is ethyl acetate, chloroform, ether or nitrogen.

Citation Information

Patent Citations

  • Self-supporting nano assembly material and preparation method thereof

    CN107746468A

  • Micro-nano material self-assembly method, substrate and application

    CN110065925A

  • Preparation method of patterned organic semiconductor and deformation tensile test method

    CN113772620A

  • Method for preparing micro-nano-scale full-liquid-phase fluid channel

    CN115245796A

  • Method and apparatus for microstructure assembly

    US20080016682A1